  1. Electrical resistivity measurements to predict abrasion resistance of ...

    Indian Academy of Sciences (India)

    WINTEC

    increasing expansion of highway and other construction works and decreasing natural aggregate resources in the world, the demand for crushed stone aggregates has in- creased from day-to-day. One of the important properties of rock aggregates is abrasion resistance. The abrasion resistance of aggregates is generally ...

  2. Usage of abrasion-resistant materials in agriculture

    Directory of Open Access Journals (Sweden)

    J Votava

    2014-06-01

    Full Text Available Agricultural soil-processing machines are subject to an extensive abrasive wear. This paper analyses technical materials and their fitness to exchangeable parts of plough bottoms, such as edge-tools and whole plough cutting edges. There were tested abrasion-resistant steels with different microstructures: austenite, martensite-bainite, and carbide. Steel with the pearlite-ferrite structure was used as an etalon. Abrasion resistance tests were processed in compliance with the norm CSN 01 5084, which is a test of abrasion wear on abrasive cloth.

  3. Electrical resistivity measurements to predict abrasion resistance

    Indian Academy of Sciences (India)

    Home; Journals; Bulletin of Materials Science; Volume 31; Issue 2. Electrical resistivity measurements to predict abrasion resistance of rock aggregates ... It was seen that correlation coefficients were increased for the rock classes. In addition ...

  4. Solidification structure and abrasion resistance of high chromium white irons

    Science.gov (United States)

    Doğan, Ö. N.; Hawk, J. A.; Laird, G.

    1997-06-01

    Superior abrasive wear resistance, combined with relatively low production costs, makes high Cr white cast irons (WCIs) particularly attractive for applications in the grinding, milling, and pumping apparatus used to process hard materials. Hypoeutectic, eutectic, and hypereutectic cast iron compositions, containing either 15 or 26 wt pct chromium, were studied with respect to the macrostructural transitions of the castings, solidification paths, and resulting microstructures when poured with varying superheats. Completely equiaxed macrostructures were produced in thick section castings with slightly hypereutectic compositions. High-stress abrasive wear tests were then performed on the various alloys to examine the influence of both macrostructure and microstructure on wear resistance. Results indicated that the alloys with a primarily austenitic matrix had a higher abrasion resistance than similar alloys with a pearlitic/bainitic matrix. Improvement in abrasion resistance was partially attributed to the ability of the austenite to transform to martensite at the wear surface during the abrasion process.

  5. Abrasion Resistance of as-Cast High-Chromium Cast Iron

    Directory of Open Access Journals (Sweden)

    Pokusová Marcela

    2014-12-01

    Full Text Available High chromium cast irons are widely used as abrasion resistant materials. Their properties and wear resistance depend on carbides and on the nature of the matrix supporting these carbides. The paper presents test results of irons which contain (in wt.% 18-22 Cr and 2-5 C, and is alloyed by 1.7 Mo + 5 Ni + 2 Mn to improve the toughness. Tests showed as-cast irons with mostly austenitic matrix achieved hardness 36-53 HRC but their relative abrasion-resistance was higher than the tool steel STN 19436 heat treated on hardness 60 HRC.

  6. Photochemical surface modification of PP for abrasion resistance

    International Nuclear Information System (INIS)

    Bahners, Thomas; Haessler, Ruediger; Gao Shanglin; Maeder, Edith; Wego, Andreas; Schollmeyer, Eckhard

    2009-01-01

    The potential of a photo-chemical approach to increase the surface hardness of polypropylene (PP) has been studied. Using a 222 nm excimer lamp, fibers and film were irradiated in the presence of multi-functional substances diallylphthalate (DAP), tetraallyloxyethane (TAE), and pentaerithritoltriacylate (PETA) and characterized with regard to the resulting effect on abrasion resistance. AFM-based methods were employed to analyze thermo-mechanical surface properties. Nanoindentation and microthermal analyses of the outermost surface layers of UV treated fibers gave clear indications of an effective cross-linking of reactive substances present during irradiation. One may assume that the reactive media polymerize on top of the surface of the PP substrate and form a thin-layer. The abrasion resistance of the PP fibers was tested by applying stress through a rotating and axially oscillating roller of defined roughness and measuring the mass loss as a function of time. The abrasion resistance was found to be remarkably improved compared to the untreated fiber. Best effects were achieved using PETA as reactive substance. The experiments clearly showed the influence of processing conditions, namely with regard to homogeneous coverage of the substrate surface with the reactive medium.

  7. Development of abrasion resistant glass-ceramics from industrial waste products. Final report

    Energy Technology Data Exchange (ETDEWEB)

    von Roode, M.

    1983-05-26

    Slag-ceramics were produced from glass compositions using pelletized slag as the major ingredient. The abrasion resistance, fracture toughness and microstructure of the prepared glass and glass-ceramics were evaluated. Glas-ceramics with good abrasion resistance were obtained when iron oxide in conjunction with carbon was used as a nucleating agent. 5 figs., 11 tabs.

  8. Assessment of thermal spray coatings for wear and abrasion resistance applications

    Science.gov (United States)

    Karode, Ishaan Nitin

    Thermal spray cermet and metallic coatings are extensively used for wear, abrasion and corrosion control in a variety of industries. The first part of the thesis focuses mainly on testing of sand erosion resistance of thermal spray coatings on carbon composites used in the manufacture of helicopter rotor blades. The test set-up employed is a sand blasting machine and is an effort to duplicate the in-flight conditions especially those encountered in hot arid conditions. The technique adopted follows the Department of Defence test method standard. Carbon Composites have excellent stiffness, strength and low weight/density. The strength to weight ratio is high. Hence, these are used in aerospace applications to a large extent. However, the biggest problem encountered with carbon composites is its low abrasion resistance as its surface is very weak. Hence, thermal spray coatings are used to improve the surface properties of CFRP. Zinc bond coats and WC-Co coatings were tested. However, high amount of thermal stresses were developed between the substrate and the coating due to large differences in the CTE's of the both, leading to high mass losses within two minutes and just 130 grams of sand sprayed on to the coatings with the sand blasting machine built; and hence the coatings with CC as a substrate could not qualify for the application. The second part of the thesis focuses on the assessment of different thermal spray coatings used for manufacture of mechanical seals in pumps and analyze the best coating material for the wear resistance application through detail quantification of material loss by block-on-ring test set-up. A machine based on Block-on-ring test set-up following ASTM G77 (Measurement of Adhesive wear resistance of thermal spray coatings) standards was built to duplicate the pump conditions. Thermally sprayed coated materials were tested in different conditions (Load, time, abrasive). WC-Co had the highest wear resistance (lower volume losses) and

  9. HYDRO-ABRASIVE RESISTANCE AND MECHANICAL PROPERTIES OF CONCRETE WITH ADDED FLY ASH

    OpenAIRE

    Ristić, Nenad; Grdić, Zoran; Topličić-Ćurčić, Gordana

    2015-01-01

    The durability of hydraulic engineering structures mostly depends on the resistance of their concrete surfaces to mechanical abrasion. In this paper, we study the hydro-abrasive resistance and mechanical properties of concrete in which cement is partially replaced with fly ash in various proportions. To evaluate these concretes, we measured their compressive strength, flexural strength, static modulus of elasticity, ultrasound velocity through concrete, and sclerometer rebound. The hydro-abra...

  10. Resistance to abrasion of extrinsic porcelain esthetic characterization techniques.

    Science.gov (United States)

    Chi, Woo J; Browning, William; Looney, Stephen; Mackert, J Rodway; Windhorn, Richard J; Rueggeberg, Frederick

    2017-01-01

    A novel esthetic porcelain characterization technique involves mixing an appropriate amount of ceramic colorants with clear, low-fusing porcelain (LFP), applying the mixture on the external surfaces, and firing the combined components onto the surface of restorations in a porcelain oven. This method may provide better esthetic qualities and toothbrush abrasion resistance compared to the conventional techniques of applying color-corrective porcelain colorants alone, or applying a clear glaze layer over the colorants. However, there is no scientific literature to support this claim. This research evaluated toothbrush abrasion resistance of a novel porcelain esthetic characterization technique by subjecting specimens to various durations of simulated toothbrush abrasion. The results were compared to those obtained using the conventional characterization techniques of colorant application only or colorant followed by placement of a clear over-glaze. Four experimental groups, all of which were a leucite reinforced ceramic of E TC1 (Vita A1) shade, were prepared and fired in a porcelain oven according to the manufacturer's instructions. Group S (stain only) was characterized by application of surface colorants to provide a definitive shade of Vita A3.5. Group GS (glaze over stain) was characterized by application of a layer of glaze over the existing colorant layer as used for Group S. Group SL (stain+LFP) was characterized by application of a mixture of colorants and clear low-fusing add-on porcelain to provide a definitive shade of Vita A3.5. Group C (Control) was used as a control without any surface characterization. The 4 groups were subjected to mechanical toothbrushing using a 1:1 water-to-toothpaste solution for a simulated duration of 32 years of clinical use. The amount of wear was measured at time intervals simulating every 4 years of toothbrushing. These parameters were evaluated longitudinally for all groups as well as compared at similar time points among

  11. Maintenance and preservation of concrete structures. Report 3: Abrasion-erosion resistance of concrete

    Science.gov (United States)

    Liu, T. C.

    1980-07-01

    This report describes a laboratory test program on abrasion-erosion resistance of concrete, including the development of a new underwater abrasion-erosion test method. This program was designed to evaluate the relative abrasion-erosion resistance of various materials considered for use in the repair of erosion-damaged concrete structures. The test program encompassed three concrete types (conventional concrete, fiber-reinforced concrete, and polymer concrete); seven aggregate types (limestone, chert, trap rock, quartzite, granite, siliceous gravel, and slag); three principal water-cement rations (0.72, 0.54, and 0.40); and six types of surface treatment (vacuum, polyurethane coating, acrylic mortar coating, epoxy mortar coating, furan resin mortar coating, and iron aggregate topping). A total of 114 specimens made from 41 batches of concrete was tested. Based on the test data obtained, a comprehensive evaluation of the effects of various parameters on the abrasion-erosion resistance of concrete was presented. Materials suitable for use in the repair of erosion-damaged concrete structures were recommended. Additional work to correlate the reported findings with field performance was formulated.

  12. Abrasion Resistance and Mechanical Properties of Waste-Glass-Fiber-Reinforced Roller-compacted Concrete

    Science.gov (United States)

    Yildizel, S. A.; Timur, O.; Ozturk, A. U.

    2018-05-01

    The potential use of waste glass fibers in roller-compacted concrete (RCC) was investigated with the aim to improve its performance and reduce environmental effects. The research was focused on the abrasion resistance and compressive and flexural strengths of the reinforced concrete relative to those of reference mixes without fibers. The freeze-thaw resistance of RCC mixes was also examined. It was found that the use of waste glass fibers at a rate of 2 % increased the abrasion resistance of the RCC mixes considerably.

  13. Abrasion Resistance of Nano Silica Modified Roller Compacted Rubbercrete: Cantabro Loss Method and Response Surface Methodology Approach

    Science.gov (United States)

    Adamu, Musa; Mohammed, Bashar S.; Shafiq, Nasir

    2018-04-01

    Roller compacted concrete (RCC) when used for pavement is subjected to skidding/rubbing by wheels of moving vehicles, this causes pavement surface to wear out and abrade. Therefore, abrasion resistance is one of the most important properties of concern for RCC pavement. In this study, response surface methodology was used to design, evaluate and analyze the effect of partial replacement of fine aggregate with crumb rubber, and addition of nano silica on the abrasion resistance of roller compacted rubbercrete (RCR). RCR is the terminology used for RCC pavement where crumb rubber was used as partial replacement to fine aggregate. The Box-Behnken design method was used to develop the mixtures combinations using 10%, 20%, and 30% crumb rubber with 0%, 1%, and 2% nano silica. The Cantabro loss method was used to measure the abrasion resistance. The results showed that the abrasion resistance of RCR decreases with increase in crumb rubber content, and increases with increase in addition of nano silica. The analysis of variance shows that the model developed using response surface methodology (RSM) has a very good degree of correlation, and can be used to predict the abrasion resistance of RCR with a percentage error of 5.44%. The combination of 10.76% crumb rubber and 1.59% nano silica yielded the best combinations of RCR in terms of abrasion resistance of RCR.

  14. Abrasive Wear Resistance of the Iron- and WC-based Hardfaced Coatings Evaluated with Scratch Test Method

    Directory of Open Access Journals (Sweden)

    A. Vencl

    2013-06-01

    Full Text Available Abrasive wear is one of the most common types of wear, which makesabrasive wear resistance very important in many industries. Thehard facing is considered as useful and economical way to improve theperformance of components submitted to severe abrasive wear conditions, with wide range of applicable filler materials. The abrasive wear resistance of the three different hardfaced coatings (two iron‐based and one WC‐based, which were intended to be used for reparation of the impact plates of the ventilation mill, was investigated and compared. Abrasive wear tests were carried‐out by using the scratch tester under the dry conditions. Three normal loads of 10, 50 and 100 N and the constant sliding speed of 4 mm/s were used. Scratch test was chosen as a relatively easy and quick test method. Wear mechanism analysis showed significant influence of the hardfaced coatings structure, which, along with hardness, has determined coatings abrasive wear resistance.

  15. Micro-Abrasion Wear Resistance of Borided 316L Stainless Steel and AISI 1018 Steel

    Science.gov (United States)

    Reséndiz-Calderon, C. D.; Rodríguez-Castro, G. A.; Meneses-Amador, A.; Campos-Silva, I. E.; Andraca-Adame, J.; Palomar-Pardavé, M. E.; Gallardo-Hernández, E. A.

    2017-11-01

    The 316L stainless steel has high corrosion resistance but low tribological performance. In different industrial sectors (biomedical, chemical, petrochemical, and nuclear engineering), improvement upon wear resistance of 316L stainless steel components using accessible and inexpensive methods is critical. The AISI 1018 steel is widely used in industry, but its tribological performance is not the best among steels. Therefore, in this study the behavior of the borided 316L stainless steel and 1018 steel is evaluated under micro-abrasion wear. The boriding was carried out at 1223 K over 6 h of exposure time, resulting in a biphase layer composed of FeB/Fe2B phases. In order to evaluate Fe2B phase with no influence from FeB phase, AISI 1018 steel samples were borided at 1273 K for over 20 min and then diffusion annealed at 1273 K over 2 h to obtain a Fe2B mono-phase layer. Micro-abrasion wear resistance was evaluated by a commercial micro-abrasion testing rig using a mix of F-1200 SiC particles with deionized water as abrasive slurry. The obtained wear rates for FeB and Fe2B phases and for the 316L stainless steel were compared. Wear resistance of 316L stainless steel increases after boriding. The wear mechanisms for both phases and for the stainless steel were identified. Also, transient conditions for rolling and grooving abrasion were determined for the FeB and Fe2B phases.

  16. Abrasion Wear Resistance, Hardness and Microstructure of Hard Linings Deposited by Means of a Submerged Arc. Dureza, microestructura y resistencia al desgaste por abrasion de recargues duros depositados con arco sumergido

    Energy Technology Data Exchange (ETDEWEB)

    Paranhos, R; Alcoforado, J M; Castillo, J A; Sauer, A

    1989-01-01

    Consumable materials for submerged arc welding of the types alloyed flux-neutral electrode and neutral flux-alloyed electrode were used to form, through multipass welding, a light alloy hard lining of the C-Mn type on ASTM A36 Type structural steel. Emphasis was put on microstructural characterization of the linings surveyed under electron scanning microscopy, and tests were performed to study their hardness and abrasion wear resistance at low pressures. As a result of these tests, a great influence of welding parameters on hardness and abrasion resistance properties of the combination active flux-neutral electrode was noticed. As the results showed no relationship between the hardness and the abrasion wear resistance of the linings surveyed, an attempt was made to relate the resulting microstructure with their abrasion wear resistance. (Author)

  17. Influence of Heat Treatment on Abrasive Wear Resistance of Silumin Matrix Composite Castings

    Directory of Open Access Journals (Sweden)

    Gawdzińska K.

    2016-03-01

    Full Text Available The authors attempted at examining the effect of heat treatment on abrasive wear resistance of metal composite castings. Metal matrix composites were made by infiltrating preforms created from unordered short fibers (graphite or silumin with liquid aluminium alloy AlSi12(b. Thus prepared composites were subject to solution heat treatment at a temperature of 520°C for four hours, then aging at a temperature of 220°C for four hours. Abrasion resistance of the material was tested before and after thermal treatment.

  18. Abrasion Properties of Steel Fiber Reinforced Silica Fume Concrete According to Los Angeles and Water Abrasion Tests

    Directory of Open Access Journals (Sweden)

    Tsan-Ching CHENG

    2014-12-01

    Full Text Available The current study mainly investigated the influence of different tests on the abrasion resistance of concrete mixed with steel fibers and silica fume. The abrasion resistance was assessed at 28, 56 and 91 days on concretes with water-binder ratios of 0.35 and 0.55 where in some mixes silica fume was substituted by 5 % of cement by weight. Steel fibers of 0.5 % and 1.0 % of concrete volume were also added into the test concrete by replacement of coarse and fine aggregates. The results showed that concrete with higher compressive strength in Los Angeles abrasion tests also had better abrasion resistance. The inclusion of steel fibers into test concrete with a water-binder ratio of 0.35 resulted in a significant increase in compressive strength. This concrete also displayed better abrasion resistance and splitting tensile strength than reference concrete; in the test sample with a water-binder ratio of 0.55, the added steel fibers was unable to effectively produce cementation with the concrete. The inclusion of silica fume improved the abrasion resistance of concretes. In water abrasion testing, the abrasion resistance of concrete containing steel fiber was worse than that of concrete without steel fibers. In the water abrasion testing, the surface of steel fiber reinforced concrete was eroded by water and steel balls, and the impact caused the steel fibers to separate from the concrete and led to higher wear loss. DOI: http://dx.doi.org/10.5755/j01.ms.20.4.6460

  19. Abrasive Wear Resistance of Tool Steels Evaluated by the Pin-on-Disc Testing

    Science.gov (United States)

    Bressan, José Divo; Schopf, Roberto Alexandre

    2011-05-01

    Present work examines tool steels abrasion wear resistance and the abrasion mechanisms which are one main contributor to failure of tooling in metal forming industry. Tooling used in cutting and metal forming processes without lubrication fails due to this type of wear. In the workshop and engineering practice, it is common to relate wear resistance as function of material hardness only. However, there are others parameters which influences wear such as: fracture toughness, type of crystalline structure and the occurrence of hard precipitate in the metallic matrix and also its nature. In the present investigation, the wear mechanisms acting in tool steels were analyzed and, by normalized tests, wear resistance performance of nine different types of tool steels were evaluated by pin-on-disc testing. Conventional tool steels commonly used in tooling such as AISI H13 and AISI A2 were compared in relation to tool steels fabricated by sintering process such as Crucible CPM 3V, CPM 9V and M4 steels. Friction and wear testing were carried out in a pin-on-disc automated equipment which pin was tool steel and the counter-face was a abrasive disc of silicon carbide. Normal load of 5 N, sliding velocity of 0.45 m/s, total sliding distance of 3000 m and room temperature were employed. The wear rate was calculated by the Archard's equation and from the plotted graphs of pin cumulated volume loss versus sliding distance. Specimens were appropriately heat treated by quenching and three tempering cycles. Percentage of alloying elements, metallographic analyses of microstructure and Vickers microhardness of specimens were performed, analyzed and correlated with wear rate. The work is concluded by the presentation of a rank of tool steel wear rate, comparing the different tool steel abrasion wear resistance: the best tool steel wear resistance evaluated was the Crucible CPM 9V steel.

  20. Predicting the Abrasion Resistance of Tool Steels by Means of Neurofuzzy Model

    Directory of Open Access Journals (Sweden)

    Dragutin Lisjak

    2013-07-01

    Full Text Available This work considers use neurofuzzy set theory for estimate abrasion wear resistance of steels based on chemical composition, heat treatment (austenitising temperature, quenchant and tempering temperature, hardness after hardening and different tempering temperature and volume loss of materials according to ASTM G 65-94. Testing of volume loss for the following group of materials as fuzzy data set was taken: carbon tool steels, cold work tool steels, hot work tools steels, high-speed steels. Modelled adaptive neuro fuzzy inference system (ANFIS is compared to statistical model of multivariable non-linear regression (MNLR. From the results it could be concluded that it is possible well estimate abrasion wear resistance for steel whose volume loss is unknown and thus eliminate unnecessary testing.

  1. Influence of Utilization of High-Volumes of Class F Fly Ash on the Abrasion Resistance of Concrete

    Directory of Open Access Journals (Sweden)

    William PRINCE

    2007-01-01

    Full Text Available Utilization of large volumes of fly ash in various concrete applications is a becoming a more general practice in an efforts towards using large quantities of fly ash. Around the world, Class C or Class F or both as available have been used in high volumes in cement-based materials. In India, majority of fly generated is of Class F type as per ASTM C 618. Yearly fly ash generation in India is approximately 95 million tonnes. Out of which around 15-20% is utilized in cement production and cement/concrete related activities. In order to increase its percentage utilization, an investigation was carried out to use it in concrete.In this paper, abrasion resistance of high volume fly ash (HVFA concretes made with 35, 45, 55, and 65% of cement replacement was evaluated in terms of its relation with compressive strength. Comparison was made between ordinary Portland cement and fly ash concrete. Test results indicated that abrasion resistance of concrete having cement replacement up to 35 percent was comparable to the normal concrete mix with out fly ash. Beyond 35% cement replacement, fly ash concretes exhibited slightly lower resistance to abrasion relative to non-fly ash concretes. Test results further indicated that abrasion resistance of concrete is closely related with compressive strength, and had a very good correlation between abrasion resistance and compressive strength (R2 value between 0.9018 and 0.9859 depending upon age.

  2. The role of the microfissuration of the rock matrix in the abrasion resistance of ornamental granitic rocks

    Science.gov (United States)

    Rodríguez-Rey, Angel; Sanchez-Delgado, Nuria; Camino, Clara; Calleja, Lope; Ruiz de Argandoña, Vicente G.; Setien, Alexia

    2015-04-01

    The microcrack density and the abrasion resistance of five ornamental granites (Albero, Gris Alba, Mondariz, Rosa Porriño and Traspieles) from Galicia (NW Spain) have been quantified as part of a research aimed to interpret the cuttability of the rocks in relation to the petrophysical properties of the rock matrix. Large blocks from the quarries have been cut with an industrial saw and the microcrack density and the abrasion resistance have been measured in two surfaces: H, parallel to the cut surface; T, perpendicular both to the cut surface and the cutting direction. Both planes are perpendicular to the rift plane, as it is known in quarry works. The microcrack density has been quantified following an stereological procedure applied to polished sections imaged under scanning electron microscopy. The magnification of the images allowed the study of microcracks as narrow as 2 microns in aperture. The density has been quantified in terms of length of microcrack traces per surface unit so possible anisotropies of the microcrack network could be detected. The obtained values are in the typical range for this type of rocks although the Traspieles granite shows a higher value due to its weathering degree (H: 5.11, T: 5.37 mm/mm2). The values measured in the two surfaces (H and T) are quite similar in four of the rocks; only the Albero granite shows a marked anisotropy (H: 2.76 T: 3.53 mm/mm2). The abrasion resistance of the rocks has been measured following the european standard EN 14157:2004 using the capon method. The rocks can be classified in two groups according to their abrasion resistance. Rosa Porriño, Gris Alba and Mondariz granites are the more resistant to abrasion with values around 16-17 mm. Albero and Traspieles granites are less resistant with values higher than 19 mm. The results show a good correlation between the microcrack density and the abrasion resistance. As can be expected the rocks with high microcrack density show low abrasion resistance. The

  3. Effects of Running Shoes with Abrasion Resistant Rubber Sole on the Exercise Capacity of the Human Body

    Directory of Open Access Journals (Sweden)

    Bo Wang

    2017-10-01

    Full Text Available With the development of industrialization, rubber has been gradually used in the manufacture of sports equipment for its favourable properties. This study involved the addition of C5 petroleum resin into brominated isobutylene-isoprene rubber (BIIR and butadiene rubber (BR while manufacturing the sole of running shoes. The effects of running shoes with abrasion resistant rubber sole on the exercise capacity of the human body were investigated by analysing the skid resistance and abrasion resistance of the running shoes, and conducting biomechanical study on naked feet and feet wearing the shoes. The results demonstrated that the rubber sole had favourable slip resistance property and mechanical properties such as stretching, abrasion resistance, and hardness. Compared to naked feet, the peak pressure intensity of the whole step of feet wearing the newly developed shoes, was significantly lower than that of feet wearing ordinary shoes. In the future, rubber can bring more comfortable experience because of its favourable properties.

  4. Development and Testing of Abrasion Resistant Hard Coats For Polymer Film Reflectors: Preprint

    Energy Technology Data Exchange (ETDEWEB)

    Jorgensen, G.; Gee, R.; DiGrazia, M.

    2010-10-01

    Reflective polymer film technology can significantly reduce the cost of solar reflectors and installed Concentrated Solar Power (CSP) plants by both reduced material cost and lower weight. One challenge of polymer reflectors in the CSP environment pertains to contact cleaning methods typically used with glass mirrors. Such contact cleaning methods can scratch the surface of polymer reflectors and thereby reduce specular reflectance. ReflecTech, Inc. (a subsidiary of SkyFuel, Inc.) and the National Renewable Energy Laboratory (NREL) initiated a cooperative research and development agreement (CRADA) to devise and develop an abrasion resistant coating (ARC) suitable for deposition onto polymer based mirror film. A number of candidate ARC products were identified as candidate formulations. Industrial collaborators prepared samples having their ARCs deposited onto ReflecTech Mirror Film pre-laminated to aluminum sheet substrates. Samples were provided for evaluation and subjected to baseline (unweathered) and accelerated exposure conditions and subsequently characterized for abrasion resistance and adhesion. An advanced ARC product has been identified that exhibits outstanding initial abrasion resistance and adhesion to ReflecTech Mirror Film. These properties were also retained after exposure to the various accelerated stress conditions. This material has been successfully manufactured as a 1.5 m wide roll-to-roll construction in a production environment.

  5. Abrasive wear resistance and microstructure of Ni-Cr-B-Si hardfacing alloys with additions of Al, Nb, Mo, Fe, Mn and C

    International Nuclear Information System (INIS)

    Berns, H.; Fischer, A.; Theisen, W.

    1987-01-01

    The development of new Ni-base hardfacing alloys for filler wire welding or metal spraying should result in materials with a good resistance against high temperature corrosion and abrasive wear. The first step is to design microstructures, which obtain a satisfactory abrasive wear behaviour at room temperature. Thus, different alloys are melted and scrutinized as to their microstructure and their abrasive wear resistance in laboratory. Compared to commercial Ni-base hardfacing alloys they show a higher volume fraction of coarse hard phases due to the additional, initial solidification of Nb-carbides and Cr-, and Mo-borides. Thus, the abrasive wear resistance is improved. For hard abrasive particles, such as corundum, the Ni-base alloys are more wear resistant than harder Fe-base alloys investigate earlier. This is due to the tougher Ni metal matrix that results in microcracking not to be the most significantly acting wear mechanism

  6. Strength and gas-abrasive wear-resistance of zirconium carbide based cerments

    International Nuclear Information System (INIS)

    Samsonov, G.V.; Dan'kin, A.A.; Markov, A.A.; Bogomol, I.V.

    1976-01-01

    Results relating to a study of cermet strength and wear resistance by means of a gas-abrasive flow are presented. It has been found that with a higher amount of the metallic binder (over 25 at.%) in zirconium carbide-based cermets the bending and compression strength and also hardness and wear resistance within the systems ZrC-Nb, ZrC-Mo, ZrC-W become lower. The interrelation of the cermet wear resistance of the various systems and their bending and compression strengths, which, in turn, depend on the electronic structure is shown

  7. The Effect of Microstructure on the Abrasion Resistance of Low Alloyed Steels

    NARCIS (Netherlands)

    Xu, X.

    2016-01-01

    The thesis attempts to develop advanced high abrasion resistant steels with low hardness in combination with good toughness, processability and low alloying additions. For this purpose, a novel multi-pass dual-indenter (MPDI) scratch test approach has been developed to approach the real continuous

  8. Silane effects on the surface morphology and abrasion resistance of transparent SiO2/UV-curable resin nano-composites

    International Nuclear Information System (INIS)

    Hsiang, Hsing-I.; Chang, Yu-Lun; Chen, Chi-Yu; Yen, Fu-Su

    2011-01-01

    Transparent ultraviolet curable nano-composite coatings consisting of nano-sized SiO 2 and acrylate resin have been developed to improve the abrasion resistance of organic polymers. The nano-sized SiO 2 particles were surface-modified using various amounts of 3-methacryloxypropyltrimethoxysilane. The 3-methacryloxypropyltrimethoxysilane concentration effects on the surface morphology and abrasion resistance of the transparent SiO 2 /ultraviolet-curable resin nano-composites were investigated using scanning electron microscopy, atomic force microscopy, and ultraviolet-visible spectrophotometer. The results showed that as the 3-methacryloxypropyltrimethoxysilane/SiO 2 weight ratio increased from 0.2 to 0.6, the dispersion, compatibility and cross-linking density between the 3-methacryloxypropyltrimethoxysilane-modified SiO 2 particles and acrylate resin were improved, leading to an increase in abrasion resistance. However, as the 3-methacryloxypropyltrimethoxysilane/SiO 2 weight ratio was increased to 1.5, the additional 3-methacryloxypropyltrimethoxysilane may exceed that needed to fill the pores with the probability of SiO 2 nano-particles existing on the coating surface was lower than that for samples with a 3-methacryloxypropyltrimethoxysilane/SiO 2 weight ratio of 0.6. This produced a decrease in abrasion resistance.

  9. Report D : self-consolidating concrete (SCC) for infrastructure elements - creep, shrinkage and abrasion resistance.

    Science.gov (United States)

    2012-08-01

    Concrete specimens were fabricated for shrinkage, creep, and abrasion resistance : testing. Variations of self-consolidating concrete (SCC) and conventional concrete were : all tested. The results were compared to previous similar testing programs an...

  10. Standard Test Method for Abrasive Wear Resistance of Cemented

    CERN Document Server

    American Society for Testing and Materials. Philadelphia

    2005-01-01

    1.1 This test method covers the determination of abrasive wear resistance of cemented carbides. 1.2 The values stated in inch-pound units are to be regarded as the standard. The SI equivalents of inch-pound units are in parentheses and may be approximate. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

  11. Abrasive wear of ceramic wear protection at ambient and high temperatures

    Science.gov (United States)

    Varga, M.; Adam, K.; Tumma, M.; Alessio, K. O.

    2017-05-01

    Ceramic wear protection is often applied in abrasive conditions due to their excellent wear resistance. This is especially necessary in heavy industries conveying large amounts of raw materials, e.g. in steel industry. Some plants also require material transport at high temperatures and velocities, making the need of temperature stable and abrasion resistant wear protection necessary. Various types and wear behaviour of ceramic protection are known. Hence, the goal of this study is to identify the best suitable ceramic materials for abrasive conditions in harsh environments at temperatures up to 950°C and severe thermal gradients. Chamottes, known for their excellent thermal shock resistance are compared to high abrasion resistant ceramic wear tiles and a cost efficient cement-bounded hard compound. Testing was done under high-stress three-body abrasion regime with a modified ASTM G65 apparatus enabling for investigations up to ~950°C. Thereto heated abrasive is introduced into the wear track and also preheated ceramic samples were used and compared to ambient temperature experiments. Results indicate a significant temperature influence on chamottes and the hard compound. While the chamottes benefit from temperature increase, the cement-bounded hard compound showed its limitation at abrasive temperatures of 950°C. The high abrasion resistant wear tiles represented the materials with the best wear resistance and less temperature influence in the investigated range.

  12. Nitriding the influence of plasma in resistance to wear micro abrasive tool steel AISI D2

    International Nuclear Information System (INIS)

    Gobbi, Vagner Joao; Gobb, Silvio Jose; Silva, Cosme Roberto Moreira da

    2010-01-01

    This work studies the influence of time of treatment in the formation of nitride layer of AISI D2 tool steel and the resistance to micro-abrasive wear from the technique of nitriding in plasma. The samples were nitrides at 400 ° C with a pressure of 4.5 mbar (450 Pa) and using a gas mixture of 80% vol.H2 and 20% vol.N2. The times of treatment were: 30, 60, 120, 180 and 360 minutes. The properties of the layers in the samples obtained nitrides were assessed by surface microhardness, profiles of microhardness, metallography analysis, X-ray diffraction and test for resistance to micro-abrasive wear. The best results for nitriding to 400 deg C, was obtained with the time of treatment of 360 minutes. In this case the increase in surface hardness was 94.6% and resistance to micro-abrasive wear of 15%. This increase in hardness may be associated with high concentration of nitrogen in the crystalline network of iron-α and additional training of nitrides. Low temperature of nitriding reduces between grain fragility to reduce the likelihood of precipitation of nitrides in a continuous manner in the austenite grain boundaries and the absence of previous ε'+ γ phases. (author)

  13. Design and evaluation of high-volume fly ash (HVFA) concrete mixes, report D : creep, shrinkage, and abrasion resistance of HVFA concrete.

    Science.gov (United States)

    2012-10-01

    The main objective of this study was to determine the effect on shrinkage, creep, : and abrasion resistance of high-volume fly ash (HVFA) concrete. The HVFA concrete : test program consisted of comparing the shrinkage, creep, and abrasion performance...

  14. LITERATURE SURVEY ON ABRASION PROBLEM IN CHENILLE YARNS

    Directory of Open Access Journals (Sweden)

    Erhan Kenan ÇEVEN

    2006-01-01

    Full Text Available Chenille yarns are traditionally used in the manufacture of furnishing fabrics, fashion knitwear, and as decorative threads in many types of broad and narrow fabrics. Chenille yarn has a very distinct weakness-it does not have very good inherent abrasion resistance. When the yarns are in use, clearly the abrasion resistance of the chenille yarn is crucially important. Either during further processing or during the eventual end-use, any removal of the effect yarn forming the beard will expose the ground yarns, which in turn will result in a bare appearance. To avoid this undesirable result, several options are available. Therefore, the studies on this area are about the investigation of the influences of some material types and machine parameters on the abrasion resistance of chenille yarns and fabrics produced with these yarns. In this paper, the experimental studies about the abrasion properties of chenille yarns in yarn, knitted and woven fabric forms are summarized.

  15. Improved Corrosion and Abrasion Resistance of Organic-Inorganic Composite Coated Electro-galvanized Steels for Digital TV Panels

    Energy Technology Data Exchange (ETDEWEB)

    Jo, Du-Hwan; Noh, Sang-Geol; Park, Jong-Tae; Kang, Choon-Ho [POSCO Technical Research Laboratories, Pohang (Korea, Republic of)

    2015-10-15

    Recently, household electronic industries require environmentally-friendly and highly functional steels in order to enhance the quality of human life. Customers especially require both excellent corrosion and abrasion resistant anti-fingerprint steels for digital TV panels. Thus POSCO has developed new functional electro-galvanized steels, which have double coated layers with organic-inorganic composites on the zinc surface of the steel for usage as the bottom chassis panel of TVs. The inorganic solution for the bottom layer consists of inorganic phosphate, magnesium, and zirconium compounds with a small amount of epoxy binder, and affords both improved adhesion properties by chemical conversion reactions and corrosion resistance due to a self-healing effect. The composite solution for the top layer was prepared by fine dispersion of organic-inorganic ingredients that consist of a urethane modified polyacrylate polymer, hardener, silica sol and a titanium complex inhibitor in aqueous media. Both composite solutions were coated on the steel surface by using a roll coater and then cured through an induction furnace in the electro-galvanizing line. New anti-fingerprint steel was evaluated for quality performance through such procedures as the salt spray test for corrosion resistance, tribological test for abrasion resistance, and conductivity test for surface electric conductance regarding to both types of polymer resin and coating weight of composite solution. New composite coated anti-fingerprint steels afford both better corrosion resistance and abrasion properties compared to conventional anti-fingerprint steel that mainly consists of acrylate polymers. Detailed discussions of both composite solutions and experimental results suggest that urethane modifications of acrylate polymers of composite solutions play a key role in enhanced quality performances.

  16. Optical tools for high-throughput screening of abrasion resistance of combinatorial libraries of organic coatings

    Science.gov (United States)

    Potyrailo, Radislav A.; Chisholm, Bret J.; Olson, Daniel R.; Brennan, Michael J.; Molaison, Chris A.

    2002-02-01

    Design, validation, and implementation of an optical spectroscopic system for high-throughput analysis of combinatorially developed protective organic coatings are reported. Our approach replaces labor-intensive coating evaluation steps with an automated system that rapidly analyzes 8x6 arrays of coating elements that are deposited on a plastic substrate. Each coating element of the library is 10 mm in diameter and 2 to 5 micrometers thick. Performance of coatings is evaluated with respect to their resistance to wear abrasion because this parameter is one of the primary considerations in end-use applications. Upon testing, the organic coatings undergo changes that are impossible to quantitatively predict using existing knowledge. Coatings are abraded using industry-accepted abrasion test methods at single-or multiple-abrasion conditions, followed by high- throughput analysis of abrasion-induced light scatter. The developed automated system is optimized for the analysis of diffusively scattered light that corresponds to 0 to 30% haze. System precision of 0.1 to 2.5% relative standard deviation provides capability for the reliable ranking of coatings performance. While the system was implemented for high-throughput screening of combinatorially developed organic protective coatings for automotive applications, it can be applied to a variety of other applications where materials ranking can be achieved using optical spectroscopic tools.

  17. A method for increase abrasive wear resistance parts by obtaining on methods casting on gasifying models

    Science.gov (United States)

    Sedukhin, V. V.; Anikeev, A. N.; Chumanov, I. V.

    2017-11-01

    Method optimizes hardening working layer parts’, working in high-abrasive conditions looks in this work: bland refractory particles WC and TiC in respect of 70/30 wt. % prepared by beforehand is applied on polystyrene model in casting’ mould. After metal poured in mould, withstand for crystallization, and then a study is carried out. Study macro- and microstructure received samples allows to say that thickness and structure received hardened layer depends on duration interactions blend harder carbides and liquid metal. Different character interactions various dispersed particles and matrix metal observed under the same conditions. Tests abrasive wear resistance received materials of method calculating residual masses was conducted in laboratory’ conditions. Results research wear resistance showed about that method obtaining harder coating of blend carbide tungsten and carbide titanium by means of drawing on surface foam polystyrene model before moulding, allows receive details with surface has wear resistance in 2.5 times higher, than details of analogy steel uncoated. Wherein energy costs necessary for transformation units mass’ substances in powder at obtained harder layer in 2.06 times higher, than materials uncoated.

  18. Abrasion-Resistant Aluminized-Coated Aramid Fabrics for Manufacture of Firefighters’ Protective Clothing

    Science.gov (United States)

    1985-05-01

    and radiacion are also produced at the cathode surface and may profoundly influence the quality of the substrate coating. These include secondary...14,265-378 (1979). Assink, R.A. Abrasion resistant polymer reflectors for solar applications. Solar Energy Mater vol. 3:263-75, (1980). Audet, N.F. Visor... solar reflectors. Solar Energy Mater vol. 3: No.1-2,277-83,(1981). *Gubareff, G.G., J.E. Janssen, and R.H. Torborg. Thermal radiation properties survey

  19. Wear resistance and structural changes in nitrogen-containing high-chromium martensitic steels under conditions of abrasive wear and sliding friction

    International Nuclear Information System (INIS)

    Makarov, A.V.; Korshunov, L.G.; Schastlivtsev, V.M.; Chernenko, N.L.

    1998-01-01

    Martensitic nitrogen-containing steels Kh17N2A0.14, Kh13A0.14, Kh14G4A0.22 as well as steel 20Kh13 were studied for their wear resistance under conditions of friction and abrasion. Metallography, X ray diffraction analysis and electron microscopy were used to investigate the structural changes taking place in a thin surface layer on wearing. It is shown that an increase of nitrogen content of 0.14 to 0.22% promotes an enhancement of steel resistance to abrasive and adhesive wear, especially after tempering in the range of 500-550 deg C. Typically, the nitrogen-containing steels exhibit lower resistance to various types of wear in comparison with the steels with high-carbon martensite due to their lower deformability under conditions of friction loading

  20. Fabricating superhydrophobic polymer surfaces with excellent abrasion resistance by a simple lamination templating method.

    Science.gov (United States)

    Xu, Qian Feng; Mondal, Bikash; Lyons, Alan M

    2011-09-01

    Fabricating robust superhydrophobic surfaces for commercial applications is challenging as the fine-scale surface features, necessary to achieve superhydrophobicity, are susceptible to mechanical damage. Herein, we report a simple and inexpensive lamination templating method to create superhydrophobic polymer surfaces with excellent abrasion resistance and water pressure stability. To fabricate the surfaces, polyethylene films were laminated against woven wire mesh templates. After cooling, the mesh was peeled from the polymer creating a 3D array of ordered polymer microposts on the polymer surface. The resulting texture is monolithic with the polymer film and requires no chemical modification to exhibit superhydrophobicity. By controlling lamination parameters and mesh dimensions, polyethylene surfaces were fabricated that exhibit static contact angles of 160° and slip angles of 5°. Chemical and mechanical stability was evaluated using an array of manual tests as well as a standard reciprocating abraser test. Surfaces remained superhydrophobic after more than 5500 abrasion cycles at a pressure of 32.0 kPa. In addition, the surface remains dry after immersing into water for 5 h at 55 kPa. This method is environmental friendly, as it employs no solvents or harsh chemicals and may provide an economically viable path to manufacture large areas of mechanically robust superhydrophobic surfaces from inexpensive polymers and reusable templates.

  1. Study on abrasion resisting material for apron of dam; Dam apron bu no taimamo sozai ni kansuru kenkyu

    Energy Technology Data Exchange (ETDEWEB)

    Inaba, H.; Hiraki, M.; Miyamoto, T. [Hokuriku Electric Power Co. Inc., Toyama (Japan)

    1995-01-25

    A `laminated rubber tile` and a `shock absorbing holed-in anchor` were devised in connection with the apron of a dam for a hydroelectric power plant. As the result of a survey on the hydroelectric power plants, ten plus places were observed where a general kind of concrete was severely worn in the company territory; but, there were substantial number of rubber materials that had still been sound for over ten years after the installation. In spite of the soundness of the rubber tiles, however, it was observed that their anchor supports had been cut and separated. An abrasion comparison test of concrete and rubber materials revealed that the rubber materials were considerably superior in abrasion resistance. Various rubber tiles were tested for abrasion resistance, tear strength, tensile strength, impact strength, etc.; and methods for fixing rubber tiles were also tested such as a holed-in anchor, chemical anchor and adhesives. As a result, a laminated rubber tile was designed with its upper layer constituted of a rubber sold on the market and its lower layer of a fiber reinforced rubber also on the market, and so was a shock absorbing type holed-in anchor. 1 ref., 11 figs., 4 tabs.

  2. On the abrasion of heat-treated 2.8C21Cr1Mo white cast iron

    Energy Technology Data Exchange (ETDEWEB)

    Al-Rubaie, Kassim S.; Preti, Orlando [Centro Universitario SOCIESC, Joinville (Brazil). Engenharia Mecanica; Pohl, Michael [Bochum Univ. (Germany). Inst. fuer Werkstoffe

    2016-09-15

    The abrasion behaviour of heat-treated 2.8C21Cr1Mo cast iron was studied. The specimens were destabilised at two temperatures, 980 and 1050 C, for 4 h, air hardened, and then tempered at five temperatures, 220, 320, 400, 500, and 620 C, for 2 h followed by air cooling. Using a pin-on-plate abrasion apparatus, the specimens were abraded on four types of bonded abrasives (silicon carbide, corundum, flint, and glass). The effect of work hardening on the abrasion resistance was investigated. It was found that the increase in alloy hardness produced by heat treatment had little effect on the abrasion resistance against silicon carbide or corundum; the inverse was true against flint or glass. The as-hardened structure containing 40% retained austenite gave the best abrasion resistance, whereas the hardened and tempered at 620 C showed the worst. Both bulk hardness and matrix hardness before wear correlated poorly with the abrasion resistance. Therefore, a general model ''equivalent hardness'' was developed, in which the hardness of the abraded matrix was considered. With this model, the abrasion behaviour can be clearly analysed.

  3. Anti-abrasive nanocoatings current and future applications

    CERN Document Server

    2015-01-01

    This book provides an overview of the fabrication methods for anti-abrasive nanocoatings. The connections among fabrication parameters, the characteristics of nanocoatings and the resulting properties (i.e. nanohardness, toughness, wear rate, load-bearing ability, friction coefficient, and scratch resistance) are discussed. Size-affected mechanical properties of nanocoatings are examined, including their uses. Anti-abrasive nanocoatings, including metallic-, ceramic-, and polymeric-based layers, as well as different kinds of nanostructures, such as multi-layered nanocomposites and thin films, are reviewed. * Provides a comprehensive overview of the fabrication methods for anti-abrasive nanocoatings* Discusses the connections among fabrication parameters, the characteristics of nanocoatings and the resulting properties* Reviews advantages and drawbacks of fabrication methods for anti-abrasive nanocoatings and clarifies the place of these nanocoatings in the world of nanotechnology

  4. Abordagem grassroots e resistência: atualizando a concepção de desenvolvimento sustentável

    Directory of Open Access Journals (Sweden)

    Augusto Marcos Carvalho de Sena

    Full Text Available Resumo Em contrapartida às especificidades impositivas do modelo de produção capitalista - incluindo-se nesse modelo os meandros de arranjos produtivos que inserem o meio ambiente enquanto alinhado à versão tríplice da concepção tradicional de desenvolvimento sustentável -, tem surgido uma massa crítica de literatura focada na resistência ao modo de funcionamento do capitalismo ocidental. Em relação à teoria, economia solidária (pilar econômico, movimentos sociais (pilar social, ecologia política (pilar ambiental e raízes culturais (pilar cultural são aparatos importantes que não devem ficar à margem na estruturação de uma concepção alternativa do desenvolvimento sustentável. Tais aparatos são considerados elementos de resistência, visto terem fatores diferenciados quando comparados com as características tradicionais dos pilares da criticada concepção de desenvolvimento sustentável. Assim, o objetivo do presente ensaio teórico é conceber alternativas à concepção padrão do desenvolvimento sustentável, considerando aspectos da abordagem grassroots importantes para esse propósito. A contribuição é relevante tendo em vista a consideração de aspectos alternativos e complementares envolvidos na leitura da atualização conjecturada. Os prospectos do desenvolvimento grassroots têm sido usados como guia prático em ações de desenvolvimento local envolvendo comunidades menos desenvolvidas em várias partes do mundo, sem a conjectura que sinaliza para elementos conceituais que podem oferecer uma conformação alternativa à concepção do desenvolvimento sustentável. Conclui-se que a versão tradicional do desenvolvimento sustentável pode ser atualizada com elementos alternativos advindos da abordagem grassroots.

  5. Hydrothermal treatment for TiN as abrasion resistant dental implant coating and its fibroblast response

    International Nuclear Information System (INIS)

    Shi, Xingling; Xu, Lingli; Munar, Melvin L.; Ishikawa, Kunio

    2015-01-01

    Dental implant made of pure titanium (Ti) is prone to scratch and abrasion during routine oral hygiene procedures. This results an increase in surface roughness and therefore, facilitates the adhesion of bacteria. In severe cases, this could lead to peri-implantitis. To overcome this problem, surface modification of Ti is necessary to improve its abrasion resistance. Besides, a strong implant–gingiva interface should also be guaranteed to prevent the adhesion of bacteria. In this study, titanium nitride (TiN) coating was first prepared with gas nitriding to increase surface hardness of pure the substrate. Then, the TiN was hydrothermally treated in CaCl 2 solution in order to improve its soft tissue biocompatibility. The effect of hydrothermal treatment temperature on surface properties of TiN was investigated and its biocompatibility was assessed in vitro using NIH3T3 fibroblast cell. It was determined that 120 °C was the critical temperature for the hydrothermal treatment condition. Treatment below 120 °C could incorporate Ca into TiN surface, oxidize TiN surface partially and then improve the wettability while preserving its morphology and hardness. Fibroblast cell attachment and proliferation were improved and cell spreading was enhanced on hydrothermally treated specimens compared with untreated ones. Improved wettability, Ca incorporation and negative surface due to interstitial N were believed to be the main reasons. Hydrothermal treatment is expected to make TiN a promising dental implant coating with excellent abrasion resistance and good soft tissue affinity. - Highlights: • Ca was incorporated into TiN surface while not sacrificing its hardness. • Interstitial N due to oxidation promoted Ca adsorption and cell adhesion. • Hydrothermal treatment makes TiN a promising coating for dental implant

  6. Hydrothermal treatment for TiN as abrasion resistant dental implant coating and its fibroblast response

    Energy Technology Data Exchange (ETDEWEB)

    Shi, Xingling, E-mail: shixingling1985@hotmail.com [School of Material Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003 (China); Department of Biomaterials, Faculty of Dental Science, Kyushu University, Fukuoka 812-8582 (Japan); Jiangsu Provincial Key Laboratory for Interventional Medical Devices, Huaiyin Institute of Technology, Huaian 223003 (China); Xu, Lingli [School of Material Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003 (China); Munar, Melvin L.; Ishikawa, Kunio [Department of Biomaterials, Faculty of Dental Science, Kyushu University, Fukuoka 812-8582 (Japan)

    2015-04-01

    Dental implant made of pure titanium (Ti) is prone to scratch and abrasion during routine oral hygiene procedures. This results an increase in surface roughness and therefore, facilitates the adhesion of bacteria. In severe cases, this could lead to peri-implantitis. To overcome this problem, surface modification of Ti is necessary to improve its abrasion resistance. Besides, a strong implant–gingiva interface should also be guaranteed to prevent the adhesion of bacteria. In this study, titanium nitride (TiN) coating was first prepared with gas nitriding to increase surface hardness of pure the substrate. Then, the TiN was hydrothermally treated in CaCl{sub 2} solution in order to improve its soft tissue biocompatibility. The effect of hydrothermal treatment temperature on surface properties of TiN was investigated and its biocompatibility was assessed in vitro using NIH3T3 fibroblast cell. It was determined that 120 °C was the critical temperature for the hydrothermal treatment condition. Treatment below 120 °C could incorporate Ca into TiN surface, oxidize TiN surface partially and then improve the wettability while preserving its morphology and hardness. Fibroblast cell attachment and proliferation were improved and cell spreading was enhanced on hydrothermally treated specimens compared with untreated ones. Improved wettability, Ca incorporation and negative surface due to interstitial N were believed to be the main reasons. Hydrothermal treatment is expected to make TiN a promising dental implant coating with excellent abrasion resistance and good soft tissue affinity. - Highlights: • Ca was incorporated into TiN surface while not sacrificing its hardness. • Interstitial N due to oxidation promoted Ca adsorption and cell adhesion. • Hydrothermal treatment makes TiN a promising coating for dental implant.

  7. Two-body, dry abrasive wear of Fe/Cr/C experimental alloys - relationship between microstructure and mechanical properties

    International Nuclear Information System (INIS)

    Kwok, C.K.S.

    1982-01-01

    A systematic study of abrasive wear resistance of Fe/Cr/Mn based alloys has been carried out using a two body pin-on-disc wear machine. Abrasives used were silicon carbide, alumina and quartz. The objective of this study was to evaluate the abrasive wear resistance and to investigate the relationships between microstructure, mechanical properties, and abrasive wear resistance for these experimental alloys. Several commercial alloys were also tested to provide a basis for comparison. The goal of this study was to develop information so as to improve wear resistance of these experimental alloys by means of thermal treatments. Grain-refinement by double heat treatment was carried out in this research

  8. Cleaning, abrasion, and polishing effect of novel perlite toothpaste abrasive.

    Science.gov (United States)

    Wang, Bo

    2013-01-01

    This study was intended to optimize perlite particle size and morphology for better tooth cleaning and lower tooth abrasion, and to evaluate the performance of a whitening toothpaste containing the optimized perlite abrasive for tooth cleaning, abrasion, and polishing. Perlite toothpaste abrasive samples were prepared by air classifying a commercial expanded perlite product. The tooth cleaning and abrasion properties for these classified perlite samples were reported via the pellicle cleaning ratio (PCR) and relative dentin abrasion (RDA). Performance of the whitening toothpaste containing the optimized perlite abrasive in tooth cleaning, polishing, and abrasion was evaluated against a widely used synthetic high-cleaning silica. Air classification removes large perlite particles and also physically changes perlite particle morphology from mostly three dimensional and angular particles to mainly two dimensional and platy particles. All the classified samples show good tooth cleaning effect, but tooth abrasion decreases significantly with decreasing particle size. Compared to high-cleaning silica whitening toothpaste, the whitening toothpaste containing the optimized perlite abrasive (PerlClean) is slightly better at tooth cleaning, lower in tooth abrasion, and significantly better at tooth polishing. Fine platy perlite particles are effective in tooth cleaning with low tooth abrasion. The enhanced performance of optimized perlite toothpaste abrasive compared to high-cleaning silica in a whitening toothpaste is attributed to the optimized particle size distribution and the unique platy particle geometry.

  9. The use of ion implantation for the improvement of abrasive wear resistance

    International Nuclear Information System (INIS)

    Delves, B.G.; Dearnaley, G.

    1979-01-01

    At the conclusion of the 1977 IPAT conference a practical problem was described which called for an economically feasible method of improving the resistance of tool steel, chromium and other alloys to abrasive wear sustained during the injection moulding of phenolic resin. This paper will describe subsequent work to investigate ion implantation as a possible means of treating steel taps, injection nozzles, feed wear pads, cavity moulds etc. Various problems were encountered and it will be described how most of these have now been overcome. Under favourable conditions factors of 4, and sometimes up to 10 times the normal life can be achieved. An attempt will be made to estimate some of the economic benefits of the process. (author)

  10. Morphologic and Chemical Properties of PMMA/ATH Layers with Enhanced Abrasion Resistance Realised by Cold Plasma Spraying at Atmospheric Pressure

    Directory of Open Access Journals (Sweden)

    L. Wallenhorst

    2018-01-01

    Full Text Available This study investigated the morphologic and chemical properties of coatings based on PMMA/ATH powder and deposited by cold plasma spraying on wood and glass. Since the deposition of pure PMMA/ATH powder with air as process gas yielded coatings with insufficient abrasion resistance, two modifications of the basic process were investigated. Previous studies showed that replacing air as process gas with forming gas did not enhance the abrasion resistance, but the addition of a phenol-formaldehyde resin (PF succeeded in stabilising the particle coatings. In this work, results from morphologic and chemical analysis suggested an encasement of the PMMA/ATH particles by plasma-modified PF and thus a fusion of individual particles, explaining the enhanced bonding. Moreover, adhesion tests confirmed an outstanding bonding between the coating and wood as well as glass, which is assumed to result from interactions between the PF’s hydroxyl groups and functional groups on the substrates’ surfaces. Studies on the wettability revealed a hydrophobic character of such coatings, therefore generally indicating a possible application, for example, to reduce water uptake by wooden materials.

  11. Adhesive, abrasive and oxidative wear in ion-implanted metals

    International Nuclear Information System (INIS)

    Dearnaley, G.

    1985-01-01

    Ion implantation is increasingly being used to provide wear resistance in metals and cemented tungsten carbides. Field trials and laboratory tests indicate that the best performance is achieved in mild abrasive wear. This can be understood in terms of the classification of wear modes (adhesive, abrasive, oxidative etc.) introduced by Burwell. Surface hardening and work hardenability are the major properties to be enhanced by ion implantation. The implantation of nitrogen or dual implants of metallic and interstitial species are effective. Recently developed techniques of ion-beam-enhanced deposition of coatings can further improve wear resistance by lessening adhesion and oxidation. In order to support such hard coatings, ion implantation of nitrogen can be used as a preliminary treatment. There is thus emerging a versatile group of related hard vacuum treatments involving intense beams of nitrogen ions for the purpose of tailoring metal surfaces to resist wear. (Auth.)

  12. Air Abrasion

    Science.gov (United States)

    ... Chapters What Is Air Abrasion? What Happens? The Pros and Cons Will I Feel Anything? Is Air ... will perform any procedures that use air-abrasion technology. Ask your dentist if he or she uses ...

  13. Abrasion-resistant concrete mix designs for precast bridge deck panels.

    Science.gov (United States)

    2010-08-01

    The report documents laboratory investigations undertaken to develop high performance concrete (HPC) for precast and pre-stressed bridge deck components that would reduce the life-cycle cost of bridges by improving the studded tire wear (abrasion) re...

  14. Study of the rheological properties and the finishing behavior of abrasive gels in abrasive flow machining

    Energy Technology Data Exchange (ETDEWEB)

    Wang, A. C.; Liu, C. H.; Liang, K. Z.; Pai, S. H. [Ching Yun University, Taipei (China)

    2007-10-15

    Abrasive flow machining (AFM) is an effective method to finish the smooth surface in the complex holes. Abrasive media are key elements which dominate the polished results in AFM. But it is hard to develop the machining model of these abrasive gels because of its complicated mechanism. In this research, a non-Newtonian flow is used to set up the abrasive mechanism of the abrasive media in AFM. Power law is a main equation of the non-Newtonian flow to describe the motion of the abrasive media. Viscosities vs. shear rates of different abrasive gels are used to establish the power law in CFD-ACE{sup +} software first. And the working parameters of AFM were applied as input to study the properties of the abrasive gels in AFM. Finally, the relationships between the simulations and the experiments were found. And the abrasive mechanism of the abrasive gels was set up in AFM. The simulated results show that the abrasive gel with high viscosity can entirely deform in the complex hole than the abrasive gel with low viscosity. And the abrasive gel with high viscosity generates a larger shear force than the abrasive gel with low viscosity in the same area. Moreover, the strain rate is seriously changed when the abrasive gel cross over the narrow cross-section of the complex hole. It also means that abrasive gel will produce large finish force in that area. And these results indeed consist with the experiments in AFM.

  15. Facile fabrication of superhydrophobic surface with excellent mechanical abrasion and corrosion resistance on copper substrate by a novel method.

    Science.gov (United States)

    Su, Fenghua; Yao, Kai

    2014-06-11

    A novel method for controllable fabrication of a superhydrophobic surface with a water contact angle of 162 ± 1° and a sliding angle of 3 ± 0.5° on copper substrate is reported in this Research Article. The facile and low-cost fabrication process is composed from the electrodeposition in traditional Watts bath and the heat-treatment in the presence of (heptadecafluoro-1,1,2,2-tetradecyl) triethoxysilane (AC-FAS). The superhydrophobicity of the fabricated surface results from its pine-cone-like hierarchical micro-nanostructure and the assembly of low-surface-energy fluorinated components on it. The superhydrophobic surface exhibits high microhardness and excellent mechanical abrasion resistance because it maintains superhydrophobicity after mechanical abrasion against 800 grit SiC sandpaper for 1.0 m at the applied pressure of 4.80 kPa. Moreover, the superhydrophobic surface has good chemical stability in both acidic and alkaline environments. The potentiodynamic polarization and electrochemical impedance spectroscopy test shows that the as-prepared superhydrophobic surface has excellent corrosion resistance that can provide effective protection for the bare Cu substrate. In addition, the as-prepared superhydrophobic surface has self-cleaning ability. It is believed that the facile and low-cost method offer an effective strategy and promising industrial applications for fabricating superhydrophobic surfaces on various metallic materials.

  16. Modeling of Micro Deval abrasion loss based on some rock properties

    Science.gov (United States)

    Capik, Mehmet; Yilmaz, Ali Osman

    2017-10-01

    Aggregate is one of the most widely used construction material. The quality of the aggregate is determined using some testing methods. Among these methods, the Micro Deval Abrasion Loss (MDAL) test is commonly used for the determination of the quality and the abrasion resistance of aggregate. The main objective of this study is to develop models for the prediction of MDAL from rock properties, including uniaxial compressive strength, Brazilian tensile strength, point load index, Schmidt rebound hardness, apparent porosity, void ratio Cerchar abrasivity index and Bohme abrasion test are examined. Additionally, the MDAL is modeled using simple regression analysis and multiple linear regression analysis based on the rock properties. The study shows that the MDAL decreases with the increase of uniaxial compressive strength, Brazilian tensile strength, point load index, Schmidt rebound hardness and Cerchar abrasivity index. It is also concluded that the MDAL increases with the increase of apparent porosity, void ratio and Bohme abrasion test. The modeling results show that the models based on Bohme abrasion test and L type Schmidt rebound hardness give the better forecasting performances for the MDAL. More models, including the uniaxial compressive strength, the apparent porosity and Cerchar abrasivity index, are developed for the rapid estimation of the MDAL of the rocks. The developed models were verified by statistical tests. Additionally, it can be stated that the proposed models can be used as a forecasting for aggregate quality.

  17. The Abrasive Wear Resistance of the Segmented Linear Polyurethane Elastomers Based on a Variety of Polyols as Soft Segments

    Directory of Open Access Journals (Sweden)

    Konrad Kwiatkowski

    2017-12-01

    Full Text Available The presented results make an original contribution to the development of knowledge on the prediction and/or modeling of the abrasive wear properties of polyurethanes. A series of segmented linear polyurethane elastomers (PUR—In which the hard segments consist of 4,4′-methylene bis(phenylisocyanate and 1,4-butanodiol, whilst polyether, polycarbonate, or polyester polyols constitute the soft segments—Were synthesized and characterized. The hardness and wear performance as functions of the variable chemical composition of polyurethane elastomers were evaluated in order to define the relationship between studied factors. The microstructure was characterized in detail, including analysis of the hydrogen bonding by Fourier transformed infrared (FT-IR spectroscopy and the phase structure by X-ray scattering (WAXS and differential scanning calorimetry (DSC methods. The presented studies provide the key features of the polymer composition affecting the abrasive resistance as well as attempts to explain the origin of the differences in the polyurethane elastomers’ performance.

  18. Influence of the metallic matrix ratio on the wear resistance (dry and slurry abrasion) of plasma sprayed cermet (chromia / stainless steel) coatings

    Czech Academy of Sciences Publication Activity Database

    Ageorges, H.; Ctibor, Pavel; Medarhri, Z.; Touimi, S.; Fauchais, P.

    2006-01-01

    Roč. 201, č. 5 (2006), s. 2006-2011 ISSN 0257-8972 R&D Projects: GA AV ČR(CZ) 1QS200430560 Institutional research plan: CEZ:AV0Z20430508 Keywords : plasma spraying * composite coating * tribology * hardness * wear * abrasion * chromia/stainless steel Subject RIV: JH - Ceramics, Fire-Resistant Materials and Glass Impact factor: 1.559, year: 2006

  19. Reduced abrasion drilling fluid

    NARCIS (Netherlands)

    2010-01-01

    A reduced abrasion drilling fluid system and method of drilling a borehole by circulating the reduced abrasion drilling fluid through the borehole is disclosed. The reduced abrasion drilling fluid comprises a drilling fluid, a first additive and a weighting agent, wherein the weighting agent has a

  20. Reduced abrasion drilling fluid

    NARCIS (Netherlands)

    2012-01-01

    A reduced abrasion drilling fluid system and method of drilling a borehole by circulating the reduced abrasion drilling fluid through the borehole is disclosed. The reduced abrasion drilling fluid comprises a drilling fluid, a first additive and a weighting agent, wherein the weighting agent has a

  1. Dynamic Mechanical Analysis and Three-Body Abrasive Wear Behaviour of Thermoplastic Copolyester Elastomer Composites

    Directory of Open Access Journals (Sweden)

    Hemanth Rajashekaraiah

    2014-01-01

    Full Text Available Various amounts of short fibers (glass and carbon and particulate fillers like polytetrafluoroethylene (PTFE, silicon carbide (SiC, and alumina (Al2O3 were systematically introduced into the thermoplastic copolyester elastomer (TCE matrix for reinforcement purpose. The mechanical properties such as storage modulus, loss modulus, and Tan δ by dynamic mechanical analysis (DMA and three-body abrasive wear performance on a dry sand rubber wheel abrasion tester have been investigated. For abrasive wear study, the experiments were planned according to L27 orthogonal array by considering three factors and three levels. The complex moduli for TCE hybrid composites were pushed to a higher level relative to the TCE filled PTFE composite. At lower temperatures (in the glassy region, the storage modulus increases with increase in wt.% of reinforcement (fiber + fillers and the value is maximum for the composite with 40 wt.% reinforcement. The loss modulus and damping peaks were also found to be higher by the incorporation of SiC and Al2O3 microfillers. The routine abrasive wear test results indicated that TCE filled PTFE composite exhibited better abrasion resistance. Improvements in the abrasion resistance, however, have not been achieved by short-fiber and particlaute filler reinforcements. From the Taguchi’s experimental findings, optimal combination of control factors were obtained for minimum wear volume and also predictive correlations were proposed. Further, the worn surface morphology of the samples was discussed.

  2. Three-body abrasive wear behaviour of metastable spheroidal carbide cast irons with different chromium contents

    Energy Technology Data Exchange (ETDEWEB)

    Efremenko, Vasily; Pastukhova, Tatiana; Chabak, Yuliia; Efremenko, Alexey [Pryazovskyi State Technical Univ., Mariupol (Ukraine); Shimizu, Kazumichi; Kusumoto, Kenta [Muroran Institute of Technology, Hokkaido (Japan); Brykov, Michail [Zaporozhye National Technical Univ., Zaporozhye (Ukraine)

    2018-02-15

    The effect of heat treatment and chromium contents (up to 9.1 wt.%) on the wear resistance of spheroidal carbide cast iron (9.5 wt.% V) was studied using optical and scanning electron microscopy, X-ray diffractometry, dilatometry and three-body abrasive testing. It was found that quenching from 760 C and 920 C improved the alloys' wear resistance compared to the as-cast state due to the formation of metastable austenite transforming into martensite under abrasion. The wear characteristics of alloys studied are 1.6 - 2.3 times higher than that of reference cast iron (12 wt.% V) having stable austenitic matrix. Chromium addition decreases surface damage due to the formation of M{sub 7}C{sub 3} carbides, while it reduces wear resistance owing to austenite stabilization to abrasion-induced martensite transformation. The superposition of these factors results in decreasing the alloys' wear behaviour with chromium content increase.

  3. Synthesis CNTs Particle Based Abrasive Media for Abrasive Flow Machining Process

    International Nuclear Information System (INIS)

    Kumar, Sonu; Walia, R.S; Dhull, S.; Murtaza, Q.; Tyagi, P. K.

    2016-01-01

    Abrasive flow machining (AFM) is a modem fine finishing process used for intricate and internal finishing of components or parts. It is based on flowing of viscoelastic abrasive media over the surface to be fine finished. The abrasive media is the important parameter in the AFM process because of its ability to accurately abrade the predefined area along it flow path. In this study, an attempt is made to develop a new abrasive, alumina with Carbon nanotubes (CNTs) in viscoelastic medium. CNT s in house produced through chemical vapour deposition technique and characterize through TEM. Performance evaluation of the new abrasive media is carried out by increasing content of CNT s with fixed extrusion pressure, viscosity of media and media flow rate as process parameters and surface finish improvement and material removal as process responses in AFM setup. Significantly improvement has been observed in material removal and maximum improvement of 100% has been observed in the surface finish on the inner cylindrical surface of the cast iron work piece. (paper)

  4. Machining with abrasives

    CERN Document Server

    Jackson, Mark J

    2011-01-01

    Abrasive machining is key to obtaining the desired geometry and surface quality in manufacturing. This book discusses the fundamentals and advances in the abrasive machining processes. It provides a complete overview of developing areas in the field.

  5. Influence of the microstructure of WC-Co cemented carbides on the fracture toughness and abrasive wear

    International Nuclear Information System (INIS)

    Zum Gahr, K.H.; Fischer, A.

