WorldWideScience
1

Radiation-annealing hardening of vanadium  

International Nuclear Information System (INIS)

A study is made of the mechanical properties of vanadium irradiated with fast neutrons up to dose 8.6.10"-"4 dpa, as a function of the temperature of post-radiation annealing. The radiation-annealing hardening (RAH) effect is observed at 300"oC, in agreement with previous studies. It is established for the first time that RAH is accompanied by fall in ductility. A phenomenological model is described which explains the dependence of RAH on radiation dose and temperature, as well as on the content of chemically active alloying impurities. (author).

2

Radiation-annealing hardening of vanadium  

International Nuclear Information System (INIS)

Mechanical properties of vanadium, irradiated with fast neutrons up to 8.6x10"-"4 dpa depending on postirradiation annealing temperature, are studied. It is shown that radiation-annealing hardening (RAH) is observed at 300 deg C, which agrees with earlier performed studies. It is first stated that RAH is accompanied by plasticity decrease. Phenomenological model permitting to explain RAH dependence on irradiation temperature and dose and also on content of chemically active alloying impurities is suggested.

3

U.S. Contribution 1994 Summary Report Task T12: Compatibility and irradiation testing of vanadium alloys  

Energy Technology Data Exchange (ETDEWEB)

Vanadium alloys exhibit important advantages as a candidate structural material for fusion first wall/blanket applications. These advantages include fabricability, favorable safety and environmental features, high temperature and high wall load capability, and long lifetime under irradiation. Vanadium alloys with (3-5)% chromium and (3-5)% titanium appear to offer the best combination of properties for first wall/blanket applications. A V-4Cr-4Ti alloy is recommended as the reference composition for the ITER application. This report provides a summary of the R&D conducted during 1994 in support of the ITER Engineering Design Activity. Progress is reported for Vanadium Alloy Production, Welding, Physical Properties, Baseline Mechanical Properties, Corrosion/Compatibility, Neutron Irradiation Effects, Helium ...

1995-03-01

4

Medium carbon vanadium micro alloyed steels for drop forging  

International Nuclear Information System (INIS)

Growing competitiveness of alternative manufacturing routes requires cost minimization in the production of drop forged components. The authors analyse the potential of medium carbon, vanadium microalloyed steels for drop forging. Laboratory and industrial experiments have been carried out emphasizing deformation and temperature cycles, strain rates and dwell times showing a typical processing path, associated mechanical properties and corresponding microstructures. The steels the required levels of mechanical properties on cooling after forging, eliminating subsequent heat treatment. The machinability of V-microalloyed steels is also improved when compared with plain medium carbon steels. (author)

5

Development of zirconium alloys. Part II  

Science.gov (United States)

A number of alloys of zirconium have been investigated as part of a program aimed at improving the high-temperature tensile and creep strength of zirconium. These alloys include aluminum, beryllium, lead, magnesium, molybdenum, niobium, tantalum, tin, titanium, tungsten, vanadium, and zinc, binary and ternary alloys. The data indicate that aluminum, lead, molybdenum niobium, tin, titanium, tungsten, and vanadium can be used successfully to harden zirconium, and that aluminum, tin, titanium, and vanadium are particularly effective in maintaining the strength of zirconium at elevated temperatures.

1952-01-02

6

Modified 9Cr-1Mo steel shows excellent potential for steam generator applications  

Energy Technology Data Exchange (ETDEWEB)

A 9Cr-1Mo steel with properties improved over other ferritics in the ranges from 9 to 12% Cr and 1 to 2% Mo and over the widely used 2 1/2 Cr-1Mo steel has recently been developed. The main changes in the modified alloy, compared with the standard alloy, include: addition of niobium and vanadium, to improve the alloy's elevated-temperature strength properties; a specified range for each element; and a specification for nitrogen, which is not listed for the standard 9Cr-1Mo. Microstructural work has indicated that the improved strength of the modified alloy comes from two factors: (1) fine M/sub 23/C/sub 6/ precipitate particles nucleate on Nb/C, N, which comes out first during the heat treatment; and (2) the vanadium enters M/sub 23/C/sub 6/ and retards its growth at the service temperature. Mechanical properties discussed were ...

1982-12-01

7

Microstructural and Mechanical Characterization of Actively Brazed Alumina Specimens  

Energy Technology Data Exchange (ETDEWEB)

Alumina (94 and 99.8% grade compositions) was brazed directly to itself with gold-based active brazing alloys (ABA's) containing vanadium additions of 1,2 and 3 weight percent. The effects of brazing conditions on the joint properties were investigated. Wetting behavior, interfacial reactions, microstructure, hermeticity and tensile strength were determined. Wetting was fair to good for the ABA and base material combinations. Microanalysis identified a discontinuous Al-V-O spinel reaction product at the alumina-braze interface. Tensile strength results for 94% alumina were uniformly good and generally not sensitive to the vanadium concentration, with tensile values of 85-105 MPa. There was more variability in the 99.8% alumina strength results, with values ranging from 25-95 MPa. The highest vanadium concentration (3 wt. %) yielded the highest joint strength for the brazed 99.8% alumina. ...

1999-08-26

9

Modification of surface properties of copper-refractory metal alloys  

Energy Technology Data Exchange (ETDEWEB)

The surface properties of copper-refractory metal (CU-RF) alloy bodies are modified by heat treatments which cause the refractory metal to form a coating on the exterior surfaces of the alloy body. The alloys have a copper matrix with particles or dendrites of the refractory metal dispersed therein, which may be niobium, vanadium, tantalum, chromium, molybdenum, or tungsten. The surface properties of the bodies are changed from those of copper to that of the refractory metal.

1993-10-12

10

Structural features of twins in transition class alloy Ti-Al-Mo-V-Cr  

International Nuclear Information System (INIS)

The alloy of Ti-Al-Mo-V-Cr system is studied for its structure in a strained state and specific features of #beta#-#alpha# transformation in a #beta#-matrix and deformation twins on ageing. It is determined that preliminary deformation initiates the decomposition of solid solution on aging. In a metastable #beta#-titanium alloy the substructure of deformation twins is shown to vary essentially with aluminium and chromium partial substitution for molybdenum and vanadium

1999-11-01

11

Titanium Alloys for Medical Instrumentation  

International Science & Technology Center (ISTC)

The New Titanium Alloys With Increased Mechanical Properties and Corrosion Resistance for Medical Instruments and their Coatings

12

Tungsten coating on low activation vanadium alloy by plasma splay process  

International Nuclear Information System (INIS)

Tungsten (W) coating on fusion candidate V-4Cr-4Ti (NIFS-HEAT-2) substrate was demonstrated with plasma spray process for the purpose of applying to protection of the plasma facing surface of a fusion blanket. Increase in plasma input power and temperature of the substrate was effective to reduce porosity of the coating, but resulted in hardening of the substrate and degradation of impact property at 77 K. The hardening seemed to be due to contamination with gaseous impurities and deformation by thermal stress during the coating process. Since all the samples showed good ductility at room temperature, further heating seems to be acceptable for the vanadium substrate. The fracture stress of the W coating was estimated from bending tests as at least 313 MPa, which well exceeds the design stress for the vanadium structure in fusion blanket. (author)

2008-03-01

13

Investigation of Destruction Mechanisms in Reactor Steels  

International Science & Technology Center (ISTC)

Investigation of Destruction Mechanisms in Reactor Steels and Alloys under Cycling Deformation

14

Elastic constants and volume changes associated with two high-pressure rhombohedral phase transformations in vanadium  

Energy Technology Data Exchange (ETDEWEB)

We present results from ab-initio electronic-structure calculations of mechanical properties of the rhombohedral phase of vanadium reported in recent experiments (R Ia), and other predicted high-pressure phases (R Ib and bcc), focusing on properties relevant to dynamic experiments. We find that of the three transitions the largest volume collapse (1.3%) is for the R Ia to R Ib transition. Calculations of the single crystal and polycrystal elastic constants reveal a remarkably small discontinuity across the phase transitions even at zero temperature where the transitions are first order.

2007-10-16

15

Flux pinning and critical currents in A-15 superconductors  

Science.gov (United States)

The relationship between processing, microstructure, and properties was studied for A-15 compounds in multifilamentary composites produced by solid-state diffusion and in thin-film samples produced by vapor deposition. Grain sizes of A-15 superconducting compounds were measured by transmission electron microscopy of multifilamentary composites reacted at various temperatures. Critical current densities at 4.2 K and fields up to 6 T were found to be similar for niobium-tin, vanadium-gallium, and vanadium-silicon of the same grain size. Study of the Cu-V-Si phase diagram led to the production of improved multifilamentary vanadium-silicon conductors. The effects of various alloying elements on A-15 layers produced by solid-state diffusion were studied. The most promising new observation was that tantalum can be incorporated into niobium-tin reaction layers, leading to an enhancement of critical currents at ...

1978-02-01

16

Characteristics of the Mechanical Properties and the Fractures ...  

Science.gov (United States)

... Accession Number : ADA136144. Title : Characteristics of the Mechanical Properties and the Fractures of an Alpha Beta Titanium Alloy,. ...

1983-11-18

19

Hydrogen effect or texture and deformation mechanism in #beta#-titanium alloy cold rolling  

International Nuclear Information System (INIS)

The relationships of hydrogen alloyed #beta#-titanium alloy deformation behaviour to its microstructure and texture are investigated. It is shown that plasticity increases and strain induced texture changes at low hydrogen contents (0.1-0.2 mass %). Possible mechanisms responsible for specific features of #beta#-Ti alloy deformation are discussed. The study is made using alloy VT35 doped with hydrogen

1999-09-01

21

Neutronic aspects of the safety and environmental performance of silicon carbide as blanket structural material  

Energy Technology Data Exchange (ETDEWEB)

Safety and environmental assessments have been made of conceptual fusion power plant designs employing silicon carbide composites (SiC/SiC) as the first wall and blanket structure material. These have used similar analysis methods to earlier studies of designs based on vanadium alloy or low-activation martensitic steel, allowing direct comparisons. The very low short-term activation of silicon carbide results in an almost insignificant level of decay heat in postulated loss of coolant accidents, and a lower {gamma}-dose rate on the timescale of relevance to handling for maintenance operations. However on the longer time-scale, of interest in possible recycling operations, decommissioning and waste management, SiC/SiC appears to perform no better than vanadium alloy or low-activation martensitic steel, due in part to the activation of impurities in a realistic composition. Furthermore, its increased ...

2001-04-01

22

Structure and Mechanical Properties of Boron-Doped Cubic ...  

Science.gov (United States)

... by the boron doping in most of the alloys except for Al66Mn9Zr25 + 50 ppm B alloy; permanent deformation at ultimate compressive strength is not ...

23

Phase diagrams  

International Nuclear Information System (INIS)

The description is presented of binary phase diagrams of titanium alloyed with the following elements: silver, aluminium, arsenic, gold, boron, barium, beryllium, bismuth, carbon, calcium, cadmium, cobalt, chromium, copper, iron, gallium, germanium, hydrogen, hafnium, indium, iridium, potassium, lithium, magnesium, manganese, molybdenum, nitrogen, sodium, niobium, nickel, oxygen, osmium, phosphorus, lead, palladium, platinum, plutonium, rhenium, lanthanium, cerium, preseodymium, neodymium, gadolinium, erbium, terbium, thulium, lutetium, rhodium, ruthenium, scandium, silicon, tin, strontium, tantalum, technetium, thorium, uranium, vanadium, tungsten, yttrium, ytterbium, zinc and zirconium.

