  1. TEM analysis of a friction stir-welded butt joint of Al-Si-Mg alloys

    International Nuclear Information System (INIS)

    Cabibbo, M.; Meccia, E.; Evangelista, E.

    2003-01-01

    The microstructure evolution of a joint of Al-Si-Mg alloys A6056-T4 and A6056-T6 has been characterized by transmission electron microscopy (TEM). Metallurgical investigations, hardness and mechanical tests were also performed to correlate the TEM investigations to the mechanical properties of the produced friction stir-welded butt joint. After friction stir-welding thermal treatment has been carried out at 530 deg. C followed by ageing at 160 deg. C (T6). The base material (T4) and the heat-treated one (T6) were put in comparison showing a remarkable ductility reduction of the joint after T6 treatment

  2. Structure-property investigations on a laser beam welded dissimilar joint of aluminium AA6056 and titanium Ti6Al4V for aeronautical applications. Part II: resistance to fatigue crack propagation and fracture

    Energy Technology Data Exchange (ETDEWEB)

    Horstmann, M.; Ventzke, V.; Petrovski, B.; Kocak, M. [GKSS Research Centre Geesthacht, Institute of Materials Research, Materials Mechanics, Geesthacht (Germany); Kocik, R.; Tempus, G. [AIRBUS Deutschland GmbH, Metal Technology, Bremen (Germany); Vaidya, W.V.

    2009-10-15

    Investigations were continued on the dissimilar laser beam welds of AA6056 and Ti6Al4V, fabricated by inserting Ti-sheet into the profiled Al-sheet and melting AA6056 alone. By using microstructure, hardness and strength as the criteria, sites exhibiting non-uniform microstructure and localized plastic deformation due to strength mismatch were investigated in two orientations: crack parallel to the weld and crack perpendicular to the weld for fatigue crack propagation and fracture toughness at room temperature. Effect of temper of AA6056 on these properties was studied for two conditions; welding in T4 followed by post weld heat treatment T6, and welding in T6 and naturally aged for a defined period. The orientation ''crack parallel to the weld'' was investigated in 3 locations on the side of AA6056: the interface and the two changeovers on the Al-side. Firstly, between the fusion zone and the heat affected zone (3 mm from the interface) and secondly, between (primary) heat affected zone and towards the base material (7 mm from the interface). Although brittle intermetallic TiAl{sub 3} had been formed at the interface, uncontrolled separation or debonding at the interface was not observed. Insofar the bond quality of the weld was good. However, the ranking of interface was the lowest since fatigue crack propagation was relatively faster than that in the fusion zone and heat affected zone, and fracture toughness was low. Therefore, unstable fatigue crack propagation is observed when the crack propagates perpendicular to the weld from AA6056 towards Ti6Al4V. The results have shown that the dissimilar joints exhibit improved performance when laser beam welded in the T6 condition. (Abstract Copyright [2009], Wiley Periodicals, Inc.) [German] Teil II: Widerstand gegen Ermuedungsrissausbreitung und Bruch Die Untersuchungen an der laserstrahlgeschweissten Mischverbindung aus AA6056 und Ti6Al4V wurden fortgesetzt. Fuer die Ermuedungsrissausbreitungs

  3. Structure-property investigations on a laser beam welded dissimilar joint of aluminium AA6056 and titanium Ti6Al4V for aeronautical applications Part I: Local gradients in microstructure, hardness and strength

    Energy Technology Data Exchange (ETDEWEB)

    Horstmann, M.; Ventzke, V.; Petrovski, B.; Kocak, M. [GKSS Research Centre Geesthacht (Germany). Institute of Materials Research, Materials Mechanics; Kocik, R.; Tempus, G. [AIRBUS Deutschland GmbH, Metal Technology, Bremen (Germany); Vaidya, W.V.

    2009-08-15

    Sheets of AA6056 and Ti6Al4V were butt-joined by inserting the Ti-sheet into the profiled Al-sheet and by melting the Al-alloy alone using a split beam Nd:YAG laser. To study microstructural effects on properties, the Al-alloy was used in two tempers; T4 followed by post weld heat treatment T6, and in T6 followed by a defined duration of natural ageing at room temperature. As a basic step for fatigue and fracture investigations, local gradients in properties of this dissimilar joint are investigated using microscopy, hardness and tensile tests. Possible sites, from which fracture may initiate, have been then identified. All property changes are found to confine to the aluminium side. An intermetallic layer, although very thin, is found to form on the interface. The changeovers, firstly between the fusion zone and the heat affected zone and secondly between the heat affected zone and the base material, are found to be associated with changes in microstructure, hardness and strength. These are identified as the possible critical sites in addition to the interface. (Abstract Copyright [2009], Wiley Periodicals, Inc.) [German] Durch eine spezielle Stossvorbereitung wurden laserstrahlgeschweisster Mischverbindungen aus den Blechwerkstoffen AA6056 und Ti6Al4V hergestellt und zwar ohne die Verwendung von Zusatzwerkstoffen. Die grosse Differenz der Schmelztemperaturen erlaubt das selektive Erschmelzen des Aluminiumwerkstoffs, der wieder um den Titanwerkstoff benetzt, sodass es zur Ausbildung einer mechanisch-stabilen und tragfaehigen Verbindung kommt. Die Al-Legierung wurde in den Waermebehandlungszustaenden T4 und T6 verschweisst, um den mikrostrukturellen Einfluss auf die Eigenschaften der Verbindungen untersuchen zu koennen. Die Prozessfolgen sahen vor, dass beim Schweissen im Zustand T4 eine Warmauslagerung, beim Schweissen im Zustand T6 eine Kaltauslagerung definierter Dauer folgte. Die Charakterisierung lokaler Eigenschaftsgradienten hinsichtlich Gefuege, Mikrohaerte

  4. Integrated FEM-DBEM simulation of crack propagation in AA2024-T3 FSW butt joints considering manufacturing effects

    DEFF Research Database (Denmark)

    Sonne, Mads Rostgaard; Carlone, P.; Citarella, R.

    2015-01-01

    This paper deals with a numerical and experimental investigation on the influence of residual stresses on fatigue crack growth in AA2024-T3 friction stir welded butt joints. An integrated FEM-DBEM procedure for the simulation of crack propagation is proposed and discussed. A numerical FEM model...... of the welding process of precipitation hardenable AA2024-T3 aluminum alloy is employed to infer the process induced residual stress field. The reliability of the FEM simulations with respect to the induced residual stresses is assessed comparing numerical outcomes with experimental data obtained by means...

  5. Influences of post weld heat treatment on tensile strength and microstructure characteristics of friction stir welded butt joints of AA2014-T6 aluminum alloy

    Science.gov (United States)

    Rajendran, C.; Srinivasan, K.; Balasubramanian, V.; Balaji, H.; Selvaraj, P.

    2016-08-01

    Friction stir welded (FSWed) joints of aluminum alloys exhibited a hardness drop in both the advancing side (AS) and retreating side (RS) of the thermo-mechanically affected zone (TMAZ) due to the thermal cycle involved in the FSW process. In this investigation, an attempt has been made to overcome this problem by post weld heat treatment (PWHT) methods. FSW butt (FSWB) joints of Al-Cu (AA2014-T6) alloy were PWHT by two methods such as simple artificial aging (AA) and solution treatment followed by artificial aging (STA). Of these two treatments, STA was found to be more beneficial than the simple aging treatment to improve the tensile properties of the FSW joints of AA2014 aluminum alloy.

  6. Modelling and Pareto optimization of mechanical properties of friction stir welded AA7075/AA5083 butt joints using neural network and particle swarm algorithm

    International Nuclear Information System (INIS)

    Shojaeefard, Mohammad Hasan; Behnagh, Reza Abdi; Akbari, Mostafa; Givi, Mohammad Kazem Besharati; Farhani, Foad

    2013-01-01

    Highlights: ► Defect-free friction stir welds have been produced for AA5083-O/AA7075-O. ► Back-propagation was sufficient for predicting hardness and tensile strength. ► A hybrid multi-objective algorithm is proposed to deal with this MOP. ► Multi-objective particle swarm optimization was used to find the Pareto solutions. ► TOPSIS is used to rank the given alternatives of the Pareto solutions. -- Abstract: Friction Stir Welding (FSW) has been successfully used to weld similar and dissimilar cast and wrought aluminium alloys, especially for aircraft aluminium alloys, that generally present with low weldability by the traditional fusion welding process. This paper focuses on the microstructural and mechanical properties of the Friction Stir Welding (FSW) of AA7075-O to AA5083-O aluminium alloys. Weld microstructures, hardness and tensile properties were evaluated in as-welded condition. Tensile tests indicated that mechanical properties of the joint were better than in the base metals. An Artificial Neural Network (ANN) model was developed to simulate the correlation between the Friction Stir Welding parameters and mechanical properties. Performance of the ANN model was excellent and the model was employed to predict the ultimate tensile strength and hardness of butt joint of AA7075–AA5083 as functions of weld and rotational speeds. The multi-objective particle swarm optimization was used to obtain the Pareto-optimal set. Finally, the Technique for Order Preference by Similarity to the Ideal Solution (TOPSIS) was applied to determine the best compromised solution.

  7. Experimental investigation of hardness of FSW and TIG joints of Aluminium alloys of AA7075 and AA6061

    Directory of Open Access Journals (Sweden)

    Chetan Patil

    2016-07-01

    Full Text Available This paper reports hardness testing conducted on welded butt joints by FSW and TIG welding process on similar and dissimilar aluminium alloys. FSW joints were produced for similar alloys of AA7075T651 and dissimilar alloys of AA7075T651- AA6061T6. The Friction stir welds of AA7075 & AA6061 aluminium alloy were produced at different tool rotational speeds of 650,700, 800, 900, 1000 and transverse speed of 30, 35, 40 mm/min. TIG welding was conducted along the rolling direction of similar and dissimilar aluminium plates. The Brinell hardness testing techniques were employed to conduct the tests; these tests were conducted on the welds to ascertain the joint integrity before characterization to have an idea of the quality of the welds

  8. Prediction of the Vickers Microhardness and Ultimate Tensile Strength of AA5754 H111 Friction Stir Welding Butt Joints Using Artificial Neural Network.

    Science.gov (United States)

    De Filippis, Luigi Alberto Ciro; Serio, Livia Maria; Facchini, Francesco; Mummolo, Giovanni; Ludovico, Antonio Domenico

    2016-11-10

    A simulation model was developed for the monitoring, controlling and optimization of the Friction Stir Welding (FSW) process. This approach, using the FSW technique, allows identifying the correlation between the process parameters (input variable) and the mechanical properties (output responses) of the welded AA5754 H111 aluminum plates. The optimization of technological parameters is a basic requirement for increasing the seam quality, since it promotes a stable and defect-free process. Both the tool rotation and the travel speed, the position of the samples extracted from the weld bead and the thermal data, detected with thermographic techniques for on-line control of the joints, were varied to build the experimental plans. The quality of joints was evaluated through destructive and non-destructive tests (visual tests, macro graphic analysis, tensile tests, indentation Vickers hardness tests and t thermographic controls). The simulation model was based on the adoption of the Artificial Neural Networks (ANNs) characterized by back-propagation learning algorithm with different types of architecture, which were able to predict with good reliability the FSW process parameters for the welding of the AA5754 H111 aluminum plates in Butt-Joint configuration.

  9. Prediction of the Vickers Microhardness and Ultimate Tensile Strength of AA5754 H111 Friction Stir Welding Butt Joints Using Artificial Neural Network

    Directory of Open Access Journals (Sweden)

    Luigi Alberto Ciro De Filippis

    2016-11-01

    Full Text Available A simulation model was developed for the monitoring, controlling and optimization of the Friction Stir Welding (FSW process. This approach, using the FSW technique, allows identifying the correlation between the process parameters (input variable and the mechanical properties (output responses of the welded AA5754 H111 aluminum plates. The optimization of technological parameters is a basic requirement for increasing the seam quality, since it promotes a stable and defect-free process. Both the tool rotation and the travel speed, the position of the samples extracted from the weld bead and the thermal data, detected with thermographic techniques for on-line control of the joints, were varied to build the experimental plans. The quality of joints was evaluated through destructive and non-destructive tests (visual tests, macro graphic analysis, tensile tests, indentation Vickers hardness tests and t thermographic controls. The simulation model was based on the adoption of the Artificial Neural Networks (ANNs characterized by back-propagation learning algorithm with different types of architecture, which were able to predict with good reliability the FSW process parameters for the welding of the AA5754 H111 aluminum plates in Butt-Joint configuration.

  10. Finite element analysis of metallurgical phase transformations in AA 6056-T4 and their effects upon the residual stress and distortion states of a laser welded T-joint

    International Nuclear Information System (INIS)

    Zain-ul-abdein, Muhammad; Nelias, Daniel; Jullien, Jean-Francois; Boitout, Frederic; Dischert, Luc; Noe, Xavier

    2011-01-01

    Aircraft industry makes extensive use of aluminium alloy AA 6056-T4 in the fabrication of fuselage panels using laser beam welding technique. Since high temperatures are involved in the manufacturing process, the precipitation/dissolution occurrences are expected as solid state phase transformations. These transformations are likely to affect the residual distortion and stress states of the component. The present work investigates the effect of metallurgical phase transformations upon the residual stresses and distortions induced by laser beam welding in a T-joint configuration using the finite element method. Two separate models were studied using different finite element codes, where the first one describes a thermo-mechanical analysis using Abaqus; while the second one discusses a thermo-metallo-mechanical analysis using Sysweld. A comparative analysis of experimentally validated finite element models has been performed and the residual stress states with and without the metallurgical phase transformations are predicted. The results show that the inclusion of phase transformations has a negligible effect on predicted distortions, which are in agreement with the experimental data, but an effect on predicted residual stresses, although the experimentally measured residual stresses are not available to support the analyses.

  11. Experimental investigation and finite element simulation of laser beam welding induced residual stresses and distortions in thin sheets of AA 6056-T4

    International Nuclear Information System (INIS)

    Zain-ul-abdein, Muhammad; Nelias, Daniel; Jullien, Jean-Francois; Deloison, Dominique

    2010-01-01

    Laser beam welding has recently found its application in the fabrication of aircraft structures where fuselage panels, made of thin sheets of AA 6056-T4 (an aluminium alloy), are welded with stiffeners of the same material in a T-joint configuration. The present work simulates laser beam welding induced residual stresses and distortions using industrially employed thermal and mechanical boundary conditions. Various measurements performed on small-scale welded test specimens provide a database of experimental results that serves as a benchmark for qualification of the simulation results. The welding simulation is performed with the commercial finite element software Abaqus and a Fortran programme encoding a conical heat source with Gaussian volumetric distribution of flux. A sequentially coupled temperature-displacement analysis is undertaken to simulate the weld pool geometry, transient temperature and displacement fields. The material is assumed to follow an elasto-plastic law with isotropic hardening behaviour (von Mises plasticity model). A comparison between the experimental and simulation results shows a good agreement. Finally, the residual stress and strain states in a T-joint are predicted.

  12. Optimization of GMAW process of AA 6063-T5 aluminum alloy butt joints based on the response surface methodology and on the bead geometry

    International Nuclear Information System (INIS)

    Miguel, V.; Martinez-Conesa, E. J.; Segura, F.; Manjabacas, M. C.; Abellan, E.

    2012-01-01

    The geometry of the weld beads is characterized by the overhead, the width and the penetration. These values are indices of the behavior of the welded joint and therefore, they can be considered as factors that control the process. This work is performed to optimize the GMAW process of the aluminum alloy AA 6063-T5 by means of the response surface methodology (RSM). The variables herein considered are the arc voltage, the welding speed, the wire feed speed and the separation between surfaces in butt joints. The response functions that are herein studied are the overhead, the width, the penetration and the angle of the bead. The obtained results by RSM show high grade of agreement with the experimental values. The procedure is experimentally validated by welding for the theoretically obtained optimized technological conditions and a wide agreement between theoretical and experimental values is found. (Author) 16 refs.

  13. A study of fatigue life distribution of butt-welded joints

    International Nuclear Information System (INIS)

    Sakai, Tatsuo; Fujitani, Keizo; Kikuchi, Toshiro; Tanaka, Takao.

    1981-01-01

    Various kinds of welded joints are being used in many structures such as ships, bridges and constructions. It is important in reliability analysis of such structures to clarify the statistical fatigue property of the welded joints. In this study, fatigue tests were carried out on the butt-welded joints of SM50A steel and a theoretical interpretation on the fatigue life distribution was attempted, assuming that a butt-welded joint is composed of a number of sliced specimens with different fatigue strengths. Main results obtained are summarized as follows; (1) The median crack initiation life of the butt-welded joint specimens coincided with that of the sliced specimens, when the crack initiation was defined by a 0.2 mm crack in the sliced specimens or the equivalent state of stress intensity factor in the joint specimens. (2) The distribution of crack initiation lives of the butt-welded joints can be theoretically derived by combining the concept of extreme distribution and the distribution model on the number of fatigue cracks. The theoretical distribution of crack initiation lives of the joints is in good agreement with the general trend of the experimental results. (3) If the distribution of crack initiation lives and the crack growth law are given experimentally, one can obtain analytically the distribution of final fatigue lives. The fatigue life distribution of the sliced specimens can be explained by the theory established in this study. (author)

  14. Tool material effect on the friction stir butt welding of AA2124-T4 Alloy Matrix MMC

    Directory of Open Access Journals (Sweden)

    Yahya Bozkurt

    2018-01-01

    Full Text Available The purpose of the present work is to study on the effect of material properties tool on friction stir butt welding of AA2124-T4 alloy matrix MMC. Uncoated tool, coated tool with a CrN, and coated tool with AlTiN were used to weld aluminum MMC plates. Macrostructure and microstructure observations, ultimate tensile strength, wear resistance, and chemical analysis were carried out to determine the appropriate tool for joining these composite plates. Results showed that the good welded joints could be obtained when a tool is coated with AlTiN.

  15. Aluminum 6060-T6 friction stir welded butt joints: fatigue resistance with different tools and feed rates

    International Nuclear Information System (INIS)

    Baragetti, S.; D'Urso, G.

    2014-01-01

    The fatigue behavior of AA6060-T6 friction stir welded butt joints was investigated. The joints were produced by using both a standard and a threaded tri-flute cylindrical-tool with flat shoulder. The friction stir welding process was carried out using different feed rates. Preliminary tensile tests, micrograph analyses and hardness profile measurements across the welds were carried out. Welded and unwelded fatigue samples were tested under axial loading (R = 0.1) with upper limits of 10 4 and 10 5 cycles, using threaded and unthreaded (standard) tools at different feed rates. The best tensile and fatigue performance was obtained using the standard tool at low feed rate.

  16. Numerical estimation of temperature field in a laser welded butt joint made of dissimilar materials

    Directory of Open Access Journals (Sweden)

    Saternus Zbigniew

    2018-01-01

    Full Text Available The paper concerns numerical analysis of thermal phenomena occurring in the butt welding of two different materials by a laser beam welding. The temperature distribution for the welded butt-joint is obtained on the basis of numerical simulations performed in the ABAQUS program. Numerical analysis takes into account the thermophysical properties of welded plate made of two different materials. Temperature distribution in analysed joints is obtained on the basis of numerical simulation in Abaqus/Standard solver, which allowed the determination of the geometry of laser welded butt-joint.

  17. Microstructure and mechanical performance of autogenously fibre laser beam welded Ti-6242 butt joints

    Energy Technology Data Exchange (ETDEWEB)

    Kashaev, Nikolai, E-mail: nikolai.kashaev@hzg.de; Pugachev, Dmitry; Ventzke, Volker; Fomin, Fedor; Burkhardt, Irmela; Enz, Josephin; Riekehr, Stefan

    2017-05-10

    This work deals with the effects of laser beam power, focus position and advance speed on the geometry, microstructure and mechanical properties such as the tensile strength and microhardness of autogenously fibre laser beam welded Ti-6Al-2Sn-4Zr-2Mo (denoted as Ti-6242) butt joints used for high temperature applications. The Ti-6242 sheet employed here is characterized by a globular (α+β) microstructure. Laser beam welded butt joints consisted of a martensitic fusion zone, inhomogeneous heat affected zones and equiaxed base materials. The microhardness increased from 330 HV 0.3 in base material to 430 HV 0.3 in fusion zone due to the martensitic transformation. Butt joints showed the base material level of strength in tensile test. The local increase in microhardness provided a shielding effect that protected the Ti-6242 butt joint against mechanical damage during the static tensile load test. The predicted critical total underfill depth that does not reduce the tensile strength of the weld was determined to be 25% of the specimen thickness. - Highlights: • Autogenous fibre LBW of Ti-6242 was successfully achieved. • Butt joints showed low levels of porosity and an appropriate seam geometry. • Base material level of strength achieved for tensile strength. • Predicted critical underfill depth is 25% of the specimen thickness.

  18. Vision and spectroscopic sensing for joint tracing in narrow gap laser butt welding

    Science.gov (United States)

    Nilsen, Morgan; Sikström, Fredrik; Christiansson, Anna-Karin; Ancona, Antonio

    2017-11-01

    The automated laser beam butt welding process is sensitive to positioning the laser beam with respect to the joint because a small offset may result in detrimental lack of sidewall fusion. This problem is even more pronounced in case of narrow gap butt welding, where most of the commercial automatic joint tracing systems fail to detect the exact position and size of the gap. In this work, a dual vision and spectroscopic sensing approach is proposed to trace narrow gap butt joints during laser welding. The system consists of a camera with suitable illumination and matched optical filters and a fast miniature spectrometer. An image processing algorithm of the camera recordings has been developed in order to estimate the laser spot position relative to the joint position. The spectral emissions from the laser induced plasma plume have been acquired by the spectrometer, and based on the measurements of the intensities of selected lines of the spectrum, the electron temperature signal has been calculated and correlated to variations of process conditions. The individual performances of these two systems have been experimentally investigated and evaluated offline by data from several welding experiments, where artificial abrupt as well as gradual deviations of the laser beam out of the joint were produced. Results indicate that a combination of the information provided by the vision and spectroscopic systems is beneficial for development of a hybrid sensing system for joint tracing.

  19. A Semi-analytical model for creep life prediction of butt-welded joints in cylindrical vessels

    International Nuclear Information System (INIS)

    Zarrabi, K.

    2001-01-01

    There have been many investigations on the life assessment of high temperature weldments used in cylindrical pressure vessels, pipes and tubes over the last two decades or so. But to the author's knowledge, currently, there exists no practical, economical and relatively accurate model for creep life assessment of butt-welded joints in cylindrical pressure vessels. This paper describes a semi-analytical and economical model for creep life assessment of butt-welded joints. The first stage of the development of the model is described where the model takes into account the material discontinuities at the welded joint only. The development of the model to include other factors such as geometrical stress concentrations, residual stresses, etc will be reported separately. It has been shown that the proposed model can estimate the redistributions of stresses in the weld and Haz with an error of less than 4%. It has also been shown that the proposed model can conservatively predict the creep life of a butt-welded joint with an error of less than 16%

  20. A Neural Network Approach for GMA Butt Joint Welding

    DEFF Research Database (Denmark)

    Christensen, Kim Hardam; Sørensen, Torben

    2003-01-01

    This paper describes the application of the neural network technology for gas metal arc welding (GMAW) control. A system has been developed for modeling and online adjustment of welding parameters, appropriate to guarantee a certain degree of quality in the field of butt joint welding with full...... penetration, when the gap width is varying during the welding process. The process modeling to facilitate the mapping from joint geometry and reference weld quality to significant welding parameters has been based on a multi-layer feed-forward network. The Levenberg-Marquardt algorithm for non-linear least...

  1. A Neural Network Approach for GMA Butt Joint Welding

    DEFF Research Database (Denmark)

    Christensen, Kim Hardam; Sørensen, Torben

    2003-01-01

    penetration, when the gap width is varying during the welding process. The process modeling to facilitate the mapping from joint geometry and reference weld quality to significant welding parameters has been based on a multi-layer feed-forward network. The Levenberg-Marquardt algorithm for non-linear least......This paper describes the application of the neural network technology for gas metal arc welding (GMAW) control. A system has been developed for modeling and online adjustment of welding parameters, appropriate to guarantee a certain degree of quality in the field of butt joint welding with full...

  2. Optimization and Prediction of Angular Distortion and Weldment Characteristics of TIG Square Butt Joints

    Science.gov (United States)

    Narang, H. K.; Mahapatra, M. M.; Jha, P. K.; Biswas, P.

    2014-05-01

    Autogenous arc welds with minimum upper weld bead depression and lower weld bead bulging are desired as such welds do not require a second welding pass for filling up the upper bead depressions (UBDs) and characterized with minimum angular distortion. The present paper describes optimization and prediction of angular distortion and weldment characteristics such as upper weld bead depression and lower weld bead bulging of TIG-welded structural steel square butt joints. Full factorial design of experiment was utilized for selecting the combinations of welding process parameter to produce the square butts. A mathematical model was developed to establish the relationship between TIG welding process parameters and responses such as upper bead width, lower bead width, UBD, lower bead height (bulging), weld cross-sectional area, and angular distortions. The optimal welding condition to minimize UBD and lower bead bulging of the TIG butt joints was identified.

  3. A Vision-Aided 3D Path Teaching Method before Narrow Butt Joint Welding.

    Science.gov (United States)

    Zeng, Jinle; Chang, Baohua; Du, Dong; Peng, Guodong; Chang, Shuhe; Hong, Yuxiang; Wang, Li; Shan, Jiguo

    2017-05-11

    For better welding quality, accurate path teaching for actuators must be achieved before welding. Due to machining errors, assembly errors, deformations, etc., the actual groove position may be different from the predetermined path. Therefore, it is significant to recognize the actual groove position using machine vision methods and perform an accurate path teaching process. However, during the teaching process of a narrow butt joint, the existing machine vision methods may fail because of poor adaptability, low resolution, and lack of 3D information. This paper proposes a 3D path teaching method for narrow butt joint welding. This method obtains two kinds of visual information nearly at the same time, namely 2D pixel coordinates of the groove in uniform lighting condition and 3D point cloud data of the workpiece surface in cross-line laser lighting condition. The 3D position and pose between the welding torch and groove can be calculated after information fusion. The image resolution can reach 12.5 μm. Experiments are carried out at an actuator speed of 2300 mm/min and groove width of less than 0.1 mm. The results show that this method is suitable for groove recognition before narrow butt joint welding and can be applied in path teaching fields of 3D complex components.

  4. Influence of friction stir welding process and tool parameters on strength properties of AA7075-T6 aluminium alloy joints

    International Nuclear Information System (INIS)

    Rajakumar, S.; Muralidharan, C.; Balasubramanian, V.

    2011-01-01

    The aircraft aluminium alloys generally present low weldability by traditional fusion welding process. The development of the friction stir welding has provided an alternative improved way of satisfactorily producing aluminium joints, in a faster and reliable manner. In this present work, the influence of process and tool parameters on tensile strength properties of AA7075-T 6 joints produced by friction stir welding was analysed. Square butt joints were fabricated by varying process parameters and tool parameters. Strength properties of the joints were evaluated and correlated with the microstructure, microhardness of weld nugget. From this investigation it is found that the joint fabricated at a tool rotational speed of 1400 rpm, welding speed of 60 mm/min, axial force of 8 kN, using the tool with 15 mm shoulder diameter, 5 mm pin diameter, 45 HRc tool hardness yielded higher strength properties compared to other joints.

  5. Optimization of GMAW process of AA 6063-T5 aluminum alloy butt joints based on the response surface methodology and on the bead geometry; Optimizacion del proceso de soldadura GMAW de uniones a tope de la aleacion AA 6063-T5 basada en la metodologia de superficie de respuesta y en la geometria del cordon de soldadura

    Energy Technology Data Exchange (ETDEWEB)

    Miguel, V.; Martinez-Conesa, E. J.; Segura, F.; Manjabacas, M. C.; Abellan, E.

    2012-11-01

    The geometry of the weld beads is characterized by the overhead, the width and the penetration. These values are indices of the behavior of the welded joint and therefore, they can be considered as factors that control the process. This work is performed to optimize the GMAW process of the aluminum alloy AA 6063-T5 by means of the response surface methodology (RSM). The variables herein considered are the arc voltage, the welding speed, the wire feed speed and the separation between surfaces in butt joints. The response functions that are herein studied are the overhead, the width, the penetration and the angle of the bead. The obtained results by RSM show high grade of agreement with the experimental values. The procedure is experimentally validated by welding for the theoretically obtained optimized technological conditions and a wide agreement between theoretical and experimental values is found. (Author) 16 refs.

  6. Assessment of NDE Methods on Inspection of HDPE Butt Fusion Piping Joints for Lack of Fusion with Validation from Mechanical Testing

    International Nuclear Information System (INIS)

    Anderson, Michael T.; Cinson, Anthony D.; Crawford, Susan L.; Doctor, Steven R.; Moran, Traci L.; Watts, Michael W.

    2010-01-01

    Studies at the Pacific Northwest National Laboratory (PNNL) in Richland, Washington, are being conducted to evaluate nondestructive examinations (NDE) coupled with mechanical testing of butt fusion joints in high-density polyethylene (HDPE) pipe for assessing lack of fusion. The work provides information to the U.S. Nuclear Regulatory Commission (NRC) on the effectiveness of volumetric inspection techniques of HDPE butt fusion joints in Section III, Division 1, Class 3, buried piping systems in nuclear power plants. This paper describes results from preliminary assessments using ultrasonic and microwave nondestructive techniques and mechanical testing with the high-speed tensile impact test and the side-bend test for determining joint integrity. A series of butt joints were fabricated in 3408, 12-in. IPS DR-11 HDPE material by varying the fusion parameters to create good joints and joints containing a range of lack-of-fusion conditions. Six of these butt joints were volumetrically examined with time-of-flight diffraction (TOFD), phased-array (PA) ultrasound, and the Evisive microwave system. The outer-diameter weld beads were removed for the microwave inspection. In two of the four pipes, both the outer and inner weld beads were removed and the pipe joints re-evaluated. The pipes were sectioned and the joints destructively evaluated with the side-bend test by cutting portions of the fusion joint into slices that were planed and bent. The last step in this limited study will be to correlate the fusion parameters, nondestructive, and destructive evaluation results to validate the effectiveness of what each NDE technology detects and what each does not detect. The results of the correlation will be used in identifying any future work that is needed.

  7. A Study on the compensation margin on butt welding joint of Large Steel plates during Shipbuilding construction

    International Nuclear Information System (INIS)

    Kim, J; Jeong, K; Chung, H; Jeong, H; Ji, M; Yun, C; Lee, J

    2015-01-01

    This paper examines the characteristics of butt welding joint shrinkage for shipbuilding and marine structures main plate. The shrinkage strain of butt welding joint which is caused by the process of heat input and cooling, results in the difference between dimensions of the actual parent metal and the dimensions of design. This, in turn, leads to poor quality in the production of ship blocks and reworking through period of correction brings about impediment on improvement of productivity. Through experiments on butt welding joint's shrinkage strain on large structures main plate, the deformation of welding residual stress in the form of I, Y, V was obtained. In addition, the results of experiments indicate that there is limited range of shrinkage in the range of 1 ∼ 2 mm in 11t ∼ 21.5t thickness and the effect of heat transfer of weld appears to be limited within 1000 mm based on one side of seam line so there was limited impact of weight of parent metal on the shrinkage. Finally, it has been learned that Shrinkage margin needs to be applied differently based on groove phenomenon in the design phase in order to minimize shrinkage. (paper)

  8. T6 and T78 tempers of AA6065 alloy: a quantitative TEM study

    Energy Technology Data Exchange (ETDEWEB)

    Tanaka, M.; Warner, T. [Compagnie de Produits Chimiques et Electrometallurgiques Pechiney, Centre de Recherches de Voreppe, 38 (France)

    2000-07-01

    Quantitative transmission electron microscopy is used to characterize the microstructure of an industrial Al-Mg-Si-Cu alloy (AA6056) in a state (T78 temper) desensitized to intergranular corrosion in comparison with the peak aged state (T6 temper). Analysis of dark-field images and of zero-loss filtered selected-area-diffraction patterns, along with EDX spectroscopy, indicates an advanced precipitation of the quaternary phase containing Si and Cu in the T78-tempered alloy compared to the T6 one. This supports the current theory of the desensitization of AA6056 alloy. However, the application of EDX analysis to provide direct evidence of the chemical composition variation in the solid solution across the grain boundary appears less satisfactory. (orig.)

  9. The microstructure of aluminum A5083 butt joint by friction stir welding

    International Nuclear Information System (INIS)

    Jasri, M. A. H. M.; Afendi, M.; Ismail, A.; Ishak, M.

    2015-01-01

    This study presents the microstructure of the aluminum A5083 butt joint surface after it has been joined by friction stir welding (FSW) process. The FSW process is a unique welding method because it will not change the chemical properties of the welded metals. In this study, MILKO 37 milling machine was modified to run FSW process on 4 mm plate of aluminum A5083 butt joint. For the experiment, variables of travel speed and tool rotational speed based on capability of machine were used to run FSW process. The concentrated heat from the tool to the aluminum plate changes the plate form from solid to plastic state. Two aluminum plates is merged to become one plate during plastic state and return to solid when concentrated heat is gradually further away. After that, the surface and cross section of the welded aluminum were investigated with a microscope by 400 x multiplication zoom. The welding defect in the FSW aluminum was identified. Then, the result was compared to the American Welding Society (AWS) FSW standard to decide whether the plate can be accepted or rejected

  10. The microstructure of aluminum A5083 butt joint by friction stir welding

    Energy Technology Data Exchange (ETDEWEB)

    Jasri, M. A. H. M.; Afendi, M. [School of Mechatronic Engineering, Universiti Malaysia Perlis, Pauh, 02600, Arau, Perlis (Malaysia); Ismail, A. [UniKL MIMET, JalanPantaiRemis, 32200, Lumut, Perak (Malaysia); Ishak, M. [Faculty of Mechanical Engineering, Universiti Malaysia Pahang, 02600, Pekan, Pahang (Malaysia)

    2015-05-15

    This study presents the microstructure of the aluminum A5083 butt joint surface after it has been joined by friction stir welding (FSW) process. The FSW process is a unique welding method because it will not change the chemical properties of the welded metals. In this study, MILKO 37 milling machine was modified to run FSW process on 4 mm plate of aluminum A5083 butt joint. For the experiment, variables of travel speed and tool rotational speed based on capability of machine were used to run FSW process. The concentrated heat from the tool to the aluminum plate changes the plate form from solid to plastic state. Two aluminum plates is merged to become one plate during plastic state and return to solid when concentrated heat is gradually further away. After that, the surface and cross section of the welded aluminum were investigated with a microscope by 400 x multiplication zoom. The welding defect in the FSW aluminum was identified. Then, the result was compared to the American Welding Society (AWS) FSW standard to decide whether the plate can be accepted or rejected.

  11. Tensile Properties of Friction Stir Welded Joints of AA 2024-T6 Alloy at Different Welding Speeds

    Science.gov (United States)

    Avula, Dhananjayulu; Devuri, Venkateswarlu; Cheepu, Muralimohan; Dwivedi, Dheerendra Kumar

    2018-03-01

    The influence of welding speed on the friction stir welded joint properties of hardness, tensile properties, defects and microstructure characterization are studied in the present study. The friction stir welding was conducted on AA2014-T6 heat treated alloy with 5 mm thickness plate in butt joint configuration. The welding speed was varied from 8 mm/min to 120 mm/min at the fixed travel speed and load conditions. It is observed that the welding speeds at higher rate with wide range can be possible to weld this alloy at higher rates of tool revolution suggesting that the inherent capability of friction stir welding technique for aluminum 2014 alloys. The strength of the joints gradually increases with enhancing of welding speed. The micro structural observations exhibited the formation of equiaxed grains in the stir zone and slightly in the thermo-mechanically affected zone. In addition, the size of the grains decreases with increase in welding speed owing to the presence of low heat input. Hence the hardness of the joints slightly increased in the stir zones over the other zones of the weld nugget. The joint strength initially increases with the welding speed and starts to decreases after reaching to the maximum value. The relationship between the welding conditions and friction stir welded joint properties has been discussed.

  12. Microstructure and mechanical properties of resistance upset butt welded 304 austenitic stainless steel joints

    International Nuclear Information System (INIS)

    Sharifitabar, M.; Halvaee, A.; Khorshahian, S.

    2011-01-01

    Graphical abstract: Three different microstructural zones formed at different distances from the joint interface in resistance upset butt welding of 304 austenitic stainless steel. Highlights: → Evaluation of microstructure in resistance upset welding of 304 stainless steel. → Evaluation of welding parameters effects on mechanical properties of the joint. → Introducing the optimum welding condition for joining stainless steel bars. -- Abstract: Resistance upset welding (UW) is a widely used process for joining metal parts. In this process, current, time and upset pressure are three parameters that affect the quality of welded products. In the present research, resistance upset butt welding of 304 austenitic stainless steel and effect of welding power and upset pressure on microstructure, tensile strength and fatigue life of the joint were investigated. Microstructure of welds were studied using scanning electron microscopy (SEM). X-ray diffraction (XRD) analysis was used to distinguish the phase(s) that formed at the joint interface and in heat affected zone (HAZ). Energy dispersive spectroscopy (EDS) linked to the SEM was used to determine chemical composition of phases formed at the joint interface. Fatigue tests were performed using a pull-push fatigue test machine and the fatigue properties were analyzed drawing stress-number of cycles to failure (S-N) curves. Also tensile strength tests were performed. Finally tensile and fatigue fracture surfaces were studied by SEM. Results showed that there were three different microstructural zones at different distances from the joint interface and delta ferrite phase has formed in these regions. There was no precipitation of chromium carbide at the joint interface and in the HAZ. Tensile and fatigue strengths of the joint decreased with welding power. Increasing of upset pressure has also considerable influence on tensile strength of the joint. Fractography of fractured samples showed that formation of hot spots at

  13. Study of the joining of polycarbonate panels in butt joint configuration through friction stir welding

    Science.gov (United States)

    Astarita, Antonello; Boccarusso, Luca; Carrino, Luigi; Durante, Massimo; Minutolo, Fabrizio Memola Capece; Squillace, Antonino

    2018-05-01

    Polycarbonate sheets, 3 mm thick, were successfully friction stir welded in butt joint configuration. Aiming to study the feasibility of the process and the influence of the process parameters joints under different processing conditions, obtained by varying the tool rotational speed and the tool travel speed, were realized. Tensile tests were carried out to characterize the joints. Moreover the forces arising during the process were recorded and carefully studied. The experimental outcomes proved the feasibility of the process when the process parameters are properly set, joints retaining more than 70% of the UTS of the base material were produced. The trend of the forces was described and explained, the influence of the process parameters was also introduced.

  14. Gas metal arc welding of butt joint with varying gap width based on neural networks

    DEFF Research Database (Denmark)

    Christensen, Kim Hardam; Sørensen, Torben

    2005-01-01

    penetration, when the gap width is varying during the welding process. The process modeling to facilitate the mapping from joint geometry and reference weld quality to significant welding parameters, has been based on a multi-layer feed-forward network. The Levenberg-Marquardt algorithm for non-linear least......This paper describes the application of the neural network technology for gas metal arc welding (GMAW) control. A system has been developed for modeling and online adjustment of welding parameters, appropriate to guarantee a certain degree of quality in the field of butt joint welding with full...

  15. A novel weld seam detection method for space weld seam of narrow butt joint in laser welding

    Science.gov (United States)

    Shao, Wen Jun; Huang, Yu; Zhang, Yong

    2018-02-01

    Structured light measurement is widely used for weld seam detection owing to its high measurement precision and robust. However, there is nearly no geometrical deformation of the stripe projected onto weld face, whose seam width is less than 0.1 mm and without misalignment. So, it's very difficult to ensure an exact retrieval of the seam feature. This issue is raised as laser welding for butt joint of thin metal plate is widely applied. Moreover, measurement for the seam width, seam center and the normal vector of the weld face at the same time during welding process is of great importance to the welding quality but rarely reported. Consequently, a seam measurement method based on vision sensor for space weld seam of narrow butt joint is proposed in this article. Three laser stripes with different wave length are project on the weldment, in which two red laser stripes are designed and used to measure the three dimensional profile of the weld face by the principle of optical triangulation, and the third green laser stripe is used as light source to measure the edge and the centerline of the seam by the principle of passive vision sensor. The corresponding image process algorithm is proposed to extract the centerline of the red laser stripes as well as the seam feature. All these three laser stripes are captured and processed in a single image so that the three dimensional position of the space weld seam can be obtained simultaneously. Finally, the result of experiment reveals that the proposed method can meet the precision demand of space narrow butt joint.

  16. Transient thermal analysis during friction stir welding between AA2014-T6 and pure copper

    Science.gov (United States)

    Gadhavi, A. R.; Ghetiya, N. D.; Patel, K. M.

    2018-04-01

    AA2xxx-Cu alloys showed larger applications in the defence sectors and in aerospace industries due to high strength to weight ratio and toughness. FSW in a butt joint configuration was carried out between AA2014-T6 and pure Copper placing AA2014 on AS and Cu on RS. Temperature profiles were observed by inserting K-type thermocouples in the mid-thickness at various locations of the plate. A sharp decrease in temperature profiles was observed on Copper side due to its higher thermal conductivity. A thermal numerical model was prepared in ANSYS to compare the simulated temperature profiles with the experimental temperature profiles and both the temperature profiles were found to be in good agreement.

  17. Application of ultrasonic NDT technique for butt fusion joints of plastic pipes

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Tae Gyung; Lim, Hyung Taik; Choi, Jeong Guen; Lee, Jae Myung [ANSCO, Daejeon (Korea, Republic of)

    2016-05-15

    The long term-durability and the soundness of the plastic pipe have been sufficiently verified through use of the plastic pipe during the past several decades. Recently, as the pipe material have been constantly developed, the application of the plastic pipe is expanded to various industrial fields, such as an increase of a use pressure, the bigger diameter of the pipe, etc. In a nuclear power plant where a carbon steel pipe and a stainless steel pipe are mainly used as a safety class III buried pipe, safety in an operation is seriously threatened by abrasion, heat deterioration or the like, frequently generated in a metal pipe. Therefore, in order to provide an alternate to this problem there is a rising interest on using high-density polyethylene (HDPE) pipes which are known to provide much enhanced corrosion, abrasion and impact resistant properties. With polyethylene piping, one of the issue that is being looked into is the integrity of butt-fusion joint. At the present time the Referencing Code and Standard for the NDT technology of for butt fusion joint of the plastic pipe have not yet established. An optimum inspection parameters were determined according to the thickness of the HDPE pipe. It was also confirmed that most of the detection results of two techniques have matched with each other. In the PAUT, it is easy to distinguish signals with from the flaws made by the thin plate and the void. Also the resolving power of PAUT on the detection in the depth direction has been demonstrated to be satisfactory.

  18. 77 FR 12106 - Kapka Butte Sno-Park Construction

    Science.gov (United States)

    2012-02-28

    ... DEPARTMENT OF TRANSPORTATION Federal Highway Administration Kapka Butte Sno-Park Construction... Construction project. SUMMARY: The FHWA is issuing this notice to advise the public that the FHWA is officially designated as the Joint-Lead Agency pursuant to 23 U.S.C. 139(c)(1) for the Kapka Butte Sno-Park Construction...

  19. PENGARUH BESAR ARUS LISTRIK DENGAN MENGGUNAKAN ELEKTRODA SMAW TERHADAP KEKUATAN SAMBUNGAN LAS BUTT JOINT PADA PLAT MILD STEEL

    Directory of Open Access Journals (Sweden)

    Sarjito Jokosisworo

    2012-03-01

    Full Text Available The influence of mechanic disposition, is one of the factor influence ship strength. This influence can be test by mechanical test in welding butt joint. The result test database analysis can be conclude that very helpful to increase safety and quality butt joint. With steel specification C= 0,15%, Si= 0,24%, Mn= 0,88%,P= 0,018%, S= 0,034%. This material give a 90, 110, 125 ampere with SMAW AC electrode diameter 3,2 mm x 350 mm with V root and 600 angle In the fabrication of mild steel products, components or equipment, manufacturers employ welding as the principal joining method. Mild steel are weldable materials, and a welded joint can provide optimum corrosion resistance, strength, and fabrication economy. However, designers should recognize that any metal, including stainless steels, may undergo certain changes during welding. It is necessary, therefore, to exercise a reasonable degree of care during welding to minimize or prevent any deleterious effects that may occur, and to preserve the same degree of corrosion resistance and strength in weld zone that is an intheren part of the base metal

  20. Butt-joint integration of active optical components based on InP/AlInGaAsP alloys

    DEFF Research Database (Denmark)

    Kulkova, Irina; Kuznetsova, Nadezda; Semenova, Elizaveta

    2014-01-01

    We demonstrate all-active planar high quality butt-joint (BJ) integration of a QW Semiconductor Optical Amplifier (SOA) and MQW Electro-Absorption Modulator (EAM) based on an InP/AlInGaAsP platform. The degradation of the optical properties in the vicinity of ~1 μm to the BJ interface was determi...

  1. Influence of groove size and reinforcements addition on mechanical properties and microstructure of friction stir welded joints

    Science.gov (United States)

    Reddy Baridula, Ravinder; Ibrahim, Abdullah Bin; Yahya, Che Ku Mohammad Faizal Bin Che Ku; Kulkarni, Ratnakar; Varma Ramaraju, Ramgopal

    2018-03-01

    The butt joints fabricated by friction stir welding were found to have more strength than the joints obtained by conventional joining process. The important outcome of this process is the successful fabrication of surface composites with improved properties. Thus in order to further enhance the strength of the dissimilar alloy joints the reinforcements can be deposited in to the aluminium matrix during the process of friction stir welding. In the present study the multi-walled carbon nanotubes were embedded in to the groove by varying the width during joining of dissimilar alloys AA2024 and AA7075. Four widths were selected with constant depth and optimum process parameters were selected to fabricate the sound welded joints. The results show that the mechanical properties of the fabricated butt joints were influenced by the size of the groove, due to variation in the deposition of reinforcement in the stir zone. The microstructural study and identification of the elements of the welded joints show that the reinforcements deposition is influenced by the size of the groove. It has also been observed that the groove with minimum width is more effective than higher width. The mechanical properties are found to be improved due to the pinning of grain boundaries.

  2. Identifying Combination of Friction Stir Welding Parameters to Maximize Strength of Lap Joints of AA2014-T6 Aluminum Alloy

    Directory of Open Access Journals (Sweden)

    Rajendrana C.

    2017-01-01

    Full Text Available AA2014 aluminum alloy (Al-Cu alloy has been widely utilized in fabrication of lightweight structures like aircraft structures, demanding high strength to weight ratio and good corrosion resistance. The fusion welding of these alloys will lead to solidification problems such as hot cracking. Friction stir welding is a new solid state welding process, in which the material being welded does not melt and recast. Lot of research works have been carried out by many researchers to optimize process parameters and establish empirical relationships to predict tensile strength of friction stir welded butt joints of aluminum alloys. However, very few investigations have been carried out on friction stir welded lap joints of aluminum alloys. Hence, in this investigation, an attempt has been made to optimize friction stir lap welding (FSLW parameters to attain maximum tensile strength using statistical tools such as design of experiment (DoE, analysis of variance (ANOVA, response graph and contour plots. By this method, it is found that maximum tensile shear fracture load of 12.76 kN can be achieved if a joint is made using tool rotational speed of 900 rpm, welding speed of 110 mm/min, tool shoulder diameter of 12 mm and tool tilt angle of 1.5°.

  3. Prediction of residual stresses and distortions due to laser beam welding of butt joints in pressure vessels

    International Nuclear Information System (INIS)

    Moraitis, G.A.; Labeas, G.N.

    2009-01-01

    A two-level three-dimensional Finite Element (FE) model has been developed to predict keyhole formation and thermo-mechanical response during Laser Beam Welding (LBW) of steel and aluminium pressure vessel or pipe butt-joints. A very detailed and localized (level-1) non-linear three-dimensional transient thermal model is initially developed, which simulates the mechanisms of keyhole formation, calculates the temperature distribution in the local weld area and predicts the keyhole size and shape. Subsequently, using a laser beam heat source model based on keyhole assumptions, a global (level-2) thermo-mechanical analysis of the LBW butt-joint is performed, from which the joint residual stresses and distortions are calculated. All the major physical phenomena associated to LBW, such as laser heat input via radiation, heat losses through convection and radiation, as well as latent heat are accounted for in the numerical model. Material properties and particularly enthalpy, which is very important due to significant material phase changes, are introduced as temperature-dependent functions. The main advantages of the developed model are its efficiency, flexibility and applicability to a wide range of LBW problems (e.g. welding for pressure vessel or pipework construction, welding of automotive, marine or aircraft components, etc). The model efficiency arises from the two-scale approach applied. Minimal or no experimental data are required for the keyhole size and shape computation by the level-1 model, while the thermo-mechanical response calculation by the level-2 model requires only process and material data. Therefore, it becomes possible to efficiently apply the developed simulation model to different material types and varying welding parameters (i.e. welding speed, heat source power, joint geometry, etc.) in order to control residual stresses and distortions within the welded structure

  4. A novel butt-joint scheme for the preparation of electro-absorptive lasers

    International Nuclear Information System (INIS)

    Cheng Yuanbing; Pan Jiaoqing; Zhou Fan; Feng Wen; Wang Baojun; Zhu Hongliang; Zhao Lingjuan; Wang Wei

    2008-01-01

    A 1.55 μm InGaAsP/InGaAsP multiple-quantum-well electro-absorption modulator (EAM) monolithically integrated with a distributed feedback laser (DFB) diode has been realized based on a novel butt-joint scheme by ultra-low metal-organic vapour phase epitaxy for the first time. The threshold current of 25 mA and an extinction ratio of more than 30 dB are obtained by using the novel structure. The beam divergence angles at the horizontal and vertical directions are as small as 19.3 deg. x 13 deg., respectively, without a spot-size converter by undercutting the InGaAsP active region. The capacitance of the ridge waveguide device with a deep mesa buried by polyimide was reduced down to 0.30 pF

  5. Comparison of Corner-Butt 45 (Cb-45 and Corner-Lap (Cl joints in friction stir welding

    Directory of Open Access Journals (Sweden)

    Setiawan Widia

    2018-01-01

    Full Text Available The 10 mm thick Aluminum 6061 plates have been corner joined using varied design and those were 45° Corner Butt and Corner Lap Joints (CB-45 & CL. Friction tool was hardened EMS 45. True experimental method was used with independent parameters is feed rate which varied at 10 mm/min, 15 mm/min and 30 mm/min respectively. Other parameter such as rotating speed was kept constant. Experiment results show that, CB-45 yields better properties than CL. The tensile strength of CB-45 reaches 163.7 MPa for 10 mm/min feed rate. Whilst CL produces joint with tensile strength equal 120 MPa for equal parameters. Microstructure observation showed that CB-45 produces fine and homogenous appearance of MgO compared to CL. This phenomenon is caused by the pin of CB-45 joint which fully penetrates the nugget zone which is not found in CL design. This microstructure in turn promotes higher tensile strength of CB-45.

  6. High-quality MOVPE butt-joint integration of InP/AlGaInAs/InGaAsP-based all-active optical components

    DEFF Research Database (Denmark)

    Kulkova, Irina; Kadkhodazadeh, Shima; Kuznetsova, Nadezda

    2014-01-01

    In this paper, we demonstrate the applicability of MOVPE butt-joint regrowth for integration of all-active InP/AlGaAs/InGaAsP optical components and the realization of high-functionality compact photonic devices. Planar high-quality integration of semiconductor optical amplifiers of various epi...

  7. Ultrasonic evaluation of friction stud welded AA 6063/AISI 1030 steel joints

    International Nuclear Information System (INIS)

    Hynes, N. Rajesh Jesudoss; Nagaraj, P.; Sujana, J. Angela Jennifa

    2014-01-01

    Highlights: • Friction stud welding of AA 6063 and AISI 1030 was done successfully. • Ultrasonic evaluation of interfacial properties. • EDX analysis confirms intermetallic compound (FeAl) in the interfacial region. - Abstract: Friction stud welding is a promising technique in many applications related to oil and gas industries. It is used to attach grating to offshore oil platforms in areas where arc welding is not permitted because of the risk of causing a fire or explosion. Attachment of anodes inside seawater discharge pipelines in a gas processing plant is performed by this process. This solid state joining process permits metal combinations such as welding of aluminum studs to steel which would be problematic with arc welding because of the formation of thick and brittle inter-metallic compounds. In the present work, AA 6063 is joined to AISI 1030 steel using friction stud welding machine. Properties that are of interest to manufacturing applications such as Young’s modulus, longitudinal velocity, bulk modulus and shear modulus are evaluated by means of an ultrasonic flaw detector. At the interface of the joint, there is an increase of 4.4%, 1.8%, 1.15% and 4.42% is observed for the properties Young’s modulus, longitudinal velocity, bulk modulus and shear modulus respectively. This is due to the formation of intermetallic compound and increase in hardness at the interfacial region. Energy Dispersive X-ray analysis confirms the presence of FeAl as the intermetallic compound. Scanning Electron Microscope evaluation shows the presence of an unbound zone at the center of the inner region which is due to the minimum rotational speed and low axial load experienced at that point. In the unbound zone, there is an incomplete bond between dissimilar metals and it is detrimental to joint strength. Optimum value of friction time and usage of pure aluminum interlayer during the friction stud welding process hinders the formation of unbound zone and enhances the

  8. Tensile behavior of friction stir welded AA 6061-T4 aluminum alloy joints

    International Nuclear Information System (INIS)

    Heidarzadeh, A.; Khodaverdizadeh, H.; Mahmoudi, A.; Nazari, E.

    2012-01-01

    Highlights: ► Range of parameters for defect-free friction stir welded AA 6061-T4 was reached. ► A model was developed for predicting UTS and EL of friction stir welded AA 6061-T4. ► The maximum values of UTS and EL of joints were estimated by developed model. ► The optimum values of FSW process parameters were determined. -- Abstract: In this investigation response surface methodology based on a central composite rotatable design with three parameters, five levels and 20 runs, was used to develop a mathematical model predicting the tensile properties of friction stir welded AA 6061-T4 aluminum alloy joints at 95% confidence level. The three welding parameters considered were tool rotational speed, welding speed and axial force. Analysis of variance was applied to validate the predicted model. Microstructural characterization and fractography of joints were examined using optical and scanning electron microscopes. Also, the effects of the welding parameters on tensile properties of friction stir welded joints were analyzed in detail. The results showed that the optimum parameters to get a maximum of tensile strength were 920 rev/min, 78 mm/min and 7.2 kN, where the maximum of tensile elongation was obtained at 1300 rev/min, 60 mm/min and 8 kN.

  9. ANSYS Simulation of Residual Strains in Butt-welded Joints

    Directory of Open Access Journals (Sweden)

    A. Atroshenko

    2014-07-01

    Full Text Available The effect of thermal-strain cycle on residual strains in thin-walled circular seams of cylindrical shells using TIG butt welds was studied. Estimates were calculated using numerical modelling. The structure was made of corrosion-resistant austenitic steels.

  10. Friction stir welding (FSW) of AA 6061 T6

    International Nuclear Information System (INIS)

    Cabot, Pedro; Monglioni, Alberto; Carella, Eduardo

    2002-01-01

    The friction-stir process (FSW) developed by England's TWI in the last decade is a new concept in solid phase friction welding that is particularly appropriate for soldering aluminum and its alloys. It offers interesting aspects and can advantageously replace the usual arch processes. It is an automatic process that solders together long pieces by butt or lap welding and, therefore, overcomes the greater limitation of the conventional friction process that can be applied only to pieces with revolution symmetry. FSW is based essentially on the use of a cylindrical tool with a special profile, which is inserted between the surfaces where the materials meet to join them together at a certain rotation speed and under a specific force. The pieces must be rigidly butt bonded or overlapped to prevent movement when the tool moves forward along the joint producing the dispersion of oxides, local plastisizing of the material and the weld. Since its creation FSW has been the subject of many international publications, but until the present work there was no technologically relevant data about tools and procedures. For this reason, when its promising and novel nature was noticed, the CNEA began its own development project in 1997. The main characteristics of the tool are reviewed here and the results of tests carried out to evaluate the influence of the feed velocity on the mechanical properties of the butt joining of a 6.25 mm thick AA6061 T6 plate. Different accumulated aspects of the experience are discussed as well (cw)

  11. Weldability of AA 5052 H32 aluminium alloy by TIG welding and FSW process - A comparative study

    Science.gov (United States)

    Shanavas, S.; Raja Dhas, J. Edwin

    2017-10-01

    Aluminium 5xxx series alloys are the strongest non-heat treatable aluminium alloy. Its application found in automotive components and body structures due to its good formability, good strength, high corrosion resistance, and weight savings. In the present work, the influence of Tungsten Inert Gas (TIG) welding parameters on the quality of weld on AA 5052 H32 aluminium alloy plates were analyzed and the mechanical characterization of the joint so produced was compared with Friction stir (FS) welded joint. The selected input variable parameters are welding current and inert gas flow rate. Other parameters such as welding speed and arc voltage were kept constant throughout the study, based on the response from several trial runs conducted. The quality of the weld is measured in terms of ultimate tensile strength. A double side V-butt joints were fabricated by double pass on one side to ensure maximum strength of TIG welded joints. Macro and microstructural examination were conducted for both welding process.

  12. Technical Letter Report - Preliminary Assessment of NDE Methods on Inspection of HDPE Butt Fusion Piping Joints for Lack of Fusion

    International Nuclear Information System (INIS)

    Crawford, Susan L.; Cumblidge, Stephen E.; Doctor, Steven R.; Hall, Thomas E.; Anderson, Michael T.

    2008-01-01

    The U.S. Nuclear Regulatory Commission (NRC) has a multi-year program at the Pacific Northwest National Laboratory (PNNL) to provide engineering studies and assessments of issues related to the use of nondestructive evaluation (NDE) methods for the reliable inspection of nuclear power plant components. As part of this program, there is a subtask 2D that was set up to address an assessment of issues related to the NDE of high density polyethylene (HDPE) butt fusion joints. This work is being driven by the nuclear industry wanting to employ HDPE materials in nuclear power plant systems. This being a new material for use in nuclear applications, there are a number of issues related to its use and potential problems that may evolve. The industry is pursuing ASME Code Case N-755 entitled 'Use of Polyethylene (PE) Plastic Pipe for Section III, Division 1, Construction and Section XI Repair/Replacement Activities' that contains the requirements for nuclear power plant applications of HDPE. This Code Case requires that inspections be performed after the fusion joint is made by visually examining the bead that is formed and conducting a pressure test of the joint. These tests are only effective in general if gross through-wall flaws exist in the fusion joint. The NRC wants to know whether a volumetric inspection can be conducted on the fusion joint that will reliably detect lack-of-fusion conditions that may be produced during joint fusing. The NRC has requested that the work that PNNL is conducting be provided to assist them in resolving this inspection issue of whether effective volumetric NDE can be conducted to detect lack of fusion (LOF) in the butt HDPE joints. PNNL had 24 HDPE pipe specimens manufactured of 3408 material to contain LOF conditions that could be used to assess the effectiveness of NDE in detecting the LOF. Basic ultrasonic material properties were measured and used to guide the use of phased arrays and time-of-flight diffraction (TOFD) work that was

  13. Development of radiographic technique for examining k-type butt weld

    International Nuclear Information System (INIS)

    Barui, K.L.; Bhattacharyya, B.

    1983-01-01

    An attempt is made to develop a radiographic technique for examining K-type full penetration butt joints in heavy duty crane girders. The existing standard techniques of radiographic examination is found to be unsuitable to assess the internal defects properly. The examination technique reported here is successful in detecting not only the nature of the internal defects but also their degree of severities - from which clues for avoiding the most probable defects can be found out. The results of radiographic examination applied on the K-type butt joints of heavy duty crane girders have been discussed and it is specified that the acceptable limit of the defects must lie between 'blue' and 'green' according to the IIW colour code. Much work is yet to be done before standard specifications regarding the acceptibility of the defects in the actual job can be formulated. (author)

  14. Corrosion Properties of Cryorolled AA2219 Friction Stir Welded Joints Using Different Tool Pin Profiles

    Science.gov (United States)

    Kamal Babu, K.; Panneerselvam, K.; Sathiya, P.; Noorul Haq, A.; Sundarrajan, S.; Mastanaiah, P.; Srinivasa Murthy, C. V.

    The purpose of this paper is to present the corrosion behavior of the Cryorolled (CR) material and its Friction Stir Welded joints. Due to the thermal cycles of Friction Stir Welding (FSW) process, the corrosion behavior of the material gets affected. Here, the cryorolling process was carried out on AA2219 alloy and CR material was joined by FSW process using four different pin tool profiles such as cylindrical, threaded cylindrical, square and hexagonal pin. The FSW joints were analyzed by corrosion resistance with the help of potentiodynamic polarization test with 3.5% NaCl solution. From the analysis, it is found that CR AA2219 material exhibits good corrosion resistance compared to the base AA2219 material, and also a hexagonal pin profile FSW joint exhibits high corrosion resistance. Among the weld joints created by four different tools, the lowest corrosion resistance was found in the cylindrical pin tool FSW welds. Further, the corroded samples were investigated through metallurgical investigations like OM, Transmission Electron Microscopy (TEM), Energy-Dispersive X-ray Spectroscopy (EDX) and X-Ray Diffraction (XRD). It was found that the amount of dissolution of Al2Cu precipitate was present in the weld nugget. The amount of dissolution of Al2Cu precipitate is higher in the weld nugget produced by hexagonal pin tool. This is due to the enhancement of the corrosion resistance.

  15. Finite element analysis of cylindrical pressure vessels having a misalignment in a circumferential joint

    International Nuclear Information System (INIS)

    Aseer Brabin, T.; Christopher, T.; Nageswara Rao, B.

    2010-01-01

    Finite element analysis (FEA) has been carried out to obtain the elastic stress distribution at cylinder-to-cylinder junction in pressurized shell structures that have applications in space - vehicle design. To validate the finite element modeling and analysis results, three joint configurations, (viz., unfilleted butt joint with equal thickness, unfilleted butt joint with unequal thickness and filleted butt joint with equal thickness) having test results in open literature were considered. The peak stress values for these configurations obtained from FEA are close to that of test results. The peak stress value is found to reduce due to filleted butt joint as expected and also confirmed through test results.

  16. Multiple Crack Growth Prediction in AA2024-T3 Friction Stir Welded Joints, Including Manufacturing Effects

    DEFF Research Database (Denmark)

    Carlone, Pierpaolo; Citarella, Roberto; Sonne, Mads Rostgaard

    2016-01-01

    A great deal of attention is currently paid by several industries toward the friction stir welding process to realize lightweight structures. Within this aim, the realistic prediction of fatigue behavior of welded assemblies is a key factor. In this work an integrated finite element method - dual...... boundary element method (FEM-DBEM) procedure, coupling the welding process simulation to the subsequent crack growth assessment, is proposed and applied to simulate multiple crack propagation, with allowance for manufacturing effects. The friction stir butt welding process of the precipitation hardened AA...... on a notched specimen. The whole procedure was finally tested comparing simulation outcomes with experimental data. The good agreement obtained highlights the predictive capability of the method. The influence of the residual stress distribution on crack growth and the mutual interaction between propagating...

  17. Investigation of effects of process parameters on properties of friction stir welded joints

    Science.gov (United States)

    Chauhan, Atul; Soota, Tarun; Rajput, S. K.

    2018-03-01

    This work deals with application of friction stir welding (FSW) using application of Taguchi orthogonal array. FSW procedure is used for joining the aluminium alloy AA6063-T0 plates in butt configuration with orthogonal combination of factors and their levels. The combination of factors involving tool rotation speed, tool travel speed and tool pin profile are used in three levels. Grey relational analysis (GRA) has been applied to select optimum level of factors for optimising UTS, ductility and hardness of joint. Experiments have been conducted with two different tool materials (HSS and HCHCr steel) with various factors level combinations for joining AA6063-T0. On the basis of grey relational grades at different levels of factors and analysis of variance (ANOVA) ideal combination of factors are determined. The influence of tool material is also studied.

  18. Simulation and experimental study on distortion of butt and T-joints using WELD PLANNER

    International Nuclear Information System (INIS)

    Sulaiman, Mohd Shahar; Manurung, Yupiter HP; Rahim, Mohammad Ridzwan Abdul Mohd; Redza, Ridhwan; Lidam, Robert Ngendang Ak.; Abas, Sunhaji Kiyai; Tham, Ghalib; Haruman, Esa; Chau, Chan Yin

    2011-01-01

    This paper investigates the capability of linear thermal elastic numerical analysis to predict the welding distortion that occurs due to GMAW process. Distortion is considered as the major stumbling block that can adversely affect the dimensional accuracy and thus lead to expensive corrective work. Hence, forecast of distortion is crucially needed and ought to be determined in advance in order to minimize the negative effects, improve the quality of welded parts and finally to reduce the production costs. In this study, the welding deformation was simulated by using relatively new FEM software WELD PLANNER developed by ESI Group. This novel Welding Simulation Solution was employed to predict welding distortion induced in butt and T-joints with thickness of 4 mm. Low carbon steel material was used for the simulation and experimental study. A series of experiments using fully automated welding process were conducted for verification purpose to measure the distortion. By comparing between the simulation and experimental results, it was found out that this program code offered fast solution analysis time in estimating weld induced distortion within acceptable accuracy

  19. Simulation and experimental study on distortion of butt and T-joints using WELD PLANNER

    Energy Technology Data Exchange (ETDEWEB)

    Sulaiman, Mohd Shahar; Manurung, Yupiter HP; Rahim, Mohammad Ridzwan Abdul Mohd; Redza, Ridhwan; Lidam, Robert Ngendang Ak.; Abas, Sunhaji Kiyai; Tham, Ghalib [Universiti Teknologi MARA, Kuala Lumpur (Malaysia); Haruman, Esa [Bakrie University, Jakarta (Indonesia); Chau, Chan Yin [ESI Group, Kuala Lumpur (Malaysia)

    2011-10-15

    This paper investigates the capability of linear thermal elastic numerical analysis to predict the welding distortion that occurs due to GMAW process. Distortion is considered as the major stumbling block that can adversely affect the dimensional accuracy and thus lead to expensive corrective work. Hence, forecast of distortion is crucially needed and ought to be determined in advance in order to minimize the negative effects, improve the quality of welded parts and finally to reduce the production costs. In this study, the welding deformation was simulated by using relatively new FEM software WELD PLANNER developed by ESI Group. This novel Welding Simulation Solution was employed to predict welding distortion induced in butt and T-joints with thickness of 4 mm. Low carbon steel material was used for the simulation and experimental study. A series of experiments using fully automated welding process were conducted for verification purpose to measure the distortion. By comparing between the simulation and experimental results, it was found out that this program code offered fast solution analysis time in estimating weld induced distortion within acceptable accuracy.

  20. Enhancement of mechanical properties and corrosion resistance of friction stir welded joint of AA2014 using water cooling

    Energy Technology Data Exchange (ETDEWEB)

    Sinhmar, S., E-mail: sinhmarsunil88@gmail.com; Dwivedi, D.K.