    1981-01-01

    Fracture toughness and abrasive wear resistance of WC-Co cemented carbides were investigated by using the indentation cracking test (Palmqvist test) and the pin-on-disk method respectively. Size distribution of tungsten carbides and means free path between them were found to be important microstructural parameters related to the mechanical behavior. Results showed that selection of cemented carbides for heavy wear loading is complicated by contradictory influence of microstructural parameters on fracture toughness and abrasion resistance. Knowledge of the relation between microstructure and resistance to fracture or wear is necessary for optimum use of cemented carbides. (orig.) [de

  6. Final Technical Report: Development of an Abrasion-Resistant Antisoiling Coating for Front-Surface Reflectors

    Energy Technology Data Exchange (ETDEWEB)

    Gee, Randy C. [Sundog Solar Technology, Arvada, CO (United States)

    2017-07-18

    A high-performance reflective film has been successfully developed for Concentrating Solar Power (CSP) solar concentrators. Anti-soiling properties and abrasion resistance have been incorporated into the reflector to reduce reflector cleaning costs and to enhance durability. This approach has also resulted in higher reflectance and improved specularity. From the outset of this project we focused on the use of established high-volume roll-to-roll manufacturing techniques to achieve low manufacturing costs on a per ubit area basis. Roll-to-roll manufacturng equipment has a high capital cost so there is an entire industry devoted to roll-to-roll “toll” manufacturing, where the equipment is operated “around the clock” to produce a multitude of products for a large variety of uses. Using this approach, the reflective film can be manufactured by toll coaters/converters on an as-needed basis.

  7. Three body abrasion of laser surface alloyed aluminium AA1200

    CSIR Research Space (South Africa)

    Mabhali, Luyolo AB

    2012-06-01

    Full Text Available Laser surface alloying of aluminium AA1200 was performed with a 4 kW Nd:YAG laser to improve the abrasion wear resistance. Aluminium surfaces reinforced with metal matrix composites and intermetallic phases were achieved. The phases present depended...

  8. Researches concerning the ultasonic energy influence on the resistence to the abrasive wear of loaded welded parts

    Directory of Open Access Journals (Sweden)

    Gh. Amza

    2013-01-01

    Full Text Available The researches presented in the paper refer to the effect of ultrasounds propagation in the liquid metal bath on the process of transferring the additive material through the electric arch and on the crystallization process, and all these effects are analyzed for loaded welded parts solicited at the abrasive wear. All these influences are conferred to these two basic phenomena due to the ultrasounds propagation in liquid environments, namely, ultra-acoustic cavitation and acceleration of the diffusion process. The results concerns the resistance to the wear obtained for the loaded parts through manual welding with electric arch and classically covered electrode and ultrasonically activated.

  9. Abrasives and possibilities of increase in efficiency of abrasive waterjets

    Czech Academy of Sciences Publication Activity Database

    Sitek, Libor; Martinec, Petr

    2016-01-01

    Roč. 9, March 2016 (2016), s. 877-881 ISSN 1805-0476 R&D Projects: GA MŠk(CZ) LO1406; GA MŠk ED2.1.00/03.0082 Institutional support: RVO:68145535 Keywords : high-speed waterjets * abrasive waterjets * abrasives * garnet * zirconia Subject RIV: JQ - Machines ; Tools http://www.mmscience.eu/content/file/archives/MM_Science_201603.pdf

  10. Empirical ranking of a wide range of WC-Co grades in terms of their abrasion resistance measured by the ASTM standard B 611-85 test

    CSIR Research Space (South Africa)

    O'Quigley, DGF

    1997-01-01

    Full Text Available This paper reports the results of a comprehensive investigation into the abrasion resistance of WC-Co alloys, as measured by the ASTM Standard B 611-85 test. The alloys ranged from 3 to 50 wt% and from 0.6 to 5 mu-m average grain size. Careful...

  11. Transforming Anaerobic Adhesives into Highly Durable and Abrasion Resistant Superhydrophobic Organoclay Nanocomposite Films: A New Hybrid Spray Adhesive for Tough Superhydrophobicity

    Science.gov (United States)

    Bayer, Ilker S.; Brown, Andrea; Steele, Adam; Loth, Eric

    2009-12-01

    The authors report fabrication of tough nanostructured self-cleaning superhydrophobic polymer-organoclay films from anaerobic acrylic adhesives displaying strong adhesion to metal surfaces. Both industrial and bio-grade anaerobic adhesives such as bone cements could be used. Montmorillonite clay filled anaerobic adhesives were modified by blending with a water dispersed fluoro-methacrylic latex in solution to form abrasion resistant interpenetrating polymer network films upon spray casting. The adhesive films could cure by thermosetting in oxygen-rich environments. Very high contact angles with low hysteresis were also measured for acidic (pH 2) and basic (pH 11) aqueous buffer solutions indicating resistance to acidic and basic media.

  12. Buen Vivir Andino: Resistência e/ou alternativa ao modelo hegemônico de desenvolvimento

    Directory of Open Access Journals (Sweden)

    Klaus Pereira da Silva

    Full Text Available Resumo Este ensaio teórico problematiza a ética do Buen Vivir como forma de resistência e/ou alternativa ao modelo hegemônico de desenvolvimento que tem sido disseminado e implementado por organizações internacionais e corporações. Após a declaração das Nações Unidas sobre os direitos indígenas, em 2007 (MAMANI, 2010, o Buen Vivir alcançou status oficial nas Constituições do Equador e da Bolívia. O Buen Vivir é uma visão de mundo distinta da ordem internacional liberal institucionalizada no pós-II Guerra Mundial; fundamenta-se nas noções de cosmovisão relacional e pluriverso (ESCOBAR, 2011, multiverso (MAMANI, 2010 ou ecosofia andina (ESTERMANN, 2013, enunciados no Sul e subalternizados por mais de cinco séculos de colonialidade. Com base nestas noções, o ensaio enfatiza a importância de repensar, segundo uma abordagem decolonial, o papel desempenhado pelos Estados e organizações governamentais internacionais no que diz respeito ao desenvolvimento local. A análise crítica da literatura sugere a existência de múltiplas visões acerca do desenvolvimento que devem ser debatidas no âmbito de estudos organizacionais.

  13. Abrasive wear behavior of heat-treated ABC-silicon carbide

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Xiao Feng; Lee, Gun Y.; Chen, Da; Ritchie, Robert O.; De Jonghe, Lutgard C.

    2002-06-17

    Hot-pressed silicon carbide, containing aluminum, boron, and carbon additives (ABC-SiC), was subjected to three-body and two-body wear testing using diamond abrasives over a range of sizes. In general, the wear resistance of ABC-SiC, with suitable heat treatment, was superior to that of commercial SiC.

  14. Cutting concrete with abrasion jet

    International Nuclear Information System (INIS)

    Yie, G.G.

    1982-01-01

    Fluidyne Corporation has developed a unique process and apparatus that allow selected abrasives to be introduced into high-speed waterjet to produce abrasive-entrained waterjet that has high material-cutting capabilities, which is termed by Fluidyne as the Abrasion Jet. Such Abrasion Jet has demonstrated capability in cutting hard rock and concrete at a modest pressure of less than 1360 bars (20,000 psi) and a power input of less than 45 kW (60 horsepower). Abrasion Jet cutting of concrete is characterized by its high rate of cutting, flexible operation, good cut quality, and relatively low costs. This paper presents a general description of this technology together with discussions of recent test results and how it could be applied to nuclear decontamination and decommissioning work. 8 references

  15. Effect of Nanosilica Particle Size on the Water Permeability, Abrasion Resistance, Drying Shrinkage, and Repair Work Properties of Cement Mortar Containing Nano-SiO2

    Directory of Open Access Journals (Sweden)

    Sattawat Haruehansapong

    2017-01-01

    Full Text Available This work presents the effect of nanosilica particle sizes on durability properties and repair work properties of cement mortar containing nanosilica (NS. Three different NS particle sizes of 12, 20, and 40 nm were used and compared with those of cement mortar without NS and cement mortar with silica fume (SF. Interesting results were obtained in which the particle size of NS affected directly the abrasion resistance and water permeability. NS with particle size of 40 nm is the optimum size and gave the highest abrasion resistance and water permeability. For repair work properties, cement mortars containing NS (12 and 20 nm and SF experienced higher drying shrinkage than that of cement mortar without NS and then presented cracking behavior and debonding between the cement mortars and concrete substrate. Cement mortar containing 40 nm of NS gave the lowest drying shrinkage, the lowest crack number, and the highest adhesive strength. These results indicate that the particle size of NS affected not only the durability properties but also the repair work properties of cement mortar.

  16. Evaluation of Resistance to Los Angeles Abrasion and Physical Factors with Grindability Properties of Some Aggregate Materials

    Directory of Open Access Journals (Sweden)

    C. Sensogut

    2017-01-01

    Full Text Available In recent years, the usage of aggregate materials has increased both in Turkey and the entire world. It can be said that the main reason of this rise is the population growth together with the demand towards the more qualitative life. Therefore, the usability of some aggregate materials was investigated in the present paper. The properties of Los Angeles abrasion resistance, freezing-thaw resistance, slake durability strength and frost resistance of basalt and andesite samples obtained from Karaman and Ankara regions were studied at the first stage. In the second order, the grindability performance of these materials was also determined from the discontinuous grinding tests and the obtained results were correlated. Whereas the Los Angeles resistance of the basalt sample was higher than the andesite sample, the mass losses after the freezing-thaw and the frost tests for the andesite sample were superior. Both of the basalt and andesite samples were classified as ‘very high’ for their slake durability strength (Id-2 values. The material percentage of the andesite sample, which is passing through the sub-size ( %90 was greater than the value obtained for the basalt sample during the same grinding time. The resistance to the crushing process was obtained to be maximum at -850+600 µm of feed size for the basalt and the andesite samples.

  17. A study on the effect of 60Co gamma ray irradiation on the abrasion of dental polymethylmethacrylate, (3)

    International Nuclear Information System (INIS)

    Kimura, Hiroshi

    1981-01-01

    This report intends to clarify the relationship between the total exposure dose and scratch resistance to the specimens SF, SH, MF and MH, giving coating treatments to P.M.M.A. (dental polymethylmethacrylate) and exposing to the irradiation of 60 Co gamma ray at each dose rate. And based on the results, it is intended to develop coated P.M.M.A. with excellent scratch resistance give by irradiation of radioactive ray. From this study, the following results have been obtained. Irradiation of 60 Co gamma ray would give the best results at the exposure at 1 x 10 6 R. The SF and SH specimens in wet condition exposed to 60 Co gamma ray irradiation at 1 x 10 6 R showed a quantity of abrasion of only 17% that of untreated P.M.M.A. and the barrel test revealed outstanding abrasion and scratch resistance. Abrasion and scratch resistance of coated specimens are better utilized in wet conditions performing three times better than those in dry conditions. (author)

  18. Development of the white cast iron with niobium alloy, heat treating, to wear of the abrasive resistance; Desenvolvimento de uma liga de ferro fundido branco alto cromo com niobio, tratada termicamente, para resistencia ao desgaste abrasivo

    Energy Technology Data Exchange (ETDEWEB)

    Farah, Alessandro Fraga

    1997-07-01

    This work presents the heat treatment and abrasion tests results of a white cast iron with niobium alloy. The hardening heat treatment were made 950, 1000, 1050 e 110 deg C temperatures cooled by forced air. The tempering treatment were made at 450, 500 e 550 deg C temperatures. The heat treating alloy were compared, in the abrasive tests, with commercial alloys used as hardfacing by welding process in wear pieces. The abrasion tests was realized in pin on disk test. Additional tests were carried out for microstructural characterization to identify the different phases presents in the alloys. In a general way, the alloy studies showed the best wear rate for the heat treatments that results in higher hardness. It performance was superior than that of the commercial alloys. (author)

  19. Effect of heat treatment on strength and abrasive wear behaviour of ...

    Indian Academy of Sciences (India)

    Administrator

    Aluminum 6061 has been used as matrix material owing to its ... Mechanical properties such as microhardness, tensile strength, and abrasive wear tests have been ... heat treatment conditions, adopted Al6061–SiCp composites exhibited better microhardness and tensile ... corrosion resistance (Ramesh et al 2005).

  20. FY 2000 report on the results of the technology development of energy use reduction of machine tools. Development of dry cutting use abrasion resistant/lubricous coated tools; 2000 nendo energy shiyo gorika kosaku kikai nado gijutsu kaihatsu seika hokokusho. Dry sessakuyo taimamo junkatsusei hifuku kogu no kaihatsu

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    2001-03-01

    For the purpose of energy conservation and reduction of environmental loads of machine tools, study was conducted on the dry cutting which is the cutting with no use of cutting oil, and the FY 2000 results were summed up. The study was made on dry cutting use abrasion resistance/lubricous coated tools coated with the composite membrane of which the cutting life become little lower than that of existing tools using coolant. In the survey of abrasion resistant/lubricous films, it was found out that in the adhesion to ultra-hard substrates, the DLC single-layer film consisting only of carbon indicated the same excellent adhesion as intermediate-layer inserts. As to the synthesis of abrasion resistant/lubricous films, the synthesis of the composite membrane (WC/C membrane) consisting of tungsten carbide (WC) and carbon (C) was made using arc ion plating device. The WC/C membrane is composed of W and C and has the structure in which at nm levels the layer with much W and the layer with less W were alternately piled. Study was made of devices necessary for the development of abrasion resistant/lubricous films and the film formation for drill. (NEDO)

  1. Sustainability of abrasive processes

    DEFF Research Database (Denmark)

    Aurich, J.C.; Linke, B.; Hauschild, Michael Zwicky

    2013-01-01

    , the content of technical presentations in STC G, and the results of a comprehensive literature study. The approach to sustainability includes environmental, social, and economic sustainability in accordance with the definition proposed in the Brundtland Report of the United Nations [156]. The main focus......This paper presents an overview of research on sustainability of abrasive processes. It incorporates results from a round robin study on ‘‘energy-efficiency of abrasive processes’’ which has been carried out within the scientific technical committee ‘‘abrasive processes’’ (STC G) of CIRP...... is on environmental and social sustainability. Economic sustainability will be considered as manufacturing productivity. © 2013 CIRP....

  2. Progress in abrasive and grinding technology

    CERN Document Server

    Xu, Xipeng

    2009-01-01

    The grinding and abrasive processing of materials are machining techniques which use bonded or loose abrasives to remove material from workpieces. Due to the well-known advantages of grinding and abrasive processes, advances in abrasive and grinding technology are always of great import in enhancing both productivity and component quality. In order to highlight the recent progress made in this field, the editor invited 21 world-wide contributions with the aim of gathering together all of the achievements of leading researchers into a single publication. The authors of the 21 invited papers, of

  3. Properties, structure and machnining capabilities sintered corundum abrasives

    Directory of Open Access Journals (Sweden)

    Cz.J. Niżankowski

    2010-07-01

    Full Text Available The diversity of sintered corundum abrasives used in both bonded and in the embankment of abrasive tools currently poses substantialproblems for their choice of technology to specific tasks. Therefore performed a comparative study of ownership structures and capacitiesof elected representatives machnining sintered corundum abrasives of different generations, and this is normal sintered alumina,submicrocrystalline alumina sintered and nanocrystalline alumina sintered. Were studied some properties of a set of abrasive particles,physicochemical properties and structural and mechanical and technological properties. The studies used the method of microscopicmeasurement to determine the shape of abrasive particles, the pycnometer to determine the density of abrasive, a spectrometer todetermine the chemical composition of the magnetic analyzer for determining the magnetic fraction, scanning electron microscope toanalysis of abrasive grains and a special position to designate the machining capacity abrasive grains. The results showed a significantincrease in machining capacity sintered corundum abrasives with increasing degree of fragmentation of the crystallites sintered corundum abrasives and distinctive bands in the emerging microchip. The originality of the development provides a comparative summary ofproperties of sintered corundum abrasives of different generations and functions obtained by the author making the change in value indexof machininhcapacity grit from cutting speeds for different generations of sintered corundum.

  4. Abrasive wear resistance optimization of three different carbide coatings by the Taguchi method

    Energy Technology Data Exchange (ETDEWEB)

    Guer, Ali Kaya [Firat Univ., Elazig (Turkey). Dept. of Metallurgy and Materials; Kaya, Sinan [Firat Univ., Elazig (Turkey). Faculty of Technology

    2017-06-01

    In this study, FeCrC, SiC and B{sub 4}C powders were alloyed on the surface of AISI 430 ferritic stainless steel by plasma arc welding. The mass losses of the abrasive wear of the AISI 430 substrate were examined under the loads of 6, 10 and 16 N and in the distances of 10, 20 and 30 m by using Taguchi design method. The results of abrasive wear test were optimized by the minimum optimal control characteristics of the Taguchi procedure and the results were analyzed by using graphical methods. The Taguchi procedure is an important approach to achieve high quality without increasing the cost during the optimization of process parameters. The orthogonal planes of maximum effects of the controllable process parameters and minimum effects of uncontrollable process parameters were employed in the Taguchi method.

  5. Aging temperature and abrasive wear behaviour of cast Al-(4%, 12%, 20%)Si-0.3% Mg alloys

    International Nuclear Information System (INIS)

    Shah, K.B.; Kumar, Sandeep; Dwivedi, D.K.

    2007-01-01

    In the present paper, influence of aging temperature during artificial age hardening treatment (T 6 ) of cast Al-(4, 12, 20%)Si-0.3% Mg on abrasive wear behaviour has been reported. Alloys were prepared by controlled melting and casting. Cast alloys were given age hardening treatment having sequence of solutionizing, quenching and artificial aging. All the alloys were solutionized at 510 deg. C for 8 h followed by water quenching (30 deg. C) and aging hardening at 150, 170, 190, 210 and 230 deg. C for 12 h. Abrasive wear tests were conducted against of 320 grade SiC abrasive medium at 5 and 10 N normal loads. It was observed that the silicon content and aging temperature significantly affect the wear resistance. Increase in aging temperature improves the wear resistance. Hypereutectic alloy showed better wear resistance than the eutectic alloy under identical conditions. Optical microstructure study of alloys under investigation has shown that cast dendritic structure is destroyed besides the spheroidization of eutectic silicon crystals after the heat treatment. The extent of change in structure depends on aging temperature. Scanning electron microscopy (SEM) of wear surface was carried to analyze the wear mechanism

  6. Development of the white cast iron with niobium alloy, heat treating, to wear of the abrasive resistance

    International Nuclear Information System (INIS)

    Farah, Alessandro Fraga

    1997-01-01

    This work presents the heat treatment and abrasion tests results of a white cast iron with niobium alloy. The hardening heat treatment were made 950, 1000, 1050 e 110 deg C temperatures cooled by forced air. The tempering treatment were made at 450, 500 e 550 deg C temperatures. The heat treating alloy were compared, in the abrasive tests, with commercial alloys used as hardfacing by welding process in wear pieces. The abrasion tests was realized in pin on disk test. Additional tests were carried out for microstructural characterization to identify the different phases presents in the alloys. In a general way, the alloy studies showed the best wear rate for the heat treatments that results in higher hardness. It performance was superior than that of the commercial alloys. (author)

  7. Abrasion of Polymeric Composites on Basis of Machining Splinters from Hardfacing Alloys – Usable in Agrocomplex

    Directory of Open Access Journals (Sweden)

    Petr Valášek

    2014-01-01

    Full Text Available A paper focuses on a description of two-body and three-body abrasion wear of polymeric particle composites with fillers on a basis of machining splinters from hardfacing alloys. The abrasive wear is typical for functional surfaces of agricultural machines processing the soil. One of possibilities of the functional surface renovation is an application of resistant layers in a form of composite systems. Just the inclusion of hard inorganic particles into a polymeric matrix significantly increases its wear resistance. So long as the primary filler is replaced by the waste – by particles from the material machining – the matrix in which the filler is dispersed is a bearer of a material recyclation. This way of the recyclation is inexpensive, economic and sensitive to environment. The paper focuses on the experimental description of the two-body and three-body abrasion and the composites hardness, it describes a production of a prototype for field tests with the functional surface on the basis of the investigated composite system at the same time.

  8. Solutionizing temperature and abrasive wear behaviour of cast Al-Si-Mg alloys

    International Nuclear Information System (INIS)

    Sharma, Rajesh; Anesh; Dwivedi, D.K.

    2007-01-01

    In the present paper, the influence of solutionizing temperature during artificial age hardening treatment (T 6 ) of cast Al-(8, 12, 16%)Si-0.3%Mg on abrasive wear behaviour has been reported. Alloys were prepared by controlled melting and casting. Cast alloys were given artificial age hardening treatment having a sequence of solutionizing, quenching and artificial aging. All the alloys were solutionized at 450 deg. C, 480 deg. C, 510 deg. C, and 550 deg. C for 8 h followed by water quenching (30 deg. C) and aging hardening at 170 deg. C for 12 h. Abrasive wear tests were conducted against 320 grade SiC polishing papers at 5 N and 10 N normal loads. It was observed that the silicon content and solution temperature affected the wear resistance significantly. Increase in solution temperature improved the wear resistance. Hypereutectic alloy showed better wear resistance than the eutectic and hypoeutectic alloys under identical conditions. Optical microstructure study of alloys revealed that the increase in solutionizing temperature improved distribution of silicon grains. Scanning electron microscopy (SEM) of wear surface was carried out to analyze the wear mechanism

  9. Splitting strength and abrasion resistance of concrete paving blocks as a function of dry bulk specific gravity and ultrasonic pulse velocity

    Directory of Open Access Journals (Sweden)

    Haktanir, T.

    2005-06-01

    Full Text Available Artificial Portland cement concrete paving blocks are widely used in many countries. These paving blocks come in a variety of designs with names such as "Interlocking" and "Italian Flower", and are manufactured with special machinery using rather high quality concrete having a compressive strength of about 50 MPa. Concrete blocks are employed instead of natural cobble stones for essentially economic reasons. The laboratoiy equipment required to measure paving block splitting strength and abrasion resistance, two of the chief properties to be tested in quality checks, is costly and the tests are time-consuming and labour-intensive. The present paper reports on a detailed experimental study performed to relate the splitting strength and abrasion resistance of concrete paving blocks to "dry bulk specific gravity" (DBSG and "ultrasonic pulse velocity" (UPV, respectively. Statistically significant regression equations describing the dependence of splitting strength on DBSG and abrasion resistance on UPV were obtained with data from random samples of material provided by seven different manufacturers.

    RESUMEN Los bloques para pavimentos (adoquines elaborados con hormigón se utilizan habitualmente en numerosos países. Estos bloques de pavimentación se diseñan de diversas formas, como por ejemplo "Entrelazado " ("Interlocking " o "Flor Italiana " ("Italian Flower"; se fabrican con maquinaria especial y con frecuencia se utiliza hormigón de la más alta calidad, con resistencia a la compresión de alrededor de 50 MPa. La razón de utilizar bloques de hormigón en lugar de bloques de piedra natural es básicamente económica. Los equipos de laboratorio necesarios para medir la resistencia a la compresión y a la abrasión -dos de las propiedades más importantes para determinar la calidad de los bloques en estudio- son costosos y los ensayos requieren tiempo y mano de obra considerables. En el presente trabajo se exponen ensayos experimentales

  10. Wear behavior of carbon fiber/aluminium-composites during abrasive loading; Verschleissverhalten von Kohlenstoffaser/Aluminium-Verbunden unter abrasiver Beanspruchung

    Energy Technology Data Exchange (ETDEWEB)

    Wielage, B.; Dorner, A. [Technische Univ. Chemnitz (Germany). Lehrstuhl fuer Verbundwerkstoffe

    1998-07-01

    Abrasive wear resistance of aluminium is significantly improved by the reinforcement with a high volume percentage of carbon fibres. The wear of unreinforced aluminium after scratching by a diamond indenter can be described as pure microgrooving without any micro-chipping. After integration of 70 vol.-% carbon fibers the damage mechanism is considerably altered and a great amount of micro-chipping occurs. The abrasive wear is strongly influenced by the fiber orientation. The best wear resistance is observed when the fibers are orientated perpendicular to the wear surface. (orig.) [Deutsch] Die Verstaerkung von Aluminium mit einem hohen Volumengehalt endloser Kohlenstoffasern verbessert erkennbar dessen Resistenz gegenueber Abrasionsverschleiss. Der Verschleiss von unverstaerktem Aluminium infolge des Ritzens mit einem Diamantindenter erfolgt in Form von reinem Mikrofurchen ohne Spanbildung. Aufgrund der Integration von 70 Vol.-% Kohlenstoffasern wird eine erhebliche Zunahme des Schaedigungsmechanismus Mikrospanen festgestellt. Die Faserorientierung hat merklichen Einfluss auf die Sensibilitaet gegenueber Abrasion. Orientierung der anisotropen Kohlenstoffasern senkrecht zur Verschleissoberflaeche bedingt den geringsten Abrasionsverschleiss. (orig.)

  11. Study on design of light-weight super-abrasive wheel

    Science.gov (United States)

    Nohara, K.; Yanagihara, K.; Ogawa, M.

    2018-01-01

    Fixed-abrasive tool, also called a grinding wheel, is produced by furnacing abrasive compound which contains abrasive grains and binding powder such as vitrified materials or resins. Fixed-abrasive tool is installed on spindle of grinding machine. And it is given 1,800-2,000 min-1 of spindle rotation for the usage. The centrifugal fracture of the compound of fixed- abrasive tool is one of the careful respects in designing. In recent years, however, super-abrasive wheel as a fixed-abrasive tool has been developed and applied widely. One of the most characteristic respects is that metal is applied for the body of grinding-wheel. The strength to hold abrasive grain and the rigidity of wheel become stronger than those of general grinding wheel, also the lifespan of fixed-abrasive tool becomes longer. The weight of fixed-abrasive tool, however, becomes heavier. Therefore, when the super-abrasive wheel is used, the power consumption of spindle motor becomes larger. It also becomes difficult for the grinding-wheel to respond to sudden acceleration or deceleration. Thus, in order to reduce power consumption in grinding and to obtain quicker frequency response of super-abrasive wheel, the new wheel design is proposed. The design accomplishes 46% weight reduction. Acceleration that is one second quicker than that of conventional grinding wheel is obtained.

  12. Abrasive water jets for controlled demolition and dismantling

    International Nuclear Information System (INIS)

    Abudaka, M.; Crofton, P.S.J.

    1988-01-01

    Abrasive water jets offer an efficient high speed cutting tool for hard materials such as reinforced concrete, tool steel and armour plate. Cutting by abrasive water jets is often described as a cold cutting operation since no heat is developed and any increase in local temperature is immediately cooled by the water jet. Moreover no sparks are generated to ignite a potentially inflammable atmosphere. Mass flow rates of water and abrasive are small (typically 4 litres/min.water and 1 kg/min abrasive) and hence are easy to collect and to dispose of. For these reasons abrasive water jets offer certain advantages in cutting difficult materials in hazardous environments such as in the nuclear industry, offshore oil rigs and petrochemical plant. Available portable cutting systems are described and the advantages of using abrasive water jets are discussed as well as some of the parameters involved in the cutting operation. Finally a description is presented of some typical applications of abrasive water jet cutting. (author)

  13. Cleaning power and abrasivity of European toothpastes.

    Science.gov (United States)

    Wülknitz, P

    1997-11-01

    For 41 toothpastes available to European consumers in 1995, the cleaning efficacy was evaluated in comparison with abrasivity on dentin (RDA value). For cleaning power assessment, a modified pellicle cleaning ratio (PCR) measurement method was developed. The method is characterized by a five-day tea-staining procedure on bovine front teeth slabs on a rotating wheel, standardized brushing of the slabs in a V8 cross-brushing machine, and brightness measurement by a chromametric technique. All tested products were in accordance with the new DIN/ISO standard 11,609 for toothpastes in terms of dentin abrasivity. Not a single product exceeded an RDA value of 200. The majority of toothpastes (80%) had an RDA value below 100. Only three products surpassed the reference in cleaning power. Most products (73%) had a cleaning power (PCR value) between 20 and 80. The correlation between cleaning power and dentin abrasion was low (r = 0.66), which can be explained with the different influence on dentin and stains by factors like abrasive type, particle surface and size, as well as the chemical influence of other toothpaste ingredients. Some major trends could be shown on the basis of abrasive types. The ratio PCR to RDA was rather good in most silica-based toothpastes. A lower ratio was found in some products containing calcium carbonate or aluminum trihydrate as the only abrasive. The addition of other abrasives, such as polishing alumina, showed improved cleaning power. Some active ingredients, especially sequenstrants such as sodium tripolyphosphate or AHBP, also improve the PCR/RDA ratio by stain-dissolving action without being abrasive. The data for some special anti-stain products did not differ significantly from standard products. Compared with data measured in 1988, a general trend toward reduced abrasivity without loss of cleaning efficacy could be noticed on the European toothpaste market. This may be mostly due to the increased use of high-performance abrasives such

  14. Ceramic-bonded abrasive grinding tools

    Science.gov (United States)

    Holcombe, Jr., Cressie E.; Gorin, Andrew H.; Seals, Roland D.

    1994-01-01

    Abrasive grains such as boron carbide, silicon carbide, alumina, diamond, cubic boron nitride, and mullite are combined with a cement primarily comprised of zinc oxide and a reactive liquid setting agent and solidified into abrasive grinding tools. Such grinding tools are particularly suitable for grinding and polishing stone, such as marble and granite.

  15. Ceramic-bonded abrasive grinding tools

    Science.gov (United States)

    Holcombe, C.E. Jr.; Gorin, A.H.; Seals, R.D.

    1994-11-22

    Abrasive grains such as boron carbide, silicon carbide, alumina, diamond, cubic boron nitride, and mullite are combined with a cement primarily comprised of zinc oxide and a reactive liquid setting agent and solidified into abrasive grinding tools. Such grinding tools are particularly suitable for grinding and polishing stone, such as marble and granite.

  16. Determination of vibration frequency depending on abrasive mass flow rate during abrasive water jet cutting

    Czech Academy of Sciences Publication Activity Database

    Hreha, P.; Radvanská, A.; Hloch, Sergej; Peržel, V.; Krolczyk, G.; Monková, K.

    2014-01-01

    Roč. 77, 1-4 (2014), s. 763-774 ISSN 0268-3768 Institutional support: RVO:68145535 Keywords : Abrasive water jet * Abrasive mass flow rate * Vibration Subject RIV: JQ - Machines ; Tools Impact factor: 1.458, year: 2014 http://link.springer.com/article/10.1007%2Fs00170-014-6497-9#page-1

  17. Tribological properties of multifunctional coatings with Shape Memory Effect in abrasive wear

    Science.gov (United States)

    Blednova, Zh. M.; Dmitrenko, D. V.; Balaev, E. U. O.

    2018-01-01

    The article gives research results of the abrasive wear process on samples made of Steel 1045, U10 and with applied composite surface layer "Nickel-Multicomponent material with Shape Memory Effect (SME) based on TiNi". For the tests we have chosen TiNiZr, which is in the martensite state and TiNiHfCu, which is in the austenitic state at the test temperature. The formation of the surface layer was carried out by high-speed oxygen-fuel deposition in a protective atmosphere of argon. In the wear test, Al2O3 corundum powder was used as an abrasive. It is shown that the wear rate of samples with a composite surface layer of multicomponent materials with SME is significantly reduced in comparison with the base, which is explained by reversible phase transformations of the surface layer with SME. After carrying out the additional surface plastic deformation (SPD), the resistance of the laminated composition to abrasion wear has greatly enhanced, due to the reinforcing effect of the SPD. It is recommended for products working in conditions of abrasive wear and high temperatures to use the complex formation technology of the surface composition "steel-nickel-material with high-temperature SME", including preparation of the substrate surface and the deposited material, high-speed spraying in the protective atmosphere of argon, followed by SPD.

  18. Effect of filler type on 3-body abrasion of dental composite

    Directory of Open Access Journals (Sweden)

    Yasini E.

    2005-06-01

    Full Text Available Statement of Problem: The relatively poor wear resistance of dental composite in stress bearing posterior situations has restricted wider clinical application of this restorative material. Purpose: The aim of this study was to evaluate the three body abrasive wear of a dental composite based on a new filler (leucite: KAl Si2O6 and to compare it with the wear resistance of a composite based on commonly used Aluminium – Barium Silicate filler. Materials and Methods: This research was an interventional study done in Iran polymer institute. Five specimens were considered in each group. All ceramic IPS Empress® (Ivoclar- Vivadent ingots based on leucite crystals were ball milled, passed through an 800 sieve and used as filler. Experimental composites were prepared by mixing the silane- treated fillers with monomers (BisGMA and TEGDMA. Camphorquinone and amine were used as photoinitiator system. Degree of conversion of the light-cured and post-cured composites was measured using FTIR spectroscopy. The prepared pastes were inserted into plexy-glass mold and light cured (700 mw/cm2, 40 s. Then for maximum degree of conversion specimens were post- cured (120ºC, 5 hours. Three body abrasion wear testing was performed using a wear machine with 50 rpm rotational movement. In this machine, pumice (150 meshes was used as the third body. Weight loss of specimens in each group was measured by balance after each 50 hours. After wear testing SEM examination was made specimens in each group. The data were analyzed and compared using ANOVA and Tukey HSD tests (P<0.05. Tetric Ceram was tested as commercial composite. Results: There were significantly differences between three body abrasive wear of composites. The ranking from lowest to highest was as follows: leucite composite (19% < Tetric Ceram (22% < glass composite (28%. leucite composite showed the highest wear resistance value, propably due to the crystalliniy and hardness of filler. Conclusion

  19. Ultrasonic Abrasive Removal Of EDM Recast

    Science.gov (United States)

    Mandel, Johnny L.; Jacobson, Marlowe S.

    1990-01-01

    Ultrasonic abrasive process removes layer of recast material generated during electrical-discharge machining (EDM) of damper pocket on turbine blade. Form-fitted tool vibrated ultrasonically in damper pocket from which material removed. Vibrations activate abrasive in pocket. Amount of material removed controlled precisely.

  20. Effects of Load and Speed on Wear Rate of Abrasive Wear for 2014 Al Alloy

    Science.gov (United States)

    Odabas, D.

    2018-01-01

    In this paper, the effects of the normal load and sliding speed on wear rate of two-body abrasive wear for 2014 Al Alloy were investigated in detail. In order to understand the variation in wear behaviour with load and speed, wear tests were carried out at a sliding distance of 11 m, a speed of 0.36 m/s, a duration of 30 s and loads in the range 3-11 N using 220 grit abrasive paper, and at a speed range 0.09-0.90 m/s, a load of 5 N and an average sliding distance of 11 m using abrasive papers of 150 grit size under dry friction conditions. Before the wear tests, solution treatment of the 2014 Al alloy was carried out at temperatures of 505 and 520 °C for 1 h in a muffle furnace and then quenched in cold water at 15 °C. Later, the ageing treatment was carried out at 185 °C for 8 h in the furnace. Generally, wear rate due to time increased linearly and linear wear resistance decreased with increasing loads. However, the wear rate was directly proportional to the load up to a critical load of 7 N. After this load, the slope of the curves decreased because the excessive deformation of the worn surface and the instability of the abrasive grains began to increase. When the load on an abrasive grain reaches a critical value, the groove width is about 0.17 of the abrasive grain diameter, and the abrasive grains begin to fail. The wear rate due to time increased slightly as the sliding speed increased in the range 0.09-0.90 m/s. The reason for this is that changes arising from strain rate and friction heating are expected with increasing sliding speeds.

  1. New Rock Abrasivity Test Method for Tool Life Assessments on Hard Rock Tunnel Boring: The Rolling Indentation Abrasion Test (RIAT)

    Science.gov (United States)

    Macias, F. J.; Dahl, F.; Bruland, A.

    2016-05-01

    The tunnel boring machine (TBM) method has become widely used and is currently an important presence within the tunnelling industry. Large investments and high geological risk are involved using TBMs, and disc cutter consumption has a great influence on performance and cost, especially in hard rock conditions. Furthermore, reliable cutter life assessments facilitate the control of risk as well as avoiding delays and budget overruns. Since abrasive wear is the most common process affecting cutter consumption, good laboratory tests for rock abrasivity assessments are needed. A new abrasivity test method by rolling disc named Rolling Indentation Abrasion Test (RIAT) has been developed. The goal of the new test design and procedure is to reproduce wear behaviour on hard rock tunnel boring in a more realistic way than the traditionally used methods. Wear by rolling contact on intact rock samples is introduced and several rock types, covering a wide rock abrasiveness range, have been tested by RIAT. The RIAT procedure indicates a great ability of the testing method to assess abrasive wear on rolling discs. In addition and to evaluate the newly developed RIAT test method, a comprehensive laboratory testing programme including the most commonly used abrasivity test methods and the mineral composition were carried out. Relationships between the achieved results from conventional testing and RIAT results have been analysed.

  2. Experimental Rock-on-Rock Abrasive Wear Under Aqueous Conditions: its Role in Subglacial Abrasion

    Science.gov (United States)

    Rutter, E. H.; Lee, A. G.

    2003-12-01

    We have determined experimentally the rate of abrasive wear of rock on rock for a range of rock types as a function of normal stress and shear displacement. Unlike abrasive wear in fault zones, where wear products accumulate as a thickening gouge zone, in our experiments wear particles were removed by flowing water. The experiments are thus directly pertinent to one of the most important processes in subglacial erosion, and to some extent in river incision. Wear was produced between rotating discs machined from rock samples and measured from the progressive approach of the disc axes towards each other under various levels of normal load. Shear displacements of several km were produced. Optical and scanning electron microscopy were used to study the worn rock surfaces, and particle size distributions in wear products were characterized using a laser particle size analyzer. Rock types studied were sandstones of various porosities and cement characteristics, schists and a granite. In all cases abrasion rate decreased logarithmically with displacement by up to 2 orders of magnitude until a steady state was approached, but only after at least 1 km displacement. The more porous, less-well cemented rocks wore fastest. Amount of abrasion could be characterized quantitatively using an exponentially decaying plus a steady-state term. Wear rate increased non-linearly with normal contact stress, apparently to an asymptote defined by the unconfined compressive strength. Microstructural study showed that the well-cemented and/or lowest porosity rocks wore by progressive abrasion of grains without plucking, whereas whole grains were plucked out of weakly-cemented and/or more porous rocks. This difference in behavior was reflected in wear-product particle size distributions. Where whole-grain plucking was possible, wear products were dominated by particles of the original grain size rather than finer rock flour. Comparison of our results to glacier basal abrasive wear estimated

  3. Recent Developments in Abrasive Hybrid Manufacturing Processes

    Directory of Open Access Journals (Sweden)

    Ruszaj Adam

    2017-06-01

    Full Text Available Recent dynamic development of abrasive hybrid manufacturing processes results from application of a new difficult for machining materials and improvement of technological indicators of manufacturing processes already applied in practice. This tendency also occurs in abrasive machining processes which are often supported by ultrasonic vibrations, electrochemical dissolution or by electrical discharges. In the paper we present the review of new results of investigations and new practical applications of Abrasive Electrodischarge (AEDM and Electrochemical (AECM Machining.

  4. Sandstone Turning by Abrasive Waterjet

    Czech Academy of Sciences Publication Activity Database

    Hlaváček, Petr; Cárach, J.; Hloch, Sergej; Vasilko, K.; Klichová, Dagmar; Klich, Jiří; Lehocká, D.

    2015-01-01

    Roč. 48, č. 6 (2015), s. 2489-2493 ISSN 0723-2632 R&D Projects: GA MŠk ED2.1.00/03.0082; GA MŠk(CZ) LO1406 Institutional support: RVO:68145535 Keywords : turning away from the jet * conventional turning towards the jet * sandstone * abrasive water jet Subject RIV: JQ - Machines ; Tools Impact factor: 2.386, year: 2015 http://www.springerprofessional.de/sandstone-turning-by-abrasive-waterjet/6038028.html

  5. Comparing the Air Abrasion Cutting Efficacy of Dentine Using a Fluoride-Containing Bioactive Glass versus an Alumina Abrasive: An In Vitro Study

    Directory of Open Access Journals (Sweden)

    Melissa H. X. Tan

    2015-01-01

    Full Text Available Air abrasion as a caries removal technique is less aggressive than conventional techniques and is compatible for use with adhesive restorative materials. Alumina, while being currently the most common abrasive used for cutting, has controversial health and safety issues and no remineralisation properties. The alternative, a bioactive glass, 45S5, has the advantage of promoting hard tissue remineralisation. However, 45S5 is slow as a cutting abrasive and lacks fluoride in its formulation. The aim of this study was to compare the cutting efficacy of dentine using a customised fluoride-containing bioactive glass Na0SR (38–80 μm versus the conventional alumina abrasive (29 μm in an air abrasion set-up. Fluoride was incorporated into Na0SR to enhance its remineralisation properties while strontium was included to increase its radiopacity. Powder outflow rate was recorded prior to the cutting tests. Principal air abrasion cutting tests were carried out on pristine ivory dentine. The abrasion depths were quantified and compared using X-ray microtomography. Na0SR was found to create deeper cavities than alumina (p<0.05 despite its lower powder outflow rate and predictably reduced hardness. The sharper edges of the Na0SR glass particles might improve the cutting efficiency. In conclusion, Na0SR was more efficacious than alumina for air abrasion cutting of dentine.

  6. Life cycle and sustainability of abrasive tools

    CERN Document Server

    Linke, Barbara

    2016-01-01

    This monograph focuses on abrasive tools for grinding, polishing, honing, and lapping operations. The book describes the life cycle of abrasive tools from raw material processing of abrasive grits and bonding, manufacturing of monolithic or multi-layered tools, tool use to tool end-of-life. Moreover, this work highlights sustainability challenges including economic, environmental, social and technological aspects. The target audience primarily comprises research and industry experts in the field of manufacturing, but the book may also be beneficial for graduate students.

  7. Abrasive wear of intermetallics

    International Nuclear Information System (INIS)

    Hawk, J.A.; Alman, D.E.; Wilson, R.D.

    1995-01-01

    The US Bureau of Mines is investigating the wear behavior of a variety of advanced materials. Among the many materials under evaluation are intermetallic alloys based on the compounds: Fe 3 Al, Ti 3 Al, TiAl, Al 3 Ti, NiAl and MoSi 2 . The high hardness, high modulus, low density, and superior environmental stability of these compounds make them attractive for wear materials. This paper reports on the abrasive wear of alloys and composites based on the above compounds. The abrasive wear behavior of these alloys and composites are compared to other engineering materials used in wear applications

  8. Abrasive water jet: a complementary tool

    International Nuclear Information System (INIS)

    Duarte, J.P.; Pecas, P.; Nunes, E.; Gouveia, H.

    1998-01-01

    The abrasive water jet is a powerful cutting tool, whose main advantages lie in the absence of thermal effects and the capability of cutting highly thick materials. Compared with Laser, the abrasive water jet allows the cutting of a larger range of thicknesses and a wider variety of materials such as: ornamental stones, metals, polymers, composites, wood, glass ceramics. The application of this technology has suffered and extensive growth, with successful applications in varied industrial sectors like the automotive, aerospace, textile, metalworking, ornamental stones, etc. The present communication aims at introducing the abrasive water jet as a complementary tool to laser cutting, presenting its advantages by showing some documented examples of pieces cut for different industries. (Author) 5 refs

  9. Assessment of mechanical and three-body abrasive wear peculiarity ...

    Indian Academy of Sciences (India)

    The three-body abrasive wear characteristic of fabricated composites has been assessed under different operating conditions. For this, the three-body abrasion test is done on dry abrasion test rig (TR-50)and analysed using Taguchi's experimental design scheme and analysis of variance. The results obtained from these ...

  10. 21 CFR 872.6030 - Oral cavity abrasive polishing agent.

    Science.gov (United States)

    2010-04-01

    ... 21 Food and Drugs 8 2010-04-01 2010-04-01 false Oral cavity abrasive polishing agent. 872.6030... (CONTINUED) MEDICAL DEVICES DENTAL DEVICES Miscellaneous Devices § 872.6030 Oral cavity abrasive polishing agent. (a) Identification. An oral cavity abrasive polishing agent is a device in paste or powder form...

  11. Abrasion of 6 dentifrices measured by vertical scanning interference microscopy.

    Science.gov (United States)

    Pascaretti-Grizon, Florence; Mabilleau, Guillaume; Chappard, Daniel

    2013-01-01

    The abrasion of dentifrices is well recognized to eliminate the dental plaque. The aims of this study were to characterize the abrasive powders of 6 dentifrices (3 toothpastes and 3 toothpowders) and to measure the abrasion on a test surface by Vertical Scanning Interference microscopy (VSI). Bright field and polarization microscopy were used to identify the abrasive particles on the crude dentifrices and after prolonged washes. Scanning electron microscopy and microanalysis characterized the shape and nature of the particles. Standardized and polished blocks of poly(methylmethacrylate) were brushed with a commercial electric toothbrush with the dentifrices. VSI quantified the mean roughness (Ra) and illustrated in 3D the abraded areas. Toothpastes induced a limited abrasion. Toothpowders induced a significantly higher roughness linked to the size of the abrasive particles. One powder (Gencix® produced a high abrasion when used with a standard testing weight. However, the powder is based on pumice particles covered by a plant homogenate that readily dissolves in water. When used in the same volume, or after dispersion in water, Ra was markedly reduced. Light and electron microscopy characterize the abrasive particles and VSI is a new tool allowing the analysis of large surface of abraded materials.

  12. Basics of cutting and abrasive processes

    CERN Document Server

    Toenshoff, Hans Kurt

    2013-01-01

    Manufacturing is the basic industrial activity generating real value. Cutting and abrasive technologies are the backbone of precision production in machine, automotive and aircraft building as well as of production of consumer goods. We present the knowledge of modern manufacturing in these technologies on the basis of scientific research. The theory of cutting and abrasive processes and the knowledge about their application in industrial practice are a prerequisite for the studies of manufacturing science and an important part of the curriculum of the master study in German mechanical engineering. The basis of this book is our lecture “Basics of cutting and abrasive processes” (4 semester hours/3 credit hours) at the Leibniz University Hannover, which we offer to the diploma and master students specializing in manufacturing science.

  13. Performance Evaluation of Abrasive Grinding Wheel Formulated ...

    African Journals Online (AJOL)

    This paper presents a study on the formulation and manufacture of abrasive grinding wheel using locally formulated silicon carbide abrasive grains. Six local raw material substitutes were identified through pilot study and with the initial mix of the identified materials, a systematic search for an optimal formulation of silicon ...

  14. Dentifrice fluoride and abrasivity interplay on artificial caries lesions.

    Science.gov (United States)

    Nassar, Hani M; Lippert, Frank; Eckert, George J; Hara, Anderson T

    2014-01-01

    Incipient caries lesions on smooth surfaces may be subjected to toothbrushing, potentially leading to remineralization and/or abrasive wear. The interplay of dentifrice abrasivity and fluoride on this process is largely unknown and was investigated on three artificially created lesions with different mineral content/distribution. 120 bovine enamel specimens were randomly allocated to 12 groups (n = 10), resulting from the association of (1) lesion type [methylcellulose acid gel (MeC); carboxymethylcellulose solution (CMC); hydroxyethylcellulose gel (HEC)], (2) slurry abrasive level [low (REA 4/ RDA 69); high (REA 7/RDA 208)], and (3) fluoride concentration [0/275 ppm (14.5 mM) F as NaF]. After lesion creation, specimens were brushed in an automated brushing machine with the test slurries (50 strokes 2×/day). Specimens were kept in artificial saliva in between brushings and overnight. Enamel surface loss (SL) was determined by optical profilometry after lesion creation, 1, 3 and 5 days. Two enamel sections (from baseline and post-brushing areas) were obtained and analyzed microradiographically. Data were analyzed by analysis of variance and Tukey's tests (α = 5%). Brushing with high-abrasive slurry caused more SL than brushing with low-abrasive slurry. For MeC and CMC lesions, fluoride had a protective effect on SL from day 3 on. Furthermore, for MeC and CMC, there was a significant mineral gain in the remaining lesions except when brushed with high-abrasive slurries and 0 ppm F. For HEC, a significant mineral gain took place when low-abrasive slurry was used with fluoride. The tested lesions responded differently to the toothbrushing procedures. Both slurry fluoride content and abrasivity directly impacted SL and mineral gain of enamel caries lesions.

  15. 29 CFR 1910.215 - Abrasive wheel machinery.

    Science.gov (United States)

    2010-07-01

    ... be securely fastened to the spindle and the bearing surface shall run true. When more than one wheel... 29 Labor 5 2010-07-01 2010-07-01 false Abrasive wheel machinery. 1910.215 Section 1910.215 Labor... OCCUPATIONAL SAFETY AND HEALTH STANDARDS Machinery and Machine Guarding § 1910.215 Abrasive wheel machinery. (a...

  16. Anisotropy abrasive wear behavior of bagasse fiber reinforced ...

    African Journals Online (AJOL)

    parallel orientation (APO) and normal orientation (NO) by using a two body abrasion wear tester. Three different types of abrasives wear behaviour have been observed in the composite in three orientations and follow the following trends: WNO ...

  17. ESTRATÉGIA DO DESENVOLVIMENTO URBANO COMO FATOR DETERMINANTE PARA O DESENVOLVIMENTO INDUSTRIAL SUSTENTÁVEL

    Directory of Open Access Journals (Sweden)

    Rúbia Tânia Welter

    2016-11-01

    Full Text Available Este artigo tem por objetivo identificar a estratégia do desenvolvimento urbano como fator do desenvolvimento industrial sustentável. Para alcançar este objetivo, foi realizada uma pesquisa documental e uma revisão histórico-bibliográfica de uma cidade, neste caso, a cidade de Joinville-SC. Foi realizado, também, um estudo sobre a evolução dos acontecimentos históricos da cidade pesquisada, como forma de estabelecer que estratégias adotadas interferiram neste processo de desenvolvimento. Como resultado, foram identificados os fatores estratégicos inerentes ou determinantes para o desenvolvimento industrial da cidade. Palavras-chave: Desenvolvimento urbano. Desenvolvimento industrial. Fatores estratégicos.

  18. Transition metal carbide and boride abrasive particles

    International Nuclear Information System (INIS)

    Valdsaar, H.

    1978-01-01

    Abrasive particles and their preparation are discussed. The particles consist essentially of a matrix of titanium carbide and zirconium carbide, at least partially in solid solution form, and grains of crystalline titanium diboride dispersed throughout the carbide matrix. These abrasive particles are particularly useful as components of grinding wheels for abrading steel. 1 figure, 6 tables

  19. Abrasive water jet: a complementary tool

    OpenAIRE

    Duarte, J. P.; Peças, P.; Nunes, E.; Gouveia, H.

    1998-01-01

    The abrasive water jet is a powerful cutting tool, whose main advantages lie in the absence of thermal effects and the capability of cutting highly thick materials. Compared with Laser, the abrasive water jet allows the cutting of a larger range of thicknesses and a wider variety of materials such as: ornamental stones, metals, polymers, composites, wood, glass and ceramics. The application of this technology has suffered an extensive growth, with successful applications in varied industrial ...

  20. Wear of dentine in vitro by toothpaste abrasives and detergents alone and combined.

    Science.gov (United States)

    Moore, C; Addy, M

    2005-12-01

    To measure in vitro the abrasion of dentine by toothpaste detergents and abrasives alone and combined. Detergents used were tego betain, sodium lauryl sulphate (SLS), adinol and pluronic diluted to 1% w/v. Abrasives were three artificial silicas, tixosil 73 and 123 and Zeodent 113, and calcium carbonate used at 2.5% w/v. Flat human dentine specimens were brushed with aqueous detergent solutions or abrasive slurries, detergent abrasive slurries and water for 20,000 brush strokes. Dentine loss was measured by non-contacting profilometry at 10,000 and 20,000 strokes. Silica particle size distribution was measured by laser deflection. Loss of dentine occurred with all detergents, abrasives and detergent abrasion combinations, but was not linear with number of brush strokes. Water appeared to remove the smear layer only, but all detergents exceeded the predicted smear layer thickness. The silica abrasives differed in abrasion properties despite similar particle size distribution. Different detergents modulated the abrasives actions in mainly positive or mainly negative directions. Detergents appear able to attack the dentine surface to produce wear. Abrasives vary considerably in wear produced under similar conditions. Detergents modulate the effect of abrasives in a way that may reflect the rheological properties of the mixture.

  1. Effect of Abrasive Machining on the Electrical Properties Cu86Mn12Ni₂ Alloy Shunts.

    Science.gov (United States)

    Misti, Siti Nabilah; Birkett, Martin; Penlington, Roger; Bell, David

    2017-07-29

    This paper studies the effect of abrasive trimming on the electrical properties of Cu 86 Mn 12 Ni₂ Manganin alloy shunt resistors. A precision abrasive trimming system for fine tuning the resistance tolerance of high current Manganin shunt resistors is proposed. The system is shown to be capable of reducing the resistance tolerance of 100 μΩ shunts from their standard value of ±5% to <±1% by removing controlled amounts of Manganin material using a square cut trim geometry. The temperature coefficient of resistance (TCR), high current, and high temperature performance of the trimmed shunts was compared to that of untrimmed parts to determine if trimming had any detrimental effect on these key electrical performance parameters of the device. It was shown that the TCR value was reduced following trimming with typical results of +106 ppm/°C and +93 ppm/°C for untrimmed and trimmed parts respectively. When subjected to a high current of 200 A the trimmed parts showed a slight increase in temperature rise to 203 °C, as compared to 194 °C for the untrimmed parts, but both had significant temporary increases in resistance of up to 1.3 μΩ. The results for resistance change following high temperature storage at 200 °C for 168 h were also significant for both untrimmed and trimmed parts with shifts of 1.85% and 2.29% respectively and these results were related to surface oxidation of the Manganin alloy which was accelerated for the freshly exposed surfaces of the trimmed part.

  2. FE simulation of the indentation deformation of SiC modified vinylester composites in respect to their abrasive wear performance

    Directory of Open Access Journals (Sweden)

    2008-10-01

    Full Text Available The abrasive sliding friction and wear behaviours of silicon carbide (SiC filled vinylester (VE composites were investigated. The average grain size of the incorporated SiC particles was varied, holding the volume content of them in every case at 16 vol%. Mechanical properties (hardness, compression modulus, yield stress of the filled and neat VE were determined. The tribological properties were investigated in block (composite – on – ring (steel test configuration. The steel counter bodies were covered with abrasive papers of different graining. Coefficient of friction (COF and specific wear rate of the VE + SiC composites were determined. It was observed that the wear resistance increases with increasing average filler grain size and with decreasing abrasiveness of the counter surface. The COF of the VE + SiC composites is independent of the size of the incorporated particles, but it is strongly influenced by the abrasiveness of the counter body. The worn surfaces of the VE + SiC systems were analysed in scanning electron microscope (SEM to deduce the typical wear mechanisms. The size effect of the SiC filler particles onto the abrasive wear characteristics was investigated by assuming that the roughness peaks of the abrasive paper and the indenter of the microhardness test cause similar micro scaled contact deformations in the composites. Therefore FE method was used to simulate the micro scaled deformation process in the VE + SiC systems during microindentation tests. The FE results provided valuable information on how to explain the size effect of the incorporated SiC filler.

  3. Method of forming an abrasive compact of cubic boron nitride

    International Nuclear Information System (INIS)

    Bell, F.R.

    1976-01-01

    This patent concerns an abrasive compact comprising diamond or cubic boron nitride or mixtures thereof held in a matrix of a refractory substance and a substance which dissolves the abrasive particle to at least a limited extent. The compact may be made by subjecting a powdered mixture of the ingredients to conditions of temperature and pressure at which the abrasive particle is crystallographically stable and the solvent substance acts to dissolve the abrasive particle. The refractory substance and solvent substance are preferably so chosen that during compact manufacture there is interaction resulting in the formation of a hard material

  4. Control technology for crystalline silica exposures in construction: wet abrasive blasting.

    Science.gov (United States)

    Golla, Vijay; Heitbrink, William

    2004-03-01

    This study was designed to document the effect that wet abrasive blasting has on reducing worker exposure to crystalline silica, which has been associated with silicosis and premature death. In this study, worker exposure to respirable crystalline silica was monitored during wet abrasive blasting on the exterior walls of a parking garage to remove surface concrete and expose the underlying aggregate. In this process a wet sand mix comprised of 80% dry sand and 20% water was used. Sampling and analysis revealed that the geometric mean respirable quartz concentration was 0.2 mg/m(3) for workers conducting abrasive blasting and 0.06 mg/m(3) for helpers. When abrasive blasting was conducted in areas that apparently had reduced natural ventilation, dust exposures appeared to increase. When compared with other published data, this case study suggests that wet abrasive blasting causes less exposure to crystalline silica than dry abrasive blasting.

  5. Submerged cutting characteristics of abrasive suspension jet

    International Nuclear Information System (INIS)

    Shimizu, Seiji; Peng, Guoyi; Oguma, Yasuyuki; Nishikata, Hiroki

    2015-01-01

    An abrasive suspension jet (ASJ) formed by propelling abrasive suspension through a nozzle has a greater cutting capability than the conventional abrasive water jet. However the cutting capability of submerged ASJs decreases drastically with increasing the standoff distance and the pressure around the jet. A sheathed nozzle nozzle with ventilation for ASJs has been developed as a mean of extending the effective stand-off distance and improving the cutting capabilities under submerged condition. In the present investigation, cutting tests by ASJs in air and under submerged condition are conducted with specimens of aluminum alloy. Air coated ASJs are formed by using a sheathed nozzle with ventilation. The relative cutting depth is defined as the cutting depth is arranged effectually by the cavitation number based on the cavity pressure measured at the sheath. (author)

  6. Influence of martensitic phase in abrasion behaviour of stainless steel 304 L

    International Nuclear Information System (INIS)

    Ruzzante, J.; Alvarez, P.; Hey, A.; Gestido, G.D.; Vosen, J.H.; Fernandez, H.A.

    1986-01-01

    Abrasion behaviour is studied in commercial stainless steels of different class compositions by standard. The work achieved guieds in structural analysis of superficial coat formed and its relation with abrasion variables, load and velocity. The abrasion is made in an equipment LF WK of high velocity with friction powers, abrasion velocity and temperature variation registered on the tested piece. The abrasion zone is studied with scanning electron microscope (SEM). The deformed superficial zone nature is studied relationing its microstructure with profile corresponding of microhardness. (C.M.C.T.R.) [pt

  7. Effect of Abrasive Machining on the Electrical Properties Cu86Mn12Ni2 Alloy Shunts

    Directory of Open Access Journals (Sweden)

    Siti Nabilah Misti

    2017-07-01

    Full Text Available This paper studies the effect of abrasive trimming on the electrical properties of Cu86Mn12Ni2 Manganin alloy shunt resistors. A precision abrasive trimming system for fine tuning the resistance tolerance of high current Manganin shunt resistors is proposed. The system is shown to be capable of reducing the resistance tolerance of 100 μΩ shunts from their standard value of ±5% to <±1% by removing controlled amounts of Manganin material using a square cut trim geometry. The temperature coefficient of resistance (TCR, high current, and high temperature performance of the trimmed shunts was compared to that of untrimmed parts to determine if trimming had any detrimental effect on these key electrical performance parameters of the device. It was shown that the TCR value was reduced following trimming with typical results of +106 ppm/°C and +93 ppm/°C for untrimmed and trimmed parts respectively. When subjected to a high current of 200 A the trimmed parts showed a slight increase in temperature rise to 203 °C, as compared to 194 °C for the untrimmed parts, but both had significant temporary increases in resistance of up to 1.3 μΩ. The results for resistance change following high temperature storage at 200 °C for 168 h were also significant for both untrimmed and trimmed parts with shifts of 1.85% and 2.29% respectively and these results were related to surface oxidation of the Manganin alloy which was accelerated for the freshly exposed surfaces of the trimmed part.

  8. MEIO AMBIENTE E DESENVOLVIMENTO

    Directory of Open Access Journals (Sweden)

    Suely Salgueiro Chacon

    2009-12-01

    Full Text Available O objetivo deste artigo é resgatar elementos para subsidiar uma reflexão crítica sobre o modelo de desenvolvimento econômico prevalente na sociedade e as relações com o meio ambiente, sob a ameaça que ronda o destino da espécie humana, conforme afirmação de Lovelock (2006, p. 20 sobre o conceito de desenvolvimento sustentável: “uma ideia adorável se a tivéssemos aplicado 200 anos atrás, quando havia um bilhão de pessoas no mundo. Agora é tarde demais. Não há mais espaço para nenhum tipo de desenvolvimento. A humanidade tem que regredir”. Este artigo apresenta a evolução do conceito de desenvolvimento econômico sob a ótica da sustentabilidade, e interliga temas como: o ambientalismo, aglutinador de distintos pensamentos sobre as relações entre a sociedade e a natureza; o movimento ambiental, a fundamentar a disseminação do conceito de desenvolvimento sustentável, e a gestão ambiental, abordada como prática orientada pelo conceito de desenvolvimento sustentável.

  9. Effect of nanofillers' size on surface properties after toothbrush abrasion.

    Science.gov (United States)

    Cavalcante, Larissa M; Masouras, Konstantinos; Watts, David C; Pimenta, Luiz A; Silikas, Nick

    2009-02-01

    To investigate the effect of filler-particle size of experimental and commercial resin composites, undergoing toothbrush abrasion, on three surface properties: surface roughness (SR), surface gloss (G) and color stability (CS). Four model (Ivoclar/Vivadent) and one commercial resin composite (Tokuyama) with varying filler-size from 100-1000 nm were examined. Six discs (10 mm x 2 mm) from each product were prepared and mechanically polished. The samples were then submitted to 20,000 brushing strokes in a toothbrush abrasion machine. SR parameters (Ra, Rt and RSm), G, and CS were measured before and after toothbrush abrasion. Changes in SR and G were analyzed by 2-way ANOVA, with Bonferroni post hoc test. CS values were submitted to one-way ANOVA and Bonferroni post hoc test (alpha=0.05). Initial G values ranged between 73-87 gloss units (GU) and were reduced after toothbrush abrasion to a range of 8-64 GU. Toothbrush abrasion resulted in significant modifications in SR and G amongst the materials tested, attributed to filler sizes. There was statistically significant difference in color (delta E* ranged from 0.38-0.88). Filler size did not affect color stability. Toothbrush abrasion resulted in rougher and matte surfaces for all materials tested. Although the individual differences in surface roughness among filler sizes were not always significant, the correlation showed a trend that larger filler sizes resulted in higher surface roughness after abrasion for the SR parameters Ra and Rt (r = 0.95; r = 0.93, respectively). RSm showed an increase after toothbrush abrasion for all resin composites, however no significant correlation was detected (r = 0.21).There was a significant correlation between G and Ra ratios (r = - 0.95).

  10. Neuro - Fuzzy Analysis for Silicon Carbide Abrasive Grains ...

    African Journals Online (AJOL)

    Grinding wheels are made of very small, sharp and hard abrasive materials or grits held together by strong porous bond. Abrasive materials are materials of extreme hardness that are used to shape other materials by a grinding or abrading action and they are used either as loose grains, as grinding wheels, or as coatings ...

  11. Third abrasive wear mode: is it possible?

    Directory of Open Access Journals (Sweden)

    Ronaldo Câmara Cozza

    2014-04-01

    Full Text Available The objective of this paper is to propose an initial discussion on the characterization of a third abrasive wear mode. The results obtained in a previous work [1] under different test conditions revealed the occurrence of the superposition of the “rolling” and “grooving” abrasive wear modes. This phenomenon was denoted “micro-rolling abrasion” due to the observation that “rolling abrasion” was found to act on “grooving abrasion”.

  12. Abrasive water jet cutting

    International Nuclear Information System (INIS)

    Leist, K.J.; Funnell, G.J.

    1988-01-01

    In the process of selecting a failed equipment cut-up tool for the process facility modifications (PFM) project, a system using an abrasive water jet (AWJ) was developed and tested for remote disassembly of failed equipment. It is presented in this paper

  13. Atmospheric particulate emissions from dry abrasive blasting using coal slag

    Energy Technology Data Exchange (ETDEWEB)

    Bhaskar Kura; Kalpalatha Kambham; Sivaramakrishnan Sangameswaran; Sandhya Potana [University of New Orleans, New Orleans, LA (United States). Department of Civil and Environmental Engineering

    2006-08-15

    Coal slag is one of the widely used abrasives in dry abrasive blasting. Atmospheric emissions from this process include particulate matter (PM) and heavy metals, such as chromium, lead, manganese, nickel. Quantities and characteristics of PM emissions depend on abrasive characteristics and process parameters. Emission factors are key inputs to estimate emissions. Experiments were conducted to study the effect of blast pressure, abrasive feed rate, and initial surface contamination on total PM (TPM) emission factors for coal slag. Rusted and painted mild steel surfaces were used as base plates. Blasting was carried out in an enclosed chamber, and PM was collected from an exhaust duct using U.S. Environment Protection Agency source sampling methods for stationary sources. Results showed that there is significant effect of blast pressure, feed rate, and surface contamination on TPM emissions. Mathematical equations were developed to estimate emission factors in terms of mass of emissions per unit mass of abrasive used, as well as mass of emissions per unit of surface area cleaned. These equations will help industries in estimating PM emissions based on blast pressure and abrasive feed rate. In addition, emissions can be reduced by choosing optimum operating conditions. 40 refs., 5 figs., 2 tabs.

  14. The structure of abrasion-resisting castings made of chromium cast iron

    Directory of Open Access Journals (Sweden)

    D. Kopyciński

    2011-01-01

    Full Text Available In this study presents the analyse of chrome iron cast structure (as-cast condition which are used in rugged conditions abrasion-percussive and high temperature. While producing the casts of chrome iron major influence has been preserve the structure of technologi cal process parameters. The addition to Fe-C-Cr alloy Ni, Mo or Cu and then proper heat treatment leads to the improvement of functional and mechanical cast qualities. Then it is possible to develop high mechanical properties which are recommended by PN-EN12513. As can it be seen from the above research silicon is an adverse chemical element in this kind of alloy cast iron. However, the reason of cracksappearing in chrome iron casts are phosphorus eutectic microareas. When the compound of Si and P reach the critical point, described inPN-88/H-83144 outdated standard, the microareas might appear.