24

Studies of superconducting A-15 vanadium-based alloys  

Science.gov (United States)

Superconductivity of binary alloys spanning the A-15 compounds V/sub 3/Si, V/sub 3/Ge, V/sub 3/Ga, and V/sub 3/Al and the pseudobinary derivatives of these stoichiometric compounds was surveyed by studying samples prepared by rf-sputtering from alloy cathodes. The possible formation of the hypothetical A-15 binaries ''V/sub 3/P,'' ''V/sub 3/B,'' and ''V/sub 3/C'' and their pseudobinary formation with V/sub 3/Si was also explored. Efforts to form these hypothetical alloys were not successful. The T/sub c/'s were measured resistively and the structure and lattice constants were determined by x-ray analysis. A maximum T/sub c/ of 11.7/sup 0/K was obtained for A-15 V/sub 3/Al, and the importance of a suitable deposition temperature and high sputtering pressures was examined. It is proposed that large variations ...

1976-05-01

25

Studies of superconducting A-15 vanadium-based alloys  

International Nuclear Information System (INIS)

Superconductivity of binary alloys spanning the A-15 compounds V_3Si, V_3Ge, V_3Ga, and V_3Al and the pseudobinary derivatives of these stoichiometric compounds was surveyed by studying samples prepared by rf-sputtering from alloy cathodes. The possible formation of the hypothetical A-15 binaries ''V_3P,'' ''V_3B,'' and ''V_3C'' and their pseudobinary formation with V_3Si was also explored. Efforts to form these hypothetical alloys were not successful. The T/sub c/'s were measured resistively and the structure and lattice constants were determined by x-ray analysis. A maximum T/sub c/ of 11.7"0K was obtained for A-15 V_3Al, and the importance of a suitable deposition temperature and high sputtering pressures was examined. It is proposed that large variations of T/sub c/ among pseudobinary alloys imply a rapid variation of the density of states at the Fermi level.

26

Fundamental reasons for the good performance of Alloy 800 in nuclear steam generators  

Energy Technology Data Exchange (ETDEWEB)

It is hypothesized that the good performance of Alloy 800 in steam generator service is due to its relative immunity to two distinct mechanisms of stress corrosion cracking; the argument also applies to intergranular corrosion. One mechanism operates in the high-nickel region (Alloy 600 and nearby model alloys) and is due to internal intergranular oxidation. The other operates in the low-nickel (stainless steel) region and is due to de-alloying of Fe and/or Cr. This latter mechanism may, under special conditions, operate in high-Ni, high-Cr alloys such as 690. Some essential features of the de-alloying mechanism are demonstrated using strong caustic solutions, and the prospect of extending this approach to dilute high-temperature environments is discussed. (author)

2007-07-01

27

Microstructure and properties of ultrafine WC-10Co composites with chemically doped VC  

British Library Electronic Table of Contents (United Kingdom)

Vanadium carbide is the most effective grain growth inhibitor for ultrafine WC-Co composites due to its high solubility and mobility in the cobalt phase at relatively low temperatures; however, there are still some debates over the best way to introduce it into the WC-Co formulation. In this paper, the differences between admixed and chemically doped grain growth inhibitors on the microstructural development and properties of an ultrafine WC-10Co composite are discussed. The densification rate of chemically doped samples is slower in the early stage of sintering and the WC grain sizes of the sintered alloys are finer than those of admixed samples, leading to the increase of hardness and transverse rupture strength of the sintered alloys. The effectiveness of the chemically doped inhibitor ...

2011-01-01

28

Improvement of structure and mechanical properties of cast titanium alloys using rapid heat treatment  

Energy Technology Data Exchange (ETDEWEB)

The possibility of rapid heat treatment (RHT) application to titanium castings has been studied. It was shown that such treatment provides a significant improvement of intragrain structure and mechanical properties of cast ({alpha}+{beta})-titanium alloys. ((orig.))

1995-01-01

29

Grain boundaries structure and mechanical properties of aluminium alloys  

Energy Technology Data Exchange (ETDEWEB)

The paper discusses the problem of influence of grain boundaries structure on mechanical properties of aluminium alloys at elevated temperatures. Showed the data amount of grain boundaries close to special and a random of grain boundaries. The results of calculation of contribution of different mechanisms of deformation to the total deformation for alloys with different types of grain boundaries are given. (orig.)

1996-08-01

30

Trace metal characterization of the U-Al matrix by atomic spectroscopy  

International Nuclear Information System (INIS)

Uranium-aluminum alloys with a significant enrichment of uranium with "2"3"3U or "2"3"5U serve as nuclear fuels in research reactors. The quality assurance of this fuel requires, among other things, precise knowledge that all trace metal constituents that affect neutron economy, fuel integrity, and fuel fabrication process parameters are well within the specification limits. Trace metal characterization of "2"3"5U-Al alloy has been carried out by atomic spectrometry. The trace metal constituents of interest are grouped into common metals (silver, boron, calcium, cadmium, cobalt, chromium, copper, iron, magnesium, manganese, molybdenum, sodium, nickel, lead, silicon, tin, titanium, vanadium, tungsten, and zinc) and lanthanides (cerium, dysprosium, europium, gadolinium, holminium, lutetium, samarium, and terbium). The elements yttrium and zirconium are grouped with the latter in view of the chemical separation procedure used. ...

31

Heat resistant nickel base alloy excellent in workability and high temperature strength properties  

Energy Technology Data Exchange (ETDEWEB)

A heat resistant nickel base alloy which is excellent in not only hot and cold workability but also high temperature strength properties and which also possesses satisfactory oxidation resistance. The nickel base alloy consists essentially of 0.001-0.15 percent carbon, 0.0005-0.05 percent calcium, 20.0-126.0 percent chromium, 4.7-9.4 percent cobalt, 5.0-16.0 percent molybdenum, 0.5-4.0 percent tungsten, with the total of molybdenum plus tungsten being from 9.0 to 16.5 percent, and the balance nickel and inevitable impurities. The alloy may further contain one selected from the group consisting of (1) 0.3-1.5 percent aluminum and 0.1-1.0 percent titanium, (2) 0.001-0.30 percent at least one of yttrium and rare earth elements, and (3) 0.001-1.0 percent at least one of niobium, vanadium and tantalum, whereby the aforementioned characteristics are further enhanced.

1984-10-02

32

Hydrogen in titanium alloy with 16 at% Mo  

International Nuclear Information System (INIS)

The effect of various hydrogen concentrations on the crystal lattice period and the hardness of titanium alloy was examined, the alloy containing about 16 at.% Mo (27.5 wt. % Mo) and having #beta# structure. The peculiar features of the mechanism of plastic deformation of the alloy were studied after adding hydrogen to it. A dependence of the crystal lattice period on the concentration of hydrogen was obtained for TixMoxH_2 alloy. It has been established that the hardness of the Ti-Mo alloy does not change when hydrogen is added to it. The presence of hydrogen introduces changes into the mechanism of deformation of #beta#-titanium alloy. The configuration of the inverse pole figures after rolling proves that the transverse slip process in an alloy with hydrogen is hampered, and that the coplanar slip ...

33

Quench effect on mechanical properties and structure of the TS6 #beta#-titanium alloy  

International Nuclear Information System (INIS)

By the methods of microstructural and electron-microscopic analyses by the tension test and impact test studied is the effect of quenching conditions on structure and mechanical properties of the TS6 titanium-#beta# alloy. It is shown that low temperature quenching from 700 deg C, recommended earlier for analogous VT15 titanium alloy, leads to appearence of intercrystalline fracture and to sharp decrease of impact strength of the TS6 alloy. Established are optimum conditions for quenching of half-finished products and articles of the TS6 alloy depending on their subsequent working or operation.

34

Mechanical properties, fracture surface characterization, and microstructural analysis of six noble dental casting alloys  

British Library Electronic Table of Contents (United Kingdom)

Statement of problem Because noble dental casting alloys for metal ceramic restorations have a wide range of mechanical properties, knowledge of these properties is needed for rational alloy selection in different clinical situations where cast metal restorations are indicated. Purpose The purpose of this study was to compare the mechanical properties and examine both the fracture and polished surfaces of 6 noble casting alloys that span many currently marketed systems. Five alloys were designed for metal ceramic restorations, and a sixth Type GPT has Type IV alloy for fixed prosthodontics (Maxigold KF) was included for comparison. Material and methods Specimens (n=6) meeting dimensional requirements for ISO Standards 9693 and 8891 were loaded to failure in tension using a universal testin...

2011-01-01

35

Anisotropy of the structure and mechanical properties of low-alloy tungsten  

Energy Technology Data Exchange (ETDEWEB)

The authors examine the relationship of the structure and mechanical properties of similar alloys of tungsten with rhenium produced by the powder metallurgy method by sintering powders. Since the alloys were deformed by rolling, we examine the effect of the resultant anisotropy of the structure on the properties of the metal in various directions. The tests were conducted on an alloy of tungsten with 2 wt.% rhenium and, for comparison purposes, an alloy of tungsten with additions of oxides of yttrium and hafnium. The mechanical properties of the alloys, i.e., strength, cracking resistance, cold shortness temperature, were determined in the bend test. Structural examination was carried out using an optical microscope, electron scanning microscopy, and the method of transmission electron microscopy.

1987-12-01

36

Effect of the molybdenum content and of further factors on the creep strength of high-temperature, CrMoV alloy tube steels. [chemical composition of the steels 0,4-1,2% Cr, 0,2-1% Mo, 0,15-0,3% V  

Energy Technology Data Exchange (ETDEWEB)

With regard to long-term high-temperature strength, molybdenum is an effective alloying element but rather expensive as well. The author describes its influence on high-temperature strength properties of CrMoV alloyed steel. Besides molybdenum, also vanadium and carbon have an increasing effect on limiting rupture stress which furthermore may be effected by heat treatment, the cooling rate being a dominating factor in this process. To guarantee optimum long-term high-temperature strength properties, a minimum of a least 0.5% Mo and 0.35% V is required. The cooling rate after austentizing must be high enough to enable transformation in the bainitic structure to take place. A two-to-three-hour tempering treatment at about 720/sup 0/C is regarded as an optimum.

1988-07-01

37

Carbon effect on the structure and plasticity characteristics of titanium #beta#-alloys  

International Nuclear Information System (INIS)

In this paper a study is made of the structure and mechanical properties of the #beta# alloy system Ti-Mo-Zr-Sn (the composition of which is equivalent to the #beta# III alloy used abroad) containing different amounts of carbon. Study of the #beta#-titanium alloy containing 0.1% C revealed the presence of particles of titanium carbide. Separation of the titanium carbide promotes a reduction in impact strength, an increased tendency toward cold shortness, and poorer workability. (author).

38

Mechanical properties of (alpha+beta)-titanium alloys with various structure within the temperature range of 20 to -196 deg C  

International Nuclear Information System (INIS)

The influence of structure on mechanical properties in the course of tensile tests in a wide range of temperatures was studied, using the VT16 structure thermally strengthened (alpha+beta)-titanium alloy by way of example. It is ascertained that transition from ductile to brittle fracture at the temperature of -196 deg C is observed only in coarse-grain alloy having alpha-eldging of beta grains.

39

Effect of cooling conditions during heat treatment on mechanical properties of titanium alloy VT3-1  

International Nuclear Information System (INIS)

Effect of cooling rates within the wide range (0.003-45 grad/s) on the complex of mechanical properties of (#alpha#-#beta#)-titanium alloy VT3-1 is studied in the process of heat treatment. Cooling conditions of semifinished product made of this alloy with a different structure providing optimum combination of strength, ductility fracture toughness, heat resistance, and endurance are determined.