    2017-01-27

    An investigation on the microstructure, mechanical properties, and corrosion behavior of friction stir welded joint of AA2014 in natural cooled (NC) and water cooled (WC) conditions have been reported. Optical microscopy, field emission scanning electron microscopy (FESEM) with Energy dispersive X-ray spectroscopy (EDS), Vicker's microhardness, tensile testing, X-ray diffraction (XRD), and electrochemical potentiodynamic polarization corrosion test (Tafel curve) were carried out to characterize the friction stir weld joints in both the cooling conditions. Water cooling resulted in higher strength and microhardness of friction stir weld joint compared to the natural cooling. The width of heat affected zone was reduced by the use of water cooling during friction stir welding (FSW) and minimum hardness zone was shifted towards weld center. The corrosion test was performed in 3.5% NaCl solution. Corrosion resistance of water cooled joint was found higher than natural cooled FSW joint. The precipitation behavior of weld nugget and heat affected zone impacts the corrosion resistance of FSW joint of AA 2014. Hardness, tensile, and corrosion properties of FSW joints produced under NC and WC conditions have been discussed in the light of microstructure.

  1. Enhancement of mechanical properties and corrosion resistance of friction stir welded joint of AA2014 using water cooling

    International Nuclear Information System (INIS)

    Sinhmar, S.; Dwivedi, D.K.

    2017-01-01

    An investigation on the microstructure, mechanical properties, and corrosion behavior of friction stir welded joint of AA2014 in natural cooled (NC) and water cooled (WC) conditions have been reported. Optical microscopy, field emission scanning electron microscopy (FESEM) with Energy dispersive X-ray spectroscopy (EDS), Vicker's microhardness, tensile testing, X-ray diffraction (XRD), and electrochemical potentiodynamic polarization corrosion test (Tafel curve) were carried out to characterize the friction stir weld joints in both the cooling conditions. Water cooling resulted in higher strength and microhardness of friction stir weld joint compared to the natural cooling. The width of heat affected zone was reduced by the use of water cooling during friction stir welding (FSW) and minimum hardness zone was shifted towards weld center. The corrosion test was performed in 3.5% NaCl solution. Corrosion resistance of water cooled joint was found higher than natural cooled FSW joint. The precipitation behavior of weld nugget and heat affected zone impacts the corrosion resistance of FSW joint of AA 2014. Hardness, tensile, and corrosion properties of FSW joints produced under NC and WC conditions have been discussed in the light of microstructure.

  2. Variant selection of martensites in steel welded joints with low transformation temperature weld metals

    International Nuclear Information System (INIS)

    Takahashi, Masaru; Yasuda, Hiroyuki Y.

    2013-01-01

    Highlights: ► We examined the variant selection of martensites in the weld metals. ► We also measured the residual stress developed in the butt and box welded joints. ► 24 martensite variants were randomly selected in the butt welded joint. ► High tensile residual stress in the box welded joint led to the strong variant selection. ► We discussed the rule of the variant selection focusing on the residual stress. -- Abstract: Martensitic transformation behavior in steel welded joints with low transformation temperature weld (LTTW) metal was examined focusing on the variant selection of martensites. The butt and box welded joints were prepared with LTTW metals and 980 MPa grade high strength steels. The residual stress of the welded joints, which was measured by a neutron diffraction technique, was effectively reduced by the expansion of the LTTW metals by the martensitic transformation during cooling after the welding process. In the LTTW metals, the retained austenite and martensite phases have the Kurdjumov–Sachs (K–S) orientation relationship. The variant selection of the martensites in the LTTW metals depended strongly on the type of welded joints. In the butt welded joint, 24 K–S variants were almost randomly selected while a few variants were preferentially chosen in the box welded joint. This suggests that the high residual stress developed in the box welded joint accelerated the formation of specific variants during the cooling process, in contrast to the butt welded joint with low residual stress

  3. Use of pulsed arc welding for butt joint fabrication

    International Nuclear Information System (INIS)

    Merkulov, B.A.

    1977-01-01

    A technology of pulsed-arc butt welding with periodic wire feed to the welding zone has been developed. The pulsed arc is suitable both for submerged and gas-shielded weldings. The technology proposed has some advantages over the stationary-arc welding. Control of the amplitude-frequency characteristics of the process enables one to affect melting and crystallization conditions of the welding crater, weld shape, relation between melting and deposited metal section areas, etc., as well as to reduce heat contribution to the base metal. The new process is shown to be applicable in power engineering. Automatic submerged welding conditions are given for low-carbon and pearlitic heat-resistant steels

  4. Laser shock peening on a 6056-T4 aluminium alloy for airframe applications

    CSIR Research Space (South Africa)

    Glaser, D

    2014-03-01

    Full Text Available stream_source_info Pityana1_2014_ABSTRACT ONLY.pdf.txt stream_content_type text/plain stream_size 1356 Content-Encoding ISO-8859-1 stream_name Pityana1_2014_ABSTRACT ONLY.pdf.txt Content-Type text/plain; charset=ISO-8859-1... Laser Shock Peening on a 6056-T4 Aluminium Alloy for Airframe Applications Daniel Glaser, Claudia Polese, Rachana D. Bedekar, Jasper Plaisier,Sisa Pityana, Bathusile Masina, Tebogo Mathebula, and Enrico Troiani Keywords: Laser Shock Peening...

  5. Effect of current and speed on porosity in autogenous Tungsten Inert Gas (TIG) welding of aluminum alloys A1100 butt joint

    Science.gov (United States)

    Milyardi, Indra; Sunar Baskoro, Ario

    2018-04-01

    Autogenous Tungsten Inert Gas (TIG) welding has been conducted on aluminum alloy A1100. The purpose of this research is to determine the proper current and speed of autogenous TIG welding with butt joint pattern. Variations on welding current are 150 A, 155 A, and 160 A with the variations on welding speed are 1 mm/seconds, 1.1 mm/seconds, 1.2 mm/seconds. The welded results were tested using non-destructive test (NDT) method using X-Ray radiography. After the test, it is found that the appropriate current for the best result without porosity can be achieved using the welding parameter of welding current of 160 A and the welding speed of 1.1 mm seconds.

  6. Friction stir welding of 6061 aluminium alloy

    International Nuclear Information System (INIS)

    Abdel Rahman, M.A.M.S.

    2009-01-01

    6061 AA (Al-Mg-Si alloy) has gathered wide acceptance in the fabrication of light weight structures requiring a high strength-to-weight ratio and good corrosion resistance such as marine frames, pipelines, storage tanks, and aircraft components [1]. It is also used for the manufacturing of fuel elements in the nuclear research reactors. Compared to many of the fusion welding processes that are routinely used for joining structural alloys, friction stir welding (FSW) is a solid state joining process in which the material that is being welded is not melted and recast [2]. The welding parameters such as tool rotational speed, welding traverse speed, and tool profile play a major role in deciding the weld quality. Several FSW tools (differ from each other in pin angle, shoulder diameter, and shoulder concavity) have been used to fabricate a number of joints in order to obtain a tool with which a sound weld can be produced. It was found that the FSW tool with tapered cone pin, concave shoulder, and shoulder diameter equal to four times the welded plate thickness is suitable to produce a sound weld. The effect of the traverse speed on the global and local tensile properties of friction stir welded joints has been investigated in the 6061-T6 AA. The global tensile properties of the FSW joints were improved with increasing the traverse speed at constant rotation rate. It is found that the global tensile strength of the FSW joint is limited by the local tensile strength of the nearest region to the weld center at which the cross section is composed mainly of the HAZ. The effect of the initial butt surface on the formation of the zigzag line on the tensile properties of the welds was examined by using three types of welding samples differ in the preparation of the initial butt surface. The first type of samples welded without removing the oxide layer from the initial butt surface (uncleaned butt surfaces joint). In the second type of samples the oxide layer was removed from

  7. The Effect of Weld Reinforcement and Post-Welding Cooling Cycles on Fatigue Strength of Butt-Welded Joints under Cyclic Tensile Loading.

    Science.gov (United States)

    Araque, Oscar; Arzola, Nelson; Hernández, Edgar

    2018-04-12

    This research deals with the fatigue behavior of butt-welded joints, by considering the geometry and post-welding cooling cycles, as a result of cooling in quiet air and immersed in water. ASTM A-36 HR structural steel was used as the base metal for the shielded metal arc welding (SMAW) process with welding electrode E6013. The welding reinforcement was 1 mm and 3 mm, respectively; axial fatigue tests were carried out to determine the life and behavior in cracks propagation of the tested welded joints, mechanical characterization tests of properties in welded joints such as microhardness, Charpy impact test and metallographic analysis were carried out. The latter were used as input for the analysis by finite elements which influence the initiation and propagation of cracks and the evaluation of stress intensity factors (SIF). The latter led to obtaining the crack propagation rate and the geometric factor. The tested specimens were analyzed, by taking photographs of the cracks at its beginning in order to make a count of the marks at the origin of the crack. From the results obtained and the marks count, the fatigue crack growth rate and the influence of the cooling media on the life of the welded joint are validated, according to the experimental results. It can be concluded that the welded joints with a higher weld reinforcement have a shorter fatigue life. This is due to the stress concentration that occurs in the vicinity of the weld toe.

  8. An investigation into the mechanism for enhanced mechanical properties in friction stir welded AA2024-T3 joints coated with cold spraying

    Science.gov (United States)

    Li, N.; Li, W. Y.; Yang, X. W.; Feng, Y.; Vairis, A.

    2018-05-01

    Using cold spraying (CS), a surface layer with a modified microstructure and enhanced mechanical properties was formed on a 3.2 mm thick friction stir welded (FSWed) AA2024-T3 joint. The combined effect of "shot peening effect (SPE)" and "heat flow effect (HFE)" during CS were used to enhance joint mechanical properties. The microstructure evolution of the FSWed AA2024-T3 joints in the surface layer following CS coatings and their effect on mechanical properties were systematically characterized with electron back-scattered diffraction, transmission electron microscopy, differential scanning calorimetry and mechanical tests. Based on these experiments, a grain refinement, finer and more S phases, and improved amount of Guinier-Preston-Bagaryatsky (GPB) zones produced by CS treatments are proposed. The deposition of aluminum coating on the joint, lead to hardness recovery in the stir zone and the development of two low hardness zones as the density of GPB increased. The tensile properties of FSWed AA2024-T3 joints improved with the application of the aluminum coatings. Experiments and analysis of the enhanced mechanical properties mechanism indicate that SPE with a high plastic deformation and HFE with an intensive heat flow are necessary for the production of refined grains and increased numbers of GPB zones.

  9. Development and modeling of hot tearing test in TIG welding of aluminum alloy 6056

    OpenAIRE

    Niel , Aurélie; Fras , Gilles; Deschaux-Beaume , Frédéric; Bordreuil , Cyril

    2010-01-01

    International audience; TIG welding process is widely used in the aeronautic industry. However, the increase of productivity which generally require an increase of welding speed is limited by the appearance of defects, such as hot tearing. This study focuses on the analysis of hot tearing in TIG welding on a 6056 aluminum alloy, used in aircraft manufacturing. Thanks to the developpement of an original hot tearing test and to numerical simulation of welding process, the influence of various p...

  10. Preliminary geologic map of the Sleeping Butte volcanic centers

    International Nuclear Information System (INIS)

    Crowe, B.M.; Perry, F.V.

    1991-07-01

    The Sleeping Butte volcanic centers comprise two, spatially separate, small-volume ( 3 ) basaltic centers. The centers were formed by mildly explosive Strombolian eruptions. The Little Black Peak cone consists of a main scoria cone, two small satellitic scoria mounds, and associated lobate lava flows that vented from sites at the base of the scoria cone. The Hidden Cone center consists of a main scoria cone that developed on the north-facing slope of Sleeping Butte. The center formed during two episodes. The first included the formation of the main scoria cone, and venting of aa lava flows from radial dikes at the northeast base of the cone. The second included eruption of scoria-fall deposits from the summit crater. The ages of the Little Black Peak and the Hidden Cone are estimated to be between 200 to 400 ka based on the whole-rock K-Ar age determinations with large analytical undertainty. This age assignment is consistent with qualitative observations of the degree of soil development and geomorphic degradation of volcanic landforms. The younger episode of the Hidden Cone is inferred to be significantly younger and probably of Late Pleistocene or Holocene age. This is based on the absence of cone slope rilling, the absence of cone-slope apron deposits, and erosional unconformity between the two episodes, the poor horizon- development of soils, and the presence of fall deposits on modern alluvial surfaces. Paleomagnetic data show that the centers record similar but not identical directions of remanent magnetization. Paleomagnetic data have not been obtained for the youngest deposits of the Hidden Cone center. Further geochronology, soils, geomorphic, and petrology studies are planned of the Sleeping Butte volcanic centers 20 refs., 3 figs

  11. Ultrasonic inspection of AA6013 laser welded joints

    Directory of Open Access Journals (Sweden)

    Adriano Passini

    2011-09-01

    Full Text Available Interest in laser beam welding for aerospace applications is continuously growing, mainly for aluminum alloys. The joints quality is usually assessed by non-destructive inspection (NDI. In this work, bead on plate laser welds on 1.6 mm thick AA6013 alloy sheets, using a 2 kW Yb-fiber laser were obtained and inspected by pulse/echo ultrasonic phased-array technique. Good and poor quality welds were inspected in order to verify the limits of inspection, comparing also to X-ray radiography and metallographic inspections. The results showed that ultrasonic phased array technique was able to identify the presence of grouped porosity, through the attenuation of the amplitude of the echo signal. This attenuation is attributed to the scattering of the waves caused by micro pores, with individual size below the resolution limit of the equipment, but when grouped, can cause a perceptive effect on the reflection spectra.

  12. Effects Of Welding On The Fatigue Behaviour Of Commercial Aluminum AA-1100 Joints

    Science.gov (United States)

    Uthayakumar, M.; Balasubramanian, V.; Rani, Ahmad Majdi Abdul; Hadzima, Branislav

    2018-04-01

    Friction Stir Welding (FSW) is an budding solid state welding process, which is frequently used for joining aluminum alloys where materials can be joined without melt and recast. Therefore, when welding alloys through FSW the phase transformations occurs will be in the solid state form. The present work is aimed in evaluating the fatigue life of friction stir welded commercial grade aluminum alloy joints. The commercial grade AA1100 aluminum alloy of 12mm thickness plate is welded and the specimens are tested using a rotary beam fatigue testing machine at different stress levels. The stress versus number of cycles (S-N) curves was plotted using the data points. The Fatigue life of tungsten inert gas (TIG) and metal inert gas (MIG) welded joints was compared. The fatigue life of the weld joints was interrelated with the tensile properties, microstructure and micro hardness properties. The effects of the notches and welding processes are evaluated and reported.

  13. Butt Welding of 2205/X65 Bimetallic Sheet and Study on the Inhomogeneity of the Properties of the Welded Joint

    Science.gov (United States)

    Gou, Ning-Nian; Zhang, Jian-Xun; Wang, Jian-Long; Bi, Zong-Yue

    2017-04-01

    The explosively welded 2205 duplex stainless steel/X65 pipe steel bimetallic sheets were butt jointed by multilayer and multi-pass welding (gas tungsten arc welding for the flyer and gas metal arc welding for the transition and parent layers of the bimetallic sheets). The microstructure and mechanical properties of the welded joint were investigated. The results showed that in the thickness direction, microstructure and mechanical properties of the welded joint exhibited obvious inhomogeneity. The microstructures of parent filler layers consisted of acicular ferrite, widmanstatten ferrite, and a small amount of blocky ferrite. The microstructure of the transition layer and flyer layer consisted of both austenite and ferrite structures; however, the transition layer of weld had a higher volume fraction of austenite. The results of the microhardness test showed that in both weld metal (WM) and heat-affected zone (HAZ) of the parent filler layers, the average hardness decreased with the increasing (from parent filler layer 1 to parent filler layer 3) welding heat input. The results of hardness test also indicated that the hardness of the WM and the HAZ for the flyer and transition layers was equivalent. The tensile test combined with Digital Specklegram Processing Technology demonstrated that the fracturing of the welded joint started at the HAZ of the flyer, and then the fracture grew toward the base metal of the parent flyer near the parent HAZ. The stratified impact test at -5 °C showed that the WM and HAZ of the flyer exhibited lower impact toughness, and the fracture mode was ductile and brittle mixed fracture.

  14. Influence of the implant-abutment connection design and diameter on the screw joint stability

    Science.gov (United States)

    Shin, Hyon-Mo; Huh, Jung-Bo; Yun, Mi-Jeong; Jeon, Young-Chan; Chang, Brian Myung

    2014-01-01

    PURPOSE This study was conducted to evaluate the influence of the implant-abutment connection design and diameter on the screw joint stability. MATERIALS AND METHODS Regular and wide-diameter implant systems with three different joint connection designs: an external butt joint, a one-stage internal cone, and a two-stage internal cone were divided into seven groups (n=5, in each group). The initial removal torque values of the abutment screw were measured with a digital torque gauge. The postload removal torque values were measured after 100,000 cycles of a 150 N and a 10 Hz cyclic load had been applied. Subsequently, the rates of the initial and postload removal torque losses were calculated to evaluate the effect of the joint connection design and diameter on the screw joint stability. Each group was compared using Kruskal-Wallis test and Mann-Whitney U test as post-hoc test (α=0.05). RESULTS The postload removal torque value was high in the following order with regard to magnitude: two-stage internal cone, one-stage internal cone, and external butt joint systems. In the regular-diameter group, the external butt joint and one-stage internal cone systems showed lower postload removal torque loss rates than the two-stage internal cone system. In the wide-diameter group, the external butt joint system showed a lower loss rate than the one-stage internal cone and two-stage internal cone systems. In the two-stage internal cone system, the wide-diameter group showed a significantly lower loss rate than the regular-diameter group (P<.05). CONCLUSION The results of this study showed that the external butt joint was more advantageous than the internal cone in terms of the postload removal torque loss. For the difference in the implant diameter, a wide diameter was more advantageous in terms of the torque loss rate. PMID:24843398

  15. Influence of the implant-abutment connection design and diameter on the screw joint stability.

    Science.gov (United States)

    Shin, Hyon-Mo; Huh, Jung-Bo; Yun, Mi-Jeong; Jeon, Young-Chan; Chang, Brian Myung; Jeong, Chang-Mo

    2014-04-01

    This study was conducted to evaluate the influence of the implant-abutment connection design and diameter on the screw joint stability. Regular and wide-diameter implant systems with three different joint connection designs: an external butt joint, a one-stage internal cone, and a two-stage internal cone were divided into seven groups (n=5, in each group). The initial removal torque values of the abutment screw were measured with a digital torque gauge. The postload removal torque values were measured after 100,000 cycles of a 150 N and a 10 Hz cyclic load had been applied. Subsequently, the rates of the initial and postload removal torque losses were calculated to evaluate the effect of the joint connection design and diameter on the screw joint stability. Each group was compared using Kruskal-Wallis test and Mann-Whitney U test as post-hoc test (α=0.05). THE POSTLOAD REMOVAL TORQUE VALUE WAS HIGH IN THE FOLLOWING ORDER WITH REGARD TO MAGNITUDE: two-stage internal cone, one-stage internal cone, and external butt joint systems. In the regular-diameter group, the external butt joint and one-stage internal cone systems showed lower postload removal torque loss rates than the two-stage internal cone system. In the wide-diameter group, the external butt joint system showed a lower loss rate than the one-stage internal cone and two-stage internal cone systems. In the two-stage internal cone system, the wide-diameter group showed a significantly lower loss rate than the regular-diameter group (P<.05). The results of this study showed that the external butt joint was more advantageous than the internal cone in terms of the postload removal torque loss. For the difference in the implant diameter, a wide diameter was more advantageous in terms of the torque loss rate.

  16. Effect of Friction Stir Welding Parameters on the Mechanical and Microstructure Properties of the Al-Cu Butt Joint

    Directory of Open Access Journals (Sweden)

    Sare Celik

    2016-05-01

    Full Text Available Friction Stir Welding (FSW is a solid-state welding process used for welding similar and dissimilar materials. FSW is especially suitable to join sheet Al alloys, and this technique allows different material couples to be welded continuously. In this study, 1050 Al alloys and commercially pure Cu were produced at three different tool rotation speeds (630, 1330, 2440 rpm and three different tool traverse speeds (20, 30, 50 mm/min with four different tool position (0, 1, 1.5, 2 mm by friction stir welding. The influence of the welding parameters on the microstructure and mechanical properties of the joints was investigated. Tensile and bending tests and microhardness measurements were used to determine the mechanical properties. The microstructures of the weld zone were investigated by optical microscope and scanning electron microscope (SEM and were analyzed in an energy dispersed spectrometer (EDS. Intermetallic phases were detected based on the X-ray diffraction (XRD analysis results that evaluated the formation of phases in the weld zone. When the welding performance of the friction stir welded butt joints was evaluated, the maximum value obtained was 89.55% with a 1330 rpm tool rotational speed, 20 mm/min traverse speed and a 1 mm tool position configuration. The higher tensile strength is attributed to the dispersion strengthening of the fine Cu particles distributed over the Al material in the stir zone region.

  17. A Study on the Optimal Welding Condition for Root-Pass in Horizontal Butt-Joint TIG Welding

    Energy Technology Data Exchange (ETDEWEB)

    Jung, Sung Hun; Kim, Jae-Woong [Yeungnam Univ., Gyeongsan (Korea, Republic of)

    2017-04-15

    In this study, to investigate the shape of the back bead as a weld quality parameter and to select the optimal condition of the root-pass TIG welding of a horizontal butt-joint, an experimental design and the response surface method (RSM) have been employed. Three parameters are used as input variables, which include the base current, peak current, and welding speed. The back bead width is selected as an output variable representing the weld quality, the target value of the width is 5.4 mm. Conducting the experiments according to the Box-Behnken experimental design, a 2nd regression model for the back bead width was made, and the validation of the model was confirmed by using the F-test. The desirability function was designed through the nominal-the-best formula for the appropriate back bead width. Finally, the following optimal condition for welding was selected using the RSM: base current of 0.9204, peak current of 0.8676, and welding speed of 0.3776 in coded values. For verification, a test welding process under the optimal condition was executed and the result showed the back bead width of 5.38 mm that matched the target value well.

  18. A Study on the Optimal Welding Condition for Root-Pass in Horizontal Butt-Joint TIG Welding

    International Nuclear Information System (INIS)

    Jung, Sung Hun; Kim, Jae-Woong

    2017-01-01

    In this study, to investigate the shape of the back bead as a weld quality parameter and to select the optimal condition of the root-pass TIG welding of a horizontal butt-joint, an experimental design and the response surface method (RSM) have been employed. Three parameters are used as input variables, which include the base current, peak current, and welding speed. The back bead width is selected as an output variable representing the weld quality, the target value of the width is 5.4 mm. Conducting the experiments according to the Box-Behnken experimental design, a 2nd regression model for the back bead width was made, and the validation of the model was confirmed by using the F-test. The desirability function was designed through the nominal-the-best formula for the appropriate back bead width. Finally, the following optimal condition for welding was selected using the RSM: base current of 0.9204, peak current of 0.8676, and welding speed of 0.3776 in coded values. For verification, a test welding process under the optimal condition was executed and the result showed the back bead width of 5.38 mm that matched the target value well.

  19. AA magnet measurement team

    CERN Multimedia

    CERN PhotoLab

    1978-01-01

    Quickly improvised measurement equipment for the AA (Antiproton Accumulator) was all the tight schedule permitted, but the high motivation of the team made up for the lack of convenience. From left to right: Roy Billinge (Joint AA Project Leader, the other one was Simon van der Meer); Bruno Autin, Brian Pincott, Colin Johnson.

  20. First circulating beam in the AA

    CERN Multimedia

    CERN PhotoLab

    1980-01-01

    On 3 July 1980, two years after project authorization, beam circulated for the first time in the AA. It was a 3.56 GeV/c proton test beam. We see an expecting crowd, minutes before the happy event. The persons are too numerous to name them all, but the 3 most prominent ones are at the centre (left to right): Roy Billinge (Joint AA Project Leader, with his hand on the control box), Eifionydd Jones (white shirt), Simon van der Meer (spiritus rector and Joint AA Project Leader). The first antiprotons were injected, made to circulate and cooled soon after, on 14 July 1980.

  1. Strength of joints brazed with two-phase solders

    International Nuclear Information System (INIS)

    Shnyakin, N.S.; Parfenova, L.V.; Ekatova, A.S.; Prilepskaya, I.V.

    1976-01-01

    Dependence of the structure and strength of soldered joints upon a gap size in case of 1Kh18N10T stainless steel soldering with a double-phase solder of Ni-Zn-Cu system is described. Butt and lap joints have been subjected to soldering with gas-flame and induction heating. The optimum conditions of the solder crystallization are determined with wedge-gap samples. The studies show that the character of distribution of a fusible β-phase in metal depends upon a gap size. With gaps up to 0.1 mm the β-phase enriched with a fusible component (zinc) runs as a continuous thin interlayer in the middle of the seam. As a result of zinc evaporation from the β-phase this interlayer becomes internally oxidized. After the sample is broken an oxidized fracture gives one the impression of a poor fusion in the middle part of the joint. The ultimate strength of butt joints is 15-20 kgf/sq.mm. A value of thermal expansion of 1Kh18N10T steel samples, 1-5 mm thick, has been experimentally determined for butt soldering. The elongation of two halves of the sample is measured by an indicator and proved to be 0.89 mm for a 50x50x2 mm sample at a soldering temperature of 1.100 deg C. The paper presents methods for the calculation of an optimal gap value for butt soldering with a local gas-flame and induction heating

  2. Interview with Gavin Butt

    DEFF Research Database (Denmark)

    Hasse Jørgensen, Stina; Alexandra Sofie, Jönsson

    2008-01-01

    We have interviewed Gavin Butt about his research interest in the cross-field between performance and performativity in the visual arts: queer theory, queer cultures and their histories, post-second world war U.S. art, contemporary art and critical theory.......We have interviewed Gavin Butt about his research interest in the cross-field between performance and performativity in the visual arts: queer theory, queer cultures and their histories, post-second world war U.S. art, contemporary art and critical theory....

  3. Microstructure and mechanical properties of GTAW welded joints of AA6105 aluminum alloy

    Directory of Open Access Journals (Sweden)

    Minerva Dorta-Almenara

    2016-09-01

    Full Text Available Gas Tungsten Arc Welding (GTAW is one of the most used methods to weld aluminum. This work investigates the influence of welding parameters on the microstructure and mechanical properties of GTAW welded AA6105 aluminum alloy joints. AA6105 alloy plates with different percent values of cold work were joined by GTAW, using various combinations of welding current and speed. The fusion zone, in which the effects of cold work have disappeared, and the heat affected zone of the welded samples were examined under optical and scanning electron microscopes, additionally, mechanical tests and measures of Vickers microhardness were performed. Results showed dendritic morphology with solute micro- and macrosegregation in the fusion zone, which is favored by the constitutional supercooling when heat input increases. When heat input increased and welding speed increased or remained constant, greater segregation was obtained, whereas welding speed decrease produced a coarser microstructure. In the heat affected zone recrystallization, dissolution, and coarsening of precipitates occurred, which led to variations in hardness and strength.

  4. Microstructure examination and microhardness of friction stir welded joint of (AA7020-O after PWHT

    Directory of Open Access Journals (Sweden)

    Ghada M.F. Essa

    2018-04-01

    Full Text Available This paper studies the microstructure and microhardness of the welded joints of the annealed aluminum alloy AA7020-O produced by friction stir welding (FSW technique. The material was applied to post weld heat treatment (solution treatment and artificially aged, T6. The traverse speed and the rotational speed are the most important process parameters of FSW, and have great influence on the heat input of the welding operation which governs the welded joints quality. To investigate their effect, the welding operation was performed using three traverse speeds, 20, 40 and 60 mm/s with two rotational speeds of 1125 and 1400 rpm, and other welding parameters were kept constant to produce comparable joints. It was found that the two rotational speeds are accepted with lower traverse speeds to produce sound joints. Microstructure of the welded joints was significantly affected by the FSW process parameters, and slight effect was reported for the grain size. Microhardness examination showed high weld joint quality with respect to the base metal hardness, which proves the reprecipitation of the hardening phase in the weld zone. The microhardness profile was strongly dependant on the rotational speed, and the average values of the joints hardness have increased with the decrease in the rotational speed, where it have been slightly affected by the welding speed. Keywords: Friction stir welding, Aluminum alloy, Mechanical properties, Microstructures

  5. A Preliminary Report on the Strength and Metallography of a Bimetallic Friction Stir Weld Joint Between AA6061 and MIL-DTL-46100E High Hardness Steel Armor

    Science.gov (United States)

    2012-11-26

    bimetallic friction stir weld joint between AA6061 and MIL-DTL-46100E High Hardness steel armor. ABSTRACT One half inch thick plates of 6061-T6 aluminum...alloy and High Hardness steel armor (MIL- STD-46100) were successfully joined by the friction stir welding (FSW) process using a tungsten-rhenium...4. TITLE AND SUBTITLE A preliminary report on the strength and metallography of a bimetallic friction stir weld joint between AA6061 and MIL-DTL

  6. Effect of laser beam position on mechanical properties of F82H/SUS316L butt-joint welded by fiber laser

    Energy Technology Data Exchange (ETDEWEB)

    Serizawa, Hisashi, E-mail: serizawa@jwri.osaka-u.ac.jp [Joining and Welding Research Institute, Osaka University, 11-1 Mihogaoka, Ibaraki, Osaka 567-0047 (Japan); Mori, Daiki; Ogiwara, Hiroyuki; Mori, Hiroaki [Graduate School of Engineering, Osaka University, 2-1 Yamadaoka, Suita, Osaka 565-0871 (Japan)

    2014-10-15

    Highlights: • The micro hardness of weld metal in F82H/SUS316L joint partially decreases after PWHT by shifting beam position to SUS316L. • Charpy impact energy of F82H/SUS316L joint obviously increases after PWHT due to the release of residual stress. • The tensile strength of weld metal in F82H/SUS316L joint is higher than that of SUS316L. • The fiber laser welding seems to be one of the most candidate methods to join between F82H and SUS316L pipes practically. - Abstract: A dissimilar butt-joint between reduced activation ferritic/martensitic steel F82H and SUS316L austenitic stainless steel was made by 4 kW fiber laser and the influence of laser beam position on its mechanical properties before and after post-weld heat treatment (PWHT) was examined at room temperature. From the nano-indentation measurements and the microstructural observations, it is found that the micro hardness of weld metal partially decreases after PWHT by shifting beam position to SUS316L because its phase seems to move from only the martensitic phase to the mixture of austenitic and martensitic phases. In addition, Charpy impact test suggests that the impact energy slightly increases by shifting beam position before PWHT and obviously increases after PWHT due to the release of residual stress. Moreover, the tensile test indicates that the tensile strength of weld metal is higher than that of SUS316L and the fracture occurs at the base metal of SUS316L regardless of laser beam position.

  7. Microstructural features of friction stir welded dissimilar Aluminium alloys AA2219-AA7475

    Science.gov (United States)

    Zaman Khan, Noor; Ubaid, Mohammed; Siddiquee, Arshad Noor; Khan, Zahid A.; Al-Ahmari, Abdulrahman; Chen, Xizhang; Haider Abidi, Mustufa

    2018-05-01

    High strength, good corrosion resistance, light weight make aluminium alloys a material of choice in many industrial sectors like aerospace, marine etc. Problems associated with welding of these alloys by fusion welding processes restricted their use in various industries. Friction stir welding (FSW), a clean solid-state joining process, easily overcomes various difficulties encountered during conventional fusion welding processes. In the present work, the effect of rotational speed (710 rpm, 900 rpm and 1120 rpm) on micro-hardness distribution and microstructure of FSWed dissimilar aluminium alloy joints were analyzed. Plates of AA7475-T761 and AA2219-O having thickness of 2.5 mm were welded by fixing AA7475 on retreating side (RS) and AA2219 on advancing side (AS). Welded joints were characterized by Vickers micro-hardness testing, scanning electron microscopy (SEM) and optical microscopy (OM). Results revealed that rotational speed significantly affects the micro-hardness due to increase in grain size, coarsening and dissolution of strengthening precipitates and re-precipitation. Higher micro-hardness values were observed in stir zone due to grain refinement and re-precipitation. Minimum micro-hardness value was observed at the TMAZ/HAZ of advancing side due to thermal softening.

  8. Through thickness property variations in a thick plate AA7050 friction stir welded joint

    International Nuclear Information System (INIS)

    Canaday, Clinton T.; Moore, Matthew A.; Tang, Wei; Reynolds, A.P.

    2013-01-01

    In this study, moderately thick (32 mm) AA7050 plates were joined by friction stir welding (FSW). Various methods were used to characterize the welded joints, including nugget grain size measurements at different locations through the thickness, micro-hardness indentation through nugget, thermo-mechanically affected zone (TMAZ), and heat affected zone (HAZ) at different cross section heights, and residual stress measurement using the cut compliance method with full thickness and partial thickness specimens. All testing results are consistent with the presence of a strong gradient in peak temperature through the plate thickness during FSW.

  9. Predicting tensile strength of friction stir welded AA6061 aluminium alloy joints by a mathematical model

    International Nuclear Information System (INIS)

    Elangovan, K.; Balasubramanian, V.; Babu, S.

    2009-01-01

    AA6061 aluminium alloy (Al-Mg-Si alloy) has gathered wide acceptance in the fabrication of light weight structures requiring a high strength-to weight ratio and good corrosion resistance. Compared to the fusion welding processes that are routinely used for joining structural aluminium alloys, friction stir welding (FSW) process is an emerging solid state joining process in which the material that is being welded does not melt and recast. This process uses a non-consumable tool to generate frictional heat in the abutting surfaces. The welding parameters such as tool rotational speed, welding speed, axial force etc., and tool pin profile play a major role in deciding the joint strength. An attempt has been made to develop a mathematical model to predict tensile strength of the friction stir welded AA6061 aluminium alloy by incorporating FSW process parameters. Four factors, five levels central composite design has been used to minimize number of experimental conditions. Response surface method (RSM) has been used to develop the model. Statistical tools such as analysis of variance (ANOVA), student's t-test, correlation co-efficient etc. have been used to validate the developed model. The developed mathematical model can be effectively used to predict the tensile strength of FSW joints at 95% confidence level

  10. Fatigue strength evaluation of friction stir welded aluminium joints using the nominal and notch stress concepts

    International Nuclear Information System (INIS)

    Barsoum, Z.; Khurshid, M.; Barsoum, I.

    2012-01-01

    Highlights: ► Fatigue testing and evaluation of friction stir welded butt and overlap joints. ► Evaluation based on nominal and effective notch stress concept. ► Comparison with different design recommendations and codes. ► Higher fatigue strength and SN-slopes is observed. ► New fatigue design recommendations proposed for FSW joints. -- Abstract: In this study the fatigue strength is investigated for Friction Stir Welded (FSW) overlap and butt welded joints in different thicknesses based on nominal and effective notch stress concepts. The fatigue test results are compared with fatigue strength recommendations according to EN 1999-1-3 and International Institute of Welding (IIW). The results are also compared with available published data and Finite Element Analysis (FEA) is carried out to investigate the effect of plate thickness and nugget size on the fatigue strength of overlap joints. 3–3 mm butt welded joints shows the highest fatigue strength in comparison with 3–5 mm butt welded and overlap joints. Slopes of the SN-curves for two different joint types differ from the slope recommended by IIW. A specific failure trend is observed in overlap FSW joints. However, the slopes of the SN-curves are in close agreement with slopes found in EN 1999-1-3. The slopes of various published results and test results presented in this study are in good agreement with each other. The suggested fatigue design curves for the nominal and effective notch stress concept have a higher slope than given for fusion welds by IIW.

  11. Analytical model of stress field in submerged arc welding butt joint with thorough penetration

    Directory of Open Access Journals (Sweden)

    Winczek Jerzy

    2018-01-01

    Full Text Available Analytical model of temporary and residual stresses for butt welding with thorough penetration was described assuming planar section hypothesis and using integral equations of stress equilibrium of the bar and simple Hooke’s law. In solution the effect of phase transformations (structure changes and structural strains has been taken into account. Phase transformations during heating are limited by temperature values at the beginning and at the end of austenitic transformation, depending on chemical composition of steel while the progress of phase transformations during cooling is determined on the basis of TTT-welding diagram. Temperature values at the beginning and at the end of transformation are conditioned by the speed of heating. Kinetics of diffusional transformation is described basing on Johnson-Mehl-Avrami-Kolmogorov equation, while martensitic transformation, basing on Koistinen-Marburger equation. Stresses in elasto-plastic state are determined by iteration, using elastic solutions method with changeable longitudinal modulus of elasticity, conditioned by stress-strain curve. Computations of stress field have been conducted for one-side butt welded of two steel flats made from S235 steel. It has enabled a clear interpretation of influence of temperature field and phase transformation on stresses caused by welding using Submerged Arc Welding (SAW method.

  12. Control of Precambrian basement deformation zones on emplacement of the Laramide Boulder batholith and Butte mining district, Montana, United States

    Science.gov (United States)

    Berger, Byron R.; Hildenbrand, Thomas G.; O'Neill, J. Michael

    2011-01-01

    parallel joints in the Butte Quartz Monzonite that, in turn, mimic Precambrian deformation fabrics found outside the district. The faults controlling the Butte veins are interpreted to have formed through activation under shear of preexisting northeast-striking joints as master faults from which splay faults formed along generally east-west and northwest joint plane orientations.

  13. Littered cigarette butts as a source of nicotine in urban waters

    Science.gov (United States)

    Roder Green, Amy L.; Putschew, Anke; Nehls, Thomas

    2014-11-01

    The effect of nicotine from littered cigarette butts on the quality of urban water resources has yet to be investigated. This two-part study addresses the spatial variation, seasonal dynamics and average residence time of littered cigarette butts in public space, as well as the release of nicotine from cigarette butts to run-off in urban areas during its residence time. Thereby, we tested two typical situations: release to standing water in a puddle and release during alternating rainfall and drying. The study took place in Berlin, Germany, a city which completely relies on its own water resources to meet its drinking water demand. Nine typical sites located in a central district, each divided into 20 plots were studied during five sampling periods between May 2012 and February 2013. The nicotine release from standardized cigarette butts prepared with a smoking machine was examined in batch and rainfall experiments. Littered cigarette butts are unevenly distributed among both sites and plots. The average butt concentration was 2.7 m-2 (SD = 0.6 m-2, N = 862); the maximum plot concentration was 48.8 butts m-2. This heterogeneity is caused by preferential littering (gastronomy, entrances, bus stops), redistribution processes such as litter removal (gastronomy, shop owners), and the increased accumulation in plots protected from mechanized street sweeping (tree pits, bicycle stands). No significant seasonal variation of cigarette butt accumulation was observed. On average, cigarette butt accumulation is characterized by a 6 days cadence due to the rhythm and effectiveness of street sweeping (mean weekly butt accumulation rate = 0.18 m-2 d-1; SD = 0.15 m-1). Once the butt is exposed to standing water, elution of nicotine occurs rapidly. Standardized butts released 7.3 mg g-1 nicotine in a batch experiment (equivalent to 2.5 mg L-1), 50% of which occurred within the first 27 min. In the rainfall experiment, the cumulative nicotine release from fifteen consecutive

  14. Sutter Buttes-the lone volcano in California's Great Valley

    Science.gov (United States)

    Hausback, Brain P.; Muffler, L.J. Patrick; Clynne, Michael A.

    2011-01-01

    The volcanic spires of the Sutter Buttes tower 2,000 feet above the farms and fields of California's Great Valley, just 50 miles north-northwest of Sacramento and 11 miles northwest of Yuba City. The only volcano within the valley, the Buttes consist of a central core of volcanic domes surrounded by a large apron of fragmental volcanic debris. Eruptions at the Sutter Buttes occurred in early Pleistocene time, 1.6 to 1.4 million years ago. The Sutter Buttes are not part of the Cascade Range of volcanoes to the north, but instead are related to the volcanoes in the Coast Ranges to the west in the vicinity of Clear Lake, Napa Valley, and Sonoma Valley.

  15. In-process monitoring and adaptive control for gap in micro butt welding with pulsed YAG laser

    International Nuclear Information System (INIS)

    Kawahito, Yousuke; Kito, Masayuki; Katayama, Seiji

    2007-01-01

    A gap is one of the most important issues to be solved in laser welding of a micro butt joint, because the gap results in welding defects such as underfilling or a non-bonded joint. In-process monitoring and adaptive control has been expected as one of the useful procedures for the stable production of sound laser welds without defects. The objective of this research is to evaluate the availability of in-process monitoring and adaptive control in micro butt welding of pure titanium rods with a pulsed neodymium : yttrium aluminium garnet (Nd : YAG) laser beam of a 150 μm spot diameter. It was revealed that a 45 μm narrow gap was detected by the remarkable jump in a reflected light intensity due to the formation of the molten pool which could bridge the gap. Heat radiation signal levels increased in proportion to the sizes of molten pools or penetration depths for the respective laser powers. As for adaptive control, the laser peak power was controlled on the basis of the reflected light or the heat radiation signals to stably produce a sound deeply penetrated weld reduced underfilling. In the case of a 100 μm gap, the underfilling was greatly reduced by half smaller than those made with a conventional rectangular pulse shape in seam welding as well as spot welding with a pulsed Nd : YAG laser beam. Consequently, the adaptive control of the laser peak power on the basis of in-process monitoring could reduce the harmful effects due to a gap in micro butt laser welding with a pulsed laser beam

  16. Analysing the Friction Stir Welded Joints of AA2219 Al-Cu Alloy in Different Heat-Treated-State

    Science.gov (United States)

    Venkateswarlu, D.; Cheepu, Muralimohan; Kranthi kumar, B.; Mahapatra, M. M.

    2018-03-01

    Aluminium alloy AA2219 is widely used in light weight structural applications where the good corrosion resistance and specific weight required. The fabrication of this alloy using friction stir welding process is gaining interest towards finding the characteristics of the weld metal properties, since this process involved in the welded materials does not melt and recast. In the present investigation, friction stir welding process was used for different heat treated conditions of 2219-T87 and 2219-T62 aluminium alloys to find the influence of base metal on characteristics of the joints. The experimental output results exhibited that, mechanical properties, weld metal characteristics and joint failure locations are significantly affected by the different heat treatment conditions of the substrate. The joints tensile and yield strength of the 2219-T87 welds was higher than the 2219-T62 welds. Hardness distribution in the stir zone was significantly varied between two different heat treaded material conditions. The microstructural features of the 2219-T62 welds reveal the coarse grains formation in the thermo-mechanically affected zone and heat affected zone. The joint efficiency of the 2219- T82 welds is 59.87%, while that of 2219-T62 welds is 39.10%. In addition, the elongation of the joint also varied and the joints failure location characteristics are different for two different types heat treated condition joints.

  17. Effect of the weld groove shape and pass number on residual stresses in butt-welded pipes

    International Nuclear Information System (INIS)

    Sattari-Far, I.; Farahani, M.R.

    2009-01-01

    This study used finite element techniques to analyze the thermo-mechanical behaviour and residual stresses in butt-welded pipes. The residual stresses were also measured in some welds by using the Hole-Drilling method. The results of the finite element analysis were compared with experimentally measured data to evaluate the accuracy of the finite element modelling. Based on this study, a finite element modelling procedure with reasonable accuracy was developed. The developed FE modelling was used to study the effects of weld groove shape and weld pass number on welding residual stresses in butt-welded pipes. The hoop and axial residual stresses in pipe joints of 6 and 10 mm thickness of different groove shapes and pass number were studied. It is shown that these two parameters may have significant effects on magnitude and distribution of residual stresses in welded pipes.

  18. Microstructure and Mechanical Characterization of a Dissimilar Friction-Stir-Welded CuCrZr/CuNiCrSi Butt Joint

    Directory of Open Access Journals (Sweden)

    Youqing Sun

    2018-05-01

    Full Text Available Dissimilar CuNiCrSi and CuCrZr butt joints were successfully frictionstirwelded at constant welding speed of 150 mm/min and rotational speed of 1400 rpm with the CuCrZr alloy or the CuNiCrSi alloy located on the advancing side (AS. The microstructure and mechanical properties of joints were investigated. When the CuCrZr alloy was located on the AS, the area of retreating material in the nugget zone was a little bigger. The Cr solute-rich particles were found in the nugget zone on CuCrZr side (CuCrZr-NZ while a larger density of solute-rich particles identified as the concentration of Cr and Si element was found in the nugget zone on CuNiCrSi side (CuNiCrSi-NZ. The Cr precipitates and δ-Ni2Si precipitates were found in the base metal on CuNiCrSi side (CuNiCrSi-BM but only Cr precipitates can be observed in the base metal on CuCrZr side (CuCrZr-BM. Precipitates were totally dissolved into Cu matrix in both CuCrZr-NZ and CuNiCrSi-NZ, which led to a sharp decrease in both micro-hardness and tensile strength from BM to NZ. When the CuNiCrSi was located on the AS, the tensile testing results showed the fracture occurred at the CuCrZr-NZ, while the fracture was found at the mixed zone of CuNiCrSi-NZ and CuCrZr-NZ for the other case.

  19. Experimental study on joining of AA6063 and AISI 1040 steel

    Science.gov (United States)

    Hynes, N. Rajesh Jesudoss; Raja, S.

    2018-05-01

    Feasibility of joining of dissimilar metals with different physical, chemical and thermal properties such as AA6063 alloy and AISI 1040 steel is worthwhile study, since it has tremendous applications in all most of all engineering domains. The mechanism of bonding is studied using scanning electron microscopy. Impact strength of AA2024/AISI joints, axial shortening distance, micro hardness distribution and joint strength are determined. Micro hardness profile shows increased hardness value at the joint interface, due to grain refinement.

  20. Butt pressure welding of wheels from vehicles consisting of steel and aluminium; Pressstumpfschweissen von Fahrzeugraedern aus Stahl und Aluminium

    Energy Technology Data Exchange (ETDEWEB)

    Grobelin, K. [Hess Engineering AG, Frauenfeld (Switzerland)

    2001-07-01

    Every year in Europe 35 million wheels for vehicles are produced. Most of them are wheels consisting of metal tapes, both of steel and of aluminium alloys. The manufacturing of wheels is explained, in detail the method known as DC upset welding used for butt joints of wheel-rims. The engaged machinery, the specials of welding various materials, the limits of the method, and the quality assurance are discussed. Advantages of the applied method are joints of first-class quality, high productivity, energy saving and environmental cleanness. (orig.)

  1. Wrought stainless steel butt-welding fittings: including reference to other corrosion resistant materials - approved 1971

    International Nuclear Information System (INIS)

    Anon.

    1975-01-01

    ANSI B16.9 is the American Standard for steel butt-welding fittings and although not so stated, it is implied that its scope deals primarily with the schedules of wall thicknesses which are common to carbon steel and the grades of alloy steel piping that are selected for pressure and temperature considerations. The purpose of this standard is to provide industry with a set of dimensional standards for butt-welding fittings that can be used with these light wall pipes of corrosion resisting materials. The center-to-end dimensions of all fittings are identical with those in ANSI B16.9 which give to industry the advantage of uniform design room practice and a maximum utilization of existing die equipment. The only departure from this is in the lap-joint stub end where for purposes of economy the face-to-end of the product has been reduced for use with thin wall piping

  2. Bali Cattle Carcass Characteristic of Different Butt Shape Condition

    Science.gov (United States)

    Hafid, H.; Nuraini; Inderawati; Kurniawan, W.

    2018-02-01

    Carcass was main product on cattle slaughtering which contain beef for human consumption and it has high nutritional and economical value. Carcass production on cattle has been influenced by several factors, such as cattle breed, feed, and body conformation. Cattle Butt Shape was one of part cattle body conformation which allegedly has have positive correlation on produced carcass. This research was aimed to evaluate Butt Shape condition influenced on Bali cattle carcass characteristic. The research was using Bali cattle which slaughter in Kendari Slaughtering House (Rumah Potong Hewan/RPH - Kendari). The observation includes weighing, and measuring parts of carcass was conducted on 60 heads of Halal process slaughtered Bali cattle which traditionally maintained. The research parameters were carcass productivity parameters i.e: slaughtering weight, carcass weight and length, leg length and circumstances. Obtained data were analyzed using Complete Randomized Design and post hoc analyzed using Least Significant Different if have any influence. The research result showed that cattle Butt Shape condition have significant (pBali cattle carcass productivity parameters. Butt shape with B category was result the best carcass productivity compare the others, while C category was better than D. It can be concluded that body and carcass weight were linearly influenced by cattle butt shape.

  3. Geographic patterns of cigarette butt waste in the urban environment.

    Science.gov (United States)

    Marah, Maacah; Novotny, Thomas E

    2011-05-01

    This reports the initial phase of a study to quantify the spatial pattern of cigarette butt waste in an urban environment. Geographic Information Systems (GIS) was used to create a weighted overlay analysis model which was then applied to the locations of businesses where cigarettes are sold or are likely to be consumed and venues where higher concentrations of butts may be deposited. The model's utility was tested using a small-scale litter audit in three zip codes of San Diego, California. We found that cigarette butt waste is highly concentrated around businesses where cigarettes are sold or consumed. The mean number of butts for predicted high waste sites was 38.1 (SD 18.87), for predicted low waste sites mean 4.8 (SD 5.9), psales and consumption. A GIS and weighted overlay model may be a useful tool in predicting urban locations of greater and lesser amounts of cigarette butt waste. These data can in turn be used to develop economic cost studies and plan mitigation strategies in urban communities.

  4. [Even cigarette butts can impact environment and health: preliminary considerations].

    Science.gov (United States)

    Martino, Gianrocco; Gorini, Giuseppe; Chellini, Elisabetta

    2013-01-01

    In Italy, every year about 72 billion of cigarette butts are thrown away in the environment. Cigarette butts represent 50% of the wastes of urban areas (parks, roads) in the world, and 40% of Mediterranean Sea wastes. In particular, total polluting load is constituted of 1,872 Bq millions of Polonium-210, assuming 75 mBq per cigarette butt, and 1,800 tons of volatile organic compounds. As a matter of fact, according to several surveys, cigarette butts are considered by smokers and non-smokers as a common and acceptable waste in the environment. In 2008, European Union issued a Directive on wastes considering the «extended producer responsibility» (i.e., every industry is liable for costs of collection, transport and disposal of its own products). In October 2012, the Italian Parliament proposed a bill that classifies cigarette butts as special wastes in the frame of this responsibility. It could be interesting in the future to follow the legislative process of that bill in the Italian Parliament in order to show how strong it will be supported.

  5. Geology of Gable Mountain-Gable Butte Area

    International Nuclear Information System (INIS)

    Fecht, K.R.

    1978-09-01

    Gable Mountain and Gable Butte are two ridges which form the only extensive outcrops of the Columbia River Basalt Group in the central portion of the Pasco Basin. The Saddle Mountains Basalt and two interbedded sedimentary units of the Ellensburg Formation crop out on the ridges. These include, from oldest to youngest, the Asotin Member (oldest), Esquatzel Member, Selah Interbed, Pomona Member, Rattlesnake Ridge Interbed, and Elephant Mountain Member (youngest). A fluvial plain composed of sediments from the Ringold and Hanford (informal) formations surrounds these ridges. The structure of Gable Mountain and Gable Butte is dominated by an east-west-trending major fold and northwest-southeast-trending parasitic folds. Two faults associated with the uplift of these structures were mapped on Gable Mountain. The geomorphic expression of the Gable Mountain-Gable Butte area resulted from the comlex folding and subsequent scouring by post-basalt fluvial systems

  6. Cold metal transfer spot plug welding of AA6061-T6-to-galvanized steel for automotive applications

    International Nuclear Information System (INIS)

    Cao, R.; Huang, Q.; Chen, J.H.; Wang, Pei-Chung

    2014-01-01

    Highlights: • Two Al-to-galvanized steel spot plug welding joints were studied by CMT method. • The optimum process variables for the two joints were gotten by orthogonal test. • Connection mechanism of the two joints were discussed. -- Abstract: In this study, cold metal transfer (CMT) spot plug joining of 1 mm thick Al AA6061-T6 to 1 mm thick galvanized steel (i.e., Q235) was studied. Welding variables were optimized for a plug weld in the center of a 25 mm overlap region with aluminum 4043 wire and 100% argon shielding gas. Microstructures and elemental distributions were characterized by scanning electron microscopy with energy dispersive X-ray spectrometer. Mechanical testing of CMT spot plug welded joints was conducted. It was found that it is feasible to join Al AA6061T6-to-galvanized steel by CMT spot plug welding method. The process variables for two joints with Al AA6061T6-to-galvanized mild steel and galvanized mild steel-to-Al AA6061T6 are optimized. The strength of CMT spot welded Al AA6061T6-to-galvanized mild steel is determined primarily by the strength and area of the brazed interface. While, the strength of the galvanized mild steel-to-Al AA6061T6 joint is mainly dependent upon the area of the weld metal

  7. The study on defects in aluminum 2219-T6 thick butt friction stir welds with the application of multiple non-destructive testing methods

    International Nuclear Information System (INIS)

    Li, Bo; Shen, Yifu; Hu, Weiye

    2011-01-01

    Research highlights: → Friction stir weld-defect forming mechanisms of thick butt-joints. → Relationship between weld-defects and friction stir welding process parameters. → Multiple non-destructive testing methods applied to friction stir welds. → Empirical criterion basing on mass-conservation for inner material-loss defects. → Nonlinear correlation between weld strengths and root-flaw lengths. -- Abstract: The present study focused on the relationship between primary friction stir welding process parameters and varied types of weld-defect discovered in aluminum 2219-T6 friction stir butt-welds of thick plates, meanwhile, the weld-defect forming mechanisms were investigated. Besides a series of optical metallographic examinations for friction stir butt welds, multiple non-destructive testing methods including X-ray detection, ultrasonic C-scan testing, ultrasonic phased array inspection and fluorescent penetrating fluid inspection were successfully used aiming to examine the shapes and existence locations of different weld-defects. In addition, precipitated Al 2 Cu phase coarsening particles were found around a 'kissing-bond' defect within the weld stirred nugget zone by means of scanning electron microscope and energy dispersive X-ray analysis. On the basis of volume conservation law in material plastic deformation, a simple empirical criterion for estimating the existence of inner material-loss defects was proposed. Defect-free butt joints were obtained after process optimization of friction stir welding for aluminum 2219-T6 plates in 17-20 mm thickness. Process experiments proved that besides of tool rotation speed and travel speed, more other appropriate process parameter variables played important roles at the formation of high-quality friction stir welds, such as tool-shoulder target depth, spindle tilt angle, and fixture clamping conditions on the work-pieces. Furthermore, the nonlinear correlation between weld tensile strengths and weld crack

  8. Special metallurgy - the electrical butt-welding by flashing of sintered magnesium-magnesium oxide composites (1963)

    International Nuclear Information System (INIS)

    Charleux, J.

    1963-01-01

    Electrical resistance welding has become quite important since World War II because of the need of a high yield in aeronautical production. Progress has been due in particular to the improvements made in electronically controlled apparatus making possible the automatic control of welding. For the butt-welding of sections requiring either a high production rate or a high quality weld, the flash butt-welding system has been very much developed these last few years. The use of this welding method is of great importance in the field of the bonding of oxidisable metals such as magnesium or aluminium and its alloys, because the welded joint is free from oxides. This study consists of general considerations on the flash-welding process with regard to temperature distribution in the parts during welding, and to electrical phenomena connected with flashing. Besides this general or theoretical section, we have applied the welding process to the bonding of sintered magnesium, a magnesium-magnesium oxide composite, whose use as a structural element in nuclear reactors is considered. (author) [fr

  9. Butt-welding technology for double walled Polyethylene pipe

    International Nuclear Information System (INIS)

    Lee, Bo-Young; Kim, Jae-Seong; Lee, Sang-Yul; Kim, Yeong K.

    2012-01-01

    Highlights: ► We developed a butt welding apparatus for doubled walled Polyethylene pipe. ► We design the welding process by analyzing thermal behaviors of the material. ► We performed the welding and tested the welded structural performances. ► We also applied the same technology to PVC pipes. ► We verified the butt welding was successful and effective for the pipes with irregular sections. -- Abstract: In this study, mechanical analyses of a butt welding technology for joining Polyethylene pipe are presented. The pipe had unique structure with double wall, and its section topology was not flat. For an effective repair of leakage and replacements of the pipe, the butt welding technology was developed and tested. For the material characterizations, thermodynamic analyses such as thermal gravimetric analysis and differential scanning calorimetry were performed. Based on the test results, the process temperature and time were determined to ensure safe joining of the pipes using a hot plate apparatus. The welding process was carefully monitored by measuring the temperature. Then, the joined pipes were tested by various methods to evaluate the quality. The analyses results showed the detail process mechanism during the joining process, and the test results demonstrated the successful application of the technology to the sewage pipe repairs.

  10. Gap Width Study and Fixture Design in Laser Butt-Welding

    DEFF Research Database (Denmark)

    Gong, Hui; Olsen, Flemming Ove

    .5-2.0 m/min, the laser power : 2 and 2.6 kW and the focal point position : 0 and -1.2 mm. Quality of all the butt welds are destructively tested according to ISO 13919-1.Influences of the variable process parameters to the maximum allowable gap width are observed as (1) the maximum gap width is inversely......This paper discusses some practical consideration for design of a mechanical fixture, which enables to accurately measure the width of a gap between two stainless steel workpieces and to steadfastly clamp the workpieces for butt-welding with a high power CO2 laser.With such a fixture, a series...... of butt-welding experiment is successfully carried out in order to find the maximum allowable gap width in laser butt-welding. The gap width study (GWS) is performed on the material of SST of W1.4401 (AISI 316) under various welding conditions, which are the gap width : 0.00-0.50 mm, the welding speed : 0...

  11. Modeling of AA5083 Material-Microstructure Evolution During Butt Friction-Stir Welding

    Science.gov (United States)

    Grujicic, M.; Arakere, G.; Yalavarthy, H. V.; He, T.; Yen, C.-F.; Cheeseman, B. A.

    2010-07-01

    A concise yet a fairly comprehensive overview of the friction stir welding (FSW) process is provided. This is followed by a computational investigation in which FSW behavior of a prototypical solution-strengthened and strain-hardened aluminum alloy, AA5083-H131, is modeled using a fully coupled thermo-mechanical finite-element procedure developed in our prior study. Particular attention is given to proper modeling of the welding work-piece material behavior during the FSW process. Specifically, competition and interactions between plastic-deformation and dynamic-recrystallization processes are considered to properly account for the material-microstructure evolution in the weld nugget zone. The results showed that with proper modeling of the material behavior under high-temperature/severe-plastic-deformation conditions, significantly improved agreement can be attained between the computed and measured post-FSW residual-stress and material-strength distribution results.

  12. Equipment for Preparing Pipeline Position Butts for Welding

    Directory of Open Access Journals (Sweden)

    Lobanov L.M.

    2015-09-01

    Full Text Available The results of developments of the Ye.O.Paton Electric Welding Institute and its specialized departments on the designing national equipment models for preparation during the assembly the edges and butt ends of pipeline position butts with the diameter from 14 up to 159 mm, repair and modernization of power engineering objects, including the power units of nuclear and heat electric stations, in chemical and machine building, at enterprises of oil-gas complex and other branches of industry are presented.

  13. A Study on the Saving Method of Plate Jigs in Hull Block Butt Welding

    Science.gov (United States)

    Ko, Dae-Eun

    2017-11-01

    A large amount of plate jigs is used for alignment of welding line and control of welding deformations in hull block assembly stage. Besides material cost, the huge working man-hours required for working process of plate jigs is one of the obstacles in productivity growth of shipyard. In this study, analysis method was proposed to simulate the welding deformations of block butt joint with plate jigs setting. Using the proposed analysis method, an example simulation was performed for actual panel block joint to investigate the saving method of plate jigs. Results show that it is possible to achieve two objectives of quality accuracy of the hull block and saving the plate jig usage at the same time by deploying the plate jigs at the right places. And the proposed analysis method can be used in establishing guidelines for the proper use of plate jigs in block assembly stage.

  14. Characterization of lap joints laser beam welding of thin AA 2024 sheets with Yb:YAG disk-laser

    Science.gov (United States)

    Caiazzo, Fabrizia; Alfieri, Vittorio; Cardaropoli, Francesco; Sergi, Vincenzo

    2012-06-01

    Lap joints obtained by overlapping two plates are widely diffused in aerospace industry. Nevertheless, because of natural aging, adhesively bonded and riveted aircraft lap joints may be affected by cracks from rivets, voids or corrosion. Friction stir welding has been proposed as a valid alternative, although large heat affected zones are produced both in the top and the bottom plate due to the pin diameter. Interest has therefore been shown in studying laser lap welding as the laser beam has been proved to be competitive since it allows to concentrate the thermal input and increases productivity and quality. Some challenges arise as a consequence of aluminum low absorptance and high thermal conductivity; furthermore, issues are due to metallurgical challenges such as both micro and macro porosity formation and softening in the fused zone. Welding of AA 2024 thin sheets in a lap joint configuration is discussed in this paper: tests are carried out using a recently developed Trumpf TruDisk 2002 Yb:YAG disk-laser with high beam quality which allows to produce beads with low plates distortion and better penetration. The influence of the processing parameters is discussed considering the fused zone extent and the bead shape. The porosity content as well as the morphological features of the beads have been examined.

  15. 75 FR 53714 - Stainless Steel Butt-Weld Pipe Fittings From Japan, Korea, and Taiwan

    Science.gov (United States)

    2010-09-01

    ...)] Stainless Steel Butt-Weld Pipe Fittings From Japan, Korea, and Taiwan AGENCY: United States International... stainless steel butt-weld pipe fittings from Japan, Korea, and Taiwan. SUMMARY: The Commission hereby gives... butt-weld pipe fittings from Japan, Korea, and Taiwan would be likely to lead to continuation or...

  16. The Effect of Tool Profiles on Mechanical Properties of Friction Stir Welded Al5052 T-Joints.

    Science.gov (United States)

    Kim, Byeong-Jin; Bang, Hee-Seon; Bang, Han-Sur

    2018-03-01

    Al5052 T butt joints with two skins (5 mm) and one stringer (3 mm) has been successfully welded by friction stir welding (FSW). Notably, this paper has been investigated the effect of tool shape on welded formation mechanism and mechanical properties. The used shapes of tool pin are two types which are cylinder (type 1) and frustum (type 2). Dimension on two types of tool pin shape is respectively pin length of 4.7 mm and pin diameter of frustum type of top (5 mm) and bottom (3 mm). The results of experiment show that inner defects in FSWed T-joints increase significantly in accordance with traverse speed. The maximum tensile strength of welded joint fabricated using type 1 is equivalent to 85% that of the base metal, which is approximately 10% higher than that of type 2. Because welded joint of type 1 has more smoothly plastic flow in comparison with type 2. Consequently, the results show that type 1 is better appropriate for friction stir welded Al5052 T butt joints than type 2.

  17. Prediction of shear and tensile strength of the diffusion bonded AA5083 and AA7075 aluminium alloy using ANN

    International Nuclear Information System (INIS)

    Sagai Francis Britto, A.; Raj, R. Edwin; Mabel, M. Carolin

    2017-01-01

    Diffusion bonding is a pressure welding technique to establish bonds by inter diffusion of atoms. Bonding characteristics were generated by varying the significant process conditions such as the bonding temperature, the pressing load and the duration of pressure while bonding the aluminium alloys AA5083 and AA7075. Deriving analytical correlation with the process variables to weld strength is quite involved due to the non-linear dependency of the process variables with the mechanical strength of the joints. An arbitrary function approximation mechanism, the artificial neural network (ANN) is therefore employed to develop the models for predicting the mechanical properties of the bonded joints. Back propagation technique, which alters the network weights to minimize the mean square error was used to develop the ANN models. The models were tested, validated and found to be satisfactory with good prediction accuracy.

  18. Prediction of shear and tensile strength of the diffusion bonded AA5083 and AA7075 aluminium alloy using ANN

    Energy Technology Data Exchange (ETDEWEB)

    Sagai Francis Britto, A. [Department of Mechanical Engineering, St.Xavier' s Catholic College of Engineering, Nagercoil 629003,Tamil Nadu (India); Raj, R. Edwin, E-mail: redwinraj@gmail.com [Department of Mechanical Engineering, St.Xavier' s Catholic College of Engineering, Nagercoil 629003,Tamil Nadu (India); Mabel, M. Carolin [Department of Electrical and Electronics Engineering, St.Xavier' s Catholic College of Engineering, Nagercoil 629003,Tamil Nadu (India)

    2017-04-24

    Diffusion bonding is a pressure welding technique to establish bonds by inter diffusion of atoms. Bonding characteristics were generated by varying the significant process conditions such as the bonding temperature, the pressing load and the duration of pressure while bonding the aluminium alloys AA5083 and AA7075. Deriving analytical correlation with the process variables to weld strength is quite involved due to the non-linear dependency of the process variables with the mechanical strength of the joints. An arbitrary function approximation mechanism, the artificial neural network (ANN) is therefore employed to develop the models for predicting the mechanical properties of the bonded joints. Back propagation technique, which alters the network weights to minimize the mean square error was used to develop the ANN models. The models were tested, validated and found to be satisfactory with good prediction accuracy.

  19. Dissimilar friction stir welds in AA5083-AA6082: The effect of process parameters on residual stress

    International Nuclear Information System (INIS)

    Steuwer, A.; Peel, M.J.; Withers, P.J.

    2006-01-01

    The effect of tool traverse and rotation speeds on the residual stresses are quantified for welds between non-age-hardening AA5083 and age-hardening AA6082 and compared to single alloy joints made from each of the two constituents. The residual stresses have been characterised non-destructively by neutron diffraction and synchrotron X-ray diffraction. The region around the weld line was characterised by significant tensile residual stress fields which are balanced by compressive stresses in the parent material. The rotation speed of the tool has been found to have a substantially greater influence than the transverse speed on the properties and residual stresses in the welds, particularly on the AA5083 side where the location of the peak stress moves from the stir zone to beyond the edge of the tool shoulder. The changes in residual stress are related to microstructural and hardness changes as determined in a previous study . In particular the larger stresses under the weld tool on the AA5083 side compared to the AA6082 side are related to a transient reduction in yield stress due to dissolution of the hardening precipitates during welding prior to natural aging after welding

  20. Regulating the disposal of cigarette butts as toxic hazardous waste.

    Science.gov (United States)

    Barnes, Richard L

    2011-05-01

    The trillions of cigarette butts generated each year throughout the world pose a significant challenge for disposal regulations, primarily because there are millions of points of disposal, along with the necessity to segregate, collect and dispose of the butts in a safe manner, and cigarette butts are toxic, hazardous waste. There are some hazardous waste laws, such as those covering used tyres and automobile batteries, in which the retailer is responsible for the proper disposal of the waste, but most post-consumer waste disposal is the responsibility of the consumer. Concepts such as extended producer responsibility (EPR) are being used for some post-consumer waste to pass the responsibility and cost for recycling or disposal to the manufacturer of the product. In total, 32 states in the US have passed EPR laws covering auto switches, batteries, carpet, cell phones, electronics, fluorescent lighting, mercury thermostats, paint and pesticide containers, and these could be models for cigarette waste legislation. A broader concept of producer stewardship includes EPR, but adds the consumer and the retailer into the regulation. The State of Maine considered a comprehensive product stewardship law in 2010 that is a much better model than EPR. By using either EPR or the Maine model, the tobacco industry will be required to cover the cost of collecting and disposing of cigarette butt waste. Additional requirements included in the Maine model are needed for consumers and businesses to complete the network that will be necessary to maximise the segregation and collection of cigarette butts to protect the environment.