  15. Submerged cutting characteristics of abrasive suspension jet

    International Nuclear Information System (INIS)

    Shimizu, Seiji; Peng, Guoyi; Oguma, Yasuyuki; Nishikata, Hiroyuki

    2015-01-01

    An abrasive suspension jet (ASJ) formed by propelling abrasive suspension through a nozzle has a greater cutting capability than the conventional abrasive water jet. However the cutting capability of submerged ASJs decreases drastically with increasing the standoff distance and the pressure around the jet. A sheathed nozzle with ventilation for ASJs has been developed as a mean of extending the effective stand-off distance and improving the cutting capabilities under submerged condition. In the present investigation, cutting tests by ASJs in air and under submerged condition are conducted with specimens of aluminum alloy. Air coated ASJs are formed by using a sheathed nozzle with ventilation. The relative cutting depth is defined as the cutting depth under submerged condition divided by the cutting depth in air at the same standoff distance. The relative cutting depth is arranged effectually by the cavitation number based on the cavity pressure measured at the sheath. (author)

  16. Analysis of coarse aggregate performance based on the modified Micro Deval abrasion test

    Directory of Open Access Journals (Sweden)

    Jiangfeng Wu

    2018-03-01

    Full Text Available The anti-abrasion property of aggregate significantly affects the performance of the pavement. In this research, the quartzite and gneiss which were produced in Lincheng County, Xingtai City, Hebei Province were selected as test samples. According to the American Society for Testing and Materials standard, the Micro-Deval abrasion test was taken every 1000 rotation times until 20,000 times, and the change trend of the Micro-Deval abrasion value was obtained. Results showed that the abrasion values were in the exponential growth rate rather than linear rate. Their R-Square coefficient was 0.99142 and 0.99916 respectively. The gravel information such as area, roundness, diameter, perimeter and so on were calculated and analyzed by Image-Pro Plus software, which provided a rapid way for the 2D morphology characteristics analysis of the coarse aggregate. Keywords: Micro-Deval abrasion test, Coarse aggregate, Anti-abrasion property, Abrasion values

  17. Nutrição e desenvolvimento Nutrition and development

    Directory of Open Access Journals (Sweden)

    Ilma K. G. de Arruda

    1994-09-01

    Full Text Available As discussões sobre desenvolvimento e nutrição freqüentemente se realizam sob um duplo enfoque: aqueles que consideram o estado nutricional como reflexo do desenvolvimento, e os que admitem que a nutrição influencia fortemente no nível e ritmo desse desenvolvimento. Os autores focalizam o tema visualizando a nutrição como um fator decisivo para um bom desenvolvimento social e econômico, particularizando o fato de que as intervenções nutricionais podem contribuir para melhorias significativas nos resultados escolares, na produtividade do trabalho e na resistência às infecções. Assim, os reflexos da desnutrição na economia seriam evidentes: quer pelas limitações na expectativa de renda, quer pelo aumento dos custos dos compromissos que a população assume para proteger-se, quer pelos avultados custos ocultos de origem social - absenteísmo, acidentes do trabalho e rotatividade de pessoal. Em face dos propósitos de modernização e competitividade da economia, é inquestionável a necessidade da nutrição figurar bem alto na lista de prioridades nacionais. Com isso, promover-se-ia o desenvolvimento dos recursos humanos e a preservação desse capital, que é o ideário de uma economia socialmente responsável.Discussions on development and nutrition frequently have a double focus: one that considers nutritional status as a reflection of development, and another that admits that nutrition strongly influences the level and rhythm of development. The authors view nutrition as a decisive factor for adequate social and economic development, specifying the fact that nutritional interventions might contribute to significant improvements in individual classroom performance, productivity at the workplace, and resistance to infections. The implications of malnutrition for the economy are thus evident: either by limitations in income expectations, increased costs deriving from burdens assumed by the population to protect themselves, or

  18. Abrasive wear of WC-NiMoCrFeCo thermally sprayed coatings in dependence on different types of abrasive sands

    Czech Academy of Sciences Publication Activity Database

    Kašparová, M.; Zahálka, F.; Houdková, Š.; Ctibor, Pavel

    2010-01-01

    Roč. 48, č. 1 (2010), s. 75-85 ISSN 0023-432X R&D Projects: GA AV ČR 1QS200430560 Institutional research plan: CEZ:AV0Z20430508 Keywords : WC-Hastelloy * abrasive wear * Al2O3 sand * SiO2 sand * braun size * abrasive efficiency Subject RIV: JG - Metallurgy Impact factor: 0.471, year: 2010 http://kovmat.sav.sk/abstract.php?rr=48&cc=1&ss=73

  19. Mangrove Cultivation For Dealing With Coastal Abrasion Case Study Of Karangsong

    Science.gov (United States)

    Fatimatuzzahroh, Feti; Hadi, Sudharto P.; Purnaweni, Hartuti

    2018-02-01

    Coastal abrasion is consequence from destructive waves and sea current. One of cause is human intervention. The effort to solve of abrasion is by mangrove cultivation. Mangroves are halophyte plant that can restrain the sea wave. Mangrove cultivation required participation community that give awareness the importance of mangrove in coastal sustainability. Mangroves in coastal Karangsong, Indramayu west java, in 2007 was through abrasion approximately 127.30 ha. Mangrove cultivation in Karangsong has been replanting since 1998 to 2003, but there was no maintenance and management. In 2007 until 2015 Karangsong replanting mangroves and has been succeed. Karangsong became the center of mangrove study for west java area in 2015. This achievement is result of cooperation between community, NGO, and local government. In addition, this effort made not only overcome the abrasion problem but also give community awareness about the importance of mangrove cultivation in preventing coastal abrasion throughout community development. This paper reviews abrasion in Karangsong and the impact for local community and empowerment in mangrove cultivation. To achieve the success mangrove cultivation required community development approach from planning process, planting, maintenance and management.

  20. Experimental Research into Technology of Abrasive Flow Machining Nonlinear Tube Runner

    Directory of Open Access Journals (Sweden)

    Junye Li

    2014-06-01

    Full Text Available In the fields of military and civil uses, some special passages exist in many major parts, such as non-linear tubes. The overall performance is usually decided by the surface quality. Abrasive flow machining (AFM technology can effectively improve the surface quality of the parts. In order to discuss the mechanism and technology of abrasive flow machining nonlinear tube, the nozzle is picked up as the researching object, and the self-designed polishing liquid is employed to make research on the key technological parameters of abrasive flow machining linear tube. Technological parameters’ impact on surface quality of the parts through the nozzle surface topography and scanning electron microscopy (SEM map is explored. It is experimentally confirmed that abrasive flow machining can significantly improve surface quality of nonlinear runner, and experimental results can provide technical reference to optimizing study of abrasive flow machining theory.

  1. The influence of rock strength on erosion processes and river morphology in central Arizona: the accumulation of damage from macro-abrasion

    Science.gov (United States)

    Larimer, J. E.; Yanites, B.

    2017-12-01

    River morphology reflects the interaction between the driving forces of erosion and the resisting properties of bedrock that limit erosion. Changes in energy dissipation at the riverbed are indicated by differences in channel geometry. To erode at the same rate, stronger rocks require more energy, and thus, an adjustment in river slope or width is necessary to accomplish this work. Therefore, morphological changes should reflect differences in the rock strength properties most relevant to the dominant erosion process. We investigate this hypothesis by comparing river morphology and rock-strength properties of reaches subject to different processes. Streams in Prescott National Forest, AZ expose bedrock through a variety of lithologies, which provides a natural testing ground. Measurements include channel geometry, surface P-wave velocity, fracture spacing, and bedload grain size distribution of 150 individual reaches, as well as 260 tensile and compressive-strength tests and P-wave velocity of cores up to depths of 20 cm. Based on observations, we infer that fluvial erosion processes in this region generally fall into three domains: (1) grain by grain abrasion, (2) progressive failure by damage accumulation due to bedload impacts or `macro-abrasion', and (3) `plucking' of jointed rocks. We focus analyses on the accumulation of damage from sub-critical stresses that weakens the surface of the bedrock, potentially leading to macroscopic fractures, fatigue, and rock failure. This plays a dual role facilitating the ease with which abrasion removes material and increasing the rate of production of pluck-able particles. We estimate the `damage potential' of saltating bedload using water discharge time-series, sediment transport models and grain size distribution. To determine the resistance to damage accumulation among different rocks, we measure the evolution of damage in core samples under uniaxial loading using strain energy and inherent flaw theory. Preliminary

  2. The effect of daily fluoride mouth rinsing on enamel erosive/abrasive wear in situ.

    Science.gov (United States)

    Stenhagen, K R; Hove, L H; Holme, B; Tveit, A B

    2013-01-01

    It is not known whether application of fluoride agents on enamel results in lasting resistance to erosive/abrasive wear. We investigated if one daily mouth rinse with sodium fluoride (NaF), stannous fluoride (SnF(2)) or titanium tetrafluoride (TiF(4)) solutions protected enamel against erosive/abrasive wear in situ (a paired, randomised and blind study). Sixteen molars were cut into 4 specimens, each with one amalgam filling (measurement reference surface). Two teeth (2 × 4 specimens) were mounted bilaterally (buccal aspects) on acrylic mandibular appliances and worn for 9 days by 8 volunteers. Every morning, the specimens were brushed manually with water (30 s) extra-orally. Then fluoride solutions (0.4% SnF(2) pH 2.5; 0.15% TiF(4) pH 2.1; 0.2% NaF pH 6.5, all 0.05 M F) were applied (2 min). Three of the specimens from each tooth got different treatment, and the fourth served as control. At midday, the specimens were etched for 2 min in 300 ml fresh 0.01 M hydrochloric acid and rinsed in tap water. This etch procedure was repeated in the afternoon. Topographic measurements were performed by a white-light interferometer. Mean surface loss (±SD) for 16 teeth after 9 days was: SnF(2) 1.8 ± 1.9 µm, TiF(4) 3.1 ± 4.8 µm, NaF 26.3 ± 4.7 µm, control 32.3 ± 4.4 µm. Daily rinse with SnF(2), TiF(4) and NaF resulted in 94, 90 and 18% reduction in enamel erosive/abrasive wear, respectively, compared with control (p < 0.05). The superior protective effect of daily rinse with either stannous or titanium tetrafluoride solutions on erosive/abrasive enamel wear is promising. Copyright © 2012 S. Karger AG, Basel.

  3. A Review on Parametric Analysis of Magnetic Abrasive Machining Process

    Science.gov (United States)

    Khattri, Krishna; Choudhary, Gulshan; Bhuyan, B. K.; Selokar, Ashish

    2018-03-01

    The magnetic abrasive machining (MAM) process is a highly developed unconventional machining process. It is frequently used in manufacturing industries for nanometer range surface finishing of workpiece with the help of Magnetic abrasive particles (MAPs) and magnetic force applied in the machining zone. It is precise and faster than conventional methods and able to produce defect free finished components. This paper provides a comprehensive review on the recent advancement of MAM process carried out by different researcher till date. The effect of different input parameters such as rotational speed of electromagnet, voltage, magnetic flux density, abrasive particles size and working gap on the performances of Material Removal Rate (MRR) and surface roughness (Ra) have been discussed. On the basis of review, it is observed that the rotational speed of electromagnet, voltage and mesh size of abrasive particles have significant impact on MAM process.

  4. Decontamination of Steam Generator tube using Abrasive Blasting Technology

    International Nuclear Information System (INIS)

    Min, B. Y.; Kim, G. N.; Choi, W. K.; Lee, K. W.; Kim, D. H.; Kim, K. H.; Kim, B. T.

    2010-01-01

    As a part of a technology development of volume reduction and self disposal for large metal waste project, We at KAERI and our Sunkwang Atomic Energy Safety (KAES) subcontractor colleagues are demonstrating radioactively contaminated steam generator tube by abrasive blasting technology at Kori-1 NPP. A steam generator is a crucial component in a PWR (pressurized Water Reactor). It is the crossing between the primary, contaminated, circuit and the secondary waste-steam circuit. The heat from the primary reactor coolant loop is transferred to the secondary side in thousands of small tubes. Due to several problems in the material of those tube, like SCC (Stress Corrosion Cracking), insufficient control in water chemistry, which can be cause of tube leakage, more and more steam generators are replaced today. Only in Korea, already 2 of them are replaced and will be replaced in the near future. The retired 300 ton heavy Steam generator was stored at the storage waste building of Kori NPP site. The steam generator waste has a large volume, so that it is necessary to reduce its volume by decontamination. A waste reduction effect can be obtained through decontamination of the inner surface of a steam generator. Therefore, it is necessary to develop an optimum method for decontamination of the inner surface of bundle tubes. The dry abrasive blasting is a very interesting technology for the realization of three-dimensional microstructures in brittle materials like glass or silicon. Dry abrasive blasting is applicable to most surface materials except those that might be shattered by the abrasive. It is most effective on flat surface and because the abrasive is sprayed and can also applicable on 'hard to reach' areas such as inner tube ceilings or behind equipment. Abrasive decontamination techniques have been applied in several countries, including Belgium, the CIS, France, Germany, Japan, the UK and the USA

  5. Innovative decontamination technology by abrasion in vibratory vessels

    International Nuclear Information System (INIS)

    Fabbri, Silvio; Ilarri, Sergio

    2007-01-01

    Available in abstract form only. Full text of publication follows: The possibility of using conventional vibratory vessel technology as a decontamination technique is the motivation for the development of this project. The objective is to explore the feasibility of applying the vibratory vessel technology for decontamination of radioactively-contaminated materials such as pipes and metal structures. The research and development of this technology was granted by the U.S. Department of Energy (DOE). Abrasion processes in vibratory vessels are widely used in the manufacture of metals, ceramics, and plastics. Samples to be treated, solid abrasive media and liquid media are set up into a vessel. Erosion results from the repeated impact of the abrasive particles on the surface of the body being treated. A liquid media, generally detergents or surfactants aid the abrasive action. The amount of material removed increases with the time of treatment. The design and construction of the machine were provided by Vibro, Argentina private company. Tests with radioactively-contaminated aluminum tubes and a stainless steel bar, were performed at laboratory level. Tests showed that it is possible to clean both the external and the internal surface of contaminated tubes. Results show a decontamination factor around 10 after the first 30 minutes of the cleaning time. (authors)

  6. Abrasive wear of enamel by bioactive glass-based toothpastes.

    Science.gov (United States)

    Mahmood, Asad; Mneimne, Mohammed; Zou, Li Fong; Hill, Robert G; Gillam, David G

    2014-10-01

    To determine the abrasivity of a 45S5 bioactive glass based toothpaste on enamel as a function of the particle size and shape of the glass. 45S5 glass was synthesized ground and sieved to give various particle sized fractions toothpastes and their tooth brush abrasivity measured according to BS EN ISO11609 methodology. Enamel loss increased with increasing particle size. The percussion milled powder exhibited particles that had sharp edges and the pastes were significantly more abrasive than the pastes made with round ball milled powders. One interesting observation made during the present study was that there was preferential wear of the enamel at the dentin-enamel junction (DEJ), particularly with the coarse particle sized pastes.

  7. An experimental modeling and acoustic emission monitoring of abrasive wear in a steel/diabase pair

    Science.gov (United States)

    Korchuganov, M. A.; Filippov, A. V.; Tarasov, S. Yu.; Podgornyh, O. A.; Shamarin, N. N.; Filippova, E. O.

    2016-11-01

    The earthmoving of permafrost soil is a critical task for excavation of minerals and construction on new territories. Failure by abrasive wear is the main reason for excavation parts of earthmoving and soil cutting machines. Therefore investigation of this type of wear is a challenge for developing efficient and wear resistant working parts. This paper is focused on conducting tribological experiments with sliding the steel samples over the surface of diabase stone sample where abrasive wear conditions of soil cutting are modeled experimentally. The worn surfaces of all samples have been examined and transfer of metal and stone particles revealed. The acoustic emission (AE) signals have been recorded and related to the results of worn surface analysis. he acoustic emission (AE) signals have been recorded and related to the results of worn surface analysis. As shown the wear intensity correlates to that of acoustic emission. Both acoustic emission signal median frequency and energy are found to be sensitive to the wear mode.

  8. Comparative evaluation of enamel abrasivity of different commercially available dentifrices – An In vitro Study

    Directory of Open Access Journals (Sweden)

    Rupali Athawale

    2018-01-01

    Full Text Available Background: Toothbrushing with toothpaste is a major contributor to dental abrasion. A number of factors such as abrasivity and concentration of the toothpaste, brushing frequency, brushing duration, force of brushing, and toothbrush bristle stiffness have a potential impact on the abrasion process of dental hard tissue. However, the abrasivity of the toothpaste is the most important parameter that affects the abrasion process of dental hard tissue. Aims: This study aims to evaluate the maximum and mean enamel abrasivity of commercially available dentifrices such as Colgate total®, Pepsodent whitening®, Vicco vajradanti®, Dabur red® in primary and permanent teeth. Materials and Methods: Human extracted 60 primary and 60 permanent teeth were randomly selected based on the inclusion criteria. Teeth were sectioned at cementoenamel junction using diamond disc and mounted in an acrylic resin blocks. Baseline profilometric measurements were recorded for all the samples. Four commonly used dentifrices were selected and labeled as Group A (Colgate Total®, B (Pepsodent Whitening®, C (Vicco Vajradanti®, and D (Dabur Red®. Toothpaste slurry was prepared. Tooth specimens were brushed in vitro using a customized brushing machine. After toothbrushing, profilometric measurements were obtained, and the differences in readings served as proxy measure to assess surface abrasion. Data were collected and analyzed using student t-test and ANOVA test. Student t-test was used to compare the enamel abrasivity prebrushing and postbrushing, and ANOVA was used to compare the enamel abrasivity among the four different commercially available toothpastes. Results: In permanent teeth, all the toothpastes were found to cause significant enamel abrasion (P = 0.000 and a significant variation was observed when maximum (P = 0.008 and mean (P = 0.036 enamel abrasivity of these toothpastes were compared. In primary teeth also, all the toothpastes caused significant abrasion

  9. Pleurectomy versus pleural abrasion for primary spontaneous pneumothorax in children.

    Science.gov (United States)

    Joharifard, Shahrzad; Coakley, Brian A; Butterworth, Sonia A

    2017-05-01

    Primary spontaneous pneumothorax (PSP) represents a common indication for urgent surgical intervention in children. First episodes are often managed with thoracostomy tube, whereas recurrent episodes typically prompt surgery involving apical bleb resection and pleurodesis, either via pleurectomy or pleural abrasion. The purpose of this study was to assess whether pleurectomy or pleural abrasion was associated with lower postoperative recurrence. The records of patients undergoing surgery for PSP between February 2005 and December 2015 were retrospectively reviewed. Recurrence was defined as an ipsilateral pneumothorax requiring surgical intervention. Bivariate logistic regressions were used to identify factors associated with recurrence. Fifty-two patients underwent 64 index operations for PSP (12 patients had surgery for contralateral pneumothorax, and each instance was analyzed separately). The mean age was 15.7±1.2years, and 79.7% (n=51) of patients were male. In addition to apical wedge resection, 53.1% (n=34) of patients underwent pleurectomy, 39.1% (n=25) underwent pleural abrasion, and 7.8% (n=5) had no pleural treatment. The overall recurrence rate was 23.4% (n=15). Recurrence was significantly lower in patients who underwent pleurectomy rather than pleural abrasion (8.8% vs. 40%, p<0.01). In patients who underwent pleural abrasion without pleurectomy, the relative risk of recurrence was 2.36 [1.41-3.92, p<0.01]. Recurrence of PSP is significantly reduced in patients undergoing pleurectomy compared to pleural abrasion. Level III, retrospective comparative therapeutic study. Copyright © 2017 Elsevier Inc. All rights reserved.

  10. Projectile Nose Mass Abrasion of High-Speed Penetration into Concrete

    Directory of Open Access Journals (Sweden)

    Haijun Wu

    2012-01-01

    Full Text Available Based on the dynamic spherical cavity expansion theory of concrete and the analysis of experimental data, a mass abrasion model of projectile considering the hardness of aggregates, the relative strength of target and projectile, and the initial impact velocity is constructed in this paper. Furthermore, the effect of mass abrasion on the penetration depth of projectile and the influence of hardness of aggregates and strength of projectile on penetration depth and mass loss are also analyzed. The results show that, for the ogive-nose projectile with the CRH of 3 and aspect ratio of 7 penetrating the concrete of 35 MPa, the “rigid-body penetration” model is available when the initial impact velocity is lower than 800 m/s. However, when the initial impact velocity is higher than 800 m/s, the “deforming/eroding body penetration” model should be adopted. Through theoretical analysis and numerical calculation, the results indicate that the initial impact velocity is the most important factor of mass abrasion. The hardness of aggregates and the strength of projectile are also significant factors. But relatively speaking, the sensitivity of strength of projectile to mass abrasion is higher, which indicates that the effect of projectile material on mass abrasion is more dramatic than the hardness of aggregates.

  11. Surface characterization of current composites after toothbrush abrasion.

    Science.gov (United States)

    Takahashi, Rena; Jin, Jian; Nikaido, Toru; Tagami, Junji; Hickel, Reinhard; Kunzelmann, Karl-Heinz

    2013-01-01

    The present study was designed to evaluate the surface roughness and the gloss of current composites before and after toothbrush abrasion. We assessed forty dimensionally standardized composite specimens (n=8/group) from five composites: two nanohybrids (i. e., IPS Empress Direct Enamel and IPS Empress Direct Dentin), two microhybrids (i. e., Clearfil AP-X and Filtek Z250) and one organically modified ceramics (Admira). All of the specimens were polished with 4000-grid silicon carbide papers. Surface roughness was measured with a profilometer and gloss was measured with a glossmeter before and after powered toothbrush abrasion with a 1:1 slurry (dentifrice/tap water) at 12,000 strokes in a toothbrush simulator. There was a significant increase in the surface roughness and a reduction in gloss after toothbrush abrasion in all of the composites except Clearfil AP-X (pgloss (R(2)=0.191, p<0.001).

  12. Baking soda as an abrasive in toothpastes: Mechanism of action and safety and effectiveness considerations.

    Science.gov (United States)

    Hara, Anderson T; Turssi, Cecilia P

    2017-11-01

    Toothpastes can be formulated with different abrasive systems, depending on their intended clinical application. This formulation potentially affects their effectiveness and safety and, therefore, requires proper understanding. In this article, the authors focused on abrasive aspects of toothpastes containing sodium bicarbonate (baking soda), which have gained considerable attention because of their low abrasivity and good compatibility, while providing clinical effectiveness (further detailed in the other articles of this special issue). The authors first appraised the role of toothpaste abrasivity on tooth wear, exploring some underlying processes and the existing methods to determine toothpaste abrasivity. The authors reviewed the available data on the abrasivity of toothpastes containing baking soda and reported a summary of findings highlighting the clinical implications. On the basis of the collected evidence, baking soda has an intrinsic low-abrasive nature because of its comparatively lower hardness in relation to enamel and dentin. Baking soda toothpastes also may contain other ingredients, which can increase their stain removal effectiveness and, consequently, abrasivity. Even those formulations have abrasivity well within the safety limit regulatory agencies have established and, therefore, can be considered safe. Copyright © 2017 American Dental Association. Published by Elsevier Inc. All rights reserved.

  13. Abrasive Wear of Four Direct Restorative Materials by Standard and Whitening Dentifrices

    Science.gov (United States)

    2013-06-01

    Weader, E., Liscombe, C., & Holt, J.S. (2005). The measurement of enamel and dentine abrasion by tooth - whitening products using an in situ model...ABRASION OF TOOTH STRUCTURE Hard tissue abrasion is a familiar consequence of toothbrushing. Enamel , dentin, and cementum differ in their...LESIONS Cervical enamel wear is common; however, relatively few epidemiologic studies have distinguished between cervical enamel wear and tooth wear in

  14. Demonstration experience with an abrasive blasting technique for decontaminating concrete pads

    International Nuclear Information System (INIS)

    Devgun, J.S.; Land, R.R.; Doane, R.W.

    1990-01-01

    A demonstration was performed for decontaminating a radioactivity contaminated concrete pad with a portable abrasive blasting system. The system utilizes a rotating blast wheel that scours the concrete surface with metal abrasive. The metal abrasive, pulverized concrete dust, and contaminants rebound into a separator chamber. The reusable metal abrasive is recycled, and the pulverized media are removed to an integral dust collection system. The exhaust is HEPA filtered to minimize release of airborne contaminants. However, the technique had limited success in reducing contamination around the cracks and seams in the concrete where the higher activity levels of contamination were detected during the radiological survey before the cleanup. The technique can be successful and cost-effective in decontaminating large areas of low contamination; however, careful characterization and planning are necessary. 3 refs., 3 figs., 1 tabs

  15. Abrasion behavior of graphite pebble in lifting pipe of pebble-bed HTR

    Energy Technology Data Exchange (ETDEWEB)

    Shen, Ke; Su, Jiageng [Institute of Nuclear and New Energy Technology, Advanced Nuclear Energy Technology Cooperation Innovation Center, The Key Laboratory of Advanced Nuclear Engineering and Safety, Ministry of Education, Beijing 10084 (China); Zhou, Hongbo [Institute of Nuclear and New Energy Technology, Advanced Nuclear Energy Technology Cooperation Innovation Center, The Key Laboratory of Advanced Nuclear Engineering and Safety, Ministry of Education, Beijing 10084 (China); Chinergy Co., LTD., Beijing 100193 (China); Peng, Wei; Liu, Bing [Institute of Nuclear and New Energy Technology, Advanced Nuclear Energy Technology Cooperation Innovation Center, The Key Laboratory of Advanced Nuclear Engineering and Safety, Ministry of Education, Beijing 10084 (China); Yu, Suyun, E-mail: suyuan@tsinghua.edu.cn [Center for Combustion Energy, The Key Laboratory for Thermal Science and Power Engineering, Ministry of Educations, Tsinghua University, Beijing 10084 (China)

    2015-11-15

    Highlights: • Quantitative determination of abrasion rate of graphite pebbles in different lifting velocities. • Abrasion behavior of graphite pebble in helium, air and nitrogen. • In helium, intensive collisions caused by oscillatory motion result in more graphite dust production. - Abstract: A pebble-bed high-temperature gas-cooled reactor (pebble-bed HTR) uses a helium coolant, graphite core structure, and spherical fuel elements. The pebble-bed design enables on-line refueling, avoiding refueling shutdowns. During circulation process, the pebbles are lifted pneumatically via a stainless steel lifting pipe and reinserted into the reactor. Inevitably, the movement of the fuel elements as they recirculate in the reactor produces graphite dust. Mechanical wear is the primary source of graphite dust production. Specifically, the sources are mechanisms of pebble–pebble contact, pebble–wall (structural graphite) contact, and fuel handling (pebble–metal abrasion). The key contribution to graphite dust production is from the fuel handling system, particularly from the lifting pipe. During pneumatic lift, graphite pebbles undergo multiple collisions with the stainless steel lifting pipe, thereby causing abrasion of the graphite pebbles and producing graphite dust. The present work explored the abrasion behavior of graphite pebble in the lifting pipe by measuring the abrasion rate at different lifting velocities. The abrasion rate of the graphite pebble in helium was found much higher than those in air and nitrogen. This gas environment effect could be explained by either tribology behavior or dynamic behavior. Friction testing excluded the possibility of tribology reason. The dynamic behavior of the graphite pebble was captured by analysis of the audio waveforms during pneumatic lift. The analysis results revealed unique dynamic behavior of the graphite pebble in helium. Oscillation and consequently intensive collisions occur during pneumatic lift, causing

  16. Lung scintigraphy evaluation in workers exposed to abrasive dusts

    International Nuclear Information System (INIS)

    Terra Filho, Mario

    1995-01-01

    The production process of abrasives use aluminium, or silicon carbide a synthetic material with a hardness only slightly less than that of a diamond. It is popularly known as carborundum since it was first manufactured as an abrasive in 1891, produced by the fusion of high grade silica and petroleum coke with sawdust. For many years silicon carbide was thought not to give rise to pulmonary lesions. Recently several researchers suggested the existence of a carborundum pneumoconiosis. The aim of this study was to evaluate the role of the pulmonary clearance of 99m Technetium chelated to diethylene-triamine penta-acetate ( 99m Tc DTPA), and 67 Gallium lung scanning in workers exposed to abrasive dusts. Thirty seven subjects, 13 smokers and 24 nonsmokers and ex smokers were studied. In 32 (86,48%) 67 Gallium lung scanning was positive including 13 (40,62%) retired workers. We conclude that non smoking workers of abrasives plants have a pulmonary alveolar epithelial permeability disturbance similar as observed in smoking workers and smoking controls. Most workers, ex-workers of these industries and in patients with carborundum pneumoconiosis there is an evidence of pulmonary inflammation measured with abnormal 67 Gallium lung scan. (author)

  17. Measurement of nanoparticle removal by abrasion

    International Nuclear Information System (INIS)

    Guiot, Arnaud; Golanski, Luana; Tardif, Francois

    2009-01-01

    A strong release limitation of single nanoparticles from commercial manufactured 'nanoproducts' is necessary to decrease potential exposure risks of consumers and represents also a pragmatic way to facilitate acceptance for nanomaterial commercialization before obtaining definitive toxicological results. So, it is of prime importance to know how to characterize the release of small materials during usage solicitations such as mechanical, thermal, UV stress: are they single nanoparticles, aggregates or nanoparticles included in a bigger piece of the matrix? In the frame of NanoSafe2 project, CEA developed and qualified a specific bench test where the material to be tested is mechanically solicited by abrasion using a normalized Taber equipment. The first results show that nanofillers can be released in usage by abrasion for non optimised nanoproducts.

  18. Numerical analysis of special-shaped surface in abrasive flow machining

    Science.gov (United States)

    Li, Junye; Zhou, Zengwei; Wu, Guiling; Lu, Hui; Sun, Zhihuai

    2018-03-01

    Solid-liquid two-phase abrasive flow machining is a method to effectively polish the surface of Special-shaped surface parts. Based on the processing characteristics of the abrasive flow machining. The standard model and the pressure-coupled SIMPLEC algorithm are used. The shear force and velocity of the near-wall surface of the runner of the solid-liquid two-phase abrasive machining with different inlet pressure are analyzed. The numerical simulation results show that the inlet pressure has little effect on the velocity, and the shear force has a linear relationship with the inlet pressure. To obtain a better polishing effect, the outlet pressure can be appropriately increased.

  19. Influence of Corrosion on the Abrasion of Cutter Steels Used in TBM Tunnelling

    Science.gov (United States)

    Espallargas, N.; Jakobsen, P. D.; Langmaack, L.; Macias, F. J.

    2015-01-01

    Abrasion on tunnel boring machine (TBM) cutters may be critical in terms of project duration and costs. Several researchers are currently studying the degradation of TBM cutter tools used for excavating hard rock, soft ground and loose soil. So far, the primary focus of this research has been directed towards abrasive wear. Abrasive wear is a very common process in TBM excavation, but with a view to the environment in which the tools are working, corrosion may also exert an influence. This paper presents a selection of techniques that can be used to evaluate the influence of corrosion on abrasion on TBM excavation tools. It also presents the influence of corrosion on abrasive wear for some initial tests, with constant steel and geomaterial and varying properties of the excavation fluids (soil conditioners, anti-abrasion additives and water). The results indicate that the chloride content in the water media greatly influences the amount of wear, providing evidence of the influence of corrosion on the abrasion of the cutting tools. The presence of conditioning additives tailored to specific rock or soil conditions reduces wear. However, when chloride is present in the water, the additives minimise wear rates but fail to suppress corrosion of the cutting tools.

  20. Shoe heel abrasion and its possible biomechanical cause: a transversal study with infantry recruits.

    Science.gov (United States)

    Baumfeld, Daniel; Raduan, Fernando C; Macedo, Benjamim; Silva, Thiago Alexandre Alves; Baumfeld, Tiago; Favato, Danilo Fabrino; de Andrade, Marco Antonio Percope; Nery, Caio

    2015-11-19

    Excessive shoe heel abrasion is of concern to patients and shoe manufacturers, but little scientific information is available about this feature and its possible causes. The purpose of this study was to relate this phenomenon with biomechanical factors that could predispose to shoe heel abrasion. Ninety-seven recruits (median age 25) were enrolled in this study. Shoe abrasion was assessed manually with a metric plastic tape on the posterior part of the heel that comes in contact with the ground. The number of sprains, foot alignment, and calf muscle shortening (Silfverskiold test) was also assessed in order to relate it with shoe heel abrasion. After using our exclusion criteria, 86 recruits and 172 were considered for this study. The most common abrasion site was the lateral portion of the heel surface (50 %). Forty-four percent of the participants had neutral hind-foot alignment and 39 % had valgus alignment. Twenty-six (30 %) patients have had previous ankle or foot sprains. Neutral foot was related with less calf muscle shortening. On the other hand, valgus hind-foot alignment was more associated with Achilles shortening (p study was able to correlate shoe heel abrasion with biomechanical causes (neutral alignment-uniform abrasion/varus alignment-central and lateral abrasion). More effort has to be done to continue evaluating outsole abrasion with its possible biomechanical cause in order to predict and treat possible associated injuries.

  1. Submerged cutting of steel by abrasive water jets

    International Nuclear Information System (INIS)

    Haferkamp, H.; Louis, H.; Meier, G.

    1990-01-01

    A special cutting head for underwater use was designed and built. Tests were carried out to find out useful parameters for submerged cutting. With regard to the production of secondary waste the abrasive flow rate had to be minimized. This was achieved by using a small water jet nozzle (up to 0.4 mm diameter) and a high pressure (up to 4000 bar) with an optimal abrasive flow rate of about 5 g/s. In the case of a higher ambient pressure a decrease of the cutting performance was measured. But this decrease is not important regarding decommissioning because the ambient pressure is less than 2 bar. An air mantle nozzle was adapted to the cutting head to improve the working distance under water. The air mantle surrounding the abrasive jet lowers the friction between jet and surrounding water and increases the cutting efficiency in the case of greater working distances. (author)

  2. Technology of magnetic abrasive finishing in machining of difficult-to-machine alloy complex surface

    Directory of Open Access Journals (Sweden)

    Fujian MA

    2016-10-01

    Full Text Available The technology of magnetic abrasive finishing is one of the important finishing technologies. Combining with low-frequency vibration and ultrasonic vibration, it can attain higher precision, quality and efficiency. The characteristics and the related current research of magnetic abrasive finishing, vibration assisted magnetic abrasive finishing and ultrasonic assisted magnetic abrasive finishing are introduced. According to the characteristics of the difficult-to-machine alloy's complex surface, the important problems for further study are presented to realize the finishing of complex surface with the technology of magnetic abrasive finishing, such as increasing the machining efficiency by enhancing the magnetic flux density of machining gap and compounding of magnetic energy and others, establishing of the control function during machining and the process planning method for magnetic abrasive finishing of complex surface under the space geometry restraint of complex surface on magnetic pole, etc.

  3. Study of Effect of Impacting Direction on Abrasive Nanometric Cutting Process with Molecular Dynamics.

    Science.gov (United States)

    Li, Junye; Meng, Wenqing; Dong, Kun; Zhang, Xinming; Zhao, Weihong

    2018-01-11

    Abrasive flow polishing plays an important part in modern ultra-precision machining. Ultrafine particles suspended in the medium of abrasive flow removes the material in nanoscale. In this paper, three-dimensional molecular dynamics (MD) simulations are performed to investigate the effect of impacting direction on abrasive cutting process during abrasive flow polishing. The molecular dynamics simulation software Lammps was used to simulate the cutting of single crystal copper with SiC abrasive grains at different cutting angles (0 o -45 o ). At a constant friction coefficient, we found a direct relation between cutting angle and cutting force, which ultimately increases the number of dislocation during abrasive flow machining. Our theoretical study reveal that a small cutting angle is beneficial for improving surface quality and reducing internal defects in the workpiece. However, there is no obvious relationship between cutting angle and friction coefficient.

  4. Wear resistance of cast iron

    Directory of Open Access Journals (Sweden)

    S. Pietrowski

    2008-10-01

    Full Text Available In this paper investigations of abrasive and adhesive wear resistance of different cast iron grades have been presented. Examinations showed, that the most advantageous pair of materials is the cast iron – the hardened steel with low-tempered martensite. It was found, that martensitic nodular cast iron with carbides is the most resistant material.

  5. Experimental Investigation on the Material Removal of the Ultrasonic Vibration Assisted Abrasive Water Jet Machining Ceramics

    Directory of Open Access Journals (Sweden)

    Tao Wang

    2017-01-01

    Full Text Available The ultrasonic vibration activated in the abrasive water jet nozzle is used to enhance the capability of the abrasive water jet machinery. The experiment devices of the ultrasonic vibration assisted abrasive water jet are established; they are composed of the ultrasonic vibration producing device, the abrasive supplying device, the abrasive water jet nozzle, the water jet intensifier pump, and so on. And the effect of process parameters such as the vibration amplitude, the system working pressure, the stand-off, and the abrasive diameter on the ceramics material removal is studied. The experimental result indicates that the depth and the volume removal are increased when the ultrasonic vibration is added on abrasive water jet. With the increase of vibration amplitude, the depth and the volume of material removal are also increased. The other parameters of the ultrasonic vibration assisted abrasive water jet also have an important role in the improvement of ceramic material erosion efficiency.

  6. Incidence of lameness and abrasions in piglets in identical farrowing pens with four different types of floor

    Directory of Open Access Journals (Sweden)

    Nilsson Ebba

    2009-05-01

    Full Text Available Abstract Background Lameness in piglets is a major animal welfare issue. Floor abrasiveness is a common cause of superficial injury in piglets in farrowing pens. The abrasion achieved may act as a gate for infections, which in turn may induce development of infectious arthritis. In this study, the influence of improvements of the floor quality and of increased ratios of straw in identical farrowing pens was measured. Methods The study was carried out at a herd with four identical farrowing units with solid concrete floor bedded with 1 kg chopped straw per sow and 1 hg per piglet and day. Nothing was changed in the management of the four identical farrowing units, but four experimental groups were created: Group I – control, Group II – the amount of bedding was doubled. The surface of the floor was repaired in two units, Group III – Piglet Floor®, Flowcrete Sweden AB, Perstorp, Sweden and Group IV – Thorocrete SL®, Växa Halland, Sweden. Three farrowing batches were studies in each unit. In total, 93 litters (1,073 piglets were examined for foot and skin lesions until the age of 3 weeks. The occurrence of lameness was registered until weaning at an average age of 4.5 weeks. Twenty seven lame piglets were culled instead of medicinally treated and subjected to necropsy including histopathological and microbiological examinations. Isolates of streptococci, staphylococci and E. coli were tested with respect to antimicrobial resistance. Results Piglet born on the repaired floors had the lowest prevalences of abrasions at carpus. Also the doubled straw ration decreased the abrasions. Skin lesions at carpus decreased significantly in magnitude in all four systems from day 10. At day 3, the sole bruising scores of the control unit were greater than the other three units (p Streptococcus dysgalactiae subsp. equisimilis (60%, Staphylococcus hyicus subsp. hyicus (35% and Escherichia coli (5%. These isolates were sensitive to all antibiotics

  7. To Evaluate Effect of Airborne Particle Abrasion using Different Abrasives Particles and Compare Two Commercial Available Zirconia on Flexural Strength on Heat Treatment

    Science.gov (United States)

    Prasad, Hari A.; Pasha, Naveed; Hilal, Mohammed; Amarnath, G. S.; Kundapur, Vinaya; Anand, M; Singh, Sumeet

    2017-01-01

    Background and objective: The popularity of ceramic restorations can be attributed to its life-like appearance, durability and biocompatibility and therefore ceramic restorations have been widely used for anterior and posterior teeth. Ceramic restorations have esthetic and biocompatible advantages but low fracture resistance. Since it has high flexural strength and fracture resistance, yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) is the dental material most commonly used for the core of ceramic crowns and fixed dental prosthesis. In spite of improved mechanical properties, acceptable marginal adaptation and biocompatibility the whitish opacity of zirconia is an obvious esthetic disadvantage. The zirconia framework is often veneered with conventional feldspathic porcelain to achieve a natural appearance. However it is difficult to achieve sufficient bond strength between zirconia and the veneering material. Achieving sufficient bond strength between the veneering ceramic and the zirconia core is a major challenge in the long term clinical success of veneered zirconia restorations. The main objective of this study is to evaluate the effect of different surface treatments on the fracture strength of the two commercially available Zirconia namely Ceramill and ZR-White (AMANNGIRRBACH and UPCERA) respectively. Method: Two commercially available pre-sinteredyttrium stabilized Zirconia blanks (ZR-White and Ceramill) from AMANNGIRRBACH and UPCERA respectively are used to produce the disc shaped specimens of size (15.2 ± 0.03 mm in diameter and 1.2 ± 0.03 mm thick) from each Zirconia blank. All disc shaped specimens are heated at 1200°C in a furnace for 2 hours to form homogenous tetragonal ZrO2. The dimensions of the specimens are measured with a digital caliper (aerospace). The thickness and diameter of each specimen are calculated as the means of 3 measurements made at random sites. 80 discs from each Zirconia blank are divided into ten groups of 8

  8. Quantitative characterization of agglomerate abrasion in a tumbling blender by using the Stokes number approach.

    Science.gov (United States)

    Willemsz, Tofan A; Nguyen, Tien Thanh; Hooijmaijers, Ricardo; Frijlink, Henderik W; Vromans, Herman; van der Voort Maarschalk, Kees

    2013-03-01

    Removal of microcrystalline cellulose agglomerates in a dry-mixing system (lactose, 100 M) predominantly occurs via abrasion. The agglomerate abrasion rate potential is estimated by the Stokes abrasion (StAbr) number of the system. The StAbr number equals the ratio between the kinetic energy density of the moving powder bed and the work of fracture of the agglomerate. Basically, the StAbr number concept describes the blending condition of the dry-mixing system. The concept has been applied to investigate the relevance of process parameters on agglomerate abrasion in tumbling blenders. Here, process parameters such as blender rotational speed and relative fill volumes were investigated. In this study, the StAbr approach revealed a transition point between abrasion rate behaviors. Below this transition point, a blending condition exists where agglomerate abrasion is dominated by the kinetic energy density of the powder blend. Above this transition point, a blending condition exists where agglomerates show (undesirable) slow abrasion rates. In this situation, the blending condition is mainly determined by the high fill volume of the filler.

  9. Impact Capacity Reduction in Railway Prestressed Concrete Sleepers with Surface Abrasions

    Science.gov (United States)

    Ngamkhanong, Chayut; Li, Dan; Kaewunruen, Sakdirat

    2017-10-01

    Railway sleepers (also called ‘railroad tie’ in North America) embedded in ballasted railway tracks are a main part of railway track structures. Its important role is to transfer the loads evenly from the rails to a wider area of ballast bed and to secure rail gauge and enable safe passages of rolling stocks. By nature, railway infrastructure is nonlinear, evidenced by its behaviours, geometry and alignment, wheel-rail contact and operational parameters such as tractive efforts. Based on our critical review, the dynamic behaviour of railway sleepers has not been fully investigated, especially when the sleepers are deteriorated by excessive wears. In fact, the ballast angularity causes differential abrasions on the soffit or bottom surface of sleepers (especially at railseat zone). Furthermore, in sharp curves and rapid gradient change, longitudinal and lateral dynamics of rails increase the likelihood of railseat abrasions in concrete sleepers due to the unbalanced loading conditions. This paper presents a structural capacity of concrete sleepers under dynamic transient loading. The modified compression field theory for ultimate strength design of concrete sleepers under impact loading will be highlighted in this study. The influences of surface abrasions, including surface abrasion and soffit abrasion, on the dynamic behaviour of prestressed concrete sleepers, are firstly highlighted. The outcome of this study will improve the rail maintenance and inspection criteria in order to establish appropriate and sensible remote track condition monitoring network in practice. Moreover, this study will also improve the understanding of the fundamental dynamic behaviour of prestressed concrete sleepers with surface abrasions. The insight into these behaviours will not only improve safety and reliability of railway infrastructure but will enhance the structural safety of other concrete structures.

  10. Refractory, Abrasive and Other Industrial Mineral Operations

    Data.gov (United States)

    Department of Homeland Security — This map layer includes refractory, abrasive, and other industrial minerals operations in the United States. The data represent commodities covered by the Minerals...

  11. Neural network approximation of tip-abrasion effects in AFM imaging

    International Nuclear Information System (INIS)

    Bakucz, Peter; Dziomba, Thorsten; Koenders, Ludger; Krüger-Sehm, Rolf; Yacoot, Andrew

    2008-01-01

    The abrasion (wear) of tips used in scanning force microscopy (SFM) directly influences SFM image quality and is therefore of great relevance to quantitative SFM measurements. The increasing implementation of automated SFM measurement schemes has become a strong driving force for increasing efforts towards the prediction of tip wear, as it needs to be ensured that the probe is exchanged before a level of tip wear is reached that adversely affects the measurement quality. In this paper, we describe the identification of tip abrasion in a system of SFM measurements. We attempt to model the tip-abrasion process as a concatenation of a mapping from the measured AFM data to a regression vector and a nonlinear mapping from the regressor space to the output space. The mapping is formed as a basis function expansion. Feedforward neural networks are used to approximate this mapping. The one-hidden layer network gave a good quality of fit for the training and test sets for the tip-abrasion system. We illustrate our method with AFM measurements of both fine periodic structures and randomly oriented sharp features and compare our neural network results with those obtained using other methods

  12. Neural network approximation of tip-abrasion effects in AFM imaging

    Science.gov (United States)

    Bakucz, Peter; Yacoot, Andrew; Dziomba, Thorsten; Koenders, Ludger; Krüger-Sehm, Rolf

    2008-06-01

    The abrasion (wear) of tips used in scanning force microscopy (SFM) directly influences SFM image quality and is therefore of great relevance to quantitative SFM measurements. The increasing implementation of automated SFM measurement schemes has become a strong driving force for increasing efforts towards the prediction of tip wear, as it needs to be ensured that the probe is exchanged before a level of tip wear is reached that adversely affects the measurement quality. In this paper, we describe the identification of tip abrasion in a system of SFM measurements. We attempt to model the tip-abrasion process as a concatenation of a mapping from the measured AFM data to a regression vector and a nonlinear mapping from the regressor space to the output space. The mapping is formed as a basis function expansion. Feedforward neural networks are used to approximate this mapping. The one-hidden layer network gave a good quality of fit for the training and test sets for the tip-abrasion system. We illustrate our method with AFM measurements of both fine periodic structures and randomly oriented sharp features and compare our neural network results with those obtained using other methods.

  13. Feasibility Study on Cutting HTPB Propellants with Abrasive Water Jet

    Science.gov (United States)

    Jiang, Dayong; Bai, Yun

    2018-01-01

    Abrasive water jet is used to carry out the experiment research on cutting HTPB propellants with three components, which will provide technical support for the engineering treatment of waste rocket motor. Based on the reliability theory and related scientific research results, the safety and efficiency of cutting sensitive HTPB propellants by abrasive water jet were experimentally studied. The results show that the safety reliability is not less than 99.52% at 90% confidence level, so the safety is adequately ensured. The cooling and anti-friction effect of high-speed water jet is the decisive factor to suppress the detonation of HTPB propellant. Compared with pure water jet, cutting efficiency was increased by 5% - 87%. The study shows that abrasive water jets meet the practical use for cutting HTPB propellants.

  14. Quantitative characterization of agglomerate abrasion in a tumbling blender by using the Stokes number approach

    NARCIS (Netherlands)

    Willemsz, Tofan A.; Nguyen, Tien Thanh; Hooijmaijers, Ricardo; Frijlink, Henderik W.; Vromans, Herman; van der Voort Maarschalk, Kees

    2013-01-01

    Removal of microcrystalline cellulose agglomerates in a dry-mixing system (lactose, 100 M) predominantly occurs via abrasion. The agglomerate abrasion rate potential is estimated by the Stokes abrasion (StAbr) number of the system. The StAbrnumber equals the ratio between the kinetic energy density

  15. A teoria do “desenvolvimento fragmentador”

    Directory of Open Access Journals (Sweden)

    Fred Scholz

    2010-04-01

    Full Text Available O pensamento desenvolvimentista do passado era dominado pela ideia de que o subdesenvolvimento do Terceiro Mundo poderia ser superado mediante ajuda técnica, financeira e pessoal dos países do Norte. A meta era alcançar o nível de desenvolvimento dos países ocidentais industrializados por meio de um desenvolvimento retardatário. Na base dessa ideia estava, por um lado, o consenso de valores ocidental-humanitários, que, o mais tardar desde a época do Esclarecimento, determinou o pensar e o devir social. Por outro lado, a ideia baseou-se na responsabilidade histórica (surgida das condições da Guerra Fria, aceita política e socialmente do "Ocidente" para com os chamados países em desenvolvimento, na sua maioria ex-colônias. Argumenta-se, neste artigo, que a ideia de um desenvolvimento retardatário deve, na era da globalização, ser substituída pelo fato de um desenvolvimento fragmentador.

  16. Experimental Study of the Ultrasonic Vibration-Assisted Abrasive Waterjet Micromachining the Quartz Glass

    Directory of Open Access Journals (Sweden)

    Rongguo Hou

    2018-01-01

    Full Text Available The ultrasonic vibration is used to enhance the capability of the abrasive water micromachining glass. And, the ultrasonic vibration is activated on the abrasive waterjet nozzle. The quality of the flow is improved, and the velocity of the abrasive is increased because of the addition of the ultrasonic energy. The relevant experimental results indicate that the erosion depth and the material volume removal of the glass are obviously increased when ultrasonic vibration is working. As for the influence of process parameters on the material removal of the glass such as vibration amplitude, system pressure, distance of the standoff, and abrasive size, the experimental results indicate that the system pressure and vibration contribute greatly to the glass material removal. Also, the erosion depth and the volume of material removal are increased with the increase in the vibration amplitude and system pressure. There are some uplifts found at the edge of erosion pit. Then, it can be inferred that the plastic method is an important material removal method during the machining process of ultrasonic vibration-assisted abrasive waterjet.

  17. A new method to test rock abrasiveness based on physico-mechanical and structural properties of rocks

    Directory of Open Access Journals (Sweden)

    V.N. Oparin

    2015-06-01

    Full Text Available A new method to test rock abrasiveness is proposed based upon the dependence of rock abrasiveness on their structural and physico-mechanical properties. The article describes the procedure of presentation of properties that govern rock abrasiveness on a canonical scale by dimensionless components, and the integrated estimation of the properties by a generalized index. The obtained results are compared with the known classifications of rock abrasiveness.

  18. Desenvolvimento econômico, desigualdade e saúde

    Directory of Open Access Journals (Sweden)

    Prata Pedro Reginaldo

    1994-01-01

    Full Text Available O autor se refere a dimensão socioeconômica, individual e coletiva do fenômeno saúde-doença. Refere-se também ao fato das populações estarem sobre a influência desigual de fatores de risco e de proteção à saúde. Discute as desigualdades no desenvolvimento e a relação entre desenvolvimento, riqueza, saúde e justiça social. Questiona as teorias de desenvolvimento econômico, diferenciando desenvolvimento de crescimento. Cunha os conceitos de armadilha do desenvolvimento e refugiados sociais. Define uma comunidade saudável. Propõe a necessidade de mudança no modelo de desenvolvimento. Baliza o papel e as limitações do setor saúde no que diz respeito a iniqüidade social.

  19. Kinetic energy density and agglomerate abrasion rate during blending of agglomerates into powders.

    Science.gov (United States)

    Willemsz, Tofan A; Hooijmaijers, Ricardo; Rubingh, Carina M; Tran, Thanh N; Frijlink, Henderik W; Vromans, Herman; van der Voort Maarschalk, Kees

    2012-01-23

    Problems related to the blending of a cohesive powder with a free flowing bulk powder are frequently encountered in the pharmaceutical industry. The cohesive powder often forms lumps or agglomerates which are not dispersed during the mixing process and are therefore detrimental to blend uniformity. Achieving sufficient blend uniformity requires that the blending conditions are able to break up agglomerates, which is often an abrasion process. This study was based on the assumption that the abrasion rate of agglomerates determines the required blending time. It is shown that the kinetic energy density of the moving powder bed is a relevant parameter which correlates with the abrasion rate of agglomerates. However, aspects related to the strength of agglomerates should also be considered. For this reason the Stokes abrasion number (St(Abr)) has been defined. This parameter describes the ratio between the kinetic energy density of the moving powder bed and the work of fracture of the agglomerate. The St(Abr) number is shown to predict the abrasion potential of agglomerates in the dry-mixing process. It appeared possible to include effects of filler particle size and impeller rotational rate into this concept. A clear relationship between abrasion rate of agglomerates and the value of St(Abr) was demonstrated. Copyright © 2011 Elsevier B.V. All rights reserved.

  20. Performance Enhancement of Abrasive Waterjet Cutting

    NARCIS (Netherlands)

    2008-01-01

    Abrasive Waterjet (AWJ) Machining is a recent non-traditional machining process. This technology is widely used in industry for cutting difficult-to-machine-materials, milling slots, polishing hard materials etc. AWJ machining has many advantages, e.g. it can cut net-shape parts, no heat is

  1. Characterization of Conventional and High-Translucency Y-TZP Dental Ceramics Submitted to Air Abrasion.

    Science.gov (United States)

    Tostes, Bhenya Ottoni; Guimarães, Renato Bastos; Noronha-Filho, Jaime Dutra; Botelho, Glauco Dos Santos; Guimarães, José Guilherme Antunes; Silva, Eduardo Moreira da

    2017-01-01

    This study evaluated the effect of air-abrasion on t®m phase transformation, roughness, topography and the elemental composition of three Y-TZP (Yttria-stabilized tetragonal zirconia polycrystal) dental ceramics: two conventional (Lava Frame and IPS ZirCad) and one with high-translucency (Lava Plus). Plates obtained from sintered blocks of each ceramic were divided into four groups: AS (as-sintered); 30 (air-abrasion with 30 mm Si-coated Al2O3 particles); 50 (air-abrasion with 50 mm Al2O3 particles) and 150 (air-abrasion with 150 mm Al2O3 particles). After the treatments, the plates were submitted to X-ray diffractometry; 3-D profilometry and SEM/EDS. The AS surfaces were composed of Zr and t phases. All treatments produced t®m phase transformation in the ceramics. The diameter of air-abrasion particles influenced the roughness (150>50>30>AS) and the topography. SEM analysis showed that the three treatments produced groove-shaped microretentions on the ceramic surfaces, which increased with the diameter of air-abrasion particles. EDS showed a decrease in Zr content along with the emergence of O and Al elements after air-abrasion. Presence of Si was also detected on the plates air-abraded with 30 mm Si-coated Al2O3 particles. It was concluded that irrespective of the type and diameter of the particles, air-abrasion produced t®m phase transformation, increased the roughness and changed the elemental composition of the three Y-TZP dental ceramics. Lava Plus also behaved similarly to the conventional Y-TZP ceramics, indicating that this high translucency ceramic could be more suitable to build monolithic ceramic restorations in the aesthetic restorative dentistry field.

  2. Abrasive water jet: a complementary tool

    Directory of Open Access Journals (Sweden)

    Duarte, J. P.

    1998-04-01

    Full Text Available The abrasive water jet is a powerful cutting tool, whose main advantages lie in the absence of thermal effects and the capability of cutting highly thick materials. Compared with Laser, the abrasive water jet allows the cutting of a larger range of thicknesses and a wider variety of materials such as: ornamental stones, metals, polymers, composites, wood, glass and ceramics. The application of this technology has suffered an extensive growth, with successful applications in varied industrial sectors like the automotive, aerospace, textile, metalworking, ornamental stones, etc. The present communication aims at introducing the abrasive water jet as a complementary tool to laser cutting, presenting its advantages by showing some documented examples of pieces cut for different industries.

    O jacto de água abrasivo é uma poderosa ferramenta de corte, tendo como principais vantagens a ausência de processo térmico e permitir o corte de elevadas espessuras. Comparativamente com o laser o jacto de água abrasivo permite cortar uma maior gama de espessuras, e uma maior diversidade de materiais: rochas ornamentais, metais, polimeros, compósitos, madeiras, vidro e cerâmicos. A aplicação desta tecnologia tem sofrido um crescimento acentuado, existindo aplicações de sucesso nos mais variados sectores industriáis como a indústria automóvel, aeroespacial, têxtil, metalomecânica e rochas ornamentáis. Esta comunição pretende apresentar o corte por jacto de agua abrasivo como uma ferramenta de corte complementar ao corte por laser, apresentando as suas vantagens documentadas através de alguns exemplos de peças executadas para as diferentes indústrias.

  3. Release of carbon nanotubes from an epoxy-based nanocomposite during an abrasion process.

    Science.gov (United States)

    Schlagenhauf, Lukas; Chu, Bryan T T; Buha, Jelena; Nüesch, Frank; Wang, Jing

    2012-07-03

    The abrasion behavior of an epoxy/carbon nanotube (CNT) nanocomposite was investigated. An experimental setup has been established to perform abrasion, particle measurement, and collection all in one. The abraded particles were characterized by particle size distribution and by electron microscopy. The abrasion process was carried out with a Taber Abraser, and the released particles were collected by a tube for further investigation. The particle size distributions were measured with a scanning mobility particle sizer (SMPS) and an aerodynamic particle sizer (APS) and revealed four size modes for all measured samples. The mode corresponding to the smallest particle sizes of 300-400 nm was measured with the SMPS and showed a trend of increasing size with increasing nanofiller content. The three measured modes with particle sizes from 0.6 to 2.5 μm, measured with the APS, were similar for all samples. The measured particle concentrations were between 8000 and 20,000 particles/cm(3) for measurements with the SMPS and between 1000 and 3000 particles/cm(3) for measurements with the APS. Imaging by transmission electron microscopy (TEM) revealed that free-standing individual CNTs and agglomerates were emitted during abrasion.

  4. Erosion wear of boron carbide ceramic nozzles by abrasive air-jets

    International Nuclear Information System (INIS)

    Deng Jianxin

    2005-01-01

    Boron carbide nozzles were produced by hot pressing. The erosion wear of this nozzle caused by abrasive particle impact was investigated by abrasive air-jets. Silica, silicon carbide and alumina powders with different hardness were used as the erodent abrasive particles. Results showed that the hardness of the erodent particles played an important role with respect to the erosion wear of the boron carbide nozzles. As the hardness of the erodent particles increases, there is a dramatic increase in erosion rate of the nozzles. The nozzle entrance area suffered from severe abrasive impact under large impact angles, and generated maximum tensile stresses. The wear mechanisms of boron carbide nozzle at this area appeared to be entirely brittle in nature with the evidence of large scale-chipping, and exhibited a brittle fracture induced removal process. While at the nozzle center wall section, most of the particles traveled parallel to the nozzle wall, and showed minimum tensile stresses. The wear mode in this area of the nozzle changed from impact to sliding erosion, and the wear mechanisms appeared to be the lateral cracking owing to a surface fatigue fracture mechanism

  5. Effect of dried sunflower seeds on incisal edge abrasion: A rare case report.

    Science.gov (United States)

    Rath, Avita; Ramamurthy, Priyadarshini H; Fernandes, Bennete Aloysius; Sidhu, Preena

    2017-01-01

    Tooth surface loss (TSL) is a complex phenomenon characterized by the loss of hard tooth structure at various locations of the teeth, usually due to more than one factor. TSL due to abrasion can be significant in patients consuming coarse, abrasive diet. The present case reports an interesting incisal edge abrasion in a female patient, attributed to a particular dietary behavior of long-term consumption of sunflower seeds. All her family members and most of the people from her native place were also reported to have similar lesions by the patient. Larger epidemiological studies to assess the prevalence and severity of such abrasive lesions in geographic areas with this particular dietary habit need to be carried out so that people may be made aware and educated about alternative ways of eating sunflower seeds that will not cause any form of tooth wear.

  6. 29 CFR 1915.134 - Abrasive wheels.

    Science.gov (United States)

    2010-07-01

    ... 29 Labor 7 2010-07-01 2010-07-01 false Abrasive wheels. 1915.134 Section 1915.134 Labor Regulations Relating to Labor (Continued) OCCUPATIONAL SAFETY AND HEALTH ADMINISTRATION, DEPARTMENT OF LABOR... wheels shall fit freely on the spindle and shall not be forced on. The spindle nut shall be tightened...

  7. Review of Artificial Abrasion Test Methods for PV Module Technology

    Energy Technology Data Exchange (ETDEWEB)

    Miller, David C. [National Renewable Energy Lab. (NREL), Golden, CO (United States); Muller, Matt T. [National Renewable Energy Lab. (NREL), Golden, CO (United States); Simpson, Lin J. [National Renewable Energy Lab. (NREL), Golden, CO (United States)

    2016-08-01

    This review is intended to identify the method or methods--and the basic details of those methods--that might be used to develop an artificial abrasion test. Methods used in the PV literature were compared with their closest implementation in existing standards. Also, meetings of the International PV Quality Assurance Task Force Task Group 12-3 (TG12-3, which is concerned with coated glass) were used to identify established test methods. Feedback from the group, which included many of the authors from the PV literature, included insights not explored within the literature itself. The combined experience and examples from the literature are intended to provide an assessment of the present industry practices and an informed path forward. Recommendations toward artificial abrasion test methods are then identified based on the experiences in the literature and feedback from the PV community. The review here is strictly focused on abrasion. Assessment methods, including optical performance (e.g., transmittance or reflectance), surface energy, and verification of chemical composition were not examined. Methods of artificially soiling PV modules or other specimens were not examined. The weathering of artificial or naturally soiled specimens (which may ultimately include combined temperature and humidity, thermal cycling and ultraviolet light) were also not examined. A sense of the purpose or application of an abrasion test method within the PV industry should, however, be evident from the literature.

  8. Liquid abrasive pressure pot scoping tests report

    International Nuclear Information System (INIS)

    Archibald, K.E.

    1996-01-01

    The primary initiatives of the LITCO Decontamination Development group at the Idaho Chemical Process Plant (ICPP) are the development of methods to eliminate the use of sodium bearing decontamination chemicals and minimization of the amount of secondary waste generated during decontamination activities. In July of 1994, a Commerce Business Daily (CBD) announcement was issued by the INEL to determine commercial interest in the development of an in-situ liquid abrasive grit blasting system. As a result of the CBD announcement, Klieber ampersand Schulz issued an Expression of Interest letter which stated they would be interested in testing a prototype Liquid Abrasive Pressure Pot (LAPP). LITCO's Decontamination group and Kleiber ampersand Schulz entered into a Cooperative Research and Development Agreement (CRADA) in which the Decontamination Development group tested the prototype LAPP in a non-radioactive hot cell mockup. Test results are provided

  9. Research on operation mode of abrasive grain during grinding

    Science.gov (United States)

    Ivanova, T. N.; Dement’ev, V. B.; Nikitina, O. V.

    2018-03-01

    The processing of materials by cutting with an abrasive tool is carried out by means of thousands of grains bonded together as a single whole. The quality of the abrasive tool is defined by cutting properties of abrasive grains and depends on features of spreading the temperature field in time and in the abrasive grain volume. Grains are exposed to heating and cooling during work. It leads to undesired effects such as a decrease of durability of grain retention in the binder, hardness, intensification of diffusion and oxidation processes between the binder and the grain, the occurrence of considerable temperature stresses in the grain itself. The obtained equation which allows calculation of temperature field of grain for one rotation of grinding wheel shows that the temperature of the wheel depends on grinding modes and thermophysical properties of abrasive material. Thus, as the time of contact of grain with processed material increases, the temperature in the cutting area rises. As thermophysical properties increase, the temperature in cutting area decreases. Thermal working conditions are determined to be different from each other depending on contact time of the grain and the material. For example, in case of creep-feed grinding, the peak value of temperature is higher than during multistep grinding; the depth of expansion is greater. While the speed of the thermal process in creep-feed grinding is 2-3 times lower than in multistep grinding, the gradient reduces 3-4 times. The analysis of machining methods shows that creep-feed grinding ensures greater depth of grain heating, a smaller heating rate and a reduced velocity gradient. It causes a decrease of probable allotropic modifications and prevents from occurring of heat strokes - cracking of grains due to high temperature falls. Consequently, it is necessary to employ creep-feed grinding to increase the efficiency of abrasive tool employing. Three operation modes of grinding wheel including blunting, full

  10. A study on the abundance of quartz in thermal coals of India and its relation to abrasion index: Development of predictive model for abrasion

    Energy Technology Data Exchange (ETDEWEB)

    Bandopadhyay, A.K. [Central Institute of Mining and Fuel Research Digwadih Campus, P.O.-FRI, Dhanbad-828108, Jharkhand (India)

    2010-10-01

    The quartz content of each of the 61 thermal coals used in power stations in India has been determined using Fourier Transform Infra-Red (FTIR) Spectroscopy. It has been observed that quartz is abundant in the thermal coals and its proportion varies from 5 to 20% by wt. The abrasion index (AI), a measure of abrasion caused by coals, has been determined for each coal according to the procedure laid down in Indian Standard IS: 9949-1986. The data generated on abrasion together with ash and quartz percentages of the coals studied have been subjected to regression and correlation analysis. Positive correlations have been found between AI and quartz content and between AI and ash yield, but the correlation between AI and ash (A) and quartz (Q) percentages has been observed to be the most significant (R{sup 2} = 0.86). The linear regression model AI = 1.00A + 1.35Q thus developed has the ability to predict AI of the thermal coals within {+-} 10 mg/kg at 95.5% confidence level. Results of application of the model to predicting abrasion of a limited number of foreign coals with different origins have been found to be encouraging. Integration of other variables like the size and the shape of the abrading particles along with other physical properties of coal, like the bulk density and the grindability, with the model, in addition to the variables already considered, has been suggested for improved prediction. (author)

  11. Prepolishing on a CNC platform with bound abrasive contour tools

    Science.gov (United States)

    Schoeffler, Adrienne E.; Gregg, Leslie L.; Schoen, John M.; Fess, Edward M.; Hakiel, Michael; Jacobs, Stephen D.

    2003-05-01

    Deterministic microgrinding (DMG) of optical glasses and ceramics is the commercial manufacturing process of choice to shape glass surfaces prior to final finishing. This process employs rigid bound matrix diamond tooling resulting in surface roughness values of 3-5μm peak to valley and 100-400nm rms, as well as mid-spatial frequency tool marks that require subsequent removal in secondary finishing steps. The ability to pre-polish optical surfaces within the grinding platform would reduce final finishing process times. Bound abrasive contour wheels containing cerium oxide, alumina or zirconia abrasives were constructed with an epoxy matrix. The effects of abrasive type, composition, and erosion promoters were examined for tool hardness (Shore D), and tested with commercial optical glasses in an Optipro CNC grinding platform. Metrology protocols were developed to examine tool wear and subsequent surface roughness. Work is directed to demonstrating effective material removal, improved surface roughness and cutter mark removal.

  12. Characterization of abrasion-induced nanoparticle release from paints into liquids and air

    Science.gov (United States)

    Golanski, L.; Gaborieau, A.; Guiot, A.; Uzu, G.; Chatenet, J.; Tardif, F.

    2011-07-01

    Two standard methods for the characterization of the abrasion nanoparticle release into air and liquid from coatings containing nanoparticles were developed. Details of the abrasion processes and the measurement methods are shown. Paints were formulated in an industrial facility. Standard abrasion conditions in wet environments were simulated. The size distribution of the particles abraded into liquid was analyzed by a laser granulometer: submicrometric and micrometric particles were observed, but no nanometric particles. The nanoparticles released in liquid were deposited on filters for SEM (Scanning Electron Microscopy) analysis. No free or agglomerated nanoparticles were observed by SEM: nanoparticles seem to remain embedded in the paint matrix. The same coatings were abraded in the air using another standard method. The ELPI (Electrical Low Pressure Impactor) was used to determine the number size distribution of the dust generated. Abrasion is found to produce submicrometric and micrometric particles in the air but no nanoparticles. Further characterizations by SEM confirmed that no free or agglomerated nanoparticles were emitted: nanoparticles seem to remain embedded in the paint matrix.

  13. Characterization of abrasion-induced nanoparticle release from paints into liquids and air

    International Nuclear Information System (INIS)

    Golanski, L; Guiot, A; Uzu, G; Tardif, F; Gaborieau, A; Chatenet, J

    2011-01-01

    Two standard methods for the characterization of the abrasion nanoparticle release into air and liquid from coatings containing nanoparticles were developed. Details of the abrasion processes and the measurement methods are shown. Paints were formulated in an industrial facility. Standard abrasion conditions in wet environments were simulated. The size distribution of the particles abraded into liquid was analyzed by a laser granulometer: submicrometric and micrometric particles were observed, but no nanometric particles. The nanoparticles released in liquid were deposited on filters for SEM (Scanning Electron Microscopy) analysis. No free or agglomerated nanoparticles were observed by SEM: nanoparticles seem to remain embedded in the paint matrix. The same coatings were abraded in the air using another standard method. The ELPI (Electrical Low Pressure Impactor) was used to determine the number size distribution of the dust generated. Abrasion is found to produce submicrometric and micrometric particles in the air but no nanoparticles. Further characterizations by SEM confirmed that no free or agglomerated nanoparticles were emitted: nanoparticles seem to remain embedded in the paint matrix.

  14. Development of a novel bioactive glass for air-abrasion to selectively remove orthodontic adhesives.

    Science.gov (United States)

    Taha, Ayam A; Hill, Robert G; Fleming, Padhraig S; Patel, Mangala P

    2018-05-01

    To develop a novel, bioactive glass for removing residual orthodontic adhesive via air-abrasion, following bracket debonding, and to evaluate its effectiveness against a proprietary bioactive glass 45S5(Sylc™)-air-abrasion, and a slow-speed tungsten carbide (TC) bur. Three glasses were prepared and their bioactivity was proved. One novel glass (QMAT3) was selected due to its appropriate hardness, lower than that of enamel/45S5(Sylc™). Sixty extracted human premolars were randomly assigned to adhesive removal using: (a) QMAT3-air-abrasion, (b) 45S5(Sylc™)-air-abrasion, and (c) TC bur, which were further subdivided (n = 10) based on the adhesive used (Transbond XT™ or Fuji Ortho LC™). Enamel roughness was assessed using scanning electron microscopy (SEM) and non-contact profilometry before bracket bonding, after removing residual adhesive following bracket debonding and after polishing. QMAT3 formed apatite faster (6 h) than 45S5(Sylc™) (24 h) in Tris solution. QMAT3-air-abrasion gave the lowest enamel roughness (Ra) after removing the adhesives. SEM images showed a pitted, roughened enamel surface in the TC bur group and to a lesser extent with 45S5(Sylc™), while a virtually smooth surface without any damage was observed in the QMAT3-air-abrasion group. The time taken for adhesive removal with QMAT3 was comparable to 45S5(Sylc™) but was twice as long with the TC bur. QMAT3-air-abrasion is a promising technique for selective removal of adhesives without inducing tangible enamel damage. A novel bioactive glass has been developed as an alternative to the use of TC burs for orthodontic adhesive removal.