40

TEM and ToF-SIMS studies on the corrosion behavior of vanadium and chromium containing WC-Co hard metals in alkaline solutions  

British Library Electronic Table of Contents (United Kingdom)

The corrosion behavior of hard metals with VC and Cr3C2 grain growth inhibitors was investigated in alkaline solutions by electrochemical methods. The two inhibitors have opposite effects on the corrosion behavior: Cr3C2 significantly improves the corrosion behavior, whereas VC-containing alloys show a poor resistance. Time-of-flight secondary ion mass spectrometry (ToF-SIMS) and analytical transmission electron microscopy (TEM) analyses of the distributions of Cr and V in the composite material, as well as in the surface layers formed during corrosion were employed to clarify the influence of these elements on the corrosion behavior. The measurements showed that VC is precipitated mostly along the WC/binder interface after the liquid-phase sintering process, while Cr3C2 is almost homogene...

2011-01-01

41

Selective oxidation of n-butane and butenes over vanadium-containing catalysts  

Science.gov (United States)

The oxidative dehydrogenation (OXDH) of n-butane, 1-butene, and trans-2-butene on different vanadia catalysts has been compared. MgO, alumina, and Mg-Al mixed oxides with Mg/(Al + Mg) ratios of 0.25 and 0.75 were used as supports. The catalytic data indicate that the higher the acid character of catalysts the lower is both the selectivity to C{sub 4}-olefins from n-butane and the selectivity to butadiene from both 1-butene or trans-2-butene. Thus, OXDH reactions are mainly observed from n-butane and butenes on basic catalysts. The different catalytic performance of both types of catalysts is a consequence of the isomerization of olefins on acid sites, which appears to be a competitive reaction with the selective way, i.e., the oxydehydrogenation process by a redox mechanism. Infrared spectroscopy data of 1-butene adsorbed on supported vanadium oxide catalysts suggest the presence of different adsorbed species. O-containing species (carbonyl and ...

2000-01-01

42

An investigation of the production of thin films of some materials which undergo phase transitions for optical applications  

CERN Document Server

The aim of this work was to study the possibility of producing a fast switching optical thin film device to react to laser radiation in the visible/near infrared region of the spectrum. The switching mechanism was to be thermally driven. A computer program was written to enable the effects of changes of the refractive index of a component of a multilayer thin film stack to be modelled. Attempts to use the phase transition in vanadium dioxide were unsuccessful because, in the spectral region of interest, the 'open-state' absorption was too great. A class of materials known as 'the bronzes' was identified as being potentially useful. Attempts were made to produce thin films of bronze compounds of vanadium, tungsten and molybdenum by the techniques of conventional thermal evaporation and laser ablation for further studies. The former technique appeared to suffer from problems of decomposition of the source material. The latter ...

1995-01-01

43

Effect of cross rolling parameters on texture formation and parameters on texture formation and anisotropy of mechanical properties of (#alpha#+#beta#)-titanium alloy sheets  

International Nuclear Information System (INIS)

Formation of basis type texture at rolling of Ti + 6.0% Al + 1.5% V + 1.0% Mo system alloy with initial prismatic texture is investigated by means of X-ray techniques. Variations of mechanical features in titanium alloy sheets depending on temperature-deformation conditions of rolling are investigated. Main conditions for formation of the intensive basis textute in the investigated alloy sheets which provides for isotropic properties in sheet plane and for increased ductility are determined.

44

Summary on performance study of corrosion resistance of zirconium alloys  

International Nuclear Information System (INIS)

Zirconium-base alloys are used primarily as fuel cladding material and other core structure material in water cooled nuclear power reactors. Main research achievements and problems about corrosion of zirconium alloys are reviewed; the present theories and challenge are summarized. In the 1980s, great progress had been made towards correlating alloy composition, microstructure and irradiation with corrosion resistance. In the 1990s, main researches are focused on exploring actual mechanism of corrosion, optimizing both alloy composition and microstructure in order to minimize the fuel cycle costs through burnup optimization.

45

SP-700 titanium alloy data sheets  

International Nuclear Information System (INIS)

SP-700, an emerging #beta#-rich #alpha#+#beta# titanium alloy, is designed to improve superplastic formability as well as mechanical properties over Ti-6Al-4V alloy. Owing to its fine microstructure and low #beta#-transus temperature, it is superplastic-formable at temperature below 1,073K (800 C) with low flow stress. Remarkable workability of this alloy is also retained in conventional Manufacturing processes. Another advantage of SP-700 is heat treatment response which includes deep hardenability and quick aging kinetics. Corrosion resistance and machinability are equivalent to or better than Ti-6Al-4V alloy.

1993-02-21

46

Mechanisms of Alloy 800 corrosion in helium  

International Nuclear Information System (INIS)

Cr_2O_3 scales are found to form on Alloy 800 and a similar pure ternary alloy in air, and 1 and 50 atm. helium containing oxidizing impurities typical of those in an SGHTR. The strong temperature dependence and neglibible helium overpressure dependence indicate that gas transport through the scales is not rate controlling. Surface oxidation rates are therefore controlled by solid state diffusion and the low oxygen partial pressure dependence of the oxidation rate in Alloy 800 is ascribed to the presence of extrinsic defects in the Cr_3O_3 (due to doping by alloying elements) or to the presence of short circuit diffusion paths. (Auth.).

47

Nickel base alloys for future steam turbines  

International Nuclear Information System (INIS)

Modern commercial alloys are not suited for future steam turbines of operating temperatures beyond 700 C. #gamma#'-hardened alloys like Waspaloy have good mechanical characteristics but have defects when large batches are melted. #gamma#'/#gamma#''-hardened alloys like Inconel 706, on the other hand, are easy to produce but have insufficient microstructural long-term stability and insufficient creep strength. Mixed crystal solidified alloys like Inconel 617 have excessive yield stress at forging temperatures. Two new alloys were therefore developed. Results so far show that they have good production characteristics but insufficient mechanical characteristics. The reasons for this are currently under investigation. (orig.)

2003-11-28

48

Irradiation-assisted stress corrosion cracking in HTH Alloy X-750 and Alloy 625  

International Nuclear Information System (INIS)

In-reactor testing of bolt-loaded compact tension specimens was performed in 360 C water to determine the irradiation-assisted stress corrosion cracking (IASCC) behavior of HTH Alloy X-750 and direct-aged Alloy 625. New data confirm previous results showing that high irradiation levels reduce SCC resistance in Alloy X-750. Heat-to-heat variability correlates with boron content, with low boron heats showing improved IASCC properties. Alloy 625 is resistant to IASCC, as no cracking was observed in any Alloy 625 specimens. Microstructural, microchemical and deformation studies were performed to characterize the mechanisms responsible for IASCC in Alloy X-750 and the lack of an effect in Alloy 625. The mechanisms under investigation are: boron transmutation effects, radiation-induced changes in ...

1995-08-06

49

Bulk amorphous and nanocrystalline Al83Fe17 alloys prepared by consolidation of mechanically alloyed amorphous powder  

British Library Electronic Table of Contents (United Kingdom)

In the present work, bulk amorphous and nanocrystalline Al83Fe17 alloys were obtained by consolidation of mechanically alloyed powders. Mechanical alloying of Al-17% Fe powder mixture yielded powder with an amorphous structure. Thermal behaviour of the milling product was examined using differential scanning calorimetry. This investigation revealed that the amorphous phase crystallised above 380^oC. The amorphous powder was compacted under a pressure of 7.7GPa in different conditions: at 380^oC for 600s and at 1000^oC for 180s. Structural investigations of the bulk material revealed that the amorphous structure was retained after consolidation process applied at 380^oC. Compaction under high pressure at 1000^oC caused crystallisation of the amorphous phase and appearance of metastable nano...

2010-01-01

50

Alloy 800 specifications in compliance with component requirements  

Energy Technology Data Exchange (ETDEWEB)

In view of the importance of the material Alloy 800 in high-temperature reactor plants (HTR), a material data bank was established which is used for statistical evaluation of mechanical and physical material behaviour. Based on investigations on the interconnection between the mechanical properties at high temperatures and the metallurgical parameters, different types of Alloy 800 were specified in compliance with the component requirements. In addition, aspects of corrosion and toughness behaviour were taken into consideration. The specifications and strength characteristics for the different variants of Alloy 800 were incorporated into draft DIN standards after discussion and approval in expert committees. Further important characteristics of the mechanical and physical material behaviour were summarized in HTR material data sheets so as to furnish an improved ...

1990-04-01

51

Alloy 800 specifications in compliance with component requirements  

International Nuclear Information System (INIS)

In view of the importance of the material Alloy 800 in high-temperature reactor plants (HTR), a material data bank was established which is used for statistical evaluation of mechanical and physical material behaviour. Based on investigations on the interconnection between the mechanical properties at high temperatures and the metallurgical parameters, different types of Alloy 800 were specified in compliance with the component requirements. In addition, aspects of corrosion and toughness behaviour were taken into consideration. The specifications and strength characteristics for the different variants of Alloy 800 were incorporated into draft DIN standards after discussion and approval in expert committees. Further important characteristics of the mechanical and physical material behaviour were summarized in HTR material data sheets so as to furnish an improved ...

53

Study of the influence of alloying additions on the passivity of aluminum. Annual report 1 Dec 89-30 Nov 90  

Energy Technology Data Exchange (ETDEWEB)

Whereas supersaturated aluminum alloys demonstrate enhanced passivity, conventional aluminum alloys spontaneously pit in air-saturated chloride solutions. We have concentrated on three areas: evaluation and characterization of Al-W alloys, which exhibit the best corrosion performance of any alloy system studied to date; characterization of the passive-film structure of Al-Mo alloys; and production and characterization of Al-W and Al-Ta powders, which will be used for compaction into bulk material. Surface analysis of the Al-W passive films formed during polarization show surprising little oxidized solute compared to other alloys. These results indicate that the barrier layer formation and electrostatic repulsion mechanisms used to explain the passivity of other alloys are not involved here. Instead the W may act to ...

1991-03-01

54

Production of powder titanium alloys with Mo, Zr, Nb additions and their properties  

International Nuclear Information System (INIS)

In order to substitute expensive cast titanium alloys by powder ones the possibility of introduction of powder additions by mechanical stock mixing is studied. It is shown that microstructure of powder alloys of Ti-Zr(1-9%) system is typical for one-phase cast #alpha#-alloys. The Ti-Mo(1-9%) and Ti-Nb(1-9%) system alloys have microstructure typical for two-phase (#alpha#+#beta#)-alloys. For homogeneous structure to be obtained the high temprature annealing is advisable after hot pressing. Alloying with Mo, Zr and Nb permits to increase considerable the strength of powder titanium products (at 9% Mo more than two times).

55

High-temperature property data: Ferrous alloys  

Energy Technology Data Exchange (ETDEWEB)

In this book over 250 alloys are organized by AISI number into 10 major sections: Irons, Carbon Steels, Alloy Steels, Low Alloy Constructional Steels, Ultra High Strength Steels, Tool Steels, Maraging Steels, Wrought Stainless Steels, Heat Resistnat Casting Alloys, and Iron Based Rought Superalloys. Each alloy record lists the designation, specifications, UNS number, composition, product forms and a comment on the high-temperature properties and applications. Referenced data is then given for physical properties such as density, specific heat, thermal conductivity, thermal expansion, electrical conductivity, Poisson's ratio, moduli of elasticity and rigidity, etc. Mechanical properties follow, and include tensile properties, shearing and bearing properties, impact properties, creep, stress rupture and stress relaxation and fatigue properties. The last ...

1987-01-01

56

Colorimetric analysis of opaque porcelain fired to different base metal alloys used in metal ceramic restorations  

British Library Electronic Table of Contents (United Kingdom)

Statement of problem. The popularity of base metal alloys has considerably increased in recent years because of their superior mechanical properties as well as the high cost of noble alloys. However, there is disagreement about their effect on the opaque porcelain color and the color differences among base metal alloys. Purpose. The purpose of this in vitro study was to determine and compare the influence of various commercially available base metal alloys (excluding titanium-based systems) on the resulting color of opaque porcelain with the use of a colorimetric device. Material and methods. Fourteen different types of Ni-Cr and 3 different types of Co-Cr porcelain bonding alloys were selected with a Au-Pd alloy (V-Delta SF) as the control group for colorimetric measurements and determina...