  1. 77 FR 42697 - Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines: Continuation...

    Science.gov (United States)

    2012-07-20

    ...] Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines: Continuation of... from Italy, Malaysia, and the Philippines.\\2\\ \\1\\ See Antidumping Duty Orders: Stainless Steel Butt...), titled Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines (Investigation...

  2. 2018-04-22T12:30:44Z https://www.ajol.info/index.php/all/oai oai:ojs ...

    African Journals Online (AJOL)

    Other complications were chronic joint dislocation, ankylosis, joint stiffness, arthrosis/arthritis, chronic osteomyelitis, Volkmann's ischaemic contracture, osteonecrosis, neuropathy, limb gangrene, delayed union and pressure ulcer. The most frequent intervention was open reduction and internal fixation (60.56%) and most of ...

  3. Influence of energy input in friction stir welding on structure evolution and mechanical behaviour of precipitation-hardening in aluminium alloys (AA2024-T351, AA6013-T6 and Al-Mg-Sc)

    Energy Technology Data Exchange (ETDEWEB)

    Weis Olea, Cesar Afonso [GKSS-Forschungszentrum Geesthacht GmbH (Germany). Inst. fuer Werkstofforschung

    2008-12-04

    Aluminium alloys AA2024 T351, AA6013 T6 and the recently developed Al-Mg-Sc for aircraft industry applications, which are usually considered difficult to weld by conventional fusion welding processes, demonstrate outstanding performance when joined by friction stir welding (FSW). The main feature of the process is to produce solid-state welds, where the maximum temperatures attained during the process are about 80 % that of the melting temperature of the base material. The process generates substantial plastic deformation, due to the solid-state stirring, and consequently creates a high dislocation density, which is a precursor to dynamic recrystallization, a metallurgical feature that characterizes the stir zone (weld centre). A relevant aspect considered, regarding precipitation-hardening aluminium alloys, is the deterioration of the mechanical properties in the weld zones, which are fundamentally attributed to changes in the characteristics of strengthening precipitates. Among the strengthening mechanisms acting in these aluminium alloys, the most important is basically dependent on the morphology, size and population of the precipitates. The thermal cycle and deformation generated during the FSW process alter the precipitation characteristics previously present in the base material. FSW input energy regulates the magnitude of the thermal cycle and the intensity of deformation taking place during the process, and it can be controlled by the welding parameters, affecting the precipitates evolution and consequently the mechanical properties of the joint. Nevertheless, there remains a lack of knowledge about the substructural evolution of these alloys during FSW, and its correlation with weld energy input and their respective mechanical properties, particularly for the Al-Mg-Sc alloy. The main objective of this work is to explain the micro and substructural evolution (emphasizing precipitates evolution) of AA2024- T351, AA6013-T6 and Al-Mg-Sc alloys in similar

  4. Very High Cycle Fatigue Crack Initiation Mechanism in Nugget Zone of AA 7075 Friction Stir Welded Joint

    Directory of Open Access Journals (Sweden)

    Chao He

    2017-01-01

    Full Text Available Very high cycle fatigue behavior of nugget zone in AA 7075 friction stir welded joint was experimentally investigated using ultrasonic fatigue testing system (20 kHz to clarify the crack initiation mechanism. It was found that the fatigue strength of nugget zone decreased continuously even beyond 107 cycles with no traditional fatigue limits. Fatigue cracks initiated from the welding defects located at the bottom side of the friction stir weld. Moreover, a special semicircular zone could be characterized around the crack initiation site, of which the stress intensity factor approximately equaled the threshold of fatigue crack propagation rate. Finally, a simplified model was proposed to estimate the fatigue life by correlating the welding defect size and applied stress. The predicted results are in good agreement with the experimental results.

  5. Metallurgical Effects of Shunting Current on Resistance Spot-Welded Joints of AA2219 Sheets

    Science.gov (United States)

    Jafari Vardanjani, M.; Araee, A.; Senkara, J.; Jakubowski, J.; Godek, J.

    2016-08-01

    Shunting effect is the loss of electrical current via the secondary circuit provided due to the existence of previous nugget in a series of welding spots. This phenomenon influences on metallurgical aspects of resistance spot-welded (RSW) joints in terms of quality and performance. In this paper RSW joints of AA2219 sheets with 1 mm thickness are investigated metallurgically for shunted and single spots. An electro-thermal finite element analysis is performed on the RSW process of shunted spot and temperature distribution and variation are obtained. These predictions are then compared with experimental micrographs. Three values of 5 mm, 20 mm, and infinite (i.e., single spot) are assumed for welding distance. Numerical and experimental results are matching each other in terms of nugget and HAZ geometry as increasing distance raised nugget size and symmetry of HAZ. In addition, important effect of shunting current on nugget thickness, microstructure, and Copper segregation on HAZ grain boundaries were discovered. A quantitative analysis is also performed about the influence of welding distance on important properties including ratio of nugget thickness and diameter ( r t), ratio of HAZ area on shunted and free side of nugget ( r HA), and ratio of equivalent segregated and total amount of Copper, measured in sample ( r Cu) on HAZ. Increasing distance from 5 mm to infinite, indicated a gain of 111.04, -45.55, and -75.15% in r t, r HA, and r Cu, respectively, while obtained ratios for 20 mm welding distance was suitable compared to single spot.

  6. Radio and television use in Butte County, California: application to fire prevention

    Science.gov (United States)

    William S. Folkman

    1975-01-01

    A sample of Butte County residents were interviewed about their radio and television use habits. Their responses were analyzed in terms of demographic, social, and economic characteristics. The findings can be used in developing more effective fire prevention programs. Most people in Butte County listen to the radio or watch television but they differ widely in the way...

  7. STUDY AND ANALYSIS OF THE EFFECT OF WELDING PROCESS ON DISTORTION WITH 304L STAINLESS STEEL WELD JOINTS

    OpenAIRE

    Dhananjay Kumar*, Dharamvir mangal

    2017-01-01

    The effect of welding process on the distortion with 304L stainless steel 12thk weld joints made by TIG (tungsten inert gas) and SMAW (Shielded metal arc welding) welding process involving different type joint configuration have been studied. The joint configurations employed were double V-groove edge preparation for double side SMAW welding and square – butt preparation for double side TIG welding. All weld joints passed by radiographic. Distortion measurements were carried out using height ...

  8. 77 FR 14002 - Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines: Final Results...

    Science.gov (United States)

    2012-03-08

    ...] Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines: Final Results of the... Duty Orders on Stainless Steel Butt-Weld Pipe Fittings from Italy, Malaysia, and the Philippines'' from... Commerce (the Department) initiated sunset reviews of the antidumping duty orders on stainless steel butt...

  9. The effect of welding parameters on surface quality of AA6351 aluminium alloy

    International Nuclear Information System (INIS)

    Yacob, S; Ariffin, N; Ali, R; Arshad, A; Wahab, M I A; Ismail, S A; Roji, NS M; Din, W B W; Zakaria, M H; Abdullah, A; Yusof, M I; Kamarulzaman, K Z; Mahyuddin, A; Hamzah, M N; Roslan, R; MAli, M A; Ahsan, Q

    2015-01-01

    In the present work, the effects of gas metal arc welding-cold metal transfer (GMAW-CMT) parameters on surface roughness are experimentally assessed. The purpose of this study is to develop a better understanding of the effects of welding speed, material thickness and contact tip to work distance on the surface roughness. Experiments are conducted using single pass gas metal arc welding-cold metal transfer (GMAW-CMT) welding technique to join the material. The material used in this experiment was AA6351 aluminum alloy with the thickness of 5mm and 6mm. A Mahr Marsuft XR 20 machine was used to measure the average roughness (Ra) of AA6351 joints. The main and interaction effect analysis was carried out to identify process parameters that affect the surface roughness. The results show that all the input process parameters affect the surface roughness of AA6351 joints. Additionally, the average roughness (Ra) results also show a decreasing trend with increased of welding speed. It is proven that gas metal arc welding-cold metal transfer (GMAW-CMT)welding process has been successful in term of providing weld joint of good surface quality for AA6351 based on the low value surface roughness condition obtained in this setup. The outcome of this experimental shall be valuable for future fabrication process in order to obtained high good quality weld. (paper)

  10. Dormaier and Chester Butte 2007 Follow-up Habitat Evaluation Procedures Report.

    Energy Technology Data Exchange (ETDEWEB)

    Ashley, Paul R.

    2008-01-01

    Follow-up habitat evaluation procedures (HEP) analyses were conducted on the Dormaier and Chester Butte wildlife mitigation sites in April 2007 to determine the number of additional habitat units to credit Bonneville Power Administration (BPA) for providing funds to enhance, and maintain the project sites as partial mitigation for habitat losses associated with construction of Grand Coulee Dam. The Dormaier follow-up HEP survey generated 482.92 habitat units (HU) or 1.51 HUs per acre for an increase of 34.92 HUs over baseline credits. Likewise, 2,949.06 HUs (1.45 HUs/acre) were generated from the Chester Butte follow-up HEP analysis for an increase of 1,511.29 habitat units above baseline survey results. Combined, BPA will be credited with an additional 1,546.21 follow-up habitat units from the Dormaier and Chester Butte parcels.

  11. 76 FR 67473 - Stainless Steel Butt-Weld Pipe Fittings from Italy, Malaysia, and The Philippines; Institution of...

    Science.gov (United States)

    2011-11-01

    ... Concerning the Antidumping Duty Orders on Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and... stainless steel butt-weld pipe fittings from Italy, Malaysia, and the Philippines would be likely to lead to... antidumping duty orders on imports of stainless steel butt-weld pipe fittings from Italy, Malaysia, and the...

  12. GAP WIDTH STUDY IN LASER BUTT-WELDING

    DEFF Research Database (Denmark)

    Gong, Hui; Olsen, Flemming Ove

    power : 2 and 2.6 kW and the focal point position : 0 and -1.2 mm. Quality of all the butt welds are destructively tested according to ISO 13919-1.Influences of the variable process parameters to the maximum allowable gap width are observed as (1) the maximum gap width is inversely related......In this paper the maximum allowable gap width in laser butt-welding is intensively studied. The gap width study (GWS) is performed on the material of SST of W1.4401 (AISI 316) under various welding conditions, which are the gap width : 0.00-0.50 mm, the welding speed : 0.5-2.0 m/min, the laser...... to the welding speed, (2) the larger laser power leads to the bigger maximum allowable gap width and (3) the focal point position has very little influence on the maximum gap width....

  13. Effect of pulsed current welding on fatigue behaviour of high strength aluminium alloy joints

    International Nuclear Information System (INIS)

    Balasubramanian, V.; Ravisankar, V.; Madhusudhan Reddy, G.

    2008-01-01

    High strength aluminium alloys (Al-Zn-Mg-Cu alloys) have gathered wide acceptance in the fabrication of light weight structures requiring high strength-to weight ratio, such as transportable bridge girders, military vehicles, road tankers and railway transport systems. The preferred welding processes of high strength aluminium alloy are frequently gas tungsten arc welding (GTAW) process and gas metal arc welding (GMAW) process due to their comparatively easier applicability and better economy. Weld fusion zones typically exhibit coarse columnar grains because of the prevailing thermal conditions during weld metal solidification. This often results inferior weld mechanical properties and poor resistance to hot cracking. In this investigation, an attempt has been made to refine the fusion zone grains by applying pulsed current welding technique. Rolled plates of 6 mm thickness have been used as the base material for preparing single pass welded joints. Single V butt joint configuration has been prepared for joining the plates. The filler metal used for joining the plates is AA 5356 (Al-5Mg (wt%)) grade aluminium alloy. Four different welding techniques have been used to fabricate the joints and they are: (i) continuous current GTAW (CCGTAW), (ii) pulsed current GTAW (PCGTAW), (iii) continuous current GMAW (CCGMAW) and (iv) pulsed current GMAW (PCGMAW) processes. Argon (99.99% pure) has been used as the shielding gas. Fatigue properties of the welded joints have been evaluated by conducting fatigue test using rotary bending fatigue testing machine. Current pulsing leads to relatively finer and more equi-axed grain structure in gas tungsten arc (GTA) and gas metal arc (GMA) welds. In contrast, conventional continuous current welding resulted in predominantly columnar grain structures. Grain refinement is accompanied by an increase in fatigue life and endurance limit

  14. 46 CFR 56.30-10 - Flanged joints (modifies 104.5.1(a)).

    Science.gov (United States)

    2010-10-01

    ... 104.5.1(a)). (a) Flanged or butt-welded joints are required for Classes I and I-L piping for nominal... Marine Safety Center. Pressure temperature ratings of the appropriate ANSI/ASME standard must not be... service pressure-temperature ratings for flanges of class 300 and lower, within the temperature...

  15. Explosive Cladding of Titanium and Aluminium Alloys on the Example of Ti6Al4V-AA2519 Joints / Wybuchowe Platerowanie Stopów Tytanu I Aluminium Na Przykładzie Połączenia Ti6Al4V-AA2519

    Directory of Open Access Journals (Sweden)

    Gałka A.

    2015-12-01

    Full Text Available Explosive cladding is currently one of the basic technologies of joining metals and their alloys. It enables manufacturing of the widest range of joints and in many cases there is no alternative solution. An example of such materials are clads that include light metals such as titanium and aluminum. ach new material combination requires an appropriate adaptation of the technology by choosing adequate explosives and tuning other cladding parameters. Technology enabling explosive cladding of Ti6Al4V titanium alloy and aluminum AA2519 was developed. The clads were tested by means of destructive and nondestructive testing, analyzing integrity, strength and quality of the obtained joint.

  16. Quantitative TEM study of the precipitation microstructure in aluminium alloy Al(MgSiCu) 6056 T6

    International Nuclear Information System (INIS)

    Delmas, F.; Casanove, M.J.; Lours, P.; Couret, A.; Coujou, A.

    2004-01-01

    The precipitate microstructure in the last-generation aluminium alloy 6056 T6 [AlMgSiCu] is investigated using three complementary techniques of transmission electron microscopy (TEM) with a special focus on the density and volume fraction of strengthening particles. High-resolution TEM allows the identification of the precipitates and the measurement of the precipitate sizes to be performed. Conventional TEM is used to evaluate the number of precipitates in the investigated area as well as their distribution in the matrix. In situ TEM straining, via the analysis of the dislocation slip traces, permits to determine precisely the thickness and the volume of the foil in the region where the precipitates are analysed. Taking into account the shape and the dimensions of precipitates with respect to the foil thickness, a novel methodology for measuring the volume density and the volume fraction of precipitates is proposed

  17. Methodic recommendations on ultrasonic testing of pipeline austenitic butt joints

    International Nuclear Information System (INIS)

    Grebennik, V.S.; Lantukh, V.M.; Tajts, M.Z.; Ermolov, I.N.; Volkov, A.S.; Vyatskov, I.A.; Kesler, N.A.; Shchedrin, I.F.

    1989-01-01

    Recommendations for the application of ultrasonic testing of austenitic welded joints of the Du 500 pipelines with the walls 32-34 mm thick made of steel Kh18N10T are developed. The optimal values of the main parameters of ultrasonic testing are determined experimentally. Principles of calculation of the optimal parameters are considered. 1 ref.; 4 figs

  18. Optimal design for laser beam butt welding process parameter using artificial neural networks and genetic algorithm for super austenitic stainless steel

    Science.gov (United States)

    Sathiya, P.; Panneerselvam, K.; Soundararajan, R.

    2012-09-01

    Laser welding input parameters play a very significant role in determining the quality of a weld joint. The joint quality can be defined in terms of properties such as weld bead geometry, mechanical properties and distortion. Therefore, mechanical properties should be controlled to obtain good welded joints. In this study, the weld bead geometry such as depth of penetration (DP), bead width (BW) and tensile strength (TS) of the laser welded butt joints made of AISI 904L super austenitic stainless steel were investigated. Full factorial design was used to carry out the experimental design. Artificial Neural networks (ANN) program was developed in MatLab software to establish the relationships between the laser welding input parameters like beam power, travel speed and focal position and the three responses DP, BW and TS in three different shielding gases (Argon, Helium and Nitrogen). The established models were used for optimizing the process parameters using Genetic Algorithm (GA). Optimum solutions for the three different gases and their respective responses were obtained. Confirmation experiment has also been conducted to validate the optimized parameters obtained from GA.

  19. 75 FR 76025 - Stainless Steel Butt-Weld Pipe Fittings From Japan, Korea, and Taiwan

    Science.gov (United States)

    2010-12-07

    ... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 731-TA-376 and 563-564 (Third Review)] Stainless Steel Butt-Weld Pipe Fittings From Japan, Korea, and Taiwan AGENCY: United States International... steel butt-weld pipe fittings from Japan, Korea, and Taiwan would be likely to lead to continuation or...

  20. MECHANICAL PROPERTIES COMPARISON OF FRICTION STIR WELDING BUTT JOINTS OF AA1100 MADE IN A CONVENTIONAL MILLING MACHINE AND A FSW MACHINE

    Directory of Open Access Journals (Sweden)

    JULIO ZAPATA

    2013-01-01

    Full Text Available En este trabajo se comparan las propiedades mecánicas de juntas a tope de una aleación de Aluminio AA1100 obtenidas por soldadura por fricción agitación en una máquina fresadora convencional y en una máquina especializada para este proceso. Para la obtención de las juntas en ambos equipos se usó la misma geometría de herramienta y parámetros de soldadura. La fresadora convencional se adaptó para asegurar control de la penetración durante la soldadura y la máquina especializada se operó bajo los modos de control de fuerza y de penetración. Las propiedades mecánicas de los cordones se evaluaron mediante ensayos de tracción y microdureza. Los defectos generados en las juntas se caracterizaron usando microscopía óptica y electrónica de barrido. Los resultados mostraron que las propiedades mecánicas fueron altamente afectadas por los parámetros del proceso mientras que el tipo de máquina influenció la presencia de defectos en las juntas. Finalmente, se encontró que las propiedades a tracción fueron más apropiadas para comparar los resultados entre los diferentes grupos de parámetros y el nivel de defectos que los barridos de dureza. Se obtuvieron mayores propiedades mecánicas y menor nivel de defectos en la máquina especializada para soldadura por fricción agitación bajo el modo de control de penetración, obteniéndose una resistencia a la tracción alrededor de 130MPa, mientras que el mayor valor obtenido en la fresadora convencional fue de 109 MPa.

  1. 78 FR 21582 - Revisions to the California State Implementation Plan, Butte County Air Quality Management...

    Science.gov (United States)

    2013-04-11

    ... the California State Implementation Plan, Butte County Air Quality Management District and Sacramento Metropolitan Air Quality Management District AGENCY: Environmental Protection Agency (EPA). ACTION: Proposed rule. SUMMARY: EPA is proposing to approve revisions to the Butte County Air Quality Management...

  2. Cigarettes butts and the case for an environmental policy on hazardous cigarette waste.

    Science.gov (United States)

    Novotny, Thomas E; Lum, Kristen; Smith, Elizabeth; Wang, Vivian; Barnes, Richard

    2009-05-01

    Discarded cigarette butts are a form of non-biodegradable litter. Carried as runoff from streets to drains, to rivers, and ultimately to the ocean and its beaches, cigarette filters are the single most collected item in international beach cleanups each year. They are an environmental blight on streets, sidewalks, and other open areas. Rather than being a protective health device, cigarette filters are primarily a marketing tool to help sell 'safe' cigarettes. They are perceived by much of the public (especially current smokers) to reduce the health risks of smoking through technology. Filters have reduced the machine-measured yield of tar and nicotine from burning cigarettes, but there is controversy as to whether this has correspondingly reduced the disease burden of smoking to the population. Filters actually may serve to sustain smoking by making it seem less urgent for smokers to quit and easier for children to initiate smoking because of reduced irritation from early experimentation. Several options are available to reduce the environmental impact of cigarette butt waste, including developing biodegradable filters, increasing fines and penalties for littering butts, monetary deposits on filters, increasing availability of butt receptacles, and expanded public education. It may even be possible to ban the sale of filtered cigarettes altogether on the basis of their adverse environmental impact. This option may be attractive in coastal regions where beaches accumulate butt waste and where smoking indoors is increasingly prohibited. Additional research is needed on the various policy options, including behavioral research on the impact of banning the sale of filtered cigarettes altogether.

  3. Cigarettes Butts and the Case for an Environmental Policy on Hazardous Cigarette Waste

    Directory of Open Access Journals (Sweden)

    Richard Barnes

    2009-05-01

    Full Text Available Discarded cigarette butts are a form of non-biodegradable litter. Carried as runoff from streets to drains, to rivers, and ultimately to the ocean and its beaches, cigarette filters are the single most collected item in international beach cleanups each year. They are an environmental blight on streets, sidewalks, and other open areas. Rather than being a protective health device, cigarette filters are primarily a marketing tool to help sell ‘safe’ cigarettes. They are perceived by much of the public (especially current smokers to reduce the health risks of smoking through technology. Filters have reduced the machine-measured yield of tar and nicotine from burning cigarettes, but there is controversy as to whether this has correspondingly reduced the disease burden of smoking to the population. Filters actually may serve to sustain smoking by making it seem less urgent for smokers to quit and easier for children to initiate smoking because of reduced irritation from early experimentation. Several options are available to reduce the environmental impact of cigarette butt waste, including developing biodegradable filters, increasing fines and penalties for littering butts, monetary deposits on filters, increasing availability of butt receptacles, and expanded public education. It may even be possible to ban the sale of filtered cigarettes altogether on the basis of their adverse environmental impact. This option may be attractive in coastal regions where beaches accumulate butt waste and where smoking indoors is increasingly prohibited. Additional research is needed on the various policy options, including behavioral research on the impact of banning the sale of filtered cigarettes altogether.

  4. 77 FR 39735 - Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines

    Science.gov (United States)

    2012-07-05

    ... revocation of the antidumping duty orders on stainless steel butt-weld pipe fittings From Italy, Malaysia... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 731-TA-865-867 (Second Review)] Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines Determination On the basis of the...

  5. The Effect of Interlayer Materials on the Joint Properties of Diffusion-Bonded Aluminium and Magnesium

    Directory of Open Access Journals (Sweden)

    Stefan Habisch

    2018-02-01

    Full Text Available Diffusion bonding is a well-known technology for a wide range of advanced joining applications, due to the possibility of bonding different materials within a defined temperature-time-contact pressure regime in solid state. For this study, aluminium alloys AA 6060, AA 6082, AA 7020, AA 7075 and magnesium alloy AZ 31 B are used to produce dissimilar metal joints. Titanium and silver were investigated as interlayer materials. SEM and EDXS-analysis, micro-hardness measurements and tensile testing were carried out to examine the influence of the interlayers on the diffusion zone microstructures and to characterize the joint properties. The results showed that the highest joint strength of 48 N/mm2 was reached using an aluminium alloy of the 6000 series with a titanium interlayer. For both interlayer materials, intermetallic Al-Mg compounds were still formed, but the width and the level of hardness across the diffusion zone was significantly reduced compared to Al-Mg joints without interlayer.

  6. Welding of AA1050 aluminum with AISI 304 stainless steel by rotary friction welding process

    Directory of Open Access Journals (Sweden)

    Chen Ying An

    2010-09-01

    Full Text Available The purpose of this work was to assess the development of solid state joints of dissimilar material AA1050 aluminum and AISI 304 stainless steel, which can be used in pipes of tanks of liquid propellants and other components of the Satellite Launch Vehicle. The joints were obtained by rotary friction welding process (RFW, which combines the heat generated from friction between two surfaces and plastic deformation. Tests were conducted with different welding process parameters. The results were analyzed by means of tensile tests, Vickers microhardness, metallographic tests and SEM-EDX. The strength of the joints varied with increasing friction time and the use of different pressure values. Joints were obtained with superior mechanical properties of the AA1050 aluminum, with fracture occurring in the aluminum away from the bonding interface. The analysis by EDX at the interface of the junction showed that interdiffusion occurs between the main chemical components of the materials involved. The RFW proves to be a great method for obtaining joints between dissimilar materials, which is not possible by fusion welding processes.

  7. Effects of Different Filler Metals on the Mechanical Behaviors of GTA Welded AA7A52(T6)

    Science.gov (United States)

    Shu, Fengyuan; Lv, Yaohui; Liu, Yuxin; Lin, Jianjun; Sun, Zhe; Xu, Binshi; He, Peng

    2014-06-01

    ER4043, ER5356, and AA7A52 on behalf of the Al-Si, Al-Mg, and Al-Zn-Mg-based welding material, respectively, were chosen as the filler metal to weld AA7A52(T6) plates by GTAW. The variance in mechanical performances of the joints caused by the various filler materials was investigated with reference to the SEM and EDS test results for the weld seam and the fracture surface. Failure was found in the seam for all the welded joints. With regard to the joint obtained with ER4043 welding wire, the total elongation was limited by the brittle intergranular compound Mg2Si of which Mg was introduced by convection mass transfer. As for the other two welds, the content ratio of Zn and Mg was found to play the dominant role in deciding the mechanical properties of the intergranular Mg-Zn compounds which were responsible for the tensile behavior of the joints. The content ratio (wt.%) of beyond 2:1 gave birth to the strengthening phase MgZn2 leading to a ductile fracture. Cr in the seam obtained with AA7A52 filler metal was found to enhance the strength of the joint through isolated particles.

  8. Application Regarding the Butt-Welding Through Intermediate Melting

    Directory of Open Access Journals (Sweden)

    Tudorel Ene

    2006-10-01

    Full Text Available It consists in presenting butt welding procedure through intermediate melting and its usage for manufacturing cutting tools type drill, tap screw, reamer by welding the active part (made of high-speed steel to the tool tail (made of unalloyed steel wit low carbon.

  9. Effects of various tool pin profiles on mechanical and metallurgical properties of friction stir welded joints of cryorolled AA2219 aluminium alloy

    Science.gov (United States)

    Kamal Babu, Karupannan; Panneerselvam, Kavan; Sathiya, Paulraj; Noorul Haq, Abdul Haq; Sundarrajan, Srinivasan; Mastanaiah, Potta; Srinivasa Murthy, Chunduri Venkata

    2018-02-01

    Friction stir welding (FSW) process was conducted on cryorolled (CR) AA2219 plate using different tool pin profiles such as cylindrical pin, threaded cylindrical pin, square pin and hexagonal pin profiles. The FSW was carried out with pairs of 6 mm thick CR aluminium plates with different tool pin profiles. The different tool pin profile weld portions' behaviors like mechanical (tensile strength, impact and hardness) and metallurgical characteristics were analyzed. The results of the mechanical analysis revealed that the joint made by the hexagonal pin tool had good strength compared to other pin profiles. This was due to the pulsating action and material flow of the tool resulting in dynamic recrystallization in the weld zone. This was confirmed by the ultra fine grain structure formation in Weld Nugget (WN) of hexagonal pin tool joint with a higher percentage of precipitate dissolution. The fractograph of the hexagonal tool pin weld portion confirmed the finer dimple structure morphology without having any interior defect compared to other tool pin profiles. The lowest weld joint strength was obtained from cylindrical pin profile weld joint due to insufficient material flow during welding. The Transmission Electron Microscope and EDX analysis showed the dissolution of the metastable θ″, θ' (Al2Cu) partial precipitates in the WN and proved the influence of metastable precipitates on enhancement of mechanical behavior of weld. The XRD results also confirmed the Al2Cu precipitation dissolution in the weld zone.

  10. Joint intentionality: from thin to thick

    Czech Academy of Sciences Publication Activity Database

    Koreň, Ladislav

    2016-01-01

    Roč. 2, č. 1 (2016), s. 75-85 ISSN 2196-9655 R&D Projects: GA ČR GA13-20785S Institutional support: RVO:67985955 Keywords : Tomasello * Cooperation * Joint intentionality * Joint action * Mindreading Subject RIV: AA - Philosophy ; Religion https://www.degruyter.com/view/j/jso.2016.2.issue-1/jso-2015-0047/jso-2015-0047.xml?format=INT

  11. Effects of Post-Weld Heat Treatment on the Microstructure and Toughness of Flash Butt Welded High-Strength Low-Alloy Steel

    Science.gov (United States)

    Shajan, Nikhil; Arora, Kanwer Singh; Asati, Brajesh; Sharma, Vikram; Shome, Mahadev

    2018-04-01

    Effect of post-weld heat treatment on the weld microstructure, texture, and its correlation to the toughness of flash butt welded joints were investigated. Upon flash butt welding, the α and γ-fiber in the parent material converted to Goss (110)[001], rotated Goss (110)[1 \\bar{1} 0], and rotated cube (001)[1 \\bar{1} 0], (001)[ \\overline{11} 0] textures along the fracture plane. Formation of these detrimental texture components was a result of shear deformation and recrystallization of austenite at temperatures above T nr resulting in a drop of toughness at the weld zone. Inter-critical and sub-critical annealing cycles proved to be less effective in reducing the Goss (110)[001], rotated Goss (110)[1 \\bar{1} 0], and rotated cube (001)[1 \\bar{1} 0], (001)[ \\overline{11} 0] texture components, and therefore, toughness values remained unaffected. Post-weld heat treatment in the austenite phase field at 1000 °C for 5 seconds resulted in the formation of new grains with different orientations leading to a reduction in the texture intensities of both Goss and rotated Goss components and therefore improved weld zone toughness. Prolonged annealing time was found to be ineffective in improving the toughness due to grain growth.

  12. 76 FR 43341 - Notice of Availability of the Record of Decision for the West Butte Wind Power Right-of-Way...

    Science.gov (United States)

    2011-07-20

    ... LVRWH09H0600; HAG 10-0338] Notice of Availability of the Record of Decision for the West Butte Wind Power Right... INFORMATION CONTACT: Steve Storo, BLM West Butte Wind Power Right-of-Way Project Lead: telephone (541) 416... INFORMATION: The applicant, West Butte Wind Power, LLC, filed right-of-way (ROW) application OR-065784 to...

  13. Evaluación del comportamiento a fatiga de una unión soldada a tope de acero AISI 1015//Evaluation of the fatigue behaviour of a butt welded joint of AISI 1015 steel

    Directory of Open Access Journals (Sweden)

    Pavel Michel Almaguer‐Zaldivar

    2015-01-01

    Full Text Available Las uniones soldadas son un componente importante de una estructura, por lo que siempre es necesario conocer la respuesta de las mismas sometidas a cargas cíclicas. El objetivo de este trabajo es obtener la curva S-N de una unión soldada a tope de acero AISI 1015 y electrodo E6013 como material de aporte. Los ensayos a fatiga se realizaron de acuerdo a la norma ASTM en una máquina universal MTS810. Se utilizaron probetas de sección rectangular. El ciclo de carga fueasimétrico a tracción, con un coeficiente de asimetría de 0,1. Se obtuvo que la unión estudiada tiene un límite de resistencia a la fatiga de 178 MPa, a un punto de corte de 2 039 093 ciclos.Palabras claves: unión soldada, fatiga, curva S-N, AISI 1015, electrodo E6013._______________________________________________________________________________AbstractWelded joints are an important component in structures, by this reason is necessary to know the behaviour of these elements under cyclic loads. The objective of this work is to obtain the S-N curve of the butt welded joint of AISI 1015 steel and electrode E6013 as the contribution material. Fatiguetest was realized within the ASTM standard in the MTS810 testing machine. Rectangular cross section specimens was used. Cyclic loads was asymmetric tensile and the asymmetry ratio used was 0,1. In this study was obtained the fatigue limit equal to 178 MPa, at the cut point of 2 039 093 cycles.Key words: welded joint, fatigue, S-N curve, AISI 1015 steel, electrode E6013.

  14. A parametric study of residual stresses in multipass butt-welded stainless steel pipes

    Energy Technology Data Exchange (ETDEWEB)

    Brickstad, B. [SAQ Inspection Ltd., Stockholm (Sweden); Josefson, L. [Chalmers Univ. of Technology, Goeteborg (Sweden). Div. of Solid Mechanics

    1996-06-01

    Multipass circumferential butt-welding of stainless steel pipes is simulated numerically in a non-linear thermo-mechanical FE-analysis. In particular, the through-thickness variation at the weld and heat affected zone, of the axial and hoop stresses and their sensitivity to variation in weld parameters are studied. Recommendations are given for the through thickness variation of the axial and hoop stresses to be used when assessing the growth of surface flaws at circumferential butt welds in nuclear piping system. 31 refs, 12 tabs, 54 figs.

  15. Joining of hybrid AA6063-6SiCp-3Grp composite and AISI 1030 steel by friction welding

    Directory of Open Access Journals (Sweden)

    N. Rajesh Jesudoss Hynes

    2017-10-01

    Full Text Available Joining of metals and aluminium hybrid metal matrix composites has significant applications in aviation, ship building and automotive industries. In the present work, investigation is carried out on Friction Welding of AISI 1030 steel and hybrid AA6063-6SiCp-3Grpcomposite, that are difficult to weld by fusion welding technique. Silicon carbide and graphite particle reinforced AA6063 matrix hybrid composite was developed successfully using stir casting method and the joining feasibility of AISI1030 steel with AA6063-6SiCp-3Grp hybrid composite was tried out by friction stud welding technique. During friction stage of welding process, the particulates (SiC & Graphite used for reinforcement, tend to increase the viscosity and lead to improper mixing of matrix and reinforcement. This eventually results in lower strength in dissimilar joints. To overcome this difficulty AA1100 interlayer is used while joining hybrid composite to AISI 1030 steel. Experimentation was carried out using Taguchi based design of experiments (DOE technique. Multiple regression methods were applied to understand the relationship between process parameters of the friction stud welding process. Micro structural examination reveals three separate zones namely fully plasticized zone, partially deformed zone and unaffected base material zone. Ultra fine dynamically recrystallized grains of about 341 nm were observed at the fully plasticized zone. EDX analysis confirms the presence of intermetallic compound Fe2Al5 at the joint interface. According to the experimental analysis using DOE, rotational speed and interlayer sheet thickness contribute about 39% and 36% respectively in determining the impact strength of the welded joints. It is found that joining with 0.5 mm interlayer sheet provides efficient joints. Developed regression model could be used to predict the axial shortening distance and impact strength of the welded joint with reasonable accuracy.

  16. Creep behavior evaluation of welded joint

    International Nuclear Information System (INIS)

    Susei, Shuzo; Matsui, Shigetomo; Mori, Eisuke; Shimizu, Shigeki; Satoh, Keisuke.

    1980-01-01

    In the creep design of high temperature structural elements, it is necessary to grasp the creep performance of joints as a whole, paying attention to the essential lack of uniformity between the material qualities of parent metals and welds. In this study, the factors controlling the creep performance of butt welded joints were investigated theoretically, when they were subjected to lateral tension and longitudinal tension. It was clarified that the rupture time in the case of laterally pulled joints was determined by the ratio of the creep rupture times of weld metals and parent metals, and the rupture time in the case of longitudinally pulled joints was determined by the ratio of the creep rupture times and the ratio of the creep strain rates of weld metals and parent metals. Moreover, when the joints of the former ratio less than 1 and the latter ratio larger than 1 were investigated experimentally, the rupture time in the case of laterally pulled joints was affected by the relative thickness, and when the relative thickness was large, the theoretical and the experimental values coincided, but the relative thickness was small, the theoretical values gave the evaluation on safe side as compared with the experimental values due to the effect of restricting deformation. In the case of longitudinally pulled joints, the theoretical and the experimental values coincided relatively well. The diagram of classifying the creep performance of welded joints was proposed. (Kako, I.)

  17. Analysis and Prediction of the Billet Butt and Transverse Weld in the Continuous Extrusion Process of a Hollow Aluminum Profile

    Science.gov (United States)

    Lou, Shumei; Wang, Yongxiao; Liu, Chuanxi; Lu, Shuai; Liu, Sujun; Su, Chunjian

    2017-08-01

    In continuous extrusions of aluminum profiles, the thickness of the billet butt and the length of the discarded extrudate containing the transverse weld play key roles in reducing material loss and improving product quality. The formation and final distribution of the billet butt and transverse weld depend entirely on the flow behavior of the billet skin material. This study examined the flow behavior of the billet skin material as well as the formation and evolution of the billet butt and the transverse weld in detail through numerical simulation and a series of experiments. In practical extrusions, even if the billet skin is removed by lathe turning shortly before extrusion, billet skin impurities are still distributed around the transverse weld and in the billet butt. The thickness of the scrap billet butt and the length of the discarded extrudate containing the transverse weld can be exactly predicted via simulation.

  18. Joint Attention and Anthropological Difference

    Czech Academy of Sciences Publication Activity Database

    Urban, Petr

    2014-01-01

    Roč. 11, č. 1 (2014), s. 59-70 ISSN 1718-0198 R&D Projects: GA ČR GAP401/10/1164 Institutional support: RVO:67985955 Keywords : joint attention * anthropological difference * phenomenology * great apes * shared intentionality Subject RIV: AA - Philosophy ; Religion

  19. 77 FR 10773 - Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines; Scheduling of...

    Science.gov (United States)

    2012-02-23

    ... Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines; Scheduling of Expedited Five-Year... orders on stainless steel butt-weld pipe fittings from Italy, Malaysia, and the Philippines would be... certificate of service. Determination.--The Commission has determined to exercise its authority to extend the...

  20. 76 FR 67146 - Stainless Steel Butt-Weld Pipe Fittings From Italy; Extension of Time Limit for Preliminary...

    Science.gov (United States)

    2011-10-31

    ... DEPARTMENT OF COMMERCE International Trade Administration [A-475-828] Stainless Steel Butt-Weld... antidumping duty order on stainless steel butt-weld pipe fittings from Italy in the Federal Register. See... preliminary results of this review within the original time frame because it needs to obtain additional...

  1. Feasibility evaluations for the integration of laser butt welding of tubes in industrial pipe coil production lines

    Science.gov (United States)

    Penasa, Mauro; Colombo, Enrico; Giolfo, Mauro

    1994-09-01

    Due to the good performance shown by laser welded joints, to the quality and repeatability achievable by this welding technique and to its high process productivity, a feature inherent to the laser technology which, together with its high flexibility, allows different operations to be performed by a single source, consistent savings in a production line may be obtained. Therefore laser welding techniques may be of high relevance for industrial applications, provided that a sufficient attention is paid to avoiding a low utilization time to the operating laser source. The paper describes a feasibility study for the integration of a laser source as an automatic unit for circumferential butt welding of tubes in production lines of pipe coils, just before the cold bending station. Using a 6 kW CO2 source, thickness ranging from 3.5 to 11.2 mm in carbon, low alloyed Cr-Mo and austenitic stainless steels, have been successfully welded. Cr-Mo steels require on line preheating treatment, which however can be achieved by laser defocused passes just before welding. The results of the preliminary qualification performed on laser welded joints of the involved topologies of product (materials, diameters and thicknesses) are described together with technological tests required for approval: laser circumferential butt welding of tubes has proven to be effective, with satisfactory and repeatable results and good joint performances. An exhaustive comparison with current welding techniques (TIG, MIG) is then carried out, along with a detailed analysis of the potential advantages and benefits which may be expected by using the laser welding technique, as well as with a first estimation of the investments and running costs. Since laser productivity is saturated only at a rough 35% during the year, an accurate analysis of other possible applications and of a possible lay out of a laser working cell integrated in the factory production lines is performed. Usually little attention is

  2. Microstructure evolution in dissimilar AA6060/copper friction stir welded joints

    Science.gov (United States)

    Kalashnikova, T. A.; Shvedov, M. A.; Vasilyev, P. A.

    2017-12-01

    Friction stir welding process has been applied for making a dissimilar copper/aluminum alloy joint. The grain microstructure and mechanical properties of the obtained joint were studied. The structure of the cross-section of the FSW compound was analyzed. The microstructural evolution of the joint was examined using optical microscopy. The mechanical properties of the intermetallic particles were evaluated by measuring the microhardness according to the Vickers method. The microhardness of the intermetallic particles was by a factor of 4 lower than that of the particles obtained by fusion welding. The results of the investigations enable using friction stir welding for making dissimilar joints.

  3. The Western Environmental Technology Office (WETO), Butte, Montana. Technology summary

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    1996-03-01

    The Western Environmental Technology Office (WETO) is a multi-purpose engineering test facility located in Butte, Montana, and is managed by MSE, Inc. WETO seeks to contribute to environmental research by emphasizing projects to develop heavy metals removal and recovery processes, thermal vitrification systems, and waste minimization/pollution prevention technologies. WETO`s environmental technology research and testing activities focus on the recovery of usable resources from waste. In one of WETO`s areas of focus, groundwater contamination, water from the Berkeley Pit, located near the WETO site, is being used in demonstrations directed toward the recovery of potable water and metal from the heavy metal-bearing water. The Berkeley Pit is part of an inactive copper mine near Butte that was once part of the nation`s largest open-pit mining operation. The Pit contains approximately 25 billion gallons of Berkeley Pit groundwater and surface water containing many dissolved minerals. As part of DOE/OST`s Resource Recovery Project (RRP), technologies are being demonstrated to not only clean the contaminated water but to recover metal values such as copper, zinc, and iron with an estimated gross value of more than $100 million. When recovered, the Berkeley Pit waters could benefit the entire Butte valley with new water resources for fisheries, irrigation, municipal, and industrial use. At WETO, the emphasis is on environmental technology development and commercialization activities, which will focus on mine cleanup, waste treatment, resource recovery, and water resource management.

  4. The Western Environmental Technology Office (WETO), Butte, Montana. Technology summary

    International Nuclear Information System (INIS)

    1996-03-01

    The Western Environmental Technology Office (WETO) is a multi-purpose engineering test facility located in Butte, Montana, and is managed by MSE, Inc. WETO seeks to contribute to environmental research by emphasizing projects to develop heavy metals removal and recovery processes, thermal vitrification systems, and waste minimization/pollution prevention technologies. WETO's environmental technology research and testing activities focus on the recovery of usable resources from waste. In one of WETO's areas of focus, groundwater contamination, water from the Berkeley Pit, located near the WETO site, is being used in demonstrations directed toward the recovery of potable water and metal from the heavy metal-bearing water. The Berkeley Pit is part of an inactive copper mine near Butte that was once part of the nation's largest open-pit mining operation. The Pit contains approximately 25 billion gallons of Berkeley Pit groundwater and surface water containing many dissolved minerals. As part of DOE/OST's Resource Recovery Project (RRP), technologies are being demonstrated to not only clean the contaminated water but to recover metal values such as copper, zinc, and iron with an estimated gross value of more than $100 million. When recovered, the Berkeley Pit waters could benefit the entire Butte valley with new water resources for fisheries, irrigation, municipal, and industrial use. At WETO, the emphasis is on environmental technology development and commercialization activities, which will focus on mine cleanup, waste treatment, resource recovery, and water resource management

  5. Fundamental Study of Electron Beam Welding of AA6061-T6 Aluminum Alloy for Nuclear Fuel Plate Assembly (II)

    International Nuclear Information System (INIS)

    Kim, Soosung; Lee, Haein; Lee, Donbae; Park, Jongman; Lee, Yoonsang

    2013-01-01

    Certain characteristics, such as solidification cracking, porosity, HAZ (Heat-affected Zone) degradation must be considered during welding. Because of high energy density and low heat input, especially LBW and EBW processes posses the advantage of minimizing the fusing zone and HAZ and producing deeper penetration than arc welding processes. In present study, to apply for the nuclear fuel plate fabrication and assembly, a fundamental EBW experiment using AA6061-T6 aluminum alloy specimens was conducted. Furthermore, to establish the welding process, and satisfy the requirements of the weld quality, EBW apparatus using a electron welding gun and vacuum chamber was developed, and preliminary investigations for optimizing the welding parameters of the specimens using AA6061-T6 aluminum plates were also performed. In this experiment, a feasibility test was carried out by tensile tester, bead-on-plate welding and metallographic examination to comply with the aluminum welding procedure. The EB weld quality of AA6061-T6 aluminum alloy for the fuel plate assembly has been also studied by the mechanical testing and microstructure examinations. This study was carried out to determine the suitable welding process and to investigate tensile strength of AA6061-T6 aluminum alloy. In the present experiment, satisfactory EBW of the square butt weld specimens was developed. In comparison with the rolling directions of test specimens, the tensile strengths were no difference between the longitudinal and transverse welds. Based on this fundamental study, fabrication and assembly of the nuclear fuel plates will be provided for the future Kijang research reactor project

  6. Optimization of friction stir welding process parameters to maximize tensile strength of stir cast AA6061-T6/AlNp composite

    International Nuclear Information System (INIS)

    Ashok Kumar, B.; Murugan, N.

    2014-01-01

    Highlights: • AA6061/AlN p cast composite was welded by FSW process. • Regression models were developed to predict UTS and elongation of the FS welded joint. • FS welded joint using the optimized parameters exhibited maximum UTS and joint efficiency. • Defect free weld joint was obtained with optimized parameters value. - Abstract: Aluminium Matrix Composites (AMCs) reinforced with particulate form of reinforcement has replaced monolithic alloys in many engineering industries due to its superior mechanical properties and tailorable thermal and electrical properties. As aluminium nitride (AlN) has high specific strength, high thermal conductivity, high electrical resistivity, low dielectric constant, low coefficient of thermal expansion and good compatibility with aluminium alloy, Al/AlN composite is extensively used in electronic packaging industries. Joining of AMCs is unavoidable in many engineering applications. Friction Stir Welding (FSW) is one of the most suitable welding process to weld the AMCs reinforced with particulate form of ceramics without deteriorating its superior mechanical properties. An attempt has been made to develop regression models to predict the Ultimate Tensile Strength (UTS) and Percent Elongation (PE) of the friction stir welded AA6061 matrix composite reinforced with aluminium nitride particles (AlN p ) by correlating the significant parameters such as tool rotational speed, welding speed, axial force and percentage of AlN p reinforcement in the AA6061 matrix. Statistical software SYSTAT 12 and statistical tools such as analysis of variance (ANOVA) and student’s t test, have been used to validate the developed models. It was observed from the investigation that these factors independently influenced the UTS and PE of the friction stir welded composite joints. The developed regression models were optimized to maximize UTS of friction stir welded AA6061/AlN p composite joints

  7. An Analysis of the Quality of the Thick-Walled S355J2+N Steel Joint Welded by the Mag Method

    Directory of Open Access Journals (Sweden)

    Krawczyk R.

    2017-06-01

    Full Text Available An analysis of the quality of the thick-walled S355J2+N steel welded joint used most frequently in the general-building, power and other contemporary steel constructions is presented in the following article. A process of examining welding technologies was made on the tick-walled butt joints of plates by using the MAG – 135 welding method. The aim of the discussed topic was to optimize the process of welding thick-walled welded joints due to their mechanical strength properties and efficiency.

  8. Effect of Friction Stir Welding Parameters on the Microstructure and Mechanical Properties of AA2024-T4 Aluminum Alloy

    Directory of Open Access Journals (Sweden)

    A. W. El-Morsy

    2018-02-01

    Full Text Available In this work, the effects of rotational and traverse speeds on the 1.5 mm butt joint performance of friction stir welded 2024-T4 aluminum alloy sheets have been investigated. Five rotational speeds ranging from 560 to 1800 rpm and five traverse speeds ranging from 11 to 45 mm/min have been employed. The characterization of microstructure and the mechanical properties (tensile, microhardness, and bending of the welded sheets have been studied. The results reveal that by varying the welding parameters, almost sound joints and high performance welded joints can be successfully produced at the rotational speeds of 900 rpm and 700 rpm and the traverse speed of 35 mm/min. The maximum welding performance of joints is found to be 86.3% with 900 rpm rotational speed and 35 mm/min traverse speed. The microhardness values along the cross-section of the joints show a dramatic drop in the stir zone where the lowest value reached is about 63% of the base metal due to the softening of the welded zone caused by the heat input during joining.

  9. Computational Modeling of Microstructural-Evolution in AISI 1005 Steel During Gas Metal Arc Butt Welding

    Science.gov (United States)

    2013-05-01

    H.K.D.H. Bhadeshia, A Model for the Microstruc- ture of Some Advanced Bainitic Steels , Mater. Trans., 1991, 32, p 689–696 19. G.J. Davies and J.G. Garland...REPORT Computational Modeling of Microstructural-Evolution in AISI 1005 Steel During Gas Metal Arc Butt Welding 14. ABSTRACT 16. SECURITY...Computational Modeling of Microstructural-Evolution in AISI 1005 Steel During Gas Metal Arc Butt Welding Report Title ABSTRACT A fully coupled (two-way

  10. Incorporation of cigarette butts into nests reduces nest ectoparasite load in urban birds: new ingredients for an old recipe?

    Science.gov (United States)

    Suárez-Rodríguez, Monserrat; López-Rull, Isabel; Garcia, Constantino Macías

    2013-02-23

    Birds are known to respond to nest-dwelling parasites by altering behaviours. Some bird species, for example, bring fresh plants to the nest, which contain volatile compounds that repel parasites. There is evidence that some birds living in cities incorporate cigarette butts into their nests, but the effect (if any) of this behaviour remains unclear. Butts from smoked cigarettes retain substantial amounts of nicotine and other compounds that may also act as arthropod repellents. We provide the first evidence that smoked cigarette butts may function as a parasite repellent in urban bird nests. The amount of cellulose acetate from butts in nests of two widely distributed urban birds was negatively associated with the number of nest-dwelling parasites. Moreover, when parasites were attracted to heat traps containing smoked or non-smoked cigarette butts, fewer parasites reached the former, presumably due to the presence of nicotine. Because urbanization changes the abundance and type of resources upon which birds depend, including nesting materials and plants involved in self-medication, our results are consistent with the view that urbanization imposes new challenges on birds that are dealt with using adaptations evolved elsewhere.

  11. Study on Tensile Fatigue Behavior of Thermal Butt Fusion in Safety Class III High-Density Polyethylene Buried Piping in Nuclear Power Plants

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Jong Sung; Lee, Young Ju [Sunchon National University, Suncheon (Korea, Republic of); Oh, Young Jin [KEPCO E and C, Yongin (Korea, Republic of)

    2015-01-15

    High-density polyethylene (HDPE) piping, which has recently been applied to safety class III piping in nuclear power plants, can be butt-joined through the thermal fusion process, which heats two fused surfaces and then subject to axial pressure. The thermal fusion process generates bead shapes on the butt fusion. The stress concentrations caused by the bead shapes may reduce the fatigue lifetime. Thus, investigating the effect of the thermal butt fusion beads on fatigue behavior is necessary. This study examined the fatigue behavior of thermal butt fusion via a tensile fatigue test under stress-controlled conditions using finite element elastic stress analysis. Based on the results, the presence of thermal butt fusion beads was confirmed to reduce the fatigue lifetime in the low-cycle fatigue region while having a negligible effect in the medium- and high-cycle fatigue regions.

  12. Study on Tensile Fatigue Behavior of Thermal Butt Fusion in Safety Class III High-Density Polyethylene Buried Piping in Nuclear Power Plants

    International Nuclear Information System (INIS)

    Kim, Jong Sung; Lee, Young Ju; Oh, Young Jin

    2015-01-01

    High-density polyethylene (HDPE) piping, which has recently been applied to safety class III piping in nuclear power plants, can be butt-joined through the thermal fusion process, which heats two fused surfaces and then subject to axial pressure. The thermal fusion process generates bead shapes on the butt fusion. The stress concentrations caused by the bead shapes may reduce the fatigue lifetime. Thus, investigating the effect of the thermal butt fusion beads on fatigue behavior is necessary. This study examined the fatigue behavior of thermal butt fusion via a tensile fatigue test under stress-controlled conditions using finite element elastic stress analysis. Based on the results, the presence of thermal butt fusion beads was confirmed to reduce the fatigue lifetime in the low-cycle fatigue region while having a negligible effect in the medium- and high-cycle fatigue regions

  13. Ultrasonic wave propagation in real-life austenitic V-butt welds: Numerical modeling and validation

    International Nuclear Information System (INIS)

    Hannemann, R.; Marklein, R.; Langenberg, K. J.; Schurig, C.; Koehler, B.; Walte, F.

    2000-01-01

    In nondestructive testing the evaluation of austenitic steel welds with ultrasound is a commonly used method. But, since the wave propagation, scattering, and diffraction effects in such complicated media are hardly understood, computer simulations are very helpful to increase the knowledge of the physical phenomena in such samples. A particularly powerful numerical time domain modeling tool is the well established Elastodynamic Finite Integration Technique (EFIT). Recently, EFIT has been extended to simulate elastic waves in inhomogeneous anisotropic media. In this paper, the step-by-step evaluation of ultrasonic wave propagation in inhomogeneous anisotropic media will be described and the results will be validated against measurements. As a simplified model, a V-butt weld with perpendicular grain structure is investigated. The coincidence between the B Scans of the simulation and the measurement of an idealized V-butt weld is remarkable and even effects predicted by theory and simulation - the appearance of two coupled quasi-SV waves - can be observed. As a next step, an improved and more realistic model of the grain orientation inside the V-butt weld is introduced. This model has been implemented in the EFIT code and has been validated against measurements. For this verification, measured and simulated B-Scans for a real-life V-butt weld have been compared and a significant coincidence has been observed. Furthermore, the main pulses in the B-Scans are interpreted by analyzing the snapshot-movies of the wavefronts

  14. Investigation and control of factors influencing resistance upset butt welding.

    NARCIS (Netherlands)

    Kerstens, N.F.H.

    2010-01-01

    The purpose of this work is to investigate the factors influencing the resistance upset butt welding process to obtain an understanding of the metal behaviour and welding process characteristics, so that new automotive steels can be welded with reduced development time and fewer failures in

  15. Effect of Shielding Gas on the Properties of AW 5083 Aluminum Alloy Laser Weld Joints

    Science.gov (United States)

    Vyskoč, Maroš; Sahul, Miroslav; Sahul, Martin

    2018-04-01

    The paper deals with the evaluation of the shielding gas influence on the properties of AW 5083 aluminum alloy weld joints produced with disk laser. Butt weld joints were produced under different shielding gas types, namely Ar, He, Ar + 5 vol.% He, Ar + 30 vol.% He and without shielding weld pool. Light and electron microscopy, computed tomography, microhardness measurements and tensile testing were used for evaluation of weld joint properties. He-shielded weld joints were the narrowest ones. On the other hand, Ar-shielded weld joints exhibited largest weld width. The choice of shielding gas had significant influence on the porosity level of welds. The lowest porosity was observed in weld joint produced in Ar with the addition of 5 vol.% He shielding atmosphere (only 0.03%), while the highest level of porosity was detected in weld joint produced in pure He (0.24%). Except unshielded aluminum alloy weld joint, the lowest tensile strength was recorded in He-shielded weld joints. On the contrary, the highest average microhardness was measured in He-shielded weld joints.

  16. 75 FR 60804 - Notice of Availability of the Final Environmental Impact Statement for the West Butte Wind Power...

    Science.gov (United States)

    2010-10-01

    ... Wind Power Right-of-Way, Crook and Deschutes Counties, OR AGENCY: Bureau of Land Management, Interior... Final Environmental Impact Statement (EIS) for the West Butte Wind Power Right-of-Way and by this Notice... Register notice. FOR FURTHER INFORMATION CONTACT: Steve Storo, BLM West Butte Wind Power Right of Way...

  17. Microstructure Stability During Creep of Friction Stir Welded AA2024-T3 Alloy

    Science.gov (United States)

    Regev, Michael; Rashkovsky, Tal; Cabibbo, Marcello; Spigarelli, Stefano

    2018-01-01

    The poor weldability of the AA2024 aluminum alloy limits its use in industrial applications. Because friction stir welding (FSW) is a non-fusion welding process, it seems to be a promising solution for welding this alloy. In the current study, FSW was applied to butt weld AA2024-T3 aluminum alloy plates. Creep tests were conducted at 250 and at 315 °C on both the parent material and the friction stir welded specimens. The microstructures of the welded and non-welded AA2024-T3 specimens before and after the creep tests were studied and compared. A comprehensive transmission electron microscopy study together with a high-resolution scanning electron microscopy study and energy-dispersive x-ray spectroscopy analysis was conducted to investigate the microstructure stability. The parent material seems to contain two kinds of Cu-rich precipitates—coarse precipitates of a few microns each and uniformly dispersed fine nanosized precipitates. Unlike the parent material, the crept specimens were found to contain the two kinds of precipitates mentioned above together with platelet-like precipitates. In addition, extensive decoration of the grain boundaries with precipitates was clearly observed in the crept specimens. Controlled aging experiments for up to 280 h at the relevant temperatures were conducted on both the parent material and the welded specimens in order to isolate the contribution of exposure to high temperatures to the microstructure changes. TEM study showed the development of dislocation networks into a cellular dislocation structure in the case of the parent metal. Changes in the dislocation structure as a function of the creep strain and the FSW process were recorded. A detailed creep data analysis was conducted, taking into account the instability of the microstructure.

  18. Stress indices for girth welded joints, including radial weld shrinkage, mismatch and tapered-wall transitions

    International Nuclear Information System (INIS)

    Rodabaugh, E.C.; Moore, S.E.

    1978-09-01

    A review is presented of B, C and K stress indices used in the ASME Nuclear Power Plant Code for girth butt welds and girth fillet welds. Theoretical stresses are presented to aid in evaluating C-indices. Fatigue test data are presented to aid in evaluating K-indices and CK-products. A limit load theory is presented to aid in evaluating B-indices. As a result of this review, recommendations are made for changes in the ASME Code. A major part of this consists of presenting definitions for girth welded joints and transitions and appropriate stress indices for those joints

  19. Geology of Pine and Crater Buttes: two basaltic constructs on the far eastern Snake River Plain

    International Nuclear Information System (INIS)

    Mazierski, P.F.; King, J.S.

    1987-01-01

    The emplacement history and petrochemical evolution of the volcanics associated with Pine Butte, Crater Butte, and other nearby vents are developed and described. Four major vents were identified in the study area and their associated eruptive products were mapped. All of the vents show a marked physical elongation or linear orientation coincident with the observed rift set. Planetary exploration has revealed the importance of volcanic processes in the genesis and modification of extraterrestrial surfaces. Interpretation of surface features has identified plains-type basaltic volcanism in various mare regions of the Moon and the volcanic provinces of Mars. Identification of these areas with features that appear analogous to those observed in the Pine Butte area suggests similar styles of eruption and mode of emplacement. Such terrestrial analogies serve as a method to interpret the evolution of volcanic planetary surfaces on the inner planets

  20. Numerical Simulation of Heat and Flow Behaviors in Butt-fusion Welding Process of HDPE Pipes with Curved Fusion Surface

    Energy Technology Data Exchange (ETDEWEB)

    Yoo, Jae Hyun; Ahn, Kyung Hyun [Seoul National University, Seoul (Korea, Republic of); Choi, Sunwoong; Oh, Ju Seok [Hannam University, Daejeon (Korea, Republic of)

    2017-08-15

    Butt-fusion welding process is used to join the polymeric pipes. Recently, some researchers suggest the curved surface to enhance a welding quality. We investigated how curved welding surface affects heat and flow behaviors of polymer melt during the process in 2D axisymmetric domain with finite element method, and discussed the effect to the welding quality. In this study, we considered HDPE pipes. In heat soak stage, curved phase interface between the melt and solid is shown along the shape of welding surface. In jointing stage, squeezing flow is generated between curved welding surface and phase interface. The low shear rate in fusion domain reduces the alignment of polymer to the perpendicular direction of pipes, and then this phenomenon is expected to help to enhance the welding quality.

  1. 77 FR 61020 - Notice of Availability of Final Environmental Impact Statement for the Sigurd to Red Butte No. 2...

    Science.gov (United States)

    2012-10-05

    ...; UTU-83067] Notice of Availability of Final Environmental Impact Statement for the Sigurd to Red Butte... (BLM) has prepared a Final Environmental Impact Statement (EIS) for the Sigurd to Red Butte No. 2--345...; Utah School and Institutional Trust Lands Administration; Millard, Sevier, Beaver, Iron, and Washington...

  2. Thermographic Analysis of Stress Distribution in Welded Joints

    Directory of Open Access Journals (Sweden)

    Domazet Ž.

    2010-06-01

    Full Text Available The fatigue life prediction of welded joints based on S-N curves in conjunction with nominal stresses generally is not reliable. Stress distribution in welded area affected by geometrical inhomogeneity, irregular welded surface and weld toe radius is quite complex, so the local (structural stress concept is accepted in recent papers. The aim of this paper is to determine the stress distribution in plate type aluminum welded joints, to analyze the reliability of TSA (Thermal Stress Analysis in this kind of investigations, and to obtain numerical values for stress concentration factors for practical use. Stress distribution in aluminum butt and fillet welded joints is determined by using the three different methods: strain gauges measurement, thermal stress analysis and FEM. Obtained results show good agreement - the TSA mutually confirmed the FEM model and stresses measured by strain gauges. According to obtained results, it may be stated that TSA, as a relatively new measurement technique may in the future become a standard tool for the experimental investigation of stress concentration and fatigue in welded joints that can help to develop more accurate numerical tools for fatigue life prediction.

  3. Thermographic Analysis of Stress Distribution in Welded Joints

    Science.gov (United States)

    Piršić, T.; Krstulović Opara, L.; Domazet, Ž.

    2010-06-01

    The fatigue life prediction of welded joints based on S-N curves in conjunction with nominal stresses generally is not reliable. Stress distribution in welded area affected by geometrical inhomogeneity, irregular welded surface and weld toe radius is quite complex, so the local (structural) stress concept is accepted in recent papers. The aim of this paper is to determine the stress distribution in plate type aluminum welded joints, to analyze the reliability of TSA (Thermal Stress Analysis) in this kind of investigations, and to obtain numerical values for stress concentration factors for practical use. Stress distribution in aluminum butt and fillet welded joints is determined by using the three different methods: strain gauges measurement, thermal stress analysis and FEM. Obtained results show good agreement - the TSA mutually confirmed the FEM model and stresses measured by strain gauges. According to obtained results, it may be stated that TSA, as a relatively new measurement technique may in the future become a standard tool for the experimental investigation of stress concentration and fatigue in welded joints that can help to develop more accurate numerical tools for fatigue life prediction.

  4. Et cigaretskod, en donation, en renere by: A cigarette butt, a donation, a cleaner city

    OpenAIRE

    Bengtsen, Monica; Patursson, Guttormur; Nedergaard, Sofie Tarpø; Madsen, Maria Chas; Drews, Anna Ørsted; Bach, Katrine Møller

    2013-01-01

    This project concerns an explanation of the problem of cigarette butts lying in the streets of Copenhagen. By using elements of the theory of nudging we have designed an ashtray ment to pledge smokers not to throw their butt in the streets. The design is a response to a design competition published by the municipality of Copenhagen, as an attempt to be the cleanest capital in Europe by the year 2015. The core of the design presentation is in cooperation with private firms, who have obligated ...

  5. Investigation of Microstructure and Microhardness in Self-Reacting Friction Stir Welded AA2014-T6 and AA2219-T87

    Science.gov (United States)

    Horton, K. Renee; McGill, Preston; Barkey, Mark

    2011-01-01

    Friction stir welding (FSW) is a solid state welding process with potential advantages for aerospace and automotive industries dealing with light alloys. Self-reacting friction stir welding (SR-FSW) is one variation of the FSW process being developed at the National Aeronautics and Space Administration (NASA) for use in the fabrication of propellant tanks. This work reports on the microstructure and microhardness of SR-FSW between two dissimilar aluminum alloys. Specifically, the study examines the cross section of the weld joint formed between an AA2014-T6 plate on the advancing side and an AA2219-T87 plate on the retreating side. The microstructural analysis shows an irregularly displaced weld seam from the advancing side past the thermo-mechanical affected zone (TMAZ) into the weld nugget region. There are sharp variations in the microhardness across the weld. These variations are described in the paper and mechanisms for their formation are discussed.

  6. Efficacy of etanercept in patients with AA amyloidosis secondary to rheumatoid arthritis.

    Science.gov (United States)

    Nakamura, T; Higashi, S; Tomoda, K; Tsukano, M; Baba, S

    2007-01-01

    The efficacy of biological therapies in rheumatoid arthritis (RA) is well known, but their hypothetical benefit in amyloid A (AA) amyloidosis secondary to RA still remains to be considered. We evaluated the efficacy and safety of etanercept in serum amyloid A (SAA) 1.3 allele Japanese patients with AA amyloidosis secondary to RA. Seven RA patients with histologically confirmed AA amyloidosis and renal involvement who were treated with etanercept were enrolled. They all had the SAA1.3 allele, which has been shown to be a risk factor not only for the association of AA amyloidosis but also for a poor prognosis in Japanese RA patients. Efficacy was assessed as a sustained decrease in RA inflammation and an amelioration of renal function. RA inflammation and AA amyloidosis were improved and stabilized after 43.4 +/- 16.5 weeks. At week 20 the number of tender (p = 0.017) and swollen (p = 0.017) joints, and levels of serum C-reactive protein (p = 0.018) and albumin (p = 0.045) had improved. The values for SAA, serum creatinine, calculated creatinine clearance, and proteinuria also ameliorated. No severe adverse events were observed. One patient eventually had to go on hemodialysis but her tolerance of etanercept remained stable. Etanercept can be used safely and effectively in AA amyloidosis secondary to RA with renal involvement, and is of clinical benefit in the short-term, even in patients on hemodialysis. It appears that SAA1.3 allele may be used as a clinical parameter for the introduction of etanercept in Japanese RA with AA amyloidosis.

  7. Improvement in properties of welded joints of titanium alloy VT22 by thermocyclic treatment

    International Nuclear Information System (INIS)

    Lyasotskaya, V.S.; Kulikov, F.R.; Kirillov, Yu.G.; Ravdonikas, N.Yu.

    1983-01-01

    The results of investigations of the thermocyclic treatment (TCT) effect on the structure and properties of butt welded joints of tubes (with external diameter 180 mm and wall thickness 20-25 mm) of the VT22 alloy are presented. Welded joints have been obtained by means of multipassing automatic argon-arc (ARAW) and electron-beam (ELB) welding. It is shown that TCT of welded joints of the VT22 alloy results in formation in all zones of substructure with disperse precipitations of α-phase which is analogous to the structure of near welded seam zone metal immediately after welding. As a result of TCT and subsequent TT of welded joints poligonization and recrystallization processes of α- and #betta#-phases, changes in parameters of structural components and thin phase structure take place. TCT with strengthening TT or annealing leads to strength increase, while TCT with annealing besides that improves placticity and impact strength of the VT22 alloy welded joints

  8. A Demonstration System for Capturing Geothermal Energy from Mine Waters beneath Butte, Montana

    Energy Technology Data Exchange (ETDEWEB)

    Blackketter, Donald [Montana Tech of the Univ. of Montana, Butte, MT (United States)

    2015-06-01

    Executive Summary An innovative 50-ton ground-source heat pump (GSHP) system was installed to provide space heating and cooling for a 56,000 square foot (5,200 square meter) building in Butte Montana, in conjunction with its heating and chiller systems. Butte is a location with winter conditions much colder than the national average. The GSHP uses flooded mine waters at 78F (25C) as the heat source and heat sink. The heat transfer performance and efficiency of the system were analyzed using data from January through July 2014. This analysis indicated that for typical winter conditions in Butte, Montana, the GSHP could deliver about 88% of the building’s annual heating needs. Compared with a baseline natural-gas/electric system, the system demonstrated at least 69% site energy savings, 38% source energy savings, 39% carbon dioxide emissions reduction, and a savings of $17,000 per year (40%) in utility costs. Assuming a $10,000 per ton cost for installing a production system, the payback period at natural gas costs of $9.63/MMBtu and electricity costs of $0.08/kWh would be in the range of 40 to 50 years. At higher utility prices, or lower installation costs, the payback period would obviously be reduced.