  15. Abrasion Testing of Critical Components of Hydrokinetic Devices

    Energy Technology Data Exchange (ETDEWEB)

    Worthington, Monty [ORPC Alaska; Ali, Muhammad [Ohio University; Ravens, Tom [University of Alaska Anchorage

    2013-12-06

    The objective of the Abrasion Testing of Critical Components of Hydrokinetic Devices (Project) was to test critical components of hydrokinetic devices in waters with high levels of suspended sediment – information that is widely applicable to the hydrokinetic industry. Tidal and river sites in Alaska typically have high suspended sediment concentrations. High suspended sediment also occurs in major rivers and estuaries throughout the world and throughout high latitude locations where glacial inputs introduce silt into water bodies. In assessing the vulnerability of technology components to sediment induced abrasion, one of the greatest concerns is the impact that the sediment may have on device components such as bearings and seals, failures of which could lead to both efficiency loss and catastrophic system failures.

  16. Analysis of abrasive wear behavior of PTFE composite using Taguchi’s technique

    Directory of Open Access Journals (Sweden)

    Yusuf Şahin

    2015-12-01

    Full Text Available Polymeric composites are widely used for structural, aerospace, and automobile sectors due to their good combination of high specific strength and specific modulus. These two main characteristics make these materials attractive, compared to conventional materials like metal or alloy ones. Some of their typical benefits include easy processing, corrosion resistance, low friction, and damping of noise and vibrations. Wear behavior of Polytetrafluoroethylenes (PTFE and its composites including glass-filled composites and carbon-filled composites are investigated using a pin-on-disc configuration. A plan of experiments in terms of Taguchi technique is carried out to acquire data in controlled way. An orthogonal array (L9 and the analysis of variance are employed to investigate the influence of process parameters on the wear of these composites. Volume loss increased with abrasive size, load, and distance. Furthermore, specific wear rate decreased with increasing grit size, load, sliding distance, whereas, slightly with compressive strength. Optimal process parameters, which minimize the volume loss, were the factor combinations of L1, G3, D1, and C3. Confirmation experiments were conducted to verify the optimal testing parameters. It was found that in terms of volume loss, there was a good agreement between the estimated and the experimental value of S/N ratio with an error of 1.604%. Moreover, abrasive size, load, and sliding distance exerted a great effect on the specific wear rate, at 51.14, 27.77, and 14.70%, respectively.

  17. Finishing of display glass for mobile electronics using 3M Trizact diamond tile abrasive pads

    Science.gov (United States)

    Zheng, Lianbin; Fletcher, Tim; Na, Tee Koon; Sventek, Bruce; Romero, Vince; Lugg, Paul S.; Kim, Don

    2010-10-01

    This paper will describe a new method being used during the finishing of glass displays for mobile electronics including mobile hand held devices and notebook computers. The new method consists of using 3M TrizactTM Diamond Tile Abrasive Pads. TrizactTM Diamond Tile is a structured fixed abrasive grinding technology developed by 3M Company. The TrizactTM Diamond Tile structured abrasive pad consists of an organic (polymeric binder) - inorganic (abrasive mineral, i.e., diamond) composite that is used with a water-based coolant. TrizactTM Diamond Tile technology can be applied in both double and single side grinding applications. A unique advantage of TrizactTM Diamond Tile technology is the combination of high stock removal and low sub-surface damage. Grinding results will be presented for both 9 micron and 20 micron grades of TrizactTM Diamond Tile abrasive pads used to finish several common display glasses including Corning GorillaTM glass and Soda Lime glass.

  18. Cryogenically assisted abrasive jet micromachining of polymers

    International Nuclear Information System (INIS)

    Getu, H; Papini, M; Spelt, J K

    2008-01-01

    The abrasive jet micromachining (AJM) of elastomers and polymers such as polydimethylsiloxane (PDMS), acrylonitrile butadiene styrene (ABS) and polytetrafluoroethylene (PTFE) for use in micro-fluidic devices was found to be very slow or impossible at room temperature. To enhance the material removal rate in such materials, a stream of liquid nitrogen (LN 2 ) was injected into the abrasive jet, cooling the target to cryogenic temperatures. Erosion rate measurements on the three polymeric materials (PDMS, ABS and PTFE) with and without the use of LN 2 were compared along with the profiles of micromachined channels and holes. It was found that the use of LN 2 cooling caused brittle erosion in PDMS, allowing it to be micromachined successfully. An erosion rate increase was also observed in PTFE and ABS at high and intermediate impact angles. The use of LN 2 also was found to reduce particle embedding

  19. Microstructure, Wear Behavior and Corrosion Resistance of WC-FeCrAl and WC-WB-Co Coatings

    Directory of Open Access Journals (Sweden)

    Janette Brezinová

    2018-05-01

    Full Text Available The paper is focused on investigating the quality of two grades of thermally sprayed coatings deposited by high-velocity oxygen fuel (HVOF technology. One grade contains WC hard particles in an environmentally progressive Ni- and Co-free FeCrAl matrix, while the second coating contains WC and WB hard particles in a cobalt matrix. The aim of the experimental work was to determine the effect of thermal cyclic loading on the coatings’ resistance to adhesive, abrasive and erosive wear. Abrasive wear was evaluated using abrasive cloth of two grit sizes, and erosive wear was evaluated by a dry-pot wear test in a pin mill at two sample angles. Adhesion wear resistance of the coatings was determined by a sliding wear test under dry friction conditions and in a 1 mol water solution of NaCl. Corrosion resistance of the coatings was evaluated using potentiodynamic polarization tests. Metallographic cross-sections were used for measurement of the microhardness and thickness and for line energy-dispersive X-ray (EDX analysis. The tests proved the excellent resistance of both coatings against adhesive, abrasive, and erosive wear, as well as the ability of the WC-WB-Co coating to withstand alternating temperatures of up to 600 °C. The “green carbide” coating (WC-FeCrAl can be recommended as an environmentally friendly replacement for Ni- and Co-containing coatings, but its operating temperature is strictly limited to 500 °C in air.

  20. High temperature resistant cermet and ceramic compositions. [for thermal resistant insulators and refractory coatings

    Science.gov (United States)

    Phillips, W. M. (Inventor)

    1978-01-01

    High temperature oxidation resistance, high hardness and high abrasion and wear resistance are properties of cermet compositions particularly to provide high temperature resistant refractory coatings on metal substrates, for use as electrical insulation seals for thermionic converters. The compositions comprise a sintered body of particles of a high temperature resistant metal or metal alloy, preferably molybdenum or tungsten particles, dispersed in and bonded to a solid solution formed of aluminum oxide and silicon nitride, and particularly a ternary solid solution formed of a mixture of aluminum oxide, silicon nitride and aluminum nitride. Ceramic compositions comprising a sintered solid solution of aluminum oxide, silicon nitride and aluminum nitride are also described.

  1. Validation of Proposed Metrics for Two-Body Abrasion Scratch Test Analysis Standards

    Science.gov (United States)

    Street, Kenneth W., Jr.; Kobrick, Ryan L.; Klaus, David M.

    2013-01-01

    Abrasion of mechanical components and fabrics by soil on Earth is typically minimized by the effects of atmosphere and water. Potentially abrasive particles lose sharp and pointed geometrical features through erosion. In environments where such erosion does not exist, such as the vacuum of the Moon, particles retain sharp geometries associated with fracturing of their parent particles by micrometeorite impacts. The relationship between hardness of the abrasive and that of the material being abraded is well understood, such that the abrasive ability of a material can be estimated as a function of the ratio of the hardness of the two interacting materials. Knowing the abrasive nature of an environment (abrasive)/construction material is crucial to designing durable equipment for use in such surroundings. The objective of this work was to evaluate a set of standardized metrics proposed for characterizing a surface that has been scratched from a two-body abrasion test. This is achieved by defining a new abrasion region termed Zone of Interaction (ZOI). The ZOI describes the full surface profile of all peaks and valleys, rather than just measuring a scratch width. The ZOI has been found to be at least twice the size of a standard width measurement; in some cases, considerably greater, indicating that at least half of the disturbed surface area would be neglected without this insight. The ZOI is used to calculate a more robust data set of volume measurements that can be used to computationally reconstruct a resultant profile for de tailed analysis. Documenting additional changes to various surface roughness par ameters also allows key material attributes of importance to ultimate design applications to be quantified, such as depth of penetration and final abraded surface roughness. Further - more, by investigating the use of custom scratch tips for specific needs, the usefulness of having an abrasion metric that can measure the displaced volume in this standardized

  2. Bio-active glass air-abrasion has the potential to remove resin composite restorative material selectively

    International Nuclear Information System (INIS)

    Milly, Hussam; Andiappan, Manoharan; Thompson, Ian; Banerjee, Avijit

    2014-01-01

    The aims of this study were to assess: (a) the chemistry, morphology and bioactivity of bio-active glass (BAG) air-abrasive powder, (b) the effect of three air-abrasion operating parameters: air pressure, powder flow rate (PFR) and the abrasive powder itself, on the selective removal of resin composite and (c) the required “time taken”. BAG abrasive particles were characterised using scanning electron microscopy-energy dispersive X-ray spectrometry (SEM-EDX) and Fourier-transform infrared spectroscopy (FTIR). Standardised resin composite restorations created within an enamel analogue block (Macor™) in vitro, were removed using air-abrasion undersimulated clinical conditions. 90 standardised cavities were scanned before and after resin composite removal using laser profilometry and the volume of the resulting 3D images calculated. Multilevel linear model was used to identify the significant factors affecting Macor™ removal. BAG powder removed resin composite more selectively than conventional air-abrasion alumina powder using the same operating parameters (p < 0.001) and the effect of altering the unit's operating parameters was significant (p < 0.001). In conclusion, BAG powder is more efficient than alumina in the selective removal of resin composite particularly under specific operating parameters, and therefore may be recommended clinically as a method of preserving sound enamel structure when repairing and removing defective resin composite restorations.

  3. Robotic edge machining using elastic abrasive tool

    Science.gov (United States)

    Sidorova, A. V.; Semyonov, E. N.; Belomestnykh, A. S.

    2018-03-01

    The article describes a robotic center designed for automation of finishing operations, and analyzes technological aspects of an elastic abrasive tool applied for edge machining. Based on the experimental studies, practical recommendations on the application of the robotic center for finishing operations were developed.

  4. The abrasive effect of commercial whitening toothpastes on eroded enamel.

    Science.gov (United States)

    Mosquim, Victor; Martines Souza, Beatriz; Foratori Junior, Gerson Aparecido; Wang, Linda; Magalhães, Ana Carolina

    2017-06-01

    To evaluate the in vitro abrasive effect of commercial whitening toothpastes on eroded bovine enamel samples in respect to erosive tooth wear. 72 bovine crowns were embedded, polished and subjected to the baseline profile analysis. The samples were then protected in 2/3 of the enamel surface and were randomly assigned to six groups (n= 12/group): G1: Oral-B 3D White, G2: Close-up Diamond Attraction Power White, G3: Sorriso Xtreme White 4D, G4: Colgate Luminous White, G5: Crest (conventional toothpaste), G6:erosion only (control). All samples were submitted to an erosive pH cycling (4 x 90 seconds in 0.1% citric acid, pH 2.5, per day) and abrasive challenges (2 x 15 seconds, per day) for 7 days. After the first and the last daily cycles, the samples were subjected to abrasive challenges, using a toothbrushing machine, soft toothbrushes and slurry of the tested toothpastes (1.5 N). Between the challenges, the samples were immersed in artificial saliva. The final profile was obtained and overlaid to the baseline profile for the calculation of the erosive tooth wear (μm). The data were subjected to Kruskal-Wallis/Dunn tests (Penamel wear (3.68±1.06 μm), similarly to G3 (3.17± 0.80 μm) and G4 (3.44± 1.29 μm). G3 and G4 performed similarly between them and compared with G5 (2.35± 1.44 μm). G2 (1.51± 0.95 μm) and G6 (0.85± 0.36 μm) showed the lowest enamel wear, which did not differ between them and from G5. Oral-B 3D White showed the highest abrasive potential while Close-up Diamond Attraction Power White showed the lowest abrasive potential on eroded enamel in vitro. This study showed that some commercial whitening toothpastes, especially those containing pyrophosphate associated with hydrated silica, enhanced enamel erosive wear.

  5. O DIREITO FUNDAMENTAL AO DESENVOLVIMENTO SUSTENTÁVEL

    OpenAIRE

    Fernandes, Jeferson Nogueira

    2012-01-01

    Este artigo jurídico trata do direito fundamental do ser humano ter um desenvolvimento sustentável, e tem como objetivo identificar o desenvolvimento sustentável como sendo um direito fundamental consagrado universalmente. Em sua elaboração foi utilizado o seguinte material: textos doutrinários, legislação nacional pertinente e documentos internacionais. A conclusão indica que: o desenvolvimento sustentável é um direito fundamental do homem e que devemos manter equilibrada a relação ambiente ...

  6. Saúde e desenvolvimento

    Directory of Open Access Journals (Sweden)

    Ana Luiza D'Ávila Viana

    Full Text Available Considerando que os modernos sistemas de saúde são o resultado da complexa interação de processos econômicos, políticos e sociais, o objetivo do trabalho é discutir a relação entre saúde e desenvolvimento no Brasil, mostrando que o esgotamento do modelo liberal de política econômica abre nova perspectiva para a retomada do desenvolvimento, entendido como combinação entre crescimento da economia, mudanças na estrutura produtiva e melhora das condições de vida da população. O complexo produtivo da saúde joga papel decisivo nesse processo, pois constitui um campo em que inovação tecnológica e acumulação de capital geram oportunidades de investimento, trabalho e renda, além de produzir avanços importantes para melhorar o estado de saúde das pessoas. A recente adoção de políticas públicas voltadas para articular, de forma positiva, aspectos da política econômica e da política social revela que a questão do desenvolvimento nacional ganhou nova centralidade na agenda governamental, o que abre a perspectiva de maior integração entre a lógica econômica e a lógica sanitária. Entretanto, é preciso reconhecer que o Brasil ainda não logrou alcançar uma associação virtuosa entre saúde e desenvolvimento.

  7. Damage to the edge of steel stampings and abrasive during ultrasonic hydroabrasive machining

    International Nuclear Information System (INIS)

    Dokuchaeva, V.A.; Chernov, A.P.

    1976-01-01

    Principles have been established explaining the fracture of abrasive material in the process of ultrasonic hydroabrasive treatment, and a method is proposed suitable for the calculation of steel barb erosion in the hydroabrasive flux. It is assumed that fracture occurs along the entire edge surface and that the losses caused by plastic deformation are small. Conclusion has been made as to the governing the change of the abrasive particle size in the time of treatment. It is shown that the most serious fracture takes place at initial stage of the treatment, terminating practically after 60 minutes of operation. Curves showing the distribution of boron carbide abrasive particles are presented

  8. Material Abrasive Water Jet Cutting Investigation by Means Accompanying Physical Phenomena

    OpenAIRE

    Kinik, D.; Gánovská, B.; Hloch, S. (Sergej); Cárach, J.; Lehocká, D.

    2013-01-01

    The paper deals with the indirect ways of on-line monitoring of technological processes of cutting. The objective of the study is a design of on-line monitoring system for the cutting technology through an abrasive water jet. In cutting by the abrasive water jet two parallel phenomena are formed. The phenomena are represented by generated surface and vibrations. For the purpose of proving of the hypothetical assumptions on dependence of generated surface quality on vibrations the ex...

  9. Chemical mechanical polishing of hard disk substrate with {alpha}-alumina-g-polystyrene sulfonic acid composite abrasive

    Energy Technology Data Exchange (ETDEWEB)

    Lei Hong, E-mail: hong_lei2005@yahoo.com.c [Research Center of Nano-science and Nano-technology, Shanghai University, Shanghai 200444 (China); Bu Naijing; Chen Ruling; Hao Ping [Research Center of Nano-science and Nano-technology, Shanghai University, Shanghai 200444 (China); Neng Sima; Tu Xifu; Yuen Kwok [Shenzhen Kaifa Magnetic Recording Co., LTD, Shenzhen, 518035 (China)

    2010-05-03

    {alpha}-Alumina-g-polystyrene sulfonic acid ({alpha}-Al{sub 2}O{sub 3}-g-PSS) composite abrasive was prepared by surface activation, graft polymerization and sulfonation, successively. The composition, dispersibility and morphology of the product were characterized by Fourier transformed infrared spectroscopy, laser particle size analysis and scanning electron microscopy, respectively. The chemical mechanical polishing (CMP) performances of the composite abrasive on hard disk substrate with nickel-phosphorous plating were investigated. The microscopy images of the polished surfaces show that {alpha}-Al{sub 2}O{sub 3}-g-PSS composite abrasive results in improved CMP and post-CMP cleaning performances than pure {alpha}-alumina abrasive under the same testing conditions.

  10. Experimental Evidence that Abrasion of Carbonate Sand is a Significant Source of Carbonate Mud

    Science.gov (United States)

    Trower, L.; Kivrak, L.; Lamb, M. P.; Fischer, W. W.

    2017-12-01

    Carbonate mud is a major sedimentary component of modern and ancient tropical carbonate environments, yet its enigmatic origin remains debated. Early views on the origin of carbonate mud considered the abrasion of carbonate sand during sediment transport as a possible mechanism. In recent decades, however, prevailing thought has generally settled on a binary explanation: 1) precipitation of aragonite needles within the water column, and 2) post-mortem dispersal of biological aragonite, in particular from algae, and perhaps aided by fish. To test these different hypotheses, we designed a model and a set of laboratory experiments to quantify the rates of mud production associated with sediment transport. We adapted a recent model of ooid abrasion rate to predict the rate of mud production by abrasion of carbonate sand as a function of grain size and sediment transport mode. This model predicts large mud production rates, ranging from 103 to 104 g CaCO3/m2/yr for typical grain sizes and transport conditions. These rate estimates are at least one order of magnitude more rapid than the 102 g CaCO3/m2/yr estimates for other mechanisms like algal biomineralization, indicating that abrasion could produce much larger mud fluxes per area as other mechanisms. We tested these estimates using wet abrasion mill experiments; these experiments generated mud through mechanical abrasion of both ooid and skeletal carbonate sand for grain sizes ranging from 250 µm to >1000 µm over a range of sediment transport modes. Experiments were run in artificial seawater, including a series of controls demonstrating that no mud was produced via homogenous nucleation and precipitation in the absence of sand. Our experimental rates match the model predictions well, although we observed small systematic differences in rates between abrasion ooid sand and skeletal carbonate sand that likely stems from innate differences in grain angularity. Electron microscopy of the experimental products revealed

  11. Liquid abrasive grit blasting literature search and decontamination scoping tests report

    International Nuclear Information System (INIS)

    Ferguson, R.L.

    1993-10-01

    Past decontamination and solvent recovery activities at the Idaho Chemical Processing Plant (ICPP) have resulted in the accumulation of 1.5 million gallons of radioactively contaminated sodium-bearing liquid waste. Future decontamination activities at the ICPP could result in the production of 5 million gallons or more of sodium-bearing waste using the current decontamination techniques of chemical/water flushes and steam jet cleaning. With the curtailment of reprocessing at the ICPP, the focus of decontamination is shifting from maintenance for continued operation of the facilities to decommissioning. As decommissioning plans are developed, new decontamination methods must be used which result in higher decontamination factors and generate lower amounts of sodium-bearing secondary waste. The primary initiative of the WINCO Decontamination Development Program is the development of methods to eliminate/minimize the use of sodium-bearing decontamination chemicals. One method that was chosen for cold scoping studies during FY-93 was abrasive grit blasting. Abrasive grit blasting has been used in many industries and a vast amount of research and development has already been conducted. However, new grits, process improvements and ICPP applicability was investigated. This evaluation report is a summary of the research efforts and scoping tests using the liquid abrasive grit blasting decontamination technique. The purpose of these scoping tests was to determine the effectiveness of three different abrasive grits: plastic beads, glass beads and alumina oxide

  12. CFD Based Erosion Modelling of Abrasive Waterjet Nozzle using Discrete Phase Method

    International Nuclear Information System (INIS)

    Kamarudin, Naqib Hakim; Prasada Rao, A K; Azhari, Azmir

    2016-01-01

    In Abrasive Waterjet (AWJ) machining, the nozzle is the most critical component that influences the performance, precision and economy. Exposure to a high speed jet and abrasives makes it susceptible to wear erosion which requires for frequent replacement. The present works attempts to simulate the erosion of the nozzle wall using computational fluid dynamics. The erosion rate of the nozzle was simulated under different operating conditions. The simulation was carried out in several steps which is flow modelling, particle tracking and erosion rate calculation. Discrete Phase Method (DPM) and K-ε turbulence model was used for the simulation. Result shows that different operating conditions affect the erosion rate as well as the flow interaction of water, air and abrasives. The simulation results correlates well with past work. (paper)

  13. Bio-active glass air-abrasion has the potential to remove resin composite restorative material selectively

    Energy Technology Data Exchange (ETDEWEB)

    Milly, Hussam [Biomaterials, Biomimetics and Biophotonics Research Group, Kings College London Dental Institute at Guy' s Hospital, King' s Health Partners, London (United Kingdom); Andiappan, Manoharan [Unit of Dental Public Health, Kings College London Dental Institute at Guy' s Hospital, King' s Health Partners, London (United Kingdom); Thompson, Ian [Biomaterials, Biomimetics and Biophotonics Research Group, Kings College London Dental Institute at Guy' s Hospital, King' s Health Partners, London (United Kingdom); Banerjee, Avijit, E-mail: avijit.banerjee@kcl.ac.uk [Biomaterials, Biomimetics and Biophotonics Research Group, Kings College London Dental Institute at Guy' s Hospital, King' s Health Partners, London (United Kingdom); Unit of Conservative Dentistry, King' s College London Dental Institute at Guy' s Hospital, King' s Health Partners, London (United Kingdom)

    2014-06-01

    The aims of this study were to assess: (a) the chemistry, morphology and bioactivity of bio-active glass (BAG) air-abrasive powder, (b) the effect of three air-abrasion operating parameters: air pressure, powder flow rate (PFR) and the abrasive powder itself, on the selective removal of resin composite and (c) the required “time taken”. BAG abrasive particles were characterised using scanning electron microscopy-energy dispersive X-ray spectrometry (SEM-EDX) and Fourier-transform infrared spectroscopy (FTIR). Standardised resin composite restorations created within an enamel analogue block (Macor™) in vitro, were removed using air-abrasion undersimulated clinical conditions. 90 standardised cavities were scanned before and after resin composite removal using laser profilometry and the volume of the resulting 3D images calculated. Multilevel linear model was used to identify the significant factors affecting Macor™ removal. BAG powder removed resin composite more selectively than conventional air-abrasion alumina powder using the same operating parameters (p < 0.001) and the effect of altering the unit's operating parameters was significant (p < 0.001). In conclusion, BAG powder is more efficient than alumina in the selective removal of resin composite particularly under specific operating parameters, and therefore may be recommended clinically as a method of preserving sound enamel structure when repairing and removing defective resin composite restorations.

  14. Pre-polishing on a CNC platform with bound abrasive contour tools

    Science.gov (United States)

    Schoeffer, Adrienne E.

    2003-05-01

    Deterministic micorgrinding (DMG) of optical glasses and ceramics is the commercial manufacturing process of choice to shape glass surfaces prior to final finishing. This process employs rigid bound matrix diamond tooling resulting in surface roughness values of 3-51.tm peak to valley and 100-400nm rms, as well as mid-spatial frequency tool marks that require subsequent removal in secondary finishing steps. The ability to pre-polish optical surfaces within the grinding platform would reduce final finishing process times. Bound abrasive contour wheels containing cerium oxide, alumina or zirconia abrasives were constructed with an epoxy matrix. The effects of abrasive type, composition, and erosion promoters were examined for tool hardness (Shore D), and tested with commercial optical glasses in an OptiproTM CNC grinding platform. Metrology protocols were developed to examine tool wear and subsequent surface roughness. Work is directed to demonstrating effective material removal, improved surface roughness and cutter mark removal.

  15. Experimental Study on Layered Ice Bonded Abrasive Polishing of Glass-ceramics

    Directory of Open Access Journals (Sweden)

    Yuli SUN

    2014-12-01

    Full Text Available Layered ice bonded abrasive tools (LIBAT is a new kind of one which not only has the ability of lapping and polishing but also has the effect of self-dressing. In this paper, two kinds of layered ice bonded abrasive tools were designed and manufactured. Experimental studies on layered ice bonded abrasive (LIBA polishing of glass-ceramics were conducted. The results show that the surface topography of glass-ceramics polished by micro α-Al2O3-nano α-Al2O3 LIBAT is better than that of polished by micro α-Al2O3-nano SiO2 LIBAT. The surface roughness Sa of glass-ceramics polished by the two kinds of LIBAT is at the nanometer scale. The reasons of this phenomenon were analyzed. The experimental results illustrate that the LIBAT shows good effect and can be used in production practice. DOI: http://dx.doi.org/10.5755/j01.ms.20.4.6149

  16. Design of a new abrasive slurry jet generator

    Science.gov (United States)

    Wang, F. C.; Shi, L. L.; Guo, C. W.

    2017-12-01

    With the advantages of a low system working pressure, good jet convergence and high cutting quality, abrasive slurry jet (ASJ) has broad application prospects in material cutting and equipment cleaning. Considering that the generator plays a crucial role in ASJ system, the paper designed a new type ASJ generator using an electric oil pump, a separate plunger cylinder, and a spring energized seal. According to the determining of structure shape, size and seal type, a new ASJ generator has been manufactured out and tested by a series of experiments. The new generator separates the abrasive slurry from the dynamic hydraulic oil, which can improve the service life of the ASJ system. And the new ASJ system can reach 40 MPa and has good performance in jet convergence, which deserves to popularization and application in materials machining.

  17. DIREITOS HUMANOS, DESENVOLVIMENTO SUSTENTÁVEL E SUSTENTABILIDADE

    OpenAIRE

    Carvalho, Sonia Aparecida de; Silva, Denival Francisco da; Adolfo, Luiz Gonzaga Silva

    2015-01-01

    Este artigo trata da relação intrínseca entre os direitos humanos, o desenvolvimento sustentável e a sustentabilidade. Seu objetivo geral consiste em analisar o modelo de desenvolvimento implementado e a necessária proteção e preservação do meio ambiente ligado à defesa dos direitos humanos. Os objetivos específicos pretendem investigar a distinção dos termos sustentabilidade e desenvolvimento sustentável, como a concretização do direito à sustentabilidade, os critérios e as dimensões da sust...

  18. Impact strength and abrasion resistance of high strength concrete with rice husk ash and rubber tires

    Directory of Open Access Journals (Sweden)

    M. B. Barbosa

    Full Text Available The paper discusses the application of High Strength Concrete (HSC technology for concrete production with the incorporation of Rice Husk Ash (RHA residues by replacing a bulk of the material caking and rubber tires with partial aggregate volume, assessing their influence on the mechanical properties and durability. For concrete with RHA and rubber, it was possible to reduce the brittleness by increasing the energy absorbing capacity. With respect to abrasion, the RHA and rubber concretes showed lower mass loss than the concrete without residues, indicating that this material is attractive to be used in paving. It is thus hoped that these residues may represent a technological and ecological alternative for the production of concrete in construction works.

  19. Gestões do desenvolvimento e desenvolvimentos da gestão: da unilateralidade reificada à dialogicidade da simbiose homem/natureza

    Directory of Open Access Journals (Sweden)

    Carlos Eduardo Justen

    Full Text Available Este artigo, ao situar culturalmente os fenômenos da gestão e do desenvolvimento, em sua concepção tradicional, no projeto da modernidade e ao identificar o predomínio da unilateralidade reificada na interface entre gestão e desenvolvimento - a primeira vista como instrumento técnico submisso à via clássica do segundo - almeja evidenciar as potencialidades da compreensão e da construção de alternativas, tanto para a gestão como para o desenvolvimento, a partir da ressignificação dessa interface. Para tanto, o esforço foi direcionado ao resgate do que é comum aos fenômenos da gestão e do desenvolvimento - os substratos antropológico e ecológico -, nucleados nos princípios da reciprocidade dialógica, concretizadora da condição antropológica, e da finitude, caracterizadora da condição ecológica. Ao final, são apresentadas oito potenciais contribuições advindas da exploração renovada da interface entre a gestão e o desenvolvimento. Propôs-se, ainda, a substituição da lógica instrumental da eficiência financeira, comum à concepção tradicional dos fenômenos estudados, pela lógica da simbiose dialógica homem/natureza, uma vez que, como fenômenos sociais, desenvolvimento e gestão, mediados pelo meio, também são ecológicos em sua essência.

  20. Effects of hardness of abrasive grains on surface roughness of work piece in PVA bonded grinding wheel

    International Nuclear Information System (INIS)

    Nitta, S.; Takata, A.; Ishizaki, K.

    2000-01-01

    The purpose of this study is to clarify relation between hardness of abrasive grains and surface roughness of work piece in the case of PVA (Polyvinyl alcohol) bonded grinding wheels. Two PVA bonded grinding wheels; with diamond or silicon carbide as abrasive grains and grinding of glass and aluminum alloy was performed. The PVA bonded grinding wheels The PVA bonded grinding wheel with silicon carbide could not grind the glass. Because insufficiency in hardness, the PVA bonded grinding wheel with the diamond abrasive grains caused deep scratch on the aluminum alloy. It was found that the final surface roughness of the work piece was not proportional to the hardness of abrasive grains. The suitable hardness of abrasive grains will be obtained by the hardness of work piece. Copyright (2000) AD-TECH - International Foundation for the Advancement of Technology Ltd

  1. Controls on wind abrasion patterns through a fractured bedrock landscape

    Science.gov (United States)

    Perkins, J. P.; Finnegan, N. J.

    2017-12-01

    Wind abrasion is an important geomorphic process for understanding arid landscape evolution on Earth and interpreting the post-fluvial history of Mars. Both the presence and orientation of wind-abraded landforms provide potentially important constraints on paleo-climatic conditions; however, such interpretations can be complicated by lithologic and structural heterogeneity. To explore the influence of pre-existing structure on wind abrasion, we exploit a natural experiment along the 10.2 Ma Lower Rio San Pedro ignimbrite in northern Chile. Here, a 3.2 Ma andesite flow erupted from Cerro de las Cuevas and deposited atop the ignimbrite, supplying wind-transportable sediment and initiating a phase of downwind abrasion. Additionally, the lava flow provides a continually varying degree of upwind topographic shielding along the ignimbrite that is reflected in a range of surface morphologies. Where fully shielded the ignimbrite surface is partially blanketed by sediment. However, as relief decreases the surface morphology shifts from large polygonal structures that emerge due to the concentration of wind abrasion along pre-existing fracture sets, to polygons that are bisected by wind-parallel grooves that cross-cut fracture sets, to linear sets of yardangs. We reconstruct the ignimbrite surface using a high-resolution digital elevation model, and calculate erosion rates ranging from 0.002 to 0.45 mm/kyr that vary strongly with degree of topographic shielding (R2 = 0.97). We use measured abrasion rates together with nearby weather station data to estimate the nondimensional Rouse number and Inertial Parameter for a range of particle sizes. From these calculations, we hypothesize that the change from fracture-controlled to flow-controlled morphology reflects increases in the grain size and inertia of particles in the suspension cloud. Where the ignimbrite experiences persistent high winds, large particles may travel in suspension and are largely insensitive to topographic

  2. Nuclear-chemical methods in a hard tooth tissue abrasion study

    International Nuclear Information System (INIS)

    Gosman, A.; Spevacek, V.; Konicek, J.; Vopalka, D.; Housova, D.; Dolezalova, L.

    1999-01-01

    The advanced method consists in implantation-labelling of the thin surface layers of the solid objects, e.g. hard tooth tissue, by atoms of suitable natural or artificial radionuclides. Nuclides from the uranium series were implanted into the surface by using nuclear recoil effect at alpha decay of 226 Ra to 222 Rn, alpha decay of 222 Rn to RaA, alpha decay of RaA to RaB (beta-emitter) and further alpha or beta emitters. With regard to chosen alpha detection and to the half-lives of the radionuclides, there was actually measured the activity of 222 Rn, RaA and RaC' in the thin surface layer. This was followed by the laboratory simulation of the abrasion in the system of 'toothbrush - various suspensions of the tooth-pastes - hard tooth tissue (or material standard - ivory)' in specially designed device - the dentoabrasion meter. The activities of the tissue surface measured before and after abrasion were used for calculations of the relative drop of the surface activity. On this basis the influence of various tooth-pastes containing various abrasive substances was determined. (author)

  3. Air-propelled abrasive grit can damage the perennial weed, quackgrass, Elytrigia repens (L.) Nevski

    Science.gov (United States)

    New techniques are needed to control quackgrass in organic crops. With greater than or equal to 2 applications of abrasive air-propelled (800 kPa) corncob grit to 15 cm tall quackgrass tillers, regrowth was minimal at 5 weeks after treatment. Abrasive grits may be effective tools to help manage pere...

  4. Thermal annealing and ionic abrasion in ZnTe

    International Nuclear Information System (INIS)

    Bensahel, D.

    1975-01-01

    Thermal annealing of the ZnTe crystal is studied first in order to obtain information on the aspect of the penetration profile. Ionic abrasion is then investigated to find out whether it produces the same effects as ionic implantation, especially for luminescence [fr

  5. Assessment of mechanical and three-body abrasive wear peculiarity ...

    Indian Academy of Sciences (India)

    directional fabric reinforcement offers a unique solution for ... showed good performance to the three-body abrasive wear. .... plied by the Pioneer Chemical Company, Delhi, India. ..... Theoretical and measured densities of composites, along.

  6. Turning of wood plastic composites by water jet and abrasive water jet

    OpenAIRE

    Hutyrová, Z.; Ščučka, J. (Jiří); Hloch, S. (Sergej); Hlaváček, P. (Petr); Zeleňák, M. (Michal)

    2015-01-01

    The paper deals with the verification of suitability of water jet and abrasive water jet application for the disintegration of rotating samples of wood plastic composites (WPCs) with diameter d=36 mm. The influence of selected technological factors (traverse speed of cutting head v [mm/ min] and size of abrasive particles [MESH]) on the topography of resulting surfaces has in particular been studied. Surface topography and quality have been assessed using the methods of optical and co...

  7. Monitoring of the Abrasion Processes (by the Example of Alakol Lake, Republic of Kazakhstan)

    Science.gov (United States)

    Abitbayeva, Ainagul; Valeyev, Adilet; Yegemberdiyeva, Kamshat; Assylbekova, Aizhan; Ryskeldieva, Aizhan

    2016-01-01

    The purpose of the study is to analyze the abrasion processes in the regions of dynamically changing Alakol lake shores. Using the field method, methods of positioning by the GPS receiver and interpretation of remote sensing data, the authors determined that abrasion processes actively contributed to the formation the modern landscape, causing the…

  8. Gingival abrasion and recession in manual and oscillating-rotating power brush users.

    Science.gov (United States)

    Rosema, N A M; Adam, R; Grender, J M; Van der Sluijs, E; Supranoto, S C; Van der Weijden, G A

    2014-11-01

    To assess gingival recession (GR) in manual and power toothbrush users and evaluate the relationship between GR and gingival abrasion scores (GA). This was an observational (cross-sectional), single-centre, examiner-blind study involving a single-brushing exercise, with 181 young adult participants: 90 manual brush users and 91 oscillating-rotating power brush users. Participants were assessed for GR and GA as primary response variables. Secondary response variables were the level of gingival inflammation, plaque score reduction and brushing duration. Pearson correlation was used to describe the relationship between number of recession sites and number of abrasions. Prebrushing (baseline) and post-brushing GA and plaque scores were assessed and differences analysed using paired tests. Two-sample t-test was used to analyse group differences; ancova was used for analyses of post-brushing changes with baseline as covariate. Overall, 97.8% of the study population had at least one site of ≥1 mm of gingival recession. For the manual group, this percentage was 98.9%, and for the power group, this percentage was 96.7% (P = 0.621). Post-brushing, the power group showed a significantly smaller GA increase than the manual group (P = 0.004); however, there was no significant correlation between number of recession sites and number of abrasions for either group (P ≥ 0.327). Little gingival recession was observed in either toothbrush user group; the observed GR levels were comparable. Lower post-brushing gingival abrasion levels were seen in the power group. There was no correlation between gingival abrasion as a result of brushing and the observed gingival recession following use of either toothbrush. © 2014 The Authors International Journal of Dental Hygiene Published by John Wiley & Sons Ltd.

  9. Assessment of Rail Seat Abrasion Patterns and Environment

    Science.gov (United States)

    2012-05-01

    Rail seat abrasion (RSA) of concrete ties is manifested by the loss of material under the rail seat area and, in extreme cases, results in loss of rail clip holding power, reverse rail cant, and gauge widening. RSA was measured in several curves on t...

  10. Improvement of finishing antifriction treatment without abrasive of the rubbing parts surfaces of agricultural machineries

    Directory of Open Access Journals (Sweden)

    I.V. Shepelenk

    2014-06-01

    Full Text Available The wear of machines and mechanisms after rubbing is a major concern. The costs of manufacturing and restoration parts for agricultural machinery are enormous such as the trunnions pinions of hydraulic pumps. Finishing treatment antifriction without abrasive (FTAA is the existing method of manufacturing and restoration, but it has disadvantages like low work efficiency and the frequent replacement of the instrument. That is why a new method of FTAA parts type ''tree'' has been developed called vibratory finishing treatment antifriction without abrasive, (VFTAA method. The study was conducted at the laboratory of the State Technical University of Kirovograd (Ukraine where turn 16K20, the profilograph-profilometer "Talysurf-5", the scanning electron microscope REM-106I, friction machine MI-1M and the stand KI-28097-02M were used respectively for machining, study of micro relief before and after the VFTAA, microstructure, wear resistance and the determination of the break-in period of parts. The results showed that the VFTAA helped reduce the roughness Ra of the samples studied by half compared to the samples processed by polishing and 1.3 times compared to those treated with the FTAA, the break-in period has been reduced four times , this leads to an increase in the life of the hydraulic pump. This technology can be recommended for manufacturing and repair of hydraulic units of agricultural machineries.

  11. Desenvolvimento de um conector de cisalhamento em chapa dentada para estruturas mistas de aço e concreto e estudo do seu comportamento

    OpenAIRE

    Gustavo de Souza Verissimo

    2007-01-01

    Este trabalho consiste do desenvolvimento de um conector de cisalhamento em chapa dentada para estruturas mistas de aço e concreto, incluindo o estudo do seu comportamento. O trabalho envolve uma ampla investigação para definição da geometria do conector, um programa experimental, o desenvolvimento de uma equação de resistência e o treinamento de redes neurais para a predição da resposta do conector. O programa experimental, envolvendo 41 ensaios tipo push-out, conforme a EN 1994-1-1:2004, fo...

  12. Meios e fins do desenvolvimento para Celso Furtado

    Directory of Open Access Journals (Sweden)

    Fabio Antonio de Campos

    2014-10-01

    Full Text Available O objetivo desse artigo é expor o conceito de desenvolvimento para Celso Furtado. Para tanto, nos interessa apresentar o desenvolvimento nacional como um fim em sua abordagem sobre a formação social brasileira Para atingir tal estágio, os meios para o autor seriam assegurados por um típico desenvolvimento capitalista. Dentro dessa problemática, mostraremos também o alcance e os limites dessa concepção para o caráter dependente e subdesenvolvido do capitalismo brasileiro.

  13. O desafio político do desenvolvimento sustentado

    OpenAIRE

    Guimarães,Roberto P.

    1995-01-01

    A unanimidade que hoje parece haver em favor do desenvolvimento sustentado contrasta com a ausência de iniciativas políticas significativas para transformar as instituições econômicas, sociais e políticas que estão comprometidas com o estilo vigente de desenvolvimento. Em particular, há uma patente contradição entre o discurso antiestatista hegemônico e as exigências do desenvolvimento sustentado, que incluem um Estado ainda mais forte, em suas capacidades reguladoras e de planificação, que o...

  14. Abrasive wear behaviour of bio-active glass ceramics containing ...

    Indian Academy of Sciences (India)

    Unknown

    Technical Education Faculty, Mersin University, 33480 Tarsus, Turkey. MS received 18 October 2005; revised 22 March 2006. Abstract. In this study, abrasive ... process were used to produce bio-active ceramics. Fracture toughness of studied ...

  15. New decontamination techniques: chemical gels, electropolishing and abrasives

    International Nuclear Information System (INIS)

    Brunel, G.; Gauchon, J.P.; Kervegant, Y.; Josso, F.

    1991-01-01

    The decommissioning of nuclear installations requires decontamination techniques that are efficient, simple to apply and producing a small amount of wastes, which are easy to process. With a view to this, three decontamination methods, which appear to be particularly suited to decommissioning, have been studied. These three methods are: - spraying of gels carrying chemical decontaminating agents, - electropolishing with a swab device, - abrasives blasting. After parametric tests on non-radioactive and active samples, the industrial application of these methods in the dismantling of installations was studied. These industrial applications concern: - decontamination of pieces coming from the German BWR ISAR by immersion and gel spraying, - decontamination, mainly by gel spraying, and dismantling of the BRENNILIS bituminisation plant, - decontamination of part of the cooling circuit of the graphite gas reactor G2 by gel spraying, - decontamination of a component of the FBR SuperPhenix, using dry abrasives blasting. During the first three applications, generated secondary wastes volume and form were determined. 33 tabs., 16 figs., 12 refs

  16. Topographical anomaly on surfaces created by abrasive waterjet

    Czech Academy of Sciences Publication Activity Database

    Hloch, S.; Valíček, Jan

    2012-01-01

    Roč. 59, 5-8 (2012), s. 593-604 ISSN 0268-3768 Institutional research plan: CEZ:AV0Z30860518 Keywords : abrasive waterjet * initial zone * surface topography Subject RIV: JQ - Machines ; Tools Impact factor: 1.205, year: 2012 http://www.springerlink.com/content/5701144k76v02372

  17. Effect of denture cleaning on abrasion resistance and surface topography of polymerized CAD CAM acrylic resin denture base.

    Science.gov (United States)

    Shinawi, Lana Ahmed

    2017-05-01

    The application of computer-aided design computer-aided manufacturing (CAD CAM) technology in the fabrication of complete dentures, offers numerous advantages as it provides optimum fit and eliminates polymerization shrinkage of the acrylic base. Additionally, the porosity and surface roughness of CAD CAM resins is less compared to conventionally processed resins which leads to a decrease in the adhesion of bacteria on the denture base, which is associated with many conditions including halitosis and aspiration pneumonia in elderly denture wearers. To evaluate the influence of tooth brushing with dentifrices on CAD CAM resin blocks in terms of abrasion resistance, surface roughness and scanning electron photomicrography. This experimental study was carried out at the Faculty of Dentistry of King Abdulaziz University during 2016. A total of 40 rectangular shaped polymerized CAD CAM resin samples were subjected to 40.000 and 60.000 brushing strokes under a 200-gram vertical load simulating three years of tooth brushing strokes using commercially available denture cleaning dentifrice. Data were analyzed by SPSS version 20, using descriptive statistics and ANOVA. ANOVA test revealed a statistical significant weight loss of CAD CAM acrylic resin denture base specimens following 40.000 and 60.000 brushing strokes as well as a statistical significant change (p=0.0.5) in the surface roughness following brushing. The CAD CAM resin samples SEM baseline imaging revealed a relatively smooth homogenous surface, but following 40,000 and 60,000 brushing strokes, imaging displayed the presence of small scratches on the surface. CAD CAM resin displayed a homogenous surface initially with low surface roughness that was significantly affected following simulating three years of manual brushing, but despite the significant weight loss, the findings are within the clinically acceptable limits.

  18. The use of abrasive polishing and laser processing for developing polyurethane surfaces for controlling fibroblast cell behaviour

    Energy Technology Data Exchange (ETDEWEB)

    Irving, Michael; Murphy, Mark F; Lilley, Francis; French, Paul W; Burton, David R [General Engineering Research Institute, Liverpool John Moores University, Liverpool, L3 3AF (United Kingdom); Dixon, Simon [Biomer Technology LTD, 10 Seymour Court, Tudor Road, Manor Park, Runcorn, Cheshire, WA7 1SY (United Kingdom); Sharp, Martin C [General Engineering Research Institute, Liverpool John Moores University, Liverpool, L3 3AF (United Kingdom)

    2017-02-01

    Studies have shown that surfaces having micro and nano-scale features can be used to control cell behaviours including; cell proliferation, migration and adhesion. The aim of this work was to compare the use of laser processing and abrasive polishing to develop micro/nano-patterned polyurethane substrates for controlling fibroblast cell adhesion, migration and proliferation. Laser processing in a directional manner resulted in polyurethane surfaces having a ploughed field effect with micron-scale features. In contrast, abrasive polishing in a directional and random manner resulted in polyurethane surfaces having sub-micron scale features orientated in a linear or random manner. Results show that when compared with flat (non-patterned) polymer, both the laser processed and abrasive polished surface having randomly organised features, promoted significantly greater cell adhesion, while also enhancing cell proliferation after 72 h. In contrast, the abrasive polished surface having linear features did not enhance cell adhesion or proliferation when compared to the flat surface. For cell migration, the cells growing on the laser processed and abrasively polished random surface showed decreased levels of migration when compared to the flat surface. This study shows that both abrasive polishing and laser processing can be used to produce surfaces having features on the nano-scale and micron-scale, respectively. Surfaces produced using both techniques can be used to promote fibroblast cell adhesion and proliferation. Thus both methods offer a viable alternative to using lithographic techniques for developing patterned surfaces. In particular, abrasive polishing is an attractive method due to it being a simple, rapid and inexpensive method that can be used to produce surfaces having features on a comparable scale to more expensive, multi-step methods. - Highlights: • Abrasive polishing can generate nano-scratches on stainless steel to cast polymer films for cell

  19. The use of abrasive polishing and laser processing for developing polyurethane surfaces for controlling fibroblast cell behaviour

    International Nuclear Information System (INIS)

    Irving, Michael; Murphy, Mark F; Lilley, Francis; French, Paul W; Burton, David R; Dixon, Simon; Sharp, Martin C

    2017-01-01

    Studies have shown that surfaces having micro and nano-scale features can be used to control cell behaviours including; cell proliferation, migration and adhesion. The aim of this work was to compare the use of laser processing and abrasive polishing to develop micro/nano-patterned polyurethane substrates for controlling fibroblast cell adhesion, migration and proliferation. Laser processing in a directional manner resulted in polyurethane surfaces having a ploughed field effect with micron-scale features. In contrast, abrasive polishing in a directional and random manner resulted in polyurethane surfaces having sub-micron scale features orientated in a linear or random manner. Results show that when compared with flat (non-patterned) polymer, both the laser processed and abrasive polished surface having randomly organised features, promoted significantly greater cell adhesion, while also enhancing cell proliferation after 72 h. In contrast, the abrasive polished surface having linear features did not enhance cell adhesion or proliferation when compared to the flat surface. For cell migration, the cells growing on the laser processed and abrasively polished random surface showed decreased levels of migration when compared to the flat surface. This study shows that both abrasive polishing and laser processing can be used to produce surfaces having features on the nano-scale and micron-scale, respectively. Surfaces produced using both techniques can be used to promote fibroblast cell adhesion and proliferation. Thus both methods offer a viable alternative to using lithographic techniques for developing patterned surfaces. In particular, abrasive polishing is an attractive method due to it being a simple, rapid and inexpensive method that can be used to produce surfaces having features on a comparable scale to more expensive, multi-step methods. - Highlights: • Abrasive polishing can generate nano-scratches on stainless steel to cast polymer films for cell

  20. High temperature resistant cermet and ceramic compositions

    Science.gov (United States)

    Phillips, W. M. (Inventor)

    1978-01-01

    Cermet compositions having high temperature oxidation resistance, high hardness and high abrasion and wear resistance, and particularly adapted for production of high temperature resistant cermet insulator bodies are presented. The compositions are comprised of a sintered body of particles of a high temperature resistant metal or metal alloy, preferably molybdenum or tungsten particles, dispersed in and bonded to a solid solution formed of aluminum oxide and silicon nitride, and particularly a ternary solid solution formed of a mixture of aluminum oxide, silicon nitride and aluminum nitride. Also disclosed are novel ceramic compositions comprising a sintered solid solution of aluminum oxide, silicon nitride and aluminum nitride.

  1. CONHECIMENTO: UM FATOR DE DESENVOLVIMENTO ORGANIZACIONAL

    Directory of Open Access Journals (Sweden)

    Adilson dos Santos Morais

    2017-09-01

    Full Text Available Cada vez mais, criar conhecimento útil para atuar em uma posição de vantagem competitiva, orientado para o desenvolvimento organizacional e valorizando o capital humano tem-se demonstrato uma estratégia eficaz. O presente artigo busca apresentar a importância do conhecimento para o desenvolvimento das organizações em âmbito geral com destaque para as comunidades de prática. Esse conhecimento é derivado das interações desenvolvidas em processos de aprendizagem que ocorrem no ambiente organizacional. Para este, realizou-se um estudo teórico, descritivo, que tem como procedimento a pesquisa bibliográfica. Deste modo, apresenta como resultado deste trabalho a evidência de que existem poucos resultados divulgados sobre retorno financeiro e os benefícios dos investimentos realizados no capital intelectual humano pelas organizações. Porém, o conhecimento agrega valor à organização aumentando o valor do capital intelectual e as literaturas sobre o conhecimento e desenvolvimento organizacional consideram o capital intelectual o fator chave para a melhoria nos sistemas estratégicos. Destaca-se que esta contribuição poderá instigar cada vez mais a criação de conhecimento como fator de reconhecimento humano e de desenvolvimento das organizações.

  2. Design and tailoring of Ni-Sn-W composites for bonded abrasive applications

    Energy Technology Data Exchange (ETDEWEB)

    Kourtoukova, G.L.; Demetry, C.; Biederman, R.R. [Worcester Polytechnic Inst., MA (United States). Materials Science and Engineering Program; Ramanath, S.; Andrews, R.M.; Jacobs, D.S. [Saint-Gobain/Norton Company, Worcester, MA (United States)

    2000-01-15

    The combination of properties ideal for metal bonds in abrasive products can rarely be achieved in a monolithic material. This research demonstrates a successful approach for producing a composite bond with higher elastic modulus without a significant increase in wear resistance, by taking advantage of the reaction between matrix and reinforcement to produce intermetallics. Composites comprised of a Ni-Sn matrix with continuous W fiber and/or W powder dispersoid were prepared by powder metallurgy methods. Composite specimens densified by hot pressing were characterized with a combination of scanning electron microscopy (SEM) and energy dispersive X-ray (EDX) analyses, measurements of wear resistance, and measurements of Young's modulus and hardness by both bulk and nanoindentation methods. A significant stiffening effect was observed; the elastic modulus of the composites was up to 30% greater than that predicted by a rule of mixtures based on the moduli of the unreacted fiber and matrix constituents alone. As desired, the wear resistance of the composite was approximately equal to that of the Ni-Sn matrix. One contribution to this combination of properties is believed to be the high elastic moduli and likely low fracture toughness of the Ni-W and Ni-Sn intermetallics that are formed. Properties of the Ni-Sn-W composites are contrasted with those of a Ni-Sn matrix reinforced with WC particulate, where no reaction occurs at the interface. (orig.)

  3. Comparação dos valores de desgaste abrasivo e de microdureza de 13 resinas compostas usadas em odontologia através do método do disco retificado Comparing abrasive wear and microhardness of 13 dental composite resins

    Directory of Open Access Journals (Sweden)

    Eduardo C. Bianchi

    2007-06-01

    Full Text Available Atualmente tem-se buscado simplificar a tarefa de caracterização da vida útil de restaurações dentárias realizadas por resinas compostas através de métodos laboratoriais, que são mais rápidos e não sofrem influência de variáveis pessoais inerentes às análises clínicas. Com este propósito, este trabalho apresenta uma nova metodologia de ensaio laboratorial para a avaliação do desgaste abrasivo de resinas compostas através do método do disco retificado. Realizaram-se ensaios de resistência ao desgaste abrasivo com 13 resinas compostas odontológicas e buscou-se analisar o comportamento da resistência ao desgaste abrasivo em relação à microdureza dessas resinas. Com a análise dos resultados concluiu-se que o método de discos retificados é eficiente para a obtenção da resistência ao desgaste abrasivo. Notou-se também ser extremamente pequeno o nível de correlação entre microdureza e desgaste abrasivo o que indica que cada resina composta tem características próprias e que o desgaste é dependente também de outros fatores.It is now commonplace to search for methods to assess the useful lifetime of dental restorations made of resins, which are quicker and less subjective than clinical analyses. With this purpose, this work presents a new methodology based on the grinding disk for evaluating the abrasive wear of composed resins. Resistance tests to the abrasive wear were made with 13 composed resins used as dental material, and a comparison was done with the hardness of those resins. From the data analysis, we concluded that the method of rectified disks is efficient for obtaining the resistance to the abrasive wear. Furthermore, the correlation between hardness and abrasive wear was very small, which indicates that each composed resin has its own characteristics and that the wear also depends on other factors.

  4. Desenvolvimento e sociologia: uma aproximação necessária

    Directory of Open Access Journals (Sweden)

    Alessandro André Leme

    2015-08-01

    Full Text Available ResumoO debate acerca do desenvolvimento na América Latina e no Brasil em particular revelou-se como um dos temas proeminentes do pensamento sociopolítico e econômico brasileiro. As interpretações do Brasil a partir da temática do desenvolvimento ganham força a partir da década de 1930, porém, será após a Segunda Guerra Mundial, com a intensificação da industrialização e a modernização da sociedade capitalista brasileira, que o tema adquire centralidade na sociologia/ciência política. Por outro lado, as discussões acerca do Estado e do desenvolvimento estão intimamente ligadas ao desenvolvimento do capitalismo brasileiro, ou seja, configura uma tríade que simultaneamente evidencia tanto um tipo historicamente determinado de Estado como um tipo particular de desenvolvimento econômico e social do país. O desenvolvimento do Brasil caracteriza-se por um embate entre o mercado e o Estado, sendo a influência desse último fundante para o padrão de desenvolvimento pretendido no país. Propomos a análise do processo de desenvolvimento como forma de revisitar o debate teórico e conceitual produzido sobre a temática no país, assim como investigar o movimento histórico, econômico e político adotado pelo Brasil como estratégia para o desenvolvimento nos anos 1990.

  5. 29 CFR 1926.303 - Abrasive wheels and tools.

    Science.gov (United States)

    2010-07-01

    ... 29 Labor 8 2010-07-01 2010-07-01 false Abrasive wheels and tools. 1926.303 Section 1926.303 Labor Regulations Relating to Labor (Continued) OCCUPATIONAL SAFETY AND HEALTH ADMINISTRATION, DEPARTMENT OF LABOR... freely on the spindle and shall not be forced on. The spindle nut shall be tightened only enough to hold...

  6. Numerical study of agglomerate abrasion in a tumbling mixer

    NARCIS (Netherlands)

    Thanh Nguyen, [No Value; Willemsz, Tofan; Frijlink, Henderik; Maarschalk, Kees van der Voort

    2014-01-01

    A numerical simulation using the Discrete Element Method (DEM) was performed to investigate the phenomena concerning the abrasion and breakage of agglomerates in a diffusion powder mixer. Agglomerates were created by defining a single structure of particles with bonds of different strengths using

  7. Release of particles by abrasion of CNT composites using a belt sander

    International Nuclear Information System (INIS)

    Matsui, Yasuto; Nobuyuki, Kato; Ishibashi, Tomonori; Nagaya, Taiki; Yoneda, Minoru

    2017-01-01

    There have been many reports on the effect of exposure to nanomaterials such as titanium dioxide, silver, and carbon nanotube (CNT) on human health. Several experiments have examined the abrasion of CNT composites, in which CNT nanoparticles are embedded within a resin or rubber matrix, yielding varying results. Separate study of free CNTs and CNT nanoparticles in relation to health is important due to the different physicochemical characteristics of the two types of material. This study investigated the abrasion of CNT composites using a belt sander inside an enclosed chamber, with variation in the applied load and belt sander speed. At lower speeds, the population of particles with diameters of ∼100 nm was observed to increase (cf. mode values of ∼10 nm), and we found a relationship between the amount of the raising dust and the abrasion conditions. From these results, we propose a robust and widely applicable method to create particles of nanomaterial-containing composite materials of various types in order to conduct accelerated exposure assessment studies. (paper)

  8. Abrasion Testing of Products Containing Nanomaterials, SOP-R-2: Scientific Operating Procedure Series: Release (R)

    Science.gov (United States)

    2016-04-01

    Nanotechnologies -- Terminology and definitions for nano-objects -- Nanoparticle, nanofibre and nanoplate Definitions Abrasion - wearing away...ER D C SR -1 6- 2 Environmental Consequences of Nanotechnologies Abrasion Testing of Products Containing Nanomaterials, SOP-R-2...ERDC online library at http://acwc.sdp.sirsi.net/client/default. Environmental Consequences of Nanotechnologies ERDC SR-16-2 April 2016

  9. Effect of Bioactive Glass air Abrasion on Shear Bond Strength of Two Adhesive Resins to Decalcified Enamel.

    Directory of Open Access Journals (Sweden)

    Alireza Eshghi

    2014-12-01

    Full Text Available Bioactive glass air abrasion is a conservative technique to remove initial decalcified tissue and caries. This study examined the shear bond strength of composite resin to sound and decalcified enamel air-abraded by bioactive glass (BAG or alumina using etch-and-rinse and self-etch adhesives.Forty-eight permanent molars were root-amputated and sectioned mesiodistally. The obtained 96 specimens were mounted in acrylic resin; the buccal and lingual surfaces remained exposed. A demineralizing solution was used to decalcify half the specimens. Both sound and decalcified specimens were divided into two groups of alumina and bioactive glass air abrasion. In each group, the specimens were subdivided into two subgroups of Clearfil SE Bond or OptiBond FL adhesives (n=12. Composite resin cylinders were bonded on enamel surfaces cured and underwent thermocycling. The specimens were tested for shear bond strength. Data were analyzed using SPSS 16.0 and three-way ANOVA (α=0.05. Similar to the experimental groups, the enamel surface of one specimen underwent SEM evaluation.No significant differences were observed in composite resin bond strength subsequent to alumina or bioactive glass air abrasion preparation techniques (P=0.987. There were no statistically significant differences between the bond strength of etch-and-rinse and self-etch adhesive groups (P=1. Also, decalcified or intact enamel groups had no significant difference (P=0.918. However, SEM analysis showed much less enamel irregularities with BAG air abrasion compared to alumina air abrasion.Under the limitations of this study, preparation of both intact and decalcified enamel surfaces with bioactive glass air abrasion results in similar bond strength of composite resin in comparison with alumina air abrasion using etch-&-rinse or self-etch adhesives.

  10. Effect of Bioactive Glass air Abrasion on Shear Bond Strength of Two Adhesive Resins to Decalcified Enamel

    Science.gov (United States)

    Eshghi, Alireza; Khoroushi, Maryam; Rezvani, Alireza

    2014-01-01

    Objective: Bioactive glass air abrasion is a conservative technique to remove initial decalcified tissue and caries. This study examined the shear bond strength of composite resin to sound and decalcified enamel air-abraded by bioactive glass (BAG) or alumina using etch-and-rinse and self-etch adhesives. Materials and Methods: Forty-eight permanent molars were root-amputated and sectioned mesiodistally. The obtained 96 specimens were mounted in acrylic resin; the buccal and lingual surfaces remained exposed. A demineralizing solution was used to decalcify half the specimens. Both sound and decalcified specimens were divided into two groups of alumina and bioactive glass air abrasion. In each group, the specimens were subdivided into two subgroups of Clearfil SE Bond or OptiBond FL adhesives (n=12). Composite resin cylinders were bonded on enamel surfaces cured and underwent thermocycling. The specimens were tested for shear bond strength. Data were analyzed using SPSS 16.0 and three-way ANOVA (α=0.05). Similar to the experimental groups, the enamel surface of one specimen underwent SEM evaluation. Results: No significant differences were observed in composite resin bond strength subsequent to alumina or bioactive glass air abrasion preparation techniques (P=0.987). There were no statistically significant differences between the bond strength of etch-and-rinse and self-etch adhesive groups (P=1). Also, decalcified or intact enamel groups had no significant difference (P=0.918). However, SEM analysis showed much less enamel irregularities with BAG air abrasion compared to alumina air abrasion. Conclusion: Under the limitations of this study, preparation of both intact and decalcified enamel surfaces with bioactive glass air abrasion results in similar bond strength of composite resin in comparison with alumina air abrasion using etch-&-rinse or self-etch adhesives. PMID:25628694

  11. Investigating selective transport and abrasion on an alluvial fan using quantitative grain size and shape analysis

    Science.gov (United States)

    Litwin, K. L.; Jerolmack, D. J.

    2011-12-01

    Selective sorting and abrasion are the two major fluvial processes that are attributed to the downstream fining of sediments in rivers and alluvial fans. Selective transport is the process by which smaller grains are preferentially transported downstream while larger grains are deposited closer to the source. Abrasion is defined by the production of fine sediments and sand that occurs by saltation of gravel, where particle-to-particle collisions supply the energy required to break apart grains. We hypothesize that abrasion results in the gradual fining of large grains and the production of fine sands and silts, while sorting accounts for the differences in transport of these two grain-size fractions produced from abrasion, thereby creating the abrupt gravel-sand transition observed in many channel systems. In this research, we explore both selective transport and abrasion processes on the Dog Canyon alluvial fan near Alamogordo, New Mexico. We complete an extensive grain size analysis down the main channel of the fan employing an image-based technique that utilizes an autocorrelation process. We also characterize changes in grain shape using standard shape parameters, as well as Fourier analysis, which allows the study of contributions of grain roughness on a variety of length scales. Sorting appears to dominate the upper portion of the fan; the grain-size distribution narrows moving downstream until reaching a point of equal mobility, at which point sorting ceases. Abrasion exerts a subtle but persistent effect on grains during transport down the fan. Shape analysis reveals that particles become more rounded by the removal of small-scale textural features, a process that is expected to only modestly influence grain size of gravel, but should produce significant quantities of sand. This study provides a better understanding of the importance of grain abrasion and sorting on the downstream fining of channel grains in an alluvial fan, as well as an improved knowledge

  12. Sliding-gate valve for use with abrasive materials

    Science.gov (United States)

    Ayers, Jr., William J.; Carter, Charles R.; Griffith, Richard A.; Loomis, Richard B.; Notestein, John E.

    1985-01-01

    The invention is a flow and pressure-sealing valve for use with abrasive solids. The valve embodies special features which provide for long, reliable operating lifetimes in solids-handling service. The valve includes upper and lower transversely slidable gates, contained in separate chambers. The upper gate provides a solids-flow control function, whereas the lower gate provides a pressure-sealing function. The lower gate is supported by means for (a) lifting that gate into sealing engagement with its seat when the gate is in its open and closed positions and (b) lowering the gate out of contact with its seat to permit abrasion-free transit of the gate between its open and closed positions. When closed, the upper gate isolates the lower gate from the solids. Because of this shielding action, the sealing surface of the lower gate is not exposed to solids during transit or when it is being lifted or lowered. The chamber containing the lower gate normally is pressurized slightly, and a sweep gas is directed inwardly across the lower-gate sealing surface during the vertical translation of the gate.

  13. Study on mineral processing technology for abrasive minerals

    Energy Technology Data Exchange (ETDEWEB)

    Hong, Seong Woong; Yang, Jung Il; Hwang, Seon Kook; Choi, Yeon Ho; Cho, Ken Joon; Shin, Hee Young [Korea Inst. of Geology Mining and Materials, Taejon (Korea, Republic of)

    1995-12-01

    Buyeo Materials in Buyeogun, Choongnam province is a company producing feldspar concentrate, but does not yet utilize the garnet as abrasive material and other useful heavy minerals wasted out from the process of feldspar ore. The purpose of this study is to develop technology and process for the recovery of garnet concentrate. As results, the garnet is defined as ferro manganese garnet. The optimum process for recovery of garnet concentrate is to primarily concentrate heavy minerals from tailings of feldspar processing. And secondly the heavy minerals concentrated is dried and separated garnet concentrate from other heavy minerals. At this time, the garnet concentrate is yield by 0.176%wt from 0.31%wt of heavy minerals in head ore. The garnet concentrate contains 33.35% SiO{sub 2}, 12.20% Al{sub 2}O{sub 3}, 28.47% Fe{sub 2}O{sub 3}, 11.96% MnO. As for utilization of abrasive materials, a fundamental data was established on technology of grinding and classification. (author). 13 refs., 47 figs., 24 tabs.

  14. CONTROL SYSTEM EVALUATION AND IMPLEMENTATION FOR THE ABRASIVE MACHINING PROCESS ON WOOD

    Directory of Open Access Journals (Sweden)

    Stephen Jackson

    2011-06-01

    Full Text Available Continuous process improvement and automation have proven to be powerful tools for the wood processing industries in order to obtain better final product quality and thus increase profits. Abrasive machining represents an important and relevant process in the manufacturing and processing of wood products, which also implies high cost of materials and labor; therefore, special attention to this process is necessary. The objective of this work was to evaluate and demonstrate a process control system for use in the abrasive machining of wood and wood-based products. A control system was created on LabView® to integrate the monitoring process and the actions required, depending on the abrasive machining process conditions. The system acquires information from the optical sensor to detect loading and activate the cleaning system. The system continuously monitors the condition of the abrasive belt (tool wear by using an acoustic emission sensor and alerts the operator of the status of the belt (green, yellow, and red lights indicating satisfactory, medium, and poor belt condition. The system also incorporates an additional safety device, which helps prevent permanent damage to the belt, equipment, or workpiece by alerting the operator when an excessive temperature has been reached. The process control system proved that automation permits enhancement in the consistency of the belt cleaning technique by the elimination of the human errors. Furthermore, this improvement also affects the cost by extending the life of the belt, which reduces setup time, belt cost, operation cost, as well as others.

  15. CERVEJA ARTESANAL E DESENVOLVIMENTO REGIONAL EM SANTA CATARINA (BRASIL)

    OpenAIRE

    Valdinho Pellin; Oklinger Mantovaneli Jr.

    2016-01-01

    Discussões relacionadas ao fortalecimento do desenvolvimento regional tem estimulado um debate em relação a contribuições que Indicações Geográficas (IGs) podem oferecer ao desenvolvimento. IGs se constituem em elemento de identificação de produtos ou serviços com seus territórios e podem oferecer contribuições importantes para o desenvolvimento regional, agregando valor aos produtos, facilitando o acesso a novos mercados e valorizando tradições locais. Este artigo procura discutir a importân...

  16. Numerical Simulation Analysis of Five-Step Variable-Diameter Pipe with Solid-Liquid Two-Phase Abrasive Flow Polishing

    Science.gov (United States)

    Li, Junye; Zhang, Hengfu; Wu, Guiling; Hu, Jinglei; Liu, Yang; Sun, Zhihui

    2018-01-01

    In many areas of precision machining abrasive flow polishing technology has an important role. In order to study the influence of abrasive flow on the polishing effect of variable diameter parts, the fifth step variable diameter tube was taken as the research object to analyze the dynamic pressure and turbulent kinetic energy distribution of inlet velocity on the fifth-order variable diameter tube influences. Through comparative analysis, the abrasive flow polished variable diameter pipe parts have very effective and significant polishing effect and the higher the inlet speed, the more significant the polishing effect.

  17. Controlled wear of vitrified abrasive materials for precision grinding ...

    Indian Academy of Sciences (India)

    R. Narasimhan (Krishtel eMaging) 1461 1996 Oct 15 13:05:22

    2Machining Research Group, Department of Engineering, University of ... ods are applied to analyse the cutting mechanism in grinding. .... (d) Chemical reaction between abrasive and workpiece material at elevated temperatures ... most common method used for measuring wear flat area employs an optical, or an electron.

  18. Turning of materials with high-speed abrasive waterjet

    Czech Academy of Sciences Publication Activity Database

    Sitek, Libor; Hlaváček, Petr

    -, October 2016 (2016), s. 1160-1165 ISSN 1805-0476 R&D Projects: GA MŠk ED2.1.00/03.0082; GA MŠk(CZ) LO1406 Institutional support: RVO:68145535 Keywords : abrasive water jet machining * turning * steel * rock * wood Subject RIV: JQ - Machines ; Tools http://www.mmscience.eu/content/file/archives/MM_Science_201692.pdf

  19. Examination of Wetting by Liquid Zinc of Steel Sheets Following Various Kinds of Abrasive Blasting

    Directory of Open Access Journals (Sweden)

    Cecotka M.