2008-01-01

57

High damping Fe-Mn martensitic alloys for engineering applications  

International Nuclear Information System (INIS)

Conventional methods for reducing vibration in engineering designs (i.e. by stiffening or detuning) may be undesirable or inadequate in conditions where size or weight must be minimized or where complex vibration spectra exist. Alloys which combine high damping capacity with good mechanical properties can provide attractive technical and economic solutions to problems involving seismic, shock and vibration isolation. To meet these trends, we have developed a new high damping Fe-17%Mn alloy. Also, the alloy has advantages of good mechanical properties and is more economical than any other known damping alloys (a quarter the cost of non-ferrous damping alloy). Thus, the high damping Fe-17%Mn alloy can be widely applied to household appliances, automobiles, industrial facilities and power plant components with its excellent ...

2000-06-01

60

Structure transformation and gain in properties of cast high-temperature T-6242 alloy by thermo-hydrogen treatment  

International Nuclear Information System (INIS)

Thermohydrogen treatment effect on microstructure and mechanical properties is studied for a cast heat resistant pseudo-#alpha#-titanium alloy Ti-6242 (Ti-6Al-2Sn-4Zn-2Mo) widely used as a heat resistant material with operating temperature up to 500 deg C. It is shown that reversible hydrogen alloying is a promising alternative to thermomechanical treatment for transformation of (#alpha#+#beta#)-titanium alloy structure. The application of thermohydrogen treatment is noted to be of particular efficiency for shaped casting technology as it allows a noticeable increase of mechanical properties at a lower cost. The alloy after thermohydrogen treatment and subsequent heat treatment in the (#alpha#+#beta#) - range possesses high values of yield strength fatigue properties, creep resistance and has a satisfactory ductility. A consideration is also given to ...

61

Correlation of mechanical properties with microstructure of Alloy 800 after annealing at 800 - 1000 "0C  

International Nuclear Information System (INIS)

The microstructures of so called high temperature alloys, which have been developed for service temperatures up to 800"0C, are not necessarily stable at higher temperatures. The mobility of alloying elements is very high in FeCrNi alloys at 950 "0C e.g. iron, chromium or nickel can diffuse up to 0.1 mm distance in one year, which is about a grain diameter. Interstitials like carbon or nitrogen show a four orders of magnitude higher diffusivity than the alloying elements. In addition, the carbon solubility in this type of alloy is reported to be very low. Therefore the alloys are supersaturated with carbon after heat treatment above 1100 "0C and water quenching although the absolute carbon content is very low. At service temperatures around 800"0C the solubility of carbon is still about one order of magnitude lower than at heat treatment temperature. This will ...

1981-05-01

62

Interrelation between grain boundary characteristics and intergranular stress corrosion cracking of thermally treated alloy 690 and shot peened alloy 800 in high temperature acidic and alkaline solution  

Energy Technology Data Exchange (ETDEWEB)

To clarify the acidic and alkaline Intergranular Stress Corrosion Cracking (IGSCC) mechanism of thermally treated alloy 690 (alloy 690 TT) and shot peened alloy 800 (alloy 800 SP), C-ring tests were conducted in deaerated HCl solutions and in deaerated NaOH solutions at 350degC, compared with the acidic and the alkaline IGSCC susceptibilities of mill-annealed alloy 600 (alloy 600 MA), full-sensitized one (alloy 600 FS) and thermally treated one (alloy 600 TT). Grain boundary characteristics, such as chromium depleted zone and chromium carbide precipitation, were examined using modified Huey test and Transmission Electron Microscopy. Potential-pH diagram for Ni, Cr, Fe-H{sub 2}O system at 350degC was constructed and the solubilities of NiO, Cr{sub 2}O{sub 3} and Fe{sub 3}O{sub 4} were also calculated ...

2001-05-01

63

Interrelation between grain boundary characteristics and intergranular stress corrosion cracking of thermally treated alloy 690 and shot peened alloy 800 in high temperature acidic and alkaline solution  

International Nuclear Information System (INIS)

To clarify the acidic and alkaline Intergranular Stress Corrosion Cracking (IGSCC) mechanism of thermally treated alloy 690 (alloy 690 TT) and shot peened alloy 800 (alloy 800 SP), C-ring tests were conducted in deaerated HCl solutions and in deaerated NaOH solutions at 350degC, compared with the acidic and the alkaline IGSCC susceptibilities of mill-annealed alloy 600 (alloy 600 MA), full-sensitized one (alloy 600 FS) and thermally treated one (alloy 600 TT). Grain boundary characteristics, such as chromium depleted zone and chromium carbide precipitation, were examined using modified Huey test and Transmission Electron Microscopy. Potential-pH diagram for Ni, Cr, Fe-H_2O system at 350degC was constructed and the solubilities of NiO, Cr_2O_3 and Fe_3O_4 were also calculated to evaluate the stability ...

2001-05-01

64

Pore formation during hybrid laser-tungsten inert gas arc welding of magnesium alloy AZ31B--mechanism and remedy  

International Nuclear Information System (INIS)

One of the major concerns during high speed welding of magnesium alloys is the presence of porosity in the weld metal that can deteriorate mechanical properties. This study seeks to analyze the presence method and quantity of pore during hybrid laser-tungsten inert gas arc (TIG) welding of magnesium alloy AZ31B by radiography, optical microscopy and electron probe microanalysis (EMPA). At the same time, it identifies both the mechanism of pore formation and a remedy for this problem. The experimental results indicate that lacking of shielding gas for laser beam is the dominant cause of macroporosity formation during the hybrid of laser-TIG welding of magnesium Alloys AZ31B plate, and hydrogen is not main cause to form large pores. A favorable weld without porosity can be obtained by appending lateral shielding gas for laser beam.

2005-01-15

65

Research on deformation characteristic of AZ31Mg alloy and its constitutive equations  

Energy Technology Data Exchange (ETDEWEB)

Superplasticity of polycrystalline metallic materials is a phenomenon which shows hundreds to thousands of percents of large plastic deformation without necking in a steady state of low stress, when the uni-axial tensile loading is done in some special thermo-mechanical conditions (some limited ranges of properly high temperature and low strain rate). The main mechanism of superplastic phenomenon is the grain boundary sliding, while the main mechanism of usual plastic deformation is the trans-granular sliding. In this research, the possibility of superplastic deformation in a magnesium alloy (AZ31Mg alloy) was experimentally investigated, because generally speaking, the magnesium alloy whose atomic structure is hexagonal does not have enough formability in a form of trans-granular sliding mechanism. In this paper, the detail of experimental ...

2004-07-01

66

Mechanical-thermal processing of a beta-titanium alloy  

International Nuclear Information System (INIS)

The mechanical properties of TS 6 (Ti--10 percent Cr--7 percent V--3.5 percent Mo--3 percent Al) alloy were studied. Results are presented in plots showing yield stress vs cold work, notched tensile strength vs unnotched tensile strength, and ultimate tensile strength vs test temperature.

67

An evaluation of beta titanium alloys for use in orthodontic appliances.  

Science.gov (United States)

A beta titanium alloy was evaluated for use in orthodontic appliances. Standard mechanical tests and aspecially designed spring test were used. Two particular thermo-mechanical treatments resulted in titanium springs with 1.8 times the extension of comparable stainless steel springs, and a 2.2 fold reduction in force per unit displacement. PMID:283089

1979-02-01

68

Specific features of radiation damage in titanium alpha-alloys  

International Nuclear Information System (INIS)

Titanium base 'alpha'-alloys (Pt-7M, RK-20 and Ti-5Al-2Zr-1.5V) are considered for their behaviour under neutron irradiation. The role of alloying elements in radiation hardening is discussed depending of neutron fluence and irradiation temperature. For PK-20 alloy three stages of change in mechanical properties are revealed which are following: incubation period and weak hardening, intense radiation hardening, radiation hardening attenuation. Irradiation temperature rise results in an increase of incubation period and threshold neutron fluence. A special attention is paid to hydrogen absorption in #alpha#-titanium alloys under irradiation. It is concluded that titanium base 'alpha'-alloys are serviceable as structural materials in nuclear plants with allowance made for peculiar features of their radiation behaviour. 4 refs.; 7 figs.; 1 tab.

69

Corrosion resistance of tungsten and molybdenum alloys with #approx# 30 at.% Re in nitrogen- and oxygen-containing environments  

International Nuclear Information System (INIS)

Formation kinetics and composition of products of interaction of binary and ternary tungsten-molybdenum-rhenium alloys containing 30#+-#3 at.% (27-47 weight %) Re with products of thermal dissociation of ammonia and nitrogen-oxygeneous mixtures are studied. Mo-45% Re-10%W ternary alloy occupies intermediate position between W-27%Re and Mo-47%Re binary alloys, while its corrosion resistance and corrosion nature are close to those of W-Re and mechanical features - to those of Mo-Re alloy. It is explained by the fact, that the variation of W and Mo ration occurs in thin surface layer of ternary alloys in contrast to the initial state and the enrichment of near-the-surface layer with tungsten occurs under hot and cold deformation, at aging in the air, and during oxidation-reduction treatment. 4 refs.; 7 figs.

70

The effects of high-temperature exposure on the properties of heat-resistant alloys  

Energy Technology Data Exchange (ETDEWEB)

The exposure of heat-resistant alloys to high temperature can significantly change their mechanical properties. This paper presents and analyzes data on the effect of thermal exposure on the tensile and impact behavior of three cast materials -- the HK-40, HP-50, and 21Cr-32Ni-Fe alloys -- and of wrought material -- Alloy 800. The changes in tensile and impact properties caused by high-temperature exposure are reviewed. Reasons for these property changes and needs for considering them in the design, operation, and life assessment of high-temperature equipment are discussed.

1994-12-31

71

Effect of tritium and helium-3 on the lifetime properties of Pd-Ag alloys in ITER tritium purification technology  

Energy Technology Data Exchange (ETDEWEB)

An experimental verification for long-term performance of a Pd-Ag permeation in ITER tritium fusion cleanup units (FCU) is needed. In addition, information is required on the influence of tritium and {sup 3}He decay on the physical and chemical properties of Pd-Ag alloys (V-1). The results of the investigations of alloys (V-1) (mechanical properties and microstructure) after long-term usage exposition in tritium are given in this report. The experimental conditions (temperature, pressure, clearance, {sup 3}He concentrations) and the previous conclusions on the V-1 alloy performance are presented. (orig.).

1996-10-01

72

Reversible Movement of Homogenously Nucleated Dislocations in a #beta#-Titanium Alloy  

International Nuclear Information System (INIS)

We demonstrate reversible movement of (1/2)[110](110) dislocation loops generated from nanodisturbances in a #beta#-titanium alloy. High resolution transmission electron microscope observations during an in situ tensile test found three reversible deformation mechanisms, nanodisturbances, dislocation loops and martensitic transformation, that are triggered in turn with increasing applied stress. All three mechanisms contribute to the nonlinear elasticity of the alloy. The experiments also revealed the evolution of the dislocation loops to disclination dipoles that cause severe local lattice rotations.

2009-01-30

73

On the hydrogen etching mechanism in plasma nitriding of metals  

International Nuclear Information System (INIS)

Iron alloys and aluminum were nitrogen implanted in a controlled oxygen atmosphere and the role of hydrogen on the surface etching mechanisms studied. The surface composition was analyzed by in situ photoemission electron spectroscopy (XPS). In iron alloys, hydrogen strongly etches oxygen, improving nitrogen retention on the surface. On the other hand, hydrogen removes nitrogen from aluminum surfaces, with a deleterious effect on the nitriding effectiveness. The oxygen removal in iron alloys is associated with the catalytic effect of electrons in d-orbitals and the nitrogen removal in aluminum is associated with a steric effect.