  9. Quality Analysis of Welded and Soldered Joints of Cu-Nb Microcomposite Wires

    Directory of Open Access Journals (Sweden)

    Nikolaj VIŠNIAKOV

    2011-03-01

    Full Text Available Quality analysis of welded and soldered joints of Cu-Nb microcomposite wires has been performed. Quality and mechanical characteristics of joints as ultimate tensile stress limit and elongation at break were measured with an universal testing machine and controlled visually using an optical microscope. Two wires joints were soldered with silver and copper solders and put into steel and copper sleeve respectively. Another two wires joints were soldered with silver solder and welded without any reinforcement. Joints soldered with the silver solder and steel sleeve have demonstrated the best mechanical characteristics: ultimate tensile stress limit of 650 MPa and elongation at break of 0.85 %. Joints soldered with the copper sleeve have no advantages comparing with the soldered butt joint. Ultimate tensile stress limit and elongation at break were in 300 MPa - 350 MPa and in 0.35 % - 0.45 % ranges respectively. Two welded joints had ultimate tensile stress limit of 470 MPa and elongation at break of 0.71 %. In all joints the microstructure of Nb filaments was destroyed and mechanical properties have been specified by mechanical strength of copper and sleeve materials only.http://dx.doi.org/10.5755/j01.ms.17.1.242

  10. Fatigue Crack Growth Behavior of Gas Metal Arc Welded AISI 409 Grade Ferritic Stainless Steel Joints

    Science.gov (United States)

    Lakshminarayanan, A. K.; Shanmugam, K.; Balasubramanian, V.

    2009-10-01

    The effect of filler metals such as austenitic stainless steel, ferritic stainless steel, and duplex stainless steel on fatigue crack growth behavior of the gas metal arc welded ferritic stainless steel joints was investigated. Rolled plates of 4 mm thickness were used as the base material for preparing single ‘V’ butt welded joints. Center cracked tensile specimens were prepared to evaluate fatigue crack growth behavior. Servo hydraulic controlled fatigue testing machine with a capacity of 100 kN was used to evaluate the fatigue crack growth behavior of the welded joints. From this investigation, it was found that the joints fabricated by duplex stainless steel filler metal showed superior fatigue crack growth resistance compared to the joints fabricated by austenitic and ferritic stainless steel filler metals. Higher yield strength and relatively higher toughness may be the reasons for superior fatigue performance of the joints fabricated by duplex stainless steel filler metal.

  11. Episodic Holocene eruption of the Salton Buttes rhyolites, California, from paleomagnetic, U-Th, and Ar/Ar dating

    Science.gov (United States)

    Wright, Heather M.; Vazquez, Jorge A.; Champion, Duane E.; Calvert, Andrew T.; Mangan, Margaret T.; Stelten, Mark E.; Cooper, Kari M.; Herzig, Charles; Schriener Jr., Alexander

    2015-01-01

    In the Salton Trough, CA, five rhyolite domes form the Salton Buttes: Mullet Island, Obsidian Butte, Rock Hill, North and South Red Hill, from oldest to youngest. Results presented here include 40Ar/39Ar anorthoclase ages, 238U-230Th zircon crystallization ages, and comparison of remanent paleomagnetic directions with the secular variation curve, which indicate that all domes are Holocene. 238U-230Th zircon crystallization ages are more precise than but within uncertainty of 40Ar/39Ar anorthoclase ages, suggesting that zircon crystallization proceeded until shortly before eruption in all cases except one. Remanent paleomagnetic directions require three eruption periods: (1) Mullet Island, (2) Obsidian Butte, and (3) Rock Hill, North Red Hill, and South Red Hill. Borehole cuttings logs document up to two shallow tephra layers. North and South Red Hills likely erupted within 100 years of each other, with a combined 238U-230Th zircon isochron age of: 2.83 ± 0.60 ka (2 sigma); paleomagnetic evidence suggests this age predates eruption by hundreds of years (1800 cal BP). Rock Hill erupted closely in time to these eruptions. The Obsidian Butte 238U-230Th isochron age (2.86 ± 0.96 ka) is nearly identical to the combined Red Hill age, but its Virtual Geomagnetic Pole position suggests a slightly older age. The age of aphyric Mullet Island dome is the least well constrained: zircon crystals are resorbed and the paleomagnetic direction is most distinct; possible Mullet Island ages include ca. 2300, 5900, 6900, and 7700 cal BP. Our results constrain the duration of Salton Buttes volcanism to between ca. 5900 and 500 years.

  12. The geology of Pine and Crater Buttes: Two basaltic constructs on the far eastern Snake River Plain

    Science.gov (United States)

    Mazierski, Paul F.; King, John S.

    1987-01-01

    The emplacement history and petrochemical evolution of the volcanics associated with Pine Butte, Crater Butte, and other nearby vents are developed and described. Four major vents were identified in the study area and their associated eruptive products were mapped. All of the vents show a marked physical elongation or linear orientation coincident with the observed rift set. Planetary exploration has revealed the importance of volcanic processes in the genesis and modification of extraterrestrial surfaces. Interpretation of surface features has identified plains-type basaltic volcanism in various mare regions of the Moon and the volcanic provinces of Mars. Identification of these areas with features that appear analogous to those observed in the Pine Butte area suggests similar styles of eruption and mode of emplacement. Such terrestrial analogies serve as a method to interpret the evolution of volcanic planetary surfaces on the inner planets.

  13. Microstructure and anisotropic mechanical behavior of friction stir welded AA2024 alloy sheets

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Zhihan [State Key Laboratory of Solidification Processing, Shaanxi Key Laboratory of Friction Welding Technologies, Northwestern Polytechnical University, Xi' an 710072, Shaanxi (China); Li, Wenya, E-mail: liwy@nwpu.edu.cn [State Key Laboratory of Solidification Processing, Shaanxi Key Laboratory of Friction Welding Technologies, Northwestern Polytechnical University, Xi' an 710072, Shaanxi (China); Li, Jinglong [State Key Laboratory of Solidification Processing, Shaanxi Key Laboratory of Friction Welding Technologies, Northwestern Polytechnical University, Xi' an 710072, Shaanxi (China); Chao, Y.J. [Department of Mechanical Engineering, University of South Carolina, Columbia, SC 29208 (United States); Vairis, A. [Mechanical Engineering Department, TEI of Crete, Heraklion, Crete 71004 (Greece)

    2015-09-15

    The anisotropic mechanical properties of friction stir welded (FSW) AA2024-T3 alloy joints were investigated based on the uniaxial tensile tests. The joint microstructure was examined by using electron back-scattered diffraction and transmission electron microscope. Results show that the evident anisotropic failure and yielding are present in the FSW joints. With the increase of loading angle from 0° to 90° the ultimate tensile strength and elongation of the specimens consistently decrease, or at first decrease and then increase, depending on the FSW process parameters. The specimen cut from the weld direction, i.e. a loading angle of 0°, exhibits the highest strength and elongation. - Highlights: • Microstructure and anisotropy of friction stir welded joints were studied. • The evident anisotropic failure and yielding are present in joints. • The lowest yield stress and UTS are at 45° and 60° loadings, respectively. • Rotation speed heavily impact on the anisotropy of joints.

  14. Microstructure and anisotropic mechanical behavior of friction stir welded AA2024 alloy sheets

    International Nuclear Information System (INIS)

    Zhang, Zhihan; Li, Wenya; Li, Jinglong; Chao, Y.J.; Vairis, A.

    2015-01-01

    The anisotropic mechanical properties of friction stir welded (FSW) AA2024-T3 alloy joints were investigated based on the uniaxial tensile tests. The joint microstructure was examined by using electron back-scattered diffraction and transmission electron microscope. Results show that the evident anisotropic failure and yielding are present in the FSW joints. With the increase of loading angle from 0° to 90° the ultimate tensile strength and elongation of the specimens consistently decrease, or at first decrease and then increase, depending on the FSW process parameters. The specimen cut from the weld direction, i.e. a loading angle of 0°, exhibits the highest strength and elongation. - Highlights: • Microstructure and anisotropy of friction stir welded joints were studied. • The evident anisotropic failure and yielding are present in joints. • The lowest yield stress and UTS are at 45° and 60° loadings, respectively. • Rotation speed heavily impact on the anisotropy of joints

  15. The effect of brazing parameters on corrosion behavior of brazed aluminum joints

    Science.gov (United States)

    Ghasimakbari, Farzam; Hadian, Ali Mohammad; Ershadrad, Soheil; Omidazad, Amir Mansour

    2018-01-01

    Fluid transmission pipes made of aluminum are widely used in petrochemical industries. For many applications, they have to be brazed to each other. The brazed joints, in many cases, are encountered with corrosive medias. This paper reports a part of a work to investigate the corrosion behavior of brazed AA6061 using AA4047 as filler metal with and without the use of flux under different brazing atmospheres. The samples brazed under air, vacuum, argon, and hydrogen atmospheres. The interfacial area of the joints was examined to ensure being free of any defects. The sides of each test piece were covered with an insulator and the surface of the joint was encountered to polarization test. The results revealed a significant difference of corrosion resistance. The samples that brazed under argon and hydrogen atmospheres had better corrosion resistance than other samples. The microstructure of the corroded joints revealed that the presence of defects, impurities due to use of flux and depth of filter metal penetration in base metal are crucial variables on the corrosion resistance of the joints.

  16. Welding of AA1050 aluminum with AISI 304 stainless steel by rotary friction welding process

    OpenAIRE

    Alves, Eder Paduan; Piorino Neto, Francisco; An, Chen Ying

    2010-01-01

    Abstract: The purpose of this work was to assess the development of solid state joints of dissimilar material AA1050 aluminum and AISI 304 stainless steel, which can be used in pipes of tanks of liquid propellants and other components of the Satellite Launch Vehicle. The joints were obtained by rotary friction welding process (RFW), which combines the heat generated from friction between two surfaces and plastic deformation. Tests were conducted with different welding process parameters. The ...

  17. Dissimilar metal study on C44300 tube to AA7075 -T651 tube plate with and without thread by FWTPET process

    Energy Technology Data Exchange (ETDEWEB)

    Radhakrishnan, E.; Kumaraswamidhas, L. A. [Indian Institute of Technology (ISM), Jharkhand (India); Muruganandam, D. [Sri Sairam Engineering College, Tamil Nadu (India); Kumaran, S. Senthil [RVS School of Engineering and Technology, Tamilnadu, (India)

    2017-05-15

    Friction welding has vital industrial role in fabricating automobiles, aerospace, ship building, heat exchangers using similar, dissimilar and bi-metal of ferrous and non-ferrous metals at mass production level. In this study, admiralty brass C44300 tube and aluminium alloy AA7075 -T651, 6 mm thick tube plate were identified as base metals. Different joint surface area profile of with and without thread of different pitch values was chosen to study the mechanical properties and micro structures of these two base metals. 0.1 mm clearance was maintained between the AA7075-T651 tube plate and C44300 tube outer diameter to make friction welding. Taguchi’s L16 orthogonal array techniques were adopted for identifying the most significant ranking process parameters. Analysis of variance (ANOVA) has been used to analyze the input parameter contribution in terms of percentage. Genetic algorithm (GA) was used to access the suitable input parameter value to obtain effective joint strength in terms of hardness, compressive strength and microstructure formation in the interface of the joint. A Compression test (CT) was conducted to evaluate the level of compressive strength of the joint. Threaded profile pair with higher pitch value proved high compressive strength over unthreaded pair. Micro structure for base metal C44300 tube and AA7075-T651 tube plate, Heat affected zone (HAZ) and Weld zone (WZ) of the joint has been studied. Hardness of base metals, HAZ and WZ was measured by micro Vickers hardness tester and the observation shows that hardness at joint interface has been found to be higher in all pairs.

  18. Influence of friction stir welding parameters on properties of 2024 T3 aluminium alloy joints

    Directory of Open Access Journals (Sweden)

    Eramah Abdsalam M.

    2014-01-01

    Full Text Available The aim of this work is to analyse the process of friction stir welding (FSW of 3mm thick aluminium plates made of high strength aluminium alloy - 2024 T3, as well as to assess the mechanical properties of the produced joints. FSW is a modern procedure which enables joining of similar and dissimilar materials in the solid state, by the combined action of heat and mechanical work. This paper presents an analysis of the experimental results obtained by testing the butt welded joints. Tensile strength of the produced joints is assessed, as well as the distribution of hardness, micro-and macrostructure through the joints (in the base material, nugget, heat affected zone and thermo-mechanically affected zone. Different combinations of the tool rotation speed and the welding speed are used, and the dependence of the properties of the joints on these parameters of welding technology is determined. [Projekat Ministarstva nauke Republike Srbije, br. TR 34018 i br. TR 35006

  19. Aa Ah Nak

    Science.gov (United States)

    Tha, Na Gya; Wus, Thay

    2017-01-01

    In this article, Aa Ah Nak, the authors' methodology presents not only various reflections but also diverse contradictions about the Aa Nii language as well as language revitalization. This article explores language foundation and how the Aa Nii language revitalization is inextricably linked to the genocide and resulting historic trauma pervasive…

  20. Assuring reliability of unconventional weld joint configurations in austenitic stainless steel pressure vessels through non-destructive examination

    International Nuclear Information System (INIS)

    Jayakumar, I.; Manimohan, M.; Chandrasekaran, G.V.; Abdul Majeeth, S.; Subrahmanyam, P.S.

    1996-01-01

    Design of weld configurations in engineering structures is based on NDE inspectability apart from other considerations. They are mostly standardised. This paper deals with the development of an effective NDE methodology for an unconventional weld joint configuration occurring in a critical pressure vessel with edge preparation orientations different from that normally encountered in fabrication of such vessels. It is K-type butt joint between a heavy load bearing member and a curved vessel wall resulting in an oblique fillet weld. The heavy load bearing functional requirement needs a high integrity fail safe joint during its operating life and the stringent quality level specified by customer was ensured at every stage of its workmanship through effective NDE relying on conventional methods as explained. (author)

  1. Modeling and control of a DC upset resistance butt welding process

    NARCIS (Netherlands)

    Naus, G.J.L.; Meulenberg, R.; Molengraft, van de M.J.G.

    2007-01-01

    This paper presents the analysis and synthesis of modeling and control of the DC upset resistance butt welding process used in rim production lines. A new control strategy is developed, enabling active control of the welding seam temperature and the upset size. As a result, set-up times and energy

  2. A new method to butt weld pipes with laser at different angles

    International Nuclear Information System (INIS)

    Gualini, M.M.S.

    1999-01-01

    Laser butt welding of pipes at different angles may be cumbersome and may require very expensive tooling. The pipe size may not allow using the laser for large volume throughputs. We propose a rotary optical head composed by an adjustable focus lens system and two reflecting mirrors. The laser beam is bent at 90 deg. C. so that weld can be performed inwards outwards. The optic head design compensates the rotary backlash and vibrations, like a penta prism thus ensuring a perfect follow up of the weld track. The optic head can be inclined at 45 deg. C. to laser butt weld pipe each other at 90 deg. C. In this case the laser beam focus position is computer controlled in order to keep the focus point always on the elliptical weld profile. The paper covers theoretical and practical aspects of the proposed device. (author)

  3. Effect of pin tool design on the material flow of dissimilar AA7075-AA6061 friction stir welds

    Science.gov (United States)

    Hasan, Mohammed M.; Ishak, M.; Rejab, M. R. M.

    2017-10-01

    Tool design is the most influential aspect in the friction stir welding (FSW) technology. Influence of pin tool geometry on material flow pattern are studied in this work during the FSW of dissimilar AA7075 and AA6061 aluminium alloys. Three truncated pin tool profiles (threaded, threaded with single flat, and unthreaded with single flat) were used to prepare the weldments. The workpieces were joined using a custom-made clamping system under 1100 rpm of spindle speed, 300 mm/min of traverse rate and 3° of tilt angle. The metallographic analysis showed that defect-free welds can be produced using the three pin tools with significant changes in the mixing stir zone structure. The results declared that the introducing of the flat on the cone of the probe deviates the pattern of the onion rings without changing the chemical composition of the created layers. This in turn improves the hardness distribution and tensile strength of the welded joint. It was also noted that both heat affected zone (HAZ) and thermal-mechanical affected zone (TMAZ) are similar in composition to their corresponding base materials (BM).

  4. Eutectic structures in friction spot welding joint of aluminum alloy to copper

    International Nuclear Information System (INIS)

    Shen, Junjun; Suhuddin, Uceu F. H.; Cardillo, Maria E. B.; Santos, Jorge F. dos

    2014-01-01

    A dissimilar joint of AA5083 Al alloy and copper was produced by friction spot welding. The Al-MgCuAl 2 eutectic in both coupled and divorced manners were found in the weld. At a relatively high temperature, mass transport of Cu due to plastic deformation, material flow, and atomic diffusion, combined with the alloy system of AA5083 are responsible for the ternary eutectic melting

  5. HAZ microstructure in joints made of X13CrMoCoVNbNB9-2-1 (PB2 steel welded with and without post-weld heat treatment

    Directory of Open Access Journals (Sweden)

    M. Łomozik

    2016-07-01

    Full Text Available The article presents the results of research butt welded joints made of X13CrMoCoVNbNB9-2-1 steel. The joints were welded with post-weld heat treatment PWHT and without PWHT, using the temper bead technique TBT. After welding the joint welded with PWHT underwent stress-relief annealing at 770 °C for 3 hours. The scope of structural tests included the microstructural examination of the coarse-grained heat affected zone (HAZ areas of the joints, the comparison of the morphology of these areas and the determination of carbide precipitate types of the coarse grain heat affected zone (CGHAZ of the joints welded with and without PWHT.

  6. Optimización del proceso de soldadura GMAW de uniones a tope de la aleación AA 6063-T5 basada en la metodología de superficie de respuesta y en la geometría del cordón de soldadura

    Directory of Open Access Journals (Sweden)

    Miguel, V.

    2012-10-01

    Full Text Available The geometry of the weld beads is characterized by the overhead, the width and the penetration. These values are indices of the behavior of the welded joint and therefore, they can be considered as factors that control the process. This work is performed to optimize the GMAW process of the aluminum alloy AA 6063-T5 by means of the response surface methodology (RSM. The variables herein considered are the arc voltage, the welding speed, the wire feed speed and the separation between surfaces in butt joints. The response functions that are herein studied are the overhead, the width, the penetration and the angle of the bead. The obtained results by RSM show high grade of agreement with the experimental values. The procedure is experimentally validated by welding for the theoretically obtained optimized technological conditions and a wide agreement between theoretical and experimental values is found.

    La geometría de los cordones de soldadura es caracterizada por el sobreespesor, la anchura y la penetración. Estos valores son indicadores del comportamiento de la unión soldada por lo que pueden considerarse como factores de control del proceso. En el presente trabajo se efectúa la optimización del proceso de soldadura por arco GMAW de la aleación AA 6063-T5 mediante la metodología de la superficie de respuesta (MSR. Las variables consideradas son la tensión del arco, la velocidad de soldeo, la velocidad de alimentación del electrodo y la separación de las superficies a unir. Las funciones de respuesta consideradas son el sobreespesor, anchura, penetración y el ángulo del cordón. Los resultados obtenidos mediante MSR se ajustan muy bien a los valores experimentales. El procedimiento es validado experimentalmente mediante el soldeo, para las condiciones tecnológicas optimizadas obtenidas de forma teórica, existiendo una gran concordancia entre los valores teóricos y los experimentales.

  7. Teacher's Guide to Architectural Styles. Skinner's Butte Historical District. Revised Edition.

    Science.gov (United States)

    Bauer, Mary; Neimand, Hahn

    This document is a teacher's guide to the historic buildings of Eugene, Oregon. Eighteen buildings in the Skinner's Butte Historical District are highlighted, including the U.S. Post Office, the Eagles Building, the Lane Hotel, the Oregon Electric Depot, the Southern Pacific Railroad Depot, and several houses. For each structure there is a brief…

  8. FIRE HAZARDS ANALYSIS - BUSTED BUTTE

    International Nuclear Information System (INIS)

    Longwell, R.; Keifer, J.; Goodin, S.

    2001-01-01

    The purpose of this fire hazards analysis (FHA) is to assess the risk from fire within individual fire areas at the Busted Butte Test Facility and to ascertain whether the DOE fire safety objectives are met. The objective, identified in DOE Order 420.1, Section 4.2, is to establish requirements for a comprehensive fire and related hazards protection program for facilities sufficient to minimize the potential for: (1) The occurrence of a fire related event. (2) A fire that causes an unacceptable on-site or off-site release of hazardous or radiological material that will threaten the health and safety of employees. (3) Vital DOE programs suffering unacceptable interruptions as a result of fire and related hazards. (4) Property losses from a fire and related events exceeding limits established by DOE. Critical process controls and safety class systems being damaged as a result of a fire and related events

  9. Effect of rotation speed and welding speed on Friction Stir Welding of AA1100 Aluminium alloy

    Science.gov (United States)

    Raja, P.; Bojanampati, S.; Karthikeyan, R.; Ganithi, R.

    2018-04-01

    Aluminum AA1100 is the most widely used grade of Aluminium due to its excellent corrosion resistance, high ductility and reflective finish, the selected material was welded with Friction Stir Welding (FSW) process on a CNC machine, using a combination of different tool rotation speed (1500 rpm, 2500 rpm, 3500 rpm) and welding speed (10 mm/min, 30 mm/min, 50 mm/min) as welding parameters. The effect of FSW using this welding parameter was studied by measuring the ultimate tensile strength of the welded joints. A high-speed steel tool was prepared for welding the Aluminium AA1100 alloy having an 8mm shoulder diameter and pin dimension of 4mm diameter and 2.8 mm length. The welded joints were tested using the universal testing machine. It was found that Ultimate Tensile Strength of FSW specimen was highest with a value of 98.08 MPa when the weld was performed at rotation speed of 1500 RPM and welding speed of 50 mm/min.

  10. Influence of PC-GTAW Parameters on the Microstructural and Mechanical Properties of Thin AISI 1008 Steel Joints

    Science.gov (United States)

    Kumar, Ravindra; Anant, Ramkishor; Ghosh, P. K.; Kumar, Ankit; Agrawal, B. P.

    2016-09-01

    Butt weld joints are prepared using pulse current gas tungsten arc welding out of thin sheets of AISI 1008 steel using various combinations of pulse parameters. During welding, the welding speed was kept high, but with the increase of welding speed the mean current was also increased to get the required weld joint at the constant heat input. The use of pulse current has led to improvement in mechanical and metallurgical properties of weld joints. It has resulted in less development of humping which is a common problem with high-speed welding. The undercut or dipped weld face is not observed severe. The tensile strength and hardness are enhanced by 12.5 and 12%. The increase of tensile strength and hardness is justified through TEM micrograph showing the presence of dislocation.

  11. Antiproton Accumulator (AA)

    CERN Multimedia

    Photographic Service

    1980-01-01

    The AA in its final stage of construction, before it disappeared from view under concrete shielding. Antiprotons were first injected, stochastically cooled and accumulated in July 1980. From 1981 on, the AA provided antiprotons for collisions with protons, first in the ISR, then in the SPS Collider. From 1983 on, it also sent antiprotons, via the PS, to the Low-Energy Antiproton Ring (LEAR). The AA was dismantled in 1997 and shipped to Japan.

  12. Effect of tool rotational speed on force generation, microstructure and mechanical properties of friction stir welded Al–Mg–Cr–Mn (AA 5052-O) alloy

    International Nuclear Information System (INIS)

    Moshwan, Raza; Yusof, Farazila; Hassan, M.A.; Rahmat, S.M.

    2015-01-01

    Highlights: • 3 mm thick AA 5052-O alloy plates were successfully joined by FSW process. • The joint was produced at 1000 rpm yielded a maximum tensile strength of 132 MPa. • The dissolution of β-Mg 2 Al 3 intermetallic phases of FSWed joints were reported. • Different axial forces acted on welding tool during welding were investigated. - Abstract: Friction stir welding (FSW) between 3 mm thick AA 5052-O aluminum alloy plates was investigated in the present study. Different welded specimens were produced by employing a constant tool traverse speed of 120 mm/min and by varying rotating speeds from 800 to 3000 rpm. The welded joints were characterized by its appearances, microstructural and mechanical properties at room temperature. The measurement of different forces acted on the tool during the FSW of AA 5052-O plates provided a significant insight to determine the quality of the welded joints. From the appearances of the welded joints it was evident that, except the tool rotational speed of 3000 rpm all other rotational speeds produced sound welded joints with smooth surface. The joint produced at 1000 rpm yielded a maximum tensile strength of 132 MPa which was 74% of the base material strength. Field emission scanning electron microscopy (FESEM) and energy dispersive spectroscopy (EDS) analyses on the stir zone suggested that, β-Mg 2 Al 3 intermetallic phases of the base material were mechanically fractured, smeared and mixed to different geometries due to tool stirring. The dissolution and redistribution of β-Mg 2 Al 3 second phase particles in the stir zone had a considerable effect on the reduction of the tensile strength of the welded joints. The reduction in hardness at the nugget zone (NZ) of the welded joints under different tool rotational speeds could be attributed to the dislocation of Mg-rich phases and segregation of Mg solute atoms at grain boundaries, which drew solute Mg atoms away from the α-aluminum matrix

  13. Microstructure and Strain Rate-Dependent Tensile Deformation Behavior of Fiber Laser-Welded Butt Joints of Dual-Phase Steels

    Science.gov (United States)

    Liu, Yang; Dong, Danyang; Han, Zhiqiang; Yang, Zhibin; Wang, Lu; Dong, Qingwei

    2018-05-01

    The microstructure and tensile deformation behavior of the fiber laser-welded similar and dissimilar dual-phase (DP) steel joints over a wide range of strain rates from 10-3 to 103 s-1 were investigated for the further applications on the lightweight design of vehicles. The high strain rate dynamic tensile deformation process and full-field strain distribution of the base metals and welded joints were examined using the digital image correlation method and high-speed photography. The strain rate effects on the stress-strain responses, tensile properties, deformation, and fracture behavior of the investigated materials were analyzed. The yield stress (YS) and ultimate tensile strength (UTS) of the dissimilar DP780/DP980 welded joints were lying in-between those of the DP780 and DP980 base metals, and all materials exhibited positive strain rate dependence on the YS and UTS. Owing to the microstructure heterogeneity, the welded joints showed relatively lower ductility in terms of total elongation (TE) than those of the corresponding base metals. The strain localization started before the maximum load was reached, and the strain localization occurred earlier during the whole deformation process with increasing strain rate. As for the dissimilar welded joint, the strain localization tended to occur in the vicinity of the lowest hardness value across the welded joint, which was in the subcritical HAZ at the DP780 side. As the strain rate increased, the typical ductile failure characteristic of the investigated materials did not change.

  14. Microstructure and Strain Rate-Dependent Tensile Deformation Behavior of Fiber Laser-Welded Butt Joints of Dual-Phase Steels

    Science.gov (United States)

    Liu, Yang; Dong, Danyang; Han, Zhiqiang; Yang, Zhibin; Wang, Lu; Dong, Qingwei

    2018-04-01

    The microstructure and tensile deformation behavior of the fiber laser-welded similar and dissimilar dual-phase (DP) steel joints over a wide range of strain rates from 10-3 to 103 s-1 were investigated for the further applications on the lightweight design of vehicles. The high strain rate dynamic tensile deformation process and full-field strain distribution of the base metals and welded joints were examined using the digital image correlation method and high-speed photography. The strain rate effects on the stress-strain responses, tensile properties, deformation, and fracture behavior of the investigated materials were analyzed. The yield stress (YS) and ultimate tensile strength (UTS) of the dissimilar DP780/DP980 welded joints were lying in-between those of the DP780 and DP980 base metals, and all materials exhibited positive strain rate dependence on the YS and UTS. Owing to the microstructure heterogeneity, the welded joints showed relatively lower ductility in terms of total elongation (TE) than those of the corresponding base metals. The strain localization started before the maximum load was reached, and the strain localization occurred earlier during the whole deformation process with increasing strain rate. As for the dissimilar welded joint, the strain localization tended to occur in the vicinity of the lowest hardness value across the welded joint, which was in the subcritical HAZ at the DP780 side. As the strain rate increased, the typical ductile failure characteristic of the investigated materials did not change.

  15. Constitutive behavior of as-cast AA1050, AA3104, and AA5182

    Science.gov (United States)

    van Haaften, W. M.; Magnin, B.; Kool, W. H.; Katgerman, L.

    2002-07-01

    Recent thermomechanical modeling to calculate the stress field in industrially direct-chill (DC) cast-aluminum slabs has been successful, but lack of material data limits the accuracy of these calculations. Therefore, the constitutive behavior of three aluminum alloys (AA1050, AA3104, and AA5182) was determined in the as-cast condition using tensile tests at low strain rates and from room temperature to solidus temperature. The parameters of two constitutive equations, the extended Ludwik equation and a combination of the Sellars-Tegart equation with a hardening law, were determined. In order to study the effect of recovery, the constitutive behavior after prestraining at higher temperatures was also investigated. To evaluate the quantified constitutive equations, tensile tests were performed simulating the deformation and cooling history experienced by the material during casting. It is concluded that both constitutive equations perform well, but the combined hardening-Sellars-Tegart (HST) equation has temperature-independent parameters, which makes it easier to implement in a DC casting model. Further, the deformation history of the ingot should be taken into account for accurate stress calculations.

  16. Effect of Multipass TIG and Activated TIG Welding Process on the Thermo-Mechanical Behavior of 316LN Stainless Steel Weld Joints

    Science.gov (United States)

    Ganesh, K. C.; Balasubramanian, K. R.; Vasudevan, M.; Vasantharaja, P.; Chandrasekhar, N.

    2016-04-01

    The primary objective of this work was to develop a finite element model to predict the thermo-mechanical behavior of an activated tungsten inert gas (ATIG)-welded joint. The ATIG-welded joint was fabricated using 10 mm thickness of 316LN stainless steel plates in a single pass. To distinguish the merits of ATIG welding process, it was compared with manual multipass tungsten inert gas (MPTIG)-welded joint. The ATIG-welded joint was fabricated with square butt edge configuration using an activating flux developed in-house. The MPTIG-welded joint was fabricated in thirteen passes with V-groove edge configuration. The finite element model was developed to predict the transient temperature, residual stress, and distortion of the welded joints. Also, microhardness, impact toughness, tensile strength, ferrite measurement, and microstructure were characterized. Since most of the recent publications of ATIG-welded joint was focused on the molten weld pool dynamics, this research work gives an insight on the thermo-mechanical behavior of ATIG-welded joint over MPTIG-welded joint.

  17. Fatigue properties of dissimilar metal laser welded lap joints

    Science.gov (United States)

    Dinsley, Christopher Paul

    This work involves laser welding austenitic and duplex stainless steel to zinc-coated mild steel, more specifically 1.2mm V1437, which is a Volvo Truck Coiporation rephosphorised mild steel. The work investigates both tensile and lap shear properties of similar and dissimilar metal laser welded butt and lap joints, with the majority of the investigation concentrating on the fatigue properties of dissimilar metal laser welded lap joints. The problems encountered when laser welding zinc-coated steel are addressed and overcome with regard to dissimilar metal lap joints with stainless steel. The result being the production of a set of guidelines for laser welding stainless steel to zinc-coated mild steel. The stages of laser welded lap joint fatigue life are defined and the factors affecting dissimilar metal laser welded lap joint fatigue properties are analysed and determined; the findings suggesting that dissimilar metal lap joint fatigue properties are primarily controlled by the local stress at the internal lap face and the early crack growth rate of the material at the internal lap face. The lap joint rotation, in turn, is controlled by sheet thickness, weld width and interfacial gap. Laser welded lap joint fatigue properties are found to be independent of base material properties, allowing dissimilar metal lap joints to be produced without fatigue failure occurring preferentially in the weaker parent material, irrespective of large base material property differences. The effects of Marangoni flow on the compositions of the laser weld beads are experimentally characterised. The results providing definite proof of the stirring mechanism within the weld pool through the use of speeds maps for chromium and nickel. Keywords: Laser welding, dissimilar metal, Zinc-coated mild steel, Austenitic stainless steel, Duplex stainless steel, Fatigue, Lap joint rotation, Automotive.

  18. Microstructure evolution of Al/Mg butt joints welded by gas tungsten arc with Zn filler metal

    International Nuclear Information System (INIS)

    Liu Fei; Zhang Zhaodong; Liu Liming

    2012-01-01

    Based on the idea of alloying welding seam, Gas tungsten arc welding method with pure Zn filler metal was chosen to join Mg alloy and Al alloy. The microstructures, phases, element distribution and fracture morphology of welding seams were examined. The results indicate that there was a transitional zone in the width of 80–100 μm between the Mg alloy substrate and fusion zone. The fusion zone was mainly composed of MgZn 2 , Zn-based solid solution and Al-based solid solution. The welding seam presented distinct morphology in different location owning to the quite high cooling rate of the molten pool. The addition of Zn metal could prevent the formation of Mg–Al intermetallics and form the alloyed welding seam during welding. Therefore, the tensile strengths of joints have been significantly improved compared with those of gas tungsten arc welded joints without Zn metal added. Highlights: ► Mg alloy AZ31B and Al alloy 6061 are welded successfully. ► Zinc wire is employed as a filler metal to form the alloyed welding seam. ► An alloyed welding seam is benefit for improving of the joint tensile strength.

  19. Effect of weld metal properties on fatigue crack growth behaviour of gas tungsten arc welded AISI 409M grade ferritic stainless steel joints

    International Nuclear Information System (INIS)

    Shanmugam, K.; Lakshminarayanan, A.K.; Balasubramanian, V.

    2009-01-01

    The effect of filler metals such as austenitic stainless steel, ferritic stainless steel and duplex stainless steel on fatigue crack growth behaviour of the gas tungsten arc welded ferritic stainless steel joints was investigated. Rolled plates of 4 mm thickness were used as the base material for preparing single 'V' butt welded joints. Centre cracked tensile (CCT) specimens were prepared to evaluate fatigue crack growth behaviour. Servo hydraulic controlled fatigue testing machine was used to evaluate the fatigue crack growth behaviour of the welded joints. From this investigation, it was found that the joints fabricated by duplex stainless steel filler metal showed superior fatigue crack growth resistance compared to the joints fabricated by austenitic and ferritic stainless steel filler metals. Higher yield strength, hardness and relatively higher toughness may be the reasons for superior fatigue performance of the joints fabricated by duplex stainless steel filler metal.

  20. The cytochrome P450 2AA gene cluster in zebrafish (Danio rerio): Expression of CYP2AA1 and CYP2AA2 and response to phenobarbital-type inducers

    Energy Technology Data Exchange (ETDEWEB)

    Kubota, Akira [Biology Department, Woods Hole Oceanographic Institution, Woods Hole, MA 02543 (United States); Bainy, Afonso C.D. [Biology Department, Woods Hole Oceanographic Institution, Woods Hole, MA 02543 (United States); Departamento de Bioquímica, CCB, Universidade Federal de Santa Catarina, Florianopolis, SC 88040-900 (Brazil); Woodin, Bruce R.; Goldstone, Jared V. [Biology Department, Woods Hole Oceanographic Institution, Woods Hole, MA 02543 (United States); Stegeman, John J., E-mail: jstegeman@whoi.edu [Biology Department, Woods Hole Oceanographic Institution, Woods Hole, MA 02543 (United States)

    2013-10-01

    The cytochrome P450 (CYP) 2 gene family is the largest and most diverse CYP gene family in vertebrates. In zebrafish, we have identified 10 genes in a new subfamily, CYP2AA, which does not show orthology to any human or other mammalian CYP genes. Here we report evolutionary and structural relationships of the 10 CYP2AA genes and expression of the first two genes, CYP2AA1 and CYP2AA2. Parsimony reconstruction of the tandem duplication pattern for the CYP2AA cluster suggests that CYP2AA1, CYP2AA2 and CYP2AA3 likely arose in the earlier duplication events and thus are most diverged in function from the other CYP2AAs. On the other hand, CYP2AA8 and CYP2AA9 are genes that arose in the latest duplication event, implying functional similarity between these two CYPs. A molecular model of CYP2AA1 showing the sequence conservation across the CYP2AA cluster reveals that the regions with the highest variability within the cluster map onto CYP2AA1 near the substrate access channels, suggesting differing substrate specificities. Zebrafish CYP2AA1 transcript was expressed predominantly in the intestine, while CYP2AA2 was most highly expressed in the kidney, suggesting differing roles in physiology. In the liver CYP2AA2 expression but not that of CYP2AA1, was increased by 1,4-bis [2-(3,5-dichloropyridyloxy)] benzene (TCPOBOP) and, to a lesser extent, by phenobarbital (PB). In contrast, pregnenolone 16α-carbonitrile (PCN) increased CYP2AA1 expression, but not CYP2AA2 in the liver. The results identify a CYP2 subfamily in zebrafish that includes genes apparently induced by PB-type chemicals and PXR agonists, the first concrete in vivo evidence for a PB-type response in fish. - Highlights: • A tandemly duplicated cluster of ten CYP2AA genes was described in zebrafish. • Parsimony and duplication analyses suggest pathways to CYP2AA diversity. • Homology models reveal amino acid positions possibly related to functional diversity. • The CYP2AA locus does not share synteny with

  1. The cytochrome P450 2AA gene cluster in zebrafish (Danio rerio): Expression of CYP2AA1 and CYP2AA2 and response to phenobarbital-type inducers

    International Nuclear Information System (INIS)

    Kubota, Akira; Bainy, Afonso C.D.; Woodin, Bruce R.; Goldstone, Jared V.; Stegeman, John J.

    2013-01-01

    The cytochrome P450 (CYP) 2 gene family is the largest and most diverse CYP gene family in vertebrates. In zebrafish, we have identified 10 genes in a new subfamily, CYP2AA, which does not show orthology to any human or other mammalian CYP genes. Here we report evolutionary and structural relationships of the 10 CYP2AA genes and expression of the first two genes, CYP2AA1 and CYP2AA2. Parsimony reconstruction of the tandem duplication pattern for the CYP2AA cluster suggests that CYP2AA1, CYP2AA2 and CYP2AA3 likely arose in the earlier duplication events and thus are most diverged in function from the other CYP2AAs. On the other hand, CYP2AA8 and CYP2AA9 are genes that arose in the latest duplication event, implying functional similarity between these two CYPs. A molecular model of CYP2AA1 showing the sequence conservation across the CYP2AA cluster reveals that the regions with the highest variability within the cluster map onto CYP2AA1 near the substrate access channels, suggesting differing substrate specificities. Zebrafish CYP2AA1 transcript was expressed predominantly in the intestine, while CYP2AA2 was most highly expressed in the kidney, suggesting differing roles in physiology. In the liver CYP2AA2 expression but not that of CYP2AA1, was increased by 1,4-bis [2-(3,5-dichloropyridyloxy)] benzene (TCPOBOP) and, to a lesser extent, by phenobarbital (PB). In contrast, pregnenolone 16α-carbonitrile (PCN) increased CYP2AA1 expression, but not CYP2AA2 in the liver. The results identify a CYP2 subfamily in zebrafish that includes genes apparently induced by PB-type chemicals and PXR agonists, the first concrete in vivo evidence for a PB-type response in fish. - Highlights: • A tandemly duplicated cluster of ten CYP2AA genes was described in zebrafish. • Parsimony and duplication analyses suggest pathways to CYP2AA diversity. • Homology models reveal amino acid positions possibly related to functional diversity. • The CYP2AA locus does not share synteny with

  2. Longitudinal study of experimental induction of AA amyloidosis in mice seeded with homologous and heterologous AA fibrils.

    Science.gov (United States)

    Muhammad, Naeem; Murakami, Tomoaki; Inoshima, Yasuo; Ishiguro, Naotaka

    2016-09-01

    To investigate pathogenesis and kinetics of experimentally induced murine AA amyloidosis seeded with homologous (murine) and heterologous (bovine) AA fibrils. Experimental AA amyloidosis was induced by administration of inflammatory stimulus and preformed AA fibrils to a total of 111 female C57/Black mice. In this longitudinal study, heterologous (bovine) as well as homologous (murine) AA fibrils were injected intraperitoneally to mice in various combinations. Re-stimulation was done at 120 or 300 days post first inoculation. To analyze the intensity of amyloid depositions in mice organs, immunohistochemical techniques and image J software were used. Assessment of cytokines level in sera was done using a Mouse Th1/Th2/Th17 Cytokine CBA Kit. Incidence and severity of AA amyloidosis were quite low in mice inoculated with heterologous bovine AA fibrils than homologous murine one. Homologous AA fibrils administration at first and second inoculation caused maximum amount of amyloid depositions and severe systemic form of amyloidosis. Increase in the level of pro-inflammatory cytokine IL-6 was observed after first inoculation, while second inoculation caused a further increase in the level of anti-inflammatory cytokine IL-10. AA amyloidosis can be induced by heterologous as well as homologous AA fibrils. Severity of AA amyloidosis induced with homologous AA fibrils is higher compared to heterologous AA fibrils.

  3. Effects of filling material and laser power on the formation of intermetallic compounds during laser-assisted friction stir butt welding of steel and aluminum alloys

    Science.gov (United States)

    Fei, Xinjiang; Jin, Xiangzhong; Peng, Nanxiang; Ye, Ying; Wu, Sigen; Dai, Houfu

    2016-11-01

    In this paper, two kinds of materials, Ni and Zn, are selected as filling material during laser-assisted friction stir butt welding of Q235 steel and 6061-T6 aluminum alloy, and their influences on the formation of intermetallic compounds on the steel/aluminum interface of the joints were first studied. SEM was used to analyze the profile of the intermetallic compound layer and the fractography of tensile fracture surfaces. In addition, EDS was applied to investigate the types of the intermetallic compounds. The results indicate that a thin iron-abundant intermetallic compound layer forms and ductile fracture mode occurs when Ni is added, but a thick aluminum-abundant intermetallic compound layer generates and brittle fracture mode occurs when Zn is added. So the tensile strength of the welds with Ni as filling material is greater than that with Zn as filling material. Besides, the effect of laser power on the formation of intermetallic compound layer when Ni is added was investigated. The preheated temperature field produced by laser beam in the cross section of workpiece was calculated, and the tensile strength of the joints at different laser powers was tested. Results show that only when suitable laser power is adopted, can suitable preheating temperature of the steel reach, then can thin intermetallic compound layer form and high tensile strength of the joints reach. Either excessive or insufficient laser power will reduce the tensile strength of the joints.

  4. Investigation and control of factors influencing resistance upset butt welding.

    OpenAIRE

    Kerstens, N.F.H.

    2010-01-01

    The purpose of this work is to investigate the factors influencing the resistance upset butt welding process to obtain an understanding of the metal behaviour and welding process characteristics, so that new automotive steels can be welded with reduced development time and fewer failures in production. In principle the welding process is rather simple, the materials to be joined are clamped between two electrodes and pressed together. Because there is an interface present with a higher resist...

  5. Summary of investigations of uranium deposits in the Pumpkin Buttes area, Johnson and Campbell Counties, Wyoming

    Science.gov (United States)

    Troyer, Max L.; McKay, Edward J.; Soister, Paul E.; Wallace, Stewart R.

    1954-01-01

    Uranium minerals were discovered in the Pumpkin Buttes area, Campbell and Johnson Counties, Wyo., by the U. S. Geological Survey in October 1951. From June to November 1952, an area of about 750 square miles was examined for uranium deposits, and 211 localities having abnormally high radioactivity were found; uranium minerals are visible at 121 of these localities. All known uranium mineralization in the area is restricted to sandstones of the Wasatch formation, except sparsely disseminated uranium in the sandstone of the White River formation, which caps the Pumpkin Buttes, mid several localities on the Great Pine Ridge southwest of the Pumpkin Buttes where iron-saturated sandstone and clinker in the Fort Union formation have above-normal radioactivity. The uranium occurrences in the Wasatch formation are in a red sandstone zone 450 to 900 feet above the base of the formation and are of two types: small concretionary masses of uranium, iron, manganese and vanadium minerals in sandstone, and irregular zones in which uranium minerals are disseminated in sandstone. The second type is usually larger but of lower grade than the first. Most of the localities at which uranium occurs are in a north-trending belt about 60 miles long and 18 miles in maximum width.

  6. Characterizing butt-rot fungi on USA-affiliated islands in the western Pacific

    Science.gov (United States)

    Phil Cannon; Ned B. Klopfenstein; Robert L. Schlub; Mee-Sook Kim; Yuko Ota; Norio Sahashi; Roland J. Quitugua; John W. Hanna; Amy L. Ross-Davis; J. D. Sweeney

    2014-01-01

    Ganoderma and Phellinus are genera that commonly cause tree butt-rot on USA-affiliated islands of the western Pacific. These fungal genera can be quite prevalent, especially in older mangrove stands. Although the majority of infections caused by these fungi lead to severe rotting of the heartwood, they typically do not directly kill the living tissues of the sapwood,...

  7. A.A., constructivism, and reflecting teams.

    Science.gov (United States)

    Nevels, B

    1997-12-01

    Numerous studies and clinical anecdotes reveal a relationship between attendance at A.A. meetings and/or degree of involvement in A.A. and maintenance of sobriety. Hypotheses as to how A.A. and/or the A.A. meeting is helpful to its members have ranged from a focus on factors common to all therapy groups, to aspects of A.A. "treatment" which are behavioral in nature. Presented here is another way of understanding A.A.'s effectiveness within the frame of more recent, constructivistic approaches to family therapy. In particular, the A.A. topic meeting is compared to the reflecting team concept of Tom Anderson.

  8. Special grain boundaries in the nugget zone of friction stir welded AA6061-T6 under various welding parameters

    Energy Technology Data Exchange (ETDEWEB)

    Tao, Wang [Key Lab of Liquid Structure and Heredity of Materials, Ministry of Education, Shandong University, Jinan 250061 (China); Yong, Zou, E-mail: yzou@sdu.edu.cn [Key Lab of Liquid Structure and Heredity of Materials, Ministry of Education, Shandong University, Jinan 250061 (China); Xuemei, Liu [Key Lab of Liquid Structure and Heredity of Materials, Ministry of Education, Shandong University, Jinan 250061 (China); Matsuda, Kenji [Department of Materials Science and Technology, Faculty of Engineering, University of Toyama, Toyama 930-8555 (Japan)

    2016-08-01

    The age hardenable AA6061-T6 plate was butt welded by friction stir welding. The total heat input, generated by friction between the tool and work piece and plastic deformation, results in a consumption of meta-stable phases in the nugget zone. Precipitation phenomena were closely related to the diffusion of the solute atoms. The existence of special grain boundaries like Σ1a and Σ3 will increase the difficulty in diffusion, which will improve the hardness in the nugget zone. Furthermore, the formation of Σ3 grain boundaries can result from an impingement of re-crystallized grains coming from texture components in twin relationship already. An appropriate strain level may benefit the development of the twin components with a similar intensity. The welding parameters have an effect on heat source mode and the strain level. Then, the type of dynamic re-crystallization and distribution of the special grain boundaries was altered by changing the parameters.

  9. Metal loading in Soda Butte Creek upstream of Yellowstone National Park, Montana and Wyoming; a retrospective analysis of previous research; and quantification of metal loading, August 1999

    Science.gov (United States)

    Boughton, G.K.

    2001-01-01

    Acid drainage from historic mining activities has affected the water quality and aquatic biota of Soda Butte Creek upstream of Yellowstone National Park. Numerous investigations focusing on metals contamination have been conducted in the Soda Butte Creek basin, but interpretations of how metals contamination is currently impacting Soda Butte Creek differ greatly. A retrospective analysis of previous research on metal loading in Soda Butte Creek was completed to provide summaries of studies pertinent to metal loading in Soda Butte Creek and to identify data gaps warranting further investigation. Identification and quantification of the sources of metal loading to Soda Butte Creek was recognized as a significant data gap. The McLaren Mine tailings impoundment and mill site has long been identified as a source of metals but its contribution relative to the total metal load entering Yellowstone National Park was unknown. A tracer-injection and synoptic-sampling study was designed to determine metal loads upstream of Yellowstone National Park.A tracer-injection and synoptic-sampling study was conducted on an 8,511-meter reach of Soda Butte Creek from upstream of the McLaren Mine tailings impoundment and mill site downstream to the Yellowstone National Park boundary in August 1999. Synoptic-sampling sites were selected to divide the creek into discrete segments. A lithium bromide tracer was injected continuously into Soda Butte Creek for 24.5 hours. Downstream dilution of the tracer and current-meter measurements were used to calculate the stream discharge. Stream discharge values, combined with constituent concentrations obtained by synoptic sampling, were used to quantify constituent loading in each segment of Soda Butte Creek.Loads were calculated for dissolved calcium, silica, and sulfate, as well as for dissolved and total-recoverable iron, aluminum, and manganese. Loads were not calculated for cadmium, copper, lead, and zinc because these elements were infrequently

  10. Detection of AA76, a Common Form of Amyloid A Protein, as a Way of Diagnosing AA Amyloidosis.

    Science.gov (United States)

    Sato, Junji; Okuda, Yasuaki; Kuroda, Takeshi; Yamada, Toshiyuki

    2016-01-01

    Reactive amyloid deposits consist of amyloid A (AA) proteins, the degradation products of serum amyloid A (SAA). Since the most common species of AA is the amino terminal portion produced by cleavage between residues 76 and 77 of SAA (AA76), the presence of AA76 in tissues could be a consequence of AA amyloid deposition. This study assessed the diagnostic significance of the detection of AA76 for AA amyloidosis using two different approaches. Biopsy specimens (n=130 from 54 subjects) from gastroduodenal mucosa or abdominal fat (n=9 from 9 subjects) of patients who had already been diagnosed with or were suspected of having AA amyloidosis were used. Fixed mucosal sections were subjected to immunohistochemistry using a newly developed antibody recognizing the carboxyl terminal end of AA76 (anti-AA76). The non-fixed materials from gastroduodenal mucosa or abdominal fat were subjected to immunoblotting for detection of the size of AA76. Among the gastroduodenal specimens (n=115) from already diagnosed patients, the positive rates of Congo red staining, immunohistochemistry using anti-AA76, and immunoblotting were 68.4%, 73.0%, and 92.2%, respectively. The anti-AA76 did not stain the supposed SAA in the blood or leakage, which was stained by anti-SAA antibody. AA76 was not detected either by immunohistochemistry or by immunoblot in the materials from patients in whom AA amyloidosis had been ruled out. In the abdominal fat, the immunoblot detected AA76 in 8 materials from 8 already diagnosed patients and did not in 1 patient whose gastroduodenal mucosa was negative. In conclusion, the detection of AA76 may alter the ability to diagnose AA amyloidosis. In immunohistochemistry for fixed specimens, the new anti-AA76 antibody can improve the specificity. Immunoblot for non-fixed materials, which can considerably improve the sensitivity, should be beneficial for small materials like abdominal fat. © 2016 by the Association of Clinical Scientists, Inc.

  11. Reduction method for residual stress of welded joint using random vibration

    International Nuclear Information System (INIS)

    Aoki, Shigeru; Nishimura, Tadashi; Hiroi, Tetsumaro

    2005-01-01

    Welded joints are used for construction of many structures. Residual stress is induced near the bead caused by locally given heat. Tensile residual stress on the surface may reduce fatigue strength. In this paper, a new method for reduction of residual stress using vibration during welding is proposed. As vibrational load, random vibration, white noise and filtered white noise are used. Two thin plates are butt-welded. Residual stress is measured with a paralleled beam X-ray diffractometer with scintillation counter after removing quenched scale chemically. It is concluded that tensile residual stress near the bead is reduced by using random vibration during welding

  12. Interfacial microstructure and mechanical property of Ti6Al4V/A6061 dissimilar joint by direct laser brazing without filler metal and groove

    International Nuclear Information System (INIS)

    Song, Zhihua; Nakata, Kazuhiro; Wu, Aiping; Liao, Jinsun

    2013-01-01

    Laser brazing of Ti6Al4V and A6061-T6 alloys with 2 mm thickness was conducted by focusing laser beam on aluminum alloy side, and the effect of laser offset distance on microstructure and mechanical properties of the dissimilar butt joint was investigated. Laser offset has a great influence on the thickness of interfacial intermetallic compound (IMC) layer and the mechanical property of joint. The thickness of interfacial IMC layer is less than 500 nm, and the average tensile strength of the joint reaches 64% of aluminum base material strength, when suitable welding conditions are used. The interfacial IMC is TiAl 3 . The formation of interfacial IMC layer and its effect on mechanical property of the joint are discussed in the present study.

  13. Mechanical properties of friction stir welded butt joint of steel/aluminium alloys: effect of tool geometry

    Science.gov (United States)

    Syafiq, W. M.; Afendi, M.; Daud, R.; Mazlee, M. N.; Majid, M. S. Abdul; Lee, Y. S.

    2017-10-01

    This paper described the mechanical properties from hardness testing and tensile testing of Friction Stir Welded (FSW) materials. In this project, two materials of aluminium and steel are welded using conventional milling machine and tool designed with different profile and shoulder size. During welding the temperature along the weld line is collected using thermocouples. Threaded pins was found to produce stronger joints than cylindrical pins. 20 mm diameter shoulder tool welded a slightly stronger joint than 18 mm diameter one, as well as softer nugget zone due to higher heat input. Threaded pins also contributed to higher weld temperature than cylindrical pins due to increase in pin contact surface. Generally, higher temperatures were recorded in aluminium side due to pin offset away from steel.

  14. Microstructure and mechanical properties of the TIG welded joints of fusion CLAM steel

    Energy Technology Data Exchange (ETDEWEB)

    Jiang Zhizhong, E-mail: zhizhongjiang2006@yahoo.com.c [School of Materials Science and Engineering, University of Science and Technology Beijing, Xueyuan Road, Beijing 100083 (China); Ren Litian; Huang Jihua; Ju Xin; Wu Huibin [School of Materials Science and Engineering, University of Science and Technology Beijing, Xueyuan Road, Beijing 100083 (China); Huang Qunying; Wu Yican [Institute of Plasma Physics, Chinese Academy of Sciences, Hefei, Anhui 230031 (China)

    2010-12-15

    The CLAM steel plates were butt-welded through manual tungsten inert gas welding (TIG) process, and the following post-welding heat treatment (PWHT) at 740 {sup o}C for 1 h. The microstructure and mechanical properties of the welded joints were measured. The results show that both hardening and softening occur in the weld joints before PWHT, but the hardening is not removed completely in the weld metal and the fusion zone after PWHT. In as-welded condition, the microstructure of the weld metal is coarse lath martensite, and softened zone in heat-affected zone (HAZ) consists of a mixture of tempered martensite and ferrite. After PWHT, a lot of carbides precipitate at all zones in weld joints. The microstructure of softened zone transforms to tempered sorbite. Tensile strength of the weld metal is higher than that of HAZ and base metal regardless of PWHT. However, the weld metal has poor toughness without PWHT. The impact energy of the weld metal after PWHT reaches almost the same level as the base metal. So it is concluded that microstructure and mechanical properties of the CLAM steel welded joints can be improved by a reasonable PWHT.

  15. 78 FR 21540 - Revisions to the California State Implementation Plan, Butte County Air Quality Management...

    Science.gov (United States)

    2013-04-11

    ... the California State Implementation Plan, Butte County Air Quality Management District and Sacramento Metropolitan Air Quality Management District AGENCY: Environmental Protection Agency (EPA). ACTION: Direct... Quality Management District (BCAQMD) and Sacramento Metropolitan Air Quality Management District (SMAQMD...

  16. Development of continuous cooling precipitation diagrams for aluminium alloys AA7150 and AA7020

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Y., E-mail: yong.zhang@outlook.com [ARC Centre of Excellence for Design in Light Metals, Department of Materials Engineering, Monash University, Clayton, VIC 3800 (Australia); Milkereit, B. [University of Rostock, Faculty of Mechanical Engineering and Marine Technology, Chair of Materials Science, 18051 Rostock (Germany); University of Rostock, Institute of Physics, Polymer Physics Group, 18051 Rostock (Germany); Kessler, O. [University of Rostock, Faculty of Mechanical Engineering and Marine Technology, Chair of Materials Science, 18051 Rostock (Germany); Schick, C. [University of Rostock, Institute of Physics, Polymer Physics Group, 18051 Rostock (Germany); Rometsch, P.A. [ARC Centre of Excellence for Design in Light Metals, Department of Materials Engineering, Monash University, Clayton, VIC 3800 (Australia)

    2014-01-25

    Highlights: • The DSC method was used for developing continuous cooling precipitation diagrams. • The quench-induced particles were observed by SEM for alloys AA7150 and AA7020. • There were more quench-induced particles in alloy AA7150. • Quench sensitivity of Al alloys can be evaluated by using the CCP diagrams. -- Abstract: Two commercial 7xxx series aluminium alloys with different solute contents and different quench-induced precipitation behaviour have been investigated by using a specialised differential scanning calorimetry (DSC) technique to record exothermal heat outputs during continuous cooling. Together with hardness testing and microstructural analysis, this DSC method was used to develop continuous cooling precipitation (CCP) diagrams for alloys AA7150 and AA7020. The results show that the total precipitation heat for each alloy decreases with increasing cooling rate. However, the excess specific heat at a given cooling rate in alloy AA7150 is much higher than that in alloy AA7020. It is evident that there are atleast three different quench-induced reactions in different temperature regimes for alloy AA7150 cooled at various linear cooling rates, but only equilibrium MgZn{sub 2} (η-phase) and Al{sub 2}CuMg (S-phase) particles were observed by scanning electron microscopy (SEM). There are at least two main precipitation peaks that can be found for alloy AA7020, which correspond to Mg{sub 2}Si and MgZn{sub 2} (η-phase). Furthermore, a method is developed to evaluate the quench sensitivity of an alloy based on a determination of the critical cooling rate. The maximum hardness values are reached at cooling rates that are faster than or similar to the critical cooling rate.

  17. Microstructure and mechanical properties of China low activation martensitic steel joint by TIG multi-pass welding with a new filler wire

    Science.gov (United States)

    Huang, Bo; Zhang, Junyu; Wu, Qingsheng

    2017-07-01

    Tungsten Inner Gas (TIG) welding is employed for joining of China low activation martensitic (CLAM) steel. A new filler wire was proposed, and the investigation on welding with various heat input and welding passes were conducted to lower the tendency towards the residual of δ ferrite in the joint. With the optimized welding parameters, a butt joint by multi-pass welding with the new filler wire was prepared to investigate the microstructure and mechanical properties. The microstructure of the joint was observed by optical microscope (OM) and scanning electron microscope (SEM). The hardness, Charpy impact and tensile tests of the joint were implemented at room temperature (25 °C). The results revealed that almost full martensite free from ferrite in the joints were obtained by multipass welding with the heat input of 2.26 kJ/mm. A certain degree of softening occurred at the heat affected zone of the joint according to the results of tensile and hardness tests. The as welded joints showed brittle fracture in the impact tests. However, the joints showed toughness fracture after tempering and relatively better comprehensive performance were achieved when the joints were tempered at 740 °C for 2 h.

  18. Ductile damage development in friction stir welded aluminum (AA2024) joints

    DEFF Research Database (Denmark)

    Nielsen, Kim Lau

    2008-01-01

    Ductile damage development in a friction stir welded aluminum joint subjected to tension is analyzed numerically by FE-analysis, based on a total Lagrangian formulation. An elastic-viscoplastic constitutive relation that accounts for nucleation and growth of microvoids is applied. Main focus...

  19. 77 FR 13072 - Salmon-Challis National Forest, Butte, Custer and Lemhi Counties, ID, Supplemental Environmental...

    Science.gov (United States)

    2012-03-05

    ... DEPARTMENT OF AGRICULTURE Forest Service Salmon-Challis National Forest, Butte, Custer and Lemhi Counties, ID, Supplemental Environmental Impact Statement to the 2009 Salmon- Challis National Forest... of intent to prepare a supplemental environmental impact statement. SUMMARY: The Salmon-Challis...

  20. Stress Distribution in the Dissimilar Metal Butt Weld of Nuclear Reactor Piping due to the Simulation Technique for the Repair Welding

    International Nuclear Information System (INIS)

    Lee, Hweeseung; Huh, Namsu; Kim, Jinsu; Lee, Jinho

    2013-01-01

    During welding, the dissimilar metal butt welds of nuclear piping are typically subjected to repair welding in order to eliminate defects that are found during post-weld inspection. It has been found that the repair weld can significantly increase the tensile residual stress in the weldment, and therefore, accurate estimation of the weld residual stress due to repair weld, especially for dissimilar metal welds using Ni-based alloy 82/182 in nuclear components, is of great importance in order to assess susceptibility to primary water stress corrosion cracking. In the present study, the stress distributions of dissimilar metal butt welds in nuclear reactor piping subjected to repair weld were investigated based on detailed nonlinear finite element analyses. Particular emphasis was placed on the variation of the stress distribution in the dissimilar metal butt weld according to the finite element welding analysis sequence for the repair welding process

  1. Multi-Objective Optimization of Friction Stir Welding Process Parameters of AA6061-T6 and AA7075-T6 Using a Biogeography Based Optimization Algorithm

    Directory of Open Access Journals (Sweden)

    Mehran Tamjidy

    2017-05-01

    Full Text Available The development of Friction Stir Welding (FSW has provided an alternative approach for producing high-quality welds, in a fast and reliable manner. This study focuses on the mechanical properties of the dissimilar friction stir welding of AA6061-T6 and AA7075-T6 aluminum alloys. The FSW process parameters such as tool rotational speed, tool traverse speed, tilt angle, and tool offset influence the mechanical properties of the friction stir welded joints significantly. A mathematical regression model is developed to determine the empirical relationship between the FSW process parameters and mechanical properties, and the results are validated. In order to obtain the optimal values of process parameters that simultaneously optimize the ultimate tensile strength, elongation, and minimum hardness in the heat affected zone (HAZ, a metaheuristic, multi objective algorithm based on biogeography based optimization is proposed. The Pareto optimal frontiers for triple and dual objective functions are obtained and the best optimal solution is selected through using two different decision making techniques, technique for order of preference by similarity to ideal solution (TOPSIS and Shannon’s entropy.

  2. Multi-Objective Optimization of Friction Stir Welding Process Parameters of AA6061-T6 and AA7075-T6 Using a Biogeography Based Optimization Algorithm.

    Science.gov (United States)

    Tamjidy, Mehran; Baharudin, B T Hang Tuah; Paslar, Shahla; Matori, Khamirul Amin; Sulaiman, Shamsuddin; Fadaeifard, Firouz

    2017-05-15

    The development of Friction Stir Welding (FSW) has provided an alternative approach for producing high-quality welds, in a fast and reliable manner. This study focuses on the mechanical properties of the dissimilar friction stir welding of AA6061-T6 and AA7075-T6 aluminum alloys. The FSW process parameters such as tool rotational speed, tool traverse speed, tilt angle, and tool offset influence the mechanical properties of the friction stir welded joints significantly. A mathematical regression model is developed to determine the empirical relationship between the FSW process parameters and mechanical properties, and the results are validated. In order to obtain the optimal values of process parameters that simultaneously optimize the ultimate tensile strength, elongation, and minimum hardness in the heat affected zone (HAZ), a metaheuristic, multi objective algorithm based on biogeography based optimization is proposed. The Pareto optimal frontiers for triple and dual objective functions are obtained and the best optimal solution is selected through using two different decision making techniques, technique for order of preference by similarity to ideal solution (TOPSIS) and Shannon's entropy.

  3. The Western Environmental Technology Office (WETO) Butte, Montana

    International Nuclear Information System (INIS)

    1994-10-01

    This document has been prepared to highlight the research, development, demonstration, testing and evaluation activities funded through the Western Environmental Technology Office (WETO) in Butte, Montana. Technologies and processes described have the potential to enhance DOE's cleanup and waste management efforts, as well as improve US industry's competitiveness in global environmental markets. This information has been assembled from recently produced Office of Technology Development (OTD) documents which highlight technology development activities within each of the OTD program elements. Projects include: Heavy metals contaminated soil project; In Situ remediation integrated program; Minimum additive waste stabilization program; Resource recovery project; Buried waste integrated demonstration; Mixed waste integrated program; Pollution prevention program; and Mine waste technology program

  4. [Risk control of traditional Chinese medicines containing aristolochis acids (AAs) based on influencing factors of content of AAs].

    Science.gov (United States)

    Tian, Jing-Zhuo; Liang, Ai-Hua; Liu, Jing; Zhang, Bo-Li

    2017-12-01

    Aristolochic acids (AAs) widely exist in such plants as Aristolochia and Asarum. The renal toxicity of AAs as well as its carcinogenicity to urinary system have been widely known. In 2003 and 2004, China prohibited the use of Aristolochiae Radix, Aristolochiae Manshuriensis Caulis and Aristolochiae Fangchi Radix, and required administering other AAs-containing medicines in accordance with the regulations for prescription drugs. In this paper, we retrieved literatures on the content determination of AAs in recent 10 years in China. It suggested that the AAs content is lower in Asarum herb, especially in its roots and rhizomes, and most of which do not show detectable amount of AA-I. Some of traditional Chinese medicines show fairly small amount of detectable AA-I. The AAs content in Aristolochia herb (including Fructus Aristolochiae, kaempfer dutchmanspipe root) is relatively high; however, there are fewer literatures for studying the content determination of AAs in Chinese patent medicines. There were many factors affecting AAs content, including the parts used, origins, processing methods, extraction process. It suggested that we should pay attention to the toxicity of Chinese medicines containing AAs and use these decoction pieces and traditional Chinese medicines cautiously. In addition, basic studies for the origins, processing methods and extraction process of Chinese patent medicines containing AAs, as well as supervision and detection of AAs content in traditional Chinese medicinal materials, decoction pieces and Chinese patent medicines shall be strengthened for reducing medication risk and guaranteeing clinical medication safety. Copyright© by the Chinese Pharmaceutical Association.

  5. Low Cycle Fatigue Behavior of Alloy 617 Base Metal and Welded Joints at Room Temperature and 850 .deg. C for VHTR Applications

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Seon Jin; Dew, Rando T. [Pukyong National Univ., Busan (Korea, Republic of); Kim, Woo Gon; Kim, Min Hwan [Korea Atomic Energy Research Institute, Daejeon (Korea, Republic of)

    2015-05-15

    Low cycle fatigue (LCF) is an important design consideration for high temperature IHX components. Moreover, some of the components are joined by welding techniques and therefore the welded joints are unavoidable in the construction of mechanical structures. Since Alloy 617 was introduced in early 1970s, many attempts have been made in the past two decades to evaluate the LCF and creep-fatigue behavior in Alloy 617 base metal at room temperature and high temperature. However, little research has focused on the evaluation and characterization of the Alloy 617 welded joints. butt-welded joint specimens was performed at room temperature and 850 .deg. C. Fatigue lives of GTAW welded joint specimens were lower than those of base metal specimens. LCF cracking and failure in welded specimens initiated in the weld metal zone and followed transgranluar dendritic paths for both at RT and 850 .deg. C.