    2016-06-01

    Full Text Available Abrasive blasting is one of the methods of surface working before hot-dip zinc-coating. It allows not only to remove products of corrosion from the surface, but it also affects the quality of the zinc coating applied later, thereby affecting wettability of surface being zinc-coated. The surface working can be done with different types of abrasive material.

  20. Safety of stationary grinding machines - impact resistance of work zone enclosures.

    Science.gov (United States)

    Mewes, Detlef; Adler, Christian

    2017-09-01

    Guards on machine tools are intended to protect persons from being injured by parts ejected with high kinetic energy from the work zone of the machine. Stationary grinding machines are a typical example. Generally such machines are provided with abrasive product guards closely enveloping the grinding wheel. However, many machining tasks do not allow the use of abrasive product guards. In such cases, the work zone enclosure has to be dimensioned so that, in case of failure, grinding wheel fragments remain inside the machine's working zone. To obtain data for the dimensioning of work zone enclosures on stationary grinding machines, which must be operated without an abrasive product guard, burst tests were conducted with vitrified grinding wheels. The studies show that, contrary to widely held opinion, narrower grinding wheels can be more critical concerning the impact resistance than wider wheels although their fragment energy is smaller.

  1. Rede de Protagonismo Local para o Desenvolvimento Global

    DEFF Research Database (Denmark)

    Weber, Ángela; Hermann, Roberto Rivas

    Este artigo pretende fazer uma reflexão sobre metodologia a ser desenvolvida e utilizada num projeto de desenvolvimento local, através das ações protagonizadas pela própria comunidade. Para isso parte de uma discussão sobre o conceito de desenvolvimento sustentável, e a seguir propõe a busca de f...

  2. Abrasive wear behaviour of bio-active glass ceramics containing ...

    Indian Academy of Sciences (India)

    In this study, abrasive wear behaviour of bio-active glass ceramic materials produced with two different processes is studied. Hot pressing process and conventional casting and controlled crystallization process were used to produce bio-active ceramics. Fracture toughness of studied material was calculated by fracture ...

  3. Improving the Wear Resistance of Moulds for the Injection of Glass Fibre–Reinforced Plastics Using PVD Coatings: A Comparative Study

    Directory of Open Access Journals (Sweden)

    Francisco Silva

    2017-02-01

    Full Text Available It is well known that injection of glass fibre–reinforced plastics (GFRP causes abrasive wear in moulds’ cavities and runners. Physical vapour deposition (PVD coatings are intensively used to improve the wear resistance of different tools, also being one of the most promising ways to increase the moulds’ lifespan, mainly when used with plastics strongly reinforced with glass fibres. This work compares four different thin, hard coatings obtained using the PVD magnetron sputtering process: TiAlN, TiAlSiN, CrN/TiAlCrSiN and CrN/CrCN/DLC. The first two are monolayer coatings while the last ones are nanostructured and consist of multilayer systems. In order to carry out the corresponding tribological characterization, two different approaches were selected: A laboratorial method, using micro-abrasion wear tests based on a ball-cratering configuration, and an industrial mode, analysing the wear resistance of the coated samples when inserted in a plastic injection mould. As expected, the wear phenomena are not equivalent and the results between micro-abrasion and industrial tests are not similar due to the different means used to promote the abrasion. The best wear resistance performance in the laboratorial wear tests was attained by the TiAlN monolayer coating while the best performance in the industrial wear tests was obtained by the CrN/TiAlCrSiN nanostructured multilayer coating.

  4. An investigation of two-body abrasive wear of laser processed surfaces

    International Nuclear Information System (INIS)

    Abass, G.

    1995-01-01

    This paper reports two body abrasive wear studies of alloy and composite deposits produced with a 2 kW continuous wave CO/sub 2/ laser. Stellite alloy 6, Alloy 4815, Stainless steel and SiC powders were used to produce alloy and composite deposits on an En 3b mild steel substrate. The cladding material was injected into the laser produced melt pool by means of a pneumatic powder delivery system. In the present studies instead of using the conventional pin-on-disc method of wear measurement, a more realistic and practical wear testing procedure was adopted. The wear testing machine used was capable of measuring wear of three comparatively larger (30 x 30 x 10 mm) clad samples by abrading simultaneously against a revolving alumina disc. A comparative study of microstructure, hardness and wear of alloy and composite clads was made. The clad deposits were found sound and continuous. The hardness and wear resistance of the composites were markedly higher than that of the alloy clads. (author) 9 figs

  5. Da revolução verde ao discurso do PRONAF: a representação do desenvolvimento nas políticas públicas de desenvolvimento rural no Brasil

    Directory of Open Access Journals (Sweden)

    Michell Leonard Duarte de Lima Tolentino

    2016-12-01

    Full Text Available Este trabalho procura refletir acerca das várias representações de desenvolvimento que embasam algumas das políticas públicas de desenvolvimento rural no Brasil, partindo das representações de desenvolvimento subjacentes à Revolução Verde e focando, posteriormente, no discurso do Programa Nacional de Fortalecimento da Agricultura Familiar (PRONAF. O trabalho se embasa em uma ampla pesquisa bibliográfica e documental. De início abordamos o discurso do desenvolvimento de forma crítica, para logo depois atentarmos para a maneira como este coloca o espaço rural. Para tanto utilizamos autores como Esteva (2000, Escobar (2000, Santos (1979 e Montenegro Gómez (2006. Posteriormente analisamos a Revolução Verde “brasileira” compreendendo o fordismo enquanto seu principal modelo de desenvolvimento. Em seguida, partimos para uma reflexão mais profunda sobre o PRONAF. O PRONAF assume fundamental importância nesse trabalho, pois o entendemos enquanto uma política de extrema relevância para se ler esse momento de inflexão das políticas públicas para o campo, de mudança nas representações sobre o espaço rural e o desenvolvimento rural brasileiro. Ao nos determos no PRONAF, discutimos a mudança de um modelo de desenvolvimento fordista para um modelo de desenvolvimento flexível.

  6. Erosion and abrasion on dental structures undergoing at-home bleaching

    Directory of Open Access Journals (Sweden)

    Tarquinio SBC

    2011-07-01

    Full Text Available Flávio Fernando Demarco1, Sônia Saeger Meireles2, Hugo Ramalho Sarmento1, Raquel Venâncio Fernandes Dantas1, Tatiana Botero3, Sandra Beatriz Chaves Tarquinio11Graduate Program in Dentistry, School of Dentistry, Federal University of Pelotas, Brazil; 2Department of Operative Dentistry, Federal University of Paraíba, Brazil; 3Cariology, Restorative Science, and Endodontics Department, School of Dentistry, University of Michigan, MI, USAAbstract: This review investigates erosion and abrasion in dental structures undergoing at-home bleaching. Dental erosion is a multifactorial condition that may be idiopathic or caused by a known acid source. Some bleaching agents have a pH lower than the critical level, which can cause changes in the enamel mineral content. Investigations have shown that at-home tooth bleaching with low concentrations of hydrogen or carbamide peroxide have no significant damaging effects on enamel and dentin surface properties. Most studies where erosion was observed were in vitro. Even though the treatment may cause side effects like sensitivity and gingival irritation, these usually disappear at the end of treatment. Considering the literature reviewed, we conclude that tooth bleaching agents based on hydrogen or carbamide peroxide have no clinically significant influence on enamel/dentin mineral loss caused by erosion or abrasion. Furthermore, the treatment is tolerable and safe, and any adverse effects can be easily reversed and controlled.Keywords: peroxide, tooth bleaching, enamel, dentin, erosion, abrasion

  7. PROPOSTA TEÓRICO-CONCEITUAL DE DESENVOLVIMENTO EM ARRANJOS PRODUTIVOS LOCAIS

    Directory of Open Access Journals (Sweden)

    Adriana Valélia Saraceni

    2013-04-01

    Full Text Available O objetivo central deste trabalho foi evidenciar algumas ferramentas para o desenvolvimento da inovação e verificar a relação com a configuração do desenvolvimento em Arranjos Produtivos Locais (APLs. Esta pesquisa pode ser considerada como exploratória e descritiva, pois envolve levantamento bibliográfico e análise de exemplos que estimulem a compreensão. Estudos sobre ferramentas de inovação tecnológica e referencias do desenvolvimento de ecossistemas industriais, foram utilizados buscando demonstrar uma proposta teórico-conceitual de integração das ferramentas. Por meio do resultado obtido com a aplicação da metodologia e do referencial teórico, verificou-se que aplicação das ferramentas de inovação tecnológica e a operacionalização com a implantação de métodos e ações cooperadas, tende a fortalecer o desempenho do processo de inovação do arranjo produtivo. A aplicação do conceito de ecologia industrial no desenvolvimento ambientalmente sustentável do aglomerado tende a fortalecer não só o desenvolvimento do APL, como também o desenvolvimento econômico e regional.

  8. Hardness and elasticity of abrasive particles measured by instrumented indentation

    Czech Academy of Sciences Publication Activity Database

    Hvizdoš, P.; Zeleňák, Michal; Hloch, Sergej

    2016-01-01

    Roč. 8, č. 1 (2016), s. 869-871 ISSN 1805-0476 Institutional support: RVO:68145535 Keywords : abrasive * garnet * hardness * elasticity * instrumental indentation Subject RIV: JQ - Machines ; Tools http://www.mmscience.eu/content/file/archives/MM_Science_201601.pdf

  9. Metal segmenting using abrasive and reciprocating saws

    International Nuclear Information System (INIS)

    Allen, R.P.; Fetrow, L.K.; Haun, F.E. Jr.

    1987-06-01

    This paper evaluates a light-weight, high-power abrasive saw for segmenting radioactively contaminated metal components. A unique application of a reciprocating mechanical saw for the remote disassembly of equipment in a hot cell also is described. The results of this work suggest that use of these techniques for selected remote sectioning applications could minimize operational and access problems and be very cost effective in comparison with other inherently faster sectioning methods. 2 refs., 7 figs

  10. Adhesive interfaces of enamel and dentin prepared by air-abrasion at different distances

    International Nuclear Information System (INIS)

    Chinelatti, Michelle Alexandra; Andreolli do Amaral, Thais Helena; Borsatto, Maria Cristina; Palma-Dibb, Regina Guenka; Corona, Silmara Aparecida Milori

    2007-01-01

    The purpose of this study was to analyse, by scanning electron microscopy (SEM), the morphology of enamel and dentin/adhesive interfaces in cavities prepared by air-abrasion at different working distances. Thirty sound third human molars were selected and, on both their buccal and lingual surfaces, class V cavities were prepared by air-abrasion, at 2-, 4-, 6-, 8- and 10-mm working distances, or high-speed bur (control group). After preparation, all cavities were etched with 35% phosphoric acid gel and restored with Single Bond/Filtek Z-250. Buccal and lingual surfaces were separated and restorations sectioned in a buccolingual direction, providing two sections of each cavity, which were analysed by scanning electron microscopy. It was observed that the distances of 6 and 8 mm promoted more homogeneous dentin/adhesive interfaces, with tags formation, and more uniform for enamel, which were similar to the control group. It may be concluded that the air-abrasion working distance can influence the morphology of enamel and dentin/adhesive interfaces, and the intermediate distances provided better adhesive interfaces

  11. The effect of boriding on wear resistance of cold work tool steel

    International Nuclear Information System (INIS)

    Anzawa, Y; Koyama, S; Shohji, I

    2017-01-01

    Recently, boriding has attracted extensive attention as surface stiffening processing of plain steel. In this research, the influence of processing time on the formation layer of cold work tool steel (KD11MAX) by Al added fused salt bath was examined. In addition, in order to improve the abrasion resistance of KD11MAX, the effect of the treatment of boronization on the formation layer has been investigated. Boriding were performed in molten borax which contained about 10 mass% Al at processing time of 1.8 ∼ 7.2 ks (processing temperature of 1303 K). As a result of the examination, the hardness of the boriding layer becomes about 1900 HV when the processing time of 3.6 ks. Also the abrasion resistance has improved remarkably. Furthermore, it was revealed that the formation layer was boronized iron from the Vickers hardness and analysis of the X-ray diffraction measurement. (paper)

  12. Microstructure and abrasive wear properties of M(Cr,Fe7C3 carbides reinforced high-chromium carbon coating produced by gas tungsten arc welding (GTAW process

    Directory of Open Access Journals (Sweden)

    Soner BUYTOZ

    2010-01-01

    Full Text Available In the present study, high-chromium ferrochromium carbon hypereutectic alloy powder was coated on AISI 4340 steel by the gas tungsten arc welding (GTAW process. The coating layers were analyzed by optical microscopy, X-ray diffraction (XRD, field-emission scanning electron microscopy (FE-SEM, X-ray energy-dispersive spectroscopy (EDS. Depending on the gas tungsten arc welding pa-rameters, either hypoeutectic or hypereutectic microstructures were produced. Wear tests of the coatings were carried out on a pin-on-disc apparatus as function of contact load. Wear rates of the all coating layers were decreased as a function of the loading. The improvement of abrasive wear resistance of the coating layer could be attributed to the high hardness of the hypereutectic M7C3 carbides in the microstruc-ture. As a result, the microstructure of surface layers, hardness and abrasive wear behaviours showed different characteristics due to the gas tungsten arc welding parameters.

  13. Effects of different lasers and particle abrasion on surface characteristics of zirconia ceramics.

    Directory of Open Access Journals (Sweden)

    Sakineh Arami

    2014-04-01

    Full Text Available The aim of this study was to assess the surface of yttrium-stabilized tetragonal zirconia (Y-TZP after surface treatment with lasers and airborne-particle abrasion.First, 77 samples of presintered zirconia blocks measuring 10 × 10 × 2 mm were made, sintered and polished. Then, they were randomly divided into 11 groups (n=7 and received surface treatments namely, Er:YAG laser irradiation with output power of 1.5, 2 and 2.5 W, Nd:YAG laser with output power of 1.5, 2 and 2.5 W, CO2 laser with output power of 3, 4 and 5 W, AL2O3 airborne-particle abrasion (50μ and no treatment (controls. Following treatment, the parameters of surface roughness such as Ra, Rku and Rsk were evaluated using a digital profilometer and surface examination was done by SEM.According to ANOVA and Tukey's test, the mean surface roughness (Ra after Nd:YAG laser irradiation at 2 and 2.5 W was significantly higher than other groups. Roughness increased with increasing output power of Nd:YAG and CO2 lasers. Treated surfaces by Er:YAG laser and air abrasion showed similar surface roughness. SEM micrographs showed small microcracks in specimens irradiated with Nd:YAG and CO2 lasers.Nd:YAG laser created a rough surface on the zirconia ceramic with many microcracks; therefore, its use is not recommended. Air abrasion method can be used with Er:YAG laser irradiation for the treatment of zirconia ceramic.

  14. EXPERIMENTAL VERIFICATION OF THE MECHANICAL RESISTANCE OF FORENSIC MARKING BY MEANS SYNTHETIC DNA

    Directory of Open Access Journals (Sweden)

    Marek HÜTTER

    2017-06-01

    Full Text Available This article deals with experimental verification of resistance of forensic identification marks (microdots in combination with artificial DNA to property. It is considered mechanical abrasion from potential offender to remove or damage readability of marking and following identification. The aim of this work is to test the hypothesis that forensic marking can be completely removed by the process of mechanical abrasion without causing damages to a protected object. To fulfill this purpose it was designed and built a test equipment, where experiments were carried out to confirm or refute the above mentioned hypothesis.

  15. Mechanical and abrasive wear characterization of bidirectional and chopped E-glass fiber reinforced composite materials

    International Nuclear Information System (INIS)

    Siddhartha,; Gupta, Kuldeep

    2012-01-01

    Highlights: ► Bi-directional and chopped E-glass fiber reinforced epoxy composites are fabricated. ► Three body abrasive wear behavior of fabricated composites has been assessed. ► Results are validated against existing microscopic models of Lancaster and Wang. ► Tensile strength of bi-directional E-glass fiber reinforced composites increases. ► Chopped glass fiber composites are found better in abrasive wear situations. -- Abstract: Bi-directional and chopped E-glass fiber reinforced epoxy composites are fabricated in five different (15, 20, 25, 30 and 35) wt% in an epoxy resin matrix. The mechanical characterization of these composites is performed. The three body abrasive wear behavior of fabricated composites has been assessed under different operating conditions. Abrasive wear characteristics of these composites are successfully analysed using Taguchi’s experimental design scheme and analysis of variance (ANOVA). The results obtained from these experiments are also validated against existing microscopic models of Ratner-Lancaster and Wang. It is observed that quite good linear relationships is held between specific wear rate and reciprocal of ultimate strength and strain at tensile fracture of these composites which is an indicative that the experimental results are in fair agreement with these existing models. Out of all composites fabricated it is found that tensile strength of bi-directional E-glass fiber reinforced composites increases because of interface strength enhancement. Chopped glass fiber reinforced composites are observed to perform better than bi-directional glass fiber reinforced composites under abrasive wear situations. The morphology of worn composite specimens has been examined by scanning electron microscopy (SEM) to understand about dominant wear mechanisms.

  16. Abrasive water jet cutting technique for biological shield concrete dismantlement

    International Nuclear Information System (INIS)

    Konno, T.; Narazaki, T.; Yokota, M.; Yoshida, H.; Miura, M.; Miyazaki, Y.

    1987-01-01

    The Japan Atomic Energy Research Institute (JAERI) is developing the abrasive-water jet cutting system to be applied to dismantling the biological shield walls of the JPDR as a part of the reactor dismantling technology development project. This is a total system for dismantling highly activated concrete. The concrete biological shield wall is cut into blocks by driving the abrasive-water jet nozzle, which is operated with a remote, automated control system. In this system, the concrete blocks are removed to a container, while the slurry and dust/mist which are generated during cutting are collected and treated, both automatically. It is a very practical method and will quite probably by used for actual dismantling of commercial power reactors in the future because it can minimize workers' exposure to radioactivity during dismantling, contributes to preventing diffusion of radiation, and reduces the volume of contaminated secondary waste

  17. Wear Resistant Thermal Sprayed Composite Coatings Based on Iron Self-Fluxing Alloy and Recycled Cermet Powders

    Directory of Open Access Journals (Sweden)

    Heikki SARJAS

    2012-03-01

    Full Text Available Thermal spray and WC-Co based coatings are widely used in areas subjected to abrasive wear. Commercial  cermet thermal spray powders for HVOF are relatively expensive. Therefore applying these powders in cost-sensitive areas like mining and agriculture are hindered. Nowadays, the use of cheap iron based self-fluxing alloy powders for thermal spray is limited. The aim of this research was to study properties of composite powders based on self-fluxing alloys and recycled cermets and to examine the properties of thermally sprayed (HVOF coatings from composite powders based on iron self-fluxing alloy and recycled cermet powders (Cr3C2-Ni and WC-Co. To estimate the properties of  recycled cermet powders, the sieving analysis, laser granulometry and morphology were conducted. For deposition of coatings High Velocity Oxy-Fuel spray was used. The structure and composition of powders and coatings were estimated by SEM and XRD methods. Abrasive wear performance of coatings was determined and compared with wear resistance of coatings from commercial powders. The wear resistance of thermal sprayed coatings from self-fluxing alloy and recycled cermet powders at abrasion is comparable with wear resistance of coatings from commercial expensive spray powders and may be an alternative in tribological applications in cost-sensitive areas.DOI: http://dx.doi.org/10.5755/j01.ms.18.1.1338

  18. Micro-scale abrasive wear behavior of medical implant material Ti-25Nb-3Mo-3Zr-2Sn alloy on various friction pairs.

    Science.gov (United States)

    Wang, Zhenguo; Huang, Weijiu; Ma, Yanlong

    2014-09-01

    The micro-scale abrasion behaviors of surgical implant materials have often been reported in the literature. However, little work has been reported on the micro-scale abrasive wear behavior of Ti-25Nb-3Mo-3Zr-2Sn (TLM) titanium alloy in simulated body fluids, especially with respect to friction pairs. Therefore, a TE66 Micro-Scale Abrasion Tester was used to study the micro-scale abrasive wear behavior of the TLM alloy. This study covers the friction coefficient and wear loss of the TLM alloy induced by various friction pairs. Different friction pairs comprised of ZrO2, Si3N4 and Al2O3 ceramic balls with 25.4mm diameters were employed. The micro-scale abrasive wear mechanisms and synergistic effect between corrosion and micro-abrasion of the TLM alloy were investigated under various wear-corrosion conditions employing an abrasive, comprised of SiC (3.5 ± 0.5 μm), in two test solutions, Hanks' solution and distilled water. Before the test, the specimens were heat treated at 760°C/1.0/AC+550°C/6.0/AC. It was discovered that the friction coefficient values of the TLM alloy are larger than those in distilled water regardless of friction pairs used, because of the corrosive Hanks' solution. It was also found that the value of the friction coefficient was volatile at the beginning of wear testing, and it became more stable with further experiments. Because the ceramic balls have different properties, especially with respect to the Vickers hardness (Hv), the wear loss of the TLM alloy increased as the ball hardness increased. In addition, the wear loss of the TLM alloy in Hanks' solution was greater than that in distilled water, and this was due to the synergistic effect of micro-abrasion and corrosion, and this micro-abrasion played a leading role in the wear process. The micro-scale abrasive wear mechanism of the TLM alloy gradually changed from two-body to mixed abrasion and then to three-body abrasion as the Vickers hardness of the balls increased. Copyright

  19. Effect of Volume Fraction of Particle on Wear Resistance of Al2O3/Steel Composites at Elevated Temperature

    Institute of Scientific and Technical Information of China (English)

    BAO Chong-gao; WANG En-ze; GAO Yi-min; XING Jian-dong

    2005-01-01

    Based on previous work,abrasive wear resistance of Al2 O3/steel composites with different Al2 O3 parti cle volume fraction (VOF) at 900 C was investigated.The experimental results showed that a suitable particle VOF is important to protect the metal matrix from wear at elevated temperature.Both too high and too low particle VOF lead to a poor abrasive wear because a bulk matrix is easily worn off by grits when it exceeds the suitable VOF and also because when VOF is low,the Al2O3 particles are easily dug out by grits during wearing as well.When the particle VOF is 39%,the wear resistance of tested composites is excellent.

  20. Wear resistance of TiB/sub 2/-Fe cermets

    International Nuclear Information System (INIS)

    Champagne, B.; Dallaire, S.

    1985-01-01

    A material which consists of TiB/sub 2/ dispersed in an iron matrix was synthesized by the exothermic reaction of ferrotitanium and boron. The as-reacted products were hot isostatically pressed to produce TiB/sub 2/-Fe cermets. The influence of HIP variables on the density and total fractional porosity of specimens is presented. Density above 95% is obtained by HIPping at temperatures below 1300 0 C. Increasing the temperature and the time of HIPping enhance the mechanical properties and wear resistance of TiB/sub 2/-Fe cermets by reducing their residual porosity. Relations obtained by regression analysis showed that the porosity strongly affects the properties of parts. Regression analysis point out that the wear loss of a 5% porosity TiB/sub 2/-Fe cermet is 270% higher than a dense HIPped cermet. Low stress and high stress abrasion resistance tests utilizing various abrasive media were carried out on dense HIPped cermets and results were compared with those obtained from WC-Co cermets and 1020 steel

  1. Wear-resistance of Aluminum Matrix Microcomposite Materials

    Directory of Open Access Journals (Sweden)

    M. Kandeva

    2011-03-01

    Full Text Available A procedure is developed for the study of wear of aluminum alloys AlSi7 obtained by casting, reinforced by TiC microparticles, before and after heat treatment. Tribological study is realized under conditions of friction on counterbody with fixed abrasive. Experimental results were obtained for mass wear, wear rate, wear intensity and wear-resistance of the alloys with different wt% of microparticles.

  2. Effect of pressing temperature on the wear resistance of a Co-based Cr-Mo powder alloy produced by hot pressing

    Energy Technology Data Exchange (ETDEWEB)

    Somunkiran, Ilyas [Firat Univ., Elazig (Turkey). Metallurgical and Materials Engineering Dept.; Balin, Ahmet [Siirt Univ. (Turkey). Dept. of Vocational High School

    2016-02-01

    In this study, Co-based Cr-Mo powder alloy was produced at different pressing temperatures by using hot pressing technique and abrasive wear behaviors of the produced specimens were examined. Produced specimens were exposed to abrasive wear experiment using block on disc wear test device by applying a load of 50 N with 100-mesh SiC abrasive paper. Each specimen was investigated at 25, 50, 75 and 100 m. At the end of the experiment, abrasive wear results of the specimens were determined by calculating their mass losses. Microstructural properties of the specimens which were produced at different pressing temperatures were investigated by optical and SEM examinations and their wear resistances were examined by abrasive wear experiments. Consequently, it was observed that in Co-based Cr-Mo powder alloy produced by hot pressing technique; as sintering temperature increased, size of neck formations between the powder grains increased, porosity decreased and abrasive wear resistance increased. [German] In diesem Beitrag zugrunde liegenden Studie wurde eine Co-basierte Cr-Mo-Legierung mittels Heisspressens hergestellt und der Abrasivverschleisswiderstand dieser Proben untersucht. Die hergestellten Proben wurden dem Abrasivverschleissversuch durch einen Block-Scheibe-Versuchsaufbau unterzogen, wobei eine Kraft von 50 N mit einem SiC-Papier (100 mesh) verwendet wurde. Jede Probe wurde ueber eine Distanz von 25, 50, 75 und 100 m untersucht. Am Ende der jeweiligen Experimente wurden die Abrasivverschleissergebnisse ermittelt, indem die Massenverluste berechnet wurden. Die mikrostrukturellen Eigenschaften der Proben, die bei verschiedenen Presstemperaturen hergestellt wurden, wurden mittels optischer und Rasterelektronenmikroskopie bestimmt und ihr Verschleisswiderstand anhand der Verschleissversuche ermittelt. Schliesslich wurde beobachtet, dass bei steigender Sintertemperatur der heissgespressten Co-basierten Cr-Mo-Pulverlegierung die Groesse der Einschnuerungen zwischen den

  3. Development and assessment of two decontamination processes: closed electropolishing system for decontamination of underwater surfaces -vibratory decontamination with abrasives

    International Nuclear Information System (INIS)

    Benavides, E.; Fajardo, M.

    1992-01-01

    Two decontamination processes have been developed to decontaminate the stainless steel components of nuclear power plants. The first process uses an underwater closed electropolishing system for the decontamination of large stainless steel surfaces in flooded systems without loss of electrolyte. Large underwater contaminated areas can be treated with an electropolishing head covering an area of 2 m 2 in one step. The decontamination factors achieved with this technique range between 100 and 1000. The second process consists in the decontamination of nuclear components using vibratory equipment with self-cleaning abrasives generating a minimum quantity of waste. This technique may reach contamination factors similar to those obtained with other abrasive methods (brush abrasion, abrasive blasting, etc...). The obtained decontamination factors range between 5 and 50. Only a small quantity of waste is generated, which is treated and reduced in volume by filtration and evaporation

  4. The model of the dependence of the abrasive wear value on the maximal linear wear

    Directory of Open Access Journals (Sweden)

    О.А. Вишневський

    2004-01-01

    Full Text Available  The relation of the contact area of the rubber roll with a sample and the maximal linear wear value is found. The mathematical model of the dependence of the wear volume weight value on the maximal dimple depth is presented with the friction on abrasive particles fixed nonrigidly. The relation of volume weight wear with the rubber roll contact surface area with a sample with the friction on abrasive particles fixed nonrigidly is established.

  5. Testing of abrasion materials

    International Nuclear Information System (INIS)

    Hummert, G.

    1983-01-01

    A method of abrasion testing according to ASTM C 704-76 a is presented for steel fibre concrete mortar, fusion-cast basalt and a surface coating material and results of practical interest are mentioned. Due to the high technical demands on these materials and their specific fields of application, the very first test already supplied interesting findings. From the user's point of view, the method is an interesting alternative to the common test methods, e.g. according to DIN 52 108 (wheel test according to Boehme). In English-speaking countries, testing according to ASTM is often mandatory in the refractory industry in order to assure constant quality of refractory materials after setting. The method is characterized by good comparability and high accuracy of measurement. Only the test piece is exchanged while the test conditions remain constant, so that accurate information on the material studied is obtained. (orig.) [de

  6. O conceito histórico de desenvolvimento econômico

    OpenAIRE

    Pereira, Luiz C. Bresser

    2006-01-01

    Uma Análise do Conceito de Desenvolvimento Econômico. o Crescimento Econômico, ou Desenvolvimento Econômico, é Visto como um Fenômeno Histórico como Resultado da Revolução Capitalista, E, Consequentemente, da Revolução Comercial, da Industrial E, no Meio Delas, da Revolução Nacional. Assim, é Necessário um Conceito Histórico de Crescimento Econômico, e não um Conceito Normativo. Visto sob este Aspecto, o Desenvolvimento Econômico é Intrinsecamente Relacionado ao Surgimento do Estado-Nação M...

  7. Superficial characterization of titanium league when submitted to abrasive blasting

    International Nuclear Information System (INIS)

    Suzuki, L.Y.; Leite, I.V.; Szesz, E.M.; Siqueira, C.J.M.

    2010-01-01

    Commercially pure titanium and some of its alloys exhibit a good biocompatibility. These characteristics are frequently used in the manufacture of orthopedic and dental implants. It is possible to modify its surface making it the bioactive using various methods, such as deposition of hydroxyapatite by plasma spray and increasing the roughness of the surface by abrasive blasting. This work is to modify the surface of titanium alloy Ti6Al4V ELI (ASTM F136: 02a) for abrasive blasting and study the morphology, crystallographic phases and the mechanical characteristics of the surface obtained. For such purpose, SEM images, diffraction of X-rays and tests of risk produced by nanoindenter. The sandblasting was done using alumina powder and blasting time of 6s. The morphology of the surfaces of Ti6Al4V ELI changed after sandblasting with increased roughness. It is possible to conclude that after sandblasting the titanium surface do not have a ductile behavior. (author)

  8. Determinantes do desenvolvimento do setor agropecuário nos municípios

    Directory of Open Access Journals (Sweden)

    Caio César de Medeiros Costa

    2013-06-01

    Full Text Available Dada a importância do setor agropecuário para a economia brasileira, é fundamental conhecer os fatores determinantes do desenvolvimento agropecuário em seus municípios. Sob a luz de referencial teórico que aborda questões relacionadas aos fatores determinantes do desenvolvimento agropecuário e do desenvolvimento econômico local, neste estudo fez-se uso das metodologias de análise multivariada conhecidas como análise fatorial e análise de cluster. Utilizou-se o estado de Minas Gerais como recorte analítico. Foram selecionadas 22 variáveis para cada município, representando diferentes dimensões do desenvolvimento, visando verificar quais os fatores determinantes do desenvolvimento agropecuário. Após a análise fatorial, optou-se pela extração de seis fatores com raiz característica maior do que um e que respondem, em conjunto, por 62,25% da variância total dos dados: desenvolvimento econômico, investimento público, qualidade de vida, condições da atividade agropecuária, condições de meio ambiente e consumo, e condições de financiamento. Pela análise de cluster, foram criados cinco grupos, de acordo com o desempenho dos membros nos fatores. Os resultados corroboram os apontamentos literários em quase sua totalidade e, além disso, destaca-se e discute-se a existência de um ciclo positivo gerado pelo incremento dos fatores determinantes do desenvolvimento agropecuário e pelas vantagens competitivas. Neste estudo, aponta-se a importância do investimento público na promoção do desenvolvimento, reforçando o proposto por trabalhos anteriores de que o Estado desempenha papel fundamental para garantir condições que propiciem o desenvolvimento do setor agropecuário. Outra constatação factível é a de que fatores isolados, tais como as boas condições da agricultura e do meio ambiente, não são capazes de propiciar desenvolvimento para o setor nos municípios mineiros.

  9. Effects of Rare Earth Metal Addition on Wear Resistance of Chromium-Molybdenum Cast Steel

    Directory of Open Access Journals (Sweden)

    Kasinska J.

    2017-09-01

    Full Text Available This paper discusses changes in the microstructure and abrasive wear resistance of G17CrMo5-5 cast steel modified with rare earth metals (REM. The changes were assessed using scanning microscopy. The wear response was determined in the Miller test to ASTM G75. Abrasion tests were supplemented with the surface profile measurements of non-modified and modified cast steel using a Talysurf CCI optical profilometer. It was demonstrated that the modification substantially affected the microstructure of the alloy, leading to grain size reduction and changed morphology of non-metallic inclusions. The observed changes in the microstructure resulted in a three times higher impact strength (from 33 to 99 kJ/cm2 and more than two times higher resistance to cracking (from 116 to 250 MPa. The following surface parameters were computed: Sa: Arithmetic mean deviation of the surface, Sq: Root-mean-square deviation of the surface, Sp: Maximum height of the peak Sv: Maximum depth of the valley, Sz: Ten Point Average, Ssk: Asymmetry of the surface, Sku: Kurtosis of the surface. The findings also indicated that the addition of rare earth metals had a positive effect on the abrasion behaviour of G17CrMo5-5 cast steel.

  10. Achievement report for fiscal 1998. Research and development of super-functional environment-resistant materials by controlling trace metal ion implantation; 1998 nendo seika hokokusho. Gokubiryo kinzoku ion chunyu seigyo ni yoru chokino taikankyo zairyo no kenkyu kaihatsu

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    1999-03-01

    The aim was to develop reliable materials high in resistance to hostile environments, greatly improved in their resistance to oxidation, abrasion, and corrosion at high temperatures. To achieve the goal, trace quantities of high melting point metals were implanted into the compound formed on the substrate surface or deep into the substrate material. This year's research and development is outlined below. Important technologies in the ion process involved materials which at high temperatures were very resistant to oxidation, abrasion, and corrosion. The high-temperature oxidation resistant material was studied for use with the automobile supercharger rotor. The study on the high-temperature abrasion resistant material involved Ti-N thin coatings: the optimization of coating conditions, slidability at room temperature, and slidability in a high-temperature atmosphere. As for the high-temperature corrosion resistant material, studies were made to use it for refuse-fueled power generation. The TiAl material was also studied: the effect of ion implantation on the improvement of its high-temperature oxidation resisting capability, analysis into oxidized alloy surface properties, ion implantation into complicatedly shaped items and the optimum material for them, and the surface treatment by ion beams for improving resistance to high-temperature corrosion. (NEDO)

  11. Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives: Synthesis and the effects on chemical mechanical polishing (CMP) performances of sapphire wafers

    Energy Technology Data Exchange (ETDEWEB)

    Liu, Tingting; Lei, Hong, E-mail: hong_lei2005@aliyun.com

    2017-08-15

    Highlights: • The novel Nd{sup 3+}-doped colloidal SiO{sub 2} abrasives were synthesized by seed-introduced method. • The Nd{sup 3+}-doped colloidal SiO{sub 2} abrasives exhibited lower Ra and higher MRR on sapphire during CMP. • The cores SiO{sub 2} were coated by the shells (SiO{sub 2}, Nd{sub 2}Si{sub 2}O{sub 7} and Nd(OH){sub 3}) via chemical bonds and hydrogen bonds. • XPS analysis revealed the solid-state chemical reaction between Nd{sup 3+}-doped colloidal SiO{sub 2} abrasives and sapphire during CMP. - Abstract: Abrasive is one of the most important factors in chemical mechanical polishing (CMP). In order to improve the polishing qualities of sapphire substrates, the novel Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives were prepared by seed-induced growth method. In this work, there were a series of condensation reactions during the synthesis process of Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives and the silica cores were coated by shells (which contains SiO{sub 2}, Nd{sub 2}Si{sub 2}O{sub 7} and Nd(OH){sub 3}) via chemical bonds and hydrogen bonds in the Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives, which made the composite abrasives’ core-shell structure more sTable Scanning electron microscopy (SEM) showed that Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives were spherical and uniform in size. And the acting mechanisms of Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives on sapphire in CMP were investigated. Time-of-flight secondary ion mass spectroscopy (TOF-SIMS) analysis and X-ray photoelectron spectroscopy (XPS) analysis demonstrated that the solid-state chemical reactions between the shells (which contained SiO{sub 2}, Nd{sub 2}Si{sub 2}O{sub 7} and Nd(OH){sub 3}) of Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives and the sapphire occurred during the CMP process. Furthermore, Nd{sup 3+}-doped colloidal SiO{sub 2} composite abrasives exhibited lower surface roughness and

  12. Small-Scale Morphological Features on a Solid Surface Processed by High-Pressure Abrasive Water Jet

    Directory of Open Access Journals (Sweden)

    Can Kang

    2013-08-01

    Full Text Available Being subjected to a high-pressure abrasive water jet, solid samples will experience an essential variation of both internal stress and physical characteristics, which is closely associated with the kinetic energy attached to the abrasive particles involved in the jet stream. Here, experiments were performed, with particular emphasis being placed on the kinetic energy attenuation and turbulent features in the jet stream. At jet pressure of 260 MPa, mean velocity and root-mean-square (RMS velocity on two jet-stream sections were acquired by utilizing the phase Doppler anemometry (PDA technique. A jet-cutting experiment was then carried out with Al-Mg alloy samples being cut by an abrasive water jet. Morphological features and roughness on the cut surface were quantitatively examined through scanning electron microscopy (SEM and optical profiling techniques. The results indicate that the high-pressure water jet is characterized by remarkably high mean flow velocities and distinct velocity fluctuations. Those irregular pits and grooves on the cut surfaces indicate both the energy attenuation and the development of radial velocity components in the jet stream. When the sample is positioned with different distances from the nozzle outlet, the obtained quantitative surface roughness varies accordingly. A descriptive model highlighting the behaviors of abrasive particles in jet-cutting process is established in light of the experimental results and correlation analysis.

  13. Small-Scale Morphological Features on a Solid Surface Processed by High-Pressure Abrasive Water Jet.

    Science.gov (United States)

    Kang, Can; Liu, Haixia

    2013-08-14

    Being subjected to a high-pressure abrasive water jet, solid samples will experience an essential variation of both internal stress and physical characteristics, which is closely associated with the kinetic energy attached to the abrasive particles involved in the jet stream. Here, experiments were performed, with particular emphasis being placed on the kinetic energy attenuation and turbulent features in the jet stream. At jet pressure of 260 MPa, mean velocity and root-mean-square (RMS) velocity on two jet-stream sections were acquired by utilizing the phase Doppler anemometry (PDA) technique. A jet-cutting experiment was then carried out with Al-Mg alloy samples being cut by an abrasive water jet. Morphological features and roughness on the cut surface were quantitatively examined through scanning electron microscopy (SEM) and optical profiling techniques. The results indicate that the high-pressure water jet is characterized by remarkably high mean flow velocities and distinct velocity fluctuations. Those irregular pits and grooves on the cut surfaces indicate both the energy attenuation and the development of radial velocity components in the jet stream. When the sample is positioned with different distances from the nozzle outlet, the obtained quantitative surface roughness varies accordingly. A descriptive model highlighting the behaviors of abrasive particles in jet-cutting process is established in light of the experimental results and correlation analysis.

  14. Abrasive wear mechanisms and surface layer structure of refractory materials after mechanical working

    International Nuclear Information System (INIS)

    Milman, Y.V.; Lotsko, D.V.

    1989-01-01

    The mechanisms of abrasive wear and surface layer structure formation after different kinds of mechanical working are considered in terms of fracture and plastic deformation mechanisms for various refractory materials. The principles for classification of abrasive wear mechanisms are proposed, the four types of wear mechanisms are distinguished for various combinations of fractures and plastic deformation types. The concept of characteristic deformation temperature t * (knee temperature) is used. Detailed examples are given of investigating the surface layer structures in grinded crystals of sapphire and molybdenum. The amorphisation tendency of the thinnest surface layer while mechanical polishing is discussed separately. 19 refs., 11 figs., 2 tabs. (Author)

  15. Development of in-situ ZrC reinforced iron based composites for wear resistance applications

    International Nuclear Information System (INIS)

    Bandyopadhyay, T.K.; Das, K.

    2002-01-01

    A common objective behind the processing of iron-based composites is to improve the wear resistance of steels by incorporating some reinforcing phases, e.g., carbides and oxides. In the present investigation, iron-based zirconium carbide reinforced composite is produced by the aluminothermic reduction of zircon sand (ZrSiO 4 ) and blue dust (Fe 2 O 3 ) in the presence of carbon. Aluminothermic reduction of blue dust and zircon sand, being highly exothermic in nature, essentially leads to a self-propagating high-temperature synthesis (SHS) of the Fe-ZrC composite. The as-cast composite is characterized by scanning electron microscopy (SEM) and X-ray diffraction (XRD). The mechanical properties of the composite and the effect of heat treatment on the microstructure are evaluated. The composite possess sufficient hardness and promising abrasive wear resistance property. The abrasive wear resistance property of the Fe-ZrC composite is compared with that of a M2 grade tool material and it is found to be better than the tool material. The composite also possess good high temperature stability. (author)

  16. A study on practical use of underwater abrasive water jet cutting

    Science.gov (United States)

    Yamaguchi, Hitoshi; Demura, Kenji

    1993-09-01

    The practicality of underwater abrasive water jet cutting technology was studied in experiments. A study of abrasives in slurried form showed that optimum polymer concentration can be selected to suit underwater conditions. For the long-distance transport of slurry from the ocean surface to the ocean floor, a direct supply system by hose proved to be practical. This system takes advantage of the insolubility of the slurry in water due to a difference in specific gravity. For cutting thick steel plate at great ocean depths, a simulation with a pressurized container revealed the requirements for actual cutting. Confirmation of remote cutting operations will become the most important technology in field applications. Underwater sound vibration characteristics were found to change significantly in direct response to modifications in cutting conditions. This will be important basic data to develop an effective sensoring method.

  17. The measurement of the velocity of abrasive particlesat the suction part of the cutting head

    Czech Academy of Sciences Publication Activity Database

    Foldyna, Josef; Zeleňák, Michal; Klich, Jiří; Hlaváček, Petr; Sitek, Libor; Říha, Zdeněk

    2015-01-01

    Roč. 22, č. 6 (2015), s. 1441-1446 ISSN 1330-3651. [Vodní paprsek 2013 - výzkum, vývoj, aplikace. Soláň, Karolinka, 22.10.2013-24.10.2013] R&D Projects: GA MŠk ED2.1.00/03.0082; GA MŠk(CZ) LO1406 Institutional support: RVO:68145535 Keywords : abrasive water jet * velocity of abrasive particles * shadowgraphy Subject RIV: JQ - Machines ; Tools Impact factor: 0.464, year: 2015 http://www.tehnicki-vjesnik.com/web/public/archive

  18. A família e a escola como contextos de desenvolvimento humano

    Directory of Open Access Journals (Sweden)

    Maria Auxiliadora Dessen

    2007-04-01

    Full Text Available Escola e família constituem dois contextos de desenvolvimento fundamentais para a trajetória de vida das pessoas. Neste artigo, são destacadas as contribuições destes contextos para a promoção do desenvolvimento humano, enfatizando suas implicações nos processos evolutivos. Questões sobre configurações, vínculos familiares e a importância da rede social de apoio para o desenvolvimento da família são discutidas. Focalizam-se as funções da escola, considerando sua influência nas pessoas em desenvolvimento. Apontam-se algumas considerações sobre a necessidade de compreender as inter-relações entre escola e família, visando facilitar a aprendizagem e desenvolvimento humano. A integração entre esses dois contextos é destacada como desafio para a prática profissional e pesquisa empírica.

  19. Valores e Desenvolvimento Humano

    NARCIS (Netherlands)

    F. Comim (Flavio); A. Macedo de Jesus (Anderson); R.C.B Oliveira (Raissa); A. Davison (Anna); S. Galeno (Sabrina); A.C.V. Ribeiro (Ana)

    2010-01-01

    markdownabstractA primeira parte desse Relatório de Desenvolvimento Humano do Brasil 2009/2010 começa com a descrição de um amplo processo de consulta aberta à sociedade, denominada Brasil Ponto a Ponto, para a escolha do tema do relatório. A Campanha Brasil Ponto a Ponto teve por objetivo

  20. Randomized Controlled Trial to Explore the Effect of Experimental Low Abrasivity Dentifrices on Enamel Gloss and Smoothness, and the Build-up of Extrinsic Tooth Stain.

    Science.gov (United States)

    Milleman, Kimberly R; Milleman, Jeffery L; Young, Sarah; Parkinson, Charles

    2017-06-01

    To evaluate and compare examiner-assessed changes in enamel gloss, extrinsic dental stain, and surface smoothness following one, two, four, and eight weeks of twice-daily use of an experimental low abrasivity desensitizing dentifrice (relative dentin abrasivity [RDA] ~40) containing 5% sodium tripolyphosphate (STP) chemical cleaning agent and 1% aluminum trioxide abrasive. This was compared with an ultra-low abrasivity dentifrice (5% STP only; RDA ~13), a moderate abrasivity fluoride dentifrice (RDA ~80), and a higher abrasivity marketed whitening dentifrice (RDA ~142). This was a single-center, examiner-blind, randomized, controlled, parallel group study in healthy adults stratified by gloss score and age. Following a washout period with a conventional silica abrasive dentifrice, subjects received a dental scale and polish and were randomized to treatment. Subjects brushed their teeth for two minutes, twice daily, with their assigned dentifrice. Enamel gloss was assessed visually by comparing the facial surfaces of the maxillary incisors to the Sturzenberger gloss standards. Extrinsic dental stain was measured on the 12 anterior teeth (facial and lingual) using the Macpherson modification of the Lobene Stain Index (MLSI). Tooth smoothness was assessed using scanning electron microscope (SEM) analysis of a silicone impression of the central incisors. Of 120 screened subjects, 95 were randomized to the study. Subjects using the low abrasivity aluminum trioxide/STP dentifrice demonstrated statistically significant (p tooth smoothness, at Week 8, statistically significant increases in surface smoothness were observed for most treatment groups compared to baseline (p tooth gloss compared to a non-alumina ultra-low abrasivity STP-containing dentifrice, and moderate and high abrasivity dentifrices, over an eight-week period.

  1. Preparando um ambiente de desenvolvimento para a plataforma android

    Directory of Open Access Journals (Sweden)

    Felipe Pires de Oliveira

    2015-11-01

    Full Text Available Este artigo descreve as etapas para a criação de um ambiente de desenvolvimento para a plataforma Android. O artigo foi dividido em quatro partes: Primeiro uma introdução sobre o assunto. Na segunda seção são mostrados os passos necessários para a configuração do ambiente de desenvolvimento. Na terceira seção, é demonstrado como criar uma aplicação para dispositivo Android que calculo Índice de Massa Corporal (IMC. A quarta seção apresenta as considerações finais. A solução abordada tem como base a IDE Eclipse e o SDK do Android, bem como o Kit de Desenvolvimento Java da Oracle (JDK.

  2. Preparando um ambiente de desenvolvimento para a plataforma android

    Directory of Open Access Journals (Sweden)

    Felipe Pires de Oliveira

    2015-12-01

    Full Text Available Este artigo descreve as etapas para a criação de um ambiente de desenvolvimento para a plataforma Android. O artigo foi dividido em quatro partes: Primeiro uma introdução sobre o assunto. Na segunda seção são mostrados os passos necessários para a configuração do ambiente de desenvolvimento. Na terceira seção, é demonstrado como criar uma aplicação para dispositivo Android que calculo Índice de Massa Corporal (IMC. A quarta seção apresenta as considerações finais. A solução abordada tem como base a IDE Eclipse e o SDK do Android, bem como o Kit de Desenvolvimento Java da Oracle (JDK.

  3. Air abrasion experiments in U-Pb dating of zircon

    Science.gov (United States)

    Goldich, S.S.; Fischer, L.B.

    1986-01-01

    Air abrasion of zircon grains can remove metamict material that has lost radiogenic Pb and zircon overgrowths that were added during younger events and thereby improve the precision of the age measurements and permit closer estimates of the original age. Age discordance that resulted from a single disturbance of the U-Pb isotopic decay systems, as had been demonstrated by T.E. Krogh, can be considerably reduced, and, under favorable conditions, the ages brought into concordancy. Two or more events complicate the U-Pb systematics, but a series of abrasion experiments can be helpful in deciphering the geologic history and in arriving at a useful interpretation of the probable times of origin and disturbances. In east-central Minnesota, U.S.A., Penokean tonalite gneiss is dated at 1869 ?? 5 Ma, and sheared granite gneiss is shown to have been a high-level granite intrusion at 1982 ?? 5 Ma in the McGrath Gneiss precursor. Tonalite gneiss and a mafic granodiorite in the Rainy Lake area, Ontario, Canada, are dated at 2736 ?? 16 and 2682 ?? 4 Ma, respectively. The tonalitic phase of the Morton Gneiss, southwestern Minnesota, is dated at 3662 ?? 42 Ma. ?? 1986.

  4. Spent coffee grounds as air-propelled abrasive grit for weed control

    Science.gov (United States)

    Spent coffee grounds (SCG) represent a significant food waste residue. Value-added uses for this material would be beneficial. Gritty agricultural residues, such as corncob grit, can be employed as abrasive air-propelled agents for organically-compatible postemergence shredding of weed seedlings sel...

  5. Amenidades ambientais e desenvolvimento rural

    OpenAIRE

    Dentinho, Tomaz; Rodrigues, Orlando

    2007-01-01

    Este texto sobre amenidades ambientais e desenvolvimento rural trata, fundamentalmente, da incerteza resultante da reacção das pessoas e das instituições face aos recursos naturais que exploram e quanto ao efeito das políticas que são implementadas.

  6. Bonding to new CAD/CAM resin composites: influence of air abrasion and conditioning agents as pretreatment strategy.

    Science.gov (United States)

    Reymus, Marcel; Roos, Malgorzata; Eichberger, Marlis; Edelhoff, Daniel; Hickel, Reinhard; Stawarczyk, Bogna

    2018-04-27

    Because of their industrially standardized process of manufacturing, CAD/CAM resin composites show a high degree of conversion, making a reliable bond difficult to achieve. The purpose of this experiment was to investigate the tensile bond strength (TBS) of luting composite to CAD/CAM resin composite materials as influenced by air abrasion and pretreatment strategies. The treatment factors of the present study were (1) brand of the CAD/CAM resin composite (Brilliant Crios [Coltene/Whaledent], Cerasmart [GC Europe], Shofu Block HC [Shofu], and Lava Ultimate [3M]); (2) air abrasion vs. no air abrasion; and (3) pretreatment using a silane primer (Clearfil Ceramic Primer, Kuraray) vs. a resin primer (One Coat 7 Universal, Coltene/Whaledent). Subsequently, luting composite (DuoCem, Coltene/Whaledent) was polymerized onto the substrate surface using a mold. For each combination of the levels of the three treatment factors (4 (materials) × 2 (air abrasion vs. no air abrasion; resin) × 2 (primer vs. silane primer)), n = 15, specimens were prepared. After 24 h of water storage at 37 °C and 5000 thermo-cycles (5/55 °C), TBS was measured and failure types were examined. The resulting data was analyzed using Kaplan-Meier estimates of the cumulative failure distribution function with Breslow-Gehan tests and non-parametric ANOVA (Kruskal-Wallis test) followed by the multiple pairwise Mann-Whitney U test with α-error adjustment using the Benjamini-Hochberg procedure and chi-square test (p CAD/CAM resin composites, the restorations should be air abraded and pretreated using a resin primer containing methyl-methacrylate to successfully bond to the luting composite. The pretreatment of the CAD/CAM resin composite using merely a silane primer results in deficient adhesion. For a reliable bond of CAD/CAM resin composites to the luting composite, air abrasion and a special pretreatment strategy are necessary in order to achieve promising long-term results.

  7. Wear- and heat resistance of vacuum-arc TiN and TiAlN based coatings with Si and Y additives

    International Nuclear Information System (INIS)

    Aksenov, I.I.; Belous, V.A.; Grigor'ev, A.N.; Ermolenko, I.G.; Zadneprovskij, Yu.A.; Kovalenko, V.I.; Lomino, N.S.; Marinin, V.G.; Tolmacheva, G.N.; Sobol', O.V.

    2011-01-01

    It is shown, that insertion of silicon additives into TiN coatings and of yttrium into TiAlN coatings in explored limits (to a few wht. %) leads to increasing of resistance against abrasive friction wear. At the same time silicon or yttrium presence in the coatings leads to loos of their columnar structure and demonstrate decrease in the cavitation resistance. It is supposed, that such distinction in behaviour of the given working performances is a consequence of that mechanisms of the coating surface fracture at action of cavitation and abrasive friction are different. All explored coatings of (Ti-Si)N composition are not oxidised up to 600 o C, and of (Ti-Al-Y)N coatings - up to 800 o C.

  8. PATRIMÔNIO CULTURAL ARQUEOLÓGICO: INSTRUMENTO DE DESENVOLVIMENTO TURÍSTICO

    OpenAIRE

    Rossano Bastos

    2012-01-01

    O presente trabalho trata das perspectivas de aproveitamento do Patrimônio Cultural Arqueológico como instrumento de desenvolvimento turístico.PALAVRAS-CHAVE: Arqueologia; Turismo;Desenvolvimento.ABSTRACT: This work considers some improvement perspectives ofthe archaeological cultural heritage as an instrument of tourism development.KEY-WORDS: Archaeology; Tourism; Development. 

  9. Study of the Contact Resistance of Interlaced Stainless Steel Yarns Embedded in Hybrid Woven Fabrics

    Directory of Open Access Journals (Sweden)

    Vasile Simona

    2017-06-01

    Full Text Available The contact resistance of two interlacing electro-conductive yarns embedded in a hybrid woven fabric will constitute a problem for electro-conductive textiles under certain circumstances. A high contact resistance can induce hotspots, while a variable contact resistance may cause malfunctioning of the components that are interconnected by the electro-conductive yarns. Moreover, the contact robustness should be preserved over time and various treatments such as washing or abrading should not alter the functioning of the electro-conductive textiles. The electrical resistance developed in the contact point of two interlacing electro-conductive yarns is the result of various factors. The influence of diameter of the electro-conductive stainless steel yarns, the weave pattern, the weft density, and the abrasion on the contact resistance was investigated. Hybrid polyester fabrics were produced according to the design of experiments (DoE and statistical models were found that describe the variation of the contact resistance with the selected input parameters. It was concluded that the diameter of the stainless steel warp and weft yarns has a statistically significant influence on the contact resistance regardless of the weave. Weft density had a significant influence on the contact resistance but only in case of the twill fabrics. Abrasion led to an increase in contact resistance regardless of the weave pattern and the type of stainless steel yarn that was used. Finally, a combination of parameters that leads to plain and twill fabrics with low contact resistance and robust contacts is recommended.

  10. Effect of Phenomena Accompanying Wear in Dry Corundum Abrasive on the Properties and Microstructure of Austempered Ductile Iron with Different Chemical Composition

    Directory of Open Access Journals (Sweden)

    Myszka D.

    2015-04-01

    Full Text Available The research described in this article is a fragment in the series of published works trying to determine the applicability of new materials for parts of the mining machinery. Tests were performed on two groups of austempered ductile iron - one of which contained 1.5% Ni and 0.5% Mo, while the other contained 1.9% Ni and 0.9% Cu. Each group has been heat treated according to the three different heat treatment variants and then the material was subjected to detailed testing of mechanical properties and abrasion wear resistance, measuring also hardness and magnetic properties, and conducting microstructural examinations. The results indicated that each of the tested materials was senstive to the surface hardening effect, which resulted in high wear resistance. It has been found that high temperature of austempering, i.e. 370°C, favours high wear resistance of ductile iron containing nickel and molybdenum. Low temperature of austempering, i.e. 270°C, develops high wear resistance in ductile iron containing nickel and copper. Both these materials offer completely different mechanical properties and as such can be used for different and specific applications.

  11. Abrasive wear of BA1055 bronze with additives of Si, Cr, Mo and/or W

    Directory of Open Access Journals (Sweden)

    B. P. Pisarek

    2008-10-01

    Full Text Available Aluminium bronzes belong to the high-grade constructional materials applied on the put under strongly load pieces of machines, aboutgood sliding, resistant properties on corrosion both in the cast state how and after the thermal processing. It moves to them Cr and Si in the aim of the improvement of their usable proprieties. The additions Mo and/or W were not applied so far. It was worked out therefore the new kind of bronzes casting including these elements. Make additions to the Cu-Al-Fe-Ni bronze of Si, Cr, Mo and/or W in the rise of these properties makes possible. The investigations of the surface distribution of the concentration of elements in the microstructure of the studied bronze on X-ray microanalyzer were conducted. It results from conducted investigations, that in the aluminium bronze BA1055 after makes additions Si, Cr, Mo and/or W the phases of the type κFe, κNi crystallize, probably as complex silicides. Elements such as: Fe and Si dissolve first of all in phases κ, in smaller stage in the matrix of the bronze; Mn, Ni and W they dissolve in matrix and phases κ. It dissolves Cr and Mo in the larger stage in phases κ than in the matrix. The sizes of the abrasive wear were compared in the state cast multicomponentnew casting Cu-Al-Fe-Ni bronzes with the additives Cr, Mo or W with the wear of the bronze CuAl10Fe5Ni5Si. The investigations of thewear were conducted on the standard device. It results from conducted investigations, that make additions to bronze BA1055 of the additives of Si, Cr, Mo, and/or W it influences the rise of the hardness (HB of the bronze in the cast state, in the result of the enlarged quantity separates of hard phases κ, and in the consequence the decrease of the abrasive wear. The addition of molybdenum made possible obtainment of the microhardness of the phase α and γ 2 on the comparable level. From the microstructure of the bronze CuAl10Fe5Ni5MoSi is characterizes the smallest abrasive wear among

  12. Abrasiveness and hardness of rocks of Cretaceous deposits of Chechen-Ingushetiya. Ob abrazivnosti i tverdosti gornykh porod melovykh otlozhenii Checheno-Ingushetii

    Energy Technology Data Exchange (ETDEWEB)

    Trofimenko, Yu.P.

    1981-01-01

    Presented are results of studies of the abrasiveness and hardness of core material taken from Upper Cretaceous deposits in the process of drilling deep boreholes in the areas of Chechen-Ingushetiya. Based on the studies it is established that the abrasiveness of rock is mainly influenced by the coarseness of the mineral grains in the rock, their mineralogical composition, and the composition of the cement. Given is a system of clasification of the investigated core material with respect to abrasiveness and hardness.

  13. Comparative evaluation of tooth substance loss and its correlation with the abrasivity and chemical composition of different dentifrices.

    Science.gov (United States)

    Singh, Ram Prakash; Sharma, Sidhartha; Logani, Ajay; Shah, Naseem; Singh, Surendra

    2016-01-01

    In India, teeth cleaning with tooth powder is common in rural and semi-urban areas. These dentifrices may contain low-quality abrasives, which may have a deleterious effect on dental hard tissues. This study aims to evaluate the tooth substance loss caused by different dentifrices and to correlate it with chemical composition, size, and shape of abrasives used. An indigenously made automated machine was used for brushing the specimens. Sixty-four freshly extracted premolars were allocated to eight groups (n = 8). Colgate toothpaste was used as the control group. Each specimen was brushed in a vertical motion for 2½ h at 200 strokes/min with a constant applied load of 200 g corresponding to 6-month brushing. The difference in weight (pre- and post-brushing) was determined by an analytical weighing machine. Chemical analysis was done to determine the presence of iron oxide by Inductively Coupled Plasma Mass Spectrometry method. Shape and size of the abrasive particles was evaluated under scanning electron microscopy (SEM). One-way analysis of variance and Paired t-test were used to analyze the data. Tooth substance loss was maximum in the group brushed with red tooth powder, which was shown to contain the highest amount of iron oxide and also exhibited large, irregularly shaped abrasive particles under SEM. Tooth substance loss was documented to be correlated with chemical composition (iron oxide) and the size and shape of abrasive particles used in dentifrices.

  14. Minimal alterations on the enamel surface by micro-abrasion: in vitro roughness and wear assessments

    Directory of Open Access Journals (Sweden)

    Marcela Charantola Rodrigues

    2013-04-01

    Full Text Available Objective: To evaluate the in vitro changes on the enamel surface after a micro-abrasion treatment promoted by different products. Material and Methods: Fifty (50 fragments of bovine enamel (15 mm × 5 mm were randomly assigned to five groups (n=10 according to the product utilized: G1 (control= silicone polisher (TDV, G2= 37% phosphoric acid (3M/ESPE + pumice stone (SS White, G3= Micropol (DMC Equipment, G4= Opalustre (Ultradent and G5= Whiteness RM (FGM Dental Products. Roughness and wear were the responsible variables used to analyze these surfaces in four stages: baseline, 60 s and 120 s after the micro-abrasion and after polishing, using a Hommel Tester T1000 device. After the tests, a normal distribution of data was verified, with repeated ANOVA analyses (p≤0.05 which were used to compare each product in different stages. One-way ANOVA and Tukey tests were applied for individual comparisons between the products in each stage (p≤0.05. Results: Means and standard deviations of roughness and wear (µm after all the promoted stages were: G1=7.26(1.81/13.16(2.67, G2=2.02(0.62/37.44(3.33, G3=1.81(0.91/34.93(6.92, G4=1.92(0.29/38.42(0.65 and G5=1.98(0.53/33.45(2.66. At 60 seconds, all products tended to produce less surface roughness with a variable gradual decrease over time. After polishing, there were no statistically significant differences between the groups, except for G1. Independent of the product utilized, the enamel wear occurred after the micro-abrasion. Conclusions: In this in vitro study, enamel micro-abrasion presented itself as a conservative approach, regardless of the type of the paste compound utilized. These products promoted minor roughness alterations and minimal wear. The use of phosphoric acid and pumice stone showed similar results to commercial products for the micro-abrasion with regard to the surface roughness and wear.

  15. Prediction Of Abrasive And Diffusive Tool Wear Mechanisms In Machining

    Science.gov (United States)

    Rizzuti, S.; Umbrello, D.

    2011-01-01

    Tool wear prediction is regarded as very important task in order to maximize tool performance, minimize cutting costs and improve the quality of workpiece in cutting. In this research work, an experimental campaign was carried out at the varying of cutting conditions with the aim to measure both crater and flank tool wear, during machining of an AISI 1045 with an uncoated carbide tool P40. Parallel a FEM-based analysis was developed in order to study the tool wear mechanisms, taking also into account the influence of the cutting conditions and the temperature reached on the tool surfaces. The results show that, when the temperature of the tool rake surface is lower than the activation temperature of the diffusive phenomenon, the wear rate can be estimated applying an abrasive model. In contrast, in the tool area where the temperature is higher than the diffusive activation temperature, the wear rate can be evaluated applying a diffusive model. Finally, for a temperature ranges within the above cited values an adopted abrasive-diffusive wear model furnished the possibility to correctly evaluate the tool wear phenomena.

  16. Os eventos programados, como alternativo do desenvolvimento do turismo

    Directory of Open Access Journals (Sweden)

    Andrés Pinassi

    2014-10-01

    Full Text Available Turismo e lazer são vistos como uma alternativa para o desenvolvimento econômico, social e cultural de uma comunidade. Ambas práticas de lazer são consolidadas como processos sócio-espaciais que podem trazer muitos impactos benéficos para os moradores de uma determinada localidade. Assim, a dinâmica de eventos programados em aldeias visa proporcionar uma alternativa oportunidades de desenvolvimento local para comunidades carentes. Nesse contexto, a pesquisa desenvolvida, em seguida, analisa o desenvolvimento de um festival especial, realizada na Provincia de Buenos Aires (Argentina. Este festival, iniciado a partir da esfera pública municipal, mostrou benefícios económicos significativos e definir um entretenimento alternativa valiosa para a população local e da área de influência.

  17. Resistência de genótipos de batata a Phthorimaea operculella (Zeller

    Directory of Open Access Journals (Sweden)

    Lopes Maria Teresa do Rêgo

    2001-01-01

    Full Text Available A traça Phthorimaea operculella (Zeller é considerada atualmente uma das principais pragas da batata. O uso de resistência varietal para controle desse inseto é uma alternativa promissora, mas que ainda precisa ser melhor pesquisada. A resistência de genótipos de batata à traça foi avaliada, em condições de laboratório, analisando-se o efeito de folhas e tubérculos sobre a biologia do inseto. Comparou-se também o desenvolvimento da traça em folhas de batata e tomate. Os experimentos foram conduzidos com os clones de batata NYL 235-4 e N 140-201 (ambos com tricomas glandulares tipo A nas folhas, as cultivares Aracy, Apuã e Itararé e a cultivar de tomate Santa Clara. Os insetos foram criados em folíolos e tubérculos dos genótipos, avaliando-se a duração e a viabilidade das fases larval e pupal e o peso de pupas. O desenvolvimento do inseto não foi afetado nas folhas dos genótipos de batata, mesmo nos materiais com tricomas glandulares. Entretanto, em folhas de tomate houve aumento do período larval e diminuição do peso de pupas, sendo este substrato menos favorável ao desenvolvimento da traça quando comparado às folhas de batata. Em testes com tubérculos, o clone NYL 235-4 apresentou resistência a P. operculella, provocando redução significativa na viabilidade larval e alongamento desta fase. O clone N 140-201 afetou o desenvolvimento do inseto de forma menos pronunciada, alongando a fase larval.

  18. Abrasive wear based predictive maintenance for systems operating in sandy conditions

    NARCIS (Netherlands)

    Woldman, M.; Tinga, T.; Heide, E. van der; Masen, M.A.

    2015-01-01

    Machines operating in sandy environments are damaged by the abrasive action of sand particles that enter the machine and become entrapped between components and contacting surfaces. In the case of the military services the combination of a sandy environment and the wide range of tasks to be

  19. Desenvolvimento e Gestão Pública: das ideias às práticas

    Directory of Open Access Journals (Sweden)

    Jackeline Amantino de Andrade

    2010-11-01

    Full Text Available Este artigo tem como objetivo tratar dos modelos de desenvolvimento no contexto brasileiro e introduzir uma discussão sobre políticas de desenvolvimento e sua gestão. Para tanto, faz-se necessário resgatar a discussão sobre desenvolvimento tanto em suas bases desenvolvimentistas como a atual proposição de desenvolvimento endógeno. Entende-se que o desenvolvimento depende de uma capacidade organizacional na articulação de vários fatores, tangíveis e intangíveis, quantitativos e qualitativos e envolve várias dimensões: econômica, social, cultural, ambiental e físico-territorial, político-institucional e científico-tecnológica e é construído através de estratégias processuais potencializadas por coletivos. A primeira parte apresenta uma discussão conceitual sobre o desenvolvimento e os processos de organizacionais e de gestão neles implicados. A segunda parte apresenta um estudo empírico de caráter exploratório de modo a ampliar a discussão sobre modelos de desenvolvimento a partir da relação entre teoria e prática. Finalmente, são tecidas algumas considerações sobre o por vir, principalmente, quando se considera que nesses tempos de globalização e de acirramento das desigualdades urge encontrar alternativas justas e solidárias para as sociedades.

  20. Numerical Thermodynamic Analysis of Two-Phase Solid-Liquid Abrasive Flow Polishing in U-Type Tube

    Directory of Open Access Journals (Sweden)

    Junye Li

    2014-08-01

    Full Text Available U-type tubes are widely used in military and civilian fields and the quality of the internal surface of their channel often determines the merits and performance of a machine in which they are incorporated. Abrasive flow polishing is an effective method for improving the channel surface quality of a U-type tube. Using the results of a numerical analysis of the thermodynamic energy balance equation of a two-phase solid-liquid flow, we carried out numerical simulations of the heat transfer and surface processing characteristics of a two-phase solid-liquid abrasive flow polishing of a U-type tube. The distribution cloud of the changes in the inlet turbulent kinetic energy, turbulence intensity, turbulent viscosity, and dynamic pressure near the wall of the tube were obtained. The relationships between the temperature and the turbulent kinetic energy, between the turbulent kinetic energy and the velocity, and between the temperature and the processing velocity were also determined to develop a theoretical basis for controlling the quality of abrasive flow polishing.