2006-12-15

74

Mechanical properties of joints welded in halogen-containing controlled atmosphere  

International Nuclear Information System (INIS)

Studied are the mechanical properties of welded joints and heat affected zones of the Kh8N10T steel and OT4 and VT1-2 titanium alloys on welding in Ar+deltaF_6 and Ar+CCl_2F_2 mixtures contributed to a decrease of porosity. Tensile and impact tests of welded joints have revealed that additions of sulfur hexafluoride into argon causes a decrease of impact strength in titanium alloy when the tensile strength does not depend on the composition of a halogen-containing atmosphere. Freon (CCl_2F_2) additions decrease only slightly the impact strength of the investigated alloys.

75

Hot workability, microstructural control and rate-controlling mechanisms in cast-homogenized AZ31 magnesium alloy  

Energy Technology Data Exchange (ETDEWEB)

Optimum conditions for microstructural control in industrial hot working of cast and homogenized AZ31 magnesium alloys are evaluated by using a processing map. The recommended window for bulk metal working of this alloy is the domain in the temperature range 300-450 C and strain rate range 1-10 s{sup -1}, and the optimum processing parameters are 400 C and 10 s{sup -1}, where grain-boundary self diffusion is the rate-controlling mechanism. (Abstract Copyright [2009], Wiley Periodicals, Inc.)

2009-03-15

76

The influence of martensitic transformation on mechanical properties of cast high alloyed CrMnNi-steel under various strain rates and temperatures  

International Nuclear Information System (INIS)

Metastable austenitic steels show excellent mechanical properties, such as high strength combined with excellent ductility and toughness due to martensitic transformation under mechanical loading (transformation induced plasticity effect). A good energy consumption, and, in the case of high-alloyed metastable austenitic steels, a high corrosion resistance, increase the potential of these materials for diverse applications, also in regard of safety requirements. Up to now, numerous wrought alloys were investigated concerning mechanical behaviour, TRIP-effect, martensitic transformation behaviour and modelling of transformation kinetics or stress-strain behaviour. New high alloyed cast CrMnNi-steels, developed at Technical University Bergakademie Freiberg, provide the chance to reduce processing steps, production time and costs. In order to understand the ...

2010-07-01

77

Hydrogen embrittlement of Ni-Cr-Fe alloys  

Energy Technology Data Exchange (ETDEWEB)

The purpose of this work was to investigate the role of chromium on hydrogen embrittlement of Ni-Cr-Fe alloys and thus to develop a better understanding of the low-temperature stress corrosion cracking (SCC) phenomenon. The effect of chromium on hydrogen embrittlement was examined using tensile tests followed by material evaluation via scanning electron microscopy (SEM) and light optical microscopy. Four alloys were prepared with chromium contents ranging from 6 to 35 wt pct. In the uncharged condition, ductility, as measured by the percent elongation or reduction in area, increased as the alloy chromium content increased. Hydrogen appeared to have only minor effects on the mechanical properties of the low-chromium alloys. The addition of hydrogen had a marked effect on the ductility of the higher-chromium alloys. In the 26 pct chromium ...

1997-03-01

78

The effect of welding processing on the creep strength of heat-resistant chromium/molybdenum/vanadium alloyed pipe steels; Einfluss der schweisstechnischen Verarbeitung auf die Zeitstandfestigkeit warmfester Chrom-Molybdaen-Vanadium-legierter Rohrstaehle  

Energy Technology Data Exchange (ETDEWEB)

This is a report on the results of creep tests of large extent on samples of welded joints. The possibilities of minimising the reduction in creep strength which occurs are also shown. The range of the pipe welded joints examined extends from superheater pipes 31.8 diam x 5 mm to hot steam pipelines 240 diam x 29 mm. The steels used are: X 20 CrMoV 12-1, X 10 CrMoVNb 9-1 and X 10 CrWMoVnB 9-2. (orig./MM) [Deutsch] Es wird ueber Ergebnisse von in groesserem Umfang laufenden Zeitstandversuchen an Proben aus Schweissverbindungen berichtet. Ausserdem werden Moeglichkeiten aufgezeigt, den eintretenden Zeitstandfestigkeitsabfall zu minimieren. Die Spanne der in Untersuchung befindlichen Rohrschweissverbindungen reicht dabei vom Ueberhitzerrohr diameter 31,8 x 5 mm bis zum Heissdampfleitungsrohr diameter 240 x 29 mm. Die verwendeten Staehle sind: X 20 CrMoV 12 -1; X 10 CrMoVnB 9-1; X 10 CrWMoVnb 9-2. (orig./MM)

1995-12-31

79

Optimization of INCOLOY alloy 800 mechanical properties for various power plant requirements  

International Nuclear Information System (INIS)

The AMSE Boiler Code development of design stresses and their optimization for alloys 800 and 800H for conventional and nuclear power plants have coincided with many successful trial installations of these grades of alloy 800. These trial installations, along with laboratory tests, have shown that alloy 800H can be used for long times with a retention of good mechanical properties, including ductility. While gamma prime can be formed, it soon loses its detrimental effect on ductility in service. Sensitization of the alloy also occurs but it, too, has a decreasing effect on corrosion resistance with time in service, especially at elevated temperatures. The authors discuss all of these aspects and conclude that alloy 800 perhaps with low carbon control in the annealed (1800 to 1950degF)(982 to 1066degC) condition gives the optimum combination of properties to ...

80

Hydrogen transport behavior of Timetal-21S alloy  

International Nuclear Information System (INIS)

Ti-15Mo-2.7Nb-3Al-0.2Si (Timetal-21S), a metastable #beta#-titanium alloy, is a candidate material for titanium matrix composite structures in hydrogen-fueled hypersonic planes because of its excellent formability and adequate mechanical properties in the 500--800 C temperature range. The alloy is strengthened through the precipitation of fine #alpha# particles in the #beta# matrix. The mechanical properties and microstructures are controlled by a solutionizing/aging heat treatment. A major concern in using titanium alloys in hydrogen service is the embrittlement caused by the precipitation of hydrides. It is believed that the large solubility of hydrogen in the #beta#-phase would preclude the precipitation of hydrides in Beta titanium alloys, especially at low hydrogen pressures. However, depending on the hydrogen content, a shift in the ductile/brittle ...

82

Electrical conductivity of the ceramic AIN under irradiation  

Energy Technology Data Exchange (ETDEWEB)

Aluminum nitride has been proposed as electrically insulating coating in connection with blankets made of vanadium alloys. Irradiations were performed with an applied DC electric field of 100 kV/m, using a 104 MeV {alpha}-particle beam. The dose achieved were 0.1 dpa at 300 C, 0.05 dpa at 400 C, and 0.06 dpa at 500 C. The out-of-beam conductivity {sigma}{sub 0} decreased at all temperatures employed during early stage of irradiation. Before 0.02 dpa had been reached, {sigma}{sub 0} dropped to low values of typically (2-4) x 10{sup -11} ({Omega} m){sup -1}. Although a moderate increase can be observed during further irradiation, {sigma}{sub 0} remained below the initial value of the unirradiated specimen for all temperatures. That is, there is no significant evidence for radiation induced electrical degradation. The in-beam conductivity {sigma}, measured continuously during irradiation, also decreased by at least one order of magnitude. Relevant ...

1996-10-01

83

Mechanical properties of Cu-Ni-Be system alloys  

International Nuclear Information System (INIS)

The effects of addition of 0.17wt%Zr, 0.1wt%Mg and 0.1wt%Co on the mechanical properties of a Cu-1.2wt%Ni-0.2wt%Be alloy have been investigated. Adding Zr, Co or Mg to the Cu-Ni-Be alloy brings about the improvement in strength and stress relaxation property. The Zr, Co or Mg addition decreases the inter-precipitate spacing of #gamma#'' precipitates, resulting in the increase in strength. The higher resistance to the stress relaxation of the Zr- or Co-added alloy is attributed to the lower density of mobile dislocations. The improvement of stress relaxation property by the Mg addition is explained by the viscous glide motion of dislocations dragging Mg atoms, in addition to the lower density of mobile dislocations.

2010-07-01

84

Fabrication of titanium components close to the final shape; Endkonturnahe Fertigung von Titanbauteilen  

Energy Technology Data Exchange (ETDEWEB)

Low-cost titanium alloy components are getting increasing attention in aerospace applications. Cost reductions are possible in the alloys themselves and in the production techniques. The former aspect is less promising as titanium alloys are costly to produce. Of course, there are some new developments like the (alpha plus beta) alloy Ti-6 Al-2 Fe-0.2 Si (TIMETAL 62S) and the beta-alloy Ti-6.8 Mo-4.5 Fe-1.5 Al (TIMETAL LCB), in which low-cost iron replaces costly beta alloying elements like vanadium or molybdenum, but these will be used mainly on the mass production markets, e.g. motor car construction. In consequence, optimisation of production methods is the more promising option. Near net shape processes will reduce the production cost and improve the fly-to-buy ratio. Some of these production processes are explained. [Deutsch] Die ...

1998-12-31

85

Electrochemical properties of Si/Ni alloy-graphite composite as an anode material for Li-ion batteries  

International Nuclear Information System (INIS)

Si/Ni alloy and graphite composites were synthesized using arc-melting followed by high energy mechanical milling (HEMM). Alloy particles comprising of NiSi2, NiSi and Si phases were distributed finely and uniformly on the surface of graphite in the composites obtained after Hem. The composite containing 60 wt.% of Si/Ni alloy exhibited a stable capacity of ?780 mAh/g. Fourier transform infrared spectroscopy (FTIR) analysis confirmed that some bonds were formed between alloy and graphite after HEMM, which appeared to retain the electrical connection between alloy and graphite during cycling. X-ray diffraction (XRD) analysis indicated that NiSi2 and NiSi phases, which acted as an inactive alloy matrix remained invariant during charge and discharge. In addition to NiSi2 and NiSi phases, disordered graphite layers also played the role of media ...

2005-09-30

86

Carburization and tensile behavior of alloy 800 in liquid sodium  

International Nuclear Information System (INIS)

The carbon transfer has been analyzed in the Alloy 800/sodium/stainless steel system by determining the carbon-uptake of Alloy 800 foils, which were exposed in liquid sodium of known carburizing potential. Under equilibrium condistions between 650 and 550_0C the measured total carbon concentrations in the Alloy 800 tabs were found to be roughly related to the carbon activities of the sodium environment by the equation already stated for the 18 Cr-8/10 Ni stainless steels, extrapolated to the chemical composition of the Ni-rich austenitic alloy. However the Alloy 800 was not found to undergo any decarburization in low-carbon activity environments. The carbon diffusion kinetics was determined as a function of temperature, it was found to be similar to that reported for the AISI-304 type of steel. The effects of sodium exposure on microstructural and mechanical ...

87

Carburization and tensile behavior of Alloy 800 in liquid sodium  

Energy Technology Data Exchange (ETDEWEB)

The carbon transfer has been analyzed in the Alloy 800/sodium/stainless steel system by determining the carbon-uptake of Alloy 800 foils, which were exposed in liquid sodium of known carburizing potential. Under equilibrium conditions between 650 and 550/sup 0/C the measured total carbon concentrations in the Alloy 800 tabs were found to be roughly related to the carbon activities of the sodium environment by the equation already stated for the 18 Cr-8/10 Ni stainless steels, extrapolated to the chemical composition of the Ni-rich austenitic alloy. However the Alloy 800 was not found to undergo any decarburization in low-carbon activity environments. The carbon diffusion kinetics was determined as a function of temperature, it was found to be similar to that reported for the AISI-304 type of steel. The effects of sodium exposure on microstructural and mechanical ...