  6. Age of the middle Palaeolithic site of La Butte d'Arvigny (Moissy-Cramayel, Seine-et-Marne); Datation du site paleolithique moyen de la Butte d'Arvigny (Moissy-Cramayel, Seine-et-Marne)

    Energy Technology Data Exchange (ETDEWEB)

    Laurent, M. [Ecole Nationale Superieure de Chimie, Lab. de Travaux Pratiques de Genie Chimique, 75 - Paris (France); Laurent, M.; Bahain, J.J.; Voinchet, P.; Ricard, J.L. [Lab. de Prehistoire du Museum National d' Histoire Naturelle, Institut de Paleontologie Humaine, UMR 6569 du CNRS, 75 - Paris (France); Rousseau, L. [Amiens Univ., Lab. de Sedimentologie et de Geochimie, 80 (France)

    2000-04-01

    The middle Palaeolithic site of La Butte d'Arvigny, close to Melun, was dated using electron spin resonance (ESR) method on burn flint. Five analysed burnt flints give a mean age of 90 000 years, which ascribes Arvigny to the Mousterian laminar complex of northern France. (authors)

  7. Observations of elk movement patterns on Fossil Butte National Monument

    Science.gov (United States)

    Olexa, Edward M.; Soileau, Suzanna Carrithers.; Allen, Leslie A.

    2014-01-01

    The elk herd that frequents Fossil Butte National Monument, a subset of the West Green River elk population, provides visitors with seasonal opportunities to view an iconic species of the western United States. Throughout the year, these elk range across a variety of private, State, and Federal lands within close proximity to the Monument. These lands are managed differently for various uses which can create challenging wildlife-management issues and influence the herd’s seasonal movements and distribution. Research lead by the USGS investigates some of the factors associated with these seasonal changes.

  8. AA under construction

    CERN Multimedia

    CERN PhotoLab

    1979-01-01

    The AA at an early stage of construction, in the newly built AA-Hall. Cable-trays already outline the shape of the accumulator ring. To the right are huge cable-drums for the pulse-forming-network (PFN) of the injection kicker. Seeing this picture, can one imagine that only 8 months later beams were circulating in the completed accumulator ring ?

  9. TIG-dressing of High Strength Butt Welded Connection. Part 2 : Physical Testing and Modelling

    NARCIS (Netherlands)

    Van Es, S.H.J.; Kolstein, M.H.; Pijpers, R.J.M.; Bijlaard, F.S.K.

    2014-01-01

    Weld improvement techniques are aimed at reducing the notch effects of welds and generally focus on two aspects: a change of geometry of the weld toe and a change of the weld residual stresses. In this paper, fatigue tests are discussed, performed on butt welded specimens in steel grades ranging

  10. TIG-dressing of high strength butt welded connection - Part 2: physical testing and modelling

    NARCIS (Netherlands)

    Es, S.H.J. van; Kolstein, M.H.; Pijpers, R.J.M.; Bijlaard, F.S.K.

    2013-01-01

    Weld improvement techniques are aimed at reducing the notch effects of welds and generally focus on two aspects: a change of geometry of the weld toe and a change of the weld residual stresses. In this paper, fatigue tests are discussed, performed on butt welded specimens in steel grades ranging

  11. Special metallurgy - the electrical butt-welding by flashing of sintered magnesium-magnesium oxide composites (1963); Metallurgie speciale - le soudage electrique en bout par etincelage du composite fritte magnesium-magnesie (1963)

    Energy Technology Data Exchange (ETDEWEB)

    Charleux, J [Commissariat a l' Energie Atomique, Saclay (France). Centre d' Etudes Nucleaires

    1963-07-01

    Electrical resistance welding has become quite important since World War II because of the need of a high yield in aeronautical production. Progress has been due in particular to the improvements made in electronically controlled apparatus making possible the automatic control of welding. For the butt-welding of sections requiring either a high production rate or a high quality weld, the flash butt-welding system has been very much developed these last few years. The use of this welding method is of great importance in the field of the bonding of oxidisable metals such as magnesium or aluminium and its alloys, because the welded joint is free from oxides. This study consists of general considerations on the flash-welding process with regard to temperature distribution in the parts during welding, and to electrical phenomena connected with flashing. Besides this general or theoretical section, we have applied the welding process to the bonding of sintered magnesium, a magnesium-magnesium oxide composite, whose use as a structural element in nuclear reactors is considered. (author) [French] Le soudage electrique par resistance a pris un essor important depuis la derniere guerre mondiale a cause du besoin de haut rendement pour la production aeronautique. Les progres ont ete possibles surtout par l'amelioration des appareils de commande electronique qui permettent un controle automatique de la soudure. Pour le soudage bout a bout de profiles, demandant soit un haut debit de fabrication, soit une haute qualite du joint soude, le procede de soudage en bout par etincelage a ete tres developpe ces dernieres annees. Ce mode de soudage a un domaine d'utilisation important dans la liaison des metaux oxydables tels le magnesium ou l'aluminium et ses alliages, du fait de la proprete du joint soude exempt d'oxydes. Cette etude comporte une consideration generale du processus de l'etincelage, quant a la repartition de la temperature dans les pieces pendant le soudage et aux

  12. Special metallurgy - the electrical butt-welding by flashing of sintered magnesium-magnesium oxide composites (1963); Metallurgie speciale - le soudage electrique en bout par etincelage du composite fritte magnesium-magnesie (1963)

    Energy Technology Data Exchange (ETDEWEB)

    Charleux, J. [Commissariat a l' Energie Atomique, Saclay (France). Centre d' Etudes Nucleaires

    1963-07-01

    Electrical resistance welding has become quite important since World War II because of the need of a high yield in aeronautical production. Progress has been due in particular to the improvements made in electronically controlled apparatus making possible the automatic control of welding. For the butt-welding of sections requiring either a high production rate or a high quality weld, the flash butt-welding system has been very much developed these last few years. The use of this welding method is of great importance in the field of the bonding of oxidisable metals such as magnesium or aluminium and its alloys, because the welded joint is free from oxides. This study consists of general considerations on the flash-welding process with regard to temperature distribution in the parts during welding, and to electrical phenomena connected with flashing. Besides this general or theoretical section, we have applied the welding process to the bonding of sintered magnesium, a magnesium-magnesium oxide composite, whose use as a structural element in nuclear reactors is considered. (author) [French] Le soudage electrique par resistance a pris un essor important depuis la derniere guerre mondiale a cause du besoin de haut rendement pour la production aeronautique. Les progres ont ete possibles surtout par l'amelioration des appareils de commande electronique qui permettent un controle automatique de la soudure. Pour le soudage bout a bout de profiles, demandant soit un haut debit de fabrication, soit une haute qualite du joint soude, le procede de soudage en bout par etincelage a ete tres developpe ces dernieres annees. Ce mode de soudage a un domaine d'utilisation important dans la liaison des metaux oxydables tels le magnesium ou l'aluminium et ses alliages, du fait de la proprete du joint soude exempt d'oxydes. Cette etude comporte une consideration generale du processus de l'etincelage, quant a la repartition de la temperature dans les pieces

  13. Tensile behavior of dissimilar friction stir welded joints of aluminium alloys

    International Nuclear Information System (INIS)

    Shanmuga Sundaram, N.; Murugan, N.

    2010-01-01

    The heat treatable aluminium alloy AA2024 is used extensively in the aircraft industry because of its high strength to weight ratio and good ductility. The non-heat treatable aluminium alloy AA5083 possesses medium strength and high ductility and used typically in structural applications, marine, and automotive industries. When compared to fusion welding processes, friction stir welding (FSW) process is an emerging solid state joining process which is best suitable for joining these alloys. The friction stir welding parameters such as tool pin profile, tool rotational speed, welding speed, and tool axial force influence the mechanical properties of the FS welded joints significantly. Dissimilar FS welded joints are fabricated using five different tool pin profiles. Central composite design with four parameters, five levels, and 31 runs is used to conduct the experiments and response surface method (RSM) is employed to develop the model. Mathematical regression models are developed to predict the ultimate tensile strength (UTS) and tensile elongation (TE) of the dissimilar friction stir welded joints of aluminium alloys 2024-T6 and 5083-H321, and they are validated. The effects of the above process parameters and tool pin profile on tensile strength and tensile elongation of dissimilar friction stir welded joints are analysed in detail. Joints fabricated using Tapered Hexagon tool pin profile have the highest tensile strength and tensile elongation, whereas the Straight Cylinder tool pin profile have the lowest tensile strength and tensile elongation. The results are useful to have a better understanding of the effects of process parameters, to fabricate the joints with desired tensile properties, and to automate the FS welding process.

  14. California State Implementation Plan; Butte County Air Quality Management District; New Source Review (NSR) Permitting Program

    Science.gov (United States)

    EPA is proposing to approve a revision to the Butte County Air Quality Management District (BCAQMD) portion of the California SIP concerning the District's New Source Review (NSR) permitting program for new and modified sources of air pollution.

  15. Fatigue strength of laser welded joint sheet; Laser yosetsu tsugite no hiro kyodo

    Energy Technology Data Exchange (ETDEWEB)

    Fujii, A; Yoshimura, T; Tsuboi, M; Takasago, T; Nishio, T [Toyota Motor Corp., Aichi (Japan)

    1997-10-01

    In this paper, fatigue strength of laser welded butt joint has been investigated. In order to obtain the influence of underfill and pitting, fatigue test was conducted with different sheet thickness and mechanical properties. Fatigue crack initiated at underfill and pitting in the weld metal. Stress concentration factor and hardness of the weld metal were considered to estimate fatigue limit. However, hardness of the weld metal has no significant effect on fatigue strength. As a result, fatigue strength was well estimated by hardness of base metal and stress concentration factor calculated from the shape of underflll and pitting. 7 refs., 9 figs., 5 tabs.

  16. 77 FR 18266 - Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines; Revised...

    Science.gov (United States)

    2012-03-27

    ... INTERNATIONAL TRADE COMMISSION [Investigation Nos. 731-TA-865-867 (Second Review)] Stainless Steel Butt-Weld Pipe Fittings From Italy, Malaysia, and the Philippines; Revised Schedule for the Subject Reviews AGENCY: United States International Trade Commission. ACTION: Notice. DATES: Effective Date: March...

  17. Laboratory Astrophysics Division of The AAS (LAD)

    Science.gov (United States)

    Salama, Farid; Drake, R. P.; Federman, S. R.; Haxton, W. C.; Savin, D. W.

    2012-10-01

    The purpose of the Laboratory Astrophysics Division (LAD) is to advance our understanding of the Universe through the promotion of fundamental theoretical and experimental research into the underlying processes that drive the Cosmos. LAD represents all areas of astrophysics and planetary sciences. The first new AAS Division in more than 30 years, the LAD traces its history back to the recommendation from the scientific community via the White Paper from the 2006 NASA-sponsored Laboratory Astrophysics Workshop. This recommendation was endorsed by the Astronomy and Astrophysics Advisory Committee (AAAC), which advises the National Science Foundation (NSF), the National Aeronautics and Space Administration (NASA), and the U.S. Department of Energy (DOE) on selected issues within the fields of astronomy and astrophysics that are of mutual interest and concern to the agencies. In January 2007, at the 209th AAS meeting, the AAS Council set up a Steering Committee to formulate Bylaws for a Working Group on Laboratory Astrophysics (WGLA). The AAS Council formally established the WGLA with a five-year mandate in May 2007, at the 210th AAS meeting. From 2008 through 2012, the WGLA annually sponsored Meetings in-a-Meeting at the AAS Summer Meetings. In May 2011, at the 218th AAS meeting, the AAS Council voted to convert the WGLA, at the end of its mandate, into a Division of the AAS and requested draft Bylaws from the Steering Committee. In January 2012, at the 219th AAS Meeting, the AAS Council formally approved the Bylaws and the creation of the LAD. The inaugural gathering and the first business meeting of the LAD were held at the 220th AAS meeting in Anchorage in June 2012. You can learn more about LAD by visiting its website at http://lad.aas.org/ and by subscribing to its mailing list.

  18. Laboratory Astrophysics Division of the AAS (LAD)

    Science.gov (United States)

    Salama, Farid; Drake, R. P.; Federman, S. R.; Haxton, W. C.; Savin, D. W.

    2012-01-01

    The purpose of the Laboratory Astrophysics Division (LAD) is to advance our understanding of the Universe through the promotion of fundamental theoretical and experimental research into the underlying processes that drive the Cosmos. LAD represents all areas of astrophysics and planetary sciences. The first new AAS Division in more than 30 years, the LAD traces its history back to the recommendation from the scientific community via the White Paper from the 2006 NASA-sponsored Laboratory Astrophysics Workshop. This recommendation was endorsed by the Astronomy and Astrophysics Advisory Committee (AAAC), which advises the National Science Foundation (NSF), the National Aeronautics and Space Administration (NASA), and the U.S. Department of Energy (DOE) on selected issues within the fields of astronomy and astrophysics that are of mutual interest and concern to the agencies. In January 2007, at the 209th AAS meeting, the AAS Council set up a Steering Committee to formulate Bylaws for a Working Group on Laboratory Astrophysics (WGLA). The AAS Council formally established the WGLA with a five-year mandate in May 2007, at the 210th AAS meeting. From 2008 through 2012, the WGLA annually sponsored Meetings in-a-Meeting at the AAS Summer Meetings. In May 2011, at the 218th AAS meeting, the AAS Council voted to convert the WGLA, at the end of its mandate, into a Division of the AAS and requested draft Bylaws from the Steering Committee. In January 2012, at the 219th AAS Meeting, the AAS Council formally approved the Bylaws and the creation of the LAD. The inaugural gathering and the first business meeting of the LAD were held at the 220th AAS meeting in Anchorage in June 2012. You can learn more about LAD by visiting its website at http://lad.aas.org/ and by subscribing to its mailing list.

  19. Butt Weldability for SS400 Using Laser-Arc Hybrid Welding

    International Nuclear Information System (INIS)

    Kim, Jong Do; Myoung, Gi Hoon; Park, Duck; Myoung, Gi Hoon; Park, In Duck

    2016-01-01

    This study presents results of an experimental investigation of the laser-arc, hybrid, butt welding process of SS400 structural steel. Welding parameters including laser power, welding current and speed were varied in order to obtain one-pass, full-penetration welds without defects. The conditions that resulted in optimal beads were identified. After welding, hardness measurements and microstructure observations were carried out in order to study weld properties. The mechanical properties of both the base material and welded specimen were compared based on the results of tensile strength measurements. The yield and tensile strengths were found to be similar

  20. Butt Weldability for SS400 Using Laser-Arc Hybrid Welding

    Energy Technology Data Exchange (ETDEWEB)

    Kim, Jong Do; Myoung, Gi Hoon; Park, Duck [Korea Maritime and Ocean Univ., Busan (Korea, Republic of); Myoung, Gi Hoon; Park, In Duck [Korea Institute of Machinery and Materials, Busan (Korea, Republic of)

    2016-07-15

    This study presents results of an experimental investigation of the laser-arc, hybrid, butt welding process of SS400 structural steel. Welding parameters including laser power, welding current and speed were varied in order to obtain one-pass, full-penetration welds without defects. The conditions that resulted in optimal beads were identified. After welding, hardness measurements and microstructure observations were carried out in order to study weld properties. The mechanical properties of both the base material and welded specimen were compared based on the results of tensile strength measurements. The yield and tensile strengths were found to be similar.

  1. Modeling knee joint endoprosthesis mode of deformation

    Science.gov (United States)

    Skeeba, V. Yu; Ivancivsky, V. V.

    2018-03-01

    The purpose of the work was to define the efficient design of the endoprosthesis, working in a multiple-cycle loading environment. Methodology and methods: triangulated surfaces of the base contact surfaces of endoprosthesis butt elements have been created using the PowerShape and SolidWorks software functional environment, and the assemblies of the possible combinations of the knee joint prosthetic designs have been prepared. The mode of deformation modeling took place in the multipurpose program complex ANSYS. Results and discussion: as a result of the numerical modeling, the following data were obtained for each of the developed knee joint versions: the distribution fields of absolute (total) and relative deformations; equivalent stress distribution fields; fatigue strength coefficient distribution fields. In the course of the studies, the following efficient design assembly has been established: 1) Ti-Al-V alloy composite femoral component with polymer inserts; 2) ceramic liners of the compound separator; 3) a Ti-Al-V alloy composite tibial component. The fatigue strength coefficient for the femoral component is 4.2; for the femoral component polymer inserts is 1.2; for the ceramic liners of the compound separator is 3.1; for the tibial component is 2.7. This promising endoprosthesis structure is recommended for further design and technological development.

  2. NCBI nr-aa BLAST: CBRC-DSIM-04-0001 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-04-0001 gb|AAS74960.1| 5-HT2 [Drosophila melanogaster] gb|AAS74962.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS74964.1| 5-HT2 [Drosophila melanogaster] gb|AAS74966.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS74970.1| 5-HT2 [Drosophila melanogaster] gb|AAS74972.1| 5-HT2 [Drosophila melanogaster]... gb|AAS74976.1| 5-HT2 [Drosophila melanogaster] gb|AAS74978.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS74979.1| 5-HT2 [Drosophila melanogaster] gb|AAS74980.1| 5-HT2 [Drosophila melanogaster

  3. NCBI nr-aa BLAST: CBRC-DSIM-04-0001 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-04-0001 gb|AAS74999.1| 5-HT2 [Drosophila melanogaster] gb|AAS75013.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS75024.1| 5-HT2 [Drosophila melanogaster] gb|AAS75026.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS75043.1| 5-HT2 [Drosophila melanogaster] gb|AAS75052.1| 5-HT2 [Drosophila melanogaster]... gb|AAS75056.1| 5-HT2 [Drosophila melanogaster] gb|AAS75073.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS75095.1| 5-HT2 [Drosophila melanogaster] AAS74999.1 1e-156 96% ...

  4. NCBI nr-aa BLAST: CBRC-DMEL-04-0001 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DMEL-04-0001 gb|AAS74999.1| 5-HT2 [Drosophila melanogaster] gb|AAS75013.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS75024.1| 5-HT2 [Drosophila melanogaster] gb|AAS75026.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS75043.1| 5-HT2 [Drosophila melanogaster] gb|AAS75052.1| 5-HT2 [Drosophila melanogaster]... gb|AAS75056.1| 5-HT2 [Drosophila melanogaster] gb|AAS75073.1| 5-HT2 [Drosophila mela...nogaster] gb|AAS75095.1| 5-HT2 [Drosophila melanogaster] AAS74999.1 1e-165 100% ...

  5. Weldability of dissimilar joint between F82H and SUS316L under fiber laser welding

    Energy Technology Data Exchange (ETDEWEB)

    Serizawa, Hisashi [Joining and Welding Research Institute, Osaka University, 11-1 Mihogaoka, Ibaraki, Osaka 567-0047 (Japan); Mori, Daiki; Shirai, Yuma; Ogiwara, Hiroyuki; Mori, Hiroaki [Graduate School of Engineering, Osaka University, 2-1 Yamadaoka, Suita, Osaka 565-0871 (Japan)

    2013-10-15

    Highlights: • The microstructure of F82H/SUS316L dissimilar joint can be divided into four regions. • In the case without beam position shift, hardness of WM cannot be reduced by PWHT. • The fiber laser welding would be applicable for constructing the dissimilar joint. -- Abstract: As one of the high beam quality heat sources, 4 kW fiber laser was applied for joining between reduced activation ferritic/martensitic steel, F82H and SUS316L austenitic stainless steel, and the microstructural analyses and Vickers hardness measurements were carried out before and after post-weld heat treatment (PWHT). The microstructure of joint can be divided into four regions which are base metal of F82H, heat affected zone (HAZ) in F82H, weld metal (WM) and base metal of SUS316L. Also, it is revealed that the high-power fiber laser can be employed for constructing butt joint between F82H and SUS316L by applying PWHT and shifting the laser beam position to SUS316L, where the distance between the contact face and beam should be set as a range from radius to diameter of laser beam.

  6. Weldability of dissimilar joint between F82H and SUS316L under fiber laser welding

    International Nuclear Information System (INIS)

    Serizawa, Hisashi; Mori, Daiki; Shirai, Yuma; Ogiwara, Hiroyuki; Mori, Hiroaki

    2013-01-01

    Highlights: • The microstructure of F82H/SUS316L dissimilar joint can be divided into four regions. • In the case without beam position shift, hardness of WM cannot be reduced by PWHT. • The fiber laser welding would be applicable for constructing the dissimilar joint. -- Abstract: As one of the high beam quality heat sources, 4 kW fiber laser was applied for joining between reduced activation ferritic/martensitic steel, F82H and SUS316L austenitic stainless steel, and the microstructural analyses and Vickers hardness measurements were carried out before and after post-weld heat treatment (PWHT). The microstructure of joint can be divided into four regions which are base metal of F82H, heat affected zone (HAZ) in F82H, weld metal (WM) and base metal of SUS316L. Also, it is revealed that the high-power fiber laser can be employed for constructing butt joint between F82H and SUS316L by applying PWHT and shifting the laser beam position to SUS316L, where the distance between the contact face and beam should be set as a range from radius to diameter of laser beam

  7. BUSTED BUTTE TEST FACILITY GROUND SUPPORT CONFIRMATION ANALYSIS

    International Nuclear Information System (INIS)

    Bonabian, S.

    1998-01-01

    The main purpose and objective of this analysis is to confirm the validity of the ground support design for Busted Butte Test Facility (BBTF). The highwall stability and adequacy of highwall and tunnel ground support is addressed in this analysis. The design of the BBTF including the ground support system was performed in a separate document (Reference 5.3). Both in situ and seismic loads are considered in the evaluation of the highwall and the tunnel ground support system. In this analysis only the ground support designed in Reference 5.3 is addressed. The additional ground support installed (still work in progress) by the constructor is not addressed in this analysis. This additional ground support was evaluated by the A/E during a site visit and its findings and recommendations are addressed in this analysis

  8. California Air Quality State Implementation Plans; Final Approval; Butte County Air Quality Management District; Stationary Source Permits

    Science.gov (United States)

    EPA is taking final action to approve a revision to the Butte County Air Quality Management District (BCAQMD) portion of the California State Implementation Plan (SIP). This revision concerns the District's New Source Review (NSR) permitting program.

  9. NCBI nr-aa BLAST: CBRC-DYAK-02-0049 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DYAK-02-0049 gb|AAS74383.1| 5-HT1B [Drosophila melanogaster] gb|AAS74385.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74397.1| 5-HT1B [Drosophila melanogaster] gb|AAS74398.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74401.1| 5-HT1B [Drosophila melanogaster] gb|AAS74414.1| 5-HT1B [Drosophila melanog...aster] gb|AAS74416.1| 5-HT1B [Drosophila melanogaster] gb|AAS74418.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74419.1| 5-HT1B [Drosophila melanogaster] gb|AAS74424.1| 5-HT1B [Drosophila mela

  10. NCBI nr-aa BLAST: CBRC-DMEL-02-0053 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DMEL-02-0053 gb|AAS74380.1| 5-HT1B [Drosophila melanogaster] gb|AAS74382.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74389.1| 5-HT1B [Drosophila melanogaster] gb|AAS74402.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74403.1| 5-HT1B [Drosophila melanogaster] gb|AAS74405.1| 5-HT1B [Drosophila melanog...aster] gb|AAS74406.1| 5-HT1B [Drosophila melanogaster] gb|AAS74411.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74412.1| 5-HT1B [Drosophila melanogaster] gb|AAS74413.1| 5-HT1B [Drosophila mela

  11. NCBI nr-aa BLAST: CBRC-DYAK-02-0049 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DYAK-02-0049 gb|AAS74384.1| 5-HT1B [Drosophila melanogaster] gb|AAS74386.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74388.1| 5-HT1B [Drosophila melanogaster] gb|AAS74390.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74392.1| 5-HT1B [Drosophila melanogaster] gb|AAS74394.1| 5-HT1B [Drosophila melanog...aster] gb|AAS74395.1| 5-HT1B [Drosophila melanogaster] gb|AAS74396.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74404.1| 5-HT1B [Drosophila melanogaster] gb|AAS74408.1| 5-HT1B [Drosophila mela

  12. NCBI nr-aa BLAST: CBRC-DMEL-02-0053 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DMEL-02-0053 gb|AAS74384.1| 5-HT1B [Drosophila melanogaster] gb|AAS74386.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74388.1| 5-HT1B [Drosophila melanogaster] gb|AAS74390.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74392.1| 5-HT1B [Drosophila melanogaster] gb|AAS74394.1| 5-HT1B [Drosophila melanog...aster] gb|AAS74395.1| 5-HT1B [Drosophila melanogaster] gb|AAS74396.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74404.1| 5-HT1B [Drosophila melanogaster] gb|AAS74408.1| 5-HT1B [Drosophila mela

  13. NCBI nr-aa BLAST: CBRC-DSIM-02-0056 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-02-0056 gb|AAS74384.1| 5-HT1B [Drosophila melanogaster] gb|AAS74386.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74388.1| 5-HT1B [Drosophila melanogaster] gb|AAS74390.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74392.1| 5-HT1B [Drosophila melanogaster] gb|AAS74394.1| 5-HT1B [Drosophila melanog...aster] gb|AAS74395.1| 5-HT1B [Drosophila melanogaster] gb|AAS74396.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74404.1| 5-HT1B [Drosophila melanogaster] gb|AAS74408.1| 5-HT1B [Drosophila mela

  14. NCBI nr-aa BLAST: CBRC-DSIM-02-0057 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-02-0057 gb|AAS74185.1| 5-HT1A [Drosophila melanogaster] gb|AAS74209.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74210.1| 5-HT1A [Drosophila melanogaster] gb|AAS74211.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74224.1| 5-HT1A [Drosophila melanogaster] gb|AAS74234.1| 5-HT1A [Drosophila melanog...aster] gb|AAS74254.1| 5-HT1A [Drosophila melanogaster] gb|AAS74258.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74262.1| 5-HT1A [Drosophila melanogaster] gb|AAS74278.1| 5-HT1A [Drosophila mela

  15. NCBI nr-aa BLAST: CBRC-DSIM-02-0056 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-02-0056 gb|AAS74383.1| 5-HT1B [Drosophila melanogaster] gb|AAS74385.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74397.1| 5-HT1B [Drosophila melanogaster] gb|AAS74398.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74401.1| 5-HT1B [Drosophila melanogaster] gb|AAS74414.1| 5-HT1B [Drosophila melanog...aster] gb|AAS74416.1| 5-HT1B [Drosophila melanogaster] gb|AAS74418.1| 5-HT1B [Drosophila mela...nogaster] gb|AAS74419.1| 5-HT1B [Drosophila melanogaster] gb|AAS74424.1| 5-HT1B [Drosophila mela

  16. NCBI nr-aa BLAST: CBRC-DSIM-02-0057 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-02-0057 gb|AAS74195.1| 5-HT1A [Drosophila melanogaster] gb|AAS74276.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74292.1| 5-HT1A [Drosophila melanogaster] gb|AAS74298.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74303.1| 5-HT1A [Drosophila melanogaster] gb|AAS74304.1| 5-HT1A [Drosophila melanog...aster] gb|AAS74321.1| 5-HT1A [Drosophila melanogaster] gb|AAS74359.1| 5-HT1A [Drosophila melanogaster] AAS74195.1 1e-176 97% ...

  17. 40 CFR Appendix A to Subpart Aa of... - Applicability of General Provisions (40 CFR Part 63, Subpart A) to Subpart AA

    Science.gov (United States)

    2010-07-01

    ... (40 CFR Part 63, Subpart A) to Subpart AA A Appendix A to Subpart AA of Part 63 Protection of... Hazardous Air Pollutants From Phosphoric Acid Manufacturing Plants Pt. 63, Subpt. AA, App. A Appendix A to Subpart AA of Part 63—Applicability of General Provisions (40 CFR Part 63, Subpart A) to Subpart AA 40 CFR...

  18. Age of the middle Palaeolithic site of La Butte d'Arvigny (Moissy-Cramayel, Seine-et-Marne)

    International Nuclear Information System (INIS)

    Laurent, M.; Laurent, M.; Bahain, J.J.; Voinchet, P.; Ricard, J.L.; Rousseau, L.

    2000-01-01

    The middle Palaeolithic site of La Butte d'Arvigny, close to Melun, was dated using electron spin resonance (ESR) method on burn flint. Five analysed burnt flints give a mean age of 90 000 years, which ascribes Arvigny to the Mousterian laminar complex of northern France. (authors)

  19. 76 FR 5205 - Carbon Steel Butt-Weld Pipe Fittings from Brazil, China, Japan, Taiwan, and Thailand

    Science.gov (United States)

    2011-01-28

    ...)] Carbon Steel Butt-Weld Pipe Fittings from Brazil, China, Japan, Taiwan, and Thailand AGENCY: United... Thailand. SUMMARY: The Commission hereby gives notice of the scheduling of expedited reviews pursuant to..., Taiwan, and Thailand would be likely to lead to continuation or recurrence of material injury within a...

  20. 75 FR 60814 - Carbon Steel Butt-Weld Pipe Fittings From Brazil, China, Japan, Taiwan, and Thailand

    Science.gov (United States)

    2010-10-01

    ...)] Carbon Steel Butt-Weld Pipe Fittings From Brazil, China, Japan, Taiwan, and Thailand AGENCY: United... Thailand. SUMMARY: The Commission hereby gives notice that it has instituted reviews pursuant to section... Thailand would be likely to lead to continuation or recurrence of material injury. Pursuant to section 751...

  1. Effect of supplementation of arachidonic acid (AA) or a combination of AA plus docosahexaenoic acid on breastmilk fatty acid composition

    NARCIS (Netherlands)

    Smit, EN; Koopmann, M; Boersma, ER; Muskiet, FAJ

    We investigated whether supplementation with arachidonic acid (20:4 omega 6; AA), ora combination of AA and docosahexaenoic acid (22:6 omega 3; DHA) would affect human milk polyunsaturated fatty acid (PUFA) composition. Ten women were daily supplemented with 300 mg AA, eight with 300 mg AA, 110 mg

  2. Activity of vegetative insecticidal proteins Vip3Aa58 and Vip3Aa59 of Bacillus thuringiensis against lepidopteran pests.

    Science.gov (United States)

    Baranek, Jakub; Kaznowski, Adam; Konecka, Edyta; Naimov, Samir

    2015-09-01

    Vegetative insecticidal proteins (Vips) secreted by some isolates of Bacillus thuringiensis show activity against insects and are regarded as insecticides against pests. A number of B. thuringiensis strains harbouring vip3A genes were isolated from different sources and identified by using a PCR based approach. The isolates with the highest insecticidal activity were indicated in screening tests, and their vip genes were cloned and sequenced. The analysis revealed two polymorphic Vip protein forms, which were classified as Vip3Aa58 and Vip3Aa59. After expression of the vip genes, the proteins were isolated and characterized. The activity of both toxins was estimated against economically important lepidopteran pests of woodlands (Dendrolimus pini), orchards (Cydia pomonella) and field crops (Spodoptera exigua). Vip3Aa58 and Vip3Aa59 were highly toxic and their potency surpassed those of many Cry proteins used in commercial bioinsecticides. Vip3Aa59 revealed similar larvicidal activity as Vip3Aa58 against S. exigua and C. pomonella. Despite 98% similarity of amino acid sequences of both proteins, Vip3Aa59 was significantly more active against D. pini. Additionally the effect of proteolytic activation of Vip58Aa and Vip3Aa59 on toxicity of D. pini and S. exigua was studied. Both Vip3Aa proteins did not show any activity against Tenebrio molitor (Coleoptera) larvae. The results suggest that the Vip3Aa58 and Vip3Aa59 toxins might be useful for controlling populations of insect pests of crops and forests. Copyright © 2015 Elsevier Inc. All rights reserved.

  3. A Precise Visual Method for Narrow Butt Detection in Specular Reflection Workpiece Welding

    Directory of Open Access Journals (Sweden)

    Jinle Zeng

    2016-09-01

    Full Text Available During the complex path workpiece welding, it is important to keep the welding torch aligned with the groove center using a visual seam detection method, so that the deviation between the torch and the groove can be corrected automatically. However, when detecting the narrow butt of a specular reflection workpiece, the existing methods may fail because of the extremely small groove width and the poor imaging quality. This paper proposes a novel detection method to solve these issues. We design a uniform surface light source to get high signal-to-noise ratio images against the specular reflection effect, and a double-line laser light source is used to obtain the workpiece surface equation relative to the torch. Two light sources are switched on alternately and the camera is synchronized to capture images when each light is on; then the position and pose between the torch and the groove can be obtained nearly at the same time. Experimental results show that our method can detect the groove effectively and efficiently during the welding process. The image resolution is 12.5 μm and the processing time is less than 10 ms per frame. This indicates our method can be applied to real-time narrow butt detection during high-speed welding process.

  4. Selected Welding Techniques, Part 2

    National Research Council Canada - National Science Library

    1964-01-01

    Partial contents: CONVENTIONAL WELD JOINTS VERSUS BUTT JOINTS IN 1-INCH ALUMINUM PLATE, SPECIAL WELD JOINT PREPARATION, UPSET METAL EDGES FOR INCREASED WELD JOINT STRENGTH, OUT-OF-POSITION WELDING OF HEAVY GAGE...

  5. Disk Laser Welding of Car Body Zinc Coated Steel Sheets / Spawanie Laserem Dyskowym Blach Ze Stali Karoseryjnej Ocynkowanej

    Directory of Open Access Journals (Sweden)

    Lisiecki A.

    2015-12-01

    Full Text Available Autogenous laser welding of 0.8 mm thick butt joints of car body electro-galvanized steel sheet DC04 was investigated. The Yb:YAG disk laser TruDisk 3302 with the beam spot diameter of 200 μm was used. The effect of laser welding parameters and technological conditions on weld shape, penetration depth, process stability, microstructure and mechanical performance was determined. It was found that the laser beam spot focused on the top surface of a butt joint tends to pass through the gap, especially in the low range of heat input and high welding speed. All test welds were welded at a keyhole mode, and the weld metal was free of porosity. Thus, the keyhole laser welding of zinc coated steel sheets in butt configuration provides excellent conditions to escape for zinc vapours, with no risk of porosity. Microstructure, microhardness and mechanical performance of the butt joints depend on laser welding conditions thus cooling rate and cooling times. The shortest cooling time t8/5 was calculated for 0.29 s.

  6. 76 FR 19788 - Carbon Steel Butt-Weld Pipe Fittings From Brazil, China, Japan, Taiwan, and Thailand

    Science.gov (United States)

    2011-04-08

    ...)] Carbon Steel Butt-Weld Pipe Fittings From Brazil, China, Japan, Taiwan, and Thailand Determinations On... fittings from Brazil, China, Japan, Taiwan, and Thailand would be likely to lead to continuation or recurrence of material injury to an industry in the United States within a reasonably foreseeable time. \\1...

  7. Hybrid FSWeld-bonded joint fatigue behaviour

    Science.gov (United States)

    Lertora, Enrico; Mandolfino, Chiara; Gambaro, Carla; Pizzorni, Marco

    2018-05-01

    Aluminium alloys, widely used in aeronautics, are increasingly involved in the automotive industry due to the good relationship between mechanical strength and specific weight. The lightening of the structures is the first objective, which allows the decreasing in the weight in motion. The use of aluminium alloys has also seen the introduction of the Friction Stir Welding (FSW) technique for the production of structural overlapping joints. FSW allows us to weld overlap joints free from defects, but with the presence of a structural notch further aggravated by the presence of a "hook" defect near the edge of the weld. Furthermore, FSW presents a weld penetration area connected to the tool geometry and penetration. The experimental activity will be focused on the combination of two different joining techniques, which can synergistically improve the final joint resistance. In particular, the welding and bonding process most commonly known as weld-bonding is defined as a hybrid process, as it combines two different junction processes. In this paper we analyse FSWelded AA6082 aluminium alloy overlapped joint with the aim of quantitatively evaluating the improvement provided by the presence of an epoxy adhesive between the plates. After optimising the weld-bonding process, the mechanical behaviour of welded joints will be analysed by static and dynamic tests. The presence of the adhesive should limit the negative effect of the structural notch inevitable in a FSW overlapped joint.

  8. NCBI nr-aa BLAST: CBRC-DMEL-02-0054 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DMEL-02-0054 gb|AAS74186.1| 5-HT1A [Drosophila melanogaster] gb|AAS74187.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74231.1| 5-HT1A [Drosophila melanogaster] gb|AAS74233.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74373.1| 5-HT1A [Drosophila melanogaster] AAS74186.1 0.0 100% ...

  9. NCBI nr-aa BLAST: CBRC-DYAK-02-0048 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DYAK-02-0048 gb|AAS74186.1| 5-HT1A [Drosophila melanogaster] gb|AAS74187.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74231.1| 5-HT1A [Drosophila melanogaster] gb|AAS74233.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74373.1| 5-HT1A [Drosophila melanogaster] AAS74186.1 1e-163 91% ...

  10. NCBI nr-aa BLAST: CBRC-DSIM-02-0057 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-02-0057 gb|AAS74196.1| 5-HT1A [Drosophila melanogaster] gb|AAS74220.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74309.1| 5-HT1A [Drosophila melanogaster] gb|AAS74310.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74335.1| 5-HT1A [Drosophila melanogaster] AAS74196.1 1e-176 97% ...

  11. NCBI nr-aa BLAST: CBRC-DSIM-02-0057 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-DSIM-02-0057 gb|AAS74184.1| 5-HT1A [Drosophila melanogaster] gb|AAS74194.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74236.1| 5-HT1A [Drosophila melanogaster] gb|AAS74326.1| 5-HT1A [Drosophila mela...nogaster] gb|AAS74372.1| 5-HT1A [Drosophila melanogaster] AAS74184.1 1e-177 97% ...

  12. Rotary friction welding of dissimilar joints and bonding interface characterization by EDX and XPS

    Energy Technology Data Exchange (ETDEWEB)

    Alves, Eder Paduan; Dollinger, Christian Avila [Instituto de Aeronautica e Espaco (IAE), Sao Jose dos Campos, SP (Brazil); Marcuzzo, Jossano Saldanha; Baldan, Mauricio Ribeiro; Toledo, Rafael Cardoso; Piorino Neto, Francisco; An, Chen Ying, E-mail: eder.padua@yahoo.com.br [Instituto Nacional de Pesquisas Espaciais (INPE), Sao Jose dos Campos, SP (Brazil)

    2016-07-01

    Full text: Welding of dissimilar materials has been a challenge to engineering. The study and development of new union processes that meet the requirements of projects in the aerospace, nuclear and aviation sector are of great importance to the scientific and productive means. The Rotary friction welding process (RFW) is a process of union that occurs in the solid state, without occurrence of fusion between the parties, and that have like the main bonding mechanisms the diffusion and mechanical mixture. This work has as objective the obtaining of dissimilar joints involving AA 6351-T6 alloy and stainless steel AISI 304l for applications in the aerospace area. The joints obtained by RFW who had procedures and qualified welding process have undergone the techniques of Energy Dispersive X-Ray Spectroscopy (EDX) and X-Ray Photoelectron Spectroscopy (XPS) for analysis of the bonding interface. Were obtained joints with superior mechanical properties the AA 6351-T6 alloy, with the fracture occurring in aluminum away from the bonding interface. The analyses carried out by EDX and XPS have shown the occurrence of interdiffusion among the main elements of the materials involved. The Rotary friction welding process proved to be a great method for obtaining of joints between dissimilar materials that are not possible by fusion welding processes. (author)

  13. Rotary friction welding of dissimilar joints and bonding interface characterization by EDX and XPS

    International Nuclear Information System (INIS)

    Alves, Eder Paduan; Dollinger, Christian Avila; Marcuzzo, Jossano Saldanha; Baldan, Mauricio Ribeiro; Toledo, Rafael Cardoso; Piorino Neto, Francisco; An, Chen Ying

    2016-01-01

    Full text: Welding of dissimilar materials has been a challenge to engineering. The study and development of new union processes that meet the requirements of projects in the aerospace, nuclear and aviation sector are of great importance to the scientific and productive means. The Rotary friction welding process (RFW) is a process of union that occurs in the solid state, without occurrence of fusion between the parties, and that have like the main bonding mechanisms the diffusion and mechanical mixture. This work has as objective the obtaining of dissimilar joints involving AA 6351-T6 alloy and stainless steel AISI 304l for applications in the aerospace area. The joints obtained by RFW who had procedures and qualified welding process have undergone the techniques of Energy Dispersive X-Ray Spectroscopy (EDX) and X-Ray Photoelectron Spectroscopy (XPS) for analysis of the bonding interface. Were obtained joints with superior mechanical properties the AA 6351-T6 alloy, with the fracture occurring in aluminum away from the bonding interface. The analyses carried out by EDX and XPS have shown the occurrence of interdiffusion among the main elements of the materials involved. The Rotary friction welding process proved to be a great method for obtaining of joints between dissimilar materials that are not possible by fusion welding processes. (author)

  14. Heat input effect of friction stir welding on aluminium alloy AA 6061-T6 welded joint

    Directory of Open Access Journals (Sweden)

    Sedmak Aleksandar

    2016-01-01

    Full Text Available This paper deals with the heat input and maximum temperature developed during friction stir welding with different parameters. Aluminium alloy (AA 6061-T6 has been used for experimental and numerical analysis. Experimental analysis is based on temperature measurements by using infrared camera, whereas numerical analysis was based on empirical expressions and finite element method. Different types of defects have been observed in respect to different levels of heat input.

  15. Comparison of susceptibility to pitting corrosion of AA2024-T4, AA7075-T651 and AA7475-T761 aluminium alloys in neutral chloride solutions using electrochemical noise analysis

    International Nuclear Information System (INIS)

    Na, Kyung-Hwan; Pyun, Su-Il

    2008-01-01

    The susceptibility to pitting corrosion of AA2024-T4, AA7075-T651 and AA7475-T761 aluminium alloys was investigated in aqueous neutral chloride solution for the purpose of comparison using electrochemical noise measurement. The experimentally measured electrochemical noises were analysed based upon the combined stochastic theory and shot-noise theory using the Weibull distribution function. From the occurrence of two linear regions on one Weibull probability plot, it was suggested that there existed two stochastic processes of uniform corrosion and pitting corrosion; pitting corrosion was distinguished from uniform corrosion in terms of the frequency of events in the stochastic analysis. Accordingly, the present analysis method allowed us to investigate pitting corrosion independently. The susceptibility to pitting corrosion was appropriately evaluated by determining pit embryo formation rate in the stochastic analysis. The susceptibility was decreased in the following order: AA2024-T4 (the naturally aged condition), AA7475-T761 (the overaged condition) and AA7075-T651 (the near-peak-aged condition)

  16. Noble Gas Isotope Evidence for Mantle Volatiles in the Cu-Mo Porphyry and Main Stage Polymetallic Veins at Butte, Montana

    Science.gov (United States)

    Hofstra, A. H.; Rusk, B. G.; Manning, A. H.; Hunt, A. G.; Landis, G. P.

    2017-12-01

    Recent studies suggest that volatiles released from mafic intrusions may be important sources of heat, sulfur, and metals in porphyry Cu-Mo-Au and epithermal Au-Ag deposits associated with intermediate to silicic stocks. The huge Cu-Mo porphyry and Main Stage polymetallic vein deposits at Butte are well suited to test this hypothesis because there is no geologic or isotopic evidence of basaltic intrusions in the mine or drill holes. The Butte porphyry-vein system is associated with quartz monzonite stocks and dikes within the southwest part of the Late Cretaceous Boulder batholith. The Boulder batholith was emplaced into Mesoproterozoic to Mesozoic sedimentary rocks and Late Cretaceous volcanic rocks. The Boulder batholith and Butte intrusions have Sri and eNd values indicative of crustal contamination. Eu and Ce anomalies in zircon from Butte intrusions provide evidence of oxidation due to magma degassing. To ascertain the source of volatiles in this system, 11 samples from the Cu-Mo porphyry and 16 from Main Stage veins were selected. The isotopic composition of Ar, Ne, and He extracted from fluid inclusions in quartz, magnetite, pyrite, chalcopyrite, sphalerite, galena, enargite, and covellite were determined. Helium isotopes exceed blank levels in all samples and Ne and Ar in some samples. On a 38Ar/36Ar vs. 40Ar/36Ar diagram, data plot near air. On a 20Ne/22Ne vs. 21Ne/22Ne diagram, data extend from air along the trajectories of OIB and MORB. On a 36Ar/4He vs. 3He/4He RA diagram, data extend from crust toward the air-mantle mixing line. The maximum 3He/4He RA values in the Cu-Mo porphyry (2.86) and Main Stage veins (3.46) are from pyrite and these values correspond to 36 and 43 % mantle helium. The Ne and He results show that fluid inclusions contain volatiles discharged from mantle magmas and that these volatiles were diluted by groundwater containing He derived from country rocks. Despite the lack of mafic intrusions in the Butte magmatic center, noble gas

  17. AA Index

    Data.gov (United States)

    National Oceanic and Atmospheric Administration, Department of Commerce — The geomagnetic aa index provides a long climatology of global geomagnetic activity using 2 antipodal observatories at Greenwich and Melbourne- IAGA Bulletin 37,...

  18. Experimental transmission of AA amyloidosis by injecting the AA amyloid protein into interleukin-1 receptor antagonist knockout (IL-1raKO) mice.

    Science.gov (United States)

    Watanabe, K; Uchida, K; Chambers, J K; Tei, M; Shoji, A; Ushio, N; Nakayama, H

    2015-05-01

    The incidence of AA amyloidosis is high in humans with rheumatoid arthritis and several animal species, including cats and cattle with prolonged inflammation. AA amyloidosis can be experimentally induced in mice using severe inflammatory stimuli and a coinjection of AA amyloid; however, difficulties have been associated with transmitting AA amyloidosis to a different animal species, and this has been attributed to the "species barrier." The interleukin-1 receptor antagonist knockout (IL-1raKO) mouse, a rodent model of human rheumatoid arthritis, has been used in the transmission of AA amyloid. When IL-1raKO and BALB/c mice were intraperitoneally injected with mouse AA amyloid together with a subcutaneous pretreatment of 2% AgNO3, all mice from both strains that were injected with crude or purified murine AA amyloid developed AA amyloidosis. However, the amyloid index, which was determined by the intensity of AA amyloid deposition, was significantly higher in IL-1raKO mice than in BALB/c mice. When IL-1raKO and BALB/c mice were injected with crude or purified bovine AA amyloid together with the pretreatment, 83% (5/6 cases) and 38% (3/8 cases) of IL-1raKO mice and 17% (1/6 cases) and 0% (0/6 cases) of BALB/c mice, respectively, developed AA amyloidosis. Similarly, when IL-1raKO and BALB/c mice were injected with crude or purified feline AA amyloid, 33% (2/6 cases) and 88% (7/8 cases) of IL-1raKO mice and 0% (0/6 cases) and 29% (2/6 cases) of BALB/c mice, respectively, developed AA amyloidosis. These results indicated that IL-1raKO mice are a useful animal model for investigating AA amyloidogenesis. © The Author(s) 2014.

  19. Partially melted zone cracking in AA6061 welds

    International Nuclear Information System (INIS)

    Prasad Rao, K.; Ramanaiah, N.; Viswanathan, N.

    2008-01-01

    Partially melted zone (PMZ) cracking susceptibility in AA6061 alloy was studied. Role of prior thermal history, gas tungsten arc welding techniques such as continuous current (CC) and pulsed current (PC) and use of different fillers (AA4043 and AA5356) were studied. Role of different grain refiners such as scandium, zirconium and Tibor in the above fillers was studied. Varestraint test was used to study the PMZ cracking susceptibility. Metallurgical analysis was done to corroborate the results. PMZ cracking was severe in T6 temper than in T4 irrespective of filler material. PMZ cracking susceptibility was more with AA5356 than in AA4043. It was less with pulsed current GTAW. PMZ cracking susceptibility was reduced with addition of grain refiners. Out of all, lowest PMZ cracking susceptibility was observed with 0.5%Sc addition to fusion zone through AA4043 filler and PC technique. The concentrations of magnesium and silicon were reduced at the PMZ grain boundaries with grain refiner additions to fusion zone through AA5356 or AA4043

  20. Partially melted zone cracking in AA6061 welds

    Energy Technology Data Exchange (ETDEWEB)

    Prasad Rao, K. [Department of Metallurgical and Materials Engineering, Indian Institute of Technology Madras, Chennai (India)], E-mail: kpr@iitm.ac.in; Ramanaiah, N. [Sri Kalahasteeswara Institute of Technology, Srikalahasti (India); Viswanathan, N. [Defence Research and Development Laboratory, Hyderabad (India)

    2008-07-01

    Partially melted zone (PMZ) cracking susceptibility in AA6061 alloy was studied. Role of prior thermal history, gas tungsten arc welding techniques such as continuous current (CC) and pulsed current (PC) and use of different fillers (AA4043 and AA5356) were studied. Role of different grain refiners such as scandium, zirconium and Tibor in the above fillers was studied. Varestraint test was used to study the PMZ cracking susceptibility. Metallurgical analysis was done to corroborate the results. PMZ cracking was severe in T6 temper than in T4 irrespective of filler material. PMZ cracking susceptibility was more with AA5356 than in AA4043. It was less with pulsed current GTAW. PMZ cracking susceptibility was reduced with addition of grain refiners. Out of all, lowest PMZ cracking susceptibility was observed with 0.5%Sc addition to fusion zone through AA4043 filler and PC technique. The concentrations of magnesium and silicon were reduced at the PMZ grain boundaries with grain refiner additions to fusion zone through AA5356 or AA4043.

  1. Influence of nanoporous structure on mechanical strength of aluminium and aluminium alloy adhesive structural joints

    International Nuclear Information System (INIS)

    Spadaro, C; Dispenza, C; Sunseri, C

    2006-01-01

    The influence of surface treatments on the mechanical strength of adhesive joints was investigated. The attention was focused on AA2024 alloy because it is extensively used in both the automotive and aerospace industries. Adhesive joints fabricated with pure aluminium were also investigated in order to evidence possible differences in the surface features after identical treatments. Before joining with a commercial epoxy adhesive, metal substrates were subjected to different kinds of treatment and the surfaces were characterized by SEM analysis. The formation of a microporous surface in the AA2024 alloy, upon etching and anodizing, is discussed on the basis of the role of the intermetallic particles and their electrochemical behaviour with respect to the aluminium matrix. Moreover, nanostructured porous oxide layers on both type of substrate were also formed, as a consequence of the anodizing process. Differences in their morphologies were revealed as a function of both the applied voltage and the presence of alloying elements. On this basis, an explanation of the different values of fracture energy measured by means of T-peel tests carried out on the corresponding joints was attempted

  2. 75 FR 430 - Notice of Intent To Prepare an Environmental Impact Statement for the Sigurd-Red Butte...

    Science.gov (United States)

    2010-01-05

    ...; UTU-83067] Notice of Intent To Prepare an Environmental Impact Statement for the Sigurd-Red Butte...) Cedar City Field Office, Cedar City, Utah, intends to prepare an Environmental Impact Statement (EIS... Fishlake National Forests), State of Utah, Millard County, Sevier County, Beaver County, Utah Division of...

  3. Features of residual stresses in duplex stainless steel butt welds

    Science.gov (United States)

    Um, Tae-Hwan; Lee, Chin-Hyung; Chang, Kyong-Ho; Nguyen Van Do, Vuong

    2018-04-01

    Duplex stainless steel finds increasing use as an alternative to austenitic stainless steel, particularly where chloride or sulphide stress corrosion cracking is of primary concern, due to the excellent combination of strength and corrosion resistance. During welding, duplex stainless steel does not create the same magnitude or distribution of weld-induced residual stresses as those in welded austenitic stainless steel due to the different physical and mechanical properties between them. In this work, an experimental study on the residual stresses in butt-welded duplex stainless steel is performed utilizing the layering technique to investigate the characteristics of residual stresses in the weldment. Three-dimensional thermos-mechanical-metallurgical finite element analysis is also performed to confirm the residual stress measurements.

  4. Microstructure feature of friction stir butt-welded ferritic ductile iron

    International Nuclear Information System (INIS)

    Chang, Hung-Tu; Wang, Chaur-Jeng; Cheng, Chin-Pao

    2014-01-01

    Highlights: • Defect-free ferritic ductile iron joints is fabricated by FSW. • The welding nugget is composed of graphite, martensite, and recrystallized ferrite. • The graphite displays a striped pattern in the surface and advancing side. • The ferritic matrix transforms into martensite structure during welding. • High degree of plastic deformation is found on the advancing side. - Abstract: This study conducted friction stir welding (FSW) by using the butt welding process to join ferritic ductile iron plates and investigated the variations of microsturcture in the joined region formed after welding. No defects appeared in the resulting experimental weld, which was formed using a 3-mm thick ductile iron plate and tungsten carbide alloy stir rod to conduct FSW at a rotational speed of 982 rpm and traveling speed of 72 mm/min. The welding region was composed of deformed graphite, martensite phase, and dynamically recrystallized ferrite structures. In the surface region and on the advancing side (AS), the graphite displayed a striped configuration and the ferritic matrix transformed into martensite. On the retreating side (RS), the graphite surrounded by martensite remained as individual granules and the matrix primarily comprised dynamically recrystallized ferrite. After welding, diffusion increased the carbon content of the austenite around the deformed graphite nodules, which transformed into martensite during the subsequent cooling process. A micro Vickers hardness test showed that the maximum hardness value of the martensite structures in the weld was approximately 800 HV. An analysis using an electron probe X-ray microanalyzer (EPMA) indicated that its carbon content was approximately 0.7–1.4%. The peak temperature on the RS, 8 mm from the center of the weld, measured 630 °C by the thermocouple. Overall, increased severity of plastic deformation and process temperature near the upper stir zone (SZ) resulted in distinct phase transformation

  5. Hot cracking of welded joints of the 7CrMoVTiB 10-10 (T/P24) steel

    Energy Technology Data Exchange (ETDEWEB)

    Adamiec, J, E-mail: janusz.adamiec@polsl.pl [Department of Materials Science, Silesian University of Technology, Krasinskiego 8, 40-019 Katowice (Poland)

    2011-05-15

    Bainitic steel 7CrMoVTiB10-10 is one the newest steels for waterwalls of modern industrial boilers. In Europe, attempts have been made to make butt welded joints of pipes made of this steel of the diameter up to 51 mm and thickness up to 8 mm. Many cracks have been observed in the welded joint, both during welding and transport and storage. The reasons of cracking and the prevention methods have not been investigated. No comprehensive research is carried out in Europe in order to automate the welding process of the industrial boiler elements made of modern bainitic steel, such as 7CrMoVTiB10-10. There is no information about its overall, operative and local weldability, influence of heat treatment, as well as about resistance of the joints to cracking during welding and use. The paper presents experience of Energoinstal SA from development of technology and production of waterwalls of boilers made of the 7CrMoVTiB 10-10 steel on a multi-head automatic welder for submerged arc welding.

  6. Experimental research on safety assurance of advanced WWER fuel cycles

    International Nuclear Information System (INIS)

    Krainov, Ju.; Kukushkin, Ju.

    2002-01-01

    The paper presents the results of experimental investigations on substantiation of implementation of a modernized butt joint for the WWER-440 reactor, carried out in the critical test facility 'P' in the RRC 'Kurchatov Institute'. The comparison results of the calculation and experimental data obtained in the physical startup of Volgodonsk NPP-1 with the WWER-1000 are also given. In the implementation of four-year fuel cycle in the WWER-440 with the average enrichment of fuel makeup 3.82% it was solved to conduct experimental research of power distribution in the vicinity of control rod butt junction. Moreover, it was assumed that adequate actions should be applied to eliminate inadmissible power jumps, if necessary. It is not available to measure their values in NPP conditions. Therefore, the power distribution near the butt joint was studied in a 19-rod bank installed in the critical test facility 'P' first for the normal design of the joint when surrounding fuel assemblies enrichment goes up. Then a set of calculation and tests was fulfilled to optimize a butt junction design. On the base of this research the composition of a butt junction was advanced by placing Hf plates into the junction. The effectiveness of modernized butt joint design was experimentally confirmed. In Volgodonsk NPP-1 with WWER-1000 the four-year fuel cycle is being implemented. During the physical startup of the reactor the measurements of the reactivity effects and coefficients were measured at the minimum controlled flux level, and the parameters of a number of critical states were recorded. The data obtained were compared with the calculation. The validity of the certified code package for forecasting the neutronic characteristics of WWER-1000 cores in the implementation of a four year fuel cycle has been supported (Authors)

  7. The AA disappearing under concrete shielding

    CERN Multimedia

    CERN PhotoLab

    1982-01-01

    When the AA started up in July 1980, the machine stood freely in its hall, providing visitors with a view through the large window in the AA Control Room. The target area, in which the high-intensity 26 GeV/c proton beam from the PS hit the production target, was heavily shielded, not only towards the outside but also towards the AA-Hall. However, electrons and pions emanating from the target with the same momentum as the antiprotons, but much more numerous, accompanied these through the injection line into the AA ring. The pions decayed with a half-time corresponding to approximately a revolution period (540 ns), whereas the electrons lost energy through synchrotron radiation and ended up on the vacuum chamber wall. Electrons and pions produced the dominant component of the radiation level in the hall and the control room. With operation times far exceeding original expectations, the AA had to be buried under concrete shielding in order to reduce the radiation level by an order of magnitude.

  8. Critical Gap distance in Laser Butt-welding

    DEFF Research Database (Denmark)

    Bagger, Claus; Olsen, Flemming Ove

    1999-01-01

    In a number of systematic laboratory experiments the critical gap distance that results in sound beads in laser butt welding is sought identified. By grinding the edges of the sheets, a number of "reference" welds are made and compared to the sheets with shear cut edges. In the tests the gap...... was set at 0.00, 0.02, 0.05, 0.08 and 0.10 mm. Mild steel (St 1203) with a thickness of 0.75 and 1.25 mm with and without zinc coating were analysed. A total of 120 welds were made at different welding speeds.As quality norm DIN 8563 was used to divide the welds into quality classes. A number of welds...... were also x-ray photographed.Of the weld combinations analysed 80 % were of high quality and 17 % of a non-acceptable quality. 90 % of the bad welds had a gap distance larger than 0.05 mm. The results showed that 85 % of the bad welds were shear cut and only 15 % grinded. Two third of the bad welds...

  9. Critical Gap distance in Laser Butt-welding

    DEFF Research Database (Denmark)

    Bagger, Claus; Olsen, Flemming Ove

    of "reference" welds are made and compared to sheets with the edges shear cut. The gap distance is precisely controlled by inserting spacers between the sheets. In the tests the gap is set at 0.00, 0.02, 0.05, 0.08 and 0.10 mm. Mild steel (St 1203) with thickness? of 0.75 and 1.25 mm with and without zinc......When butt-welding metal sheets with high power lasers the gap distance between the sheets determine the final quality of the seam. In a number of systematic laboratory experiments the critical gap distance that results in sound beads is identified. By grinding the edges of the sheets, a number...... coating were analysed. A total of 120 welds are made at different welding speeds.As quality norm DIN 8563 is used to divide the welds into quality classes. Since this norm only deals with surface defects a number of welds are also x-ray photographed.According to DIN 8563 the welds have classes of either B...

  10. Monogenetic volcanoes fed by interconnected dikes and sills in the Hopi Buttes volcanic field, Navajo Nation, USA

    Science.gov (United States)

    Muirhead, James D.; Van Eaton, Alexa R.; Re, Giuseppe; White, James D. L.; Ort, Michael H.

    2016-01-01

    Although monogenetic volcanic fields pose hazards to major cities worldwide, their shallow magma feeders (networks. Analysis of vent alignments using the pyroclastic massifs and other eruptive centers (e.g., maar-diatremes) shows a NW-SE trend, parallel to that of dikes in the region. We therefore infer that dikes fed many of the eruptions. Dikes are also observed in places transforming to transgressive (ramping) sills. Estimates of the observable volume of dikes (maximum volume of 1.90 × 106 m3) and sills (minimum volume of 8.47 × 105 m3) in this study reveal that sills at Hopi Buttes make up at least 30 % of the shallow intruded volume (∼2.75 × 106 m3 total) within 350 m of the paeosurface. We have also identified saucer-shaped sills, which are not traditionally associated with monogenetic volcanic fields. Our study demonstrates that shallow feeders in monogenetic fields can form geometrically complex networks, particularly those intruding poorly consolidated sedimentary rocks. We conclude that the Hopi Buttes eruptions were primarily fed by NW-SE-striking dikes. However, saucer-shaped sills also played an important role in modulating eruptions by transporting magma toward and away from eruptive conduits. Sill development could have been accompanied by surface uplifts on the order of decimeters. We infer that the characteristic feeder systems described here for the Hopi Buttes may underlie monogenetic fields elsewhere, particularly where magma intersects shallow, and often weak, sedimentary rocks. Results from this study support growing evidence of the important role of shallow sills in active monogenetic fields.

  11. Minimal contribution of cell-bound antibodies to the immunoscintigraphy of inflamed joints with 99mTc-anti-CD4 monoclonal antibodies

    International Nuclear Information System (INIS)

    Kinne, R.W.; Palombo-Kinne, E.; Wolski, A.; Wolf, F.; Emmrich, F.; Becker, W.

    2002-01-01

    Aim: The cellular joint infiltrate in rheumatoid arthritis patients is rich in CD4-positive T-helper lymphocytes and macrophages, rendering anti-CD4 monoclonal antibodies (mAbs) suitable for specific immunoscintigraphy of human/experimental arthritis. Following intravenous injection, however, mAbs are present both in the free form and bound to CD4-positive, circulating monocytes and T-cells. Thus, the present study aimed at analyzing the relative contribution of the free and the cell-bound component to the imaging of inflamed joints in experimental adjuvant arthritis (AA). Methods: AA rat pertioneal macrophages or lymph node T-cells were incubated in vitro with saturating amounts of 99mTc-anti-CD4 mAb (W3/25) and injected i.v. into rats with AA. Results: In vitro release of 99m Tc-anti-CD4 mAb from the cells was limited (on average 1.57%/h for macrophages and 0.84%/h for T-cells). Following i.v. injection, whole body/joints scans and tissue measurements showed only negligible accumulation of radioactivity in inflamed ankle joints (tissue: 0.22 and 0.34% of the injected activity, respectively), whereas the radioactivity was concentrated in liver (tissue: 79% and 71%, respectively), kidney, and urinary bladder. Unlike macrophages, however, anti-CD4 mAb-coated T-cells significantly accumulated in lymphoid organs, the inflamed synovial membrane of the ankle joints, as well as in elbow and knee joints. Conclusion: While the overall contribution of cell-bound mAbs to the imaging of arthritic joints with anti-CD4 mAbs is minimal, differential accumulation of macrophages and T-cells in lymphoid organs and the inflamed synovial membrane indicates preferential migration patterns of these 2 cell populations in arthritic rats. Although only validated for 99m Tc-anti-CD4 mAbs, extrapolation of the results to other anticellular mAbs with similar affinity for their antigen may be possible. (orig.) [de

  12. Obesity is a significant susceptibility factor for idiopathic AA amyloidosis.

    Science.gov (United States)

    Blank, Norbert; Hegenbart, Ute; Dietrich, Sascha; Brune, Maik; Beimler, Jörg; Röcken, Christoph; Müller-Tidow, Carsten; Lorenz, Hanns-Martin; Schönland, Stefan O

    2018-03-01

    To investigate obesity as susceptibility factor in patients with idiopathic AA amyloidosis. Clinical, biochemical and genetic data were obtained from 146 patients with AA amyloidosis. Control groups comprised 40 patients with long-standing inflammatory diseases without AA amyloidosis and 56 controls without any inflammatory disease. Patients with AA amyloidosis had either familial Mediterranean fever (FMF) or long-standing rheumatic diseases as underlying inflammatory disease (n = 111, median age 46 years). However, in a significant proportion of patients with AA amyloidosis no primary disease was identified (idiopathic AA; n = 37, median age 60 years). Patients with idiopathic AA amyloidosis were more obese and older than patients with AA amyloidosis secondary to FMF or rheumatic diseases. Serum leptin levels correlated with the body mass index (BMI) in all types of AA amyloidosis. Elevated leptin levels of more than 30 µg/l were detected in 18% of FMF/rheumatic + AA amyloidosis and in 40% of patients with idiopathic AA amyloidosis (p = .018). Finally, the SAA1 polymorphism was confirmed as a susceptibility factor for AA amyloidosis irrespective of the type of the disease. Obesity, age and the SAA1 polymorphism are susceptibility factors for idiopathic AA amyloidosis. Recent advances in treatment of FMF and rheumatic disorders will decrease the incidence of AA amyloidosis due to these diseases. Idiopathic AA, however, might be an emerging problem in the ageing and increasingly obese population.

  13. TIG-dressing of High Strength Steel Butt Welded Connections. Part 1 : Weld Toe Geometry and Local Hardness

    NARCIS (Netherlands)

    Van Es, S.H.J.; Kolstein, M.H.; Pijpers, R.J.M.; Bijlaard, F.S.K.

    2014-01-01

    This paper presents the results of extensive measurements on weld toe geometry of as-welded and TIG-dressed butt welded connections in high strength steels S460, S690 and very high strength steels S890 and S1100. Descriptions of the measurement techniques and data analysis are presented. Four weld

  14. TIG-dressing of high strength steel butt welded connections - Part 1: weld toe geometry and local hardness

    NARCIS (Netherlands)

    Es, S.H.J. van; Kolstein, M.H.; Pijpers, R.J.M.; Bijlaard, F.S.K.

    2013-01-01

    This paper presents the results of extensive measurements on weld toe geometry of as-welded and TIG-dressed butt welded connections in high strength steels S460, S690 and very high strength steels S890 and S1100. Descriptions of the measurement techniques and data analysis are presented. Four weld

  15. Microstructure and mechanical properties of China low activation martensitic steel joint by TIG multi-pass welding with a new filler wire

    Energy Technology Data Exchange (ETDEWEB)

    Huang, Bo [Key Laboratory of Neutronics and Radiation Safety, Institute of Nuclear Energy Safety Technology, Chinese Academy of Sciences, Hefei, Anhui, 230031 (China); Zhang, Junyu [Key Laboratory of Neutronics and Radiation Safety, Institute of Nuclear Energy Safety Technology, Chinese Academy of Sciences, Hefei, Anhui, 230031 (China); University of Science and Technology of China, Hefei, Anhui, 230027 (China); Wu, Qingsheng, E-mail: qingsheng.wu@fds.org.cn [Key Laboratory of Neutronics and Radiation Safety, Institute of Nuclear Energy Safety Technology, Chinese Academy of Sciences, Hefei, Anhui, 230031 (China)

    2017-07-15

    Tungsten Inner Gas (TIG) welding is employed for joining of China low activation martensitic (CLAM) steel. A new filler wire was proposed, and the investigation on welding with various heat input and welding passes were conducted to lower the tendency towards the residual of δ ferrite in the joint. With the optimized welding parameters, a butt joint by multi-pass welding with the new filler wire was prepared to investigate the microstructure and mechanical properties. The microstructure of the joint was observed by optical microscope (OM) and scanning electron microscope (SEM). The hardness, Charpy impact and tensile tests of the joint were implemented at room temperature (25 °C). The results revealed that almost full martensite free from ferrite in the joints were obtained by multipass welding with the heat input of 2.26 kJ/mm. A certain degree of softening occurred at the heat affected zone of the joint according to the results of tensile and hardness tests. The as welded joints showed brittle fracture in the impact tests. However, the joints showed toughness fracture after tempering and relatively better comprehensive performance were achieved when the joints were tempered at 740 °C for 2 h. - Highlights: •A new filler material was proposed to control ferrite content in CLAM weld metal. •Heat input affected ferrite content through influencing cooling rate during welding. •Multipass welding was a promising way to eliminate the ferrite in the weld.