  1. Performance tests of an abrasive cut-off systems for the finishing of high-precision casts

    Directory of Open Access Journals (Sweden)

    A. Fedoryszyn

    2008-10-01

    Full Text Available The paper summarizes the performance data of a newly designed and engineered grinding and cut-off system. The machine is used forseparation of models manufactured by the investment casting method. The machine comprises the following units:- base supporting other assemblies and elements: abrasive disc holder and drives; this solution enables an easy replacement and access toholding elements while a belt transmission allows the disc rpm to be varied,- mechanism moving the spindle in the horizontal, hence the abrasive disc position with respect to the batch can be precisely controlled,depending on the cast position and their shape,- holding and positioning-control of the batch to enable the fore and aft movements and rotations,- guide systems ensuring the travel of the batch in the specified direction and adjusting the travel speed to the required cutting rate,- centering, control, exhaust system, housing.Extensive tests were performed, including the tests of operating parameters of abrasive discs depending on the cast material, cyclograms ofthe applied treatment are obtained accordingly.

  2. Performance tests of an abrasive cut-off systems for the finishing of high-precision casts

    Directory of Open Access Journals (Sweden)

    A. Fedoryszyn

    2008-07-01

    Full Text Available The paper summarizes the performance data of a newly designed and engineered grinding and cut-off system. The machine is used for separation of models manufactured by the investment casting method. The machine comprises the following units:- base supporting other assemblies and elements: abrasive disc holder and drives; this solution enables an easy replacement and access to holding elements while a belt transmission allows the disc rpm to be varied,- mechanism moving the spindle in the horizontal, hence the abrasive disc position with respect to the batch can be precisely controlled, depending on the cast position and their shape,- holding and positioning-control of the batch to enable the fore and aft movements and rotations,- guide systems ensuring the travel of the batch in the specified direction and adjusting the travel speed to the required cutting rate,- centering, control, exhaust system, housingExtensive tests were performed, including the tests of operating parameters of abrasive discs depending on the cast material, cyclograms of the applied treatment are obtained accordingly.

  3. Metallurgical/Alloy Optimization of High Strength and Wear Resistant Structural Quench and Tempered Steels

    Science.gov (United States)

    Stalheim, Douglas G.; Peimao, Fu; Linhao, Gu; Yongqing, Zhang

    Structural steels with yield strength requirements greater or equal to 690 MPa can be produced through controlled recrystallization hot rolling coupled with precipitation strengthening or purposeful heat treatment through quench and tempering (Q&T). High strength structural steel and wear/abrasion resistant requirements greater or equal to 360 Brinell hardness (BHN) are produced by the development of microstructures of tempered lower bainite and/or martensite through the Q&T process. While these Q&T microstructures can produce very high strengths and hardness levels making them ideal for 690 MPa plus yield strength or wear/abrasion resistant applications, they lack toughness/ductility and hence are very brittle and prone to cracking. While tempering the microstructures helps in improving the toughness/ductility and reducing the brittleness, strength and hardness can be sacrificed. In addition, these steels typically consist of alloy designs containing boron with carbon equivalents (CE) greater than 0.50 to achieve the desired microstructures. The higher CE has a negative influence on weldability.

  4. Hard Coat Layers by PE-CVD Process for the Top Surface of Touch Panel

    International Nuclear Information System (INIS)

    Okunishi, T; Sato, N; Yazawa, K

    2013-01-01

    In order to protect surface from damages, the high pencil hardness and the high abrasion resistance are required for the hard coat layers on polyethylene telephthalate (PET) films for the application of touch panel surface. We have already found that the UV-curing-hard-coat-polymer (UHP) coated PET films show the poor abrasion resistance, while they have the high pencil hardness. It reveals that the abrasion resistance of hard coat layers of the UHP is not simply dependent on the pencil hardness. In this work, we have studied to improve the abrasion resistance of SiOC films as hard coat layers, which were formed by PE-CVD process on UHP coated PET. The abrasion resistance was evaluated by Taber abrasion test. PE-CVD hard coat layers which formed on UHP coater PET films have showed the better abrasion resistance and have the possibility of substitution to the thin glass sheets for touch panel application.

  5. Desenvolvimento de um monitor de apneia pediátrico

    OpenAIRE

    Caldeira, Gonçalo José Martins

    2009-01-01

    O trabalho apresentado tem por base o desenvolvimento de um monitor de apneia do sono pediátrico. Aborda questões ao nível da fisiologia respiratória e da mecânica pulmonar de um indivíduo. Apresenta uma proposta de desenvolvimento de um monitor de aquisição e identificação de sinais respiratórios, a fim de efectuar a detecção da apneia do sono.

  6. Desenvolvimento sustentável: um discurso sobre a relação entre desenvolvimento e natureza Sustainable development: a discourse about the relation between development and nature

    Directory of Open Access Journals (Sweden)

    Hugo Juliano Duarte Matias

    2008-04-01

    Full Text Available Trata-se do estudo de definições de desenvolvimento sustentável, elemento fundamental de repertórios interpretativos para a relação entre desenvolvimento e natureza. As definições respondiam a um questionário aplicado a 355 estudantes de vários cursos de uma universidade federal. Realizou-se uma análise de conteúdo que buscou a concepção de natureza e sua relação com desenvolvimento nessas definições. Foram encontradas três matrizes discursivas: (a "economicista" - a necessidade de desenvolvimento subordina a necessidade de preservação da natureza, cujo sentido é "recursos naturais"; (b discurso "bem intencionado" - a necessidade de desenvolvimento subordina a de preservação da natureza, cujo sentido é "fragilidade"; (c "esvaziado" - desenvolvimento e natureza são disjuntos. Conclui-se sobre a importância do estudo da atribuição de significado à natureza para explicar como as pessoas pensam a relação entre desenvolvimento e natureza, e sobre como essas matrizes discursivas podem justificar práticas sociais.This study presents the analysis of definitions of sustainable development, as a basic element of interpretative repertoires for the relation between development and nature. Three hundred and fifty five students of several courses of a federal university answered a questionnaire, providing the definitions, thereafter submitted to content analysis to examine the concept of nature and its relation with development. Three discursive matrixes were found: (a the "economic bias" one - the necessity of development subordinates the need of nature preservation nature is a "natural resources"; (b the "good intentions" discourse - the necessity of development subordinates the necessity of preservation - nature is "fragility"; (c the "empty" - one development and nature are separate. It is concluded that the attribution of meaning to nature is important to explain how people think about the relation between development and

  7. Desenvolvimentos recentes no domínio da conexão aço concreto no contexto das estruturas mistas

    OpenAIRE

    Cruz, Paulo J. S.; Valente, Isabel; Veríssimo, G. S.; Paes, J. L. R.; Fakury, R. H.

    2006-01-01

    Este trabalho apresenta desenvolvimentos recentes sobre conexão aço-concreto para estruturas mistas. Os estudos realizados envolvem campanhas experimentais com diversos tipos de conectores de cisalhamento, utilizando-se concreto normal e concretos leves de alta resistência. A caracterização do comportamento das conexões tem sido realizada através de ensaios tipo push-out. Os resultados experimentais recentemente obtidos são comparados com resultados de outros autores. Os resultados das pesqui...

  8. Inglês como língua franca: desenvolvimentos recentes

    Directory of Open Access Journals (Sweden)

    Telma Gimenez

    Full Text Available Em face da atual posição do inglês como uma língua franca global, este artigo tem como principal objetivo discutir os desenvolvimentos recentes dessa área, tomando como base os trabalhos apresentados durante a 7th International Conference on English as a Lingua Franca, realizada em Atenas, Grécia, em setembro de 2014. As reflexões, aprofundadas nos tópicos i Teorizações sobre ILF; ii ILF e formação de professores; iii Desenvolvimentos futuros, trazem um olhar analítico sobre os temas discutidos no evento. Espera-se que as informações e reflexões aqui contempladas possam contribuir para o desenvolvimento de uma "curiosidade acadêmica" a respeito do paradigma ILF (inglês como língua franca e para o engajamento com suas questões e implicações.

  9. CERVEJA ARTESANAL E DESENVOLVIMENTO REGIONAL EM SANTA CATARINA (BRASIL

    Directory of Open Access Journals (Sweden)

    Valdinho Pellin

    2016-12-01

    Full Text Available Discussões relacionadas ao fortalecimento do desenvolvimento regional tem estimulado um debate em relação a contribuições que Indicações Geográficas (IGs podem oferecer ao desenvolvimento. IGs se constituem em elemento de identificação de produtos ou serviços com seus territórios e podem oferecer contribuições importantes para o desenvolvimento regional, agregando valor aos produtos, facilitando o acesso a novos mercados e valorizando tradições locais. Este artigo procura discutir a importância da cerveja artesanal no contexto do desenvolvimento regional em Santa Catarina. Para tanto explora como objetivos específicos: (i caracterizar as discussões que estão ocorrendo em torno do reconhecimento da IG para chope e cerveja artesanal na região de Blumenau (SC; (ii identificar contribuições e desafios para o Desenvolvimento Regional de um possível reconhecimento da IG; e (iii caracterizar limites e potencialidades sinalizados pela iniciativa em curso. Metodologicamente trata-se de pesquisa analítica e descritiva baseada em estudo de caso de natureza exploratória. Como instrumento de coleta de dados se realizou entrevistas semiestruturadas com gestores de micro cervejarias artesanais da região e atores públicos e privados envolvidos diretamente nas discussões. Além destas fontes primárias o estudo fundamentou-se em fontes consubstanciadas pelos documentos produzidos nas reuniões de trabalho realizadas até o presente. Os principais resultados de análise destacam que um possível reconhecimento da IG poderia contribuir para o fortalecimento do setor, aumentando a competitividade, além de fortalecer a atividade turística na região. Entretanto para isso, alguns conflitos, surgidos no âmbito das discussões, precisam ser assumidos, superados ou mitigados

  10. Sustainable and long-time 'rejuvenation' of biomimetic water-repellent silica coating on polyester fabrics induced by rough mechanical abrasion.

    Science.gov (United States)

    Rosu, Cornelia; Lin, Haisheng; Jiang, Lu; Breedveld, Victor; Hess, Dennis W

    2018-04-15

    The economical use of water-repellent coatings on polymeric materials in commercial and industrial applications is limited by their mechanical wear robustness and long-term durability. In this study, we demonstrate that polyethylene terephthalate (PET) fabric modified with inorganic, methyltrimethoxysilane (MTMS)-based coatings shows excellent resistance against various types of wear damage, thereby mimicking superhydrophobic biological materials. These features were facilitated by the rational design of coating processing that also enabled tunable hierarchical surface structure. A series of custom and standard testing protocols revealed that coating-to-substrate adhesion was remarkably high, as was the resistance to various mechanical abradents. The most intriguing characteristic observed during aging and abrasion cycles was the enhancement in non-wettability or 'rejuvenation' reflected by water droplet roll-off behavior, a characteristic of self-cleaning materials. Water-repellent properties of coated polyester were also enhanced by prolonged thermal annealing and were maintained after custom laundry. The developed technology offers opportunities to design low cost, durable and functional textiles for both indoor and outdoor applications. Copyright © 2018 Elsevier Inc. All rights reserved.

  11. Superior quality diamond heel inserts improve cutting structure and seal life in abrasive and directional applications

    Energy Technology Data Exchange (ETDEWEB)

    Cobb, Tyler; Scott, Dan; Nelms, Derek [Society of Petroleum Engineers (United States)

    2011-07-01

    In the oil and gas industry, continuous improvements over the last century have led to the development of increasingly efficient drilling equipment. Among the new technologies is the polycrystalline diamond compact bit which has become more efficient than roller cone bits for several applications; the utilization of roller cone bits is now restricted to tough applications such as directional drilling and drilling through hard and abrasive formations. The aim of this paper is to present the development of improved roller cone bits using new designs and diamond inserts of superior quality. Two case studies on the use of improved roller cone bits are presented herein. Results showed that the novel diamond inserts combined with the design improvements provide better wear resistance. This paper demonstrated that roller cone bits have achieved greater reliability and longevity thanks to the new generation of diamond inserts and to design improvements.

  12. Tutorial para o Desenvolvimento de Jogos 2D usando a Linguagem Java

    Directory of Open Access Journals (Sweden)

    Soraia Teixeira Barbosa

    2015-07-01

    Full Text Available Atualmente é grande o estudo e desenvolvimento de jogos eletrônicos tanto no meio acadêmico como fora dele. Entretanto o desenvolvimento do mesmo não é uma tarefa trivial. Este artigo mostra o desenvolvimento de um jogo computacional através de uma versão do conhecido jogo de arcade Space Invaders. O artigo proposto tem como objetivo mostrar os passos básicos para a construção de um jogo computacional em duas dimensões utilizando a linguagem de programação Java.

  13. Abrasive Wear of Alloyed Cast Steels Applied for Heavy Machinery

    Directory of Open Access Journals (Sweden)

    Studnicki A.

    2015-03-01

    Full Text Available In the paper the results and analysis of abrasive wear studies were shown for two grades of cast steels: low-alloyed cast steel applied for heavy machinery parts such as housing, covers etc. and chromium cast steels applied for kinetic nodes of pin-sleeve type. Studies were performed using the modified in Department of Foundry pin-on-disc method.

  14. Preliminary results of experimental cutting of porcine bones by abrasive waterjet

    Czech Academy of Sciences Publication Activity Database

    Hloch, S.; Valíček, Jan; Kozak, D.

    2011-01-01

    Roč. 18, č. 3 (2011), s. 467-470 ISSN 1330-3651 Institutional research plan: CEZ:AV0Z30860518 Keywords : abrasive waterjet cutting * porcine bones * surface quality Subject RIV: JQ - Machines ; Tools Impact factor: 0.347, year: 2011 http://hrcak.srce.hr/index.php?show=clanak&id_clanak_jezik=107026

  15. DANÇA E O DESENVOLVIMENTO MOTOR DE PORTADORES DE NECESSIDADES EDUCATIVAS ESPECIAIS - PNEEs

    Directory of Open Access Journals (Sweden)

    Liliane de Oliveira

    2012-04-01

    Full Text Available O estudo objetivou verificar as modificações nos padrões de desenvolvimento motor de PNEEs mediante prática da dança. Participaram 14 PNEEs do CIEP/Cruz Alta. O instrumento foi a Escala de Desenvolvimento Motor (Rosa Neto, 1996. Utilizou-se a estatística descritiva e teste “t” para análise dos dados. Observou-se diferenças estatisticamente significativas (p<0,05 entre pré e pós-testes nas variáveis idade cronológica, motora geral, motricidade ampla e equilíbrio. Concluiu-se que o programa de dança contribuiu significativamente para o desenvolvimento motor de PNEEs. Palavras chave: dança, motor, desenvolvimento, especial, educação.

  16. Elaboração e avaliação de um website sobre o desenvolvimento da linguagem infantil: portal dos bebês - desenvolvimento da linguagem

    Directory of Open Access Journals (Sweden)

    Aline Martins

    2015-02-01

    Full Text Available OBJETIVO: criar e desenvolver um website na área de fonoaudiologia com enfoque no desenvolvimento da linguagem de bebês de 0 a 48 meses, além de avaliar a qualidade do conteúdo apresentado e os recursos tecnológicos utilizados. MÉTODOS: na primeira fase do projeto foi realizado um levantamento de dados por meio de revisão de literatura sobre o desenvolvimento e aquisição da linguagem infantil. Em seguida esse conteúdo foi inserido no website e avaliado por 20 pais e/ou cuidadores. RESULTADO: o website Portal dos Bebês - Desenvolvimento da Linguagem foi desenvolvido com linguagem voltada a pais e/ou cuidadores, e seu conteúdo foi dividido em três temas: "Desenvolvimento da Linguagem", "Fala e Linguagem" e "Linguagem e o Ambiente". No que se refere à qualidade do conteúdo e da apresentação, o website foi avaliado como "excelente" por todos os participantes da amostra. Quanto à avaliação sobre o vocabulário utilizado e a forma de apresentação do conteúdo, 70% e 75% respectivamente, consideraram o website como "excelente". Em relação à apresentação visual, 85% dos participantes classificaram como "excelentes", já o tipo de navegação foi classificado como "satisfatório" por 50% dos participantes. Quanto à importância que os pais e/ou cuidadores julgam sobre o site a maioria classificou como "excelente" o auxilio que o mesmo dá no desenvolvimento da linguagem da criança. CONCLUSÃO: o website Portal dos Bebês - Desenvolvimento da Linguagem pode ser acessado pelo endereço online http://portaldosbebes.fob.usp.br, e seu conteúdo e recursos tecnológicos utilizados foram avaliados como satisfatório a excelente pelos pais e/ou cuidadores participantes.

  17. Technology Demonstration of Wet Abrasive Blasting for Removal of Lead- and Asbestos-Containing Paint

    National Research Council Canada - National Science Library

    Race, Timothy

    2003-01-01

    ...). This technology demonstration showed that wet blasting using an engineered abrasive can safely and effectively remove lead- and asbestos-containing paint from exterior concrete masonry unit walls...

  18. A COMPLEXIDADE ECONÔMICA DOS DIREITOS HUMANOS: UMA DIMENSÃO ESCONDIDA DO DESENVOLVIMENTO HUMANO

    Directory of Open Access Journals (Sweden)

    Leilane Serratine Grubba

    2012-10-01

    Full Text Available Este artigo tem por objeto a complexidade econômica dos direitos humanos, mais precisamente, a investigação da relação entre a complexidade econômica e o desenvolvimento humano. Nesse sentido, objetivou demonstrar a intrínseca relação e dependência do desenvolvimento humano à complexidade econômica dos direitos humanos, que influi na positivação dos direitos, assim como na luta pelo acesso aos bens necessários a uma vida digna. Por meio do método dedutivo, o artigo problematizou a relação entre o ser humano e seu contexto econômico-social para o desenvolvimento da vida em dignidade. Diante disso, em primeiro lugar, foi apresentada a noção de complexidade dos direitos humanos, isto é, as suas múltiplas dimensões. No segundo momento, foi analisada a questão econômica do desenvolvimento humano, ou seja, a relação entre o desenvolvimento da vida digna e a dimensão econômica da sociedade, e, finalmente, foi apresentada a complexidade econômica dos direitos humanos. O desenvolvimento humano não está apenas vinculado à dimensão econômica, mas compreende todas as dimensões (complexidade que perfazem uma vida digna de ser vivida. A vida se desenvolve em dignidade mediante o acesso aos bens materiais e imateriais. As políticas do desenvolvimento humano, nesse sentido, devem se integrar a uma estrutura que apoie um crescimento com equidade e sustentabilidade. Palavras-chave: Pensamento complexo. Complexidade econômica. Direitos humanos. Desenvolvimento humano. Dignidade humana.

  19. Clinical study on the removal of gingival melanin pigmentation: comparison between Nd:YAG laser ablation and mechanical abrasion

    International Nuclear Information System (INIS)

    Lopes, Luis Mario de Melo

    2002-01-01

    Melanin pigmentation occurs as a result of excessive deposition of melanin, produced by the melanocytes present in the basal layer of the epithelium. This study compares clinical parameters such as inflammation and/or hemorrhage, healing process and re-pigmentation, caused by the Nd:YAG laser ablation and the mechanical abrasion of the melanin, by means of photographic images, taken during the first 30 days after the treatment. The patients comfort was monitored during the first ten days after the treatment using the method of the Visual Analog Scale to measure the pain. Six patients with gingival melanin pigmentation were selected. The left upper gingival quadrant was treated with the Nd:YAG laser using 125 mJ per pulse and 20 Hz, the right upper gingival quadrant received mechanical abrasion and the lower quadrants served for control. Both techniques did not result in inflammation and/or hemorrhage. The healing process was slower with the laser. Using mechanical abrasion, ali patients showed remaining pigmentation or re-pigmentation of varying intensity after a period of 30 days. With the laser 50 % of the patients did not show any re-pigmentation after this period. The pain analysis showed that the pain sensed 24 hours after the treatment with the laser is higher than using mechanical abrasion. (author)

  20. Lung scintigraphy evaluation in workers exposed to abrasive dusts; Avaliacao cintilografica pulmonar em trabalhadores de industria de abrasivos

    Energy Technology Data Exchange (ETDEWEB)

    Terra Filho, Mario

    1996-12-31

    The production process of abrasives use aluminium, or silicon carbide a synthetic material with a hardness only slightly less than that of a diamond. It is popularly known as carborundum since it was first manufactured as an abrasive in 1891, produced by the fusion of high grade silica and petroleum coke with sawdust. For many years silicon carbide was thought not to give rise to pulmonary lesions. Recently several researchers suggested the existence of a carborundum pneumoconiosis. The aim of this study was to evaluate the role of the pulmonary clearance of {sup 99m} Technetium chelated to diethylene-triamine penta-acetate ({sup 99m} Tc DTPA), and {sup 67} Gallium lung scanning in workers exposed to abrasive dusts. Thirty seven subjects, 13 smokers and 24 nonsmokers and ex smokers were studied. In 32 (86,48%) {sup 67} Gallium lung scanning was positive including 13 (40,62%) retired workers. We conclude that non smoking workers of abrasives plants have a pulmonary alveolar epithelial permeability disturbance similar as observed in smoking workers and smoking controls. Most workers, ex-workers of these industries and in patients with carborundum pneumoconiosis there is an evidence of pulmonary inflammation measured with abnormal {sup 67} Gallium lung scan. (author) 101 refs., 2 figs., 11 tabs.

  1. Lung scintigraphy evaluation in workers exposed to abrasive dusts; Avaliacao cintilografica pulmonar em trabalhadores de industria de abrasivos

    Energy Technology Data Exchange (ETDEWEB)

    Terra Filho, Mario

    1995-12-31

    The production process of abrasives use aluminium, or silicon carbide a synthetic material with a hardness only slightly less than that of a diamond. It is popularly known as carborundum since it was first manufactured as an abrasive in 1891, produced by the fusion of high grade silica and petroleum coke with sawdust. For many years silicon carbide was thought not to give rise to pulmonary lesions. Recently several researchers suggested the existence of a carborundum pneumoconiosis. The aim of this study was to evaluate the role of the pulmonary clearance of {sup 99m} Technetium chelated to diethylene-triamine penta-acetate ({sup 99m} Tc DTPA), and {sup 67} Gallium lung scanning in workers exposed to abrasive dusts. Thirty seven subjects, 13 smokers and 24 nonsmokers and ex smokers were studied. In 32 (86,48%) {sup 67} Gallium lung scanning was positive including 13 (40,62%) retired workers. We conclude that non smoking workers of abrasives plants have a pulmonary alveolar epithelial permeability disturbance similar as observed in smoking workers and smoking controls. Most workers, ex-workers of these industries and in patients with carborundum pneumoconiosis there is an evidence of pulmonary inflammation measured with abnormal {sup 67} Gallium lung scan. (author) 101 refs., 2 figs., 11 tabs.

  2. Abrasion and algal fouling of coarse material on the Murman littoral

    Directory of Open Access Journals (Sweden)

    Malavenda S. V.

    2017-03-01

    Full Text Available On the Murmansk coast of the Barents Sea the boulder littoral zone is widely spread mostly covered by Fucus communities. This is one of the most productive benthic communities of the Barents Sea. The studies of intertidal communities have the long history, but the dynamics of intertidal ecosystems due to surf and storms is not clear. The goal of the work is to identify the leading factors that determine the rate of abrasion of coarse material and fouling algae-macrophytes of the intertidal zone of Murman. The study has been conducted in the Zelenetskaya Bay of the Barents Sea on the basis of the biological station of the MMBI KSC RAS. The rate of abrasion has been carried out during 2004–2013, phyto-overgrowing – 2009–2013. In three pilot landfills 12 samples of coarse material have been exposed during the year (from July to next July. The weight change of the sample as well as species composition and biomass of algae of fouling communities have been investigated. The influence of the surf intensity, temperature of water and air has been analyzed (univariate analysis of variance ANOVA has been applied. It has been shown that on the littoral of the Murmansk coast the abrasion of coarse material is determined primarily by the number of storms, so the storm rate has been proposed. It has been revealed that the density of fouling boulders with macroalgae depends primarily on the intensity of the surf and the average gradient of air temperature. The basis for the emerging communities of annual species are green (Acrosiphonia arcta, Blidingia minima, Spongomorpha aeruginosa and brown algae (Pylaiella littoralis, Dictyosiphon chordaria. These algae groups are found everywhere in Fucus communities of the boulder intertidal zone of the Murman coast and probably they are the intermediate stage of fouling the coarse-grained material

  3. Simplified Abrasion Test Methodology for Candidate EVA Glove Lay-Ups

    Science.gov (United States)

    Rabel, Emily; Aitchison, Lindsay

    2015-01-01

    During the Apollo Program, space suit outer-layer fabrics were badly abraded after performing just a few extravehicular activities (EVAs). For example, the Apollo 12 commander reported abrasive wear on the boots that penetrated the outer-layer fabric into the thermal protection layers after less than 8 hrs of surface operations. Current plans for the exploration planetary space suits require the space suits to support hundreds of hours of EVA on a lunar or Martian surface, creating a challenge for space suit designers to utilize materials advances made over the last 40 years and improve on the space suit fabrics used in the Apollo Program. Over the past 25 years the NASA Johnson Space Center Crew and Thermal Systems Division has focused on tumble testing as means of simulating wear on the outer layer of the space suit fabric. Most recently, in 2009, testing was performed on 4 different candidate outer layers to gather baseline data for future use in design of planetary space suit outer layers. In support of the High Performance EVA Glove Element of the Next Generation Life Support Project, testing a new configuration was recently attempted in which require 10% of the fabric per replicate of that need in 2009. The smaller fabric samples allowed for reduced per sample cost and flexibility to test small samples from manufacturers without the overhead to have a production run completed. Data collected from this iteration was compared to that taken in 2009 to validate the new test method. In addition the method also evaluated the fabrics and fabric layups used in a prototype thermal micrometeoroid garment (TMG) developed for EVA gloves under the NASA High Performance EVA Glove Project. This paper provides a review of previous abrasion studies on space suit fabrics, details methodologies used for abrasion testing in this particular study, results of the validation study, and results of the TMG testing.

  4. Scratch resistance of SiO2 and SiO2 - ZrO2 sol-gel coatings on glass-ceramic obtained by sintering

    International Nuclear Information System (INIS)

    Soares, V. O.; Soares, P.; Peitl, O.; Zanotto, E. D.; Duran, A.; Castro, Y.

    2013-01-01

    The sol-gel process is widely used to obtain coatings on glass-ceramic substrates in order to improve the scratch and abrasion resistance, also providing a bright and homogeneous appearance of a glaze avoiding expensive final polishing treatments. This paper describes the preparation of silica and silica / zirconia coatings by sol-gel method on Li 2 O-Al 2 O3-SiO 2 (LAS) glassceramic substrates produced by sintering. The coatings were deposited by dip-coating on LAS substrates and characterized by optical microscopy and spectral ellipsometry. On the other hand, hardness and elastic modulus, coefficient of friction and abrasion and scratch resistance of the coatings were determined and compared with the substrate properties. Coatings deposited on LAS glass-ceramic confere the substrate a bright and homogeneous aspect, similar to a glaze, improving the appearance and avoiding the final polishing. However these coatings do not increase the scratch resistance of the substrate only equaling the properties of the glass-ceramic. (Author)

  5. [Influences of composition on brush wear of composite resins. Influences of particle size and content of filler].

    Science.gov (United States)

    Yuasa, S

    1990-07-01

    The influences of the composition on abrasion resistance of composite resins were examined using various experimental composite resins which had various matrix resin, filler size and content. The abrasion test was conducted by the experimental toothbrush abrasion testing machine developed in our laboratory. Three series of heat-curing composite resins were tested. One series was made from a Bis-MPEPP or UDMA monomer, and a silica filler with an average particle size of 0.04, 1.9, 3.8, 4.3, 7.5, 13.8 and 14.1 microns. The filler content of this series was constant at 45 wt%. The second series contained a silica filler of 4.3 microns in a content ranging from 35 to 75 wt%. The third series contained a microfiller (0.04 microns) and macrofiller (4.3 microns) in total content of 45 wt%. In this series, the microfiller was gradually replaced by 5, 15, 25 and 45 wt% of the macrofiller. The results obtained for these three series indicated that the abrasion resistance of composite resins was controlled by the inorganic filler, mainly filler size and content. The abrasion loss did not vary with the difference of matrix resin. When the particle size of the filler was below about 5 microns, the abrasion resistance decreased markedly with the decrease in filler size. The composite resin which contained a 0.04 or 1.9 micron filler was less resistant to toothbrush wear than the unfilled matrix resin. However, the microfiller also contributed to abrasion resistance when used in combination with the macrofiller, although abrasion resistance decreased with the increase in the microfiller concentration. The increase of filler content clearly improved the abrasion resistance when used the macrofiller. The analysis of these results and SEM observations of the brushed surfaces of samples suggested that the toothbrush abrasion was three-body abrasion caused by the abrasive in the toothpaste, and affected by the difference in the particle size between abrasive and filler, and between

  6. Thickness-Independent Ultrasonic Imaging Applied to Abrasive Cut-Off Wheels: An Advanced Aerospace Materials Characterization Method for the Abrasives Industry. A NASA Lewis Research Center Technology Transfer Case History

    Science.gov (United States)

    Roth, Don J.; Farmer, Donald A.

    1998-01-01

    Abrasive cut-off wheels are at times unintentionally manufactured with nonuniformity that is difficult to identify and sufficiently characterize without time-consuming, destructive examination. One particular nonuniformity is a density variation condition occurring around the wheel circumference or along the radius, or both. This density variation, depending on its severity, can cause wheel warpage and wheel vibration resulting in unacceptable performance and perhaps premature failure of the wheel. Conventional nondestructive evaluation methods such as ultrasonic c-scan imaging and film radiography are inaccurate in their attempts at characterizing the density variation because a superimposing thickness variation exists as well in the wheel. In this article, the single transducer thickness-independent ultrasonic imaging method, developed specifically to allow more accurate characterization of aerospace components, is shown to precisely characterize the extent of the density variation in a cut-off wheel having a superimposing thickness variation. The method thereby has potential as an effective quality control tool in the abrasives industry for the wheel manufacturer.

  7. Evaluation of Parameters Affecting Magnetic Abrasive Finishing on Concave Freeform Surface of Al Alloy via RSM Method

    Directory of Open Access Journals (Sweden)

    Mehrdad Vahdati

    2016-01-01

    Full Text Available The attempts of researchers in industries to obtain accurate and high quality surfaces led to the invention of new methods of finishing. Magnetic abrasive finishing (MAF is a relatively new type of finishing in which the magnetic field is used to control the abrasive tools. Applications such as the surface of molds are ones of the parts which require very high surface smoothness. Usually this type of parts has freeform surface. In this study, the effect of magnetic abrasive process parameters on freeform surfaces of parts made of aluminum is examined. This method is obtained through combination of magnetic abrasive process and Control Numerical Computer (CNC. The use of simple hemisphere for installation on the flat area of the magnets as well as magnets’ spark in curve form is a measure done during testing the experiments. The design of experiments is based on response surface methodology. The gap, the rotational speed of the spindle, and the feed rate are found influential and regression equations governing the process are also determined. The impact of intensity of the magnetic field is obtained using the finite element software of Maxwell. Results show that in concave areas of the surface, generally speaking, the surface roughness decreases to 0.2 μm from its initial 1.3 μm roughness. However, in some points the lowest surface roughness of 0.08 μm was measured.

  8. Assessment of abrasiveness for research of rock cutting

    Directory of Open Access Journals (Sweden)

    Milan Labaš

    2012-12-01

    Full Text Available Rock abrasiveness is ability of rock to wear down the working tool during the mutual interaction between the working indentorand the rock in the mechanical rock cutting process. The cutting indentor is worn down during the interaction, which changes itsgeometric dimensions causing the enlargement of a contact area between the tool and the rock surface. The changes in these dimensionsconsequently alter the rate of advance of the drilling machine and the specific cutting energy. We have determined the abrasivenessaccording to the norm ON 44 1121 (1982 on the testing device constructed at the Institute of Geotechnics SAS.

  9. The grain-size distribution of pyroclasts: Primary fragmentation, conduit sorting or abrasion?

    Science.gov (United States)

    Kueppers, U.; Schauroth, J.; Taddeucci, J.

    2013-12-01

    Explosive volcanic eruptions expel a mixture of pyroclasts and lithics. Pyroclasts, fragments of the juvenile magma, record the state of the magma at fragmentation in terms of porosity and crystallinity. The grain size distribution of pyroclasts is generally considered to be a direct consequence of the conditions at magma fragmentation that is mainly driven by gas overpressure in bubbles, high shear rates, contact with external water or a combination of these factors. Stress exerted by any of these processes will lead to brittle fragmentation by overcoming the magma's relaxation timescale. As a consequence, most pyroclasts exhibit angular shapes. Upon magma fragmentation, the gas pyroclast mixture is accelerated upwards and eventually ejected from the vent. The total grain size distribution deposited is a function of fragmentation conditions and transport related sorting. Porous pyroclasts are very susceptible to abrasion by particle-particle or particle-conduit wall interaction. Accordingly, pyroclastic fall deposits with angular clasts should proof a low particle abrasion upon contact to other surfaces. In an attempt to constrain the degree of particle interaction during conduit flow, monomodal batches of washed pyroclasts have been accelerated upwards by rapid decompression and subsequently investigated for their grain size distribution. In our set-up, we used a vertical cylindrical tube without surface roughness as conduit. We varied grain size (0.125-0.25; 0.5-1; 1-2 mm), porosity (0; 10; 30 %), gas-particle ratio (10 and 40%), conduit length (10 and 28 cm) and conduit diameter (2.5 and 6 cm). All ejected particles were collected after settling at the base of a 3.3 m high tank and sieved at one sieve size below starting size (half-Φ). Grain size reduction showed a positive correlation with starting grain size, porosity and overpressure at the vent. Although milling in a volcanic conduit may take place, porous pyroclasts are very likely to be a primary product

  10. The influence of varnish and high fluoride on erosion and abrasion in a laboratory investigation.

    Science.gov (United States)

    Sar Sancakli, H; Austin, R S; Al-Saqabi, F; Moazzez, R; Bartlett, D

    2015-03-01

    The aim of this study was to investigate the potential of concentrated fluoride varnishes to reduce enamel loss from repeated cycles of citric acid erosion and toothbrush abrasion in vitro. Polished human enamel samples were exposed to fluoride varnishes: Bifluorid10® (NaF&CaF2- 45,200 ppmF), Duraphat® (NaF 22,600 ppmF), Fluor-Protector® (difluorsilane 1000 ppmF) and a control coating of copal ether varnish (0 ppmF) group and a deionized water group. For each group of 16 samples, nine cycles of erosion and nine cycles of erosion-abrasion [1 cycle=erosion (0.3% citric acid, pH 3.2, 5 min)+artificial saliva (1 h, pH 7.0)+abrasion (120 linear strokes in artificial saliva from Oral B medium soft brushes 300 g loading]. The change in the enamel surface was evaluated using optical profilometry. Duraphat® and Bifluorid10® applications had a median (IQR) step height of 4.21 um (1.59) and 5.01 um (1.02). This was statistically significantly less than Fluor-Protector® 6.83 um (1.25), copal ether 7.22 um (1.97) and water 7.39 um (1.96) (pDental Association.

  11. Influence of Air Abrasion and Sonic Technique on Microtensile Bond Strength of One-Step Self-Etch Adhesive on Human Dentin

    Directory of Open Access Journals (Sweden)

    Baraba Anja

    2015-01-01

    Full Text Available The purpose of this in vitro study was to evaluate the microtensile bond strength of one-step self-etch adhesive to human dentin surface modified with air abrasion and sonic technique and to assess the morphological characteristics of the pretreated dentin surface. The occlusal enamel was removed to obtain a flat dentin surface for thirty-six human molar teeth. The teeth were randomly divided into three experimental groups (n = 12 per group, according to the pretreatment of the dentin: (1 control group, (2 air abrasion group, and (3 sonic preparation group. Microtensile bond strength test was performed on a universal testing machine. Two specimens from each experimental group were subjected to SEM examination. There was no statistically significant difference in bond strength between the three experimental groups (P > 0.05. Mean microtensile bond strength (MPa values were 35.3 ± 12.8 for control group, 35.8 ± 13.5 for air abrasion group, and 37.7 ± 12.0 for sonic preparation group. The use of air abrasion and sonic preparation with one-step self-etch adhesive does not appear to enhance or impair microtensile bond strength in dentin.

  12. Desenvolvimento humano: contribuições da psicologia moral

    Directory of Open Access Journals (Sweden)

    Yves de La Taille

    2007-03-01

    Full Text Available Procuramos avaliar as contribuições do conhecimento acumulado pela Psicologia Moral para a compreensão do desenvolvimento humano, para sustentar a tese segundo a qual a fonte energética do dever moral precisa ser procurada não só em sentimentos exclusivamente morais, mas também em sentimentos que desempenham um papel para o próprio desenvolvimento humano no seu conjunto. Três são os passos da análise deste artigo. Em primeiro lugar, verifi car se há possibilidade de articulação entre teorias psicológicas que enfatizam a dimensão afetiva da moralidade (Freud e Durkheim e outras que enfatizam a dimensão intelectual (Piaget e Kohlberg. Em segundo lugar, uma vez constatada a impossibilidade dessa articulação, sustentar que o sentimento de vergonha, presente na moralidade mas também em outras dimensões do desenvolvimento humano, é condição necessária ao sentimento de obrigatoriedade. Finalmente, analisar se tal sentimento é passível de ser evocado como fonte energética essencial nas abordagens que enfatizam a dimensão intelectual da moralidade.

  13. O desenvolvimento econômico da Venezuela, 1950/2006

    OpenAIRE

    Romina Batista de Lucena de Souza

    2008-01-01

    O objetivo desta tese é avaliar a contribuição do petróleo no desenvolvimento econômico da Venezuela, entre 1950/2006. Investiga-se por que uma economia rica em petróleo ainda não conseguiu industrializar-se. Seguindo os diferentes períodos governamentais, examinam-se a contribuição das políticas macroeconômicas sobre o desenvolvimento e a questão da doença holandesa e do capitalismo rentístico. Segundo a teoria da base econômica, as regiões crescem em torno de uma base exportadora, exercendo...

  14. Planos diretores: o caminho para o desenvolvimento sustentável das cidades

    Directory of Open Access Journals (Sweden)

    Alexsandro da Miranda

    2013-11-01

    Full Text Available Os Planos Diretores efetivam a existência de uma legislação geral estabelecendo as normas necessárias à implementação de políticas urbanas, previstas na Constituição Federal e no Estatuto da Cidade (Lei Federal 10.257/2001 e que em seu foco principal está o desenvolvimento e a expansão urbana.  Assim, o presente artigo aborda uma breve discussão teórica do tema, suas problemáticas e contextualizações na perspectiva de fundamentá-las à luz das teorias existentes. Três principais diretrizes devem ser destacadas: o desenvolvimento sustentável, a gestão democrática da cidade e o planejamento do desenvolvimento das cidades, onde os municípios, devem, portanto, utilizar as diretrizes e instrumentos do Estatuto da Cidade com o objetivo de estabelecer as regras que propiciem o pleno desenvolvimento econômico, social, ambiental e sustentável, com vistas a garantir o direito à cidade para todos os que nela vivem.

  15. Desenvolvimento econômico, desigualdade e saúde Economic development, inequality, and health

    Directory of Open Access Journals (Sweden)

    Pedro Reginaldo Prata

    1994-09-01

    Full Text Available O autor se refere a dimensão socioeconômica, individual e coletiva do fenômeno saúde-doença. Refere-se também ao fato das populações estarem sobre a influência desigual de fatores de risco e de proteção à saúde. Discute as desigualdades no desenvolvimento e a relação entre desenvolvimento, riqueza, saúde e justiça social. Questiona as teorias de desenvolvimento econômico, diferenciando desenvolvimento de crescimento. Cunha os conceitos de armadilha do desenvolvimento e refugiados sociais. Define uma comunidade saudável. Propõe a necessidade de mudança no modelo de desenvolvimento. Baliza o papel e as limitações do setor saúde no que diz respeito a iniqüidade social.The author refers to the social, economic, individual, and collective dimensions of the relationship between health and disease. He considers that individuals and populations are not equally exposed to protective and risk factors. He highlights the uneven development between nations and Brazilian regions, and communities, as well as discussing the relationship between development, wealth, health, and social justice. The article analyzes development theories and makes a distinction between economic development and growth. The concepts of development trap and social refugees are coined. The author defines a healthy community, points to the need for a shift in the current development model, and delineates the health sector's role and limitations in dealing with social inequality.

  16. Investigations on mechanical and two-body abrasive wear behaviour of glass/carbon fabric reinforced vinyl ester composites

    International Nuclear Information System (INIS)

    Suresha, B.; Kumar, Kunigal N. Shiva

    2009-01-01

    The aim of the research article is to study the mechanical and two-body abrasive wear behaviour of glass/carbon fabric reinforced vinyl ester composites. The measured wear volume loss increases with increase in abrading distance/abrasive particle size. However, the specific wear rate decreases with increase in abrading distance and decrease in abrasive particle size. The results showed that the highest specific wear rate is for glass fabric reinforced vinyl ester composite with a value of 10.89 x 10 -11 m 3 /Nm and the lowest wear rate is for carbon fabric reinforced vinyl ester composite with a value of 4.02 x 10 -11 m 3 /Nm. Mechanical properties were evaluated and obtained values are compared with the wear behaviour. The worn surface features have been examined using scanning electron microscope (SEM). Photomicrographs of the worn surfaces revealed higher percentage of broken glass fiber as compared to carbon fiber. Also better interfacial adhesion between carbon and vinyl ester in carbon reinforced vinyl ester composite was observed.

  17. Effect of nitrogen alloying on the microstructure and abrasive wear of stainless steels

    International Nuclear Information System (INIS)

    Hawk, J.A.; Simmons, J.W.; Rawers, J.C.

    1994-01-01

    Alloying stainless steels with nitrogen has distinct advantages. Nitrogen is a strong austenite stabilizer and a potent solid-solution strengthener, and nitrogen has greater solubility than carbon iron. This study investigates the relationship among nitrogen concentration, precipitate microstructure, and abrasive wear using two high-nitrogen stainless steel alloys: Fe-19Cr-5Mn-5Ni-3Mo (SS1) and Fe-16Cr-7Mn-5Ni(SS2). Alloy SS1 contained 0.7 wt% N and was solution annealed at 1,150 C, thereby dissolving the nitrogen interstitially in the austenite. Subsequent aging, or cold work and aging, at 900 C led to the grain-boundary, cellular, and transgranular precipitation of Cr 2 N. Alloy SS2 was remelted in a high-pressure (200 MPa) N 2 atmosphere, leading to a spatial gradient of nitrogen in the alloy in the form of interstitial nitrogen and Cr 2 N and CrN precipitates. Nitrogen contents varied from a low of approximately 0.7 wt% at the bottom of the billet to a high of 3.6 wt% at the top. Nitrogen in excess of approximately 0.7 wt% formed increasingly coarser and more numerous Cr 2 N and CrN precipitates. The precipitate morphology created in alloy SS1 due to aging, or cold work and aging, had little effect on the abrasive wear of the alloy. However, a decrease in the abrasive wear rate in alloy SS2 was observed to correspond to the increase in number and size of the Cr 2 N and CrN precipitates

  18. Abrasive water jet drilling of cooling holes in aeroengines: preliminary experimental study

    Czech Academy of Sciences Publication Activity Database

    Hlaváček, Petr; Zlámal, T.; Sitek, Libor

    2018-01-01

    Roč. 1, č. 1 (2018), s. 2218-2222 ISSN 1803-1269 R&D Projects: GA MŠk(CZ) LO1406; GA MPO(CZ) FV10446 Institutional support: RVO:68145535 Keywords : abrasive water jet * drilling * thermal barrier coating Subject RIV: JQ - Machines ; Tools OBOR OECD: Mechanical engineering http://www.mmscience.eu/2018.html

  19. DESENVOLVIMENTO DE RECURSOS DIDÁCTICOS INFORMATIZADOS NO ÂMBITO DA EDUCAÇÃO PARA O DESENVOLVIMENTO SUSTENTÁVEL. O EXEMPLO DO COURSEWARE SeRe

    Directory of Open Access Journals (Sweden)

    Patrícia Sá

    2010-02-01

    Full Text Available A falta de recursos didácticos informatizados de qualidade para o 1º e 2º Ciclos do Ensino Básico (1º/2º CEB, concebidos no âmbito da Educação para o Desenvolvimento Sustentável (EDS, numa perspectiva de Ensino por Pesquisa, determinou a organização de uma equipa multidisciplinar para o desenvolvimento do «Courseware Sere - O Ser Humano e os Recursos Naturais». Ajustando alguns princípios de desenvolvimento de software, particularmente de Design Centrado noUtilizador (DCU, o trabalho da equipa multidisciplinar, constituída por elementos com diversas competências (ao nível da Didáctica das Ciências, da Tecnologia Educativa, de Design e de Programação, centrou-se no desenvolvimento de um recurso didáctico informatizado que integra várias tipologias de software, nomeadamente simulações e visualizações, com as actividades didácticas. A orientação do recurso, as temáticas propostas e as metodologias e estratégias de exploração privilegiadas fundamentam-se: i na identificação das orientações nacionais e internacionais da EDS; ii na identificação das necessidades e interesses dos professores quanto à implementação de actividades com orientação EDS (Sá, 2008; Sá e Martins, 2007, iii no paradigma de ensino por competências (Cachapuz, Sá-Chaves e Paixão, 2004 e iv no recurso a um design interactivo centrado no utilizador (Costa, Loureiro, Reis, Sá, Guerra e Vieira, 2009; Guerra, 2007. Neste artigo faz-se uma apresentação do processo de desenvolvimento do recurso didáctico, das temáticas propostas e dasmetodologias e estratégias de exploração perspectivadas pelos autores do recurso.

  20. Floor tile glass-ceramic glaze for improvement of the resistance to surface abrasion

    Science.gov (United States)

    Gajek, M.; Lis, J.; Partyka, J.; Wójczyk, M.

    2011-10-01

    The results of research aimed at the study on frits and glass-ceramic glazes for floor tiles, based on compositions located in the primary field of cordierite crystallization within the system MgO-Al2O3-SiO2, have been presented. The results comprise investigations on the frits crystallization abilities, stability of the crystallizing phase under conditions of single-stage a fast firing cycle (time below 60 minutes) depending on their chemical composition and the influence of the nucleation agents. The influence of the nucleating agents namely TiO2, ZrO2, V2O5 on phase composition of obtained crystalline glazes, mechanical parameters and microstructure, has been examined. The strength tests proved increased mechanical resistance of crystalline glazes. Obtained glazes are characterized by high microhardness in range 6~8 GPa, as well as the increased wear resistance measured by the loss of weight below 100 mg / 55 cm2 (PN-EN ISO 10545-7). Significant increase of these parameters as compared with non-crystalline glazes, where micro-hardness values range between 5~6 GPa and the wear resistance values range from 120 to 200 mg, has been proved. Starting glasses (frits) and glazes of the ternary system MgO-SiO2-Al2O3, were examined with use of DTA, XRD and SEM methods.

  1. Floor tile glass-ceramic glaze for improvement of the resistance to surface abrasion

    International Nuclear Information System (INIS)

    Gajek, M; Lis, J; Partyka, J; Wojczyk, M

    2011-01-01

    The results of research aimed at the study on frits and glass-ceramic glazes for floor tiles, based on compositions located in the primary field of cordierite crystallization within the system MgO-Al 2 O 3 -SiO 2 , have been presented. The results comprise investigations on the frits crystallization abilities, stability of the crystallizing phase under conditions of single-stage a fast firing cycle (time below 60 minutes) depending on their chemical composition and the influence of the nucleation agents. The influence of the nucleating agents namely TiO 2 , ZrO 2 , V 2 O 5 on phase composition of obtained crystalline glazes, mechanical parameters and microstructure, has been examined. The strength tests proved increased mechanical resistance of crystalline glazes. Obtained glazes are characterized by high microhardness in range 6∼8 GPa, as well as the increased wear resistance measured by the loss of weight below 100 mg / 55 cm 2 (PN-EN ISO 10545-7). Significant increase of these parameters as compared with non-crystalline glazes, where micro-hardness values range between 5∼6 GPa and the wear resistance values range from 120 to 200 mg, has been proved. Starting glasses (frits) and glazes of the ternary system MgO-SiO 2 -Al 2 O 3 , were examined with use of DTA, XRD and SEM methods.

  2. A laser-abrasive method for the cutting of enamel and dentin.

    Science.gov (United States)

    Altshuler, G B; Belikov, A V; Sinelnik, Y A

    2001-01-01

    This paper introduced a new method for the removal of hard dental tissue based upon the use of particles accelerated by laser irradiation, which the authors have called the laser-abrasive method. The particles used were sapphire as powder or an aqueous suspension. The effect of the products of enamel ablation was also investigated. The particles were accelerated using submillisecond pulses of Er:YAG and Nd:YAG lasers. A strobing CCD camera was used to measure the speed of the ejected particles. The additional contribution of these particles to the efficiency of laser ablation of enamel and dentin was also investigated. The results showed that the enamel particles produced by the beam-tissue interaction were also accelerated by this process of ablation and were effective in the removal of enamel and dentin. The use of an aqueous suspension of sapphire particles increased the efficiency of enamel removal threefold when compared with the use of an Er:YAG laser with water spray. The laser-abrasive method allowed for the removal of enamel and dentin at speeds approaching those of the high-speed turbine. Copyright 2001 Wiley-Liss, Inc.

  3. A mesoeconomia do desenvolvimento econômico: o papel das instituições

    Directory of Open Access Journals (Sweden)

    Huáscar Pessali

    2011-01-01

    Full Text Available O desenvolvimento econômico depende das instituições e as instituições, ao mesmo tempo, são uma medida do desenvolvimento econômico. Assim, correlação e causalidade se confundem num processo cumulativo e circular - uma espiral de mudanças que condiciona a ampliação das liberdades dos indivíduos. A contribuição pretendida por este ensaio é reunir e propor uma organização de várias idéias dispersas no tema "instituições e desenvolvimento econômico". Nossa releitura adiciona um breve exemplo da relação entre mercados, firmas e estado no âmbito do desenvolvimento. Isto permite defender o retorno a uma análise econômica que não se limite às falhas de mercado, mas que encare a responsabilidade de lidar com um emaranhado mais complexo de interações.

  4. O TRABALHO COMO ATIVIDADE PRINCIPAL NO DESENVOLVIMENTO PSÍQUICO DO INDIVÍDUO ADULTO

    Directory of Open Access Journals (Sweden)

    Camila Fernanda Moro Rios

    2017-12-01

    Full Text Available Este artigo visa analisar, por meio da revisão teórica de autores clássicos e contemporâneos da psicologia histórico-cultural, o trabalho como atividade principal na vida adulta, isto é, como a atividade que orienta as principais mudanças no psiquismo humano e na personalidade nessa idade. Para tanto, abstrai e generaliza elementos constantes nos estudos sobre periodização do desenvolvimento psíquico humano. Por um lado, identifica os conteúdos e processos psicológicos que, produzidos pelo trabalho, evidenciam sua relevância para o desenvolvimento do indivíduo adulto. Por outro, aborda os processos de alienação inerentes à sociedade capitalista, que alienam o trabalho como atividade principal. Assim, o trabalho se apresenta, dialeticamente, como atividade humanizadora e alienada. Entende-se que este estudo contribui para o avanço teórico-metodológico da psicologia histórico-cultural por abordar a questão do trabalho como atividade principal, uma discussão que se encontra ainda incipiente e pouco sistematizada. Além disso, supera o enfoque dos estudos sobre o desenvolvimento centrados na infância e reitera o rompimento com a perspectiva maturacionista de que a vida adulta é um período de estagnação do desenvolvimento. Pela análise do trabalho como atividade principal conclui-se que o desenvolvimento psicológico, produzido na vida adulta, se expressa, principalmente, por uma série de aquisições de habilidades e capacidades, pelo exercício da criatividade, por uma complexa reestruturação da esfera afetivo-motivacional da personalidade, pelo desenvolvimento da autoconsciência e pelo movimento dialético da consciência de classe, que tensiona a contradição entre o polo humanizador e o polo alienado/alienante do trabalho numa sociedade que limita e empobrece esse mesmo desenvolvimento.

  5. Behavior and biological action of 239Pu while getting into skin abrasions

    International Nuclear Information System (INIS)

    Bazhin, A.G.; Lyubchanskij, Eh.R.; Nifatov, A.N.; Sinyakov, E.G.

    1983-01-01

    The levels of the radionuclide resorption are given through abrasions in applying 224-906 kBk of 239 Pu on them (0.6=1.5 % for 600 days), the nature of distribution and parameters of its exchange in the test skin area, skeleton and liver. Data of morphological studies are presented. The influence of prolonged complexon therapy on 239 Pu content in organs and tissues, mean life span, the frequency of appearance of morphological changes in test skin areas with the contamination density of 40; 184 and 722 kBk of 239 Pu/cm 2 and the frequency of tumor development including malignancy in case of applying 224 and 906 kBk of 239 Pu to abrasions is evaluated. It has been established that as a result of complexon therapy dosage exposure of the skeleton lessened by 4-5 times, the mean life span of rats with tumors increased, the development of osteosarcomas caused by Pu reduced from 23.6-36.2 to 4.4-6.2 % but the therapy did not influence the frequency of pathological changes in the test skin area

  6. Comparative Efficacy of a Soft Toothbrush with Tapered-tip Bristles to an ADA Reference Toothbrush on Gingival Abrasion over a 12-Week Period.

    Science.gov (United States)

    Gallob, John; Petrone, Dolores M; Mateo, Luis R; Chaknis, Patricia; Morrison, Boyce M; Panagakos, Foti; Williams, Malcolm

    2016-06-01

    Evaluation of the impact of a soft toothbrush with tapered-tip (Test Toothbrush) bristles and an ADA reference toothbrush (ADA Toothbrush) on gingival abrasion over a 12-week period. This was a randomized, single-center, examiner-blind, two-cell, parallel clinical research study and used the Danser Gingival Abrasion Index to assess the level of gingival abrasion after a single brushing, as well as after six weeks and 12 weeks of twice-daily brushing. Adult male and female subjects from the Central New Jersey, USA area refrained from all oral hygiene procedures for 24 hours. They reported to the study site after refraining from eating, drinking, and smoking for four hours. Following a qualifying examination using plaque and gingivitis scores along with a baseline gingival abrasion examination, subjects were randomized into two balanced groups, each group using one of the two study toothbrushes. Subjects were instructed to brush their teeth for one minute, under supervision, with their assigned toothbrush and a commercially available fluoride toothpaste (Colgate© Cavity Protection Toothpaste), after which they were again evaluated for gingival abrasion. Subjects were dismissed from the study site with their assigned toothbrush and toothpaste, and instructed to brush twice daily at home for the next 12 weeks. The subjects were instructed to brush for one minute during each tooth brushing. The subjects reported to the study site after six weeks and 12 weeks of product use, at which time they were evaluated for gingival abrasion. Seventy-one (71) subjects complied with the protocol and completed the clinical study. The results of this study showed that the Test Toothbrush provided statistically significantly (p ADA Toothbrush after a single tooth brushing, after six weeks, and after 12 weeks of product use (75.0%, 85.5%, 73.9%, respectively). The soft toothbrush with tapered-tip bristles produced significantly less gingival abrasion after 12 weeks of product use as

  7. Influence of Surface Abrasion on Creep and Shrinkage of Railway Prestressed Concrete Sleepers

    Science.gov (United States)

    Li, Dan; Ngamkhanong, Chayut; Kaewunruen, Sakdirat

    2017-10-01

    Ballasted railway track is very suitable for heavy-rail networks because of its many superior advantages in design, construction, short- and long-term maintenance, sustainability, and life-cycle cost. The sleeper, which supports rail and distributes loads from rail to ballast, is a very important component of rail track system. Prestressed concrete is very popular used in manufacturing sleepers. Therefore, improved knowledge about design techniques for prestressed concrete (PC) sleepers has been developed. However, the ballast angularity causes differential abrasions on the soffit or bottom surface of sleepers. Furthermore, in sharp curves and rapid gradient change, longitudinal and lateral dynamics of rails increase the likelihood of abrasions in concrete sleepers. This paper presents a comparative investigation using a variety of methods to evaluate creep and shrinkage effects in railway prestressed concrete sleepers. The outcome of this study will improve the material design, which is very critical to the durability of railway track components.

  8. Floor tile glass-ceramic glaze for improvement of the resistance to surface abrasion

    Energy Technology Data Exchange (ETDEWEB)

    Gajek, M; Lis, J; Partyka, J; Wojczyk, M, E-mail: mgajek@agh.edu.pl [AGH University of Science and Technology, Faculty of Materials Science and Ceramic, al. Mickiewicza 30, 30-059 Cracow (Poland)

    2011-10-29

    The results of research aimed at the study on frits and glass-ceramic glazes for floor tiles, based on compositions located in the primary field of cordierite crystallization within the system MgO-Al{sub 2}O{sub 3}-SiO{sub 2}, have been presented. The results comprise investigations on the frits crystallization abilities, stability of the crystallizing phase under conditions of single-stage a fast firing cycle (time below 60 minutes) depending on their chemical composition and the influence of the nucleation agents. The influence of the nucleating agents namely TiO{sub 2}, ZrO{sub 2}, V{sub 2}O{sub 5} on phase composition of obtained crystalline glazes, mechanical parameters and microstructure, has been examined. The strength tests proved increased mechanical resistance of crystalline glazes. Obtained glazes are characterized by high microhardness in range 6{approx}8 GPa, as well as the increased wear resistance measured by the loss of weight below 100 mg / 55 cm{sup 2} (PN-EN ISO 10545-7). Significant increase of these parameters as compared with non-crystalline glazes, where micro-hardness values range between 5{approx}6 GPa and the wear resistance values range from 120 to 200 mg, has been proved. Starting glasses (frits) and glazes of the ternary system MgO-SiO{sub 2}-Al{sub 2}O{sub 3}, were examined with use of DTA, XRD and SEM methods.

  9. Efficient Havinga–Kondepudi resolution of conglomerate amino acid derivatives by slow cooling and abrasive grinding

    NARCIS (Netherlands)

    Leeman, Michel; Noorduin, Wim L.; Millemaggi, Alessia; Vlieg, Elias; Meekes, Hugo; Enckevort, Willem J.P. van; Kaptein, Bernard; Kellogg, Richard M.

    2010-01-01

    The complete resolution of the conglomerate racemates of two amino acid derivatives susceptible to racemization in solution was achieved by slow crystallization from a supersaturated solution accompanied by cooling and abrasive grinding.

  10. On-line monitoring of technological process of material abrasive water jet cutting

    Czech Academy of Sciences Publication Activity Database

    Kinik, D.; Gánovská, B.; Hloch, Sergej; Monka, P.; Monková, K.; Hutyrová, Z.

    2015-01-01

    Roč. 22, č. 2 (2015), s. 351-357 ISSN 1330-3651 R&D Projects: GA MŠk ED2.1.00/03.0082 Institutional support: RVO:68145535 Keywords : abrasive water jet * vibrations * monitoring Subject RIV: JQ - Machines ; Tools Impact factor: 0.464, year: 2015 http://hrcak.srce.hr/index.php?show=clanak&id_clanak_jezik=203519

  11. Adaptation of high pressure water jets with abrasives for nuclear installations dismantling

    International Nuclear Information System (INIS)

    Rouviere, R.; Pinault, M.; Gasc, B.; Guiadeur, R.; Pilot, M.

    1989-01-01

    This report presents the work realized for adjust the cutting technology with high pressure water jet with abrasives for nuclear installation dismantling. It has necessited the conception and the adjustement of a remote tool and the realization of cutting tests with waste produce analysis. This technic can be ameliorated with better viewing systems and better fog suction systems

  12. Influence of sodium content on the properties of bioactive glasses for use in air abrasion.

    Science.gov (United States)

    Farooq, Imran; Tylkowski, Maxi; Müller, Steffen; Janicki, Tomasz; Brauer, Delia S; Hill, Robert G

    2013-12-01

    Air abrasion is used in minimally invasive dentistry for preparing cavities, while removing no or little sound dentine or enamel, and the use of bioactive glass (rather than alumina) as an abrasive could aid in tooth remineralization. Melt-derived bioactive glasses (SiO2-P2O5-CaO-CaF2-Na2O) with low sodium content (0 to 10 mol% Na2O in exchange for CaO) for increased hardness, high phosphate content for high bioactivity and fluoride content for release of fluoride and formation of fluorapatite were produced, and particles between 38 and 80 µm in size were used for cutting soda-lime silicate glass microscope slides and human enamel. Vickers hardness increased with decreasing Na2O content, owing to a more compact silicate network in low sodium content glasses, resulting in shorter cutting times. Cutting times using bioactive glass were significantly longer than using the alumina control (29 µm) when tested on microscope slides; however, glasses showed more comparable results when cutting human enamel. The bioactive glasses formed apatite in Tris buffer within 6 h, which was significantly faster than Bioglass® 45S5 (24 h), suggesting that the hardness of the glasses makes them suitable for air abrasion application, while their high bioactivity and fluoride content make them of interest for tooth remineralization.

  13. O coaching enquanto prática de desenvolvimento de recursos humanos

    OpenAIRE

    Soares, Luciana Rocha

    2013-01-01

    A presente investigação visa identificar os benefícios do coaching para o desenvolvimento de recursos humanos, procurando entender como esta prática contribui para o desenvolvimento de competências, para a melhoria de desempenhos e resultados organizacionais. Sendo uma pesquisa de natureza qualitativa, foram realizadas entrevistas semiestruturadas a 10 coaches profissionais, as quais foram submetidas a análise de conteúdo. Não representativos da população, os resultados obti...

  14. Study of abrasive wear process of lining of grinding chamber of vortex-acoustic disperser

    Science.gov (United States)

    Perelygin, D. N.

    2018-03-01

    The theoretical and experimental studies of the process of gas-abrasive wear of the lining of a vortex-acoustic disperser made it possible to establish the conditions and patterns of their occurrence and also to develop proposals for its reduction.

  15. Wear Resistance of Piston Sleeve Made of Layered Material Structure: MMC A356R, Anti-Abrasion Layer and FGM Interface

    Directory of Open Access Journals (Sweden)

    Hernik Szymon

    2016-09-01

    Full Text Available The aim of this paper is the numerical analysis of the one of main part of car engine – piston sleeve. The first example is for piston sleeve made of metal matrix composite (MMC A356R. The second improved material structure is layered. Both of them are comparison to the classical structure of piston sleeve made of Cr-Ni stainless steel. The layered material structure contains the anti-abrasion layer at the inner surface of piston sleeve, where the contact and friction is highest, FGM (functionally graded material interface and the layer of virgin material on the outer surface made of A356R. The complex thermo-elastic model with Archard's condition as a wear law is proposed. The piston sleeve is modelling as a thin walled cylindrical axisymmetric shell. The coupled between the formulation of thermo-elasticity of cylindrical axisymmetric shell and the Archard’s law with functionally changes of local hardness is proposed.

  16. Desenvolvimento Policêntrico na Europa : Uma reflexao critica sobre um conceito de politicas normativas

    NARCIS (Netherlands)

    Meijers, E.J.

    Durante a última década, o desenvolvimento policêntrico tornou-se um conceito-chave no desenvolvimento territorial europeu. Em muitos aspectos, é um conceito difuso que significa diferentes coisas para diferentes pessoas em diferentes escalas espaciais. Neste artigo, analisamos as variadas

  17. Artificial evolutionary approaches to produce smoother surface in magnetic abrasive finishing of hardened AISI 52100 steel

    Energy Technology Data Exchange (ETDEWEB)

    Teimouri, Reza; Baseri, Hamid [Babol University of Technology, Babol (Iran, Islamic Republic of)

    2013-02-15

    In this work, two models of feed forward back-propagation neural network (FFBP-NN) and adaptive neuro-fuzzy inference system (ANFIS) have been developed to predict the performance of magnetic abrasive finishing process, based on experimental data of literature. Input parameters of process are electromagnet's voltage, mesh number of abrasive particles, poles rotational speed and weight percent of abrasive particles, and also the output is percentage of surface roughness variation. In order to select the best model, a comparison between developed models has been done based on their mean absolute error (MAE) and root mean square error (RMSE). Moreover, optimization methods based on simulated annealing (SA) and particle swarm optimization (PSO) algorithms were used to maximize the percent of surface roughness variation and select the optimal process parameters. Results indicated that the models based on artificial intelligence predict much more precise values with respect to predictive regression model developed in main literature. Also, the ANFIS model had a lowest value of MAE and RMSE with respect to others. So it was used as an objective function to maximize the surface roughness variation by using SA and PSO. Comparison between the obtained optimal solutions and analysis of results in main literature indicated that SA and PSO could find the optimal answers logically and precisely.

  18. Tangential turning of Incoloy alloy 925 using abrasive water jet technology

    Czech Academy of Sciences Publication Activity Database

    Cárach, J.; Hloch, S.; Hlaváček, Petr; Ščučka, Jiří; Martinec, Petr; Petrů, J.; Zlámal, T.; Zeleňák, Michal; Monka, P.; Lehocká, D.; Krolczyk, J.

    2016-01-01

    Roč. 82, č. 9 (2016), s. 1747-1752 ISSN 0268-3768 R&D Projects: GA MŠk ED2.1.00/03.0082; GA MŠk(CZ) LO1406 Institutional support: RVO:68145535 Keywords : incoloy alloy 925 * abrasive water jet turning * traverse speed Subject RIV: JQ - Machines ; Tools Impact factor: 2.209, year: 2016 http://link.springer.com/article/10.1007%2Fs00170-015-7489-0

  19. Resistência de plantas daninhas aos herbicidas Weed resistance to herbicides

    Directory of Open Access Journals (Sweden)

    Pedro J. Christoffoleti

    1994-01-01

    Full Text Available A resistência de plantas daninhas aos herbicidas ocorre em função de um processo evolutivo. O desenvolvimento de biótipos de plantas daninhas resistentes é imposto pela agricultura moderna, através da pressão de seleção causada pelo uso intensivo dos herbicidas. O conhecimento dos mecanismos e fatores que favorecem o aparecimento de biótipos de plantas daninhas resistentes é fundamental para que técnicas de manejo sejam utilizadas no sentido de evitar ou retardar o aparecimento de plantas resistentes em uma área. São poucos os relatos ou citações de literatura no Brasil. Sendo assim, este trabalho de revisão procura relatar os principais avanços e descobertas na área de plantas daninhas resistentes aos herbicidas.Weed herbicide resistance has evolved from weed evolution. The modern agriculture is responsible for this evolution because of the intensive use of herbicides. The knowledge of mechanisms and factors that influence the weed herbicide resistance play an important role in the weed manegement techniques used to avoid or delay herbicide resistance appearence. There are not many report or scientific papers about herbi cide resistance in Brasil. Therefore, this literature review aims to provide information about the main advances and discoveries in the field of weed herbicide resistance.

  20. ADVANCED 3D LASER MICROSCOPY FOR MEASUREMENTS AND ANALYSIS OF VITRIFIED BONDED ABRASIVE TOOLS

    Directory of Open Access Journals (Sweden)

    WOJCIECH KAPLONEK

    2012-12-01

    Full Text Available In many applications, when a precise non-contact assessment of an abrasive tools’ surface is required, alternative measurement methods are often used. Their use offers numerous advantages (referential method as they introduce new qualities into routinely realized measurements. Over the past few years there has been a dynamic increase in the interest for using new types of classical confocal microscopy. These new types are often defined as 3D laser microscopy. This paper presents select aspects of one such method’s application – confocal laser scanning microscopy – for diagnostic analysis of abrasive tools. In addition this paper also looks at the basis for operation, the origins and the development of this measurement technique.The experimental part of this paper presents the select results of tests carried out on grinding wheel active surfaces with sintered microcrystalline corundum grains SG™ bound with glass-crystalline bond. The 3D laser measuring microscopes LEXT OLS3100 and LEXT OLS4000 by Olympus were used in the experiments. Analysis of the obtained measurement data was carried out in dedicated OLS 5.0.9 and OLS4100 2.1 programs, supported by specialist TalyMap Platinum 5.0 software. The realized experiments confirmed the possibility of using the offered measurement method. This concerns both the assessment of grinding wheel active surfaces and their defects, as well as the internal structures of the tools (grain-bond connections. The method presented is an interesting alternative to the typical methods used in the diagnostics of abrasive tools.