1983-05-01

88

Structure and properties of a metastable #beta#-alloy aged after plastic deformation  

International Nuclear Information System (INIS)

Phase and structural transformations in a multicomponent (5.05 mas.% Mo-4.95V-3.00Cr-3.05Al) metastable #beta#-titanium alloy on aging after plastic deformation are studied using methods of electron microscopy and X-ray diffraction analysis. The alloy is deformed by twinning in a #left brace#332#right brace# system, and even at initial stages the formation of a twin skeleton takes place in the structure, on further loading the deformation of the skeleton is by secondary twinning resulting in a high plasticity of the alloy. On annealing mechanical twins transform into #alpha#-phase - a ductile twin skeleton is replaced by a rigid skeleton of #alpha#-phase plates. The aging enhances the yield strength of the alloy but decreases sharply its plasticity

2004-12-01

89

On the temperature sensing capability of a fibre optic SPR mechanism based on bimetallic alloy nanoparticles  

Energy Technology Data Exchange (ETDEWEB)

In this work, we have investigated the capability of different bimetallic nanoparticle alloy combinations to be used in fibre optic temperature sensing based on the technique of surface plasmon resonance (SPR). The metals considered for the present analysis are silver, gold and aluminium. The analysis is derived mainly from the thermo-optic effect along with some fundamental concepts of metal optics such as surface scattering, phonon-electron scattering and electron-electron scattering. The performance of the sensor with three different bimetallic nanoparticle alloy combinations is evaluated and compared, numerically, in terms of its sensitivity and accuracy. On the basis of the comparison and some logistic criterion, we predict the best possible bimetallic alloy combination along with a requisite alloy composition ratio that simultaneously provides higher values of both sensitivity and accuracy which ...

2009-02-21

90

Design and microstructural analysis of magnesium alloys for dynamical applications  

British Library Electronic Table of Contents (United Kingdom)

A microanalytical characterization of cast magnesium alloys of eutectic origin based on the Mg?Al?Ca ternary matrix system has been carried out in order to investigate the influence of alloying elements on their microstructure as well as microchemistry-processing-microstructural relations using structure-sensitive techniques of electron microscopy, mechanical spectroscopy (internal friction), X-ray diffractometry, and advanced microanalytical methods including electron probe compositional analysis. Following the data obtained here there is direct correlation of microstructure with creep properties of the new experimental magnesium alloys. The creep and heat-induced properties of the multicomponent magnesium alloys containing low range of inexpensive additions of titanium (0.07?0.2%) or str...

2011-01-01

91

Cycleable graphite/FeSi{sub 6} alloy composite as a high capacity anode material for Li-ion batteries  

Energy Technology Data Exchange (ETDEWEB)

FeSi{sub 6}/graphite composite was prepared by mechanical ball milling. The FeSi{sub 6} alloy particles consist of an electrochemically active silicon phase and inactive phases FeSi{sub 2}, distributed uniformly in the graphite matrix. The composite anode offers a large reversible capacity (about 800 mAh g{sup -1}) and good cycleability, due to the buffering effect of the inactive FeSi{sub 2} phase and graphite layers on the volumetric changes of Si phase during lithium-Si alloying reaction. Since FeSi{sub 6} alloy is a low-cost industrial material, this alloy compound provides a possible alternative for development of high capacity lithium-ion batteries. (author)

2008-10-01

92

Mechanical properties of B-modified Ti-6Al-4V alloys  

International Nuclear Information System (INIS)

Minor addition of B to the Ti-6Al-4V alloy reduces the prior #beta# grain size by more than an order of magnitude. TiB formed in-situ in the process has been noted to decorate the grain boundaries. This microstructural modification influences the mechanical behavior of the Ti-6Al-4V alloy significantly. In this paper, an overview of our current research on tensile properties, fracture toughness as well as notched and un-notched fatigue properties of Ti-6Al-4V-xB with x varying between 0.0 to 0.55 wt.% is presented. A quantitative relationship between the microstructural length scales and the various mechanical properties have been developed. Moreover, the effect of the presence of hard and brittle TiB has also been studied.

2010-07-01

93

Effect of the morphology of the primary alpha phase on the mechanical properties of Beta-CEZ alloy  

International Nuclear Information System (INIS)

A new metastable beta titanium alloy, Beta-CEZ, has been developed by CEZUS. This alloy was designed for use at moderate temperatures up to 450 C (840 F). Alloy requirements also included high mechanical strength, high fracture toughness and improved creep resistance as compared to existing beta alloys. The understanding of the relationships between processing/microstructure/mechanical properties in the alloy may lead to applications of such promising material in current and future airplanes. In this study, a combination of several forging routes, which included through-transus, hot-die and warm-die forging, with subsequent heat treatments were selected in order to evaluate the microstructure-mechanical property relationships. It was found that the recrystallized prior beta grain boundary alpha, characteristic of the ...

1993-02-21

94

Assessment of predictive models for the failure of titanium and ferrous alloys due to hydrogen effects. Report for the period of June 16 to September 15, 1981  

Energy Technology Data Exchange (ETDEWEB)

The 1977 version of the Simpson-Puls-Dutton model appears to be the most amenable with respect to utilizing known or readily estimated quantities. The Pardee-Paton model requires extensive calculations involving estimated quantities. Recent observations by Koike and Suzuki on vanadium support the general assumption that crack growth in hydride forming metals is determined by the rate of hydride formation, and their hydrogen atmosphere-displacive transformation model is of potential interest in explaining hydrogen embrittlement in ferrous alloys as well as hydride formers. The discontinuous nature of cracking due to hydrogen embrittlement appears to depend very strongly on localized stress intensities, thereby pointing to the role of microstructure in influencing crack initiation, fracture mode and crack path. The initiation of hydrogen induced failures over relatively short periods of time can be characterized with fair reliability using ...

1982-04-01

95

Complexing of vanadium(3) with chromotropic acid derivatives  

International Nuclear Information System (INIS)

A spectrophotometric study has been made of the complex formation of vanadium (3) with arsenazo(1), arsenazo(3) and some monosubstituted derivatives of chromotropic acid and sulphanylamides. In acid medium vanadium (3) reacts with each of these reagents to produce a 1:1 complex. Optimum conditions of the complex formation was found. The effect of H"+ on the complex formation of vanadium (3) with chromotropic acid derivatives was established. It was found by the graphical method that the formation of the complex is accompanied by the elimination of one proton. Patterns were found of the influence of the nature of substituents in the organic compound on the ionization constants of acid groups and stability of complexes. Molar extinction coefficients, equilibrium constants of the formation reactions and instability constants for the complexes were calculated. The structure of complexes was suggested. Similar behaviour of all ...

1976-01-01

96

The influence of yttrium (Y) on the corrosion of Mg-Y binary alloys  

International Nuclear Information System (INIS)

Research highlights: #-># The Y-intermetallic can accelerate corrosion and Y can increase the protectiveness of the surface layer. #-># In 0.1 M NaCl, the corrosion rate of Mg-Y alloys increased with increasing Y due to the Y intermetallic. #-># In 0.1 M NaCl, there was filiform corrosion. #-># In 0.1 M Na_2SO_4, the corrosion rate of Mg-Y alloys decreased with increasing Y in the range 3-7%Y. #-># Hydrogen evolution was observed from particular parts of the alloy surface. - Abstract: Corrosion of Mg-Y alloys was studied using electrochemical evaluations, immersion tests and direct observations. There were two important effects. In 0.1 M NaCl, the corrosion rate increased with increasing Y content due to increasing amounts of the Y-containing intermetallic. In 0.1 M Na_2SO_4, the corrosion rate decreased with increasing Y content above 3%, attributed to a more protective surface film, ...

2010-11-01

97

Evaluation of microstructures and mechanical properties in the HAZ of SA 508 Gr.4N Low Alloy Steel  

International Nuclear Information System (INIS)

In the heat-affected zones (HAZ) of low alloy steels used for nuclear pressure vessel, microstructural changes, such as grain coarsening, carbide precipitation, and martensite formation, generally occur and cause a deterioration of toughness and an increase in sensitivity to brittle fracture. Metallographic analyses of low alloy steel welds reveal significantly different regions in HAZ microstructures. In 2-pass welds, there were seven characteristic regions in the HAZ determined by the peak temperature, to which the region was exposed during the weld thermal cycle: a coarse-grained region, a fine-grained region, an intercritical region, and subcritical region. The coarse-grained region can be categorized into four zones according to the reheating temperature as follows : an unaltered coarse-grained zone (UCGHAZ), a supercritically reheated coarse grained zone (SCRCGHAZ), an intercritically reheated coarse-grained zone (ICRCGHAZ), and an ...

2006-11-02

98

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 2. Roles on hydrogen pickup  

Energy Technology Data Exchange (ETDEWEB)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. In the previous paper, corrosion mechanism was elucidated by the anodic protection-precipitates degradation model. This paper describes the roles on hydrogen pickup. 633 K pure water autoclave test was performed on high purity zirconium, Zr-0.2Fe, Zr-0.2Cr, and Zr-0.1Fe-0.1Cr alloys. Hydrogen analysis after the corrosion test showed that hydrogen pickup ratio of Zr-0.2Fe alloy was about 80%. It was much higher than about 30% of pure Zr and about 10% of both Zr-0.2Cr and Zr-0.1Fe-0.1Cr alloys. Larger hydrogen content was introduced into Zr-0.2Fe alloy than the other ones by the cathodic hydrogen charging under coulombic equivalence. The ...

2000-08-01

99

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 2. Roles on hydrogen pickup  

International Nuclear Information System (INIS)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. In the previous paper, corrosion mechanism was elucidated by the anodic protection-precipitates degradation model. This paper describes the roles on hydrogen pickup. 633 K pure water autoclave test was performed on high purity zirconium, Zr-0.2Fe, Zr-0.2Cr, and Zr-0.1Fe-0.1Cr alloys. Hydrogen analysis after the corrosion test showed that hydrogen pickup ratio of Zr-0.2Fe alloy was about 80%. It was much higher than about 30% of pure Zr and about 10% of both Zr-0.2Cr and Zr-0.1Fe-0.1Cr alloys. Larger hydrogen content was introduced into Zr-0.2Fe alloy than the other ones by the cathodic hydrogen charging under coulombic equivalence. The ...

2000-08-01

100

Active groups for oxidative activation of C-H bond in C{sub 2}-C{sub 5} paraffins on V-P-O catalysts  

Energy Technology Data Exchange (ETDEWEB)

For the first time in scientific literature, in our joint work with Dr. G. Ladwig in 1978 it was established phase portraite of the oxide vanadium-phosphorus system within wide range of P/V ratios from 0.5 to 3.2. Some later those data were confirmed. By investigation of the properties of individual vanadium-phosphorus phases it was also shown that the active component of such catalysts in n-butane oxidation was vanadyl pyrophosphate phase (VO){sub 2}Pr{sub 2}O{sub 7}. From then the conclusion has been evidenced by numerous publications and at present it has been out of doubt practically all over the world. It was hypothized that the unique properties of (VO){sub 2}P{sub 2}O{sub 7} in the reaction of n-butane oxidation could be explained by the presence of paired vanadyl groups and nearness of the distances between neighbouring vanadyl pairs and that between the first and fourth carbon atoms in n-butane molecule. The molecule activation occured ...

1998-12-31

101

Mechanical properties of excimer laser modified titanium surfaces  

Energy Technology Data Exchange (ETDEWEB)

Excimer laser processing enables both thermally-driven transformations and the incorporation of solutes into the surface of materials through melting and diffusional mixing. We have examined the effect of excimer laser processing on the microstructure and surface mechanical properties of titanium alloys. Changes in the surface hardness due to laser processing were studied using a Nanoindenter [trademark]. Alloying experiments using both mixing of evaporated surface layers of boron and laser gas alloying in air and in nitrogen all result in changes in the surface hardness of the material. Alloying with boron results in an amorphous surface which is somewhat harder than the as polished surface. Laser processing in air and pure nitrogen results in incorporation of oxygen and nitrogen and the development of fine ([approximately] 50 nm) precipitates of TiO and TiN respectively. ...