  16. Dissimilar friction stir welding of 6061 Al to T2 pure Cu adopting tooth-shaped joint configuration: Microstructure and mechanical properties

    Energy Technology Data Exchange (ETDEWEB)

    Zhang, Wei; Shen, Yifu, E-mail: yfshen_nuaa@hotmail.com; Yan, Yinfei; Guo, Rui

    2017-04-06

    In this paper, dissimilar 6061aluminum alloy and commercial pure copper were friction stir butt welded adopting tooth-shaped joint configuration to investigate the influence of Al/Cu content in welding bead (WB) on the microstructure and mechanical properties of the joint. At preliminary tests, optimal welding parameters were determined to guarantee proper heat input. Welding experiments were performed with the dimensions of the tooth as variables, which is a special technique to tailor Al/Cu content in WB. Macro and microstructure of the cross section of the joints were characterized via optical microscopy (OM) and Scanning Electron Microscopy (SEM) equipped with energy dispersive spectroscopy (EDS). Special band structure(BS) showing lamellar-like flow characteristic is worthy of noticing. Additionally, dispersive Cu particles (DP), forming composite-like structure, were captured. High Cu concentration, however, yielded a harsh material flow due to its high plasticized temperature and poor flowability and can not produce reliable metallurgical bonding. Microhardness of the joint was investigated and the high hardness was caused mainly by the hard intermetallic compounds (IMCs). Besides, tensile tests were conducted to evaluate the joint performance. Based on the result analysis, this joint form has special advantage in tailoring Al/Cu content in WB and controlling the microstructure that imposes significant influence on mechanical properties of the joints.

  17. Dissimilar friction stir welding of 6061 Al to T2 pure Cu adopting tooth-shaped joint configuration: Microstructure and mechanical properties

    International Nuclear Information System (INIS)

    Zhang, Wei; Shen, Yifu; Yan, Yinfei; Guo, Rui

    2017-01-01

    In this paper, dissimilar 6061aluminum alloy and commercial pure copper were friction stir butt welded adopting tooth-shaped joint configuration to investigate the influence of Al/Cu content in welding bead (WB) on the microstructure and mechanical properties of the joint. At preliminary tests, optimal welding parameters were determined to guarantee proper heat input. Welding experiments were performed with the dimensions of the tooth as variables, which is a special technique to tailor Al/Cu content in WB. Macro and microstructure of the cross section of the joints were characterized via optical microscopy (OM) and Scanning Electron Microscopy (SEM) equipped with energy dispersive spectroscopy (EDS). Special band structure(BS) showing lamellar-like flow characteristic is worthy of noticing. Additionally, dispersive Cu particles (DP), forming composite-like structure, were captured. High Cu concentration, however, yielded a harsh material flow due to its high plasticized temperature and poor flowability and can not produce reliable metallurgical bonding. Microhardness of the joint was investigated and the high hardness was caused mainly by the hard intermetallic compounds (IMCs). Besides, tensile tests were conducted to evaluate the joint performance. Based on the result analysis, this joint form has special advantage in tailoring Al/Cu content in WB and controlling the microstructure that imposes significant influence on mechanical properties of the joints.

  18. Experimental immunologically mediated aplastic anemia (AA) in mice: cyclosporin A fails to protect against AA

    International Nuclear Information System (INIS)

    Knospe, W.H.; Steinberg, D.; Gratwohl, A.; Speck, B.

    1984-01-01

    Immunologically mediated aplastic anemia (AA) in mice was induced by the i.v. injection of 10(7) lymph node cells (LNC) from H-2k identical but Mls mismatched CBA/J donor mice into previously irradiated (600 rad total body gamma) C3H/HeJ mice. Cyclosporin A (CsA), 25 mg/kg, was administered subcutaneously from day -1 to day 30. Control mice included C3H/HeJ mice which received 600 rad alone, C3H/HeJ mice which received 600 rad plus CsA as above, and C3H/HeJ mice which received 600 rad total body irradiation followed by 10(7) LNC from CBA/J donors. CsA failed to prevent lethal AA. These results suggest that the pathogenetic mechanisms operating in immunologically mediated AA differ from the mechanisms operating in rodents transplanted with allogeneically mismatched marrow or spleen cells which develop graft-versus-host disease. The results are consistent with a non-T cell-dependent mechanism causing the AA

  19. The Antiproton Accumulator (AA)

    CERN Multimedia

    1980-01-01

    A section of the AA where the dispersion (and hence the horizontal beam size) is large. One can distinguish (left to right): A large vacuum-tank, a quadrupole (QDN09*), a bending magnet (BST08), another vacuum-tank, a wide quadrupole (QFW08) and (in the background) a further bending magnet (BST08). The tanks are covered with heating tape for bake-out. The tank left of QDN09 contained the kickers for stochastic pre-cooling (see 790621, 8002234, 8002637X), the other one served mainly as vacuum chamber in the region where the beam was large. Peter Zettwoch works on QFW08. * see: H. Koziol, Antiproton Accumulator Parameter List, PS/AA/Note 84-2 (1984) See under 7911303, 7911597X, 8004261 and 8202324. For photos of the AA in different phases of completion (between 1979 and 1982) see: 7911303, 7911597X, 8004261, 8004608X, 8005563X, 8005565X, 8006716X, 8006722X, 8010939X, 8010941X, 8202324, 8202658X, 8203628X .

  20. Effects of Heat Input on the Mechanical and Metallurgical Characteristics of Tig Welded Incoloy 800Ht Joints

    Directory of Open Access Journals (Sweden)

    Kumar S. Arun

    2017-09-01

    Full Text Available This study focuses on the effect of heat input on the quality characteristics of tungsten inert arc gas welded incoloy 800HT joints using inconel-82 filler wire. Butt welding was done on specimens with four different heat inputs by varying the process parameters like welding current and speed. The result indicated that higher heat input levels has led to the formation of coarser grain structure, reduced mechanical properties and sensitization issues on the weldments. The formation of titanium nitrides provided resistance to fracture and increased the tensile strength of the joints at high temperatures. Further aging was done on the welded sample at a temperature of 750°C for 500 hours and the metallographic result showed formation of carbides along the grain boundaries in a chain of discrete and globular form which increased the hardness of the material. The formation of spinel NiCr2O4 provided oxidation resistance to the material during elevated temperature service.

  1. Ascorbic acid (AA) metabolism in protection against radiation damage

    International Nuclear Information System (INIS)

    Rose, R.C.; Koch, M.J.

    1986-01-01

    The possibility is considered that AA protects tissues against radiation damage by scavenging free radicals that result from radiolysis of water. A physiologic buffer (pH 6.7) was incubated with 14 C-AA and 1 mM thiourea (to slow spontaneous oxidation of AA). Aliquots were assayed by HPLC and scintillation spectrometry to identify the 14 C-label. Samples exposed to Cobalt-60 radiation had a half time of AA decay of 30 minutes) indicating that AA scavenges radiation-induced free radicals and forms the ascorbate free radical (AFR). Pairs of 14 C-AFR disproportionate, with the net effect of 14 C-dehydroascorbic acid formation from 14 C-AA. Having established that AFR result from ionizing radiation in an aqueous solution, the possibility was evaluated that a tissue factor reduces AFR. Cortical tissue from the kidneys of male rats was minced, homogenized in buffer and centrifuged at 8000 xg. The supernatant was found to slow the rate of radiation-induced AA degradation by > 90% when incubated at 23 0 C in the presence of 15 μM 14 C-AA. Samples of supernatant maintained at 100 0 C for 10 minutes or precipitated with 5% PCA did not prevent radiation-induced AA degradation. AA may have a specific role in scavenging free radicals generated by ionizing radiation and thereby protect body tissues

  2. Influencia de los parámetros de la soldadura metálica fría en las aleaciones AA5083 y AA6061//Influence of the colt metal welding parameters on the AA5083 and AA6061 aluminum

    Directory of Open Access Journals (Sweden)

    René Eduardo de‐Luna‐Alanís

    2015-01-01

    Full Text Available El trabajo tuvo como objetivo evaluar la influencia de la velocidad de la soldadura y de las correcciones del arco y pulso en el proceso de Transferencia Metálica Fría sobre las propiedades mecánicas de las aleaciones AA5083 y AA6061. Se desarrolló un diseño experimental de tipo factorial multinivel, con 4 factores independientes (Corrección de Arco, Pulso, Velocidad de Soldadura y Aleación. Los parámetros fundamentales fueron: Corriente de base 250 A; Voltaje de arco 21 V y Polaridad (Direct current electrode positive, DCEP. La evaluación se realizó a través de un ensayo de tracción transversal sobre probetas planas obtenidas de los cupones soldados. Se demuestra que el modelo aplicado es adecuado, revelándose en los experimentos diferencias sustanciales en las propiedades Tensión de fluencia 29,56 %, Módulo de elasticidad 51,16 % y Trabajo específico de deformación elástica 42,30 %, el cual no posee una dependencia lineal con elresto de las propiedades anteriores.Palabras claves: transferencia metálica fría, aleación AA5083, aleación AA6061, propiedades mecánicas._______________________________________________________________________________AbstractThe work objective was to evaluatethe influence of Cold Metal Transfer process arc and pulse corrections and welding speed on the mechanical properties of AA5083 and AA6061 aluminum alloys. For it, a Factorial Multilevel experimental design whit 4 independent factor (arc correction, pulse correction, welding speed and alloy was developed. The essential welding parameters employed were: base current 250 A; arc voltage 21 V and polarity (DCEP. The evaluation was made whit a transverse traction test of plate welded coupons. The experimental model applied wasadequate and substantial differences was showed between yield tensile strength 29,56 %, elasticity module (51,16 % and specific work of elastic deformation 42,30 %, which it does not possess a lineal dependence whit the rest

  3. Geology of the Pumpkin Buttes Area of the Powder River Basin, Campbell and Johnson Counties, Wyoming

    Science.gov (United States)

    Sharp, William Neil; White, Amos McNairy

    1956-01-01

    About 200 uranium occurrences have been examined in the Pumpkin Buttes area, Wyoming. Uranium minerals are visible at most of these places and occur in red and buff sandstone lenses in the Wasatch formation of Eocene age. The uranium minerals are disseminated in buff sandstone near red sandstone, and also occur in red sandstone in manganese oxide concretions and uraninite concretions.

  4. Finite element modelling and updating of friction stir welding (FSW joint for vibration analysis

    Directory of Open Access Journals (Sweden)

    Zahari Siti Norazila

    2017-01-01

    Full Text Available Friction stir welding of aluminium alloys widely used in automotive and aerospace application due to its advanced and lightweight properties. The behaviour of FSW joints plays a significant role in the dynamic characteristic of the structure due to its complexities and uncertainties therefore the representation of an accurate finite element model of these joints become a research issue. In this paper, various finite elements (FE modelling technique for prediction of dynamic properties of sheet metal jointed by friction stir welding will be presented. Firstly, nine set of flat plate with different series of aluminium alloy; AA7075 and AA6061 joined by FSW are used. Nine set of specimen was fabricated using various types of welding parameters. In order to find the most optimum set of FSW plate, the finite element model using equivalence technique was developed and the model validated using experimental modal analysis (EMA on nine set of specimen and finite element analysis (FEA. Three types of modelling were engaged in this study; rigid body element Type 2 (RBE2, bar element (CBAR and spot weld element connector (CWELD. CBAR element was chosen to represent weld model for FSW joints due to its accurate prediction of mode shapes and contains an updating parameter for weld modelling compare to other weld modelling. Model updating was performed to improve correlation between EMA and FEA and before proceeds to updating, sensitivity analysis was done to select the most sensitive updating parameter. After perform model updating, total error of the natural frequencies for CBAR model is improved significantly. Therefore, CBAR element was selected as the most reliable element in FE to represent FSW weld joint.

  5. Strength of vacuum brazed joints for repair; Haallfasthet hos reparationer utfoerda med vakuumloedning

    Energy Technology Data Exchange (ETDEWEB)

    Berglin, Leif [Siemens Industrial Turbomachinery AB, Finspaang (Sweden)

    2005-04-01

    Strength data are missing for braze joints. Repaired components cannot fully make use of the strength of the braze, and lifetime will be underestimated. The goal of the project was to generate material data to be able to prolong the lifetime of the components. Two different material combinations were tested, 12% Chromium steel brazed with BNi-2, and a nickel base alloy, IN792 brazed with BNi-5. Tensile testing at room temperature and elevated temperature was performed in the project. Target group is purchasers and suppliers of repaired components. A tensile test specimen with butt joint was developed in the project. The used test specimen worked well for the 12% Chromium steel. The results from testing show that proof stress and tensile strength are strongly depending on the joint gap, particularly at room temperature. High strength, close to base material strength, was achieved with joint gaps smaller than 50{mu}m. For wider joint gaps, strength was lower. Strength was approximately 25% of base material strength for joint gaps over 100{mu}m. The results can be explained by changes in microstructure. Joint gaps wider than 50{mu}m showed evidence of two-phase structure. At 500 deg C, the results also showed a connection between joint gap, microstructure and strength. The generated strength data can be used for calculations of lifetime for repaired components. Two different process errors were discovered in the manufacturing process of the brazed IN792 test specimens. The generated material data are therefor erroneous. The reason for this was two manufacturing errors. The tack welding was done with too high heat input. The surfaces of the joint gap became oxidised and the oxide hindered wetting of the braze. The second reason was that the brazing was done without the prescribed hold time at maximum temperature. The melting of the braze was therefor not completed when cooling started. As a result, the strength of the IN792 specimens was low at both temperatures.

  6. Microstructures and mechanical properties of magnesium alloy and stainless steel weld-joint made by friction stir lap welding

    International Nuclear Information System (INIS)

    Wei, Yanni; Li, Jinglong; Xiong, Jiangtao; Huang, Fu; Zhang, Fusheng

    2012-01-01

    Highlights: → Friction stir lap welding technology with cutting pin was successfully employed to form lap joint of magnesium and steel. → The cutting pin made the lower steel participate in deformation and the interface was no longer flat. → A saw-toothed structure formed due to a mechanical mixing of the magnesium and steel was found at the interface. → A high-strength joint was produced which fractured in the magnesium side. -- Abstract: Friction stir lap welding was conducted on soft/hard metals. A welding tool was designed with a cutting pin of rotary burr made of tungsten carbide, which makes the stirring pin possible to penetrate and cut the surface layer of the hard metal. Magnesium alloy AZ31 and stainless steel SUS302 were chosen as soft/hard base metals. The structures of the joining interface were analyzed by scanning electron microscopy (SEM). The joining strength was evaluated by tensile shear test. The results showed that flower-like interfacial morphologies were presented with steel flashes and scraps, which formed bonding mechanisms of nail effect by long steel flashes, zipper effect by saw-tooth structure and metallurgical bonding. The shear strength of the lap joint falls around the shear strength of butt joint of friction stir welded magnesium alloy.

  7. 76 FR 21331 - Certain Carbon Steel Butt-Weld Pipe Fittings From Brazil, Japan, Taiwan, Thailand, and the People...

    Science.gov (United States)

    2011-04-15

    ... the People's Republic of China: Continuation of Antidumping Duty Orders AGENCY: Import Administration... butt-weld pipe fittings from Brazil, Japan, Taiwan, Thailand, and the People's Republic of China (PRC), pursuant to section 751(c) of the Tariff Act of 1930, as amended (the Act). See Initiation of Five-Year...

  8. Structural Phase Evolution in Ultrasonic-Assisted Friction Stir Welded 2195 Aluminum Alloy Joints

    Science.gov (United States)

    Eliseev, A. A.; Fortuna, S. V.; Kalashnikova, T. A.; Chumaevskii, A. V.; Kolubaev, E. A.

    2017-10-01

    The authors examined the structural and phase state of fixed joints produced by method of friction stir welding (FSW) and ultrasonic-assisted friction stir welding (UAFSW) from extruded profile of aluminum alloy AA2195. In order to identify the role of ultrasonic application in the course of welding, such characteristics, as volume fraction and average size of secondary particles are compared in the base material and stir zones of FSW and UAFSW joints. By applying the methods of SEM and TEM analysis, researchers established the complex character of phase transitions as a result of ultrasonic application.

  9. Individual optimization of InAlGaAsP-InP sections for 1.55-μm passively mode-locked lasers

    DEFF Research Database (Denmark)

    Kulkova, Irina; Larsson, David; Semenova, Elizaveta

    2012-01-01

    We present integrated single QW semiconductor optical amplifier and MQW electroabsorber modulator based on InAlGaAsP-InP materials for application in a monolithic mode-locked laser. Optimized structures with high-quality butt-joint interfaces are demonstrated.......We present integrated single QW semiconductor optical amplifier and MQW electroabsorber modulator based on InAlGaAsP-InP materials for application in a monolithic mode-locked laser. Optimized structures with high-quality butt-joint interfaces are demonstrated....

  10. Microstructural and mechanical behaviors of nano-SiC-reinforced AA7075-O FSW joints prepared through two passes

    Energy Technology Data Exchange (ETDEWEB)

    Bahrami, Mohsen, E-mail: Mohsen.bahrami@aut.ac.ir [Faculty of Mining and Materials Engineering, Amirkabir University of Technology (AUT), Hafez Aveenue, Tehran (Iran, Islamic Republic of); Farahmand Nikoo, Mohsen [Faculty of Mining and Materials Engineering, Amirkabir University of Technology (AUT), Hafez Aveenue, Tehran (Iran, Islamic Republic of); Besharati Givi, Mohammad Kazem [Department of Mechanical Engineering, University of Tehran, Tehran (Iran, Islamic Republic of)

    2015-02-25

    In this paper, a threaded tapered pin tool was employed to fabricate a 2-pass friction stir welded (FSWed) joint. To investigate the benefits of nano-sized SiC particles on microstructural and mechanical properties of the joint, the experiment was repeated while SiC particles had been inserted along the joint line. In another joint, a square pin tool was applied in the second pass to evaluate the effectiveness of switching pin geometry between passes on the aforementioned properties. Microstructural features including grain size, second phase particles and reinforcement distribution were examined via optical and scanning electron microscopy (SEM) techniques. In addition to satisfactory connections between SiC particles and the matrix, the most homogenous particles distribution was observed in the specimen FSWed with both pin tools. This observation was further supported by atomic force microscopy (AFM) examination. Additionally, the foregoing joint demonstrated the maximum tensile strength which was synonymous with its smallest grain size. During tensile testing, SiC-free joint and SiC-reinforced ones fractured from stir zone (SZ) and base metal, respectively. Moreover, SiC-free joint showed necking phenomenon. SEM results showed that the SiC-reinforced specimens possessed ductile fracture morphologies. On the other hand, SiC-free specimen showed a quasi-cleavage fracture mode confirming its moderate percent elongation. In the meantime, SiC-reinforced specimens exhibited superior hardness level to SiC-free specimen.

  11. Side effects of AAS abuse: an overview.

    Science.gov (United States)

    Turillazzi, E; Perilli, G; Di Paolo, M; Neri, M; Riezzo, I; Fineschi, V

    2011-05-01

    Anabolic - androgenic steroids (AAS) were originally developed to promote growth of skeletal muscle. AAS abuse is commonly associated with bodybuilders, weightlifters, and other athletes. The issue of AAS toxicity is not yet completely understood since the adverse effects outline a varied scenario with side effects reported affecting many organs and systems in humans. The true incidence of AAS related medical problems is not known, due to several drawbacks in human studies. The entity of side effects depends on the sex, the dose, the duration of treatment, whether they are taken during exercise training or under sedentary conditions, and the susceptibility of the individuals themselves to androgen exposure partly depending on genetic factors. Both the acute and the chronic effects can lead to toxicity, but generally the serious and even fatal effects depend on the time and the duration of AAS administration. A limitation of human studies is represented by the fact that information about the intake of steroids are, generally, self reported and it is hardly possible to assess the exact dosage. AAS are often used in combination with other dugs or substances, so it is difficult to separate their toxic effects from those caused by the other drugs abused. Hence experimental studies conducted on animal models are mandatory to investigate the mechanisms underlying to AAS toxicity and the organ alterations due to these substances. Finally, clinicians should be aware of the complex and varied pattern of toxicity so as to be able to perform correct diagnoses and treatments.

  12. Creep failure analysis of butt welded tubes

    International Nuclear Information System (INIS)

    Browne, R.J.; Parker, J.D.; Walters, D.J.

    1981-01-01

    As part of a major research programme to investigate the influence of butt welds on the life expectancy of tubular components, a series of internal-pressure, stress-rupture tests have been carried out. Thick walled 1/2Cr 1/2Mo 1/4V tube specimens were welded with mild steel, 1Cr 1/2Mo steel, 2 1/4Cr 1Mo steel or nominally matching 1/2Cr 1/2Mo 1/4V steel to give a wide range of weld metal creep strengths relative to the parent tube. The weldments were tested at 565 0 C at two values of internal pressure, and gave failure lives of up to 44,000 hrs. Finite element techniques have been used to determine the stationary state stress distribution in the weldment which was represented by a three material model. Significant stress redistribution was indicated and these results enabled the position and orientation of cracking and the rupture life to be predicted. The theoretical and experimental results have been used to highlight the limitations of current design methods which are based on the application of the mean diameter hoop stress to the parent material stress rupture data. (author)

  13. Experimental and numerical investigation on under-water friction stir welding of armour grade AA2519-T87 aluminium alloy

    Directory of Open Access Journals (Sweden)

    S. Sree Sabari

    2016-08-01

    Full Text Available Friction stir welding (FSW is a promising welding process that can join age hardenable aluminium alloys with high joint efficiency. However, the thermal cycles experienced by the material to be joined during FSW resulted in the deterioration of mechanical properties due to the coarsening and dissolution of strengthening precipitates in the thermo-mechanical affected zone (TMAZ and heat affected zone (HAZ. Under water friction stir welding (UWFSW is a variant of FSW process which can maintain low heat input as well as constant heat input along the weld line. The heat conduction and dissipation during UWFSW controls the width of TMAZ and HAZ and also improves the joint properties. In this investigation, an attempt has been made to evaluate the mechanical properties and microstructural characteristics of AA2519-T87 aluminium alloy joints made by FSW and UWFSW processes. Finite element analysis has been used to estimate the temperature distribution and width of TMAZ region in both the joints and the results have been compared with experimental results and subsequently correlated with mechanical properties.

  14. Simulation Study on Multipassed Welding Distortion of Combined Joint Types using Thermo-Elastic-Plastic FEM

    Directory of Open Access Journals (Sweden)

    RN Lidam

    2012-12-01

    Full Text Available This paper investigates the angular distortion induced by the gas metal arc welding (GMAW process on the combined butt and T-joint with a thickness of 9 mm. The material used in this study was low manganese carbon steel S355J2G3. A 2-D and 3-D thermo-elastic-plastic finite element (FE analysis has been developed to simulate the induced distortion of multipassed welding. In this research, SYSWELD 2010 with its computation management tool, known as multipassed welding advisor (MPA, was applied to analyze the distortion behavior of combined joint types. To model the heat source of GMAW, Goldak's double ellipsoid representation, which is available within this finite element analysis (FEA code was selected. Prior to the results discussion, this paper also shows the step-bystep procedures to simulate combined jointing which begins with metallurgical and customized heat source modeling, and is followed by creating geometrical mesh using Visual-Mesh 6.5 for analyzing and processing the results. Apart from 2-D and 3-D comparison analysis, the final objective of this research is also aimed to be a baseline study to provide preliminary information in preparing the tools and equipment for experimental investigation.

  15. Multi-Scale Computational Modeling of Ni-Base Superalloy Brazed Joints for Gas Turbine Applications

    Science.gov (United States)

    Riggs, Bryan

    , ductile a-Ni phase that formed at the joint interface and a hard, brittle multi-phase centerline eutectic. CrB and Ni3B type borides were identified in the eutectic region via electron probe micro-analysis, and a boron diffusion gradient was observed in the BM adjacent to the joint. The volume fraction of centerline eutectic was found to be highly dependent on the extent of the boron diffusion that occurred during brazing and therefore a function of the primary process parameters; hold time, temperature, FM/BM composition, and joint gap. Thermo-Calc(TM) and DICTRA(TM) simulations were used to model the BM dissolution, isothermal solidification and phase transformations that occurred during brazing to predict the final joint microstructure based on these process parameters. Good agreement was found between experimental and simulated joint microstructures at various joint gaps demonstrating the application of these simulations for brazed joints. However, thermodynamic/kinetic databases available for brazing FMs were limited. A variety of mechanical testing was performed to determine the mechanical properties of CMSX-4/BNi-2 and IN718/BNi-2 brazed joints including small-scale tensile tests, standard-size butt joints and lap shear tests. Small-scale tensile testing provided a novel method for studying microstructure-property relationships in brazed joints and indicated that both joint strength and ductility decrease significantly with an increase in the volume fraction of centerline eutectic. In-situ observations during small-scale testing also showed strain localization and crack initiation occurs around the hard, eutectic phases in the joint microstructure during loading. The average tensile strength for standard-size IN718/BNi-2 butt joints containing a low volume fraction of centerline eutectic was found to be 152.8 ksi approximately 90% of the BM yield strength (˜170 ksi). The average lap shear FM stress was found to decrease from 70 to 20 ksi for IN718/BNi-2 joints and

  16. Microstructure and Fatigue Properties of Laser Welded DP590 Dual-Phase Steel Joints

    Science.gov (United States)

    Xie, Chaojie; Yang, Shanglei; Liu, Haobo; Zhang, Qi; Cao, Yaming; Wang, Yuan

    2017-08-01

    In this paper, cold-rolled DP590 dual-phase steel sheets with 1.5 mm thickness were butt-welded by a fiber laser, and the evolution and effect on microhardness, tensile property and fatigue property of the welded joint microstructure were studied. The results showed that the base metal is composed of ferrite and martensite, with the martensite dispersed in the ferrite matrix in an island manner. The microstructure of the weld zone was lath-shaped martensite that can be refined further by increasing the welding speed, while the heat-affected zone was composed of ferrite and tempered martensite. The microhardness increased with increasing welding speed, and the hardness reached its highest value—393.8 HV—when the welding speed was 5 m/min. Static tensile fracture of the welded joints always occurred in the base metal, and the elongation at break was more than 16%. The conditional fatigue limits of the base metal and the weld joints were 354.2 and 233.6 MPa, respectively, under tension-tension fatigue tests with a stress rate of 0.1. After observation of the fatigue fracture morphology, it was evident that the fatigue crack of the base metal had sprouted into the surface pits and that its expansion would be accelerated under the action of a secondary crack. The fatigue source of the welded joint was generated in the weld zone and expanded along the martensite, forming a large number of fatigue striations. Transient breaking, which occurred in the heat-affected zone of the joint as a result of the formation of a large number of dimples, reflected the obvious characteristics of ductile fracture.

  17. Effect of post weld heat treatment on tensile properties and microstructure characteristics of friction stir welded armour grade AA7075-T651 aluminium alloy

    Directory of Open Access Journals (Sweden)

    P. Sivaraj

    2014-03-01

    Full Text Available This paper reports the effects of post weld heat treatments, namely artificial ageing and solution treatment followed by artificial ageing, on microstructure and mechanical properties of 12 mm thick friction stir welded joints of precipitation hardenable high strength armour grade AA7075-T651 aluminium alloy. The tensile properties, such as yield strength, tensile strength, elongation and notch tensile strength, are evaluated and correlated with the microhardness and microstructural features. The scanning electron microscope is used to characterie the fracture surfaces. The solution treatment followed by ageing heat treatment cycle is found to be marginally beneficial in improving the tensile properties of friction stir welds of AA7075-T651 aluminium alloy.

  18. Joint properties of dissimilar Al6061-T6 aluminum alloy/Ti–6%Al–4%V titanium alloy by gas tungsten arc welding assisted hybrid friction stir welding

    International Nuclear Information System (INIS)

    Bang, HanSur; Bang, HeeSeon; Song, HyunJong; Joo, SungMin

    2013-01-01

    Highlights: • Hybrid friction stir welding for Al alloy and Ti alloy joint has been carried out. • Mechanical strength of dissimilar joint by HFSW and FSW has been compared. • Microstructure of dissimilar joint by HFSW and FSW has been compared. - Abstract: Hybrid friction stir butt welding of Al6061-T6 aluminum alloy plate to Ti–6%Al–4%V titanium alloy plate with satisfactory acceptable joint strength was successfully achieved using preceding gas tungsten arc welding (GTAW) preheating heat source of the Ti alloy plate surface. Hybrid friction stir welding (HFSW) joints were welded completely without any unwelded zone resulting from smooth material flow by equally distributed temperature both in Al alloy side and Ti alloy side using GTAW assistance for preheating the Ti alloy plate unlike friction stir welding (FSW) joints. The ultimate tensile strength was approximately 91% in HFSW welds by that of the Al alloy base metal, which was 24% higher than that of FSW welds without GTAW under same welding condition. Notably, it was found that elongation in HFSW welds increased significantly compared with that of FSW welds, which resulted in improved joint strength. The ductile fracture was the main fracture mode in tensile test of HFSW welds

  19. Merging high resolution geophysical and geochemical surveys to reduce exploration risk at glass buttes, Oregon

    Energy Technology Data Exchange (ETDEWEB)

    Walsh, Patrick [Ormat Nevada, Inc., Reno, NV (United States); Fercho, Steven [Ormat Nevada, Inc., Reno, NV (United States); Perkin, Doug [Ormat Nevada, Inc., Reno, NV (United States); Martini, Brigette [Corescan Inc., Ascot (Australia); Boshmann, Darrick [Oregon State Univ., Corvallis, OR (United States)

    2015-06-01

    The engineering and studies phase of the Glass Buttes project was aimed at reducing risk during the early stages of geothermal project development. The project’s inclusion of high resolution geophysical and geochemical surveys allowed Ormat to evaluate the value of these surveys both independently and in combination to quantify the most valuable course of action for exploration in an area where structure, permeability, and temperature are the most pressing questions. The sizes of the thermal anomalies at Glass Buttes are unusually large. Over the course of Phase I Ormat acquired high resolution LIDAR data to accurately map fault manifestations at the surface and collected detailed gravity and aeromagnetic surveys to map subsurface structural features. In addition, Ormat collected airborne hyperspectral data to assist with mapping the rock petrology and mineral alteration assemblages along Glass Buttes faults and magnetotelluric (MT) survey to try to better constrain the structures at depth. Direct and indirect identification of alteration assemblages reveal not only the geochemical character and temperature of the causative hydrothermal fluids but can also constrain areas of upflow along specific fault segments. All five datasets were merged along with subsurface lithologies and temperatures to predict the most likely locations for high permeability and hot fluids. The Glass Buttes temperature anomalies include 2 areas, totaling 60 km2 (23 mi2) of measured temperature gradients over 165° C/km (10° F/100ft). The Midnight Point temperature anomaly includes the Strat-1 well with 90°C (194 °F) at 603 m (1981 ft) with a 164 °C/km (10°F/100ft) temperature gradient at bottom hole and the GB-18 well with 71°C (160 °F) at 396 m (1300 ft) with a 182°C/km (11°F/100ft) gradient. The primary area of alteration and elevated temperature occurs near major fault intersections associated with Brothers Fault Zone and Basin and Range systems. Evidence for faulting is

  20. Analysis of cooling media effects on microstructure and mechanical properties during FSW/UFSW of AA 6082-T6

    Science.gov (United States)

    Atif Wahid, Mohd; Siddiquee, Arshad Noor; Khan, Zahid A.; Sharma, Nidhi

    2018-04-01

    The aim of the present study is to investigate the effect of cooling media on the temperature distribution, microstructure and mechanical properties of the joint produced during Underwater Friction Stir Welding (UFSW) in normal water, cold water (water with crushed ice (CFSW)) and air (FSW), for aluminum alloy (AA) 6082-T6. The results showed that peak temperature during UFSW and CFSW were significantly lower than the FSW. The temperature at the advancing side (AS) of the joint was higher than the retreating side (RS). Substantial reduction in TMAZ/HAZ width was observed during UFSW and CFSW as compared to FSW. Al-Mn-Fe-Si intermetallic phases were seen in all the joints along with the BM. The main strengthening precipitates found in UFSW and CFSW was β″ (Mg5Si6) which changed to β (Mg2Si) precipitates during FSW due to increased temperature. The tensile strength of the joints was best during UFSW followed by FSW and CFSW. The controlled temperature distribution resulted in improved tensile strength whereas both undercooling and overcooling resulted in decreased tensile strength, however, increased cooling rate does not improve the elongation. A typical ‘W’ shape hardness profile was observed in all the joints irrespective of the cooling media used. Maximum hardness was obtained in the UFSW joint due to refined grain structure, high-density dislocations and presence of β″ phases.

  1. (PCL/AA) hydrogel for controlled drug delivery

    Indian Academy of Sciences (India)

    Administrator

    applications, (iii) dental applications, (iv) injectable polymers, (v) ... PCL with AA grafted PCL(PCL-g-AA) on the structure ... porosity. Structure, morphology and crystallinity of PCL/ .... X-ray diffraction patterns were recorded, in reflection,.

  2. Comparison of calculated and experimentally determined SID of CP and AA in complex diets differing in AA contents for grower finisher pigs.

    Science.gov (United States)

    Büsing, K; Berk, A; Müller, S; Kieckhäven, S; Krüger, K; Zeyner, A

    2017-10-01

    In practice, the content of standardized ileal digestible AA in complex feeds for pigs is calculated on the basis of tabulated values for individual feedstuffs. It comes into question, however, whether this truly reflects an accurate content based upon the estimate made for the individual feedstuffs. The objective of this study was to compare standardized ileal digestibility (SID) of crude protein (CP) and selected AA in complex feeds for grower and finisher pigs either calculated or experimentally determined. Six diets with increasing AA levels were prepared for grower (BW from 30 to 70 kg) and finisher (BW from 70 to 120 kg) feed. Crystalline L-lys, DL-met and L-thr were added to both diets, L-trp and L-val only to the grower feed. SID of both CP and AA was calculated from feed tables and experimentally determined in six adult minipigs (MINILEWE) with ileorectal anastomosis. With increasing AA levels, experimentally determined SID of supplemented AA increased (p AA via tabulated values for individual feedstuffs, however, seems to be acceptable for practical use. Journal of Animal Physiology and Animal Nutrition © 2017 Blackwell Verlag GmbH.

  3. Caracterização microestrutural e comportamento mecânico das ligas de alumínio AA2139 T3 e T8 soldadas por fricção rotativa com mistura Microstructural characterization and mechanical behavior of an AA2139 T3 and T8 aluminum alloy joined by friction stir welding (FSW

    Directory of Open Access Journals (Sweden)

    Vinícius Toledo Saccon

    2010-12-01

    Full Text Available Este trabalho visou analisar a caracterização microestrutural e o comportamento mecânico das ligas de alumínio AA2139 T3 e T8 quando são soldadas pelo processo Soldagem por Fricção Rotativa com Mistura, o qual é realizado na fase sólida. A análise microestrutural foi realizada utilizando microscopia óptica e eletrônica de varredura, e o comportamento mecânico foi avaliado através de medidas de microdureza e ensaio de tração convencional complementado pelo sistema ARAMIS. As ligas foram soldadas nos mesmos parâmetros de soldagem e com a mesma ferramenta, a fim de avaliar a qualidade da junta soldada para as duas condições de tratamento térmico, T3 e T8. Os resultados obtidos mostraram soldas resistentes para ambos os tratamentos térmicos, porém com melhores propriedades mecânicas para a liga AA2139 T3.This work aimed to study the microstructural characterization and mechanical behavior of AA2139 T3 and T8 aluminum alloys joined by FSW - Friction Stir Welding. The microstructural analysis has been done using optical microscope and scanning electron microscopy, and the mechanical analysis were evaluate through microhardness testing and conventional tensile test using the ARAMIS system . Each alloy were welded using the same welding parameters and the same tool in order to evaluate the joint quality for both heat treatment used for this work, T3 and T8. The result showed sounds joints for both heat treatments, although with better mechanical properties for the alloy AA2139 T3.

  4. A Methodology for the Assessment of Unconventional (Continuous) Resources with an Application to the Greater Natural Buttes Gas Field, Utah

    International Nuclear Information System (INIS)

    Olea, Ricardo A.; Cook, Troy A.; Coleman, James L.

    2010-01-01

    The Greater Natural Buttes tight natural gas field is an unconventional (continuous) accumulation in the Uinta Basin, Utah, that began production in the early 1950s from the Upper Cretaceous Mesaverde Group. Three years later, production was extended to the Eocene Wasatch Formation. With the exclusion of 1100 non-productive ('dry') wells, we estimate that the final recovery from the 2500 producing wells existing in 2007 will be about 1.7 trillion standard cubic feet (TSCF) (48.2 billion cubic meters (BCM)). The use of estimated ultimate recovery (EUR) per well is common in assessments of unconventional resources, and it is one of the main sources of information to forecast undiscovered resources. Each calculated recovery value has an associated drainage area that generally varies from well to well and that can be mathematically subdivided into elemental subareas of constant size and shape called cells. Recovery per 5-acre cells at Greater Natural Buttes shows spatial correlation; hence, statistical approaches that ignore this correlation when inferring EUR values for untested cells do not take full advantage of all the information contained in the data. More critically, resulting models do not match the style of spatial EUR fluctuations observed in nature. This study takes a new approach by applying spatial statistics to model geographical variation of cell EUR taking into account spatial correlation and the influence of fractures. We applied sequential indicator simulation to model non-productive cells, while spatial mapping of cell EUR was obtained by applying sequential Gaussian simulation to provide multiple versions of reality (realizations) having equal chances of being the correct model. For each realization, summation of EUR in cells not drained by the existing wells allowed preparation of a stochastic prediction of undiscovered resources, which range between 2.6 and 3.4 TSCF (73.6 and 96.3 BCM) with a mean of 2.9 TSCF (82.1 BCM) for Greater Natural Buttes

  5. Dicty_cDB: FC-AA02 [Dicty_cDB

    Lifescience Database Archive (English)

    Full Text Available FC (Link to library) FC-AA02 (Link to dictyBase) - - - Contig-U16527-1 FC-AA02Z (Li...nk to Original site) - - FC-AA02Z 458 - - - - Show FC-AA02 Library FC (Link to library) Clone ID FC-AA02 (Link to dic...linum small subunit ribosomal RNA gene, partial sequence. 149 2e-47 2 AY179984 |AY179984.1 Uncultured alveo... CP000930_2283( CP000930 |pid:none) Heliobacterium modesticaldum Ic... 33 2.3 AP009386_1894( AP009386 |pid:none) Burkholderia multi... EU955514 |pid:none) Zea mays clone 1535262 hypothetica... 50 2e-05 BA000023_1285

  6. Lamination sheet of AA BST magnet

    CERN Multimedia

    CERN PhotoLab

    1979-01-01

    The AA had 2 types of bending magnets: BLG (window-frame, long and narrow)and BST (H-type, short and wide). The BST had a very wide aperture, 0.564 m of "good field". To demonstrate the size, the petite AA secretary, Val Mansfield, poses with a lamination sheet. See also 7811105, 7906163, 8006050.

  7. 76 FR 30962 - Notice of Availability of Draft Environmental Impact Statement for the Sigurd to Red Butte No. 2...

    Science.gov (United States)

    2011-05-27

    ...; UTU-83067] Notice of Availability of Draft Environmental Impact Statement for the Sigurd to Red Butte..., as amended, the Bureau of Land Management (BLM) has prepared a Draft Environmental Impact Statement... Service; State of Utah; Millard, Sevier, Beaver, Iron, and Washington counties, Utah; and the cities of St...

  8. Geomagnetic aa Indices

    Data.gov (United States)

    National Oceanic and Atmospheric Administration, Department of Commerce — The geomagnetic aa indices are the continuation of the series beginning in the year 1868. A full description of these indices is given in the International...

  9. States' Flexibility Waiver Plans for Alternate Assessments Based on Alternate Achievement Standards (AA-AAS). Synthesis Report 96

    Science.gov (United States)

    Lazarus, Sheryl S.; Edwards, Lynn M.; Thurlow, Martha L.; Hodgson, Jennifer R.

    2014-01-01

    All states have alternate assessments based on alternate achievement standards (AA-AAS) for students with the most significant cognitive disabilities. For accountability purposes, the Elementary and Secondary Education Act (ESEA) allows up to 1% of students to be counted as proficient with this assessment option. In 2011 the U.S. Department of…

  10. Numerical modeling of friction welding of bi-metal joints for electrical applications

    Science.gov (United States)

    Velu, P. Shenbaga; Hynes, N. Rajesh Jesudoss

    2018-05-01

    In the manufacturing industries, and more especially in electrical engineering applications, the usage of non-ferrous materials plays a vital role. Today's engineering applications relies upon some of the significant properties such as a good corrosion resistance, mechanical properties, good heat conductivity and higher electrical conductivity. Copper-aluminum bi-metal joint is one such combination that meets the demands requirements for electrical applications. In this work, the numerical simulation of AA 6061 T6 alloy/Copper was carried out under joining conditions. By using this developed model, the temperature distribution along the length of the dissimilar joint is predicted and the time-temperature profile has also been generated. Besides, a Finite Element Model has been developed by using the numerical simulation Tool "ABAQUS". This developed FEM is helpful in predicting various output parameters during friction welding of this dissimilar joint combination.

  11. [AA amyloidosis: a little-known complication of chronic leg ulcer].

    Science.gov (United States)

    Waton, J; Fays-Michel, S; Chandeclerc, M L; Corby, S; Cuny, J F; Barbaud, A; Schmutz, J-L

    2008-02-01

    AA amyloidosis, secondary to inflammatory chronic diseases like rheumatoid arthritis, is often complicated by renal failure. Chronic inflammatory dermatoses constitute rare causes of AA amyloidosis. We describe two cases of AA amyloidosis discovered after renal failure in patients presenting leg ulcers for several years. AL amyloidosis was suspected in both cases because of a history of monoclonal gammopathy in one patient and of plasmocytoma in the other. The diagnosis of AA amyloidosis was confirmed on renal histology through the detection of AA antibodies in amyloid deposits. No extrarenal amyloidosis was seen in either patient and there were no inflammatory diseases other than chronic leg ulcers. AA amyloidosis is caused by serum amyloid protein A (SAA), a reactive inflammatory protein. AA amyloidosis is thus caused by chronic inflammatory diseases, but only rarely by cutaneous inflammatory diseases. To our knowledge, the literature contains only seven other published cases of AA amyloidosis secondary to chronic leg ulcers. A review of the literature does not indicate whether cure of ulcers has any effect on the accompanying renal failure. We imagine that AA amyloidosis secondary to leg ulcer is in fact under-diagnosed. However, since the first specific treatment for AA amyloidosis is currently being evaluated by the Food and Drug Administration, it is essential that this serious complication of chronic leg ulcers be widely recognised.

  12. Fatigue Strength Assessment of Welded Mild Steel Joints Containing Bulk Imperfections

    Directory of Open Access Journals (Sweden)

    Martin Leitner

    2018-04-01

    Full Text Available This work investigates the effect of gas pores, as bulk imperfections, on the fatigue strength of welded mild steel joints. Two test series containing different butt joint geometries and weld process parameters are included in order to achieve two variable types of pore sizes. Based on the √area-parameter by Murakami, the test series can be grouped into imperfections exhibiting √area < 1000 µm and √area > 1000 µm. Fatigue tests at a load stress ratio of R = 0.1 are performed, which act as comparison for the subsequent fatigue estimation. To assess the fatigue resistance, the approaches by Murakami, De Kazinczy, and Mitchell are utilized, which highlight certain differences in the applicability depending on the imperfection size. It is found that, on one hand, Murakami’s approach is well suitable for both small and large gas pores depending on the applied model parameters. On the other hand, the fatigue concepts by De Kazinczy and Mitchell are preferably practicable for large defects with √area > 1000 µm. In addition, the method by Mitchell incorporates the stress concentration factor of the imperfection, which can be numerically computed considering the size, shape, and location of the gas pore, as presented in this paper.

  13. The Western Environmental Technology Office (WETO), Butte, Montana. Technology summary (Revised)

    Energy Technology Data Exchange (ETDEWEB)

    NONE

    1996-03-01

    This document has been prepared by the US Department of Energy`s (DOE`s) Office of Environmental Management (EM) Office of Science and Technology (OST) to highlight its research, development, demonstration, testing, and evaluation (RDDT&E) activities funded through the Western environmental Technology Office (WETO) in Butte, Montana. Technologies and processes described in this document have the potential to enhance DOE`s cleanup and waste management efforts, as well as improve US industry`s competitiveness in global environmental markets. The information presented in this document has been assembled from recently produced OST documents that highlight technology development activities within each of the OST program elements and Focus Areas. This document presents one in a series for each of DOE`s Operations Office and Energy Technology Centers.

  14. The Western Environmental Technology Office (WETO), Butte, Montana. Technology summary (Revised)

    International Nuclear Information System (INIS)

    1996-03-01

    This document has been prepared by the US Department of Energy's (DOE's) Office of Environmental Management (EM) Office of Science and Technology (OST) to highlight its research, development, demonstration, testing, and evaluation (RDDT ampersand E) activities funded through the Western environmental Technology Office (WETO) in Butte, Montana. Technologies and processes described in this document have the potential to enhance DOE's cleanup and waste management efforts, as well as improve US industry's competitiveness in global environmental markets. The information presented in this document has been assembled from recently produced OST documents that highlight technology development activities within each of the OST program elements and Focus Areas. This document presents one in a series for each of DOE's Operations Office and Energy Technology Centers

  15. Microstructural evolution and properties of friction stir welded aluminium alloy AA2219

    International Nuclear Information System (INIS)

    Gupta, R. K.; Biju, S.; Ghosh, B. R.; Sinha, P. P.

    2007-01-01

    Low weld strength of fusion welded joints of aluminium alloy AA2219 is a concern in fabrication of pressure vessels and is attributable to the presence of weld defects, as well as various metallurgical factors. Friction stir welding (FSW), being a solid state joining process has obvious advantages over fusion welding. Results of preliminary FSW experiments conducted on 10 mm thick plate using a particular tool configuration are presented here. Microscopic studies show the presence of very fine equiaxed recrystallised grain at the weld nugget and a flow pattern of grains due to heavy deformation in defect-free weld coupons. Mechanical properties are correlated with the microstructure and process variables. Fractographic analysis complements the observations of optical microscopy and mechanical properties

  16. Interface and properties of the friction stir welded joints of titanium alloy Ti6Al4V with aluminum alloy 6061

    International Nuclear Information System (INIS)

    Wu, Aiping; Song, Zhihua; Nakata, Kazuhiro; Liao, Jinsun; Zhou, Li

    2015-01-01

    Highlights: • Friction stir butt welding of titanium alloy Ti6Al4V and aluminum alloy A6061-T6. • Welding parameters affect interfacial microstructure of the joint. • Welding parameters affect the mechanical property of joint and fracture position. • Joining mechanism of Ti6Al4V/A6061 dissimilar alloys by FSW is investigated. - Abstract: Titanium alloy Ti6Al4V and aluminum alloy 6061 dissimilar material joints were made with friction stir welding (FSW) method. The effects of welding parameters, including the stir pin position, the rotating rate and the travel speed of the tool, on the interface and the properties of the joints were investigated. The macrostructure of the joints and the fracture surfaces of the tensile test were observed with optical microscope and scanning electron microscope (SEM). The interface reaction layer was investigated with transmission electron microscopy (TEM). The factors affecting the mechanical properties of the joints were discussed. The results indicated that the tensile strength of the joints and the fracture location are mainly dependent on the rotating rate, and the interface and intermetallic compound (IMC) layer are the governing factor. There is a continuous 100 nm thick TiAl 3 IMC at the interface when the rotating rate is 750 rpm. When the welding parameters were appropriate, the joints fractured in the thermo-mechanically affected zone (TMAZ) and the heat affected zone (HAZ) of the aluminum alloy and the strength of the joints could reach 215 MPa, 68% of the aluminum base material strength, as well as the joint could endure large plastic deformation

  17. Abia, AA

    African Journals Online (AJOL)

    Abia, AA. Vol 4, No 6 (2010) - Articles Studies on the kinetics and intraparticle diffusivities of BOD, colour and TSS reduction from palm oil mill effluent (POME) using boiler fly ash. Abstract PDF. ISSN: 1996-0786. AJOL African Journals Online. HOW TO USE AJOL... for Researchers · for Librarians · for Authors · FAQ's · More ...

  18. Primary water stress corrosion cracking resistance of alloy 690 heat affected zones of butt welds

    International Nuclear Information System (INIS)

    Fournier, L.; Calonne, O.; Toloczko, M.B.; Bruemmer, S.M.; Massoud, J.P.; Lemaire, E.; Gerard, R.; Somville, F.; Richnau, A.; Lagerstrom, J.

    2015-01-01

    A wide V-groove butt weld was fabricated from Alloy 690 plates using Alloy 152 filler material, maximum allowable heat input, and very stiff strong-backs. Alloy 690 heat affected zones (HAZ) was characterized in terms of microstructure and plastic strains induced by weld shrinkage. Crack initiation tests were carried out in pure hydrogenated steam at 400 C. degrees for 4000 h. Crack growth rate tests were performed in simulated PWR primary water at a temperature of 360 C. degrees. A maximum plastic strain around 5% was measured in the vicinity of the fusion line, which decreased almost linearly with the distance from the fusion line. Crack initiation tests on Alloy 690 HAZ specimens as well as on 30% cold-rolled Alloy 690 specimens were performed in pure hydrogenated steam at 400 C. degrees (partial pressure of hydrogen = 0.7 bar) for a total of 4000 h using cylindrical notched tensile specimens, reverse U-bends and flat micro-tensile specimens. No crack initiation was detected. Stress corrosion propagation rates revealed extremely low SCC (Stress Corrosion Cracking) growth rates both in the base metal and in the HAZ region whose magnitudes are of no engineering significance. Overall, the results indicated limited plastic strain induced by weld shrinkage in butt weld HAZ, and to no particular susceptibility of primary water stress corrosion cracking. (authors)

  19. Microsolvation of the acetanilide cation (AA(+)) in a nonpolar solvent: IR spectra of AA(+)-L(n) clusters (L = He, Ar, N2; n ≤ 10).

    Science.gov (United States)

    Schmies, Matthias; Patzer, Alexander; Schütz, Markus; Miyazaki, Mitsuhiko; Fujii, Masaaki; Dopfer, Otto

    2014-05-07

    Infrared photodissociation (IRPD) spectra of mass-selected cluster ions of acetanilide (N-phenylacetamide), AA(+)-Ln, with the ligands L = He (n = 1-2), Ar (n = 1-7), and N2 (n = 1-10) are recorded in the hydride stretch (amide A, νNH, νCH) and fingerprint (amide I-III) ranges of AA(+) in its (2)A'' ground electronic state. Cold AA(+)-Ln clusters are generated in an electron impact ion source, which predominantly produces the most stable isomer of a given cluster ion. Systematic vibrational frequency shifts of the N-H stretch fundamentals (νNH) provide detailed information about the sequential microsolvation process of AA(+) in a nonpolar (L = He and Ar) and quadrupolar (L = N2) solvent. In the most stable AA(+)-Ln clusters, the first ligand forms a hydrogen bond (H-bond) with the N-H proton of trans-AA(+) (t-AA(+)), whereas further ligands bind weakly to the aromatic ring (π-stacking). There is no experimental evidence for complexes with the less stable cis-AA(+) isomer. Quantum chemical calculations at the M06-2X/aug-cc-pVTZ level confirm the cluster growth sequence derived from the IR spectra. The calculated binding energies of De(H) = 720 and 1227 cm(-1) for H-bonded and De(π) = 585 and 715 cm(-1) for π-bonded Ar and N2 ligands in t-AA(+)-L are consistent with the observed photofragmentation branching ratios of AA(+)-Ln. Comparison between charged and neutral AA((+))-L dimers indicates that ionization switches the preferred ion-ligand binding motif from π-stacking to H-bonding. Electron removal from the HOMO of AA(+) delocalized over both the aromatic ring and the amide group significantly strengthens the C[double bond, length as m-dash]O bond and weakens the N-H bond of the amide group.

  20. Wintercuring of Prunus dulcis cv ‘Butte,’ P. webbii and their interspecific hybrid in response to Xylella fastidiosa infections

    Science.gov (United States)

    Clonal replicates of Prunus dulcis cv ‘Butte,’ P. webbii and their interspecific hybrid P 63-61 were inoculated with Xylella fastidiosa strain M23 and evaluated for Almond Leaf Scorch Disease and subsequent wintercuring of infections during three growing seasons. Initial inoculations established gr...

  1. Molecular dynamics modeling of bonding two materials by atomic scale friction stir welding

    Science.gov (United States)

    Konovalenko S., Iv.; Konovalenko, Ig. S.; Psakhie, S. G.

    2017-12-01

    Molecular dynamics model of atomic scale friction stir welding has been developed. Formation of a butt joint between two crystallites was modeled by means of rotating rigid conical tool traveling along the butt joint line. The formed joint had an intermixed atomic structure composed of atoms initially belonged to the opposite mated piece of metal. Heat removal was modeled by adding the extra viscous force to peripheral atomic layers. This technique provides the temperature control in the tool-affected zone during welding. Auxiliary vibration action was added to the rotating tool. The model provides the variation of the tool's angular velocity, amplitude, frequency and direction of the auxiliary vibration action to provide modeling different welding modes.

  2. Thermo-Mechanical Characterization of Friction Stir Spot Welded AA7050 Sheets by Means of Experimental and FEM Analyses.

    Science.gov (United States)

    D'Urso, Gianluca; Giardini, Claudio

    2016-08-11

    The present study was carried out to evaluate how the friction stir spot welding (FSSW) process parameters affect the temperature distribution in the welding region, the welding forces and the mechanical properties of the joints. The experimental study was performed by means of a CNC machine tool obtaining FSSW lap joints on AA7050 aluminum alloy plates. Three thermocouples were inserted into the samples to measure the temperatures at different distance from the joint axis during the whole FSSW process. Experiments was repeated varying the process parameters, namely rotational speed, axial feed rate and plunging depth. Axial welding forces were measured during the tests using a piezoelectric load cell, while the mechanical properties of the joints were evaluated by executing shear tests on the specimens. The correlation found between process parameters and joints properties, allowed to identify the best technological window. The data collected during the experiments were used to validate a simulation model of the FSSW process, too. The model was set up using a 2D approach for the simulation of a 3D problem, in order to guarantee a very simple and practical solution for achieving results in a very short time. A specific external routine for the calculation of the thermal energy due to friction acting between pin and sheet was developed. An index for the prediction of the joint mechanical properties using the FEM simulations was finally presented and validated.

  3. Thermo-Mechanical Characterization of Friction Stir Spot Welded AA7050 Sheets by Means of Experimental and FEM Analyses

    Directory of Open Access Journals (Sweden)

    Gianluca D’Urso

    2016-08-01

    Full Text Available The present study was carried out to evaluate how the friction stir spot welding (FSSW process parameters affect the temperature distribution in the welding region, the welding forces and the mechanical properties of the joints. The experimental study was performed by means of a CNC machine tool obtaining FSSW lap joints on AA7050 aluminum alloy plates. Three thermocouples were inserted into the samples to measure the temperatures at different distance from the joint axis during the whole FSSW process. Experiments was repeated varying the process parameters, namely rotational speed, axial feed rate and plunging depth. Axial welding forces were measured during the tests using a piezoelectric load cell, while the mechanical properties of the joints were evaluated by executing shear tests on the specimens. The correlation found between process parameters and joints properties, allowed to identify the best technological window. The data collected during the experiments were used to validate a simulation model of the FSSW process, too. The model was set up using a 2D approach for the simulation of a 3D problem, in order to guarantee a very simple and practical solution for achieving results in a very short time. A specific external routine for the calculation of the thermal energy due to friction acting between pin and sheet was developed. An index for the prediction of the joint mechanical properties using the FEM simulations was finally presented and validated.

  4. Effects of Friction Stir Welding on Corrosion Behaviors of AA2024-T4 Aluminum Alloy

    Directory of Open Access Journals (Sweden)

    Ales Steve Korakan

    2017-01-01

    Full Text Available In this work, the corrosion behavior of welded joints of AA2024-T4 Al alloy produced by friction stir welding process has been investigated. Tests were performed in an aerated 3.5% NaCl aqueous solution with pH = 7 at 20±2°C. Corrosion rate and corrosion morphology of weld regions were evaluated and compared to those of the parent metal. The microstructure of weld nugget, thermomechanical affected zone, heated affected zone, and parent metal were analyzed using scanning electron microscopy and energy dispersive spectroscopy. It was observed that corrosion initiated at FSW related spots and the sizes of local corrosion increased with time.

  5. The Western Environmental Technology Office (WETO), Butte, Montana, technology summary

    International Nuclear Information System (INIS)

    1994-09-01

    This document has been prepared by the DOE Environmental Management (EM) Office of Technology Development (OTD) to highlight its research, development, demonstration, testing, and evaluation activities funded through the Western Environmental Technology Office (WETO) in Butte, Montana. Technologies and processes described have the potential to enhance DOE's cleanup and waste management efforts, as well as improve US industry's competitiveness in global environmental markets. WETO's environmental technology research and testing activities focus on the recovery of useable resources from waste. Environmental technology development and commercialization activities will focus on mine cleanup, waste treatment, resource recovery, and water resource management. Since the site has no record of radioactive material use and no history of environmental contamination/remediation activities, DOE-EM can concentrate on performing developmental and demonstration activities without the demands of regulatory requirements and schedules. Thus, WETO will serve as a national resource for the development of new and innovative environmental technologies

  6. Characteristics of AA amyloidosis patients in San Francisco.

    Science.gov (United States)

    Lejmi, Hiba; Jen, Kuang-Yu; Olson, Jean L; James, Sam H; Sam, Ramin

    2016-04-01

    AA amyloidosis due to subcutaneous injection of drugs of abuse has been described in the USA, but all the existing literature is from more than 20 years ago. There is more recent literature from Europe. We have observed a high incidence of AA amyloidosis in the county hospital in San Francisco. Here, we describe 24 patients who had kidney biopsy-proven AA amyloidosis from our hospital from 1998 to 2013. All the patients were thought to have AA amyloidosis from skin popping of illicit drugs after having exhausted the intravenous route. These patients with biopsy-proven AA amyloidosis were analysed further. All patients were found to have hepatitis C infection, hypertension was not common, most had advanced kidney failure, and acidosis was common as was tubulointerstitial involvement on the kidney biopsy. Other organ involvement included hepatomegaly and splenomegaly in a number of patients; direct myocardial involvement was not seen, but pulmonary hypertension, history of deep vein thrombosis and pulmonary embolism were common. The prognosis of these patients was poor. The mortality rate approached 50% 1 year after biopsy, and most of the patient needed dialysis shortly after diagnosis. Cessation of drug use seemed beneficial but rarely achievable. AA amyloidosis from skin popping is common in San Francisco. Most patients with renal involvement end up on dialysis, and mortality rates are exceedingly high. © 2015 Asian Pacific Society of Nephrology.

  7. Residual-stress distributions near stainless steel butt weldments

    International Nuclear Information System (INIS)

    Elligson, W.A.; Shack, W.J.

    1978-01-01

    Concern for the integrity of stainless steel butt-weldments in boiling-water-reactor (BWR) piping systems has stimulated study of the conditions that cause stress corrosion cracking (SCC) in the heat-affected zones (HAZ) of the weldments. It is generally agreed that a high stress exceeding the initial yield strength is one of the essential elements for crack initiation. Since design procedures usually ensure that load stresses are below initial yield, the source of the high stresses necessary to produce SCC is thought to be the residual stresses due to welding. To examine the level of residual stresses in the weldments of interest, bulk residual stresses were measured on 100 mm (4-in.) and 254 mm (10-in.) diameter Schedule 80 piping weldments using strain relief techniques. Both laboratory welded specimens and field welded specimens from reactors in service were studied. Axial bulk residual stress distributions were obtained at 45 0 intervals around the circumference. At each azimuthal position, the residual stresses were measured at seven axial positions: on the weld centerline and 13, 20, and 25 mm on either side of the weld centerline on both the inside and outside surfaces

  8. Effect of friction stir welding on microstructure, mechanical and wear properties of AA6061/ZrB2 in situ cast composites

    International Nuclear Information System (INIS)

    Dinaharan, I.; Murugan, N.

    2012-01-01

    Highlights: ► Application of FSW to join AA6061/ZrB 2 in situ composites. ► Homogenous distribution of ZrB 2 particles in the weld zone. ► Clusters in the parent composite are fragmented by the stirring action of the tool. ► Hardening of weld zone. ► FSW enhanced the wear resistance of the composite. - Abstract: Inadequate development of fabrication methods restricts the applications of new families of aluminum matrix composites (AMCs). Friction stir welding (FSW) is a potential candidate to join AMCs without any defects associated with conventional fusion welding processes. The primary objective of the present work is to apply FSW process to join AA6061/(0, 5 and 10 wt.%) ZrB 2 in situ cast composites and evaluate the joint properties. The composites were prepared by reacting inorganic salts K 2 ZrF 6 and KBF 4 with molten aluminum and joined using a FSW machine at a tool rotational speed of 1150 rpm, welding speed of 50 mm/min and axial force of 6 kN. The joints showed the presence of various zones such as weld zone (WZ), thermomechanically affected zone (TMAZ) and heat affected zone (HAZ). The weld zone was characterized with a homogenous distribution of ZrB 2 particles. The stirring action of the tool resulted in fragmentation of several clusters present in the parent composite. The weld zone exhibited higher hardness than that of the parent composite. The tensile strength of welded joints was comparable to that of parent composites. The wear resistance of the composites improved subsequent to FSW.

  9. Summary of 21st joint EU-US transport task force workshop.

    Czech Academy of Sciences Publication Activity Database

    Mantica, P.; Bourdelle, C.; Camenen, Y.; Dejarnac, Renaud; Evans, T.; Görler, T.; Hillesheim, J.; Idomura, Y.; Jakubowski, M.; Ricci, P.; White, A.

    2017-01-01

    Roč. 57, č. 8 (2017), č. článku 087001. ISSN 0029-5515. [Joint EU-US Transport Task Force workshop/21./. Leysin, 05.09.2016-08.09.2016] EU Projects: European Commission(XE) 633053 - EUROfusion Institutional support: RVO:61389021 Keywords : transport * confinement * turbulence Subject RIV: BL - Plasma and Gas Discharge Physics OBOR OECD: Fluids and plasma physics (including surface physics) Impact factor: 3.307, year: 2016 http://iopscience.iop.org/article/10.1088/1741-4326/aa753f/meta

  10. The Antiproton Accumulator (AA)

    CERN Multimedia

    1980-01-01

    Section 06 - 08*) of the AA where the dispersion (and hence the horizontal beam size) is large. One can distinguish (left to right): A vacuum-tank, two bending magnets (BST06 and BST07 in blue) with a quadrupole (QDN07, in red) in between, another vacuum-tank, a wide quadrupole (QFW08) and a further tank . The tanks are covered with heating tape for bake-out. The tank left of BST06 contained the stack core pickup for stochastic cooling (see 7906193, 7906190, 8005051), the two other tanks served mainly as vacuum chambers in the region where the beam was large. Peter Zettwoch works on BST06. *) see: H. Koziol, Antiproton Accumulator Parameter List, PS/AA/Note 84-2 (1984)

  11. Effect of pressurized steam on AA1050 aluminium

    DEFF Research Database (Denmark)

    Jariyaboon, Manthana; Møller, Per; Ambat, Rajan

    2012-01-01

    Purpose - The purpose of this paper is to understand the effect of pressurized steam on surface changes, structures of intermetallic particles and corrosion behavior of AA1050 aluminium. Design/methodology/approach - Industrially pure aluminium (AA1050, 99.5 per cent) surfaces were exposed...... reactivities was observed due to the formation of the compact oxide layer. Originality/value - This paper reveals a detailed investigation of how pressurized steam can affect the corrosion behaviour of AA1050 aluminium and the structure of Fe-containing intermetallic particles....

  12. Effect of Activated Flux on the Microstructure, Mechanical Properties, and Residual Stresses of Modified 9Cr-1Mo Steel Weld Joints

    Science.gov (United States)

    Maduraimuthu, V.; Vasudevan, M.; Muthupandi, V.; Bhaduri, A. K.; Jayakumar, T.

    2012-02-01

    A novel variant of tungsten inert gas (TIG) welding called activated-TIG (A-TIG) welding, which uses a thin layer of activated flux coating applied on the joint area prior to welding, is known to enhance the depth of penetration during autogenous TIG welding and overcomes the limitation associated with TIG welding of modified 9Cr-1Mo steels. Therefore, it is necessary to develop a specific activated flux for enhancing the depth of penetration during autogeneous TIG welding of modified 9Cr-1Mo steel. In the current work, activated flux composition is optimized to achieve 6 mm depth of penetration in single-pass TIG welding at minimum heat input possible. Then square butt weld joints are made for 6-mm-thick and 10-mm-thick plates using the optimized flux. The effect of flux on the microstructure, mechanical properties, and residual stresses of the A-TIG weld joint is studied by comparing it with that of the weld joints made by conventional multipass TIG welding process using matching filler wire. Welded microstructure in the A-TIG weld joint is coarser because of the higher peak temperature in A-TIG welding process compared with that of multipass TIG weld joint made by a conventional TIG welding process. Transverse strength properties of the modified 9Cr-1Mo steel weld produced by A-TIG welding exceeded the minimum specified strength values of the base materials. The average toughness values of A-TIG weld joints are lower compared with that of the base metal and multipass weld joints due to the presence of δ-ferrite and inclusions in the weld metal caused by the flux. Compressive residual stresses are observed in the fusion zone of A-TIG weld joint, whereas tensile residual stresses are observed in the multipass TIG weld joint.

  13. Reinforcement with alumina particles at the interface region of AA6101-T6 and AA1350 alloys during friction stir welding

    Science.gov (United States)

    Ashok Kumar, R.; Thansekhar, M. R.

    2018-04-01

    This paper deals the combinational effect of friction stir welding and friction stir processing on dissimilar AA6101-T6 and AA1350 aluminium alloys. For that, alumina particles are reinforced at interface region of AA6101-T6 and AA1350 aluminium alloys. Friction Stir Welding and Friction Stir Processing are done simultaneously for various sizes of groove. To analyze the welding quality and surface modifications, mechanical, wear and microstructural tests are carried out. Among these, smallest groove of 0.5 mm width and 1 mm depth reveals highest tensile and bending strengths and largest groove of 2 mm width and 3 mm depth gives maximum hardness and wear resistance. Taguchi technique shows that groove width is most influencing parameter. Developed second order models with interaction predict the responses with minimum error.

  14. Fiber laser welding of nickel based superalloy Inconel 625

    Science.gov (United States)

    Janicki, Damian M.

    2013-01-01

    The paper describes the application of single mode high power fiber laser (HPFL) for the welding of nickel based superalloy Inconel 625. Butt joints of Inconel 625 sheets 0,8 mm thick were laser welded without an additional material. The influence of laser welding parameters on weld quality and mechanical properties of test joints was studied. The quality and mechanical properties of the joints were determined by means of tensile and bending tests, and micro hardness tests, and also metallographic examinations. The results showed that a proper selection of laser welding parameters provides non-porous, fully-penetrated welds with the aspect ratio up to 2.0. The minimum heat input required to achieve full penetration butt welded joints with no defect was found to be 6 J/mm. The yield strength and ultimate tensile strength of the joints are essentially equivalent to that for the base material.