  1. Método Ágil aplicado ao desenvolvimento de software confiável baseado em componentes

    OpenAIRE

    Alan Braz

    2013-01-01

    Resumo: Os Métodos Ágeis, ou Desenvolvimento Ágil de Software (DAS), tem se popularizado, na última década, por meio de métodos como Extreme Programming (XP) e Scrum e isso fez com que fossem aplicadas no desenvolvimento de sistemas computacionais de diversos tamanhos, complexidades técnica e de domínio, e de rigor quanto à confiabilidade. Esse fato evidencia a necessidade de processos de desenvolvimento de software que sejam mais rigorosos e que possuam uma quantidade adequada de modelagem e...

  2. O desenvolvimento do conhecimento na Pesquisa e Desenvolvimento e o registro através de patentes no Brasil – uma experiência profissional

    Directory of Open Access Journals (Sweden)

    Cynthia Helena Soares Bouças Teixeira

    2017-11-01

    Full Text Available Este trabalho tem como objetivo fornecer um detalhamento sobre o processo de busca do conhecimento, partindo de uma ferramenta básica que é a informação. No contexto que envolve Pesquisa & Desenvolvimento, o conhecimento pode ser estruturado para o desenvolvimento de novas tecnologias, produtos ou processos, em que o registro do conhecimento pode ocorrer  através das patentes. Dado que é preciso conhecer a legislação do país de depósito,trataremos mais especificamente do sistema de registro de patentes brasileiro denominado Instituto Nacional da Propriedade Intelectual – INPI. As reflexões apresentadas são provenientes de uma experiência profissional.

  3. Disc Bit Abrasion Parameters in TBM Tunnelling regarded exemplarily for the Gotthard Base Tunnel

    Directory of Open Access Journals (Sweden)

    Edmund a Wax

    2005-11-01

    Full Text Available In this article the author presents Amund Bruland’s empirical approach to determine the disc bit abrasion of TBMs (Tunnel Boring Machines, transforms the respective empirical dependencies into approximated mathematical relations and verifies them exemplarily for the currently constructed Gotthard Base Tunnel.

  4. Comparison of the structure and wear resistance of Al2O3 -13 wt%TiO2 coatings made by GSP and WSP plasma process with two different powders

    Czech Academy of Sciences Publication Activity Database

    Ageorges, H.; Ctibor, Pavel

    2008-01-01

    Roč. 202, č. 18 (2008), s. 4362-4368 ISSN 0257-8972 R&D Projects: GA AV ČR 1QS200430560 Institutional research plan: CEZ:AV0Z20430508 Keywords : Alumina * titania * plasma spraying * wear resistance * slurry abrasion Subject RIV: JH - Ceramics, Fire-Resistant Materials and Glass Impact factor: 1.860, year: 2008

  5. Desenvolvimento moral: considerações teóricas a partir de uma abordagem sociocultural construtivista

    Directory of Open Access Journals (Sweden)

    Martins Lincoln Coimbra

    2001-01-01

    Full Text Available Partindo da análise de trabalhos tradicionalmente realizados na área de desenvolvimento moral, o artigo sinaliza a necessidade de desenvolver uma abordagem teórica que trate o tema dentro de um enfoque que considere os aspectos socioculturais, cognitivos e afetivos. A questão central reside em abordar de forma sistêmica e integrada a dinâmica do desenvolvimento moral do indivíduo, resgatando a dimensão interativa e contextual envolvida na resolução dos conflitos morais e no desenvolvimento de crenças e valores. O trabalho parte dos pressupostos da perspectiva histórica socio-cultural construtivista do desenvolvimento humano, explicitando as exigências metodológicas implicadas na adoção dos conceitos e categorias utilizados no âmbito de tal perspectiva.

  6. Desenvolvimento moral: considerações teóricas a partir de uma abordagem sociocultural construtivista

    Directory of Open Access Journals (Sweden)

    Lincoln Coimbra Martins

    Full Text Available Partindo da análise de trabalhos tradicionalmente realizados na área de desenvolvimento moral, o artigo sinaliza a necessidade de desenvolver uma abordagem teórica que trate o tema dentro de um enfoque que considere os aspectos socioculturais, cognitivos e afetivos. A questão central reside em abordar de forma sistêmica e integrada a dinâmica do desenvolvimento moral do indivíduo, resgatando a dimensão interativa e contextual envolvida na resolução dos conflitos morais e no desenvolvimento de crenças e valores. O trabalho parte dos pressupostos da perspectiva histórica socio-cultural construtivista do desenvolvimento humano, explicitando as exigências metodológicas implicadas na adoção dos conceitos e categorias utilizados no âmbito de tal perspectiva.

  7. Comprehensive study of the abrasive wear and slurry erosion behavior of an expanded system of high chromium cast iron and microstructural modification for enhanced wear resistance

    Science.gov (United States)

    Chung, Reinaldo Javier

    High chromium cast irons (HCCIs) have been demonstrated to be an effective material for a wide range of applications in aggressive environments, where resistances to abrasion, erosion and erosion-corrosion are required. For instance, machinery and facilities used in mining and extraction in Alberta's oil sands suffer from erosion and erosion-corrosion caused by silica-containing slurries, which create challenges for the reliability and maintenance of slurry pumping systems as well as other processing and handling equipment. Considerable efforts have been made to determine and understand the relationship between microstructural features of the HCCIs and their wear performance, in order to guide the material selection and development for specific service conditions with optimal performance. The focus was previously put on a narrow group of compositions dictated by ASTM A532. However, with recent advances in casting technology, the HCCI compositional range can be significantly expanded, which potentially brings new alloys that can be superior to those which are currently employed. This work consists of three main aspects of study. The first one is the investigation of an expanded system of white irons with their composition ranging from 1 to 6 wt.% C and 5 to 45 wt.% Cr, covering 53 alloys. This work has generated wear and corrosion maps and established correlation between the performance and microstructural features for the alloys. The work was conducted in collaboration with the Materials Development Center of Weir Minerals in Australia, and the results have been collected in a database that is used by the company to guide materials selection for slurry pump components in Alberta oil sands and in other mining operations throughout the world. The second part consists of three case studies on effects of high chromium and high carbon, respectively, on the performance of the HCCIs. The third aspect is the development of an approach to enhance the wear resistance of

  8. Evaluation of planarization performance for a novel alkaline copper slurry under a low abrasive concentration

    International Nuclear Information System (INIS)

    Jiang Mengting; Liu Yuling; Yuan Haobo; Chen Guodong; Liu Weijuan

    2014-01-01

    A novel alkaline copper slurry that possesses a relatively high planarization performance is investigated under a low abrasive concentration. Based on the action mechanism of CMP, the feasibility of using one type of slurry in copper bulk elimination process and residual copper elimination process, with different process parameters, was analyzed. In addition, we investigated the regular change of abrasive concentration effect on copper and tantalum removal rate and within wafer non-uniformity (WIWNU) in CMP process. When the abrasive concentration is 3 wt%, in bulk elimination process, the copper removal rate achieves 6125 Å/min, while WIWNU is 3.5%, simultaneously. In residual copper elimination process, the copper removal rate is approximately 2700 Å/min, while WIWNU is 2.8%. Nevertheless, the tantalum removal rate is 0 Å/min, which indicates that barrier layer isn't eliminated in residual copper elimination process. The planarization experimental results show that an excellent planarization performance is obtained with a relatively high copper removal rate in bulk elimination process. Meanwhile, after residual copper elimination process, the dishing value increased inconspicuously, in a controllable range, and the wafer surface roughness is only 0.326 nm (sq < 1 nm) after polishing. By comparison, the planarization performance and surface quality of alkaline slurry show almost no major differences with two kinds of commercial acid slurries after polishing. All experimental results are conducive to research and improvement of alkaline slurry in the future. (semiconductor technology)

  9. Influence of sodium content on the properties of bioactive glasses for use in air abrasion

    International Nuclear Information System (INIS)

    Farooq, Imran; Brauer, Delia S; Hill, Robert G; Tylkowski, Maxi; Müller, Steffen; Janicki, Tomasz

    2013-01-01

    Air abrasion is used in minimally invasive dentistry for preparing cavities, while removing no or little sound dentine or enamel, and the use of bioactive glass (rather than alumina) as an abrasive could aid in tooth remineralization. Melt-derived bioactive glasses (SiO 2 –P 2 O 5 –CaO–CaF 2 –Na 2 O) with low sodium content (0 to 10 mol% Na 2 O in exchange for CaO) for increased hardness, high phosphate content for high bioactivity and fluoride content for release of fluoride and formation of fluorapatite were produced, and particles between 38 and 80 µm in size were used for cutting soda-lime silicate glass microscope slides and human enamel. Vickers hardness increased with decreasing Na 2 O content, owing to a more compact silicate network in low sodium content glasses, resulting in shorter cutting times. Cutting times using bioactive glass were significantly longer than using the alumina control (29 µm) when tested on microscope slides; however, glasses showed more comparable results when cutting human enamel. The bioactive glasses formed apatite in Tris buffer within 6 h, which was significantly faster than Bioglass® 45S5 (24 h), suggesting that the hardness of the glasses makes them suitable for air abrasion application, while their high bioactivity and fluoride content make them of interest for tooth remineralization. (paper)

  10. Colour improvement and stability of white spot lesions following infiltration, micro-abrasion, or fluoride treatments in vitro.

    Science.gov (United States)

    Yetkiner, Enver; Wegehaupt, Florian; Wiegand, Annette; Attin, Rengin; Attin, Thomas

    2014-10-01

    White spot lesions (WSLs) are unwelcome side effects of fixed appliances that compromise the treatment outcome. Recently, infiltration of WSLs has been introduced as a viable treatment alternative. The objective was to evaluate the colour improvement of WSLs and their stability against discolouration following infiltration, fluoride, or micro-abrasion treatments in vitro. Artificial WSLs were created in bovine enamel (N = 96) using acidic buffer solution (pH 5, 10 days) and were randomly allocated to four groups. Specimens were treated with infiltration (Icon, DMG), fluoride (Elmex Caries Protection, GABA), and micro-abrasion (Opalustre, Ultradent) or remained untreated (control). Groups were discoloured for 24 hours in tea or tea + citric acid. Colour components and visible colour change (L*, a*, b*, ΔE) were measured spectrophotometrically on following time points: baseline, after WSL formation, after treatment, and during discolouration (8, 16, and 24 hours). Data were analysed using Kruskal-Wallis and Mann-Whitney tests. WSL formation increased (L*) in all groups. Only infiltration reduced this effect to baseline. Highest ΔE improvement was obtained by infiltration and micro-abrasion followed by fluoride. This improvement was stable only for infiltration during discolouration. L*, a*, and b* changed significantly during discolouration in all groups except infiltration. Within the same treatment group, discolouration solutions did not differ significantly. In vitro testing cannot replicate the actual mode of colour improvement or stability but can be used for ranking materials and techniques. Infiltration and micro-abrasion treatments were capable of diminishing the whitish appearance of WSLs. Only infiltrated WSLs were stable following discolouration challenge. © The Author 2014. Published by Oxford University Press on behalf of the European Orthodontic Society. All rights reserved. For permissions, please email: journals.permissions@oup.com.

  11. U-Pb dating by zircon dissolution method using chemical abrasion

    Energy Technology Data Exchange (ETDEWEB)

    Takehara, Lucy, E-mail: lucytakehara@gmail.com.br [Servico Geologico do Brasil (CPRM), Brasilia, DF (Brazil); Chemale Junior, Farid [Universidade de Brasilia (UnB), Brasilia, DF (Brazil). Inst. de Geociencias. Lab. de Geocronologia; Hartmann, Leo A. [Universidade Federal do Rio Grande do Sul (UFRS), Porto Alegre, RS (Brazil). Inst. de Geociencias; Dussin, Ivo A.; Kawashita, Koji [Universidade de Sao Paulo (USP), SP, (Brazil). Centro de Pesquisa Geocronologicas

    2012-06-15

    Chemical abrasion was carried out on zircons grains of the Temora II standard for U-Pb dating prior to analyses using in situ Laser Ablation-Multi Collector Ion Coupled Plasma Mass Spectrometer (LA-ICPMS) followed by the Isotope Dissolution Thermal Ionization Mass Spectrometer (ID-TIMS) method. The proposed methodology was herein applied in order to reduce primarily the effects of secondary Pb loss, the presence of common lead and/or silicate impurities. Nine Temora II zircon grains were analyzed by the laser ablation method yielding an age of 418.3 +- 4.3 Ma. Zircon grains of a same population were separated for chemical abrasion before dissolution and mass spectrometry analyses. Six fractions of them were separated for isotope dissolution using {sup 235}U-{sup 205}Pb mixed spike after we have checked and assured the laboratory conditions of low blank values for total Pb of less than 2 pg/g. The obtained U-Pb zircon age by the ID-TIMS method was 415.7 +- 1.8 Ma (error 0.43 %) based on four successful determinations. The results are consistent with the published ages for the Temora diorite (Temora I - 416.75 +- 1.3 Ma; Temora II - 416.78 +- 0.33 Ma) and established as 416 +- 0.33 Ma. The technique is thus recommended for high precision U-Pb zircon analyses (error < 1 %), mainly for high resolution stratigraphic studies of Phanerozoic sequences. (author)

  12. Effect of Crack Tip Stress Concentration Factor on Fracture Resistance in Vacuum Environment

    Science.gov (United States)

    2015-01-20

    indicate: (1) in all alloys, the fracture resistance is highest for blunt-notches (smaller Kt), and is lowest for fatigue -sharpened precracked...paths are transgranular and the fracture mode is ductile void coalescence in all cases, irrespective of the stress concentration factor. 20-01-2015...because of corrosion and/or various loading conditions such as fatigue , fretting, abrasion, etc. Also, the geometry of the structure may cause an

  13. Avaliação do crescimento e desenvolvimento de crianças institucionalizadas

    Directory of Open Access Journals (Sweden)

    Caroline Magna Pessoa Chaves

    2013-10-01

    Full Text Available O estudo objetivou avaliar o crescimento e desenvolvimento de crianças de 0 a 6 anos institucionalizadas. Abordagem descritiva, transversal e de natureza quantitativa. Foi realizado em um abrigo da Secretaria do Trabalho e Desenvolvimento Social do Governo do Estado do Ceará, nos meses de março e abril de 2011. A amostra foi composta por 44 crianças. Prevaleceram crianças de sexo masculino (59,1%; faixa etária entre 24 a 72 meses (56,8%, e tempo de abrigamento superior a um ano (72,7%. Verificou-se que as crianças estavam na faixa de normalidade nutricional. Porém, 65,9% das crianças não alcançaram pelo menos um dos marcos do desenvolvimento propostos pelo Ministério da Saúde. O estudo possibilitou uma reflexão sobre como as crianças residentes em abrigos estão sendo assistidas pela equipe de saúde, tornando-se necessário realizar o acompanhamento de seu crescimento e desenvolvimento, a fim de intervir sobre as alterações encontradas.

  14. Rock Abrasion and Ventifact Formation on Mars from Field Analog, Theoretical, and Experimental Studies

    Science.gov (United States)

    Bridges, N. T.; Laity, J. E.

    2001-01-01

    Rocks observed by the Viking Landers and Pathfinder Lander/Sojourner rover exhibit a suite of perplexing rock textures. Among these are pits, spongy textures, penetrative flutes, lineaments, crusts, and knobs Fluvial, impact, chemical alteration, and aeolian mechanisms have been proposed for many of these. In an effort to better understand the origin and characteristics of Martian rock textures, abraded rocks in the Mojave Desert and other regions have been studied. We find that most Martian rock textures, as opposed to just a few, bear close resemblance to terrestrial aeolian textures and can most easily be explained by wind, not other, processes. Flutes, grooves, and some pits on Mars are consistent with abrasion by saltating particles, as described previously. However, many other rock textures probably also have an aeolian origin. Sills at the base of rocks that generally lie at high elevations, such as Half Dome, are consistent with such features on Earth that are related to moats or soil ramps that shield the basal part of the rock from erosion. Crusts consisting of fluted fabrics, such as those on Stimpy and Chimp, are similar to fluted crusts on Earth that spall off over time. Knobby and lineated rocks are similar to terrestrial examples of heterogeneous rocks that differentially erode. The location of specific rock textures on Mars also gives insight into their origin. Many of the most diagnostic ventifacts found at the Pathfinder site are located on rocks that lie near the crests or the upper slopes of ridges. On Earth, the most active ventifact formation occurs on sloped or elevated topography, where windflow is accelerated and particle kinetic energy and flux are increased. Integrated 0 together, these observations point to significant aeolian 0 modification of rocks on Mars and cast doubt on whether many primary textures resulting from other processes are preserved. Experimental simulations of abrasion in the presence of abundant sand indicate that

  15. The Optimum Production Method for Quality Improvement of Recycled Aggregates Using Sulfuric Acid and the Abrasion Method

    Directory of Open Access Journals (Sweden)

    Haseog Kim

    2016-07-01

    Full Text Available There has been increased deconstruction and demolition of reinforced concrete structures due to the aging of the structures and redevelopment of urban areas resulting in the generation of massive amounts of construction. The production volume of waste concrete is projected to increase rapidly over 100 million tons by 2020. However, due to the high cement paste content, recycled aggregates have low density and high absorption ratio. They are mostly used for land reclamation purposes with low added value instead of multiple approaches. This study was performed to determine an effective method to remove cement paste from recycled aggregates by using the abrasion and substituting the process water with acidic water. The aim of this study is to analyze the quality of the recycled fine aggregates produced by a complex method and investigate the optimum manufacturing conditions for recycled fine aggregates based on the design of experiment. The experimental parameters considered were water ratio, coarse aggregate ratio, and abrasion time and, as a result of the experiment, data concerning the properties of recycled sand were obtained. It was found that high-quality recycled fine aggregates can be obtained with 8.57 min of abrasion-crusher time and a recycled coarse aggregate ratio of over 1.5.

  16. Using of abrasive water jet for measurement of residual stress in railway wheels

    Czech Academy of Sciences Publication Activity Database

    Hlaváček, Petr; Brumek, J.; Horsák, L.

    2012-01-01

    Roč. 2, č. 19 (2012), s. 387-390 ISSN 1330-3651 R&D Projects: GA MŠk ED2.1.00/03.0082 Institutional support: RVO:68145535 Keywords : abrasive water jet * railway wheel * residual stress Subject RIV: JQ - Machines ; Tools Impact factor: 0.601, year: 2012 http://hrcak.srce.hr/index.php?show=clanak&id_clanak_jezik=124848

  17. Effect of cuticular abrasion and recovery on water loss rates in queens of the desert harvester ant Messor pergandei.

    Science.gov (United States)

    Johnson, Robert A; Kaiser, Alexander; Quinlan, Michael; Sharp, William

    2011-10-15

    Factors that affect water loss rates (WLRs) are poorly known for organisms in natural habitats. Seed-harvester ant queens provide an ideal system for examining such factors because WLRs for mated queens excavated from their incipient nests are twofold to threefold higher than those of alate queens. Indirect data suggest that this increase results from soil particles abrading the cuticle during nest excavation. This study provides direct support for the cuticle abrasion hypothesis by measuring total mass-specific WLRs, cuticular abrasion, cuticular transpiration, respiratory water loss and metabolic rate for queens of the ant Messor pergandei at three stages: unmated alate queens, newly mated dealate queens (undug foundresses) and mated queens excavated from their incipient nest (dug foundresses); in addition we examined these processes in artificially abraded alate queens. Alate queens had low WLRs and low levels of cuticle abrasion, whereas dug foundresses had high WLRs and high levels of cuticle abrasion. Total WLR and cuticular transpiration were lowest for alate queens, intermediate for undug foundresses and highest for dug foundresses. Respiratory water loss contributed ~10% of the total WLR and was lower for alate queens and undug foundresses than for dug foundresses. Metabolic rate did not vary across stages. Total WLR and cuticular transpiration of artificially abraded alate queens increased, whereas respiratory water loss and metabolic rate were unaffected. Overall, increased cuticular transpiration accounted for essentially all the increased total water loss in undug and dug foundresses and artificially abraded queens. Artificially abraded queens and dug foundresses showed partial recovery after 14 days.

  18. Particulate Matter from the Road Surface Abrasion as a Problem of Non-Exhaust Emission Control

    Directory of Open Access Journals (Sweden)

    Magdalena Penkała

    2018-01-01

    Full Text Available Along with house heating and industry, emissions from road traffic (exhaust and tire, brake, car body or road surface abrasions are one of the primary sources of particulate matter (PM in the atmosphere in urban areas. Though numerous regulations and vehicle-control mechanisms have led to a significant decline of PM emissions from vehicle exhaust gases, other sources of PM remain related to road and car abrasion are responsible for non-exhaust emissions. Quantifying these emissions is a hard problem in both laboratory and field conditions. First, we must recognize the physicochemical properties of the PM that is emitted by various non-exhaust sources. In this paper, we underline the problem of information accessibility with regards to the properties and qualities of PM from non-exhaust sources. We also indicate why scarce information is available in order to find the possible solution to this ongoing issue.

  19. Mathematical model of temperature field distribution in thin plates during polishing with a free abrasive

    Directory of Open Access Journals (Sweden)

    Avilov Alex

    2017-01-01

    Full Text Available The purpose of this paper is to estimate the dynamic characteristics of the heating process of thin plates during polishing with a free abrasive. A mathematical model of the temperature field distribution in space and time according to the plate thickness is based on Lagrange equation of the second kind in the thermodynamics of irreversible processes (variation principle Bio. The research results of thermo elasticity of thin plates (membranes will allow to correct the modes of polishing with a free abrasive to receive the exact reflecting surfaces of satellites reflector, to increase temperature stability and the ability of radio signal reflection, satellite precision guidance. Calculations of temperature fields in thin plates of different thicknesses (membranes is held in the Excel, a graphical characteristics of temperature fields in thin plates (membranes show non-linearity of temperature distribution according to the thickness of thin plates (membranes.

  20. Turning of wood plastic composites by water jet and abrasive water jet

    Czech Academy of Sciences Publication Activity Database

    Hutyrová, Z.; Ščučka, Jiří; Hloch, Sergej; Hlaváček, Petr; Zeleňák, Michal

    -, September 2015 (2015), s. 1-9 ISSN 0268-3768 R&D Projects: GA MŠk ED2.1.00/03.0082; GA MŠk(CZ) LO1406 Institutional support: RVO:68145535 Keywords : wood plastic composite * water jet * size of abrasive particles * surface quality * traverse speed Subject RIV: JQ - Machines ; Tools Impact factor: 1.568, year: 2015 http://link.springer.com/article/10.1007/s00170-015-7831-6

  1. Turning of wood plastic composites by water jet and abrasive water jet

    Czech Academy of Sciences Publication Activity Database

    Hutyrová, Z.; Ščučka, Jiří; Hloch, Sergej; Hlaváček, Petr; Zeleňák, Michal

    2016-01-01

    Roč. 84, 5-8 (2016), s. 1615-1623 ISSN 0268-3768 R&D Projects: GA MŠk(CZ) LO1406; GA MŠk ED2.1.00/03.0082 Institutional support: RVO:68145535 Keywords : wood plastic composite * water jet * turning * traverse speed * size of abrasive particles Subject RIV: JQ - Machines ; Tools Impact factor: 2.209, year: 2016 http://link.springer.com/article/10.1007/s00170-015-7831-6

  2. Nacionalismo e desenvolvimento

    Directory of Open Access Journals (Sweden)

    Paulo Nogueira Batista Jr.

    2007-03-01

    Full Text Available Este texto discute o nacionalismo, tomando emprestadas algumas proposições de um filósofo declarada e radicalmente antinacionalista, Friedrich Nietzsche. Procura-se argumentar que, ressalvados os raros casos de integração regional profunda, o nacionalismo é, na prática, o único caminho para o desenvolvimento econômico e a melhoria das condições de vida das populações na periferia da economia internacional.This paper discusses nationalism, borrowing some propositions from a philosopher who was openly and radically antinationalist, Friedrich Nietzsche. It argues that, with the exception of the rare cases of deep regional integration, nationalism is, in practice, the only route to economic development and the improvement of the standards of living of populations in the periphery of the international economy.

  3. Influence of silicon content and heat treatment on wear resistance of white chromium cast irons under high speed solidification conditions; Influencia del contenido de silicio y el tratamiento termico en la resistencia al desgaste de fundiciones blancas al cromo en condiciones de rapida solidificacion

    Energy Technology Data Exchange (ETDEWEB)

    Goyo, L.; Varela, A.; Verhaege, M.; Garcia, A.; Mier, J.; Moors, M.

    2012-11-01

    The influence of silicon content and heat treatment on microstructure, abrasive and dry friction wear resistance of a 3 % C, 12 % Cr cast iron, under fast solidification conditions is studied. The fast solidification condition diminishes the carbide volume and the silicon content increases their dispersion and finesses. All matrixes obtained were perlitics, whit different finesses. No intermediate transformation products were noticed. Hardness had little variation. Austenization treatment show little effectivity, with tendency to increase wear in reference to as cast and maintenance treatments. Behavior under dry friction and abrasive wear were similar under test conditions applied whit more influence of carbide morphology in the abrasive wear conditions. (Author) 32 refs.

  4. A comparison of the tribological behaviour of Y-TZP in tea and coffee under micro-abrasion conditions

    International Nuclear Information System (INIS)

    Sharifi, S; Stack, M M

    2013-01-01

    The micro-abrasion of Y-TZP, a candidate dental restorative material, was investigated in a range of caffeine-containing solutions which included tea and coffee. Additions of sugar and milk were used to test the effects of viscosity and pH on the wear rate. The results indicated a significant increase in wear rate in the various solutions, with some correlation between wear rate and increases in viscosity and this was linked to enhance particle entrainment in the more viscous solutions. The generally lower wear rate in tea compared to coffee was associated with a longer ageing period in this solution before uniform wear was observed. Micro-abrasion maps were used to characterize the differences in performance for the material in the environments studied. (paper)

  5. A comparison of the tribological behaviour of Y-TZP in tea and coffee under micro-abrasion conditions

    Science.gov (United States)

    Sharifi, S.; Stack, M. M.

    2013-10-01

    The micro-abrasion of Y-TZP, a candidate dental restorative material, was investigated in a range of caffeine-containing solutions which included tea and coffee. Additions of sugar and milk were used to test the effects of viscosity and pH on the wear rate. The results indicated a significant increase in wear rate in the various solutions, with some correlation between wear rate and increases in viscosity and this was linked to enhance particle entrainment in the more viscous solutions. The generally lower wear rate in tea compared to coffee was associated with a longer ageing period in this solution before uniform wear was observed. Micro-abrasion maps were used to characterize the differences in performance for the material in the environments studied.

  6. A new eye gel containing sodium hyaluronate and xanthan gum for the management of post-traumatic corneal abrasions

    Directory of Open Access Journals (Sweden)

    Faraldi F

    2012-05-01

    Full Text Available Francesco Faraldi,1 Vincenzo Papa,2 Debora Santoro,2 Daria Rasà,2 Annamaria L Mazza,2 Maria M Rabbione,1 Simona Russo21Department of Ophthalmology III, Presidio Ospedaliero Oftalmico, Torino, Italy; 2SIFI SpA, Catania, ItalyPurpose: The aim of this study was to investigate the effects of an ophthalmic gel containing sodium hyaluronate and xanthan gum in addition to the antibiotic netilmicin in the management of traumatic corneal abrasions.Patients and methods: Patients with traumatic corneal abrasions were randomly treated as follows: Group A (n = 20 with an occlusive patching for 12 hours plus one drop of an eye gel containing 0.15% sodium hyaluronate, 1% xanthan gum and 0.3% netilmicin qid for 5 days; and Group B (n = 20 with an occlusive patching for 2–3 days plus one application of 0.3% netilmicin ophthalmic ointment qid for 5 days. All patients were evaluated after the third and seventh day by slit-lamp examination, fluorescein staining, and corneal defect photograph in order to assess corneal re-epithelialization. Conjunctival hyperaemia, lid oedema, subjective symptoms of discomfort, and conjunctival swabs were also evaluated.Results: No statistically significant difference was observed between the groups in terms of the extent of corneal healing after 3 days of treatment. Both treatments were also highly effective in decreasing the erosion score and the conjunctival hyperemia (P < 0.0001, P < 0.005, respectively without any significant difference between the two types of treatment. Subjective symptoms of discomfort and conjunctival swabs were also evaluated.Conclusion: In the management of traumatic corneal abrasions, the administration of an eye gel containing sodium hyaluronate and xanthan gum is able to reduce the length of occlusive patching. In addition, the presence of netilmicin guarantees good antibiotic prophylaxis during the wound repair process.Keywords: netilmicin, xanthan gum, wound healing, patching, corneal abrasion

  7. Saúde e desenvolvimento Healthcare and development

    Directory of Open Access Journals (Sweden)

    Ana Luiza D'Ávila Viana

    2007-11-01

    Full Text Available Considerando que os modernos sistemas de saúde são o resultado da complexa interação de processos econômicos, políticos e sociais, o objetivo do trabalho é discutir a relação entre saúde e desenvolvimento no Brasil, mostrando que o esgotamento do modelo liberal de política econômica abre nova perspectiva para a retomada do desenvolvimento, entendido como combinação entre crescimento da economia, mudanças na estrutura produtiva e melhora das condições de vida da população. O complexo produtivo da saúde joga papel decisivo nesse processo, pois constitui um campo em que inovação tecnológica e acumulação de capital geram oportunidades de investimento, trabalho e renda, além de produzir avanços importantes para melhorar o estado de saúde das pessoas. A recente adoção de políticas públicas voltadas para articular, de forma positiva, aspectos da política econômica e da política social revela que a questão do desenvolvimento nacional ganhou nova centralidade na agenda governamental, o que abre a perspectiva de maior integração entre a lógica econômica e a lógica sanitária. Entretanto, é preciso reconhecer que o Brasil ainda não logrou alcançar uma associação virtuosa entre saúde e desenvolvimento.As modern healthcare systems are the outcome of complex interactions among economic, political and social processes, the purpose of this paper is to discuss the links between health and development in Brazil, showing that the depletion of the liberal economic policy model paves the way for a return to development, understood as a blend of economic growth, changes in the production structure and better living standards. The healthcare production complex plays a crucial role in this process, as a field where technological innovation and capital build-up generate opportunities for investment, work and income, in addition to spurring major steps forward in terms of upgrading individual health. The recent adoption of

  8. Study on Abrasive Wear of Brake Pad in the Large-megawatt Wind Turbine Brake Based on Deform Software

    Science.gov (United States)

    Zhang, Shengfang; Hao, Qiang; Sha, Zhihua; Yin, Jian; Ma, Fujian; Liu, Yu

    2017-12-01

    For the friction and wear issues of brake pads in the large-megawatt wind turbine brake during braking, this paper established the micro finite element model of abrasive wear by using Deform-2D software. Based on abrasive wear theory and considered the variation of the velocity and load in the micro friction and wear process, the Archard wear calculation model is developed. The influence rules of relative sliding velocity and friction coefficient in the brake pad and disc is analysed. The simulation results showed that as the relative sliding velocity increases, the wear will be more serious, while the larger friction coefficient lowered the contact pressure which released the wear of the brake pad.

  9. Properties of pre-cast terrazzo tiles and recommended specifications Propriedades de telhas de terrazzo pré-moldadas e especificações recomendadas

    Directory of Open Access Journals (Sweden)

    G. Karam

    2009-03-01

    Full Text Available A targeted experimental program was carried out to establish basic reference physical and mechanical properties of commercially available pre-cast marble chip terrazzo tiles and to investigate the effects of varying manufacturing process parameters on those properties. The transverse strength, density, water absorption, and abrasion resistance were measured as a function of casting pressure and residence time in the casting mold for a standard mix design. A simple surface abrasion index test was developed and applied comparing pre-cast terrazzo tiles with reference natural tiling stones. Recommendations for improving existing specifications and developing quality control measures are presented.Foi feito um programa experimental direcionado para estabelecer propriedades físicas e mecânicas como referências básicas de telhas de terrazzo de peças de mármore pré-moldadas disponíveis comercialmente e para investigar os efeitos de vários parâmetros de processo de fabricação nessas propriedades. A resistência transversal, a densidade, a absorção de água e a resistência ao desgaste foram medidas em função da pressão de moldagem e do tempo de residência do molde de um projeto de mistura padrão. Um teste simples de índice de desgaste de superfície foi desenvolvido e aplicado na comparação de telhas de terrazzo pré-moldadas com pedras de telhas naturais de referência. As recomendações para a melhoria das especificações existentes e o desenvolvimento de medidas para controle de qualidade são apresentadas.

  10. CONTROL SYSTEM EVALUATION AND IMPLEMENTATION FOR THE ABRASIVE MACHINING PROCESS ON WOOD

    OpenAIRE

    Stephen Jackson; Richard Lemaster; Daniel E. Saloni

    2011-01-01

    Continuous process improvement and automation have proven to be powerful tools for the wood processing industries in order to obtain better final product quality and thus increase profits. Abrasive machining represents an important and relevant process in the manufacturing and processing of wood products, which also implies high cost of materials and labor; therefore, special attention to this process is necessary. The objective of this work was to evaluate and demonstrate a process control s...

  11. Standardization of a Volumetric Displacement Measurement for Two-Body Abrasion Scratch Test Data Analysis

    Science.gov (United States)

    Street, K. W. Jr.; Kobrick, R. L.; Klaus, D. M.

    2011-01-01

    A limitation has been identified in the existing test standards used for making controlled, two-body abrasion scratch measurements based solely on the width of the resultant score on the surface of the material. A new, more robust method is proposed for analyzing a surface scratch that takes into account the full three-dimensional profile of the displaced material. To accomplish this, a set of four volume- displacement metrics was systematically defined by normalizing the overall surface profile to denote statistically the area of relevance, termed the Zone of Interaction. From this baseline, depth of the trough and height of the plowed material are factored into the overall deformation assessment. Proof-of-concept data were collected and analyzed to demonstrate the performance of this proposed methodology. This technique takes advantage of advanced imaging capabilities that allow resolution of the scratched surface to be quantified in greater detail than was previously achievable. When reviewing existing data analysis techniques for conducting two-body abrasive scratch tests, it was found that the ASTM International Standard G 171 specified a generic metric based only on visually determined scratch width as a way to compare abraded materials. A limitation to this method was identified in that the scratch width is based on optical surface measurements, manually defined by approximating the boundaries, but does not consider the three-dimensional volume of material that was displaced. With large, potentially irregular deformations occurring on softer materials, it becomes unclear where to systematically determine the scratch width. Specifically, surface scratches on different samples may look the same from a top view, resulting in an identical scratch width measurement, but may vary in actual penetration depth and/or plowing deformation. Therefore, two different scratch profiles would be measured as having identical abrasion properties, although they differ

  12. Investigation of Sandwich Material Surface Created by Abrasive Water Jet (AWJ) via Vibration Emission

    Czech Academy of Sciences Publication Activity Database

    Hreha, P.; Hloch, S.; Monka, P.; Monková, K.; Knapčíková, L.; Hlaváček, Petr; Zeleňák, Michal; Samardžič, I.; Kozak, D.

    2013-01-01

    Roč. 53, č. 1 (2013), s. 29-32 ISSN 0543-5846 Institutional support: RVO:68145535 Keywords : sandwich material * stainless steel * abrasive water jet cutting Subject RIV: JJ - Other Materials Impact factor: 0.755, year: 2013 http://public.carnet.hr/metalurg/Metalurgija/2014_vol_53/No_1/MET_53_1_29-32_Hreha.pdf

  13. Biopolítica e Desenvolvimento? Foucault e Agamben sobre Estado, Governo e Violência

    Directory of Open Access Journals (Sweden)

    Guilherme F. W. Radomsky

    2015-06-01

    Full Text Available Este artigo analisa as relações entre biopolítica e desenvolvimento sob o ângulo das noções de Estado, governo e violência. O objetivo consiste em examinar elementos analíticos que gravitam em torno de perspectivas críticas do desenvolvimento buscando um eixo interpretativo sobre a ambivalência das ações do Estado a partir de duas possibilidades teóricas que convergem no pensamento de Giorgio Agamben: a análise do biopoder e do governo em Foucault e as articulações entre violência e lei que remetem a Walter Benjamin. A reflexão sobre os argumentos teóricos é realizada examinando-se dados oriundos de pesquisa de abordagem qualitativa sobre políticas para a agricultura ecológica no sul do Brasil. As conclusões mostram que o desenvolvimento e seus benefícios podem ser problematizados pelo olhar do biopoder e da violência, que reconfiguram o que seja desenvolvimento, menos como expansão do bem-estar e mais como impulso modernizante de mudança que se ampara em administrar a vida.

  14. A Study on Abrasive Wear Behavior of Spacer Grid Materials for Nuclear Power Plant

    Energy Technology Data Exchange (ETDEWEB)

    Park, J. M.; Kim, J. H. [Chungnam National University, Daejeon (Korea, Republic of); Park, J. K.; Jeon, K. L. [Korea Nuclear Fuel, Daejeon (Korea, Republic of)

    2010-10-15

    Spacer grid is one of the key components of a light water reactor (LWR) fuel assembly. The most important function of it is to hold the fuel rods to maintain the distance between the fuel rods inside a fuel assembly. At the reactor core in operating power plants, a fretting damage has been frequently reported between a nuclear fuel rod and its supporting spring/dimple of the fuel assemblies. This is due to a flow induced vibration (FIV), Which results from the primary coolant that rapidly passes around the fuel rod to remove the excess heat generated by the nuclear reaction. Fretting damage is generally caused by fretting wear, which includes various wear mechanisms such as an oxidative, adhesive, abrasive wear, etc., or fretting fatigue, which includes a surface or bulk fatigue. The purpose of the present work are to investigate the variation of the materials with increasing number of cycles and sliding velocity under abrasive wear test and to examine the wear mechanism at each test condition

  15. Estudo longitudinal do desenvolvimento da comunicação em diversas economias mundiais.

    Directory of Open Access Journals (Sweden)

    Emílio José Montero Arruda Filho

    2012-08-01

    Full Text Available O desenvolvimento do setor de comunicação de um país possui relações com o seu desenvolvimento econômico e é possível demonstrar essa conexão estatisticamente, como tem sido feito por pesquisadores de instituições como a ITU (International Telecommunications Union. Como esses dados estão apenas apresentados na forma simples e não levam em conta fatores de interconexão, é importante desenvolver pesquisas que avaliem a conexão entre variáveis relevantes no campo. Este trabalho visa analisar os fatores de desenvolvimento tecnológico de comunicação que melhor descrevem o posicionamento econômico de um país, integrando a usabilidade dos serviços de comunicação com o status econômico. Foram utilizados dados de 56 países, escolhidos aleatoriamente. Uma pesquisa na forma de datamining foi realizada, a qual analisou os dados existentes já previamente coletados por instituições de pesquisa tais como ITU, World Bank, e outras. Cada fator de usabilidade, preferência e serviço analisado é apontado como um reflexo de outros serviços e usos anteriormente desenvolvidos. Parte da literatura sobre esse tópico (ARRUDA FILHO; CASSIA; MARINO, 2008; CHERRY, 2007; DAVIES; HARDT; KELLY, 2004 argument que o desenvolvimento econômico de certos países existe como resultado de um aumento do desenvolvimento tecnológico, porém outras demonstram ou informam o contrário. Este artigo apresenta essas relações em certos países, escolhidos pela quantidade de informação disponível considerando sua posição de desenvolvimento global, relacionando diretamente o comportamento de crescimento ou redução no uso das tecnologias, tais como telefone e internet. Este trabalho coletou dados de duas fontes mundiais de informação dos setores mencionados: a International Telecommunications Union (ITU e o World Bank. Utilizaram-se as técnicas estatísticas de regressão e análise de variância para a análise de dados de 56 países ao longo de

  16. TECNOLOGIAS DIGITAIS: PROMOVENDO O DESENVOLVIMENTO SUSTENTÁVEL PARA O JOVEM DO CAMPO

    OpenAIRE

    Zarpelon, Mirian Cátia; Kolcenti, Cassiane; Balestrin, Deisi; Tortelli, Luana; Blazszack, Vinicíus; Guedes, Anibal Lopes

    2015-01-01

    O desenvolvimento sustentável é hoje em dia, um dos principais desafios a ser enfrentado na atualidade. Inclui-se neste universo a agricultura, através da consolidação das atividades produtivas a fim de desenvolver de forma sustentável, a gestão da propriedade rural, bem como sua condição ambiental e social, sem degradar o capital natural e mantendo o bem estar da sociedade. Dentro desse processo, as novas tecnologias proporcionam o desenvolvimento de soluções criativas simples que visam melh...

  17. Economia e Desenvolvimento Social: A Possibilidade da Utilização de Indicadores Sociais na Avaliação do Desenvolvimento Paranaense

    Directory of Open Access Journals (Sweden)

    Daniel Vitor Vicente

    2013-12-01

    Full Text Available Este trabalho pretende analisar a progressão de indicadores sociais no Paraná a partir dos anos 1990, utilizando como base de dados os indicadores sociais de Educação, Emprego e Renda, Saúde e Saneamento, disponibilizados pelo Instituto Paranaense de Desenvolvimento Econômico e Social - IPARDES. Para o desdobramento de tal reflexão, será resgatado brevemente o desenvolvimento econômico Brasileiro, cujo projeto de Estado está embasado no que se conhece por novo desenvolvimentismo. Do mesmo modo, também será abordada a possibilidade de serem utilizados indicadores sociais públicos e gratuitos, a fim de que os mesmos auxiliem nos procedimentos de análise e problematização de questões sociais que interessam às Ciências Sociais, utilizando-se como exemplo os dados que serão apresentados.

  18. Plasma immersion ion implantation on 15-5PH stainless steel: influence on fatigue strength and wear resistance

    Science.gov (United States)

    Bonora, R.; Cioffi, M. O. H.; Voorwald, H. J. C.

    2017-05-01

    Surface improvement in steels is of great interest for applications in industry. The aim of this investigation is to study the effect of nitrogen ion implantation on the axial fatigue strength and wear resistance of 15-5 PH stainless steel. It is well know that electroplated coatings, which are used to improve abrasive wear and corrosion properties, affects negatively the fatigue strength. It is also important to consider requirements to reduce the use of coated materials with electroplated chromium and cadmium, that produce waste, which is harmful to health and environment. The HVOF (High velocity oxygen fuel) process provides hardness, wear strength and higher fatigue resistance in comparison to electroplated chromium. Plasma immersion ion implantation has been used to enhance the hardness, wear, fatigue and corrosion properties of metals and alloys. In the present research the fatigue life increased twice for 15-5 PH three hours PIII treated in comparison to base material. From the abrasive wear tests a lower pin mass reduction was observed, associated to the superficial treatments. The improvement of fatigue and mechanical performance is attributed to a combination of nitrides phase structure and compressive residual stresses during the PIII treatment.

  19. Plasma immersion ion implantation on 15-5PH stainless steel: influence on fatigue strength and wear resistance

    International Nuclear Information System (INIS)

    Bonora, R; Cioffi, M O H; Voorwald, H J C

    2017-01-01

    Surface improvement in steels is of great interest for applications in industry. The aim of this investigation is to study the effect of nitrogen ion implantation on the axial fatigue strength and wear resistance of 15-5 PH stainless steel. It is well know that electroplated coatings, which are used to improve abrasive wear and corrosion properties, affects negatively the fatigue strength. It is also important to consider requirements to reduce the use of coated materials with electroplated chromium and cadmium, that produce waste, which is harmful to health and environment. The HVOF (High velocity oxygen fuel) process provides hardness, wear strength and higher fatigue resistance in comparison to electroplated chromium. Plasma immersion ion implantation has been used to enhance the hardness, wear, fatigue and corrosion properties of metals and alloys. In the present research the fatigue life increased twice for 15-5 PH three hours PIII treated in comparison to base material. From the abrasive wear tests a lower pin mass reduction was observed, associated to the superficial treatments. The improvement of fatigue and mechanical performance is attributed to a combination of nitrides phase structure and compressive residual stresses during the PIII treatment. (paper)

  20. Treatment of Gingival Recessions Associated to Cervical Abrasion Lesions with Subepithelial Connective Tissue Graft: A Case Report

    Science.gov (United States)

    Deliberador, Tatiana M.; Bosco, Alvaro F.; Martins, Thiago M.; Nagata, Maria J. H.

    2009-01-01

    Extensive gingival recessions associated with cervical abrasions are common among the population. Several different surgical and/or restorative therapies have been proposed to correct these lesions. This manuscript reports the treatment of multiple gingival recessions associated to cervical abrasions. The procedure involved the utilization of subepithelial connective tissue graft (SCTG) combined with coronally advanced flap onto a previously restored root surface. At the postoperative follow-up visits, the success of the restorative/surgical approach was confirmed by the absence of bleeding to probing and periodontal pockets as well as presence of gingival tissue with normal color, texture and contouring. After 18 months of follow-up, the clinical conditions are stable with satisfactory root coverage and periodontal health. An excellent esthetical outcome was achieved and the patient is satisfied with case resolution. PMID:19826605

  1. Numerical simulation of the combination effect of external magnetic field and rotating workpiece on abrasive flow finishing

    Energy Technology Data Exchange (ETDEWEB)

    Kheradmand, Saeid; Esmailian, Mojtaba; Fatahy, A. [Malek-Ashtar University of Technology (MUT), Isfahan (Iran, Islamic Republic of)

    2017-04-15

    Finishing of a workpiece is a main process in the production. This affects the quality and lifetime. Finishing in order of nanometer, nowadays, is a main demand of the industries. Thus, some new finishing process, such as abrasive flow finishing, is introduced to respond this demand. This may be aided by rotating workpiece and imposing a magnetic field. Numerical simulation of this process can be beneficial to reduce the expense and predict the result in a minimum time. Accordingly, in this study, magnetorheological fluid finishing is numerically simulated. The working medium contains magnetic and abrasive particles, blended in a base fluid. Some hydrodynamic parameters and surface roughness variations are studied. It is found that combination of rotating a workpiece and imposing a magnetic field can improve the surface roughness up to 15 percent.

  2. ATIVIDADES CORPORAIS AQUÁTICAS EM ESPECIAL O MERGULHO E O DESENVOLVIMENTO DO PSIQUISMO

    Directory of Open Access Journals (Sweden)

    Celi Taffarel

    2015-04-01

    Full Text Available O presente estudo situa-se entre os que investigam o desenvolvimento do psiquismo ressaltando o papel da educação escolar e o acesso ao conhecimento clássico sobre as atividades corporais aquáticas, e dentre elas o mergulho, no desenvolvimento dos processos funcionais, através do ensino e da aprendizagem de conteúdos nucleares na escola. Objetivo:Analisar o desenvolvimento do psiquismo à luz da psicologia histórico-cultural e propor o trato com o conhecimento clássico sobre atividades aquáticas, em especial o mergulho, a luz da pedagogia histórico-critica, defendendo este conhecimento como nuclear no currículo escolar, nos estudos sobre a relação “ser humano-água”, para a elevação da capacidade teórica dos estudantes, através da metodologia do ensino critico-suparadora.

  3. NK cells modulate the inflammatory response to corneal epithelial abrasion and thereby support wound healing

    Science.gov (United States)

    Natural killer cells are lymphocytes of the innate immune system that have crucial cytotoxic and regulatory roles in adaptive immunity and inflammation. Herein, we consider a role for these cells in corneal wound healing. After a 2-mm central epithelial abrasion of the mouse cornea, a subset of clas...

  4. A taxa de câmbio no centro da teoria do desenvolvimento

    Directory of Open Access Journals (Sweden)

    Luiz Carlos Bresser-Pereira

    2012-08-01

    Full Text Available Este artigo apresenta as principais ideias da macroeconomia estruturalista do desenvolvimento - a teoria por trás de novo-desenvolvimentismo. Seu foco é a taxa de câmbio que é pela primeira vez colocada no centro da economia do desenvolvimento. A teoria econômica geralmente vê a taxa de câmbio como um problema de curto prazo a ser discutido na macroeconomia. A macroeconomia estruturalista do desenvolvimento mostra que há, nos países em desenvolvimento, a tendência à sobreapreciação cíclica da taxa de câmbio causada pela falta de neutralização da doença holandesa e por entradas de capital excessivas. Em consequência, considera a taxa de câmbio cronicamente sobreapreciada e, por isso, um grande obstáculo ao crescimento econômico. No processo de desenvolvimento, a taxa de câmbio tem a função de um interruptor de luz que conecta ou desconecta as empresas nacionais que utilizam a tecnologia no estado da arte mundial dos mercados mundiais.This paper presents the main ideas of structuralist development macroeconomics - the theory behind new developmentalism. Its focus is on the exchange rate that is positioned for the first time in the core of development economics. Economic theory usually views the exchange rate as a short term problem to be discussed in open macroeconomics. Structuralist development macroeconomics argues that there is in developing countries a tendency to the cyclical overvaluation of the exchange rate caused by the lack of neutralization of the Dutch disease and by excessive capital inflows. In consequence it views the exchange rate as chronically overvalued, and, for that reason, a major obstacle to economic growth. In the development process, the exchange rate has the role of light switch that connects or disconnects the national business enterprises utilizing technology in the world state of the art from world markets.

  5. A Cooperação Triangular e as Transformações da Cooperação Internacional para o Desenvolvimento

    OpenAIRE

    Bruno Ayllón Pino

    2013-01-01

    Nas últimas décadas, a Cooperação Internacional para o Desenvolvimento (CID) tem experimentado modalidades alternativas de execução, integrando países desenvolvidos, países em desenvolvimento e organismos multilaterais em formatos triangulares. Em um contexto de crise econômica, as limitações da CID para promover o desenvolvimento, somadas às dúvidas sobre o cumprimento dos compromissos financeiros dos doadores da Organização para a Cooperação e Desenvolvimento Econômico (OCDE), propiciaram o...

  6. Desenvolvimento inicial de mudas de Butia odorata (Barb. Rodr. Noblick cultivadas em recipientes

    Directory of Open Access Journals (Sweden)

    Claudimar Sidnei Fior

    2014-10-01

    Full Text Available Butia odorata (Barb.Rodr. Noblick (butiazeiro é uma palmeira nativa do sul do Brasil, com grande demanda para usos ornamental e agroindustrial. O objetivo deste estudo foi avaliar o desenvolvimento inicial de mudas de butiazeiro, em recipientes com diferentes composições de substratos. O experimento foi desenvolvido em casa de vegetação sem controle de temperatura e umidade. Foram utilizadas mudas com 60 dias após a germinação, e avaliados os substratos, em cinco proporções, dos componentes casca de arroz carbonizada e casca de pinus. Em etapa posterior, monitorou-se o efeito do pH do substrato no desenvolvimento das mudas mantidas nos mesmos recipientes e tratamentos. Para tanto, as plantas foram distribuídas em igual número e representação dos tratamentos, em quatro grupos, com quatro níveis de pH do substrato (4,0; 4,9; 5,8 e 6,7. Noventa dias após o início da primeira etapa, e 161 dias após o início da segunda, foram avaliados o desenvolvimento das plantas, a condutividade elétrica e o pH dos substratos. Na primeira etapa, constatou-se diferença entre os tratamentos somente para altura das plantas e pH do substrato, ambas relacionadas diretamente com a proporção de casca de pinus na formulação. Na segunda etapa, a composição do substrato foi determinante para o maior desenvolvimento das mudas. Somente o número de folhas não apresentou diferença significativa entre os tratamentos. Contudo, para todas as variáveis, a presença de casca de pinus, mesmo em baixa proporção, foi suficiente para favorecer o desenvolvimento vegetativo.

  7. Charles Darwin: um observador do desenvolvimento humano

    Directory of Open Access Journals (Sweden)

    Eloisa Helena Rubello Valler Celeri

    2010-12-01

    Full Text Available Os autores traduzem, pela primeira vez para o português, o artigo de Charles Darwin "A Biographical Sketch of an Infant", publicado no periódico Mind em julho de 1877. Utilizando anotações de observações do desenvolvimento de seus filhos, especialmente de seu filho mais velho William Erasmus (Doddy, Darwin descreve e estuda, a partir de seu enfoque naturalista, o filhote humano, narrando os primeiros indicativos comportamentais de emoções tais como raiva e medo, curiosidade e senso moral, o brincar e o prazer envolvido nesta atividade, a capacidade de imitação e os primeiros indícios daquilo que hoje conhecemos como "teoria da mente". Colocando-se questões sobre as capacidades do bebê, como eles aprendem e como se comunicam e levantando hipóteses sobre possíveis significados de certos comportamentos, questões ainda hoje fundamentais para o estudo do desenvolvimento humano, Darwin mostra-se também um pioneiro no estudo do bebê e da criança pequena, numa época na qual as capacidades dos bebês eram extremamente subestimadas e desconsideradas.

  8. O Estado (de Bem-Estar Social como Ator do Desenvolvimento: Uma História das Ideias

    Directory of Open Access Journals (Sweden)

    Celia Lessa Kerstenetzky

    2015-09-01

    Full Text Available Reconstruímos neste artigo uma história das ideias, abstratas ou incorporadas em práticas concretas, da ação estatal voltada ao desenvolvimento, da concepção de "Estados-poder" a "Estados de Bem-Estar", seguindo o fluxo e o refluxo de argumentos em favor da intervenção. Justificativas de intervenção baseadas na necessidade de superar descontinuidades econômicas são contrapostas a argumentos que apontam os riscos e antídotos da captura do Estado por interesses privados, bem como à abordagem mais ampla ao desenvolvimento de Amartya Sen. Experiências nacionais de desenvolvimento e de Estado de Bem-Estar Social são também rastreadas, como "ideias incorporadas". Identificamos uma defesa da intervenção do Estado que integra os campos econômico, político e social e aponta a democracia e o Estado de Bem-Estar como temas emergentes no discurso do desenvolvimento.

  9. The possible use of Bayer process cyclone fines for manufacture of abrasives

    OpenAIRE

    Sancho, J.; García, M. P.; García, M. F.; Ayala, J.; Verdeja, L. E.

    2002-01-01

    This paper deals with the feasibihty of producing synthetic abrasives from a by-product of the Bayer process: the cyclone fines, through synthesis aided by mineralizers addition. The main result has been the production of a low temperature (1200-1300 °C) polish by adding fluoride mineralizers, that could be in clear competence with synthetic corundum obtained also in this work by a more traditional way: sodium removal, using of magnesium oxide as mineralizer, and high calcination temperatures...

  10. Resiliência e Justiça Organizacional como Antecedentes da Percepção de Desenvolvimento Profissional

    Directory of Open Access Journals (Sweden)

    Ana Claudia Monteiro

    Full Text Available RESUMO O mercado competitivo da atualidade tem exigido mais qualificação dos trabalhadores, o que aumenta a relevância do construto desenvolvimento profissional. O objetivo deste estudo foi testar um modelo de predição da percepção do desenvolvimento profissional. Participaram da pesquisa 320 trabalhadores de diferentes categorias profissionais de organizações públicas e privadas. O questionário continha três escalas, todas com bons indicadores psicométricos. Os resultados apontados a partir da regressão múltipla confirmaram que percepção de justiça organizacional e resiliência predizem positivamente a percepção de desenvolvimento profissional, sendo que esta demonstra maior poder preditivo. Os resultados foram discutidos de acordo com a teoria do desenvolvimento profissional.

  11. Bonding of composite resins to PEEK: the influence of adhesive systems and air-abrasion parameters.

    Science.gov (United States)

    Stawarczyk, Bogna; Taufall, Simon; Roos, Malgorzata; Schmidlin, Patrick R; Lümkemann, Nina

    2018-03-01

    The objective of the study was to investigate the tensile bond strength (TBS) to polyaryletheretherketone (PEEK) after different pretreatment and conditioning methods. Four hundred PEEK specimens were fabricated and allocated to the following air-abrasion methods (n 1  = 80/pretreatment): (i) 50 μm Al 2 O 3 (0.05 MPa); (ii) 50 μm Al 2 O 3 (0.35 MPa); (iii) 110 μm Al 2 O 3 (0.05 MPa); (iv) 110 μm Al 2 O 3 (0.35 MPa); and (v) Rocatec 110 μm (0.28 MPa). These pretreatments were combined with the following conditioning methods (n 2  = 20/pretreatment/conditioning): (a) visio.link (VL); (b) Monobond Plus/Heliobond (MH); (c) Scotchbond Universal (SU); and (d) dialog bonding fluid (DB). After veneering of all specimens with dialog occlusal and aging (28 days H 2 O, 37 °C + 20,000 thermal cycles, 5/55 °C), TBS was measured. Data was analysed using Kaplan-Meier survival analysis with Breslow-Gehan test and Cox-regressions. The major impact on TBS showed the conditioning, followed by the air-abrasion-pressure, while the grain size of the air-abrasion powder did not show any effect. Specimens air-abraded at 0.35 MPa showed the highest survival rates. However, within VL groups, this observation was not statistically significant. Within MH groups, pretreatment using 110 μm Al 2 O 3 and 0.05 MPa resulted in higher survival rates compared to groups treated with 50 and 110 μm Al 2 O 3 using a pressure of 0.35 MPa. The use of VL showed the highest survival rates between the adhesive systems and the TBS values higher than 25 MPa independent of the pretreatment method. As an exception, only VL showed significantly higher survival rates when compared to MH. The adequate choice of the adhesive system and higher pressures improved the TBS between PEEK and veneering resin composite. The particle size had no major impact. According to this study, best veneering of PEEK with dialog occlusal can be achieved by conditioning with visio.link in combination with

  12. Mesorregião Grande Fronteira do Mercosul: perfil locacional do desenvolvimento regional

    Directory of Open Access Journals (Sweden)

    Jandir Ferrera de Lima

    2010-05-01

    Full Text Available O objetivo deste artigo é analisar o perfil das desigualdades regionais na área de abrangência na região Grande Fronteira do Mercosul (GFM, através da mensuração do coeficiente de desenvolvimento regional e do padrão de localização do emprego formal. No âmbito dessa análise ficaram demonstrados dois fenômenos espaciais: um processo de reestruturação espacial e a forte desigualdade das mesorregiões Sudoeste PR, Noroeste RS e Fronteira Oeste RS em relação às outras mesorregiões do Sul do Brasil. Esse resultado fortalece a identificação de particularidades espaciais capazes de esclarecer um padrão de desenvolvimento econômico regional diferenciado nas fronteiras, em particular na Região Sul do Brasil. Os resultados deste estudo forneceram elementos para a intervenção regional, pois é possível, via políticas públicas adequadas, buscar a retomada do dinamismo econômico e o desenvolvimento socioeconômico na GFM.

  13. Modification of UV absorption profile of polymer film reflectors to increase solar-weighted reflectance

    Science.gov (United States)

    Jorgensen, Gary; Gee, Randall C.; White, David

    2017-05-02

    Provided are reflective thin film constructions including a reduced number of layers, which provides for increased solar-weighted hemispherical reflectance and durability. Reflective films include those comprising an ultraviolet absorbing abrasion resistant coating over a metal layer. Also provided are ultraviolet absorbing abrasion resistant coatings and methods for optimizing the ultraviolet absorption of an abrasion resistant coating. Reflective films disclosed herein are useful for solar reflecting, solar collecting, and solar concentrating applications, such as for the generation of electrical power.

  14. Estilos parentais e personalidade: competências sociais e o desenvolvimento do processo resiliente

    OpenAIRE

    Ferreira, Sara Patrícia Duarte

    2016-01-01

    Dissertação de Mestrado em Psicologia Clínica De acordo com a literatura, as vivências afetivas e relacionais experienciadas no seio familiar, nomeadamente na relação entre pais-filhos, têm um papel privilegiado no desenvolvimento dos jovens. Nesta medida, postula-se que um estilo parental baseado na assertividade e responsividade assuma um papel significativo e protetor face ao desenvolvimento de características e competências adaptativas dos adolescentes e jovens adultos. A presente inve...

  15. Influence of Plasma Transferred Arc Process Parameters on Structure and Mechanical Properties of Wear Resistive NiCrBSi-WC/Co Coatings

    Directory of Open Access Journals (Sweden)

    Eitvydas GRUZDYS

    2011-07-01

    Full Text Available Self-fluxing NiCrBSi and related coatings received considerable interest due to their good wear as well as corrosion resistance at moderate and elevated temperatures. Hard tungsten carbide (WC particles can be included in NiCrBSi for further increase of the coating hardness and abrasive wear resistance. Flame spray technique is widely used for fabrication of NiCrBSi films. However, in such a case, subsequent remelting of the deposited coatings by flame, arc discharge or high power laser beam is necessary. In present study NiCrBSi-WC/Co coatings were formed using plasma transferred arc process. By adjusting plasma parameters, such as current, plasma gas flow, shielding gas flow, a number of coatings were formed on steel substrates. Structure of the coatings was investigated using X-ray diffractometry. Microstructure of cross-sectioned coatings was examined using scanning electron microscopy. Hardness of the coating was evaluated by means of the Vickers hardness tests. Wear tests were also performed on specimens to determine resistance to abrasive wear. Acquired results allowed estimating the influence of the deposition process parameters on structure and mechanical properties of the coatings.http://dx.doi.org/10.5755/j01.ms.17.2.482

  16. Modelling detrital coral grain-size and age: Insights from sediment abrasion process of Yongle Atoll of South China Sea

    Science.gov (United States)

    Li, Y.; Zou, X.; Ge, C.; Tan, M.; Wang, C.

    2017-12-01

    Reef islands situated on the rims of atolls are composed almost exclusively of bioclastic materials locally supplied from adjacent coral reefs. Major skeletal component of these islands include coral, coralline algae, mollusks and foraminifera, produced in adjacent reefs. As the island builder, the bioclastic material is the sedimentary products, which also is the point of penetration to decipher the process. The bioclast of coral islands decrease in size with the transportation process. The grain-size provides a proxy record for the abrasion history of the unconsolidated sediment. The 230Th age of coral record the abrasion time. We hereby present a model to calculate the abrasion rate based on the data of 230Th age and grain-size of Yongle Atoll of Xisha Island, South China Sea. The grain size pattern in Yongle Atoll environment have confirm that the coral article diminution behave exponentially. The sediment composition of Yongle Atoll is identified, coral is dominant sediment constituent and the Th230 age is shown to exert an age distribution characteristics of coral detritus. We illustrate this approach by calculate the coral debris age of Xude Atoll, which located near the Yongle Atoll and then by comparing actual measured age and calculated age and to explore the dependence of the model. Observed 230 Th ages are well matched by predicted ages for medium age sediment. A poorer match for young and old sediment may result from some combination of large analytical uncertainties in the detrital ages and inhomogeneous erosion rates within the atoll. Such mismatches emphasize the need for more accurate kinematic models and for sampling strategies that are adapted to atoll-specific geologic and geomorphic conditions. Results presented constitute important new insights into regional sediment abrasion processed and on the evolution of coral atoll islands.

  17. Indução e desenvolvimento de calos e embriões somáticos em mamoeiro

    OpenAIRE

    Almeida,Eliane Pires de; Oliveira,Roberto Pedroso de; Dantas,Jorge Luis Loyola

    2001-01-01

    Este trabalho teve por objetivo estabelecer um protocolo para a indução e desenvolvimento de calos e embriões somáticos em mamoeiro (Carica papaya L. cv. Tainung n.1). Foram utilizados quatro tipos de explantes (hipocótilo com folhas cotiledonares, hipocótilo, folhas cotiledonares e epicótilo) e duas condições de cultivo (escuro e 16 horas de luz). A indução e o desenvolvimento de calos foram avaliados nos meios de cultura ½MS2, ½MS10 e HMH e a indução e o desenvolvimento de embriões somático...

  18. Planejamento no estado brasileiro: dificuldades estruturais para a concretização constitucional do desenvolvimento regional

    OpenAIRE

    Rodrigo Soldi

    2009-01-01

    A dissertação visa identificar os entraves para a construção e a articulação do planejamento de desenvolvimento nacional e regional no contexto das atribuições da União, como ente chave na construção do federalismo cooperativo. Parte da investigação da distinção das expressões crescimento e desenvolvimento, para compreender a noção de desenvolvimento nacional, como um dos fundamentos da República Federativa do Brasil. Delineia a noção de planejamento, de plano econômico e sua relação com o di...

  19. Perfil do desenvolvimento motor em escolares com excesso de peso

    Directory of Open Access Journals (Sweden)

    Mayara Moura Alves da Cruz

    2017-12-01

    Full Text Available Introdução: Diferenças relacionadas ao peso e as habilidades motoras em crianças em idade escolar ainda apresentam controversias. Objetivo: Analisar a relação entre desenvolvimento motor e nível de atividade física com o índice de massa corporal (IMC de escolares com excesso de peso. Métodos: Foram avaliados 85 escolares de ambos os sexos, de 6 a 10 anos, de Presidente Prudente, São Paulo, Brasil. Os instrumentos utilizados foram a classificação do IMC/idade, a Escala de Desenvolvimento Motor e o Questionário do Nível de Atividade Física Modificado e Adaptado. A amostra foi dividida em dois grupos: grupo com excesso de peso (GEP, com 50 escolares com diagnostico nutricional de sobrepeso e obesidade; e grupo com normopeso (GNP, com 35 escolares eutroficos. Para analise dos dados obtidos foram utilizados: Shapiro Wilk (normalidade, teste t de Student não pareado ou Mann Whitney (amostras independentes, teste de Spearman (correlação e teste do χ2 (proporção, com nível de significância p<0,05. Resultados: O GEP apresentou resultados inferiores significantes no desenvolvimento motor geral (91,32±10,68 versus 97,14±9,06; p=0,010, nas áreas de motricidade fina – QM1 (93,21±21,59 versus 103,1±13,12; p=0,0138 e motricidade global – QM2 (90,31±23,54 versus 112,6±16,07; p<0,0001. Observou-se correlação positiva significativa entre o nível de atividade física e o desenvolvimento motor no GEP, nas áreas de equilibrio – QM3 (0,35080; p=0,0125 e organização espacial – QM5 (0,41820; p=0,0025. Conclusão: O GEP, quando comparado com o GNP, demonstrou resultados inferiores no quociente motor geral (QMG, QM1 e QM2.

  20. O uso de múltiplas escalas geográficas no planejamento do desenvolvimento regional

    Directory of Open Access Journals (Sweden)

    Vivian Costa Brito

    2017-01-01

    Full Text Available O uso de múltiplas escalas geográficas aplicadas ao planejamento de políticas públicas de desenvolvimento regional é recente no Brasil. Remete à criação da Política Nacional de Desenvolvimento Regional (PNDR em 2003. A ênfase dada na categoria socioespacial reflete uma abordagem de caráter territorialista, que se contrapõe ao planejamento com enfoque estritamente macrorregional e com viés econômico. Este artigo analisa a conformação de estruturação e implementação desse arranjo multiescalar, para compreender a dimensão do planejamento na PNDR I e II. Como eixo central de articulação da política tem-se a relação intergovernamental e extragovernamental com inserção de todos os setores, abarcando estratégias de ação multiescalares. A abordagem multiescalar precisa avançar sobre a questão do ritmo e direção do desenvolvimento. As ferramentas da transversalidade e da intersetorialidade devem refletir em mudança social. Sem isso, o desenvolvimento regional torna-se contraditório, longe de representar uma oportunidade para regiões deprimidas tanto econômica quanto socialmente.

  1. Os desafios do desenvolvimento da engenharia genética na agricultura : percepção de riscos e regulação

    OpenAIRE

    Izaias de Carvalho Borges

    2010-01-01

    Resumo:Nos últimos 15 anos a engenharia genética vem sendo usada para o desenvolvimento de cultivos geneticamente modificados (GM) com diversos atributos de interesses para a produção agrícola, tais como tolerância a herbicidas, resistência a insetos e modificações nas características nutricionais de diversos cultivos. Os cultivos GM estão sendo utilizados na produção de produtos de grande importância no mercado mundial de commodities agrícolas, tais como algodão, milho e soja. Agricultores d...

  2. Desenvolvimento e Sustentabilidade na América Latina: Velha História, Novos Caminhos

    Directory of Open Access Journals (Sweden)

    Tayso Silva

    2014-06-01

    Full Text Available O desenvolvimento, considerado durante muito tempo um valor universalmente aceito, e meta de toda sociedade moderna, hoje é questionado, inclusive sobre a forma como é produzido. É demonstrada a importância do desenvolvimento sustentável em direção à conquista de melhores condições de vida. Determinou-se como objetivo principal deste estudo apresentar insights para a maximização da sustentabilidade enquanto dinamizadora da trajetória de desenvolvimento na América Latina. Foram considerados o Painel Intergovernamental sobre Mudanças Climáticas, a Organização das Nações Unidas, o Protocolo de Quioto, entre outros estudos de validade e aceitabilidade internacional para propor parâmetros estratégicos aos negócios da AL. DOI:10.5585/riae.v13i2.2095

  3. Erosion resistance comparison of alternative surface treatments

    Science.gov (United States)

    Česánek, Z.; Schubert, J.; Houdková, Š.