1993-01-01

102

Texture development of AZ31 magnesium alloy during ECAE processing  

Energy Technology Data Exchange (ETDEWEB)

Mg-3%Al-1%Zn (AZ31) alloy was subjected to ECAE processing at 523 and 573 K. Microstructure observation and texture analysis were carried out using optical microscope and SEM-EBSD technique in order to investigate the process of microstructural changes including texture development during ECAE processing. Grain refinement during ECAE processing is enhanced by dynamic continuous recrystallization. The texture of the ECAE-processed AZ31 alloy specimens change with ECAE processing temperature, and the textural changes relate to deformation mechanisms that change with ECAE processing temperature. (orig.)

2003-07-01

103

High temperature fatigue example of creep life time prediction for grade 2 alloy 800 at 550 C  

Energy Technology Data Exchange (ETDEWEB)

Experimental data on the material characteristics of structures subjected to thermal and mechanical cycling are needed for designing structural parts for creep and creep-fatigue interaction. Moreover, high-temperature low-cycle fatigue data are not sufficient to predict the fatigue creep lifetime. In order to check the reliability of steam generators, tests on pipe materials are conducted under cyclic thermal loading. The tests have been performed on an iron-nickel chromium alloy (alloy 800). Isothermal low-cycle fatigue tests have been conducted at 550 C. 15 refs.

1994-04-01

104

An influence of ion bombardment on plasma nitriding process of Ti6Al14V alloy at 843 K temperature  

International Nuclear Information System (INIS)

This work presents results of investigations on d.c. glow discharge nitriding of #alpha#+#beta# Ti-6Al-4V titanium alloy. The treatment was performed at 843 K in nitrogen-hydrogen atmosphere, pressure 300 Pa. Special attention was paid to nitriding mechanism and determination of the role of ion bombarding in nitriding process of titanium alloys. Produced as a result of d.c. plasma nitriding surface layers were subjected to macroscopic observations, microstructure studies, microhardness testing and X-ray analysis. (author)

2004-06-20

105

A review of the behaviour of alloy 800 in liquid sodium  

International Nuclear Information System (INIS)

Although there is service experience of Alloy 800 as tubing for superheaters in conventional and nuclear (HTR) power stations and in PWR heat exchangers, there is no corresponding service experience in sodium-cooled fast reactor steam generators. However, some limited experimental studies have been made of corrosion behaviour, and of possible structure modifications and effects on mechanical properties which occur during exposure of this material to a high temperature sodium environment, and these are summarised in the paper. It is concluded that further work needs to be done before Alloy 800 can be confidently endorsed for use as tubing in fast reactor steam generators. (author).

106

Dislocation plasticity and complementary deformation mechanisms in polycrystalline Mg alloys  

Energy Technology Data Exchange (ETDEWEB)

Deformation mechanisms of Mg-Al-Zn (AZ31) alloys were investigated by performing tensile test at room temperature. In fine grain Mg alloys deformed at room temperature, nonbasal slip systems were found to be active as well as basal slip systems because of grain-boundary compatibility effect. Slip-induced grain-boundary sliding occurred as a complementary deformation mechanism to give rise to c-axis component of strain. With increasing grain size, the activation of the nonbasal slip systems was limited near grain boundaries. Instead of grain-boundary sliding, twinning occurred as a complementary deformation mechanism in large grained samples. Orientation analysis of twins indicated that twinning is induced by stress concentration due to the pile up of basal dislocations. The grain-size dependence on deformation mechanism was found to affect yielding behavior both ...

2004-07-01

107

Study of transformation behavior in a Ti-4.4 Ta-1.9 Nb alloy  

International Nuclear Information System (INIS)

An alloy of composition Ti-4.4 wt.% Ta-1.9 wt.% Nb is being developed as a structural material for corrosion applications, as titanium and its alloys possess excellent corrosion resistance in many oxidizing media. The primary physical metallurgy database for the Ti-4.4 wt.% Ta-1.9 wt.% Nb alloy is being presented for the first time. Determination of the #beta# transus, M_s temperature and classification of the alloy have been carried out, employing a variety of microscopy techniques, X-ray diffraction (XRD), micro-hardness and differential scanning calorimetry (DSC). The #beta# transition temperature or #beta# transus determined using different experimental techniques was found to agree very well with evaluations based on empirical calculations. Based on chemistry and observed room temperature microstructure, the alloy has been classified as an #alpha# + #beta# titanium ...

2005-01-15

108

Optimizing the microstructure of implant alloy TiAl5Fe2.5 by microprobe analysis  

International Nuclear Information System (INIS)

For optimizing the microstructure of the (#alpha# + #beta#)-titanium alloy TiAl5Fe2.5 the content of the two alloying elements aluminium and iron in the #alpha#- and #beta#-phase was determined by microprobe analysis. The alloys with the composition of the #alpha#- and of the #beta#-phase at 850 degC TiAl6Fe0.5 (#alpha#-phase) and TiAl3.5Fe6.5 (#beta#-phase) were prepared by arc melting and rolling at 850 degC. The mechanical properties of the '#alpha#'- and of the '#beta#'-phase-alloy are compared with the properties of the (#alpha# + #beta#)-alloy TiAl5Fe2.5 in the as rolled and swaged condition and after an additional aging at 550 degC. By this optimizing process it was possible to achieve a tensile strength of Rsub(m) = 1012 N/mm"2, an yield strength of Rsub(p0.2) 954 N/mm"2 and an elongation at fracture A = 14.5% in the ...

1985-05-13

109

Strength of VT22 titanium alloy in various structural states  

International Nuclear Information System (INIS)

The influence of heat treatment on the structure, mechanical properties and fracture peculiarities of high-strength (#alpha#+#beta#)-titanium alloy VT22 has been studied. It is ascertained that thermal cycling and subsequent high-temperature aging permit to reduce considerably crack growth rate. Thermal cycling is realized in the following mode: heating in #beta#-region, cooling and allowance in (#alpha#+#beta#)-region, heating in #beta#-region.

110

Low temperature superplasticity of a metastable #beta#-titanium alloy  

International Nuclear Information System (INIS)

Superplasticity in Ti alloys has been widely investigated in the past and superplastic forming of aerospace components has thus been developed over the last two decades. The Ti alloy most studied in this framework is undoubtedly the Ti-6Al-4V (wt %) alloy, for which maximum elongations are obtained in the temperature range [880-900C]. The development of the superplastic properties has been demonstrated to be in close relation with quite similar volume fractions of the #alpha# and #beta# phases, the #beta# transus temperature for this alloy ranging from 980-1000 C. Attempts have been carried out to reduce the temperature of superplastic forming of Ti-6Al-4V by the addition of elements like Fe, Co, or Ni. Such an introduction of alloying elements indeed results in a decrease of the optimum forming temperature to values as low as 820 C. This decrease is mainly attributed to a change in ...

111

Science of materials. Progress report, January 1-December 21, 1982  

Energy Technology Data Exchange (ETDEWEB)

Progress is reported in the following areas: metallurgy and ceramics (structure of materials, mechanical properties, physical properties), experimental research, and particle-solid interactions (irradiation effects on alloys). (DLC)

1982-01-01

112

Development of engineered structural barriers for nuclear-waste packages  

Energy Technology Data Exchange (ETDEWEB)

The development of structural barriers for nuclear waste packages involves selection of candidate materials, their screening by mechanical and corrosion testing, rigorous accelerated testing, and evaluation and comparison with other package elements. This document presents results from work conducted on titanium and ferrous alloys.

1981-09-01

113

Moessbauer study of mechanically alloyed powders  

Energy Technology Data Exchange (ETDEWEB)

Using the [sup 57]Fe Moessbauer spectroscopy, the microscopic behavior of Fe powders has been investigated during and after the mechanical alloying (MA) process for Al-Fe and Ag-Fe systems. A repeated rolling method as well as a conventional ball-milling method are employed in order to understand the microscopic process of the kneading of Al and Fe powders during their MA and the resultant powders show quite similar Moessbauer spectra suggesting that the kneading by an impact between colliding balls is the same process as that of the thickness reduction by cold rolling. Moessbauer spectra show clearly the occurrence of the mutual atomic dispersion for the thermodynamically immiscible Ag-Fe system. (orig.).

1991-11-01

114

Damage mechanism in high temperature fatigue of alloy 800 H  

Energy Technology Data Exchange (ETDEWEB)

In order to investigate the influence of grain boundary cavities on the life time of Alloy 800 H various fatigue tests have been performed at 800/sup 0/C. Cavity formation has been observed only in asymmetrical tests. Compared to the corresponding symmetrical tests, the cyclic life time is shorter. As the cavitation damage increases, the ratio of life times in vacuum and in air steadily decreases from an initial value of 5. In extreme cases it can reach a value close to 1. In this case, cavitation damage dominates over the usual damage mechanism, which is cracks from the surface.

1986-09-01

115

A new high nitrogen super austenitic stainless steel with improved structure stability and corrosion resistance properties  

International Nuclear Information System (INIS)

A new highly alloyed (Cr, Mo, W, N) super austenitic grade has been developed. This grade offers high mechanical properties combined with excellent corrosion resistance in chloride acid media. This grade is particularly designed for applications in chloride, oxidizing acid media encountered in the chemical, transportation, pollution control, offshore and pulp and paper industries. Mechanical properties, corrosion resistance and weldability of this grade are presented and compared to that of other stainless steels and nickel base alloys.

1996-03-24

116

Thermomechanical treatment of medium-carbon, microalloyed ferrite-pearlite steels. Final report; Thermomechanische Behandlung von mikrolegierten ferritisch-perlitischen Staehlen mit mittlerem Kohlenstoffgehalt. Schlussbericht  

Energy Technology Data Exchange (ETDEWEB)

The precipitation hardened, ferrite-pearlite medium-carbon steels microalloyed with vanadium (AFP steels) have been developed over the last few years as materials allowing processing by controlled, continuous cooling down from forging temperatures, for achieving benefits such as reducing the number of required heat treatment and working processes and saving expensive alloying materials. Due to their cost-saving advantages, the steels rapidly have been accepted as an alternative material to the quenched and tempered steels and re particularly used for fabrication of automobile parts. Their drawbacks however are the lower yield strength, and low ductility and toughness as compared to the heat-treatable steels. The research project therefore was intended to enhance the properties of the microalloyed, medium-carbon steels and widen their applicability by establishing further and improving existing thermomechanical treatment processes that will ...

1996-10-01

117

Influence of tempering on microstructure and hardness of high-temperature 9%Cr-steels; Einfluss des Anlassens auf Gefuege und Haerte warmfester 9%Cr-Staehle  

Energy Technology Data Exchange (ETDEWEB)

The influences of temperature and duration of tempering on hardness and microstructure were investigated at high-temperature martensitic and low-carbon steels with 9% chrome and the further alloying elements molybdenium, vanadium, niobium and partially tungsten. After austenitizing and subsequent air cooling the steels were tempered at temperatures below, at and above Ac{sub 1b} for different times and finally a hardness test was performed. Making use of the temperature dependence of the hardness tempering diagrams were constructed and the Hollomon-Jaffe-Parameter on the three steels was determined within its application limits. Micrographs of the structure shows the formation of the carbides and the martensite. At tempering temperatures below Ac{sub 1b} a decrease of hardness occurs, above Ac{sub 1b}, a hardness rise due to the partial austenitizing was obtained. While hardening below Ac{sub 1b}, the tempering quality increases from P 91, NF ...