  15. Simon van der Meer in the AA Control Room

    CERN Multimedia

    CERN PhotoLab

    1984-01-01

    Simon van der Meer, spiritus rector of the Antiproton Accumulator, in the AA Control Room. Inventor of stochastic cooling, on which the AA was based, and of the magnetic horn, with which the antiprotons were focused, he also wrote most of the software with which the AA was controlled, and spent uncountable numbers of hours in this chair to tickle the AA to top performance. 8 months after this picture was taken, he received, in October 1984, the Nobel prize, together with Carlo Rubbia, the moving force behind the whole Proton-Antiproton Collider project that led to the discovery, in 1983, of the W and Z intermediate bosons.

  16. Inclusive cross sections in AA collisions at high energies

    International Nuclear Information System (INIS)

    Braun, M.A.

    1988-01-01

    Inclusive cross sections in AA collisions at high energies are considered in the Glauber multiple scattering theory taking into account many-nucleon collisions. Correspondence is found between the AA amplitude and the effective action of the two-dimensional quantum field theory with exponential interaction. The tree and one-loop contributions are calculated in this formalism. The rules are derived, which relate the absorption part of the AA-collision amplitudes associated with various inclusive cross sections to the absorption parts of NN amplitudes. These rules generalize the well-known Agranowsky-Gribov-Kanchelli rules for hh and hA collisions. Formulas are written for single and double inclusive cross sections in AA collisions

  17. Bake hardening of nanograin AA7075 aluminum alloy

    International Nuclear Information System (INIS)

    Dehghani, Kamran

    2011-01-01

    Highlights: ► The bake hardening behavior of AA7075 was studied and compared with its coarse-grain counterpart. ► Nanograin AA7075 exhibited 88–100% increase in bake hardenability. ► Nanograin AA7075 exhibited 36–38% increase in final yield strength after baking. ► Maximum bake hardenability and final yield stress were about 185 MPa and 719 MPa. - Abstract: In the present work, the bake hardening of nanostructured AA7075 aluminum alloy was compared with that of its coarse-grain counterpart. Surface severe plastic deformation (SSPD) was used to produce nanograin layers on both surfaces of workpieces. The nanostructured layers were characterized using scanning electron microscopy (SEM) and atomic force microscopy (AFM) techniques. The thickness of nanostructured layer, having the grains of 50–110 nm, was about 75 μm on each side of workpiece. The bake hardenability of nanograin and coarse-grain AA7075 was then compared by pre-straining to 2, 4 and 6% followed by baking at 100 °C and 200 °C for 20 min. Comparing to coarse-grain case, there was about 88–100% increase in bake hardenability and about 36–38% increase in yield strength after the bake hardening of present nanograin AA7075. Such an increase in bake hardenability and strength was achieved when the thickness of two nanograin layers was about only one-tenth of the whole thickness.

  18. Effect of post weld heat treatment on tensile properties and microstructure characteristics of friction stir welded armour grade AA7075-T651 aluminium alloy

    OpenAIRE

    Sivaraj, P.; Kanagarajan, D.; Balasubramanian, V.

    2014-01-01

    This paper reports the effects of post weld heat treatments, namely artificial ageing and solution treatment followed by artificial ageing, on microstructure and mechanical properties of 12 mm thick friction stir welded joints of precipitation hardenable high strength armour grade AA7075-T651 aluminium alloy. The tensile properties, such as yield strength, tensile strength, elongation and notch tensile strength, are evaluated and correlated with the microhardness and microstructural features....

  19. The Western Environmental Technology Office (WETO), Butte, Montana, technology summary

    Energy Technology Data Exchange (ETDEWEB)

    1994-09-01

    This document has been prepared by the DOE Environmental Management (EM) Office of Technology Development (OTD) to highlight its research, development, demonstration, testing, and evaluation activities funded through the Western Environmental Technology Office (WETO) in Butte, Montana. Technologies and processes described have the potential to enhance DOE`s cleanup and waste management efforts, as well as improve US industry`s competitiveness in global environmental markets. WETO`s environmental technology research and testing activities focus on the recovery of useable resources from waste. Environmental technology development and commercialization activities will focus on mine cleanup, waste treatment, resource recovery, and water resource management. Since the site has no record of radioactive material use and no history of environmental contamination/remediation activities, DOE-EM can concentrate on performing developmental and demonstration activities without the demands of regulatory requirements and schedules. Thus, WETO will serve as a national resource for the development of new and innovative environmental technologies.

  20. Residual stress in a thick section high strength T-butt weld

    International Nuclear Information System (INIS)

    Pearce, S.V.; Linton, V.M.; Oliver, E.C.

    2008-01-01

    Residual stresses in a structure are generated as a result of the various fabrication and welding processes used to make the component. Being able to quantify these residual stresses is a key step in determining the continuing integrity of a structure in service. In this work, the residual stresses around a high strength, quenched and tempered steel T-butt web to curved plate weld have been measured using neutron strain scanning. The results show that the residual stresses near the weld were dominated by the welding residual stresses, while the stresses further from the weld were dominated by the bending residual stresses. The results suggest that the combination of welding-induced residual stress and significant pre-welding residual stress, as in the case of a thick bent section of plate can significantly alter the residual stress profile from that in a flat plate

  1. A non-conventional technique for evaluating welded joints based on the electrical conductivity

    Energy Technology Data Exchange (ETDEWEB)

    Santos, T.G.; Sorger, G., E-mail: telmo.santos@fct.unl.pt, E-mail: lgs18243@campus.fct.unl.pt [Universidade Nova de Lisboa, UNIDEMI, Departamento de Engenharia Mecanica e Industrial, Faculdade de Ciencias e Tecnologia, Caparica (Portugal); Vilaca, P., E-mail: pedro.vilaca@aalto.fi [Aalto Univ., Dept. of Engineering Design and Production, School of Engineering, Aalto (Finland); Miranda, R., E-mail: rmiranda@fct.unl.pt [Universidade Nova de Lisboa, UNIDEMI, Departamento de Engenharia Mecanica e Industrial, Faculdade de Ciencias e Tecnologia, Caparica (Portugal)

    2015-01-15

    Recent studies showed that electrical conductivity is a valuable technique to identify the different zones of solid-state welded joints with a good correlation with the microstructure and hardness. This is a relevant result since this technique is fast and, in some cases, non destructive, The concept was applied to other welding processes such as the ones involving fusion to a wide range of materials, For this, a comprehensive study was performed using friction stir welding, tungsten inert gas (TlG) and gas metal arc (MAG) welding processes in either bead on plate or butt joints in: carbon steel, magnesium and titanium, Eddy current nondestructive testing (NDT) was used to measure the electrical conductivity at different depths in transverse sections of the processed materials. The profiles were compared to the hardness profiles in the same sections. As a result, a correlation was observed in most materials welded by solid state and by fusion processes. The variation of the electrical conductivity closely follows that measured in the hardness. Another interesting conclusion is that, even for fusion welding of carbon steels, the technique has potential to complement the hardness measurements and microstructural observations, allowing the identification of the distinct zones of welds in materials commonly used in industry. (author)

  2. Mechanical and corrosion properties of AA8011 sheets and foils:

    OpenAIRE

    Asanović, Vanja; Dalijić, Kemal; Radonjić, Dragan

    2006-01-01

    The mechanical and corrosion properties of a twin-roll cast Al-Fe-Si aluminum alloy with 0.74 % Fe and 0.52 % Si (AA8011) were investigated. The influence of the thermo-mehanical processing route on the mechanical behavior of AA8011 sheets was determined. Comparisons were made with AA3003 and A199.5 sheets. The restoration of the mechanical properties was used in the analysis of the recrystallization behavior of the twin-roll cast AA8011 alloy deformed under cold-working conditions and subseq...

  3. CSI 2264: Probing the inner disks of AA Tauri-like systems in NGC 2264

    Science.gov (United States)

    McGinnis, P. T.; Alencar, S. H. P.; Guimarães, M. M.; Sousa, A. P.; Stauffer, J.; Bouvier, J.; Rebull, L.; Fonseca, N. N. J.; Venuti, L.; Hillenbrand, L.; Cody, A. M.; Teixeira, P. S.; Aigrain, S.; Favata, F.; Fűrész, G.; Vrba, F. J.; Flaccomio, E.; Turner, N. J.; Gameiro, J. F.; Dougados, C.; Herbst, W.; Morales-Calderón, M.; Micela, G.

    2015-05-01

    Context. The classical T Tauri star (CTTS) AA Tau has presented photometric variability that was attributed to an inner disk warp, caused by the interaction between the inner disk and an inclined magnetosphere. Previous studies of the young cluster NGC 2264 have shown that similar photometric behavior is common among CTTS. Aims: The goal of this work is to investigate the main causes of the observed photometric variability of CTTS in NGC 2264 that present AA Tau-like light curves, and verify if an inner disk warp could be responsible for their observed variability. Methods: In order to understand the mechanism causing these stars' photometric behavior, we investigate veiling variability in their spectra and u - r color variations and estimate parameters of the inner disk warp using an occultation model proposed for AA Tau. We also compare infrared Spitzer IRAC and optical CoRoT light curves to analyze the dust responsible for the occultations. Results: AA Tau-like variability proved to be transient on a timescale of a few years. We ascribe this variability to stable accretion regimes and aperiodic variability to unstable accretion regimes and show that a transition, and even coexistence, between the two is common. We find evidence of hot spots associated with occultations, indicating that the occulting structures could be located at the base of accretion columns. We find average values of warp maximum height of 0.23 times its radial location, consistent with AA Tau, with variations of on average 11% between rotation cycles. We also show that extinction laws in the inner disk indicate the presence of grains larger than interstellar grains. Conclusions: The inner disk warp scenario is consistent with observations for all but one star with AA Tau-like variability in our sample. AA Tau-like systems are fairly common, comprising 14% of CTTS observed in NGC 2264, though this number increases to 35% among systems of mass 0.7 M⊙ ≲ M ≲ 2.0 M⊙. Assuming random

  4. Fred-Jaiyesimi, AA

    African Journals Online (AJOL)

    Fred-Jaiyesimi, AA. Vol 12 (2008) - Articles Hypoglycaemic And Alpha-Amylase Inhibitory Activities Of Fermented Seeds Of Parkia Biglobosa (Jacq) Benth Abstract. ISSN: 1118-6267. AJOL African Journals Online. HOW TO USE AJOL... for Researchers · for Librarians · for Authors · FAQ's · More about AJOL · AJOL's ...

  5. Gas tungsten arc welding assisted hybrid friction stir welding of dissimilar materials Al6061-T6 aluminum alloy and STS304 stainless steel

    International Nuclear Information System (INIS)

    Bang, HanSur; Bang, HeeSeon; Jeon, GeunHong; Oh, IkHyun; Ro, ChanSeung

    2012-01-01

    Highlights: ► GTAW assisted hybrid friction stir welding (HFSW) has been carried out for dissimilar butt joint. ► Mechanical strength of dissimilar butt joint by HFSW and FSW has been investigated and compared. ► Microstructure of dissimilar butt joint by HFSW and FSW has been investigated and compared. -- Abstract: The aim of this research is to evaluate the potential for using the gas tungsten arc welding (GTAW) assisted hybrid friction stir welding (HFSW) process to join a stainless steel alloy (STS304) to an aluminum alloy (Al6061) in order to improve the weld strength. The difference in mechanical and microstructural characteristics of dissimilar joint by friction stir welding (FSW) and HFSW has been investigated and compared. Transverse tensile strength of approximately 93% of the aluminum alloy (Al6061) base metal tensile strength is obtained with HFSW, which is higher than the tensile strength of FSW welds. This may be due to the enhanced material plastic flow and partial annealing effect in dissimilar materials due to preheating of stainless steel surface by GTAW, resulting in significantly increased elongation of welds. The results indicate that HFSW that integrates GTAW preheating to FSW is advantageous in joining dissimilar combinations compared to conventional FSW.

  6. The Calculated and Measured Resistance for Splices between Conductors in a MICE Superconducting Coil

    International Nuclear Information System (INIS)

    Green, Michael A.; Dietderich, Dan; Higley, Hugh; Pan, Heng; Tam, Darren; Trillaud, Federic; Wang, Li; Wu, Hong; Xu, Feng Yu

    2009-01-01

    The resistance of superconducting joints within MICE coils is an important issue particularly for the coupling coils. The MICE tracker solenoids have only two superconducting joints in the three spectrometer set (end coil 1, the center coil and end coil 2). The AFC magnets may have only a single joint within the coil. The coupling coils may have as many as fifteen joints within the coil, due to relatively short piece lengths of the superconductor. LBNL and ICST looked at three types of coil joints. They are: (1) cold fusion butt joints, (2) side-by-side lap joints, and (3) up-down lap joints. A theoretical calculation of the joint resistance was done at LBNL and checked by ICST. After looking at the theoretical resistance of the three types of joints, it was decided that the cold welded butt joint was not an attractive alternative for joints within a MICE superconducting magnet coil. Side-by-side and up-down lap joints were fabricated at ICST using two types of soft solder between the conductors. These conductor joints were tested at LBNL at liquid helium temperatures over a range of magnetic fields. The joint resistance was compared with the theoretical calculations. Measurements of splice strength were also made at 300 K and 77 K.

  7. Displaying Now-Understanding: The Finnish Change-of-State Token "aa"

    Science.gov (United States)

    Koivisto, Aino

    2015-01-01

    This article discusses the use of the Finnish change-of-state token "aa" that has previously not been identified. The central claim is that even though "aa" indicates a cognitive shift experienced by the speaker, it does not function as a receipt of new information. Instead, the token "aa" indicates that the speaker…

  8. Recreational Use and Value of Water at Elephant Butte and Navajo Reservoirs. New Mexico State University Agricultural Experiment Station Bulletin 535.

    Science.gov (United States)

    Coppedge, Robert O.; Gray, James R.

    This document is a descriptive study of the recreational use and the value of water at Elephant Butte and Navajo Reservoirs. Previous research studies, as well as the study areas and recreational characteristics and procedures of investigation used in this study (sampling and data collection, data organization, analysis) are described. Discussions…

  9. Dynamic Response and Microstructure Evolution of AA2219-T4 and AA2219-T6 Aluminum Alloys

    Science.gov (United States)

    Olasumboye, A.; Owolabi, G.; Odeshi, A.; Zeytinci, A.; Yilmaz, N.

    2018-02-01

    In this study, the dynamic deformation behavior of AA2219 aluminum alloy was investigated in two different temper conditions: T4 and T6, with a view to determining the effect of heat treatment on the microstructure and flow behavior of the material under high strain rates. Split Hopkinson pressure bar experiment was used in determining the dynamic response of the alloy while a digital image correlation system was employed in visualizing and tracking the surface deformation of the specimens. Optical microscopy and scanning electron microscopy were used to assess the microstructure of the material after following standard metallographic specimen preparation techniques. The results obtained showed heterogeneous deformation of the alloy in the two temper conditions. It was observed that the dynamic mechanical behavior of each sample preparation was dependent on its strength properties due to aging type, which in turn controls the metamorphosis of the strengthening precipitates and the initial microstructure. At the maximum strain rate of 3500 s-1, transformed bands leading to crack nucleation was observed in the AA2219-T4 aluminum alloy while AA2219-T6 had fractured at the same strain rate. The modes of crack formation and growth in the two alloys were found to be similar: nucleation, growth and coalescence of voids. However, shear band bifurcation phenomenon was observed only in the AA2219-T6 alloy.

  10. Influence of Friction Stir Welding on Mechanical Properties of Butt Joints of AZ61 Magnesium Alloy

    Directory of Open Access Journals (Sweden)

    Seung-Ju Sun

    2017-01-01

    Full Text Available In this study, the effect of heat input on the mechanical properties and fracture behaviors of AZ61 magnesium alloy joints has been studied. Magnesium alloy AZ61 plates with thickness of 5 mm were welded at different ratios of tool rotational speed to welding speed (ω/ν. The average ultimate tensile strength of all weld conditions satisfying a ω/ν ratio of 3 reached 100% of the strength of the base material. Fractures occurred at the interface between the thermomechanical affected zone at advancing side and the stir zone in all welded specimens. From the scanning electron microscope and electron backscatter diffraction analysis, it was determined that the interface between the thermomechanical affected zone and the stir zone, which is the region where the grain orientation changes, was the weakest part; the advancing side region was relatively weaker than the retreating side region because the grain orientation change occurred more dramatically in the advancing side region.

  11. Spontaneous, Experimentally Induced, and Transmissible AA Amyloidosis in Japanese Quail ( Coturnix japonica).

    Science.gov (United States)

    Nakayama, Yumi; Kamiie, Junichi; Watanabe, Gen; Suzuki, Kazuhiko; Murakami, Tomoaki

    2017-11-01

    The authors describe a spontaneous case of amyloid A (AA) amyloidosis in an adult female Japanese quail ( Coturnix japonica). The bird developed AA amyloidosis secondary to chronic peritonitis caused by a Gram-negative bacillus infection. Mild amyloid deposition was also identified in the intestinal tract of apparently healthy adult individuals, suggesting that quail may develop intestinal amyloidosis with age. Based on these observations, it was hypothesized that quail can develop AA amyloidosis following inflammatory stimulation with lipopolysaccharide (LPS). Therefore, adult quail were repeatedly injected with LPS and the development of AA amyloidosis was confirmed. The amyloid deposition in this model increased when quail amyloid was intravenously injected as an amyloid-enhancing factor. The experiments were repeated with young quail, but amyloid deposits were not observed following LPS injections. However, AA amyloidosis did develop when quail amyloid was injected in addition to LPS. These results indicated that adult quail develop AA amyloidosis after inflammatory stimulation with LPS. Furthermore, quail AA amyloidosis was shown to have transmissibility regardless of age. Interestingly, the authors found that administration of chicken amyloid fibrils also induced AA amyloidosis in young quail. This is the first report of cross-species transmission of avian AA amyloidosis.

  12. Integrated Modelling of Crack Propagation in AA2024-T3 FSW Butt Joints Considering The Residual Stresses from the Manufacturing Process

    DEFF Research Database (Denmark)

    Sonne, M. R.; Carlone, P.; Citarella, R.

    2015-01-01

    This research is focused on one of the problems frequently encountered in spot welding in industry. In many applications several spot welds are made close to each other. The spots made after the first spot may become smaller in size due to shunt effect. A numerical and experimental study has been...... conducted to investigate the effect of shunting on nugget size in spot welding of HSLA steel sheets. Different cases with different spacing between weld spots have been examined. The nugget sizes have been measured by metallographic examination and have been compared with 3D finite element simulations...

  13. AA Attendance and Abstinence for Dually Diagnosed Patients: A Meta-Analytic Review.

    Science.gov (United States)

    Scott Tonigan, J; Pearson, Matthew R; Magill, Molly; Hagler, Kylee J

    2018-05-29

    There is consensus that best clinical practice for dual diagnosis (DD) is integrated mental health and substance use treatment augmented with Alcoholics Anonymous (AA) attendance. This is the first quantitative review of the direction and magnitude of the association between AA attendance and alcohol abstinence for DD patients. A systematic literature search (1993-2017) identified 22 studies yielding 24 effect sizes that met our inclusion criteria (8,075 patients). Inverse-variance weighting of correlation coefficients (r) was used to aggregate sample-level findings and study aims were addressed using random and mixed effect models. Sensitivity and publication bias analyses were conducted to assess the likelihood of bias in the overall estimate of AA-related benefit. AA exposure and abstinence for DD patients were significantly and positively associated (r w =.249; 95% CI.203-.293; Tau=.097). There was also significant heterogeneity in the distribution of effect sizes, (Q(23)=90.714, pAA-related benefit did not differ between 6 (k=7) and 12 (k=12) month follow-up, (Q=.068, pAA benefit was not adversely or substantively impacted by pooling RCT and observational samples (Q=.763, pAA (Q=.023, pAA) is common and, in many cases, DD patients who attend AA will report higher rates of alcohol abstinence relative to DD patients who do not attend AA. This article is protected by copyright. All rights reserved.

  14. Assessment of undiscovered oil and gas resources in the Uteland Butte Member of the Eocene Green River Formation, Uinta Basin, Utah

    Science.gov (United States)

    Johnson, Ronald C.; Birdwell, Justin E.; Mercier, Tracey J.; Brownfield, Michael E.; Charpentier, Ronald R.; Klett, Timothy R.; Leathers, Heidi M.; Schenk, Christopher J.; Tennyson, Marilyn E.

    2015-09-03

    Using a geology-based assessment methodology, the U.S. Geological Survey estimated mean undiscovered resources of 214 million barrels of oil, 329 billion cubic feet of associated/dissolved natural gas, and 14 million barrels of natural gas liquids in the informal Uteland Butte member of the Green River Formation, Uinta Basin, Utah.

  15. Antiangiogenic effects of AA-PMe on HUVECs in vitro and zebrafish in vivo.

    Science.gov (United States)

    Jing, Yue; Wang, Gang; Xiao, Qi; Zhou, Yachun; Wei, Yingjie; Gong, Zhunan

    2018-01-01

    Angiogenesis plays a vital role in many physiological and pathological processes and several diseases are connected with its dysregulation. Asiatic acid (AA) has demonstrated anticancer properties and we suspect this might be attributable to an effect on angio-genesis. A modified derivative of AA, N-(2α,3β,23-acetoxyurs-12-en-28-oyl)-L-proline methyl ester (AA-PMe), has improved efficacy over its parent compound, but its effect on blood vessel development remains unclear. In this study, we investigated the antiangiogenic activity of AA and AA-PMe in zebrafish embryos and human umbilical vein endothelial cells (HUVECs). First of all, we treated HUVECs with increasing concentrations of AA-PMe or AA, with or without vascular endothelial growth factor (VEGF) present, and assessed cell viability, tube formation, and cell migration and invasion. Quantitative real-time polymerase chain reaction and Western blot analysis were later used to determine the role of vascular endothelial growth factor receptor 2 (VEGFR2)-mediated signaling in AA-PMe inhibition of angiogenesis. We extended these studies to follow angiogenesis using Tg(fli:EGFP) transgenic zebrafish embryos. For these experiments, embryos were treated with varying concentrations of AA-PMe or AA from 24 to 72 hours postfertilization prior to morphological observation, angiogenesis assessment, and endogenous alkaline phosphatase assay. VEGFR2 expression in whole embryos following AA-PMe treatment was also determined. We found AA-PMe decreased cell viability and inhibited migration and tube formation in a dose-dependent manner in HUVECs. Similarly, AA-PMe disrupted the formation of intersegmental vessels, the dorsal aorta, and the posterior cardinal vein in zebrafish embryos. Both in vitro and in vivo AA-PMe surpassed AA in its ability to block angiogenesis by suppressing VEGF-induced phosphorylation of VEGFR2 and disrupting downstream extracellular regulated protein kinase and AKT signaling. For the first time

  16. My Most Memorable AAS Meeting-December 1957, Butler University, Indianapolis, Indiana

    Science.gov (United States)

    Edmondson, F. K.

    1999-05-01

    My attendance at AAS meetings began with the 46th meeting in September 1931 at the brand new Perkins Observatory. This was the first semester of my junior year at Indiana University. Professor Wilbur Cogshall, my astronomy professor, took me to the meeting, and paid my expenses for dormitory accommodations and meals. Hence, my attendance at AAS meetings covers a span of nearly 68 years. There have been so many "memorable" meetings that it is hard to pick just one. However, the 99th meeting in December 1957 at Butler University in Indianapolis, a joint meeting with the AAAS, is memorable because I was in a wheel chair and using crutches, following an injury to my right knee cap. I was a member of the AAAS Committee to select the "best paper" presented at the meeting to receive the Newcomb Cleveland Prize, and Martin Schwarzschild's first report of results from Project Stratoscope was on the program. I showed up at the Committee meeting in my wheel chair, and nominated Martin's paper for the "best paper" award. The Committee asked a lot of questions and then approved the paper by a unanimous vote. The wheel chair and crutches obviously played a role in convincing the Committee that I had strong feelings about the merits of Martin's paper. Allan Sandage was the Warner Prize Lecturer, and reported on the current status of his revision of the cosmic distance scale. Hubble's 1936 distances needed to be increased by a factor of five to ten.

  17. Controlled release of bioactive PDGF-AA from a hydrogel/nanoparticle composite.

    Science.gov (United States)

    Elliott Donaghue, Irja; Shoichet, Molly S

    2015-10-01

    Polymer excipients, such as low molar mass poly(ethylene glycol) (PEG), have shown contradictory effects on protein stability when co-encapsulated in polymeric nanoparticles. To gain further insight into these effects, platelet-derived growth factor (PDGF-AA) was encapsulated in polymeric nanoparticles with vs. without PEG. PDGF-AA is a particularly compelling protein, as it has been demonstrated to promote cell survival and induce the oligodendrocyte differentiation of neural stem/progenitor cells (NSPCs) both in vitro and in vivo. Here we show, for the first time, the controlled release of bioactive PDGF-AA from an injectable nanoparticle/hydrogel drug delivery system (DDS). PDGF-AA was encapsulated, with high efficiency, in poly(lactide-co-glycolide) nanoparticles, and its release from the drug delivery system was followed over 21 d. Interestingly, the co-encapsulation of low molecular weight poly(ethylene glycol) increased the PDGF-AA loading but, unexpectedly, accelerated the aggregation of PDGF-AA, resulting in reduced activity and detection by enzyme-linked immunosorbent assay (ELISA). In the absence of PEG, released PDGF-AA remained bioactive as demonstrated with NSPC oligodendrocyte differentiation, similar to positive controls, and significantly different from untreated controls. This work presents a novel delivery method for differentiation factors, such as PDGF-AA, and provides insights into the contradictory effects reported in the literature of excipients, such as PEG, on the loading and release of proteins from polymeric nanoparticles. Previously, the polymer poly(ethylene glycol) (PEG) has been used in many biomaterials applications, from surface coatings to the encapsulation of proteins. In this work, we demonstrate that, unexpectedly, low molecular weight PEG has a deleterious effect on the release of the encapsulated protein platelet-derived growth factor AA (PDGF-AA). We also demonstrate release of bioactive PDGF-AA (in the absence of PEG

  18. The structure of Ti-Ta welded joint and microhardness distribution over the cross section

    Science.gov (United States)

    Fomin, Aleksandr A.; Koshuro, Vladimir A.; Egorov, Ivan S.; Shelkunov, Andrey Yu.; Zakharevich, Andrey M.; Steinhauer, Natalia N.; Rodionov, Igor V.

    2018-04-01

    In order to create highly efficient medical systems and measuring biosensors, an approach is frequently used, in which the constructive basis of the product is made of a high-strength biocompatible material (titanium, stainless steel), and the functional layer is made of a more expensive metal (Ta, Zr, Au, Pt, etc.) or ceramics (Ta2O5, ZrO2, CaTiO3, etc.). For a strong connection, e.g. titanium with tantalum, it is proposed to use diffusion butt welding. The heat generated by passing electric current (I is not less than 1.95-2.05 kA, P - not less than 9 kW, t = 250-1000 ms) and applied pressure (30-50 MPa) ensure an integral connection. To improve the quality of the joint, i.e. to exclude cracks and tightness, it is necessary to choose the right combination of the thickness of the welded parts. It was established that when titanium (2 mm thick) and tantalum (0.1-0.5 mm) are combined, a better Ti-Ta welded joint is formed when tantalum foil is used (0.5 mm). Here the distribution of hardness over the cross section of the sample, including the welding areas, is uniform and has no extremely high residual stresses of the tensile type.

  19. Effect of Manganese on the Mechanical Properties of Welded As-Cast Aluminium Joint

    Directory of Open Access Journals (Sweden)

    Isiaka Oluwole OLADELE

    2013-11-01

    Full Text Available The effects of manganese on the mechanical properties of welded and un-weld as-cast 6063 aluminium alloy has been studied. Alloys of varying percentage of manganese from 0.019 to 0.24 were sand cast. A wooden pattern of dimensions 200×100×100mm was used, the aluminium (500g was charged into an induction furnace and heated to 750°C for 15 minutes, this was followed by the addition of weighed powdered manganese, stirred and heated at the same temperature for another 5 minutes and thereafter poured into the already prepared sand mould at a temperature of 690°C. The as-cast aluminium samples, were sectioned into two equal parts of 45mm each using power hack saw; a weld groove was created between the sides of the samples using an electric hand grinding machine, the groove served as the path along which the filler metal was deposited on the aluminium, a single v butt joint was produced from each sample and Metal Inert Gas Welding process was carried out to produce the required joint design. The different cast samples were machined to the different test pieces after which they were assessed to determine their mechanical properties (impact, hardness (welded joint and heat affected zone and tensile tests. The microstructures of the welded samples were also studied. From the results, it was observed that Sample F, which has 0.172% Mn, has the best hardness and impact strength while sample C with 0.160% Mn has the highest ultimate tensile strength.

  20. Nondestructive Evaluation of Friction Stir-Welded Aluminum Alloy to Coated Steel Sheet Lap Joint

    Science.gov (United States)

    Das, H.; Kumar, A.; Rajkumar, K. V.; Saravanan, T.; Jayakumar, T.; Pal, Tapan Kumar

    2015-11-01

    Dissimilar lap joints of aluminum sheet (AA 6061) of 2 mm thickness and zinc-coated steel sheet of 1 mm thickness were produced by friction stir welding with different combinations of rotational speed and travel speed. Ultrasonic C- and B-scanning, and radiography have been used in a complementary manner for detection of volumetric (cavity and flash) and planar (de bond) defects as the defects are in micron level. Advanced ultrasonic C-scanning did not provide any idea about the defects, whereas B-scanning cross-sectional image showed an exclusive overview of the micron-level defects. A digital x-ray radiography methodology is proposed for quality assessment of the dissimilar welds which provide three-fold increase in signal-to-noise ratio with improved defect detection sensitivity. The present study clearly shows that the weld tool rotational speed and travel speed have a decisive role on the quality of the joints obtained by the friction stir welding process. The suitability of the proposed NDE techniques to evaluate the joint integrity of dissimilar FSW joints is thus established.

  1. Creep properties of welded joints in OFHC copper for nuclear waste containment

    International Nuclear Information System (INIS)

    Ivarsson, B.; Oesterberg, J.O.

    1988-08-01

    In Sweden it has been suggested that copper canisters are used for containment of spent nuclear fuel. These canisters will be subjected to temperatures up to 100 degrees C and external pressures up to 15 MPa. Since the material is pure (OFHC) copper, creep properties must be considered when the canisters are dimensioned. The canisters are sealed by electron beam welding which will affect the creep properties. Literature data for copper - especially welded joints - at the temperatures of interest is very scare. Therefore uniaxial creep tests of parent metal, weld metal, and simulated HAZ structures have been performed at 110 degrees C. These tests revealed considerable differences in creep deformation and rupture strength. The weld metal showed creep rates and rupture times ten times higher and ten times shorter, respectively, than those of the parent metal. The simulated HAZ was equally strongen than the parent metal. These differences were to some extent verified by results from creep tests of cross-welded specimens which, however, showed even shorter rupture times. Constitutive equations were derived from the uniaxial test results. To check the applicability of these equations to multiaxial conditions, a few internal pressure creep tests of butt-welded tubes were performed. Attemps were made to simulate their creep behaviour by constitutive equations were used. These calculations failed due to too great differences in creep deformation behaviour across the welded joint. (authors)

  2. Magnetic horn of the Antiproton Accumulator (AA)

    CERN Multimedia

    Photographic Service

    1988-01-01

    In the 1960s, the invention of this "current sheet lens" has helped to greatly improve the flux of neutrino beams. It was used again at the AA, collecting antiprotons from the production target at angles too large to fit into the acceptance of the AA. It was machined from aluminium to a thickness of 1.4 mm and pulsed at 400 kA for 15 microseconds (half-sine).

  3. Inhibitory effect of propolis on the development of AA amyloidosis.

    Science.gov (United States)

    Harata, Daichi; Tsuchiya, Yuya; Miyoshi, Tomoyuki; Yanai, Tokuma; Suzuki, Kazuhiko; Murakami, Tomoaki

    2018-04-01

    In the several types of amyloidoses, participation of oxidative stresses in the pathogenesis and the effect of antioxidants on amyloidosis have been reported. Meanwhile, the relationship between oxidative stresses and pathogenesis of amyloid A (AA) amyloidosis is still unclear. In this study, we used an antioxidant, Brazilian propolis, to investigate the inhibitory effects on AA amyloidosis. The results showed that AA deposition was inhibited by administration of propolis. Increased expression of antioxidant markers was detected in molecular biological examinations of mice treated with propolis. Although serum amyloid A (SAA) levels were strongly correlated with the immunoreactive area of AA deposits in the control group, the correlation was weaker in the propolis-treated groups. In addition, there were no changes in SAA levels between the control group and the propolis-treated groups. The results indicate that propolis, an antioxidant, may induce inhibitory effects against AA amyloidosis.

  4. NCBI nr-aa BLAST: CBRC-XTRO-01-0674 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-XTRO-01-0674 ref|YP_001022362.1| putative heme O oxygenase (cytochrome aa3-controlling...) transmembrane protein [Methylibium petroleiphilum PM1] gb|ABM96127.1| putative heme O oxygenase (cytochrome aa3-controlling

  5. Effect of the weld thermal cycles by the modified indirect electric arc (MIEA) on the mechanical properties of the AA6061-T6 alloy; Efecto de los ciclo termicos de soldadura por arco electrico indirecto modificado (AEIM) en las propiedades mecanicas de la aleacion AA6061-T6

    Energy Technology Data Exchange (ETDEWEB)

    Ambriz, R. A.; Barrera, G.; Garcia, R.; Lopez, V. H.

    2009-07-01

    Results of temperature measurements during welding of 12.7 mm thick AA6061-T6 alloy plates by modified indirect electric arc (MIEA) are presented. This study describes the thermal cycles of the heat affected zone (HAZ) and also in the fusion zone. Depending upon the position of the transducers, the maximum temperatures measured in the HAZ range from 308 to 693 degree centigrade, these measurements were related with the tensile test results, and the failure zone reported previously by the authors. It was observed that, there is a decrease in the mechanical strength of the welded joints, due to the microstructural changes suffered by AA6061-T6 alloy in which formation of the {beta}occurs according to the TTT transformation diagram. The inherent cooling conditions of the weld pool observed for the MIEA technique (only one pass of welding), have permitted to establish the characteristics of solidification and microstructure for a specific cooling rate. (Author) 24 refs.

  6. Outcomes From AAS Hack Day at the 227th AAS Meeting

    Science.gov (United States)

    Kohler, Susanna

    2016-01-01

    Editors Note:This is a final post from the 227th AAS Meeting in Kissimmee, FL. This special summary of AAS Hack Day, a meeting of AAS members to collaboratively work on various small projects, was written by Meredith Rawls (@Merrdiff) and was originally posted on astrobites.com.As the 227thAmerican Astronomical Society meeting drew to a close (see highlights from Day 1, Day 2, Day 3, and Day 4), a group of at least 50 attendees spent Day 4working on small projects fondly called hacks. Thanks to sponsorship from LSST and Northrup Grumman, the industrious hackers werewell-caffeinated and fed so we could devote time and energy toworking in groups on one-day projects.TheHack Day beganat 10am with pitches. Anybody with a project idea was welcome to briefly speak and try to convince others to work with them. Only someideas panned out, but the enthusiasm was palpable. Its not every day you get a full room of astronomers and affiliates eager to spend hours working on fun and useful projects to benefit the community.#hackAAS is getting underway! #aas227 pic.twitter.com/yX7jlOnSCK James R A Davenport (@jradavenport) January 8, 2016Here is a rundown of what we accomplished. Pretty impressive for a single day! Many thanks to fellow astrobiter Erika Nesvold (now at Carnegie DTM; @erikanesvold) whose hack was live-documenting all the other hacks. Her tweets as @astrobites appeared with the #hackaas hashtag, and her notes made this recap post infinitely easier to write.Interested in joining the fun? Sign up for Hack Day at the 2017 JanuaryAAS meeting (its free with meeting registration), and consider applying for the .Astronomy conference this summer.Towards Optimal Session Scheduling:Adrian Price-Whelan (Columbia), David Hogg (NYU), and Scott Idem (AAS) began writing a program to take all submitted abstracts to a conference like AAS and sort them using keywords to avoid scheduling similar talks in parallel sessions. Its impossible to make everyone happy, but minimizing conflicts

  7. Corrosion issues of powder coated AA6060 aluminium profiles

    DEFF Research Database (Denmark)

    Din, Rameez Ud; Valgarðsson, Smári; Jellesen, Morten Stendahl

    2015-01-01

    In this study detailed microstructural investigation of the reason for unexpected corrosion of powder coated aluminium alloy AA6060 windows profiles has been performed. The results from this study reveals that the failure of the window profiles was originated from the surface defects present...... on the extruded AA6060 aluminium profile after metallurgical process prior to powder coating. Surface defects are produced due to intermetallic particles in the alloy, which disturb the flow during the extrusion process. The corrosion mechanism leading to the failure of the powder coated AA6060 aluminium profiles...

  8. Core–corona PSt/P(BA–AA) composite particles by two-stage emulsion polymerization

    Energy Technology Data Exchange (ETDEWEB)

    Xie, Delong; Ren, Xiaolin; Zhang, Xinya, E-mail: cexyzh@scut.edu.cn; Liao, Shijun [South China University of Technology, School of Chemistry and Chemical Engineering (China)

    2016-03-15

    Raspberry-shaped composite particles with polystyrene (PSt) as core and poly(n-butyl acrylate-co-acrylic acid) (P(BA–AA)) as corona were synthesized via emulsion polymerization. The random copolymer, P(BA–AA), was pre-prepared and used as a polymeric surfactant, its emulsifying properties adjusted by changing the mass ratio of BA and AA. The morphology of the resulting core–corona composite particles, P(St/P(BA–AA)), could be regulated and controlled by varying the concentrations of P(BA–AA) or the mass ratio of BA:AA in P(BA–AA). The experimental results indicate that 3.0–6.0 wt% of P(BA–AA) is required to obtain stable composite emulsions, and P(BA–AA) with a mass ratio of BA:AA = 1:2 is able to generate distinct core–corona structures. A mechanism of composite particle formation is proposed based on the high affinity between the PSt core and the hydrophobic segments of P(BA–A). The regular morphology of the colloidal film is expected to facilitate potential application of core–corona particles in the field of light scattering. Furthermore, the diversity of core–corona particles can be expanded by replacing P(BA–AA) corona particles with other amphiphilic particles.

  9. Microstructure, mechanical properties and texture of an AA6061/AA5754 composite fabricated by cross accumulative roll bonding

    Energy Technology Data Exchange (ETDEWEB)

    Verstraete, K., E-mail: kevin.verstraete@u-psud.fr [Université Paris-Sud, SP2M, ICMMO, UMR CNRS 8182, 91405 Orsay Cedex (France); Helbert, A.L. [Université Paris-Sud, SP2M, ICMMO, UMR CNRS 8182, 91405 Orsay Cedex (France); Brisset, F. [Université Paris-Sud, ICMMO, UMR CNRS 8182, 91405 Orsay Cedex (France); Benoit, A.; Paillard, P. [Institut des Matériaux Jean Rouxel (IMN), UMR 6502, Polytech’Nantes, Nantes Cedex (France); Baudin, T. [Université Paris-Sud, SP2M, ICMMO, UMR CNRS 8182, 91405 Orsay Cedex (France)

    2015-07-29

    AA6061 alloy is a widely used material in the automotive and aerospace industries, but is prone to hot cracking, which limits its weldability. To prevent this phenomenon, the AA6061/AA5754 composite was formed using a severe plastic deformation technique, Cross Accumulative Roll Bonding (CARB), at an elevated temperature (350 °C) to ensure good bonding between layers. This technique was efficient to maintain a small grain size, even under the process temperature conditions, and consequently, preserve good mechanical properties. The composite had better mechanical properties than the initial aluminium alloys. Microstructure and texture remained stable after two cycles and yield stress tended towards an equal value in the rolling and the transverse directions. After two cycles, the main component was the {001}〈110〉 rotated Cube, which was maintained for up to 10 cycles. Diffusion was more effective as the strain increased. Finally, a tungsten inert gas (TIG) welding process was performed on the composite and confirmed resistance to hot cracking.

  10. Practicing for 2023 and 2024: What the AAS Solar Eclipse Task Force Learned from the "Great American Eclipse" of 2017

    Science.gov (United States)

    Fienberg, R. T.; Speck, A. K.; Habbal, S. R.

    2017-12-01

    More than three years ahead of the "Great American Eclipse" of August 2017, the American Astronomical Society formed the AAS Solar Eclipse Task Force to function as a think tank, coordinating body, and communication gateway to the vast resources available about the 2017 eclipse and solar eclipses more generally. The task force included professional and amateur astronomers, formal and informal educators, and science journalists; many had experienced total solar eclipses before, and others would experience their first totality in August 2017. The AAS task force secured funding from the AAS Council, the National Science Foundation, and NASA. These resources were used mainly for three purposes: (1) to build a website that contains basic information about solar eclipses, safe viewing practices, and eclipse imaging and video, along with resources for educators and the media and a searchable map of eclipse-related events and activities, with links to other authoritative websites with more detailed information; (2) to solicit, receive, evaluate, and fund proposals for mini-grants to support eclipse-related education and public outreach to underrepresented groups both inside and outside the path of totality; and (3) to organize a series of multidisciplinary workshops across the country to prepare communities for the eclipse and to facilitate collaborations between astronomers, meteorologists, school administrators, and transporation and emergency-management professionals. Most importantly, the AAS Solar Eclipse Task Force focused on developing and disseminating appropriate eclipse safety information. The AAS and NASA jointly developed safety messaging that won the endorsement of the American Academies of Opthalmology and Optometry. In the weeks immediately preceding the eclipse, it became clear that the marketplace was being flooded by counterfeit eclipse glasses and solar viewers, leading to a last minute change in our communication strategy. In this talk, we'll review the

  11. Radiographic and ultrasonic testings of welded joints of 6063 aluminium alloy

    International Nuclear Information System (INIS)

    Oliveira e Silva Mury, A.G. de.

    1980-05-01

    A study on evaluation of weld defects in aluminium butt joints was made in a comparative way through the radiographic and ultrasonic testing. This work was conducted with pipes 5 IPS (6,35 mm thickness) of 6063 aluminium alloy, circumferential TIG welded, due to the difficulty on performing non-destructive testing with this schedule. It was concluded thta ultrasonic testing has adequate sensitivity when setting gain adjustment is made with aid of a reference curve constructed by using a Reference Block (among others studied) with 1,5 mm dia. Hole as reference reflector, and a 5 MHz angle beam search-unit. In this case the ultrasonic testing is more accurate than radiographic testing to detect planar defects like lack of fusion and lack of penetration. Defect sizing by ultrasonic methods employed were 6 and 20 dB drop methods. In spite of your observed limitations concerning the establishment of the real size of defects, the procedure applied was precise for locate and define the weld defects that where found in this study. (author) [pt

  12. Antiangiogenic effects of AA-PMe on HUVECs in vitro and zebrafish in vivo

    Directory of Open Access Journals (Sweden)

    Jing Y

    2018-04-01

    Full Text Available Yue Jing,1,2,* Gang Wang,1,* Qi Xiao,1 Yachun Zhou,1 Yingjie Wei,3 Zhunan Gong1 1Center for New Drug Research and Development, College of Life Science, Nanjing Normal University, Nanjing, China; 2Central Laboratory of Stomatology, Nanjing Stomatological Hospital, Medical School of Nanjing University, Nanjing, China; 3Key Laboratory of Oral Drug Delivery System of Chinese Materia Medica of State Administration of Traditional Chinese Medicine, Jiangsu Branch of China Academy of Chinese Medical Science, Nanjing, China *These authors contributed equally to this work Abstract: Angiogenesis plays a vital role in many physiological and pathological processes and several diseases are connected with its dysregulation. Asiatic acid (AA has demonstrated anticancer properties and we suspect this might be attributable to an effect on angiogenesis. A modified derivative of AA, N-(2α,3β,23-acetoxyurs-12-en-28-oyl-L-proline methyl ester (AA-PMe, has improved efficacy over its parent compound, but its effect on blood vessel development remains unclear. Methods: In this study, we investigated the antiangiogenic activity of AA and AA-PMe in zebrafish embryos and human umbilical vein endothelial cells (HUVECs. First of all, we treated HUVECs with increasing concentrations of AA-PMe or AA, with or without vascular endothelial growth factor (VEGF present, and assessed cell viability, tube formation, and cell migration and invasion. Quantitative real-time polymerase chain reaction and Western blot analysis were later used to determine the role of vascular endothelial growth factor receptor 2 (VEGFR2-mediated signaling in AA-PMe inhibition of angiogenesis. We extended these studies to follow angiogenesis using Tg(fli:EGFP transgenic zebrafish embryos. For these experiments, embryos were treated with varying concentrations of AA-PMe or AA from 24 to 72 hours postfertilization prior to morphological observation, angiogenesis assessment, and endogenous alkaline

  13. Role and mechanism of AT1-AA in the pathogenesis of HELLP syndrome.

    Science.gov (United States)

    Bu, Shurui; Wang, Yuxian; Sun, Shuqing; Zheng, Yanqian; Jin, Zhu; Zhi, Jianming

    2018-01-10

    HELLP syndrome remains a leading cause of maternal and neonatal mortality and morbidity worldwide, which symptoms include hemolysis, elevated liver enzymes and low platelet count. The objective of this study was to determine whether HELLP is associated with AT1-AA. The positive rate and titer of AT1-AA in plasma from pregnant women were determined, and the correlation of AT1-AA titer with the grade of HELLP was analyzed. A HELLP rat model established by intravenous injection of AT1-AA. Our experimental results show the AT1-AA titer and positive rate were significantly higher in HELLP group, and AT1-AA titer were positively correlated with the level of TNF-α and ET-1 in plasma and the grade of HELLP syndrome. The results of animal experiments showed that the typical features of HELLP in the pregnant rats after AT1-AA injection. The levels of TNF-α and ET-1 in plasma and liver tissue were significantly increased in AT1-AA-treated rats compared with control rats. The HELLP syndrome induced by AT1-AA was attenuated markedly after administration of losartan. These data support the hypothesis that one the potential pathway that AT1-AA induce damage to capillary endothelial cells and liver during pregnancy is through activation of TNF-α and ET-1.

  14. Stress Corrosion Cracking Behavior of Multipass TIG-Welded AA2219 Aluminum Alloy in 3.5 wt pct NaCl Solution

    Science.gov (United States)

    Venugopal, A.; Sreekumar, K.; Raja, V. S.

    2012-09-01

    The stress corrosion cracking (SCC) behavior of the AA2219 aluminum alloy in the single-pass (SP) and multipass (MP) welded conditions was examined and compared with that of the base metal (BM) in 3.5 wt pct NaCl solution using a slow-strain-rate technique (SSRT). The reduction in ductility was used as a parameter to evaluate the SCC susceptibility of both the BM and welded joints. The results showed that the ductility ratio ( ɛ NaCl/( ɛ air) was 0.97 and 0.96, respectively, for the BM and MP welded joint, and the same was marginally reduced to 0.9 for the SP welded joint. The fractographic examination of the failed samples revealed a typical ductile cracking morphology for all the base and welded joints, indicating the good environmental cracking resistance of this alloy under all welded conditions. To understand the decrease in the ductility of the SP welded joint, preexposure SSRT followed by microstructural observations were made, which showed that the decrease in ductility ratio of the SP welded joint was caused by the electrochemical pitting that assisted the nucleation of cracks in the form of corrosion induced mechanical cracking rather than true SCC failure of the alloy. The microstructural examination and polarization tests demonstrated a clear grain boundary (GB) sensitization of the PMZ, resulting in severe galvanic corrosion of the SP weld joint, which initiated the necessary conditions for the localized corrosion and cracking along the PMZ. The absence of PMZ and a refined fusion zone (FZ) structure because of the lesser heat input and postweld heating effect improved the galvanic corrosion resistance of the MP welded joint greatly, and thus, failure occurred along the FZ.

  15. Fecal transmission of AA amyloidosis in the cheetah contributes to high incidence of disease

    Science.gov (United States)

    Zhang, Beiru; Une, Yumi; Fu, Xiaoying; Yan, Jingmin; Ge, FengXia; Yao, Junjie; Sawashita, Jinko; Mori, Masayuki; Tomozawa, Hiroshi; Kametani, Fuyuki; Higuchi, Keiichi

    2008-01-01

    AA amyloidosis is one of the principal causes of morbidity and mortality in captive cheetahs (Acinonyx jubatus), which are in danger of extinction, but little is known about the underlying mechanisms. Given the transmissible characteristics of AA amyloidosis, transmission between captive cheetahs may be a possible mechanism involved in the high incidence of AA amyloidosis. In this study of animals with AA amyloidosis, we found that cheetah feces contained AA amyloid fibrils that were different from those of the liver with regard to molecular weight and shape and had greater transmissibility. The infectious activity of fecal AA amyloid fibrils was reduced or abolished by the protein denaturants 6 M guanidine·HCl and formic acid or by AA immunodepletion. Thus, we propose that feces are a vehicle of transmission that may accelerate AA amyloidosis in captive cheetah populations. These results provide a pathogenesis for AA amyloidosis and suggest possible measures for rescuing cheetahs from extinction. PMID:18474855

  16. Wired for success: A history of the Butte, Anaconda & Pacific Railway, 1892--1985

    Science.gov (United States)

    Mutschler, Charles Vincent

    The Butte, Anaconda & Pacific Railway (BA&P) was a standard gauge common carrier short line railroad within the state of Montana. A subsidiary of the Anaconda Copper Mining Company, the BA&P was built to carry ore from mines at Butte, Montana to Anaconda, twenty-six miles away, for concentrating and smelting. Other freight and passenger business was of secondary importance. In 1912, when General Electric contracted to convert the BA&P from steam to electric operation, the short line became a proving ground for main line railroad electrification, and the center of attention from advocates for electric power. Electric operation was demonstrated to be mechanically superior to the use of steam locomotives on the BA&P. Immediately after the BA&P proved the technological feasibility of high voltage direct current for moving heavy freight trains, the Chicago Milwaukee & St. Paul (CM&St.P) electrified over 600 miles of transcontinental main line using the basic technology demonstrated on the BA&P. However, on long distances of track with relatively few trains such as the CM&St.P, the capital cost of the electric distribution system exceeded the operational savings obtained by use of electric locomotives. Steam locomotives remained the primary form of railroad motive power in the United States until the 1950's, when the diesel-electric locomotive combined the mechanical efficiency of electric motors with an on-board diesel generating plant, eliminating the need for expensive electric power supply and distribution wires of conventional electrics. The BA&P purchased three diesels in the early 1950's, but relied primarily on its electric locomotives until 1967, when diesel operation became less costly than continued use of electric motive power. The BA&P offers a microcosmic view of the transformation of one industry in response to technological and economic forces as the United States moved from reliance on coal-burning steam power to electric power and internal combustion

  17. Large magnetoresistance in (AA')2FeReO6 double perovskites

    International Nuclear Information System (INIS)

    Teresa, J.M. de; Serrate, D.; Blasco, J.; Ibarra, M.R.; Morellon, L.

    2005-01-01

    We review the main structural, magnetic and magnetotransport properties of the intriguing (AA') 2 FeReO 6 magnetic double perovskites. As the average cation size decreases, the crystallographic structure at room temperature evolves from cubic [(AA') 2 =Ba 2 , Ba 1.5 Sr 0.5 , BaSr, Ba 0.5 Sr 1.5 ] to tetragonal [(AA') 2 =Sr 2 ] and monoclinic [(AA') 2 =Ca 0.5 Sr 1.5 , CaSr, Ca 1.5 Sr 0.5 , Ca 2 ]. The Curie temperature increases anomalously from ∼303K for Ba 2 to ∼522K for Ca 2 in sharp contrast with the observed behaviour in the isostructural compounds (AA') 2 FeMoO 6 . Other anomalous features in the (AA') 2 FeReO 6 series are: the large magnetic anisotropy, the large magnetoelastic coupling and the semiconducting behaviour of the monoclinic compounds. The monoclinic compounds undergo a structural/magnetic transition at T S below 125K. Three different magnetoresistance mechanisms have been identified: the intergrain negative magnetoresistance effect, which is present across the whole series of compounds, and in the case of the monoclinic compounds below T S a negative magnetoresistance effect associated to the melting of the low-temperature phase and a positive magnetoresistance effect only present in (AA') 2 =Ca 2 below T∼50K

  18. The Drentsche Aa valley system

    International Nuclear Information System (INIS)

    Gans, W. de.

    1981-01-01

    This thesis is composed of five papers concerned with Late Quaternary geology and geomorphology of the Aa valley system. The correlation and chronostratigraphic position of the layers have been established by radiocarbon dating. (Auth.)

  19. An Evaluation of Global and Local Tensile Properties of Friction-Stir Welded DP980 Dual-Phase Steel Joints Using a Digital Image Correlation Method.

    Science.gov (United States)

    Lee, Hyoungwook; Kim, Cheolhee; Song, Jung Han

    2015-12-04

    The effect of the microstructure heterogeneity on the tensile plastic deformation characteristic of friction-stir-welded (FSW) dual-phase (DP) steel was investigated for the potential applications on the lightweight design of vehicles. Friction-stir-welded specimens with a butt joint configuration were prepared, and quasi-static tensile tests were conducted, to evaluate the tensile properties of DP980 dual-phase steels. The friction-stir welding led to the formation of martensite and a significant hardness rise in the stir zone (SZ), but the presence of a soft zone in the heat-affected zone (HAZ) was caused by tempering of the pre-existing martensite. Owing to the appearance of severe soft zone, DP980 FSW joint showed almost 93% joint efficiency with the view-point of ultimate tensile strength and relatively low ductility than the base metal (BM). The local tensile deformation characteristic of the FSW joints was also examined using the digital image correlation (DIC) methodology by mapping the global and local strain distribution, and was subsequently analyzed by mechanics calculation. It is found that the tensile deformation of the FSW joints is highly heterogeneous, leading to a significant decrease in global ductility. The HAZ of the joints is the weakest region where the strain localizes early, and this localization extends until fracture with a strain near 30%, while the strain in the SZ and BM is only 1% and 4%, respectively. Local constitutive properties in different heterogeneous regions through the friction-stir-welded joint was also briefly evaluated by assuming iso-stress conditions. The local stress-strain curves of individual weld zones provide a clear indication of the heterogeneity of the local mechanical properties.

  20. AaERF1 positively regulates the resistance to Botrytis cinerea in Artemisia annua.

    Directory of Open Access Journals (Sweden)

    Xu Lu

    Full Text Available Plants are sessile organisms, and they can not move away under abiotic or biotic stresses. Thus plants have evolved a set of genes that response to adverse environment to modulate gene expression. In this study, we characterized and functionally studied an ERF transcription factor from Artemisia annua, AaERF1, which plays an important role in biotic stress responses. The AaERF1 promoter had been cloned and GUS staining results of AaERF1 promoter-GUS transgenic A. annua showed that AaERF1 is expressed ubiquitiously in all organs. Several putative cis-acting elements such as W-box, TGA-box and Py-rich element, which are involved in defense responsiveness, are present in the promoter. The expression of AaERF1 can be induced vigorously by methyl jasmonate as well as by ethephon and wounding, implying that AaERF1 may activate some of the defense genes via the jasmonic acid and ethylene signaling pathways of A. annua. The results of electrophoretic mobility shift assay (EMSA and yeast one-hybrid experiments showed that AaERF1 was able to bind to the GCC box cis-acting element in vitro and in yeast. Ectopic expression of AaERF1 could enhance the expression levels of the defense marker genes PLANT DEFENSIN1.2 (PDF1.2 and BASIC CHITINASE (ChiB, and increase the resistance to Botrytis cinerea in the 35S::AaERF1 transgenic Arabidopsis. The down-regulated expression level of AaERF1 evidently reduced the resistance to B. cinerea in A. annua. The overall results showed that AaERF1 positively regulated the resistance to B. cinerea in A. annua.

  1. AA amyloidosis complicating the hereditary periodic fever syndromes.

    Science.gov (United States)

    Lane, Thirusha; Loeffler, Jutta M; Rowczenio, Dorota M; Gilbertson, Janet A; Bybee, Alison; Russell, Tonia L; Gillmore, Julian D; Wechalekar, Ashutosh D; Hawkins, Philip N; Lachmann, Helen J

    2013-04-01

    AA amyloidosis is a life-threatening complication of the hereditary periodic fever syndromes (HPFS), which are otherwise often compatible with normal life expectancy. This study was undertaken to determine the characteristics, presentation, natural history, and response to treatment in 46 patients who had been referred for evaluation at the UK National Amyloidosis Centre. Disease activity was monitored by serial measurement of serum amyloid A. Renal function was assessed by measurement of serum creatinine and albumin levels, the estimated glomerular filtration rate, and proteinuria from 24-hour urine collections. The amyloid load was measured by serum amyloid P scintigraphy. Twenty-four patients had familial Mediterranean fever, 12 patients had tumor necrosis factor receptor-associated periodic syndrome, 6 patients had cryopyrin-associated periodic syndromes, and 4 patients had mevalonate kinase deficiency. The median age at onset of HPFS was 5 years; median age at presentation with AA amyloidosis was 38 years. Diagnosis of an HPFS had not been considered prior to presentation with AA amyloidosis in 23 patients (50%). Eleven patients (24%) had end-stage renal failure (ESRF) at presentation; of these, 3 had received transplants prior to referral. A further 13 patients developed ESRF over the followup period, with 10 undergoing renal transplantation. The median time to progression to ESRF from onset of AA amyloidosis was 3.3 years (interquartile range [IQR] 2-8), with a median time to transplant of 4 years (IQR 3-6). Eleven patients (24%) died. The median survival in the entire cohort was 19 years from diagnosis of AA amyloidosis. Of the 37 patients who were treated successfully, or in whom at least partial suppression of the underlying HPFS was achieved, 17 (46%) showed amyloid regression, 14 (38%) showed a stable amyloid load, and 2 (5%) showed increased amyloid deposition over the followup period. AA amyloidosis remains a challenging and serious late complication

  2. Failure analysis of fusion clad alloy system AA3003/AA6xxx sheet under bending

    Energy Technology Data Exchange (ETDEWEB)

    Shi, Y., E-mail: shiyh@mcmaster.ca [Department of Mechanical Engineering, McMaster University, 1280 Main Street West, Hamilton, Ontario, Canada L8S 4L7 (Canada); Jin, H. [Novelis Global Technology Center, P.O. Box 8400, Kingston, Ontario, Canada K7L 5L9 (Canada); Wu, P.D. [Department of Mechanical Engineering, McMaster University, 1280 Main Street West, Hamilton, Ontario, Canada L8S 4L7 (Canada); Lloyd, D.J. [Aluminum Materials Consultants, 106 Nicholsons Point Road, Bath, Ontario, Canada K0H 1G0 (Canada); Embury, D. [Department of Mechanical Engineering, McMaster University, 1280 Main Street West, Hamilton, Ontario, Canada L8S 4L7 (Canada)

    2014-07-29

    An ingot of AA6xxx Al–Si–Mg–Cu alloy clad with AA3003 Al–Mn alloy was co-cast by Fusion technology. Bending tests and numerical modeling were performed to investigate the potential for sub-surface cracking for this laminate system. To simulate particle-induced crack initiation and growth, both random and stringer particles have been selected to mimic the particle distribution in the tested samples. The morphology of cracking in the model was similar to that observed in clad sheet tested in the Cantilever bend test. The crack initiated in the core close to the clad-core interface where the strain in the core is highest, between particles or near particles and propagates along local shear bands in the core, while the clad layer experiences extreme thinning before failure.

  3. An Analysis of the Rise and Fall of the AA-MAS Policy

    Science.gov (United States)

    Lazarus, Sheryl S.; Thurlow, Martha L.; Ysseldyke, James E.; Edwards, Lynn M.

    2015-01-01

    In 2005, to address concerns about students who might fall in the "gap" between the regular assessment and the alternate assessment based on alternate achievement standards (AA-AAS), the U.S. Department of Education announced that states could develop alternate assessments based on modified achievement standards (AA-MAS). This article…

  4. Effect of the weld thermal cycles by the modified indirect electric arc (MIEA) on the mechanical properties of the AA6061-T6 alloy

    International Nuclear Information System (INIS)

    Ambriz, R. A.; Barrera, G.; Garcia, R.; Lopez, V. H.

    2009-01-01

    Results of temperature measurements during welding of 12.7 mm thick AA6061-T6 alloy plates by modified indirect electric arc (MIEA) are presented. This study describes the thermal cycles of the heat affected zone (HAZ) and also in the fusion zone. Depending upon the position of the transducers, the maximum temperatures measured in the HAZ range from 308 to 693 degree centigrade, these measurements were related with the tensile test results, and the failure zone reported previously by the authors. It was observed that, there is a decrease in the mechanical strength of the welded joints, due to the microstructural changes suffered by AA6061-T6 alloy in which formation of the βoccurs according to the TTT transformation diagram. The inherent cooling conditions of the weld pool observed for the MIEA technique (only one pass of welding), have permitted to establish the characteristics of solidification and microstructure for a specific cooling rate. (Author) 24 refs

  5. Tobacco industry responsibility for butts: a Model Tobacco Waste Act.

    Science.gov (United States)

    Curtis, Clifton; Novotny, Thomas E; Lee, Kelley; Freiberg, Mike; McLaughlin, Ian

    2017-01-01

    Cigarette butts and other postconsumer products from tobacco use are the most common waste elements picked up worldwide each year during environmental cleanups. Under the environmental principle of Extended Producer Responsibility, tobacco product manufacturers may be held responsible for collection, transport, processing and safe disposal of tobacco product waste (TPW). Legislation has been applied to other toxic and hazardous postconsumer waste products such as paints, pesticide containers and unused pharmaceuticals, to reduce, prevent and mitigate their environmental impacts. Additional product stewardship (PS) requirements may be necessary for other stakeholders and beneficiaries of tobacco product sales and use, especially suppliers, retailers and consumers, in order to ensure effective TPW reduction. This report describes how a Model Tobacco Waste Act may be adopted by national and subnational jurisdictions to address the environmental impacts of TPW. Such a law will also reduce tobacco use and its health consequences by raising attention to the environmental hazards of TPW, increasing the price of tobacco products, and reducing the number of tobacco product retailers. Published by the BMJ Publishing Group Limited. For permission to use (where not already granted under a licence) please go to http://www.bmj.com/company/products-services/rights-and-licensing/.

  6. INAA and flame AAS of various vegetable reference materials

    International Nuclear Information System (INIS)

    Djingova, R.; Arpadjan, S.; Kuleff, I.

    1991-01-01

    INAA and flame AAS have been used for the analysis of a large number of vegetable reference materials. Out of all determined elements (28 by INAA and 11 by AAS) nine are common for both methods (Ca, Cd, Co, Cu, Fe, Mg, Mn, Na, Zn) and for these the possibilities of the two methods have been compared. (orig.)

  7. PDGF-AA-induced filamentous mitochondria benefit dermal papilla cells in cellular migration.

    Science.gov (United States)

    Mifude, C; Kaseda, K

    2015-06-01

    Human dermal papilla cells (HDPCs) play essential roles in hair follicular morphogenesis and postnatal hair growth cycles. Previous reports demonstrated that platelet-derived growth factor-AA (PDGF-AA) enhanced the formation of dermal condensates in hair follicular development. Additionally, PDGF-AA induces/maintains the anagen phase of the hair cycle. It is likely that mitochondrial morphology and functions are tightly coupled with maintenance of these energy-demanding activities. However, little is known about the mitochondrial regulation in HDPCs. Thus, we investigated the PDGF-involved mitochondrial regulation in HDPCs. The mitochondrial morphologies of HDPCs were examined in the presence or absence of PDGF-AA under a fluorescent microscope. ATP production and cellular motility were investigated. The relationship between mitochondrial morphology and the cellular functions was discussed. We observed that primary HDPCs contained mitochondria with filamentous and/or rounded morphologies. Both types of mitochondria showed similar membrane potentials. Interestingly, in the presence of PDGF-AA, but not PDGF-BB, the balance between the two morphologies shifted towards the filamentous form. Concomitantly, both mitochondrial enzymatic activity and total cellular ATP level were augmented by PDGF-AA. These two parameters were closely correlated, suggesting the mitochondrial involvement in the PDGF-augmented ATP production. Moreover, PDGF-AA accelerated the migration of HDPCs in a gap-filling assay, but did not change the rate of cellular proliferation. Notably, filamentous mitochondria dominated migrating HDPCs. PDGF-AA benefits HDPCs in the process of migration, by increasing the number of filamentous mitochondria. © 2014 Society of Cosmetic Scientists and the Société Française de Cosmétologie.

  8.  Ischemic Stroke Secondary to Aortic Dissection Following Rifle Butt Recoil Chest Injury: A Case Report

    Directory of Open Access Journals (Sweden)

    John Valiath

    2011-11-01

    Full Text Available  Ischemic stroke secondary to aortic dissection is not uncommon. We present a patient with left hemiplegia secondary to Stanford type A aortic dissection extending to the supra-aortic vessels, which was precipitated by rifle butt recoil chest injury. The diagnosis of aortic dissection was delayed due to various factors. Finally, the patient underwent successful Bentall procedure with complete resolution of symptoms. This case emphasizes the need for caution in the use of firearms for recreation and to take precautions in preventing such incidents. In addition, this case illustrates the need for prompt cardiovascular physical examination in patients presenting with stroke.

  9. [A review for recent advances in AA amyloid research and therapeutic approach to AA amyloidosis complicating rheumatoid arthritis].

    Science.gov (United States)

    Tamura, Hiroaki; Hasegawa, Kiminori

    2009-02-01

    AA amyloidosis is a life threatening clinical complication of chronic inflammatory diseases such as rheumatoid arthritis. It has been demonstrated biochemically that amyloidosis resulted from abnormal folding of proteins, which are deposited as insoluble fibrils in extracellular tissue, leading to the disruption of their normal function. In this regard, amyloidosis has been recognized as a conformation disorder. Interestingly, genetic polymorphisms of amyloid precursor protein (SAA) have been reported to associate with increased risk for AA amyloidosis. Also recent biochemical research revealed that SAA is synthesized under the influence of the proinflammatory cytokines, such as IL-6, TNF-alpha, IL-1. Additionally, it was suggested that amyloid deposits in extracellular tissue could reflect to the serum level of SAA in the reversible fashion, leading to the hypothesis that the control of the SAA synthesis could be beneficial to the treatment of amyloidosis. In this context, anti-cytokine therapies may be most effective. Especially the inhibition of IL-6 is critical to suppression of SAA production, so treatment with a humanized monoclonal antibody against human IL-6 receptor may not only ameliorate RA disease activity but also pave the way for the treatment of AA amyloidosis.