    2017-05-01

    Erosion is a process characterized by the particle separation and the damage of component functional surfaces. Thermal spraying technology HP/HVOF (High Pressure / High Velocity Oxygen Fuel) is commonly used for protection of component surfaces against erosive wear. Alloy as well as cermet based coatings meet the requirements for high erosion resistance. Wear resistance is in many cases the determining property of required component functioning. The application suitability of coating materials is particularly influenced by different hardness. This paper therefore presents an erosion resistance comparison of alloy and cermet based coatings. The coatings were applied on steel substrates and were subjected to the erosive test using the device for evaluation of material erosion resistance working on the principle of centrifugal erodent flow. Abrasive sand Al2O3 with grain size 212-250 μm was selected as an erosive material. For this purpose, the specimens were prepared by thermal spraying technology HP/HVOF using commercially available powders Stellite 6, NiCrBSi, Cr3C2-25%NiCr, Cr3C2-25%CoNiCrAlY, Hastelloy C-276 and experimental coating TiMoCN-29% Ni. Erosion resistance of evaluated coatings was compared with erosive resistance of 1.4923 high alloyed steel without nitridation and in nitrided state and further with surface treatment using technology PVD. According to the evaluation, the resulting erosive resistance depends not only on the selected erodent and surface protection, but also on the erodent impact angle.

  4. The development and treatment of impulsivity = O desenvolvimento e tratamento da impulsividade

    Directory of Open Access Journals (Sweden)

    Amorim Neto, Roque do Carmo

    2011-01-01

    Full Text Available Impulsividade é um fator presente em várias desordens psicológicas, incluindo ADHD, drogadição, comportamentos agressivos e automutiladores, e obesidade infantil. Impulsividade também é um fator de risco para o abandono de tratamento. Este artigo tem por objetivo apresentar as raízes da impulsividade do ponto de vista biológico, sociológico e do desenvolvimento humano, bem como as formas de tratamento mais comuns para pessoas com extrema impulsividade. Aqui também se inclui pesquisas das áreas de desenvolvimento neuronal e regulação emocional

  5. Investigações epidemiológicas sobre demência nos países em desenvolvimento

    Directory of Open Access Journals (Sweden)

    M Scazufca

    2002-12-01

    Full Text Available Na medida em que a população mundial está envelhecendo, a demência está se constituindo em importante problema de saúde pública, particularmente nos países em desenvolvimento. Investigações epidemiológicas nestes países são escassas e apresentam dificuldades metodológicas adicionais, principalmente no que se refere à adequação sociocultural dos instrumentos utilizados para a definição de casos. Tendo em vista estas preocupações, foi fundado o "Grupo de Pesquisa em Demência 10/66", que é constituído por uma rede internacional de pesquisadores, predominantemente de países em desenvolvimento. O nome do grupo tem como referência o paradoxo de que menos de 10% dos estudos populacionais sobre demência são dirigidos aos 2/3 ou mais de casos de pessoas com demência que vivem em países em desenvolvimento. O objetivo do artigo é atualizar informações da literatura sobre as diferenças de prevalência e incidência de demência encontradas em países desenvolvidos e em desenvolvimento.

  6. Investigações epidemiológicas sobre demência nos países em desenvolvimento

    Directory of Open Access Journals (Sweden)

    Scazufca M

    2002-01-01

    Full Text Available Na medida em que a população mundial está envelhecendo, a demência está se constituindo em importante problema de saúde pública, particularmente nos países em desenvolvimento. Investigações epidemiológicas nestes países são escassas e apresentam dificuldades metodológicas adicionais, principalmente no que se refere à adequação sociocultural dos instrumentos utilizados para a definição de casos. Tendo em vista estas preocupações, foi fundado o "Grupo de Pesquisa em Demência 10/66", que é constituído por uma rede internacional de pesquisadores, predominantemente de países em desenvolvimento. O nome do grupo tem como referência o paradoxo de que menos de 10% dos estudos populacionais sobre demência são dirigidos aos 2/3 ou mais de casos de pessoas com demência que vivem em países em desenvolvimento. O objetivo do artigo é atualizar informações da literatura sobre as diferenças de prevalência e incidência de demência encontradas em países desenvolvidos e em desenvolvimento.

  7. Preparation and Properties of Superamphiphobic Wear-resistance PPS-based Coating

    Directory of Open Access Journals (Sweden)

    WANG Huai-yuan

    2017-01-01

    Full Text Available Superamphiphobic wear-resistance PPS-based coatings were prepared by a simple spraying method with a pore-forming reagent of NH4HCO3 and nano-filler of carbon nanotubes (CNTs.The surface morphology and the hydrophobicity,oleophobicity of the coating were analyzed by scanning electron microscope (SEM and contact angle meter.The wear-resistance of the coating was verified by sanding method with given load.The results indicate that a rough surface is obtained after pore-forming,and the porous structures in combination with the CNTs construct the special micro/nano-scale network structures.When the mass fraction of NH4HCO3 is 5%,the contact angles of the coating for water,glycerine and ethylene glycol are 162°,158° and 152°,showing superamphiphobic property.After polished 10000 times by abrasive paper,the coating shows slight friction marks and remains high hydrophobicity,exhibiting excellent wear-resistance.

  8. Corrosion resistance of Cu-Al coatings produced by thermal spray

    Directory of Open Access Journals (Sweden)

    Laura Marcela Dimaté Castellanos

    2012-01-01

    Full Text Available Many components in the shipbuilding industry are made of copper-based alloys. These pieces tend to break due to corrosion generated by a marine environment; such components can be salvaged through surface engineering, through deposition of suitable coatings. This paper studied the influence of three surface preparation methods involving phosphor bronze substrates concerning the corrosion resistance of commercial coatings having Al-Cu +11% Fe chemical composition. The surface was prepared using three methods: sand blasting, shot blasting and metal polishing with an abrasive disk (with and without a base layer. The deposited coatings were micro-structurally characterised by x-ray diffraction (XRD, optical microscopy and scanning electron microscopy (SEM. Corrosion resistance was evaluated by electrochemical test electrochemical impedance spectroscopy (EIS. Surfaces prepared by sandblasting showed the best resistance to corrosion, so these systems could be a viable alternative for salvaging certain parts in the marine industry. The corrosion mechanisms for the coatings produced are discussed in this research.

  9. O papel das Forças Armadas na I&D da Defesa como vector de desenvolvimento nacional

    OpenAIRE

    Simões, Luís

    2010-01-01

    A humanidade sempre se preocupou com o seu bem-estar, de alguma forma. Neste âmbito, o desenvolvimento económico tem vindo a desempenhar um papel fundamental. Após a revolução industrial, mas particularmente depois da II Guerra Mundial, os Estados têm-se preocupado com o respectivo desenvolvimento económico sustentável, entre outras questões, como garante de bem-estar das suas populações. A investigação e desenvolvimento (I&D), no seu conjunto, têm sido apontados como um possível vector de de...

  10. Individualidade, conhecimento e linguagem na concepção dialética de desenvolvimento em Vigotski

    Directory of Open Access Journals (Sweden)

    Newton Duarte

    2016-01-01

    Full Text Available Neste artigo são exploradas as relações, na psicologia vigotskiana, entre o indivíduo em desenvolvimento e as formas mais ricas de individualidade, de conhecimento e de linguagem. A proposição metodológica que Karl Marx apresenta em sua clássica análise do método da economia política, segundo a qual, a anatomia humana é uma chave para a anatomia do macaco, ou seja, a forma mais desenvolvida é uma referência para a compreensão da menos desenvolvida, é vista por Vigotski como força motora do desenvolvimento psíquico humano. Esse psicólogo defende que a relação com o adulto é necessária ao desenvolvimento da criança. Igualmente ele postula que a individualidade se desenvolve do “em si” ao “para si” e que os sistemas de instrumentos psicológicos mais ricos são indispensáveis ao alcance de níveis mais elevados de desenvolvimento psíquico.

  11. Microstructure and wear resistance of spray-formed supermartensitic stainless steel

    Directory of Open Access Journals (Sweden)

    Guilherme Zepon

    2013-06-01

    Full Text Available Since the early 90's the oil industry has been encouraging the development of corrosion and wear resistant alloys for onshore and offshore pipeline applications. In this context supermartensitic stainless steel was introduced to replace the more expensive duplex stainless steel for tubing applications. Despite the outstanding corrosion resistance of stainless steels, their wear resistance is of concern. Some authors reported obtaining material processed by spray forming, such as ferritic stainless steel, superduplex stainless steel modified with boron, and iron-based amorphous alloys, which presented high wear resistance while maintaining the corrosion performance1,2. The addition of boron to iron-based alloys promotes the formation of hard boride particles (M2B type which improve their wear resistances3-9. This work aimed to study the microstructure and wear resistance of supermartensitic stainless steel modified with 0.3 wt. (% and 0.7 wt. (% processed by spray forming (SF-SMSS 0.3%B and SF-SMSS 0.7%B, respectively. These boron contents were selected in order to improve the wear resistance of supermartensitic stainless steel through the formation of uniformly distributed borides maintaining the characteristics of the corrosion resistant matrix. SF-SMSS 0.7%B presents an abrasive wear resistance considerably higher than spray-formed supermartensitic stainless steel without boron addition (SF-SMSS.

  12. Proposition of a Solution for the Setting of the Abrasive Waterjet Cutting Technology

    Czech Academy of Sciences Publication Activity Database

    Valíček, Jan; Harničárová, M.; Kušnerová, M.; Grznárik, R.; Zavadil, J.

    2013-01-01

    Roč. 13, č. 5 (2013), s. 279-285 ISSN 1335-8871 R&D Projects: GA MŠk ED2.1.00/03.0082 Institutional support: RVO:68145535 Keywords : abrasive waterjet cutting of materials * surface topography function * correlation relations * surface roughness * optimization of technology Subject RIV: JQ - Machines ; Tools Impact factor: 1.162, year: 2013 http://www.degruyter.com/view/j/msr.2013.13.issue-5/msr-2013-0041/msr-2013-0041. xml

  13. Insulina e glicose como moduladores do desenvolvimento de plântulas de milho doce (Su1)

    OpenAIRE

    Oliveira Júnior, Luiz Fernando Ganassali; Bressan-Smith, Ricardo; Oliveira, Antônia Elenir Amâncio de; Pereira, Messias Gonzaga; Silva, Luciana Belarmindo; Viana, Leandro Hespanhol; Vieira, Henrique Duarte

    2009-01-01

    Durante a germinação e o desenvolvimento pós-germinativo de milho, o fluxo metabólico é intenso, ocorrendo síntese e degradação de açúcares (glicose, frutose e sacarose) e hidrólise de amido, além da redução da concentração do ácido abscísico (ABA). Acredita-se que altas concentrações de glicose exógena, promovam acúmulo de ABA, proporcionando atraso na germinação e desenvolvimento de plântulas. Concentrações menores, por outro lado, podem ocasionar estímulo na germinação e desenvolvimento. N...

  14. Desenvolvimento regional sob o enfoque pós-keynesiano

    Directory of Open Access Journals (Sweden)

    Júlia Elisabete Barden

    2007-01-01

    Full Text Available Este trabalho tem como objetivo fazer uma revisão bibliográfica acerca de estudosque analisam o desenvolvimento regional sob a perspectiva da teoria pós-keynesiana. Osresultados destes demonstram que o sistema financeiro, em especial os bancos,influenciam no grau de desenvolvimento das regiões, sobretudo, porque o comportamentodestes agentes segue um conceito importante utilizado pela teoria, a preferência pelaliquidez. Assim, a disponibilidade de crédito para investimento no sistema produtivosofrerá impactos importantes conforme a preferência pela liquidez dos bancos.Abstract This paper has as objective to bring a bibliographical review about the studies thatanalyze the regional development on the Post-Keynesian theory perspective. The resultsobtained show that the financial system especially the banks, however these agentsbehavior follow an important concept used by the theory, the preference to the liquidity.Yet, the credit responsibility for the investment in the productive system will sufferimportant impacts due to the preference for the liquidity from the banks.

  15. Um metodo para modelagem de exceções em desenvolvimento baseado em componentes

    OpenAIRE

    Patrick Henrique da Silva Brito

    2005-01-01

    Resumo: Devido a grande popularização do Desenvolvimento Baseado em Componentes (DBC), ele vem sendo empregado inclusive no desenvolvimento de sistemas computacionais críticos. O emprego do DBC na construção de sistemas confiáveis evidencia a necessidade de se desenvolver componentes de software que sejam robustos e que possuam uma garantia maior do seu funcionamento correto. Tratamento de exceções é uma técnica bastante conhecida para a verificação e tratamento de erros em sistemas de softwa...

  16. Avaliação da influência da temperatura sobre o desenvolvimento de Aedes albopictus

    Directory of Open Access Journals (Sweden)

    Daniéla Cristina Calado

    2002-04-01

    Full Text Available OBJETIVO: Verificar a influência da temperatura sobre os estágios de desenvolvimento de Aedes albopictus sob condições de laboratório. MÉTODOS: Foi avaliado o período de desenvolvimento dos estágios de ovo, larva e pupa em quatro temperaturas constantes de 15ºC, 20ºC, 25ºC e 30ºC em câmaras climatizadas com umidade relativa do ar oscilando entre 70% e 85% e fotoperíodo de CE 12:12 horas. Pela análise de variância, foram testados os efeitos das quatro temperaturas constantes. RESULTADOS: O período de incubação dos ovos compreendeu 38,38; 19,09; 13,10; e 10,44 dias; o período larval dos indivíduos machos atingiu 30,13; 13,83; 7,36; e 5,57 dias; o período larval para fêmeas apresentou duração de 33,22; 15,00; 8,06; e 6,16 dias; o período pupal em machos compreendeu 8,01; 4,92; 2,40; e 1,76 dias, enquanto nas fêmeas foi de 8,15; 5,11; 2,60; e 1,88 dias sob as temperaturas de 15ºC, 20ºC, 25ºC e 30ºC, respectivamente. Em todos os estágios de desenvolvimento, foram encontradas diferenças significativas, entre as temperaturas avaliadas, em torno de 5% no tempo de desenvolvimento. O período de desenvolvimento foi inversamente relacionado à temperatura, com o período larval mais breve em machos que em fêmeas. Nas temperaturas de 20ºC a 30ºC, o desenvolvimento foi mais breve e com maior viabilidade que a 15ºC. CONCLUSÕES: Nas condições em que foram realizados os experimentos, a temperatura afetou de forma significativa e inversamente proporcional os estágios imaturos de Aedes albopictus. Esses resultados mostram que os estágios imaturos são mais suscetíveis durante os períodos de baixas temperaturas devido ao maior tempo necessário para completar o desenvolvimento, informação que pode ser utilizada em estratégias de controle.

  17. Desenvolvimento puberal em meninas tratadas de LLA

    Directory of Open Access Journals (Sweden)

    Monteiro I.M.M.

    1998-01-01

    Full Text Available OBJETIVO: Com o objetivo de avaliar o desenvolvimento puberal após o tratamento de leucemia linfóide aguda (LLA na infância, foi realizado um estudo retrospectivo, em meninas tratadas de janeiro de 1980 a janeiro de 1991, no Centro de Investigações Hematológicas "Dr. Domingos A. Boldrini", em Campinas-SP. CASUÍSTICA E MÉTODO: Foram selecionadas 42 meninas, tratadas antes da puberdade com quimioterapia sistêmica e intratecal e radioterapia cranial, utilizando doses de 18 ou 24 Grays (Gy. RESULTADOS: As idades médias da telarca, pubarca e menarca foram inferiores às do grupo-controle, embora com significância estatística apenas para a idade da telarca. Não houve diferenças entre os grupos tratados com 18 ou 24Gy. As meninas tratadas antes dos cinco anos de idade apresentaram idade média da menarca estatisticamente inferior àquelas tratadas após cinco anos e em relação ao grupo-controle. CONCLUSÃO: Os resultados mostraram que o desenvolvimento puberal em meninas tratadas de LLA na infância foi mais precoce que o de meninas saudáveis.

  18. Descrição do desenvolvimento neuropsicomotor e visual de crianças com deficiência visual

    Directory of Open Access Journals (Sweden)

    Telma de Araujo Souza

    2010-12-01

    Full Text Available Objetivo: Avaliar o desenvolvimento neuropsicomotor e visual de crianças com deficiência visual. Métodos: Foram avaliadas 45 crianças, de ambos os gêneros, em um período de 6 meses. As crianças foram distribuidas em dois grupos de estudo: experimental e de controle. Dessa forma aplicou-se a avaliação do desenvolvimento neuropsicomotor e da funcionalidade visual. Resultado: No grupo controle 86,66% da amostra estava inadequado quanto ao comportamento da coordenação, entretanto, todos os aspectos analisados estavam inadequados. As diferenças entre os grupos mostraram-se significativas, já que valores como p<0,05 foram evidenciados, tanto no comportamento da funcionalidade visual, quanto no desenvolvimento neuropsicomotor. Conclusão: Na amostra estudada, observou-se que os deficientes visuais caracterizavam-se por apresentar atraso global, do desenvolvimento, principalmente no comportamento da coordenação.

  19. Effects of mechanical cleaning by manual brushing and abrasive blasting on lime render coatings on Architectural Heritage

    Directory of Open Access Journals (Sweden)

    Iglesias-Campos, M. A.

    2014-12-01

    Full Text Available This research studies the effects of mechanical cleaning by brushing and by abrasive blasting on the lime render coating of a façade. After analysing the properties of the material, the deposits to be removed and their possible influence on the treatment, different cleaning tests were made by manual brushing and by blasting with three varieties of abrasives at 45° and 75° angles, keeping the other parameters constant. Taking the restorer’s perspective as a starting point, and in order to fulfil the practical requirements of an intervention, tests were evaluated with macro-photography, USB digital microscope and stereomicroscope with 3D visualization and measurement. From the results can be concluded that abrasives with low friability and greater grain size than the space between mortar aggregates blasted at a 75° angle reduce the differential erosion compared to other abrasives; although manual brushing has less impact on the surface.En este trabajo se estudian los efectos de las limpiezas mecánicas con cepillado y con proyección de abrasivos sobre un revestimiento exterior de cal. Tras documentar las propiedades del material, de los depósitos superficiales y de su posible influencia en el tratamiento, se realizaron diferentes catas de limpieza con cepillado manual y con proyección de tres abrasivos con ángulos de 45° y 75° manteniendo constantes el resto de parámetros. Partiendo de la visión del conservador-restaurador y de un carácter práctico según las necesidades reales de intervención, los ensayos se evaluaron con macrofotografía, microscopio digital USB y microscopio estereoscópico con visualización y medición en 3D. De los resultados se determina que los abrasivos de baja friabilidad y granulometría mayor que el espacio entre los áridos del mortero proyectados con un ángulo de 75° reducen la erosión diferencial en comparación a otros abrasivos, aunque el cepillado manual altera menos la superficie.

  20. OS MODELOS DE CRESCIMENTO E DE DESENVOLVIMENTO ECONÔMICO E SUA APLICABILIDADE NAS ECONOMIAS REGIONAIS NÃO DESENVOLVIDAS

    OpenAIRE

    Adelmo M. França

    2012-01-01

    Neste artigo serão apresentadas as definições de crescimento e desenvolvimento econômico e as algumas discussões propostas pelos principais modelos econômicos voltados ao crescimento e desenvolvimento econômicos, questionando o fato deles terem suas origens nas economias desenvolvidas e, portanto, distantes das realidades sociais, políticas e econômicas dos países e das regiões pobres ou em fase de desenvolvimento. As abordagens sobre o tema estarão focadas na realidade econômica brasileira d...

  1. Effect of distribution of striated laser hardening tracks on dry sliding wear resistance of biomimetic surface

    Science.gov (United States)

    Su, Wei; Zhou, Ti; Zhang, Peng; Zhou, Hong; Li, Hui

    2018-01-01

    Some biological surfaces were proved to have excellent anti-wear performance. Being inspired, Nd:YAG pulsed laser was used to create striated biomimetic laser hardening tracks on medium carbon steel samples. Dry sliding wear tests biomimetic samples were performed to investigate specific influence of distribution of laser hardening tracks on sliding wear resistance of biomimetic samples. After comparing wear weight loss of biomimetic samples, quenched sample and untreated sample, it can be suggested that the sample covered with dense laser tracks (3.5 mm spacing) has lower wear weight loss than the one covered with sparse laser tracks (4.5 mm spacing); samples distributed with only dense laser tracks or sparse laser tracks (even distribution) were proved to have better wear resistance than samples distributed with both dense and sparse tracks (uneven distribution). Wear mechanisms indicate that laser track and exposed substrate of biomimetic sample can be regarded as hard zone and soft zone respectively. Inconsecutive striated hard regions, on the one hand, can disperse load into small branches, on the other hand, will hinder sliding abrasives during wear. Soft regions with small range are beneficial in consuming mechanical energy and storing lubricative oxides, however, soft zone with large width (>0.5 mm) will be harmful to abrasion resistance of biomimetic sample because damages and material loss are more obvious on surface of soft phase. As for the reason why samples with even distributed bionic laser tracks have better wear resistance, it can be explained by the fact that even distributed laser hardening tracks can inhibit severe worn of local regions, thus sliding process can be more stable and wear extent can be alleviated as well.

  2. Desenvolvimento territorial rural no Brasil: limites e potencialidades dos CONSADs

    Directory of Open Access Journals (Sweden)

    Antonio César Ortega

    2007-06-01

    Full Text Available A motivação principal desse trabalho é avaliar a capacidade da abordagem territorial em contribuir com o enfrentamento da pobreza e das desigualdades sociais brasileiras, representando uma alternativa de geração de emprego e renda em territórios rurais deprimidos. Por meio dos Consórcios de Segurança Alimentar e Desenvolvimento Local (CONSADs analisa-se as potencialidades e as dificuldades que essa estratégia vem enfrentando para estabelecer a cooperação entre o poder público e a sociedade civil voltada para o fomento, o apoio logístico e a canalização de recursos para as iniciativas territoriais, projetos e ações estruturantes que visam a geração de emprego e renda, com a garantia de segurança alimentar e do desenvolvimento local.This paper aims at evaluating the capacity of the territorial approach to contribute to poverty issues and Brazilian social inequalities, representing an alternative of employment and income generation in depressed rural territories. Through Consórcios de Segurança Alimentar e Desenvolvimento Local-CONSADs (Food Safety Consortia and Local Development we analyzed the potentialities and difficulties the strategy is facing to establish the cooperation between public power and civil society regarding fomentation, logistic support and canalization of resources for territorial initiatives, projects and structuring actions that seek employment and income generation with food safety warranty and local development.

  3. The effectiveness of dentifrices without and with sodium lauryl sulfate on plaque, gingivitis and gingival abrasion--a randomized clinical trial.

    Science.gov (United States)

    Sälzer, S; Rosema, N A M; Martin, E C J; Slot, D E; Timmer, C J; Dörfer, C E; van der Weijden, G A

    2016-04-01

    The aim of this study was to compare the efficacy of a dentifrice without sodium lauryl sulfate (SLS) to a dentifrice with SLS in young adults aged 18-34 years on gingivitis. One hundred twenty participants (non-dental students) with a moderate gingival inflammation (bleeding on probing at 40-70 % of test sites) were included in this randomized controlled double blind clinical trial. According to randomization, participants had to brush their teeth either with dentifrice without SLS or with SLS for 8 weeks. The primary outcome was bleeding on marginal probing (BOMP). The secondary outcomes were plaque scores and gingival abrasion scores (GA) as well as a visual analogue scale (VAS) score at exit survey. Baseline and end differences were analysed by univariate analysis of covariance (ANCOVA) test, between group differences by independent t test and within groups by paired sample t test. BOMP improved within groups from on average 0.80 at baseline to 0.60 in the group without SLS and to 0.56 in the group with SLS. No statistical difference for BOMP, plaque and gingival abrasion was found between both groups. VAS scores for taste, freshness and foaming effect were significantly in favour of the SLS-containing dentifrice. The test dentifrice without SLS was as effective as a regular SLS dentifrice on gingival bleeding scores and plaque scores. There was no significant difference in the incidence of gingival abrasion. In patients diagnosed with gingivitis, a dentifrice without SLS seems to be equally effective compared to a dentifrice with SLS and did not demonstrate any significant difference in gingival abrasion. In patient with recurrent aphthous ulcers, the absence of SLS may even be beneficial. However, participants indicate that they appreciate the foaming effect of a dentifrice with SLS more.

  4. A influência da família no desenvolvimento da superdotação

    Directory of Open Access Journals (Sweden)

    Paulo Vinícius Carvalho Silva

    Full Text Available Vários estudos destacam a importância da família para a manifestação, desenvolvimento e reconhecimento da superdotação. O desenvolvimento de comportamentos de superdotação impõe novos desafios e demandas aos próprios indivíduos superdotados e seus familiares, que, em algumas ocasiões, não possuem o esclarecimento necessário para atendê-las. Sendo assim, o objetivo geral deste ensaio é sintetizar e analisar criticamente as investigações realizadas sobre a relação entre a família e o indivíduo superdotado nas áreas esportiva, musical, artística e acadêmica. Estas pesquisas indicam uma grande variedade de práticas parentais e características familiares associadas ao desenvolvimento de comportamentos de superdotação. A análise crítica dos artigos examinados poderá suscitar a realização de outras pesquisas sobre a participação da família no processo de desenvolvimento do talento. Além disso, os esclarecimentos deste ensaio poderão auxiliar a elaboração e implementação de programas de atendimento a indivíduos superdotados e suas respectivas famílias.

  5. Single layer and multilayer wear resistant coatings of (Ti,Al)N: a review

    International Nuclear Information System (INIS)

    PalDey, S.; Deevi, S.C.

    2003-01-01

    We review the status of (Ti,Al)N based coatings obtained by various physical vapor deposition (PVD) techniques and compare their properties. PVD techniques based on sputtering and cathodic arc methods are widely used to deposit wear resistant (Ti,Al)N coatings. These techniques were further modified to improve the metal ionization rate and to eliminate macrodroplets from plasma streams. We summarize manufacture of target/cathode, substrate materials for deposition of coatings, deposition parameters, and the effect of deposition parameters on the physical and mechanical properties of (Ti,Al)N coatings. It is shown that (Ti,Al)N coatings by PVD enhance the wear, thermal, and oxidation resistance of a wide variety of tool materials. We discuss the wear resistant properties of (Ti,Al)N for various machining applications as compared with coatings such as TiN, Ti(C,N) and (Ti,Zr)N. High hardness (∼28-32 GPa), relatively low residual stress (∼5 GPa), superior oxidation resistance, high hot hardness, and low thermal conductivity make (Ti,Al)N coatings most desirable in dry machining and machining of abrasive alloys at high speeds. Multicomponent coatings based on different metallic and nonmetallic elements combine the benefit of individual components leading to a further refinement of coating properties. Alloying additions such as Cr and Y drastically improve the oxidation resistance, Zr and V improve the wear resistance, whereas, Si increases the hardness and resistance to chemical reactivity of the film. Addition of boron improves the abrasive wear behavior of Ti-Al based coatings due to the formation of TiB 2 and BN phases depending on the deposition conditions. Hafnium based nitrides and carbides have potential for resistance to flank and crater wear. The presence of a large number of interfaces between individual layers of a multilayered structure results in a drastic increase in hardness and strength. (Ti,Al)N multilayer super lattice coatings with lattice

  6. Considerações sobre o desenvolvimento de jogos por meio do framework Scrum

    Directory of Open Access Journals (Sweden)

    Olívia Hamada

    2016-02-01

    Full Text Available Os jogos (games se configuram como a contemporânea maneira das pessoas se relacionarem com as soluções tecnológicas e com os aplicativos. As expansões nas vendas dos dispositivos, dos aplicativos e os números de usuários, ano a ano, aumentam em proporções interessantes em termos de negócios e de consolidação de tendências nos hábitos. Desta forma, o desenvolvimento rápido, eficaz e de qualidade para os jogos se torna essencial para as empresas e para os parceiros que participam das suas elaborações, comercialização, suporte e disseminação. Utilizam-se metodologias diversas para esse desenvolvimento, tendo as metodologias ágeis as maiores possibilidades de sucesso. Este artigo trata do desenvolvimento dos jogos, as metodologias aplicadas e, em particular, do framework Scrum. Conclui-se que o Scrum é efetivamente uma boa opção para a construção de jogos, em função de suas características próprias.

  7. The abrasive blasting technique. Matching the waste minimisation precept

    International Nuclear Information System (INIS)

    Welbers, Philipp; Noll, Thomas; Braehler, Georg; Sohnius, Bern

    2010-01-01

    Nowadays main challenges in the nuclear industry are, besides the development and design of new facilities, the dismantling of outlived nuclear installations and subsequent waste handling. Not only Germany but all countries and institutions which are involved in our business face similar problems: A large quantity of slightly contaminated waste, equipment and civil structures, arise inevitably during operation and, especially, during dismantling. This waste occurs in a huge amount due to its bulky nature, e.g. pipe-work. Storage of bulky items is very expensive and would not be compatible with the waste minimisation precept. Treatment in an ecological correct and economical beneficial way is the key factor in dealing with this waste. This means decontamination of the waste up to clearance levels where possible. A suitable solution is the Abrasive Blasting Technique. (orig.)

  8. Influence of Surface Pretreatment on the Corrosion Resistance of Cold-Sprayed Nickel Coatings in Acidic Chloride Solution

    Science.gov (United States)

    Scendo, Mieczyslaw; Zorawski, Wojciech; Staszewska-Samson, Katarzyna; Makrenek, Medard; Goral, Anna

    2018-03-01

    Corrosion resistance of the cold-sprayed nickel coatings deposited on the Ni surface (substrate) without and with abrasive grit-blasting treatment of the substrate was investigated. The corundum powder with different grain sizes was used. The corrosive environment contained an acidic chloride solution. The mechanism of the corrosion of nickel was suggested and discussed. Corrosion electrochemical parameters were determined by electrochemical methods. The corrosion effect of a nickel coating depends on the grain size used to prepare the substrate. The nickel coating after the medium grit-blasting treatment of the substrate was found to be the most corrosion resistant. However, the smallest resistance on the corrosion effect should be attributed to the nickel coating on the substrate after the coarse grit-blasting treatment.

  9. O desafio político do desenvolvimento sustentado The political challenge of sustainable development

    Directory of Open Access Journals (Sweden)

    Roberto P. Guimarães

    1995-01-01

    Full Text Available A unanimidade que hoje parece haver em favor do desenvolvimento sustentado contrasta com a ausência de iniciativas políticas significativas para transformar as instituições econômicas, sociais e políticas que estão comprometidas com o estilo vigente de desenvolvimento. Em particular, há uma patente contradição entre o discurso antiestatista hegemônico e as exigências do desenvolvimento sustentado, que incluem um Estado ainda mais forte, em suas capacidades reguladoras e de planificação, que o Estado intervencionista do passado.The seeming unanimity in favour of sustainable development stands in contrast to the absence of meaningful political initiatives in order to change the economic, social and political intitutions linked to the ongoing style of development In particular there is a patent contradiction between the hegemonic antistatist discourse and the requirements for sustainable development, including a state with even more regulatory and planning powers than the interventionist state of the past.

  10. Wear resistance of layers hard faced by the high-alloyed filler metal

    OpenAIRE

    Dušan Arsić; Vukić Lazić; Ruzica R. Nikolic; Milan Mutavdžić; Srbislav Aleksandrović; Milan Djordjević

    2016-01-01

    The objective of this work was to determine the wear resistance of layers hard faced by the high-alloyed filler metal, with or without the austenite inter-layer, on parts that operate at different sliding speeds in conditions without lubrication. The samples were hard faced with the filler metal E 10-UM-60-C with high content of C, Cr and W. Used filler metal belongs into group of alloys aimed for reparatory hard facing of parts damaged by abrasive and erosive wear and it is characterized by ...

  11. Investigation of sandwich material surface created by abrasive water jet (AWJ via vibration emission

    Directory of Open Access Journals (Sweden)

    P. Hreha

    2014-01-01

    Full Text Available The paper presents research a of abrasive waterjet cutting of heterogeneous “sandwich“ material with different Young modulus of elasticity of the cutted surface geometry by means of vibration emission. In order to confirm hypothetical assumptions about direct relation between vibration emission and surface quality an experiment in heterogeneous material consisting of stainless steel (DIN 1.4006 / AISI 410 and alloy AlCuMg2 has been provided.

  12. Estudo longitudinal do desenvolvimento da comunicação em diversas economias mundiais

    OpenAIRE

    Arruda Filho, Emílio José Montero

    2012-01-01

    O desenvolvimento do setor de comunicação de um país possui relações com o seu desenvolvimento econômico e é possível demonstrar essa conexão estatisticamente, como tem sido feito por pesquisadores de instituições como a ITU (International Telecommunications Union). Como esses dados estão apenas apresentados na forma simples e não levam em conta fatores de interconexão, é importante desenvolver pesquisas que avaliem a conexão entre variáveis relevantes no campo. Este trabalho visa analisar o...

  13. Study of Stainless Steel Resistance in Conditions of Tribocorrosion Wear

    Directory of Open Access Journals (Sweden)

    Goran Rozing

    2015-07-01

    Full Text Available Analyzed was the influence of tribocorrosion wear due to effects of fatty acids present in the processed medium. The analysis was conducted on samples made of two austenitic and two martensitic stainless steels. Austenitic steels were tested in their nitrided state and martensitic in their induction hardened state. Conducted were laboratory tests of corrosion resistance of samples, analysis of the microstructure and hardness. To see how the applied processes for modifying the surface of stainless steels behave in realistic conditions, it was conducted the examination of samples/parts of a sunflower cake chain conveyer. Based on the comparison of results obtained in the laboratory and in real conditions, it was estimated that steels AISI 420 and AISI 431 with induction hardened surfaces have a satisfactory resistance to abrasive-adhesive wear in the presence of fatty acids.

  14. Desenvolvimento do feijoeiro sob o uso de biofertilizante e adubação mineral.

    OpenAIRE

    Galbiatti, João A.; Silva, Flávia G. da; Franco, Claudenir F.; Caramelo, Anaira D.

    2011-01-01

    A produção intensiva de alimentos exige manejo adequado do solo para garantir a produtividade e a sustentabilidade ambiental. Uma das alternativas é a utilização de resíduos orgânicos no desenvolvimento das culturas, diminuindo a dependência de adubos minerais. Com o objetivo de avaliar o desenvolvimento da cultura de feijão (Phaseolus vulgaris L.), utilizando biofertilizante e adubação mineral, conduziu-se o experimento com seis tratamentos dispostos ao acaso, em esquema fatorial, em quatro ...

  15. Effect of Abrasive Waterjet Peening Surface Treatment of Steel Plates on the Strength of Single-Lap Adhesive Joints

    Directory of Open Access Journals (Sweden)

    Kamil Anasiewicz

    2017-09-01

    Full Text Available The paper presents results of comparative study of shear strength of single–lap adhesive joints, depending on the method of surface preparation of steel plates with increased corrosion resistance. The method of preparing adherend surfaces is often one of the most important factors determining the strength of adhesive joints. Appropriate geometric surface development and cleaning of the surface enhances adhesion forces between adherend material and adhesive. One of the methods of shaping engineering materials is waterjet cutting, which in the AWJP – abrasive waterjet peening variant, serves to shape flat surfaces of the material by changing the roughness and introducing stresses into the surface layer. These changes are valuable when preparing adhesive joints. In the study, surface roughness parameters obtained with AWJP treatment, were analyzed in direct relation to the strength of the adhesive joint. As a consequence of the experimental results analysis, the increase in the strength of the adhesive joints was observed in a certain range of parameters used for AWJP treatment. A decrease in shear strength of adhesive joint with the most modified topography of overlap surface was observed.

  16. Desenvolvimento, complexo industrial da saúde e política industrial

    Directory of Open Access Journals (Sweden)

    Gadelha Carlos Augusto Grabois

    2006-01-01

    Full Text Available O artigo situa a questão da saúde no contexto do desenvolvimento nacional e da política industrial. Tomou-se a idéia de corte estruturalista, marxista e schumpeteriano, onde a indústria e as inovações constituem os elementos determinantes do dinamismo das economias capitalistas e de sua posição relativa na economia mundial. Todos os países que se desenvolveram e passaram a competir em melhores condições com os países avançados associaram uma indústria forte com uma base endógena de conhecimento, de aprendizado e de inovação. Todavia, na área da saúde essa visão é problemática, uma vez que os interesses empresariais se movem pela lógica econômica do lucro e não para o atendimento das necessidades da saúde. A noção de complexo industrial da saúde constitui uma tentativa e fornecer um referencial teórico que permita articular duas lógicas distintas: a sanitária e a do desenvolvimento econômico. O trabalho procurou mostrar, com base em dados de comércio exterior, como a desconsideração da lógica do desenvolvimento nas políticas de saúde levou a uma situação de vulnerabilidade econômica do setor que pode limitar os objetivos de universalidade, eqüidade e integralidade. Nesse contexto, propõe-se uma ruptura cognitiva e política com as visões antagônicas que colocam, de um lado, as necessidades da saúde e, de outro, da indústria. Um país que pretende chegar a uma condição de desenvolvimento e de independência requer, ao mesmo tempo, indústrias fortes e inovadoras, e um sistema de saúde inclusivo e universal.

  17. Desenvolvimento, complexo industrial da saúde e política industrial

    Directory of Open Access Journals (Sweden)

    Carlos Augusto Grabois Gadelha

    2006-08-01

    Full Text Available O artigo situa a questão da saúde no contexto do desenvolvimento nacional e da política industrial. Tomou-se a idéia de corte estruturalista, marxista e schumpeteriano, onde a indústria e as inovações constituem os elementos determinantes do dinamismo das economias capitalistas e de sua posição relativa na economia mundial. Todos os países que se desenvolveram e passaram a competir em melhores condições com os países avançados associaram uma indústria forte com uma base endógena de conhecimento, de aprendizado e de inovação. Todavia, na área da saúde essa visão é problemática, uma vez que os interesses empresariais se movem pela lógica econômica do lucro e não para o atendimento das necessidades da saúde. A noção de complexo industrial da saúde constitui uma tentativa e fornecer um referencial teórico que permita articular duas lógicas distintas: a sanitária e a do desenvolvimento econômico. O trabalho procurou mostrar, com base em dados de comércio exterior, como a desconsideração da lógica do desenvolvimento nas políticas de saúde levou a uma situação de vulnerabilidade econômica do setor que pode limitar os objetivos de universalidade, eqüidade e integralidade. Nesse contexto, propõe-se uma ruptura cognitiva e política com as visões antagônicas que colocam, de um lado, as necessidades da saúde e, de outro, da indústria. Um país que pretende chegar a uma condição de desenvolvimento e de independência requer, ao mesmo tempo, indústrias fortes e inovadoras, e um sistema de saúde inclusivo e universal.

  18. Rugged Packaging for Damage Resistant Inertial Fusion Energy Optics

    Energy Technology Data Exchange (ETDEWEB)

    Stelmack, Larry

    2003-11-17

    The development of practical fusion energy plants based on inertial confinement with ultraviolet laser beams requires durable, stable final optics that will withstand the harsh fusion environment. Aluminum-coated reflective surfaces are fragile, and require hard overcoatings resistant to contamination, with low optical losses at 248.4 nanometers for use with high-power KrF excimer lasers. This program addresses the definition of requirements for IFE optics protective coatings, the conceptual design of the required deposition equipment according to accepted contamination control principles, and the deposition and evaluation of diamondlike carbon (DLC) test coatings. DLC coatings deposited by Plasma Immersion Ion Processing were adherent and abrasion-resistant, but their UV optical losses must be further reduced to allow their use as protective coatings for IFE final optics. Deposition equipment for coating high-performance IFE final optics must be designed, constructed, and operated with contamination control as a high priority.

  19. ESTRUTURA FUNDIÁRIA E DESENVOLVIMENTO HUMANO: UMA ANÁLISE PARA AS MICRORREGIÕES DO RIO GRANDE DO SUL

    Directory of Open Access Journals (Sweden)

    Adilson Giovanini

    2011-12-01

    Full Text Available A partir da perspectiva do desenvolvimento como expansão das capacitações de Amartya Sen, o artigo testa a hipótese de que a concentração fundiária pode ser um fator prejudicial ao desenvolvimento humano nas microrregiões do Rio Grande do Sul. A pesquisa se caracteriza como histórico-empírica na medida em que busca na história a contextualização da atual estrutura fundiária e estatística e econométrica uma vez que estima a relação entre indicadores de desenvolvimento humano e de estrutura fundiária. Para tanto, calcula-se a correlação e ajustam-se regressões múltiplas entre indicadores de estrutura fundiária e de desenvolvimento humano. Um dos resultados encontrados é o de que as microrregiões com uma estrutura fundiária mais desigual possuem piores indicadores de expectativa de vida ao nascer.

  20. Improvement of a separation method for the reduction of secondary waste from the water-jet abrasive suspension cutting technique

    International Nuclear Information System (INIS)

    Brandauer, M.; Gentes, S.; Heneka, A.; Krauss, C.O.; Geckeis, H.; Plaschke, M.; Schild, D.; Tobie, W.

    2017-01-01

    Full text of publication follows. Disassembling the reactor pressure vessel and its built-in components is a huge challenge in the deconstruction of a nuclear power plant. After being exposed to neutron irradiation for years, the activated components need to be disassembled and packed by remote controlled techniques. Underwater disassembling systems have the advantage of the shielding effect of water against radiation. To avoid the generation of aerosols, cold cutting processes are preferred. A cutting method that meets these requirements is the water-jet abrasive suspension cutting technique (WASS). This method provides high flexibility and is immune towards mechanical stress in the components. During the cutting process, a mixture of abrasive particles and radioactive steel particles from the cut components is generated. Depending on the operational conditions, the amount of this secondary waste increases substantially. Therefore, despite of its intrinsic technical benefits, WASS has a serious disadvantage towards other cutting techniques due to the huge disposal costs of secondary waste. During our previous joint research project between KIT and AREVA GmbH called NENAWAS ('New Disposal Methods for the Secondary Waste Treatment of the Water-jet Abrasive Suspension Cutting Technique', funded by the German ministry for education and research, BMBF), a prototype separation device for WASS secondary waste was developed and tested. Using a magnetic filter, steel particles could be successfully separated from the rest of the secondary waste. The separation process is examined using elemental analysis (ICP-OES) for quantification of the separation grade. Additionally, morphologies of particles and particle aggregates before and after the separation process were examined by scanning electron microscopy (SEM). In the abrasive particle fraction after separation of the steel particles a remaining contamination by tiny steel particles could be detected by elemental and

  1. CARTOGRAFIAS DO PIAUÍ: RELACIONANDO INFRAESTRUTURA E DESENVOLVIMENTO SOCIAL

    Directory of Open Access Journals (Sweden)

    Paulo Antônio Barbosa Júnior

    2016-08-01

    Full Text Available Durante as décadas de 50 a 90, o Piauí foi o Estado mais pobre do Brasil. Recentemente, o Piauí tem apresentado acelerado crescimento econômico, devido em parte ao fortalecimento dos setores de comércio e construção, e a implantação da agricultura moderna na porção do Cerrado piauiense da região MAPITOBA. Apesar do recente incremento econômico, percebe-se que no Piauí, assim como em outros estados do Brasil, o desenvolvimento se dá de forma irregular com relação aos aspectos sociais e seus padrões de distribuição no território. Neste sentido, o presente trabalho busca mostrar que no Piauí a concentração de bens e pessoas está em parte condicionada a infraestrutura de transporte, com exceção da mesorregião Sudoeste Piauiense, onde o modelo de desenvolvimento adotado é essencialmente diferente do modelo das demais regiões. Desta forma, a baixa integração regional no Piauí tem contribuído para o surgimento de duas porções territoriais distintas e isoladas: uma ao norte, com características predominantemente urbanas e relativa concentração de bens e pessoas; e outra ao sul, onde se estabeleceu a última fronteira agrícola do país, com a implantação da agricultura moderna em áreas de vazios demográficos e baixos índices de desenvolvimento social. Assim, partindo-se da demanda por estudos que melhor descrevam as especificidades do território e que contribuam para a elaboração de políticas públicas adjetivadas ao local, o trabalho faz uso da Cartografia Temática e da Análise Espacial para descrever a situação atual do estado do Piauí com relação a Renda e Educação.

  2. Monitoring and control of fine abrasive finishing processes

    DEFF Research Database (Denmark)

    Lazarev, Ruslan

    In engineering, surfaces with specified functional properties are of high demand in various applications. Desired surface finish can be obtained using several methods. Abrasive finishing is one of the most important processes in the manufacturing of mould and dies tools. It is a principal method ...... was segmented using discretization methods. The applied methodology was proposed for implementation as an on-line system and is considered to be a part of the next generation of STRECON NanoRAP machine....... to remove unwanted material, obtain desired geometry, surface quality and surface functional properties. The automation and computerization of finishing processes involves utilisation of robots, specialized machines with several degrees of freedom, sensors and data acquisition systems. The focus...... of this work was to investigate foundations for process monitoring and control methods in application to semi-automated polishing machine based on the industrial robot. The monitoring system was built on NI data acquisition system with two sensors, acoustic emission sensor and accelerometer. Acquired sensory...

  3. Disponibilidades e auto-implicação: desenvolvimento profissional e plurilinguismo

    Directory of Open Access Journals (Sweden)

    Gonçalves, Maria de Lurdes

    2007-01-01

    Full Text Available A crescente importância e o relevo que o plurilinguismo vem adquirindo, alargou o âmbito do trabalho dos docentes de línguas. Assim, a educação plurilingue e intelectual constitui um importante desafio para o crescimento profissional de um educador em línguas, sendo os programas de formação, enquanto mecanismos de desenvolvimento profissional, uma condição necessária para responder a esse desafio. Este texto apresenta um programa de formação para o desenvolvimento do plurilinguismo e analisa as disponibilidades e auto-implicação que esta proposta de formação encontrou no seio do grupo de professores de línguas de uma escola secundária em Portugal

  4. O desenvolvimento sustentável: uma palavra e as coisas

    Directory of Open Access Journals (Sweden)

    Wolf-Dietrich SAHR

    1998-12-01

    Full Text Available A discussão sobre o desenvolvimento sustentável é um exercício interessante para se entender as novas formas do relacionamento entre a ciência e a política que surgiram durante os trinta anos passados. Originalmente vindo do âmbito da economia e modificado por abordagens ecológicas, o conceito se transformou, durante os anos 80, em palavra-chave nas discussões internacionais e interdisciplinares sobre o desenvolvimento em sua relação com a natureza. Percebe-se que várias qualidades clássicas da metodologia científica, como exatidão das definições e termos técnicos, epistemologias disciplinares e rígidas formulações de teorias, perderam gradativamente sua relevância durante esse processo. Isso colocou os limites da própria ciência acadêmica em questão. Através de uma crítica do economicismo ecológico, que até hoje domina no discurso, abre-se um espaço para a incorporação de abordagens epistemológicas diferentes da ciência pura como atividades sociais, métodos psico-analíticos e até mesmo atividades da arte e da religião. O discurso do desenvolvimento sustentável apresenta-se, deste modo, como uma modificação cultural do próprio meio académico nas condições da pós-modernidade.

  5. A CONTRIBUIÇÃO DO GERENCIAMENTO DE PROJETOS NO PROCESSO DE DESENVOLVIMENTO DE PRODUTOS

    Directory of Open Access Journals (Sweden)

    Paulo Fernando Pinto Barcellos

    2014-09-01

    Full Text Available Em um ambiente complexo, caracterizado por uma demanda crescente de produtos customizados e personalizados, a diminuição do tempo de ciclo para o lançamento de novos produtos torna-se um ponto importante para obtenção de um maior retorno do investimento nos projetos de desenvolvimento. Assim, o objetivo proposto neste artigo foi investigar a contribuição das metodologias de gerenciamento de projetos para a diminuição do tempo de desenvolvimento de produtos. Para a realização deste estudo, e tendo em vista o objetivo proposto, foi utilizada metodologia qualitativa bibliográfica. As análises, realizadas no sentido de entender qual o tipo de processo de gerenciamento de projetos pode melhor contribuir para o desenvolvimento de produtos, trouxeram resultados contraditórios no sentido da utilização de métodos prescritivos e adaptativos. Este fato levou a reflexão de que a contribuição apresentada pelas práticas de gerenciamento de projetos para o desenvolvimento de produtos se dá com a verificação do cenário e o grau de inovação do projeto de produto que está sendo desenvolvido e com a utilização de metodologias adaptativas para projetos inovadores em ambientes complexos e metodologias prescritivas para projetos de concepção de rotina em ambientes simples.

  6. MODIFIED KACHUGIN METHOD OF ALTERNATIVE SOFTWARE-BASED PROJECTION OF THE PATTERN OF REORGANIZATION OF ABRASION SHORES OF WATER RESERVOIRS IN THE FLAT TERRAIN

    Directory of Open Access Journals (Sweden)

    Sobol' Il'ya Stanislavovich

    2012-10-01

    Full Text Available Presently, effective regulations employed in the Russian Federation recommend the use of the methods developed by E.G. Kachuchin, G.S. Zolotarev, I.A. Pecherkin, etc. for the projection of patterns of reorganization of coastlines of water reservoirs. One of these methods, developed by E.G. Kachugin, belongs to the group of power methods based on the hypothesis that the amplitudes of destruction of the coast are proportionate to the total wave energy alongside the coastline. The Kachugin method was reworked into a computer-based two-dimensional engineering model of reorganization of the abrasion shore. The model generates alternative projections. It simulates the processes of washout and accumulation of soil in the coastal area and solves the problem of predicting the potential profile of the shore within a pre-set time period or until the abrasion is smoothed away in the course of formation of coastal shallows. The model testing has proven its efficiency in solving the engineering problems of projecting the line of reservoir abrasion shores with a high degree of reliability.

  7. Effects of enamel abrasion, salivary pellicle, and measurement angle on the optical assessment of dental erosion

    Science.gov (United States)

    Lussi, Adrian; Bossen, Anke; Höschele, Christoph; Beyeler, Barbara; Megert, Brigitte; Meier, Christoph; Rakhmatullina, Ekaterina

    2012-09-01

    The present study assessed the effects of abrasion, salivary proteins, and measurement angle on the quantification of early dental erosion by the analysis of reflection intensities from enamel. Enamel from 184 caries-free human molars was used for in vitro erosion in citric acid (pH 3.6). Abrasion of the eroded enamel resulted in a 6% to 14% increase in the specular reflection intensity compared to only eroded enamel, and the reflection increase depended on the erosion degree. Nevertheless, monitoring of early erosion by reflection analysis was possible even in the abraded eroded teeth. The presence of the salivary pellicle induced up to 22% higher reflection intensities due to the smoothing of the eroded enamel by the adhered proteins. However, this measurement artifact could be significantly minimized (pmeasurement angles from 45 to 60 deg did not improve the sensitivity of the analysis at late erosion stages. The applicability of the method for monitoring the remineralization of eroded enamel remained unclear in a demineralization/remineralization cycling model of early dental erosion in vitro.

  8. POLITIZAÇÃO, AMBIENTALIZAÇÃO E DESENVOLVIMENTO TERRITORIAL EM RESERVAS EXTRATIVISTAS

    Directory of Open Access Journals (Sweden)

    Maria José da S. A. Teisserenc

    Full Text Available Esse artigo, resultante de pesquisas no contexto de duas Resex marinhas do estado do Pará, Mãe Grande do Curuçá e São João da Ponta, trata de mudanças que vêm ocorrendo no poder local, relacionadas à criação de áreas protegidas na Amazônia brasileira. Observa-se, então, uma politização dos desafios locais, manifesta como resultado do trabalho realizado nos Conselhos Deliberativos, nos quais a mobilização das comunidades e o engajamento de seus representantes possibilitam debates que dizem respeito ao desenvolvimento de seu território conforme exigências ambientais. Trata-se de uma dinâmica significativa de um desenvolvimento territorial que se beneficia de uma ambientalização geral gerada com a criação das Reservas e do valor deliberativo dos compromissos de membros conselheiros como uma instância política. Essa situação constitui interessante oportunidade de análise das relações entre práticas de democracia local de tipo deliberativo e uma orientação de desenvolvimento que inspira o engajamento dos atores locais em instituições novas, como os Conselhos Deliberativos.

  9. AGROECOLOGIA: UMA ALTERNATIVA DE DESENVOLVIMENTO RURAL SUSTENTÁVEL PARA OS ASSENTAMENTOS RURAIS

    Directory of Open Access Journals (Sweden)

    Nivea Massaretto Verges

    2013-03-01

    Full Text Available Atualmente, observa-se o aumento das discussões, dentro das dimensões acadêmica, econômica, política e social, em relação à agricultura do país e do mundo, dentre as discussões está a questão do desenvolvimento rural sustentável, que existe em documentos, porém está ausente na prática. Um exemplo da ausência do desenvolvimento rural sustentável pode ser encontrado nas famílias de produtores assentadas que, em meio a muitas pressões, acabam se rendendo ao capital, deixando de produzir e desenvolver em seus lotes. Diante disso, este trabalho buscou analisar as características dos assentamentos rurais do Pontal do Paranapanema, identificando seus potenciais e impasses a fim de apresentar as práticas agroecológicas como alternativa para o desenvolvimento rural sustentável dos assentamentos, destacando alguns esboços para um projeto a fim de proporcionar embasamento para que o processo de integração econômica e social dos assentados seja efetivado de forma autônoma pelos mesmos. Para a realização desse trabalho foi utilizado levantamentos bibliográficos e dados obtidos junto ao IBGE e DATALUTA.

  10. Desdobramento da qualidade no desenvolvimento de filmes flexíveis para embalagens

    Directory of Open Access Journals (Sweden)

    Miguel Paulo A. Cauchick

    2003-01-01

    Full Text Available Um dos métodos atuais importantes para o desenvolvimento de produtos é o QFD (Quality Function Deployment ou Desdobramento da Função Qualidade. O QFD consiste em um processo sistemático para traduzir a opinião do cliente em requisitos técnicos e operacionais, mostrando e documentando as informações na forma de matrizes. O método objetiva enfocar os itens mais importantes, proporcionando um mecanismo para alcançar vantagens competitivas no processo de desenvolvimento. Este trabalho destaca o conceito do QFD, citando uma aplicação em uma empresa que produz filmes flexíveis de polipropileno (BOPP. O trabalho apresenta alguns aspectos da introdução do método na empresa, apontando as dificuldades encontradas, resultados e benefícios decorrentes da implantação. Dentre os benefícios gerados, destacam-se a importância do papel do QFD como um método para sistematizar o processo de desenvolvimento, bem como outros benefícios para a equipe, tais como melhoria nas habilidades de planejamento, disseminação do conhecimento e melhoria de comunicação entre as áreas funcionais.

  11. Resistindo ao desenvolvimento neocolonial: a luta do povo de Andalgalá contra projetos megamineiros

    OpenAIRE

    Misoczky,Maria Ceci; Böhm,Steffen

    2013-01-01

    A América Latina vem experimentando uma nova era de declarada fé dos governos no mito do desenvolvimento, em articulação com a expansão de políticas extrativistas exportadoras em um contexto de renovada dependência. A face mais dramática do extrativismo na região tem sido a crescente presença de corporações mineiras transnacionais apoiadas por governos nacionais e regionais e por instituições internacionais financeiras e de apoio ao desenvolvimento, e intensamente resistidas por movimentos so...

  12. Administração endovenosa de antibióticos e resistência bacteriana : responsabilidade da enfermagem

    OpenAIRE

    Hoefel, Heloisa Helena Karnas; Lautert, Liana

    2006-01-01

    O sucesso da terapêutica com antibióticos e o desenvolvimento da resistência bacteriana dependem de diversos fatores, sendo que os relacionados ao cuidado de enfermagem são o seu preparo e a sua administração. Objetivo: realizar uma revisão da literatura sobre falhas na administração de antibióticos analisando sua possível influência na resistência bacteriana. Delineamento: realizada uma pesquisa bibliográfica das fontes do LILACS e Medline. Métodos: realizada revisão bibliográfica sistematiz...

  13. Avaliação do desenvolvimento cognitivo e afetivo-social de crianças com perda auditiva

    Directory of Open Access Journals (Sweden)

    Maria de Lourdes M. Tabaquim

    2013-12-01

    Full Text Available OBEJTIVO: avaliar o nível de desenvolvimento cognitivo e afetivo-social de crianças com diagnóstico de deficiência auditiva. MÉTODO: participaram do estudo 50 crianças com diagnóstico de deficiência auditiva, com idade média de 16,1 meses, de ambos os gêneros. Empregou-se a entrevista semi-estruturada com os pais para a obtenção da história de vida da criança, a Escala de Desenvolvimento Comportamental e a Escala de Avaliação da Reação de Retração do Bebê. RESULTADO: o estudo identificou 80% das crianças com perda auditiva profunda bilateral. O Quociente de Desenvolvimento na normalidade ocorreu em 76% da amostra, sendo as funções da linguagem e pessoal-social, as mais prejudicadas. Os níveis de ajustamento afetivo e interacional foram caracterizados pelas reações de alarme para problemas de interação pessoal-social. CONCLUSÃO: as competências defasadas de habilidades verbais e não-verbais mostraram implicações no desenvolvimento cognitivo, sugestivas da condição da criança com perda auditiva e dos fatores de risco associados, com limitação circunstancial a trocas comunicativas que promovem o desenvolvimento de competências adaptativas e o fortalecimento da auto-estima para as relações.

  14. EFECTO DEL CONTENIDO DE CARBONO SOBRE LA RESISTENCIA AL DESGASTE ABRASIVO DE RECUBRIMIENTOS DE CrC DEPOSITADOS POR PULVERIZACIÓN CATÓDICA MAGNETRÓN EFEITO DO CONTEÚDO DE CARBONO SOBRE A RESISTÊNCIA AO DESGASTE ABRASIVO DE RECOBRIMENTOS DE CrC DEPOSITADOS POR PULVERIZAÇÃO CATÓDICA MAGNETRÃO EFFECT OF THE CARBON CONTENT IN ABRASIVE WEAR RESISTANCE OF CrC COATINGS DEPOSITED BY MAGNETRON SPUTTERING

    Directory of Open Access Journals (Sweden)

    Maryory Astrid Gómez

    2012-12-01

    diamante. O volume das impressões de abrasão mediu-se com as imagens obtidas no microscópio interferométrico e ademais se corroborou com o cálculo do volume geométrico baseado em seções medidas com o perfilômetro. O comportamento ao desgaste abrasivo mostrou uma marcada dependência com o conteúdo de carbono. O desgaste abrasivo mais baixo obtevese para os recobrimentos com o mais alto conteúdo de carbono.Chromium carbide coatings on steel are a good candidate for applications on forming and molding dies. The high mechanical strength, chemical resistance and high temperature stability of Cr3C2 phase can be compatible with the severe abrasive wear and corrosion found in those manufacture operations. In this work chromium carbide coatings deposited by means of RF magnetron sputtering showed carbon contents between 25 % and 58 % by EDS analysis. Hardness values of these coatings were between 15 and 24 GPa, being the hardest values in the samples with carbon content in the 39-53 % range. The abrasive wear behavior of the coatings was evaluated by using a dimple grinder with diamond powder. The volume of the abrasion craters was measured from the images obtained with the interferometric microscope, and further corroborated by geometrical volume calculation based in profilometer sections that were measured. Abrasive wear behavior showed a marked dependence with carbon content. The lowest abrasive wear was obtained for the coatings with the highest carbon content.

  15. Surface integrity analysis of abrasive water jet-cut surfaces of friction stir welded joints

    Czech Academy of Sciences Publication Activity Database

    Kumar, R.; Chattopadhyaya, S.; Dixit, A. R.; Bora, B.; Zeleňák, Michal; Foldyna, Josef; Hloch, Sergej; Hlaváček, Petr; Ščučka, Jiří; Klich, Jiří; Sitek, Libor; Vilaca, P.

    2017-01-01

    Roč. 88, č. 5 (2017), s. 1687-1701 ISSN 0268-3768 R&D Projects: GA MŠk(CZ) LO1406; GA MŠk ED2.1.00/03.0082 Institutional support: RVO:68145535 Keywords : friction stir welding (FSW) * abrasive water jet (AWJ) * optical profilometer * topography * surface roughness Subject RIV: JQ - Machines ; Tools OBOR OECD: Mechanical engineering Impact factor: 2.209, year: 2016 http://link.springer.com/article/10.1007/s00170-016-8776-0

  16. Abrasive slurry jet cutting model based on fuzzy relations

    Science.gov (United States)

    Qiang, C. H.; Guo, C. W.

    2017-12-01

    The cutting process of pre-mixed abrasive slurry or suspension jet (ASJ) is a complex process affected by many factors, and there is a highly nonlinear relationship between the cutting parameters and cutting quality. In this paper, guided by fuzzy theory, the fuzzy cutting model of ASJ was developed. In the modeling of surface roughness, the upper surface roughness prediction model and the lower surface roughness prediction model were established respectively. The adaptive fuzzy inference system combines the learning mechanism of neural networks and the linguistic reasoning ability of the fuzzy system, membership functions, and fuzzy rules are obtained by adaptive adjustment. Therefore, the modeling process is fast and effective. In this paper, the ANFIS module of MATLAB fuzzy logic toolbox was used to establish the fuzzy cutting model of ASJ, which is found to be quite instrumental to ASJ cutting applications.

  17. Fatores prognósticos para o desenvolvimento cognitivo de prematuros de muito baixo peso

    Directory of Open Access Journals (Sweden)

    Maria Dalva Barbosa Baker Méio

    2003-06-01

    Full Text Available OBJETIVO: Crianças prematuras, de muito baixo peso, podem apresentar alterações em seu desenvolvimento cognitivo. No Brasil, pouco se conhece sobre a evolução dessas crianças na idade pré-escolar. O objetivo do estudo foi descrever o desenvolvimento cognitivo de uma população de recém-nascidos prematuros de muito baixo peso e verificar possíveis fatores prognósticos para desenvolvimento cognitivo anormal. MÉTODOS: Um estudo de coorte foi realizado com uma população de crianças pré-escolares, nascidas prematuras, de muito baixo peso, entre janeiro de 1991 e setembro de 1993. O desenvolvimento cognitivo foi avaliado por meio do teste WPPSI-R (Wechsler Preschool and Primary Intelligence Scales aplicado por psicólogas, utilizando dois pontos de corte para definição de anormalidade: escores abaixo de 1 e 2, desvios padrões da média (DP. RESULTADOS: Foram avaliadas 79 crianças de quatro a cinco anos de idade. A média do escore total do teste WIPPSI-R foi de 75,6 (±11,9. A incidência de escore total anormal foi de 77,2% e de 32,9% (1DP e 2 DP, respectivamente. Após o ajuste por "tipo de parto", ser pequeno para a idade gestacional (OR=6,19; IC95% 1,60-23,86, ultra-som transfontanela anormal (OR=5,90; IC95% 1,04-9,83 e ser do sexo masculino (OR=3,20; IC 95% 1,32-26,35 foram os fatores que predisseram escore total <70 (2 DP. CONCLUSÃO: Houve maior comprometimento do desenvolvimento cognitivo nas crianças estudadas do que o descrito na literatura. Ser pequeno para idade gestacional, ultra-som transfontanela anormal e sexo masculino foram fatores prognósticos de pior evolução.

  18. DESENVOLVIMENTO LOCAL E MANEJO DA CAATINGA NO ASSENTAMENTO HIPÓLITO, EM MOSSORÓ/RN

    Directory of Open Access Journals (Sweden)

    E. D. G. Pereira

    2007-12-01

    Full Text Available Nas últimas décadas tem havido uma preocupação muito grande com o tipo de desenvolvimento que vem sendo implementado pelos governos. A partir daí, criou-se a noção de desenvolvimento sustentável, o qual se baseia em um crescimento econômico que seja acompanhado por eqüidade social e prudência ecológica. Em muitos projetos de assentamentos têm sido desenvolvidos pesquisas com o objetivo de analisar como vem se processando tais experiências. Nossa investigação teve como meta verificar os impactos sócio-ambientais trazidos a partir do uso da caatinga no assentamento Hipólito, no município de Mossoró, no Oeste do RN. Preocupou-nos saber se naquele projeto de assentamento tem ocorrido um desenvolvimento local, baseado em critérios de sustentabilidade. A metodologia empregada foi a realização de entrevistas com 29 assentados, o que corresponde a 20% da população total do assentamento, além de leituras de outros trabalhos e artigos de jornais. O trabalho está em fase de conclusão, porém a partir de estudos de campo, realizados no mês de agosto de 2004, podemos apresentar os seguintes resultados: quanto ao aspecto sócio-econômico, os assentados têm na agricultura de sequeiro a atividade econômica principal; a produtividade é baixa e a renda é complementada com “bicos”, aposentadorias e/ou com o dinheiro advindo dos planos de assistência social do Governo Federal; a agricultura é realizada sem os devidos cuidados com o meio ambiente, e o desmatamento desordenado tem agravado ainda mais os problemas presentes no bioma caatinga, tais como salinização, a desertificação e o desaparecimento de espécies da fauna e da flora. Face ao exposto, podemos concluir que a realidade observada no assentamento aponta para a insustentabilidade sócio-econômica e ambiental naquela área. Palavras-chave: sustentabilidade; caatinga; assentamento; desenvolvimento rural; desenvolvimento local.

  19. Leucemia Mielóide Crônica: novas drogas em desenvolvimento

    Directory of Open Access Journals (Sweden)

    Cármino A. de Souza

    Full Text Available A LMC é um modelo de investigação biológica e clinica que deve ser seguido nesta nova fase da oncologia moderna. A resposta terapêutica ao uso do imatinibe como droga de primeira linha mudou os conceitos e paradigmas e criou uma expectativa que drogas mais potentes possam ser desenvolvidas no futuro. Infelizmente nem todos conseguem atingir essa situação ideal. Por esta razão, Baccarani M sugeriu que a falência de resposta subótima, precaução ou alerta fossem estudadas no sentido de serem desenvolvidas intervenções terapêuticas diferenciadas mais precoces. A resistência ao imatinibe existe e depende de vários mecanismos. Tanto mais tardia a introdução do imatinibe e mais avançada for a fase evolutiva da doença maior a freqüência de resistência. Do ponto de vista biológico, a superexpressão do BCR-ABL, os defeitos genéticos adicionais e as mutações que podem atingir várias regiões da molécula - a alça de fosfato, a alça de ativação, o domínio da quinase são os mais importantes fatores associados à resistência ao imatinibe. Por esta razão, são necessárias outras opções terapêuticas e hoje há o desenvolvimento de um grande número de drogas para um número maior de alvos. Inicialmente temos o dasatinibe, já aprovado nos EUA, na Europa e também no Brasil; o nilotinibe, em fase avançada de estudos clínicos (inclusive de fase III, e também já aprovado para uso nos EUA; o bosutinibe, o INNO - 406 bem como outras drogas que atuam em alvos como as aurora-quinases ou inibidores de histona-deacetilases.

  20. Study on wear resistance of vanadium alloying compacted/vermicular graphite cast iron

    International Nuclear Information System (INIS)

    Park, Yoon Woo

    1987-01-01

    Wear resistance of the Compacted/Vermicular graphite cast irons was studied by changing the vanadium content in the cast irons. The results obtained in this work are summarized as follows. 1. When the same amount of vanadium was added to the flake graphite cast iron, spheroidal graphitecast iron and Compacted/Vermicular graphite cast iron, spheroidal graphite cast iron and Compacted/Vermicular graphite cast iron wear resistance decreased in following sequence, that is, flake graphite cast iron> spheroidal graphite cast iron>Compacted/Vermicular graphite cast iron. 2. Addition of vanadium to the Compacted/Vermicular cast iron leaded to a remarkable increase in hardness because it made the amount of pearlite in matrix increase. 3. Addition of vanadium to the compacted/Vermicular graphite cast iron significantly enhanced wear resistance and the maximum resistance was achieved at about 0.36% vanadium. 4. The maximum amount of wear apppeared at sliding speed of about 1.4m/sec and wear mode was considered to be oxidation abrasion from the observation of wear tracks. (Author)