  10. Influence of tool pin profile on microstructure and corrosion behaviour of AA2219 Al–Cu alloy friction stir weld nuggets

    Directory of Open Access Journals (Sweden)

    Ch. Venkata Rao

    2015-09-01

    Full Text Available To overcome the problems of fusion welding of aluminium alloys, the friction stir welding (FSW is recognized as an alternative joining method to improve the mechanical and corrosion properties. Tool profile is one of the important variables which affect the performance of the FS weld. In the present work, the effect of tool profile on the weld nugget microstructure and pitting corrosion of AA2219 aluminium–copper alloy was studied. FSW of AA2219 alloy was carried out using five profiles, namely conical, square, triangle, pentagon and hexagon. The temperature measurements were made in the region adjacent to the rotating pin. It was observed that the peak temperature is more in hexagonal tool pin compared to the welds produced with other tool pin profiles. It is observed that the extensive deformation experienced at the nugget zone and the evolved microstructure strongly influences the hardness and corrosion properties of the joint during FSW. It was found that the microstructure changes like grain size, misorientation and precipitate dissolution during FSW influence the hardness and corrosion behaviour. Pitting corrosion resistance of friction stir welds of AA2219 was found to be better for hexagon profile tool compared to other profiles, which was attributed to material flow and strengthening precipitate morphology in nugget zone. Higher amount of heat generation in FS welds made with hexagonal profile tool may be the reason for greater dissolution of strengthening precipitates in nugget zone.

  11. Busted Butte Phase 2: Introduction and Analytical Modeling of Nonreactive Tracer and Lithium Breakthrough

    International Nuclear Information System (INIS)

    Turin, H.J.; Soll, W.E.

    2002-01-01

    The Busted Butte Unsaturated-Zone Transport Test Facility is located approximately 8 km southeast of Yucca Mountain, and was designed to address uncertainties associated with flow and transport in the UZ site-process models for Yucca Mountain. Busted Butte Phase 2 consisted of a 10m x 10m x 7m test block. From July 1988 through October 2000, complex tracer mixtures were injected continuously at 77 discrete points located along eight parallel 10-m boreholes arranged in two horizontal planes. In August 1999, iodide was added to the tracer mixture to explore the effects of initial hydraulic transients. During the course of the experiment, porewater samples were collected at regular intervals using sorbing-paper collection pads, emplaced into fifteen horizontal and inclined 10-m collection boreholes, oriented perpendicular to the injection boreholes. Potential travel distances ranged from 20 cm to over 500 cm. Nonreactive tracer and weakly sorbing lithium breakthrough was observed at most of the collection points during the injection period. Following termination of injection, approximately 800 rock samples were collected using overcore and mineback techniques, and analyzed for tracer concentration. Rock analyses are discussed in a subsequent paper. To complement complex 3-dimensional finite-element modeling of the entire block, bromide, iodide, and lithium breakthrough onto the collection pads has been modeled with CXTFIT. This simple 1-dimensional analytical code uses a non-linear curve-fitting routine to estimate transport parameters including apparent velocity, dispersivity, and field retardation factors. Preliminary results show that: (1) Bromide and iodide behaved similarly, despite the fact that bromide was injected in a strongly transient flow field, while iodide injection began after flow had approached steady state conditions. (2) With the exception of the closest collection points, tracer velocities remained relatively constant, indicating that transport was

  12. Yield and flow properties of aluminum alloy AA 8001

    International Nuclear Information System (INIS)

    Lyons, J.S.; Johnson, H.W.; Han, E.G.

    1995-01-01

    Aluminum alloy AA 8001 is being used at the Westinghouse Savannah River Company (WSRC) for nuclear reactor fuel and target components. The objective of this research was to determine parameters for predictive models of the compressive flow properties of AA 8001. Seventy-five true strain-rate, hot compression tests were performed. New, quantitative information about the yield and flow behavior of aluminum alloy AA 8001 was determined. Parameters were determined to use in a hyperbolic sine constitutive law so that the yield stress, the peak stress, and the peak strain can be predicted from the temperature-compensated strain-rate, Z. It was found that the onset of strain softening was more strongly dependent on Z than the onset of yielding was

  13. Absorption spectra of AA-stacked graphite

    International Nuclear Information System (INIS)

    Chiu, C W; Lee, S H; Chen, S C; Lin, M F; Shyu, F L

    2010-01-01

    AA-stacked graphite shows strong anisotropy in geometric structures and velocity matrix elements. However, the absorption spectra are isotropic for the polarization vector on the graphene plane. The spectra exhibit one prominent plateau at middle energy and one shoulder structure at lower energy. These structures directly reflect the unique geometric and band structures and provide sufficient information for experimental fitting of the intralayer and interlayer atomic interactions. On the other hand, monolayer graphene shows a sharp absorption peak but no shoulder structure; AA-stacked bilayer graphene has two absorption peaks at middle energy and abruptly vanishes at lower energy. Furthermore, the isotropic features are expected to exist in other graphene-related systems. The calculated results and the predicted atomic interactions could be verified by optical measurements.

  14. Fatique Resistant, Energy Efficient Welding Program, Final Technical Report

    Energy Technology Data Exchange (ETDEWEB)

    Egland, Keith; Ludewig, Howard

    2006-05-25

    The program scope was to affect the heat input and the resultant weld bead geometry by synchronizing robotic weave cycles with desired pulsed waveform shapes to develop process parameters relationships and optimized pulsed gas metal arc welding processes for welding fatique-critical structures of steel, high strength steel, and aluminum. Quality would be addressed by developing intelligent methods of weld measurement that accurately predict weld bead geometry from process information. This program was severely underfunded, and eventually terminated. The scope was redirected to investigate tandem narrow groove welding of steel butt joints during the one year of partial funding. A torch was designed and configured to perform a design of experiments of steel butt weld joints that validated the feasability of the process. An initial cost model estimated a 60% cost savings over conventional groove welding by eliminating the joint preparation and reducing the weld volume needed.

  15. Association between AA-NAT gene polymorphism and reproductive performance in sheep

    OpenAIRE

    Ding-ping,Bai; Cheng-jiang,Yu; Yu-lin,Chen

    2012-01-01

    Arylalkylamine N-acetyltransferase (AA-NAT) is critical enzyme in Melatonin (MLT) biosynthesis for MLT regulating the animal seasonal breeding. In this study, DNA sequencing methods were applied to detect the polymorphisms of the AA-NAT gene in 179 Chinese sheep belonging to two non-seasonal reproduction breeds and two seasonal reproduction breeds. One mutation at exon 3 (NM_001009461:c.486A > G) was firstly described at the sheep AA-NAT locus. Hence, we described the SmaI PCR-RFLP m...

  16. TRANSIENT FINITE ELEMENT SIMULATION AND MICROSTRUCTURE EVOLUTION OF AA2219 WELD JOINT USING GAS TUNGSTEN ARC WELDING PROCESS

    Directory of Open Access Journals (Sweden)

    Sivaraman Arunkumar

    2016-09-01

    Full Text Available In this study we focus on finite element simulation of gas tungsten arc welding (GTAW of AA2219 aluminum alloy and the behavioral of the microstructure before and after weld. The simulations were performed using commercial COMSOL Multiphysics software. The thermal history of the weld region was studied by initially developed mathematical model. A sweep type meshing was used and transient analysis was performed for one welding cycle. The highest temperature noted was 3568 °C during welding. The welding operation was performed on 200×100×25 mm plates. Through metallurgical characterization, it was observed that a fair copper rich cellular (CRC network existed in the weld region. A small amount of intermetallic compounds like Al2Cu is observed through the XRD pattern.

  17. 46 CFR 56.70-15 - Procedure.

    Science.gov (United States)

    2010-10-01

    ... joints for pipe diameters exceeding three-fourth inch nominal pipe size. The use of a single welded butt... cavity to be repaired may differ in contour and dimensions from the original joint. The types, extent... if there is no added reinforcement). tmin=the smaller of tn or te. tw=dimension of partial...

  18. Systemic AA amyloidosis in the red fox (Vulpes vulpes).

    Science.gov (United States)

    Rising, Anna; Cederlund, Ella; Palmberg, Carina; Uhlhorn, Henrik; Gaunitz, Stefan; Nordling, Kerstin; Ågren, Erik; Ihse, Elisabet; Westermark, Gunilla T; Tjernberg, Lars; Jörnvall, Hans; Johansson, Jan; Westermark, Per

    2017-11-01

    Amyloid A (AA) amyloidosis occurs spontaneously in many mammals and birds, but the prevalence varies considerably among different species, and even among subgroups of the same species. The Blue fox and the Gray fox seem to be resistant to the development of AA amyloidosis, while Island foxes have a high prevalence of the disease. Herein, we report on the identification of AA amyloidosis in the Red fox (Vulpes vulpes). Edman degradation and tandem MS analysis of proteolyzed amyloid protein revealed that the amyloid partly was composed of full-length SAA. Its amino acid sequence was determined and found to consist of 111 amino acid residues. Based on inter-species sequence comparisons we found four residue exchanges (Ser31, Lys63, Leu71, Lys72) between the Red and Blue fox SAAs. Lys63 seems unique to the Red fox SAA. We found no obvious explanation to how these exchanges might correlate with the reported differences in SAA amyloidogenicity. Furthermore, in contrast to fibrils from many other mammalian species, the isolated amyloid fibrils from Red fox did not seed AA amyloidosis in a mouse model. © 2017 The Protein Society.

  19. Chang'aa Drinking in Kibera Slum: The Harmful Effects of ...

    African Journals Online (AJOL)

    Chang'aa Drinking in Kibera Slum: The Harmful Effects of Contemporary Changes in the Production and Consumption of Traditional Spirits. ... African Journal of Drug and Alcohol Studies ... This article examines the harmful effects of drinking chang'aa, an illegal spirit produced locally, in Kibera slum in Nairobi, Kenya.

  20. On detection and automatic tracking of butt weld line in thin wall pipe welding by a mobile robot with visual sensor

    International Nuclear Information System (INIS)

    Suga, Yasuo; Ishii, Hideaki; Muto, Akifumi

    1992-01-01

    An automatic pipe welding mobile robot system with visual sensor was constructed. The robot can move along a pipe, and detect the weld line to be welded by visual sensor. Moreover, in order to make an automatic welding, the welding torch can track the butt weld line of the pipes at a constant speed by rotating the robot head. Main results obtained are summarized as follows: 1) Using a proper lighting fixed in front of the CCD camera, the butt weld line of thin wall pipes can be recongnized stably. In this case, the root gap should be approximately 0.5 mm. 2) In order to detect the weld line stably during moving along the pipe, a brightness distribution measured by the CCD camera should be subjected to smoothing and differentiating and then the weld line is judged by the maximum and minimum values of the differentials. 3) By means of the basic robot system with a visual sensor controlled by a personal computer, the detection and in-process automatic tracking of a weld line are possible. The average tracking error was approximately 0.2 mm and maximum error 0.5 mm and the welding speed was held at a constant value with error of about 0.1 cm/min. (author)

  1. Changes in depression mediate the effects of AA attendance on alcohol use outcomes.

    Science.gov (United States)

    Wilcox, Claire E; Tonigan, J Scott

    2018-01-01

    Depression may contribute to increased drinking in individuals with alcohol use disorder. Although Alcoholics Anonymous (AA) attendance predicts drinking reductions, there is conflicting information regarding the intermediary role played by reductions in depression. We explored whether AA attendance reduces depressive symptoms, the degree to which improvement in depression results in reductions in drinking, and in which subgroups these effects occur. 253 early AA affiliates (63% male) were recruited and assessed at baseline 3, 6, 9, 12, 18, and 24 months. Depression was measured using the Beck Depression Inventory (BDI) and was administered at baseline 3, 6, 12, 18, and 24 months. AA attendance and alcohol use outcomes were obtained with the Form 90. Mediation analyses were performed at early (3, 6, and 9 months) and late (12, 18, and 24 months) follow-up to investigate the degree to which reductions in depression mediated the effect of AA attendance on drinking, controlling for concurrent drinking. In addition, a series of moderated mediation analyses were performed using baseline depression severity as a moderator. At early follow-up, reductions in depression (6 months) mediated the effects of AA attendance (3 months) on later drinking (drinks per drinking day) (9 months) (b = -0.02, boot CI [-0.055, -0.0004]), controlling for drinking at 6 months. Baseline depression severity did not moderate the degree to which BDI mediated the effects of AA attendance on alcohol use (ps > .05). These findings provide further evidence that depression reduction is a mechanism by which AA attendance leads to reductions in alcohol use. Improving depression may help reduce alcohol use in individuals with AUD, and AA attendance may be an effective way to achieve that goal.

  2. Preparation and Characteristics of Corn Straw-Co-AMPS-Co-AA Superabsorbent Hydrogel

    Directory of Open Access Journals (Sweden)

    Wei-Min Cheng

    2015-11-01

    Full Text Available In this study, the corn straw after removing the lignin was grafted with 2-acrylamido-2-methylpropanesulfonic acid (AMPS to prepare sulfonated cellulose. The grafting copolymerization between the sulfonated cellulose and acrylic acid (AA was performed using potassium persulfate and N,N′-methylenebisacrylamide as the initiator and crosslinking agent, respectively, to prepare corn straw-co-AMPS-co-AA hydrogels. The structure and properties of the resulting hydrogels were characterized by Fourier transform infrared spectroscopy, X-ray diffraction, scanning electron microscopy, thermogravimetric analysis, and dynamic rheometry. The effects of initiator, crosslinker, monomer neutralization degree, and temperature on the swelling ratio of the hydrogels were studied. The water retention, salt resistance, and recyclability of the corn straw-co-AMPS-co-AA hydrogels were also investigated. The optimum water absorptivity of the corn straw hydrogels was obtained at a polymerization temperature of 50 °C with 1.2% crosslinker, 1:7 ratio of the pretreated corn straw and AA, 2% initiator, and 50% neutralized AA.

  3. Ultrasonic testing X gammagraphy

    International Nuclear Information System (INIS)

    Mello Campos, A.M. de

    1989-01-01

    The experience of 10 years for substituting gammagraphy tests by ultrasonic tests is related. A comparative evaluation of data obtained from both techniques applied to welded butt joints is presented. (author)

  4. INVESTIGATION OF EFFECT OF COOLING CONDITIONS ON HARDNESS OF THE AA 2024 AND AA 2014 WROUGHT ALUMINIUM ALLOYS

    Directory of Open Access Journals (Sweden)

    Hülya KAÇAR DURMUŞ

    2003-01-01

    Full Text Available Mechanical properties of some aluminum alloys can be changed with precipitation hardening. This intermetallic precipitates are incoherent with the main structure and increased mechanical properties. Cooling rates after solid solution process effects properties after precipitation. In applications, however this is not taken into consideration. In this study, AA 2014 and AA 2024 Aluminium Alloy specimens were hold for one hour at 495±3 0C and formed a solid solution. Specimens were quenched at this temperature with different cooling rtes . later artificial aging was applied at 150 0C and 180 0C. The hardness and microstructure variations of the specimens were investigated depending on the cooling rates and artificial aging temperatures.

  5. AA, bending magnet, BLG

    CERN Multimedia

    CERN PhotoLab

    1980-01-01

    The very particular lattice of the AA required 2 types of dipole (bending magnets; BLG, long and narrow; BST, short and wide). The BLG had a steel length of 4.70 m, a good field width of 0.24 m, and a weight of about 70 t. Jean-Claude Brunet inspects the lower half of a BLG. For the BST magnets see 7811105 and 8006036.

  6. Identifying a typology of men who use anabolic androgenic steroids (AAS).

    Science.gov (United States)

    Zahnow, Renee; McVeigh, Jim; Bates, Geoff; Hope, Vivian; Kean, Joseph; Campbell, John; Smith, Josie

    2018-05-01

    Despite recognition that the Anabolic Androgenic Steroid (AAS) using population is diverse, empirical studies to develop theories to conceptualise this variance in use have been limited. In this study, using cluster analysis and multinomial logistic regression, we identify typologies of people who use AAS and examine variations in motivations for AAS use across types in a sample of 611 men who use AAS. The cluster analysis identified four groups in the data with different risk profiles. These groups largely reflect the ideal types of people who use AAS proposed by Christiansen et al. (2016): Cluster 1 (You Only Live Once (YOLO) type, n = 68, 11.1%) were younger and motivated by fat loss; Cluster 2 (Well-being type, n = 236, 38.6%) were concerned with getting fit; Cluster 3 (Athlete type, n = 155, 25.4%) were motivated by muscle and strength gains; Cluster 4 (Expert type, n = 152, 24.9%) were focused on specific goals (i.e. not 'getting fit'). The results of this study demonstrate the need to make information about AAS accessible to the general population and to inform health service providers about variations in motivations and associated risk behaviours. Attention should also be given to ensuring existing harm minimisation services are equipped to disseminate information about safe intra-muscular injecting and ensuring needle disposal sites are accessible to the different types. Copyright © 2018 Elsevier B.V. All rights reserved.

  7. Composite Sunrise Butte pluton: Insights into Jurassic–Cretaceous collisional tectonics and magmatism in the Blue Mountains Province, northeastern Oregon

    Science.gov (United States)

    Johnson, Kenneth H.; Schwartz, J.J.; Žák, Jiří; Verner, Krystof; Barnes, Calvin G.; Walton, Clay; Wooden, Joseph L.; Wright, James E.; Kistler, Ronald W.

    2015-01-01

    The composite Sunrise Butte pluton, in the central part of the Blue Mountains Province, northeastern Oregon, preserves a record of subduction-related magmatism, arc-arc collision, crustal thickening, and deep-crustal anatexis. The earliest phase of the pluton (Desolation Creek unit) was generated in a subduction zone environment, as the oceanic lithosphere between the Wallowa and Olds Ferry island arcs was consumed. Zircons from this unit yielded a 206Pb/238U age of 160.2 ± 2.1 Ma. A magmatic lull ensued during arc-arc collision, after which partial melting at the base of the thickened Wallowa arc crust produced siliceous magma that was emplaced into metasedimentary rocks and serpentinite of the overthrust forearc complex. This magma crystallized to form the bulk of the Sunrise Butte composite pluton (the Sunrise Butte unit; 145.8 ± 2.2 Ma). The heat necessary for crustal anatexis was supplied by coeval mantle-derived magma (the Onion Gulch unit; 147.9 ± 1.8 Ma).The lull in magmatic activity between 160 and 148 Ma encompasses the timing of arc-arc collision (159–154 Ma), and it is similar to those lulls observed in adjacent areas of the Blue Mountains Province related to the same shortening event. Previous researchers have proposed a tectonic link between the Blue Mountains Province and the Klamath Mountains and northern Sierra Nevada Provinces farther to the south; however, timing of Late Jurassic deformation in the Blue Mountains Province predates the timing of the so-called Nevadan orogeny in the Klamath Mountains. In both the Blue Mountains Province and Klamath Mountains, the onset of deep-crustal partial melting initiated at ca. 148 Ma, suggesting a possible geodynamic link. One possibility is that the Late Jurassic shortening event recorded in the Blue Mountains Province may be a northerly extension of the Nevadan orogeny. Differences in the timing of these events in the Blue Mountains Province and the Klamath–Sierra Nevada Provinces suggest that

  8. Microstructural characterization of fly ash particulate reinforced AA6063 aluminium alloy for aerospace applications

    Science.gov (United States)

    Razzaq, A. M.; Majid, D. L. Abang Abdul; Ishak, M. R.; Uday, M. B.

    2017-12-01

    Aluminium-fly ash (FA) particulate reinforced composites (AA6063-FA) have been used in automotive and aerospace industries because of their low density and good mechanical properties. Three different weight fraction of FA: 2%, 4% and 6% are added to AA6063 alloy using compocasting method. The effect of FA particulates on microstructure, density and compression strength of AA6063- FA composites are investigated. Field Emission Scanning Electron Microscope (FESEM) micrographs reveal that the FA particulates are uniformly distributed in AA6063 alloy. The results also show that density, compression strength and microstructure of the AA6063-FA composites are significantly influenced by the FA amount. The increase in the weight fraction of FA will improve the microstructure and enhance the compression strength. The density of AA6063-FA composites decreases as the incorporation of FA increases.

  9. The effect of joint surface contours and glass fiber reinforcement on the transverse strength of repaired acrylic resin: An in vitro study.

    Science.gov (United States)

    Anasane, Nayana; Ahirrao, Yogesh; Chitnis, Deepa; Meshram, Suresh

    2013-03-01

    Denture fracture is an unresolved problem in complete denture prosthodontics. However, the repaired denture often experiences a refracture at the repaired site due to poor transverse strength. Hence, this study was conducted to evaluate the effect of joint surface contours and glass fiber reinforcement on the transverse strength of repaired acrylic resins. A total of 135 specimens of heat polymerized polymethyl methacrylate resin of dimensions 64 × 10 × 2.5 mm were fabricated. Fifteen intact specimens served as the control and 120 test specimens were divided into four groups (30 specimens each), depending upon the joint surface contour (butt, bevel, rabbet and round), with two subgroups based on type of the repair. Half of the specimens were repaired with plain repair resin and the other half with glass fibers reinforced repair resin. Transverse strength of the specimens was determined using three-point bending test. The results were analyzed using one-way ANOVA and Tukey post-hoc test (α= 0.05). Transverse strength values for all repaired groups were significantly lower than those for the control group (P transverse strength; hence, it can be advocated for repair of denture base resins.

  10. AAS 227: Day 1

    Science.gov (United States)

    Kohler, Susanna

    2016-01-01

    Editors Note:This week were at the 227th AAS Meeting in Kissimmee, FL. Along with several fellow authors from astrobites.com, I will bewritingupdates on selectedevents at themeeting and posting at the end of each day. Follow along here or at astrobites.com, or catch ourlive-tweeted updates from the @astrobites Twitter account. The usual posting schedule for AAS Nova will resumenext week.Things kicked off last night at our undergraduate reception booth. Thanks to all of you who stopped by we were delightedto have so many people tell us that they already know about and useastrobites, and we were excited to introduce a new cohort of students at AAS to astrobites for the first time.Tuesday morning was the official start of the meeting. Here are just a few of the talks and workshops astrobiters attended today.Opening Address (by Becky Smethurst)The President of the AAS, aka our fearless leader Meg Urry kicked off the meeting this morning at the purely coffee powered hour of 8am this morning. She spoke about the importance of young astronomers at the meeting (heres looking at you reader!) and also the importance of the new Working Group for Accessibility and Disabilities (aka WGAD pronounced like wicked) at the AAS. The Society has made extra effort this year to make the conference accessible to all,a message which was very well received by everyone in attendance.Kavli Lecture: New Horizons Alan Stern (by Becky Smethurst)We were definitely spoilt with the first Plenary lecture at this years conference Alan Stern gave us a a review of the New Horizons mission of the Pluto Fly By (astrobites covered the mission back in July with this post). We were treated to beautiful images, wonderful results and a foray into geology.Before (Hubble) and after #NewHorizons. #thatisall #science #astro alanstern #aas227 pic.twitter.com/kkMt6RsSIR Science News (@topsciencething) January 5, 2016Some awesome facts from the lecture that blew my mind:New Horizons is now 2AU (!) beyond Pluto

  11. AAS 228: Day 1 morning

    Science.gov (United States)

    Kohler, Susanna

    2016-06-01

    occur at different times and have different depths in the light curve each time they orbit. Their misalignment may have been caused by a past collision with another planet, which was kicked out of the system in the process. The LIGO-VIRGO Forum on Hunting Gravitational Wave Counterparts(by Gourav Khullar)This parallel session, organized by Peter Shawhan (University of Maryland, advancedLIGO) discussed the first major followup campaign of the GW150914 gravitational wave (GW) discovery event by the physics and astronomy community around the world. It was extremely exciting to hear the speakers talk of the actual process behind the mega-collaborative effort following the first GW event. This paper, published on June 3rd this year, was described by Peter, with a strong emphasis on the timeline following the GW alert in raw LIGO data back in September 2015, along with description of the sky map and raw data given to different facilities and collaborations that LIGO-VIRGO had signed Memorandums of Understanding (MOUs) with for rapid and robust followups. The talk also focussed on resources and tutorials available now to unpack and characterize future alerts data from LIGO-VIRGO. This talk was followed by the description of the all sky survey PAN-STARRS, and its joint efforts with LIGO. It was pointed out that PAN-STARRS had already scanned the sky multiple times, which gave the program an edge in determining transients, i.e. recent features appearing on their new maps but not the old. This extensive survey also allowed better characterization of the transient source, which would be the next step for PAN-STARRS and other similar projects. Our @LIGO booth at #AAS228 is up and running drop by for a chat about #gravitationalwaves pic.twitter.com/akt9wsVPT6 pic.twitter.com/kmPz3oxzJf LIGO (@LIGO) June 13, 2016Following this was a talk by Andy Howell, of the newly formed Las Cumbres Observatory A Global Telescope Network (LCOGT), made up of multiple telescopes across the US, Chile

  12. The coal deposits of the Alkali Butte, the Big Sand Draw, and the Beaver Creek fields, Fremont County, Wyoming

    Science.gov (United States)

    Thompson, Raymond M.; White, Vincent L.

    1952-01-01

    Large coal reserves are present in three areas located between 12 and 20 miles southeast of Riverton, Fremont County, central Wyoming. Coal in two of these areas, the Alkali Butte coal field and the Big Sand Draw coal field, is exposed on the surface and has been developed to some extent by underground mining. The Beaver Creek coal field is known only from drill cuttings and cores from wells drilled for oil and gas in the Beaver Creek oil and gas field.These three coal areas can be reached most readily from Riverton, Wyo. State Route 320 crosses Wind River about 1 mile south of Riverton. A few hundred yards south of the river a graveled road branches off the highway and extends south across the Popo Agie River toward Sand Draw oil and gas field. About 8 miles south of the highway along the Sand Draw road, a dirt road bears east and along this road it is about 12 miles to the Bell coal mine in the Alkali Butte coal field. Three miles southeast of the Alkali Butte turn-off, 3 miles of oiled road extends southwest into the Beaver Creek oil and gas field. About 6 miles southeast of the Beaver Creek turn-off, in the valley of Little Sand Draw Creek, a dirt road extends east 1. mile and then southeast 1 mile to the Downey mine in the Big Sand Draw coal field. Location of these coal fields is shown on figure 1 with their relationship to the Wind River basin and other coal fields, place localities, and wells mentioned in this report. The coal in the Alkali Butte coal field is exposed partly on the Wind River Indian Reservation in Tps. 1 and 2 S., R. 6 E., and partly on public land. Coal in the Beaver Creek and Big Sand Draw coal fields is mainly on public land. The region has a semiarid climate with rainfall averaging less than 10 in. per year. When rain does fall the sandy-bottomed stream channels fill rapidly and are frequently impassable for a few hours. Beaver Creek, Big Sand Draw, Little Sand Draw, and Kirby Draw and their smaller tributaries drain the area and flow

  13. Requirements to gap widths and clamping for CO2 laser butt welding

    DEFF Research Database (Denmark)

    Gong, Hui; Juhl, Thomas Winther

    1999-01-01

    In the experimental study of fixturing and gap width requirements a clamping device for laser butt welding of steel sheets has been developed and tested. It has fulfilled the work and made the gap width experiments possible.It has shown that the maximum allowable gap width to some extent...... is inversely related to the welding speed. Also larger laser power leads to bigger allowable gap widths. The focal point position, though, has little influence on the maximum allowable gap width.During analysis X-ray photos show no interior porosity in the weld seam. Other methods have been applied to measure...... responses from variations in welding parameters.The table below lists the results of the study, showing the maximum allowable gap widths and some corresponding welding parameters.Maximum allowable Gap Width; Welding Speed; Laser Power:0.10 mm2 m/min2, 2.6 kW0.15 mm1 m/min2 kW0.20 mm1 m/min2.6 kW0.30 mm0.5 m...

  14. Overview of the Antiproton Accumulator (AA)

    CERN Multimedia

    1982-01-01

    See photo 8202324. For photos of the AA in different phases of completion (between 1979 and 1982) see: 7911303, 7911597X, 8004261, 8004608X, 8005563X, 8005565X, 8006716X, 8006722X, 8010939X, 8010941X, 8202324, 8202658X, 8203628X .

  15. A Status Report on the AAS Astronomy Ambassadors Program

    Science.gov (United States)

    Fienberg, Richard Tresch; Fraknoi, Andrew; Gurton, Suzanne; Hurst, Anna; Schatz, Dennis L.

    2014-06-01

    The American Astronomical Society, in partnership with the Astronomical Society of the Pacific (ASP), has launched a series of professional-development workshops and a community of practice designed to improve early-career astronomers’ ability to communicate effectively with students and the public. Called AAS Astronomy Ambassadors, the program provides training and mentoring for young astronomers, from advanced undergraduates to beginning faculty; it also provides them access to resources and a network of contacts within the astronomy education and public outreach (EPO) community. Ambassadors are provided with a library of outreach activities and resource materials suitable for a range of venues and audiences. For much of this library we are using resources developed by organizations such as the ASP, the Pacific Science Center, and the Center for Astronomy Education for other outreach programs, though some resources have been created by one of us (AF) specifically for this program. After a period of evaluation and revision, the program’s “Menu of Outreach Opportunities for Science Education” (MOOSE) is now posted on the AAS website at http://aas.org/outreach/moose-menu-outreach-opportunities-science-education.The first two Astronomy Ambassadors workshops were held at AAS meetings in January 2013 and January 2014; each served 30 young astronomers chosen from about twice that many applicants. Web-based follow-up activities are being provided through a website at the ASP designed to keep cohorts of educators trained in their programs in touch with one another. The AAS is exploring ways to fund additional workshops at future winter meetings; suggestions are most welcome. Meanwhile, the Astronomy Ambassadors trained to date have logged more than 150 outreach events, reaching many thousands of children and adults across the U.S. and Canada.

  16. The Effect of Applied Tensile Stress on Localized Corrosion in Sensitized AA5083

    Science.gov (United States)

    2015-09-01

    corrosion, but if exposed to elevated temperature for prolonged periods of time the alloy becomes sensitized. Since the β phase is more anodic than the...degree of localized corrosion for sensitized AA5083 under an applied tensile stress. AA5083 is an aluminum -magnesium alloy that experiences severe...direction. 14. SUBJECT TERMS Aluminum alloy , AA5083, IGSCC, intergranular stress corrosion cracking, localized corrosion, sensitized aluminum 15

  17. Astrocytes mediated the nootropic and neurotrophic effects of Sarsasapogenin-AA13 via upregulating brain-derived neurotrophic factor.

    Science.gov (United States)

    Dong, Dong; Mao, Yu; Huang, Cui; Jiao, Qian; Pan, Hui; Ma, Lei; Wang, Rui

    2017-01-01

    Rhizoma Anemarrhena , a widely used traditional Chinese medicine, has previously been shown to have neuroprotective effect. Sarsasapogenin-AA13 (AA13) is a novel synthetic derivative of Sarsasapogenin, which is extracted from Rhizoma Anemarrhena . The aim of this study is to investigate the nootropic and neurotrophic effects of AA13 and underlying mechanisms. In vitro , cell viability of rat primary astrocytes treated with AA13 and neurons cultured with conditioned medium of AA13-treated rat primary astrocytes was tested by MTT assays. In vivo , a pharmacological model of cognitive impairment induced by scopolamine was employed and spatial memory of the mice was assessed by Morris water maze. This study found that AA13 increased cell viability of primary astrocytes and AA13-treated astrocyte-conditioned medium enhanced the survival rate of primary neurons. Interestingly, AA13 markedly enhanced the level of BDNF in astrocytes. Furthermore, AA13 (6 mg/kg) improved the cognitive deficits in animal models (p<0.05) and BDNF and PSD95 levels were increased in brain. Therefore, we hypothesize that AA13 exerts nootropic and neurotrophic activities through astrocytes mediated upregulation of BDNF secretion. The results suggest that AA13 could be a potential compound for cognitive impairment after further research.

  18. The Search for Hot Jupiters using Red Buttes Observatory

    Science.gov (United States)

    Sorber, Rebecca L.; Kar, Aman; Hancock, Daniel A.; Leuquire, Jacob D.; Suhaimi, Afiq; Kasper, David; Jang-Condell, Hannah

    2018-01-01

    The goal of this research is to use the University of Wyoming’s Red Buttes Observatory (RBO) to perform manual, remote, or automated observations of transiting exoplanet candidates. The data contributes to discovery of star systems that include never before identified exoplanets. RBO houses a 0.6-meter telescope and is located approximately 10 miles south of the University of Wyoming’s campus. Our targets are catalogued by the KELT (Kilodegree Extremely Little Telescope) Survey, a photometric search for transiting exoplanets around bright main sequence stars. The KELT Follow-up Network (KELT-FUN), a collaboration of small-aperture telescope users located all over the world, confirms new exoplanet candidates. As part of KELT-FUN, students use the RBO to monitor candidates identified by the KELT team. RBO typically detects transits around stars that are 8-12 in V magnitude, with transit durations of ~1-4 hours and full depth relative changes in brightness above 2 mmags. Using AstroImageJ, we process the data and we look for any indication of a transit occurrence in the processed lightcurve which might confirm the presence of the potential exoplanet. Our team has contributed over 50 light curves to KELT-FUN to date. We are able to compare our data with simultaneous observations by other members of KELT-FUN to maximize the utility of our observations. This project gives undergraduates an authentic scientific research experience, learning how to operate an observatory, process data, and participate in a scientific collaboration.

  19. Adverse effects of doping with anabolic androgenic steroids (AAS) in competitive athletics, recreational sports and bodybuilding.

    Science.gov (United States)

    Vorona, Elena; Nieschlag, Eberhard

    2018-02-19

    Despite the fact that sports organizations and legislators have introduced various mechanisms to discourage athletes from using performance and appearance enhancing substances a high percentage of athletes admits to their unabated application. In competitive athletics, bodybuilding and in recreational sports anabolic androgenic steroids (AAS) continue to be the substances most abused. This review summarizes the side effects of AAS abuse on organs and system functions in both sexes. High doses of AAS cause a significant increase of erythrocytes und haemoglobin concentration, which may lead to thromboembolism, intracardiac thrombosis and stroke. Long-term AAS abusers have a higher incidence of arrhythmias, atherosclerosis, concentric left-ventricular myocardial hypertrophy with impaired diastolic function and also sudden cardiac death. Changes of liver function and structure, up to hepatocellular carcinoma, have been described, mainly in cases of chronic misuse of 17α-alkylated AAS. Sleeplessness, increased irritability, depressive mood status are often observed in AAS abuse. In former AAS abusers depression, anxiety and melancholy may persist for many years. Due to negative feedback in the regulation of the hypothalamic-pituitary-gonadal axis AAS can cause reversible suppression of spermatogenesis up to azoospermia. In women the changes most often caused by AAS abuse are hirsutism, irreversible deepening of voice, dysmenorrhoea, secondary amenorrhoea with anovulation and infertility. AAS abuse notwithstanding, under clinical conditions testosterone remains the most important hormone for substitution therapy of male hypogonadism.

  20. 76 FR 6794 - 30-Day Submission Period for Requests for ONC-Approved Accreditor (ONC-AA) Status

    Science.gov (United States)

    2011-02-08

    ... Accreditor (ONC-AA) Status AGENCY: Office of the National Coordinator for Health Information Technology... submission of requests for ONC-Approved Accreditor (ONC-AA) status. Authority: 42 U.S.C. 300jj-11. DATES: The... for ONC-AA status may be submitted. The 30-day period for submission of requests for ONC-AA status...

  1. Modeling of AA5083 Material-Microstructure Evolution During Butt Friction-Stir Welding

    Science.gov (United States)

    2010-07-01

    a rigid material. Its density and thermal properties are set to that of AISI- H13 , the hot-worked tool steel which is often used as a FSW- tool ...joining process (Ref 1-3). Within FSW, a (typically) cylindrical tool - pin (threaded at the bottom and terminated with a circular-plate shape shoulder...applied to the shoulder and owing to frictional sliding and plastic deforma- tion, substantial amount of heat is generated at the tool /work- piece

  2. Material flow in butt friction stir welds in AA2024-T3

    International Nuclear Information System (INIS)

    Schmidt, H.N.B.; Dickerson, T.L.; Hattel, J.H.

    2006-01-01

    The properties of a workpiece joined by friction stir welding (FSW) are directly related to the material flow around the tool. In the present work, the material flow is investigated by traditional metallography as well as X-ray and computer tomography (CT). By introducing a thin copper strip in the workpiece and welding through it, thus, acting as a marker material, detailed information about the flow field is gathered. The two- and three-dimensional CT images are used in parallel with micrographs for visualization of the flow field. Two procedures for estimating the average velocities for material flowing through the shear layer are presented. The procedures depend on the configuration of marker material relative to the welding direction, i.e. longitudinal and transverse. As such, the present work constitutes the first attempt in the literature to estimate flow velocities in FSW based on thorough experimental investigations

  3. AAS 228: Day 3 afternoon

    Science.gov (United States)

    Kohler, Susanna

    2016-06-01

    Editors Note:This week were at the 228th AAS Meeting in San Diego, CA. Along with a team ofauthors from astrobites.com, I will bewritingupdates on selectedevents at themeeting and posting twiceeach day. Follow along here or atastrobites.com, or catch ourlive-tweeted updates from the@astrobites Twitter account. The usual posting schedule for AAS Nova will resumenext week.Wikipedia Year of Science Editathon (by Meredith Rawls)Whats your first go-to source for an unfamiliar topic on the internet? If you said Wikipedia, youre not alone. For many people, Wikipedia is the primary source of information about astronomy and science. However, many Wikipedia articles about science topics are incomplete or missing, and women are underrepresented among scientists with biographies.To address this, the AAS Astronomy Education Board teamed up with the Wiki Education Foundation to host an edit-a-thon as part of the Wikipedia Year of Science. More than forty attendees spent the better part of three hours working through tutorials, creating new articles, and editing existing ones. The session was generously sponsored by the Simons Foundation.The Year of Science initiative seeks to bring Wikipedia editing skills to the classroom and help new editors find sustainable ways to contribute to Wikipedia in the long term. Anybody can create a free account and start editing!As a first-time Wikipedia contributor, I took the time to go through nearly all the tutorial exercises and familiarize myself with the process of editing a page. I decided to flesh out one section in an existing page about asteroseismology. Others created biography pages from scratch or selected various astronomical topics to write about. To me, the editing process felt like a cross between writing a blog post and a journal article, in a hack day type environment. Working through the tutorial and some examples renewed my empathy for learners who are tackling a new skill set for the first time. A full summary of our

  4. Effects of chronic ethanol ingestion on arachidonic acid (AA) metabolism in rat macrophages

    International Nuclear Information System (INIS)

    Chanmugam, P.; Boudreau, M.; Hymel, G.; Jeffers, G.; Hwang, D.H.

    1986-01-01

    In a previous report, preincubation of rat platelets with ethanol resulted in dose dependent inhibition of AA metabolites whereas chronic ingestion of ethanol enhanced the synthesis of AA metabolites. Thus, the authors studied whether chronic ethanol ingestion also affects AA metabolism in MACS. Two groups of rats (10 each) were fed DeCarli/Lieber liquid diet containing 36 caloric % ethanol for 3 weeks. The control group was pair fed the same diet made isocaloric with dextrin-maltose. Resident MACS were collected by peritoneal lavage. The monolayers of MACS were incubated for 20 min with calcium ionophore (5μg/ml), and the incubation stopped with 4 vol. of ethanol. PGE 2 , LTB 4 and 5-HETE were assayed by radioimmunoassay. The results indicated that chronic ethanol ingestion did not affect the capacity of MACS to synthesize AA metabolites. There was also no difference in the levels of AA metabolites in heart and lung homogenates between the two groups

  5. Studying the Issues in Laser Joining of Lightweight Materials in a Coach-Peel Joint Configuration

    Science.gov (United States)

    Yang, Guang

    In the automotive industry, aluminum alloys have been widely used and partially replaced the conventional steel structures in order to decrease the weight of a car and improve its fuel efficiency. This Thesis focuses on the development of laser joining of light-weight materials, such as aluminum alloys and high-strength galvanized steels. Among different joint types, the coach-peel configuration is of a specific design that requires a heat source capable of heating up a large surface area of the joint. Coach-peel joints applied on the visible exterior of a car require a smooth transition from the weld surface to the panel surface and low surface roughness without any need for post-processing. Although these joints are used as non-load-bearing components, a desirable strength of the weld is also needed. A fusion-brazing process using a dual-beam laser allows the automotive components such as the roof and side member panels to be joined in a coach-peel configuration with a high surface quality as well as an acceptable strength of the weld. To improve the weld surface quality, processing parameters such as laser beam configuration, laser-wire position, and shielding gas parameters were optimized for joining of aluminum alloy to aluminum alloy. Laser power was optimized for dual-beam laser joining of aluminum alloy to galvanized steel at high speed. The feasibility of joining as-received panels with lubricant was also explored. The identification of strain hardening models of aluminum alloys was conducted for the mechanical finite element analysis of the joint. Control of the molten pool solidification through the selection of laser beam configuration is one approach to improve joint quality. Laser joining of aluminum alloy AA 6111-T4 coach peel panels with the addition of AA 4047 filler wire was investigated using three configurations of laser beam: a single beam, dual beams in-line with the weld bead, and dual beams aligned perpendicular to the weld bead (herein

  6. Coarsening of AA6013-T6 Precipitates During Sheet Warm Forming Applications

    Science.gov (United States)

    Di Ciano, M.; DiCecco, S.; Esmaeili, S.; Wells, M. A.; Worswick, M. J.

    2018-03-01

    The use of warm forming for AA6xxx-T6 sheet is of interest to improve its formability; however, the effect warm forming may have on the coarsening of precipitates and the mechanical strength of these sheets has not been well studied. In this research, the coarsening behavior of AA6013-T6 precipitates has been explored, in the temperature range of 200-300 °C, and time of 30 s up to 50 h. Additionally, the effect of warm deformation on coarsening behavior was explored using: (1) simulated warm forming tests in a Gleeble thermo-mechanical simulator and (2) bi-axial warm deformation tests. Using a strong obstacle model to describe the yield strength (YS) evolution of the AA6013-T6 material, and a Lifshitz, Slyozov, and Wagner (LSW) particle coarsening law to describe the change in precipitate size with time, the coarsening kinetics were modeled for this alloy. The coarsening kinetics in the range of 220-300 °C followed a trend similar to that previously found for AA6111 for the 180-220 °C range. There was strong evidence that coarsening kinetics were not altered due to warm deformation above 220 °C. For warm forming between 200 and 220 °C, the YS of the AA6013-T6 material increased slightly, which could be attributed to strain hardening during warm deformation. Finally, a non-isothermal coarsening model was used to assess the potential reduction in the YS of AA6013-T6 for practical processing conditions related to auto-body manufacturing. The model calculations showed that 90% of the original AA6013-T6 YS could be maintained, for warm forming temperatures up to 280 °C, if the heating schedule used to get the part to the warm forming temperature was limited to 1 min.

  7. Long-term biases in geomagnetic K and aa indices

    Science.gov (United States)

    Love, J.J.

    2011-01-01

    Analysis is made of the geomagnetic-activity aa index and its source K-index data from groups of ground-based observatories in Britain, and Australia, 1868.0-2009.0, solar cycles 11-23. The K data show persistent biases, especially for high (low) K-activity levels at British (Australian) observatories. From examination of multiple subsets of the K data we infer that the biases are not predominantly the result of changes in observatory location, localized induced magnetotelluric currents, changes in magnetometer technology, or the modernization of K-value estimation methods. Instead, the biases appear to be artifacts of the latitude-dependent scaling used to assign K values to particular local levels of geomagnetic activity. The biases are not effectively removed by weighting factors used to estimate aa. We show that long-term averages of the aa index, such as annual averages, are dominated by medium-level geomagnetic activity levels having K values of 3 and 4. ?? 2011 Author(s).

  8. Long-term biases in geomagnetic K and aa indices

    Directory of Open Access Journals (Sweden)

    J. J. Love

    2011-08-01

    Full Text Available Analysis is made of the geomagnetic-activity aa index and its source K-index data from groups of ground-based observatories in Britain, and Australia, 1868.0–2009.0, solar cycles 11–23. The K data show persistent biases, especially for high (low K-activity levels at British (Australian observatories. From examination of multiple subsets of the K data we infer that the biases are not predominantly the result of changes in observatory location, localized induced magnetotelluric currents, changes in magnetometer technology, or the modernization of K-value estimation methods. Instead, the biases appear to be artifacts of the latitude-dependent scaling used to assign K values to particular local levels of geomagnetic activity. The biases are not effectively removed by weighting factors used to estimate aa. We show that long-term averages of the aa index, such as annual averages, are dominated by medium-level geomagnetic activity levels having K values of 3 and 4.

  9. Friction stir welding of dissimilar AA2024 and AA7075 aluminum alloys

    International Nuclear Information System (INIS)

    Khodir, Saad Ahmed; Shibayanagi, Toshiya

    2008-01-01

    The present study focuses on the microstructure and mechanical properties of dissimilar joints of 2024-T3 Al alloy to 7075-T6 Al alloy produced by friction stir welding. Effects of welding speed and fixed location of base metals on microstructures, hardness distributions, and tensile properties of the welded joints were investigated. SEM-EDS analysis revealed that the stir zone contains a mixed structure and onion ring pattern with a periodic change of grain size as well as a heterogeneous distribution of alloying elements. The maximum tensile strength of 423.0 MPa was achieved for the joint produced at welding speed of 1.67 mm/s when 2024 Al alloy was located on the advancing side

  10. Relationship between patient-reported outcomes and clinical outcomes in metastatic castration-resistant prostate cancer: post hoc analysis of COU-AA-301 and COU-AA-302.

    Science.gov (United States)

    Cella, D; Traina, S; Li, T; Johnson, K; Ho, K F; Molina, A; Shore, N D

    2018-02-01

    Patient-reported outcomes (PROs) are used to assess benefit-risk in drug development. The relationship between PROs and clinical outcomes is not well understood. We aim to elucidate the relationships between changes in PRO measures and clinical outcomes in metastatic castration-resistant prostate cancer (mCRPC). We investigated relationships between changes in self-reported fatigue, pain, functional well-being (FWB), physical well-being (PWB) and prostate cancer-specific symptoms with overall survival (OS) and radiographic progression-free survival (rPFS) after 6 and 12 months of treatment in COU-AA-301 (N = 1195) or COU-AA-302 (N = 1088). Eligible COU-AA-301 patients had progressed after docetaxel and had Eastern Cooperative Oncology Group performance status (ECOG PS) ≤ 2. Eligible COU-AA-302 patients had no prior chemotherapy and ECOG PS 0 or 1. Patients were treated with abiraterone acetate (1000 mg/day) plus prednisone (10 mg/day) or prednisone alone daily. Association between self-reported fatigue, pain and functional status, and OS and/or rPFS, using pooled data regardless of treatment, was assessed. Cox proportional hazard regression modeled time to death or radiographic progression. In COU-AA-301 patients, PRO improvements were associated with longer OS and longer time to radiographic progression versus worsening or stable PROs (P AA-302 patients, worsening PROs were associated with higher likelihood of radiographic progression (P ≤ 0.025) compared with improved or stable PROs. In multivariate models, worsening PWB remained associated with worse rPFS. The 12-month analysis confirmed the 6-month results. PROs are significantly associated with clinically relevant time-to-event efficacy outcomes in clinical trials and may complement and help predict traditional clinical practice methods for monitoring patients for disease progression. © The Author 2017. Published by Oxford University Press on behalf of the European Society for

  11. Effect of gaussian beam on microstructural and mechanical properties of dissimilarlaser welding ofAA5083 and AA6061 alloys

    Science.gov (United States)

    Srinivas, B.; Cheepu, Muralimohan; Sivaprasad, K.; Muthupandi, V.

    2018-03-01

    The present study focuses on a sheet thickness of 4 mm using different laser power and welding rate by the laser beam welding (LBW) at a beam size180 μm. The observations on the weldments are showing that thermal conductivity of the materials plays a major role on microstructural changes. The as-welded mechanical properties were studied by correlation with its microstructures. Due to the steeper temperature gradient during the laser beam welding AA6061 was showing the greater variation compares with AA5083 side in the micro hardness studies.Also, the tensile strength of 241 MPa has been reported as highest with the welds made of laser powerat 3.5 kW and welding rate at 3.5 mmin-1.

  12. Raadioteatril elu sees. Elu sees? / Mart Aas, Tõnis Leemets ; interv. Kutt Kommel

    Index Scriptorium Estoniae

    Aas, Mart

    2007-01-01

    Eesti Raadio raadioteatri 78. sünnipäeval esietendus Vikerraadios dokumentaalkuuldemäng "Elu sees" Aleksander Alleni (hilisema nimega Aleksander Aas) mälestuste põhjal. Theatrumi lavastuse on raadiole seadnud Mart Aas, Marius Peterson, Toomas Lõhmuste ja Tõnis Leemets

  13. AAS Publishing News: Astronomical Software Citation Workshop

    Science.gov (United States)

    Kohler, Susanna

    2015-07-01

    Do you write code for your research? Use astronomical software? Do you wish there were a better way of citing, sharing, archiving, or discovering software for astronomy research? You're not alone! In April 2015, AAS's publishing team joined other leaders in the astronomical software community in a meeting funded by the Sloan Foundation, with the purpose of discussing these issues and potential solutions. In attendance were representatives from academic astronomy, publishing, libraries, for-profit software sharing platforms, telescope facilities, and grantmaking institutions. The goal of the group was to establish “protocols, policies, and platforms for astronomical software citation, sharing, and archiving,” in the hopes of encouraging a set of normalized standards across the field. The AAS is now collaborating with leaders at GitHub to write grant proposals for a project to develop strategies for software discoverability and citation, in astronomy and beyond. If this topic interests you, you can find more details in this document released by the group after the meeting: http://astronomy-software-index.github.io/2015-workshop/ The group hopes to move this project forward with input and support from the broader community. Please share the above document, discuss it on social media using the hashtag #astroware (so that your conversations can be found!), or send private comments to julie.steffen@aas.org.

  14. Microstructural characterisation of friction stir welding joints of mild steel to Ni-based alloy 625

    Energy Technology Data Exchange (ETDEWEB)

    Rodriguez, J. [Brazilian Nanotechnology National Laboratory (LNNano), P.O. Box 6192, Campinas, SP (Brazil); University of Campinas (UNICAMP), Campinas, SP (Brazil); Ramirez, A.J., E-mail: ramirezlondono.1@osu.edu [Brazilian Nanotechnology National Laboratory (LNNano), P.O. Box 6192, Campinas, SP (Brazil); University of Campinas (UNICAMP), Campinas, SP (Brazil); Department of Materials Science and Engineering, The Ohio State University — OSU, Columbus, OH 43221 (United States)

    2015-12-15

    In this study, 6-mm-thick mild steel and Ni-based alloy 625 plates were friction stir welded using a tool rotational speed of 300 rpm and a travel speed of 100 mm·min{sup −1}. A microstructural characterisation of the dissimilar butt joint was performed using optical microscopy, scanning and transmission electron microscopy, and energy dispersive X-ray spectroscopy (XEDS). Six different weld zones were found. In the steel, the heat-affected zone (HAZ) was divided into three zones and was composed of ferrite, pearlite colonies with different morphologies, degenerated regions of pearlite and allotriomorphic and Widmanstätten ferrite. The stir zone (SZ) of the steel showed a coarse microstructure consisting of allotriomorphic and Widmanstätten ferrite, degenerate pearlite and MA constituents. In the Ni-based alloy 625, the thermo-mechanically affected zone (TMAZ) showed deformed grains and redistribution of precipitates. In the SZ, the high deformation and temperature produced a recrystallised microstructure, as well as fracture and redistribution of MC precipitates. The M{sub 23}C{sub 6} precipitates, present in the base material, were also redistributed in the stir zone of the Ni-based alloy. TMAZ in the steel and HAZ in the Ni-based alloy could not be identified. The main restorative mechanisms were discontinuous dynamic recrystallisation in the steel, and discontinuous and continuous dynamic recrystallisation in the Ni-based alloy. The interface region between the steel and the Ni-based alloy showed a fcc microstructure with NbC carbides and an average length of 2.0 μm. - Highlights: • Comprehensive microstructural characterisation of dissimilar joints of mild steel to Ni-based alloy • Friction stir welding of joints of mild steel to Ni-based alloy 625 produces sound welds. • The interface region showed deformed and recrystallised fcc grains with NbC carbides and a length of 2.0 μm.

  15. Overall view of AA (Bld 193)

    CERN Multimedia

    1980-01-01

    See under 7911303, 7911597X, 8004261 and 8202324. For photos of the AA in different phases of completion (between 1979 and 1982) see: 7911303, 7911597X, 8004261, 8004608X, 8005563X, 8005565X, 8006716X, 8006722X, 8010939X, 8010941X, 8202324, 8202658X, 8203628X .

  16. The use of CR1aa for ovine in vitro embryo production

    Directory of Open Access Journals (Sweden)

    Yulnawati

    2006-06-01

    Full Text Available The aim of this study was to investigate the capacity of CR1aa as a simple medium for maturation, fertilization and culture of ovine embryo in vitro. Oocytes were collected by slicing method in Phosphate Buffer Saline (PBS supplemented with 5% Fetal Bovine Serum (FBS and 100 IU/ml penicillin streptomycin. Oocytes were matured in Tissue Culture Medium (TCM-199 as control or CR1aa as treatment medium. Both maturation medium were supplemented with 10% Fetal Bovine Serum (FBS, 10 IU/ml Follicle Stimulating Hormone (FSH, 10 IU/ml Luteinizing Hormone (LH, 1 μg/ml Estradiol and 100 IU/ml penicillin-streptomycin. Oocytes were incubated in 5% CO2 incubator, 38˚C for 24 h. Matured oocytes were fertilized in BO or CR1aa medium, supplemented with 2.5 mM caffeine benzoate and 20 mg /ml heparin. After 18 h in vitro fertilization, oocytes were cultured in TCM-199 or CR1aa medium, both supplemented with 5% FBS, 5 mg/ml insulin and 100 IU/ml penicillin streptomycin. Results showed that the highest maturation rate was found in TCM-199 medium (73.27% and significantly different (P0.05 between cleavage rate of ovine embryos in TCM-199 and CR1aa medium (39.45% vs 50.94%. In conclusion, optimum result on ovine in vitro embryo production can be achieved from a combination of TCM-199 as maturation medium and CR1aa as fertilization and culture medium.

  17. NCBI nr-aa BLAST: CBRC-MMUS-04-0013 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-MMUS-04-0013 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  18. NCBI nr-aa BLAST: CBRC-PTRO-07-0067 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-PTRO-07-0067 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  19. NCBI nr-aa BLAST: CBRC-RMAC-04-0050 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-RMAC-04-0050 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  20. NCBI nr-aa BLAST: CBRC-CFAM-12-0016 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-CFAM-12-0016 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  1. NCBI nr-aa BLAST: CBRC-ACAR-01-0845 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-ACAR-01-0845 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  2. NCBI nr-aa BLAST: CBRC-FRUB-02-0074 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-FRUB-02-0074 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  3. NCBI nr-aa BLAST: CBRC-TBEL-01-1883 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-TBEL-01-1883 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  4. NCBI nr-aa BLAST: CBRC-LAFR-01-1734 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-LAFR-01-1734 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  5. NCBI nr-aa BLAST: CBRC-TNIG-10-0006 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-TNIG-10-0006 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  6. NCBI nr-aa BLAST: CBRC-OCUN-01-1522 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-OCUN-01-1522 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  7. NCBI nr-aa BLAST: CBRC-FCAT-01-1020 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-FCAT-01-1020 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  8. NCBI nr-aa BLAST: CBRC-GACU-18-0022 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-GACU-18-0022 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  9. NCBI nr-aa BLAST: CBRC-CJAC-01-1332 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-CJAC-01-1332 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  10. NCBI nr-aa BLAST: CBRC-TNIG-14-0023 [SEVENS

    Lifescience Database Archive (English)

    Full Text Available CBRC-TNIG-14-0023 ref|NP_031752.1| cannabinoid receptor 1 (brain) [Mus musculus] sp...|P47746|CNR1_MOUSE Cannabinoid receptor 1 (CB1) (CB-R) (Brain-type cannabinoid receptor) gb|AAD34624.1|AF153345_1 CB1 cann...abinoid receptor [Mus musculus] gb|AAA64413.1| CB1 cannabinoid receptor gb|AAA91176.1| neuronal cann...abinoid receptor emb|CAB42647.1| cannabinoid CB1 receptor [Mus musculus] gb|AAS91800.1| striatal can...nabinoid receptor type 1 protein [Mus musculus] gb|AAS91801.1| striatal cannabinoid

  11. Influence of aluminium sheet surface modification on the self-piercing riveting process and the joint static lap shear strength

    OpenAIRE

    Li, Dezhi

    2017-01-01

    Self-piercing riveting (SPR) has been widely used in automotive as one of the major joining technologies for aluminium structures due to its advantages over some of the more traditional joining technologies. Research has shown that friction is a very important factor that influences both the riveting process and the joint strength for SPR, but these influences have not been fully understood. In this paper, AA5754 sheets with different surface textures, such as original with solid wax, hot wat...

  12. Lu AA21004, a novel multimodal antidepressantwith activity exerted through serotonergic targets

    DEFF Research Database (Denmark)

    Mork, A.; Pehrson, A.; Montezinho, L. C. P.

    2012-01-01

    Background: Lu AA21004 is a multimodal antidepressant that functions as a 5-HT3 and 5-HT7 receptor antagonist, 5-HT1B receptor partial agonist, 5-HT1A receptor agonist and inhibitor of the 5-HT transporter in vitro. Here we investigated preclinical effects of Lu AA21004 1) on target occupancies, 2...... (5-HT), noradrenaline (NA), dopamine (DA), acetylcholine (ACh), histamine (Hist)] were measured by microdialysis. Antidepressant potential was assessed in the forced swim test using Flinders Sensitive Line (FSL) rats. Moreover, effects of Lu AA21004 on acquisition, consolidation and recall...

  13. AA, vacuum tank for stochastic precooling

    CERN Multimedia

    CERN PhotoLab

    1979-01-01

    The vaccum tank in which the fast stochastic precooling kicker was installed. It is clad with heating jackets for bake-out to 200 deg C, indispensable for reaching the operational vacuum of 7E-11 Torr. Alain Poncet, responsible for AA vacuum, is looking on. See also 7910268, 8002234.

  14. AAS 227: Day 2

    Science.gov (United States)

    Kohler, Susanna

    2016-01-01

    Editors Note:This week were at the 227th AAS Meeting in Kissimmee, FL. Along with several fellow authors from astrobites.com, I will bewritingupdates on selectedevents at themeeting and posting at the end of each day. Follow along here or atastrobites.com, or catch ourlive-tweeted updates from the@astrobites Twitter account. The usual posting schedule for AAS Nova will resumenext week.Welcome to Day 2 of the winter American Astronomical Society (AAS) meeting in Kissimmee! Several of us are attending the conference this year, and we will report highlights from each day here on astrobites. If youd like to see more timely updates during the day, we encourage you to follow @astrobites on twitter or search the #aas227 hashtag.Plenary Session: Black Hole Physics with the Event Horizon Telescope (by Susanna Kohler)If anyone needed motivation to wake up early this morning, they got it in the form of Feryal Ozel (University of Arizona) enthralling us all with exciting pictures, videos, and words about black holes and the Event Horizon Telescope. Ozel spoke to a packed room (at 8:30am!) about where the project currently stands, and where its heading in the future.The EHT has pretty much the coolest goal ever: actually image the event horizons of black holes in our universe. The problem is that the largest black hole we can look at (Sgr A*, in the center of our galaxy) has an event horizon size of 50 as. For this kind of resolution roughly equivalent to trying to image a DVD on the Moon! wed need an Earth-sized telescope. EHT has solved this problem by linking telescopes around the world, creating one giant, mm-wavelength effective telescope with a baseline the size of Earth.Besides producing awesome images, the EHT will be able to test properties of black-hole spacetime, the no-hair theorem, and general relativity (GR) in new regimes.Ozel walked us through some of the theory prep work we need to do now in order to get the most science out of the EHT, including devising new

  15. Thermo-mechanical FE-analysis of butt-welding of a Cu-Fe canister for spent nuclear fuel

    International Nuclear Information System (INIS)

    Josefson, B.L.; Karlsson, L.; Lindgren, L.E.; Jonsson, M.

    1992-10-01

    In the Swedish nuclear waste program it has been proposed that spent nuclear fuel shall be placed in composite copper-steel canisters. These canisters will be placed in holes in tunnels located some 500 m underground in a rock storage. The canisters consists of two cylinders of 4850 mm length, one inner cylinder made of steel and one outer cylinder made of copper. The outer diameter of the canister is 880 mm and the wall thickness for each cylinder is 50 mm. At the storage, the steel cylinder, which contains the spent nuclear fuel, is placed inside the copper cylinder. Thereafter, a copper end is butt welded to the copper cylinder using electron beam welding. To obtain penetration through the thickness with this weld method a backing ring is placed at the inside of the copper cylinder. In the present paper, the temperature, strain and stress fields present during welding and after cooling after welding are calculated numerically using the FE-code NIKE-2D. The aim is to use the results of the present calculations to estimate the risk for creep fracture during the subsequent design life. A large strain formulation is employed for the calculation of transient and residual stresses in the canister based on the calculated history of the temperature field present in the canister during the welding process. The contact algorithm available in NIKE-2D is used to detect possible contact between the steel and copper cylinders during the welding. To simplify the numerical calculations and reduce the computational time, rotational symmetry is assumed. For large gap distances between the steel and copper cylinders the residual stress field is calculated to have a shape similar to that observed in butt welded pipes with maximum axial stress values at the yield stress level. For small gap distances the backing ring will come in contact with the steel cylinder which leads to large residual stresses in the backing ring. The maximum accumulated plastic strain in the weld metal and

  16. Joint Cementation of liquid and solid radioactive waste in decommissioning of atomic objects

    International Nuclear Information System (INIS)

    Varlakov, A.; Varlakova, G.; Germanov, A.; Sukhanov, L.

    2015-01-01

    Joint cementation of liquid and solid radioactive waste (RW) directly in the containers that serve as the final packaging allows the reduction of waste amounts sent for storage and disposal. In the A.A. Bochvar Research Institute we have created a mobile unit and conducted tests on joint grouting of solid RW with the use of cement mixtures prepared on the basis of liquid RW. Two variants of void filling between the fragments of solid RW in a container: pouring and impregnation were examined. Impregnation is the so-called method suggested to be used for the solid RW with small fragments and dense filling layer. In this case the gaps between the waste are filled with the cement compound by using special technological procedures, in particular, the vibration action on the container filled with waste and the use of cement mixture with high level of penetration. It was observed that the pouring method is right for the cementation of solid RW with fragment sizes not exceeding 100-150 mm. Impregnation method can be used for the joint grouting of practically all types of solid RW regardless their size and fragments homogeneity. Cementation of densely packed and large size solid RW by impregnation guarantees the joint grouting of the lower layers of the waste in the container and can be controlled by determination of the impregnation degree and density of the cement mixture that passed through the waste layer

  17. Vip3Aa induces apoptosis in cultured Spodoptera frugiperda (Sf9) cells.

    Science.gov (United States)

    Jiang, Kun; Mei, Si-Qi; Wang, Ting-Ting; Pan, Jin-Hua; Chen, Yue-Hua; Cai, Jun

    2016-09-15

    The vegetative insecticidal proteins (Vip) secreted by many Bacillus thuringiensis strains during their vegetative growth stage are regarded as second generation insecticidal proteins, as they share no sequence or structural homology with known crystal insecticidal proteins (Cry) and have a broad insecticidal spectrum. Compared with insecticidal crystal proteins (ICPs), the insecticidal mechanisms of Vips have been little studied. Here we investigated the mechanism responsible for Vip3Aa toxicity in cultured insect cells. Using, flow cytometry analyzes, TUNEL staining and DNA fragmentation assays, we show that Vip3Aa can induce apoptosis in Spodoptera frugiperda (Sf9) cells and cause cells to arrest at the G2/M phase. We also show that Vip3Aa can disrupt mitochondrial membrane potential (ΔΨm), leading to the activation of Sf-caspase-1, suggesting that a mitochondrial mediated and caspase dependent pathway may be involved in Vip3Aa-induced apoptosis in Sf9 cells. Copyright © 2016 Elsevier Ltd. All rights reserved.

  18. Rectification induced in N2AA-doped armchair graphene nanoribbon device

    International Nuclear Information System (INIS)

    Chen, Tong; Wang, Ling-Ling; Luo, Kai-Wu; Xu, Liang; Li, Xiao-Fei

    2014-01-01

    By using non-equilibrium Green function formalism in combination with density functional theory, we investigated the electronic transport properties of armchair graphene nanoribbon devices in which one lead is undoped and the other is N 2 AA -doped with two quasi-adjacent substitutional nitrogen atoms incorporating pairs of neighboring carbon atoms in the same sublattice A. Two kinds of N 2 AA -doped style are considered, for N dopants substitute the center or the edge carbon atoms. Our results show that the rectification behavior with a large rectifying ratio can be found in these devices and the rectifying characteristics can be modulated by changing the width of graphene nanoribbons or the position of the N 2 AA dopant. The mechanisms are revealed to explain the rectifying behaviors.

  19. Cell volume regulation in hemoglobin CC and AA erythrocytes

    International Nuclear Information System (INIS)

    Berkowitz, L.R.; Orringer, E.P.

    1987-01-01

    Swelling hemoglobin CC erythrocytes stimulates a ouabain-insensitive K flux that restores original cell volume. Studies were performed with the K analog, 86 Rb. This volume regulatory pathway was characterized for its anion dependence, sensitivity to loop diuretics, and requirement for Na. The swelling-induced K flux was eliminated if intracellular chloride was replaced by nitrate and both swelling-activated K influx and efflux were partially inhibited by 1 mM furosemide or bumetanide. K influx in swollen hemoglobin CC cells was not diminished when Na in the incubation medium was replaced with choline, indicating Na independence of the swelling-induced flux. Identical experiments with hemoglobin AA cells also demonstrated a swelling-induced increase in K flux, but the magnitude and duration of this increase were considerably less than that seen with hemoglobin CC cells. The increased K flux in hemoglobin AA cells was likewise sensitive to anion replacement and to loop diuretics and did not require the presence of Na. These data indicate that a volume-activated K pathway with similar transport characteristics exists in both hemoglobin CC and AA red cells

  20. Petrographic Analysis and Geochemical Source Correlation of Pigeon Peak, Sutter Buttes, CA

    Science.gov (United States)

    Novotny, N. M.; Hausback, B. P.

    2013-12-01

    The Sutter Buttes are a volcanic complex located in the center of the Great Valley north of Sacramento. They are comprised of numerous inter-intruding andesite and rhyolite lava domes of varying compositions surrounded by a shallow rampart of associated tephras. The Pigeon Peak block-and-ash flow sequence is located in the rampart and made up of a porphyritic Biotite bearing Hornblende Andesite. The andesite blocks demonstrate a high degree of propylization in hornblende crystals, highly zoned plagioclase, trace olivine, and display a red to gray color gradation. DAR is an andesite dome located less than one mile from Pigeon Peak. Of the 15 to 25 andesite lava domes within four miles from Pigeon Peak, only DAR displays trace olivine, red to grey color stratification, low biotite content, and propylitized hornblende. These characteristic similarities suggest that DAR may be the source for Pigeon Peak. My investigation used microprobe analysis of the DAR and Pigeon Peak feldspar crystals to identify the magmatic history of the magma body before emplacement. Correlation of the anorthite zoning within the feldspars from both locations support my hypothesis that DAR is the source of the Pigeon Peak block-and-ash flow.