1999-06-01

118

Temperature Dependent Constitutive Modeling for Magnesium Alloy Sheet  

International Nuclear Information System (INIS)

Magnesium alloys have been increasingly used in automotive and electronic industries because of their excellent strength to weight ratio and EMI shielding properties. However, magnesium alloys have low formability at room temperature due to their unique mechanical behavior (twinning and untwining), prompting for forming at an elevated temperature. In this study, a temperature dependent constitutive model for magnesium alloy (AZ31B) sheet is developed. A hardening law based on non linear kinematic hardening model is used to consider Bauschinger effect properly. Material parameters are determined from a series of uni-axial cyclic experiments (T-C-T or C-T-C) with the temperature ranging 150-250 deg. C. The influence of temperature on the constitutive equation is introduced by the material parameters assumed to be functions of temperature. Fitting process of the assumed model to measured data is presented ...

2010-06-15

119

Surface modification of magnesium base alloys by gas/plasma nitridation  

Energy Technology Data Exchange (ETDEWEB)

Gas and plasma nitriding processes were executed in the magnesium with modification by titanium in search for an effective surface treatment method for magnesium alloys. Magnesium-nitrogen system has completely no solid solution or solubility, so that nitride should be only formed by eutectic reaction in the liquid phase. Hence, magnesium is difficult or nearly impossible to have its surface modified by nitriding. Addition of nitride forming element into magnesium enables us to lower the onset temperature of nitriding. Magnesium-titanium alloys with 1 to 5 wt% are yielded by the bulk mechanical alloying and, subjected to gas nitriding for various process conditions. Successful co-formation of Mg{sub 3}N{sub 2} as well as TiN becomes a proof to demonstrate the possibility of gas/plasma nitriding in the solid-state magnesium with aid of nitride former. (orig.)

2000-07-01

120

Mechanical deformation and tensile super-elastic behaviors of a Ti-Mo based shape memory alloy  

Science.gov (United States)

Ni-free shape memory alloys are promising functional materials for medical applications. A newly developed Ti-Mo based shape memory alloy shows superelasticity after thermomechanical treatment. However, the microstructure evolution and precipitation during thermomechanical processes are still not well understood. In the present paper, compressive deformation behavior at a series of temperatures of 298K - 973K and tensile deformation behavior of the alloy after aged at 573K - 973K have been investigated systematically. It is found that the compressive yield stress and ultimate compressive strength change with the deformation temperature. The ultimate tensile strength and yield stress of aged specimens also change with the aging temperature following a non-linear relationship. Microstructures of aged specimens as well as effects of lattice softening and aging-induced precipitates on the deformation behavior have been ...

2011-03-01

121

Manufacturing of oxide-dispersion-strengthened steels with the use of preliminary surface oxidation  

British Library Electronic Table of Contents (United Kingdom)

Regularities of deformation-induced dissolution of a surface layer of iron oxides in matrixes of iron-based alloys with bcc and fcc lattices have been studied by the methods of M?ssbauer spectroscopy, transmission electron microscopy, and X-ray diffraction. A method of producing iron alloys strengthened by dispersed oxide nanoparticles and alloyed with elements possessing a high affinity to oxygen (titanium and yttrium) has been proposed, which implies a dynamic dissolution of a surface layer of iron oxides upon strong cold deformation and a precipitation of secondary yttrium and titanium nanooxides upon a subsequent high-temperature sintering of mechanically alloyed powders. There has been demonstrated a possibility of oxide strengthening of pure iron upon its interaction with air without...

2011-01-01

122

Investigation of passive films on nickel Alloy 690 in lead-containing environments  

Energy Technology Data Exchange (ETDEWEB)

Passive films formed on Alloy UNS N06690 were investigated in simulated crevice chemistries. It was found the role of lead in corrosion processes is strongly dependent on the pH value of the testing solutions. At pH 1.5 the effect of lead is narrowly noticeable; while at pH 12.7, lead has a significant influence on the electrochemical performance of alloy UNS N06690. The lead alters the surface morphologies at both pH and account for higher hydroxide content in the surface film at pH 12.7. The lead incorporation hinders the formation of spinel oxides during the passivation in alkaline solution. Nanoindentation tests indicate a significant lead-induced degradation in the mechanical properties of passive films. The passivation degradation is attributed to detrimental effects of lead via interrupting the dehydration process and hindering the formation of protective layers on the alloy surface.

2008-09-01

123

Friction welding of AZ31 magnesium alloy  

Energy Technology Data Exchange (ETDEWEB)

In this paper, for an acceleration of utilization of magnesium alloy which is being interested in recent years, friction welding of AZ31 magnesium alloy was carried out, and the joint performance was discussed in relation to the deformation heat input in the upset stage and upset loss as a evaluation factor. Where, the deformation heat input in the upset stage is mechanical work represented by the product of upset speed and axial pressure. As a result, it was made clear that the friction welding of AZ31 magnesium alloy was easy in the atmosphere, and good welded joints without a non- adhesion area at the weld interface could de obtained. Moreover, the evaluation factors discussed were possible to evaluate to joint performance. (orig.)

2003-07-01

124

Effect of chemical composition on the structure and mechanical properties of Mn-Al-C alloys in the magnetic region  

Energy Technology Data Exchange (ETDEWEB)

The thermal stability and deformability of Mn-Al-C alloys containing 0.6 pct C are investigated experimentally as a function of excess phase content. It is shown that an increase in Mn content from 68.9 to 73.5 pct leads to increased stability of the high-temperature epsilon phase. The enrichment of the system Mn-Al-Cu in Mn and Al above the optimum composition leads to the formation of nonmagnetic excess phases, eta and beta, which reduce the magnetization of the alloy. In addition, a decrease in thermal stability is observed in the alloy with 73.5 pct Mn due to the decomposition of the ferromagnetic phase. 7 references.

1988-01-01

125

Effect of alloying on the phase transformations and properties of a nickel alloy  

Energy Technology Data Exchange (ETDEWEB)

The phase transformations and properties of a precipitation-hardened Ni-Cr-based alloy are investigated as a function of C, B, Nb, and Cr contents. It is found that the primary role of Nb consists in the formation of an independent phase, delta-Ni3Nb, a part of a gamma/gamma-prime-delta eutectoid (for high C and B concentrations) and in stimulating the gamma-sigma reaction consecutively with the gamma double prime-delta reaction (for low C and B concentrations). In both cases, the long-term strength characteristics of the Nb-alloyed system are relatively low. The substitution of boron for carbon contributes to a reduction in the number of nucleation sites for topologically close-packed phases and to the formation of more stable (with respect to excess compounds) M3B2 and MB2 borides. The high-boron material exhibits better properties and phase stability under mechanical and thermal loading. 13 references.

1986-07-01

126

Dual-ion irradiation effects on microstructure of austenitic alloys  

International Nuclear Information System (INIS)

An Fe-15Cr-20Ni ternary model alloy and a Type 316 stainless steel were irradiated by dual-ions at 1 to 50 appm of He/dpa ratios, to investigate the helium effects on microstructural development in austenitic alloys under irradiation. Quantitative analysis on resultant microstructures revealed that the Frank loop nucleation rate and the network dislocation density positively correlate and Frank loop growth rate negatively correlate with the He/dpa ratio, while the cavity growth rate has its peak at an intermediate helium injection rate. Although He/dpa dependence of various microstructural features were similar for the model alloy and the 316SS, the rates of their development and the mechanism which had assisted cavity growth were significantly different in these two materials. (orig.).

127

Assessment of effects of Fort St. Vrain HTGR primary coolant on Alloy 800. Final report  

Energy Technology Data Exchange (ETDEWEB)

A comprehensive review was conducted of primary helium coolant chemistry data, based on current and past operating histories of helium-cooled, high-temperature reactors (HTGRs), including the Fort St. Vrain (FSV) HTGR. A reference observed FSV reactor coolant environment was identified. Further, a slightly drier expected FSV coolant chemistry was predicted for reactor operation at 100% of full power. The expected environment was compared with helium test environments used in the US, United Kingdom, Germany, France, and Japan. Based on a comprehensive review and analysis of mechanical property data reported for Alloy 800 tested in controlled-impurity helium environments (and in air when appropriate for comparison), an assessment was made of the effect of FSV expected helium chemistry on material properties of alloy 800, with emphasis on design properties of the Alloy 800 material utilized in the FSV ...

1982-08-01

128

Assessment of effects of Fort St. Vrain HTGR primary coolant on Alloy 800. Final report  

International Nuclear Information System (INIS)

A comprehensive review was conducted of primary helium coolant chemistry data, based on current and past operating histories of helium-cooled, high-temperature reactors (HTGRs), including the Fort St. Vrain (FSV) HTGR. A reference observed FSV reactor coolant environment was identified. Further, a slightly drier expected FSV coolant chemistry was predicted for reactor operation at 100% of full power. The expected environment was compared with helium test environments used in the US, United Kingdom, Germany, France, and Japan. Based on a comprehensive review and analysis of mechanical property data reported for Alloy 800 tested in controlled-impurity helium environments (and in air when appropriate for comparison), an assessment was made of the effect of FSV expected helium chemistry on material properties of alloy 800, with emphasis on design properties of the Alloy 800 material utilized in the FSV ...

129

The diffusion bonding and theoretical model including void growth mechanism in magnesium alloys  

Energy Technology Data Exchange (ETDEWEB)

There are many factors affecting diffusion bonding in order to obtain high quality joining. Therefore, in the beginning, we constructed diffusion bonding model based on void growth mechanism to predict bonding pressures and times. In addition, in order to compare theoretical values with experimental values, diffusion bonding tests were carried out by using commercial AZ31 magnesium alloy sheets with different grain sizes, 16 and 130 {mu}m. The present AZ31 alloys were successfully diffusion bonded at several conditions, and the bonding strength was more than 0.8 of each parent materials. The experimental bonding conditions in high quality joining, times and pressures, were good agreed with prediction analysis. (orig.)

2003-07-01

130

Study of phase composition and mechanical properties of Al-Mg alloys doped with Ce and Y after various conditions of heat treatment  

International Nuclear Information System (INIS)

By means of the light microscopy and by the measurement of the mechanical properties one investigated into the phase composition and the properties of Al-Mg-Ce and Al-Mg-Y system alloys. One plotted the isothermal cross sections of the mentioned systems under 430 and 275 deg C temperatures at up to 16% magnesium concentration and up to 0.7% yttrium concentration. One determined the yield limit and strength, the relative elongation of Al-Mg base hardened and deformed alloys containing 7.0-9.9% Mg and Ce, Y, Mn, Zr dopes upon ageing under 175, 200, 250 and 300 deg C temperatures within the ageing time ensuring the hardening maximum effect

131

Precipitation mechanisms and subsequent hardening kinetics in the #beta#-CEZ alloy  

International Nuclear Information System (INIS)

The #beta#-CEZ alloy : Ti-5%Al-2%Sn-4%Zr-4%Mo-2%Cr-1%Fe is a near #beta# titanium alloy. Since its processing routes include heat treatment (consisting of solution treatment and ageing), it has been decided to study the influence of the #beta# phase stability on #alpha# phase precipitation and hardening kinetics. Small sized specimens, coming from industrial heats, have been heat treated above and below the #beta# transus, and then water quenched. Therefore, several degree of #beta# stability are obtained. When it is increased (i.e. the solution treatment temperature is lowered), #alpha# or #omega# phases precipitations are delayed, as well as the hardening phenomena. Moreover, the #omega# stability domain is reduced. The mechanisms of #alpha# or #omega# precipitation are discussed, and related to the hardening kinetics. (orig.).

132

Influence of annealing on the microstructure of commercial Mg alloy AZ31 after mechanical forming  

International Nuclear Information System (INIS)

The microstructure of commercial rolled magnesium alloy AZ31B (nominal composition Mg-3Al-0.9Zn-0.15Mn in wt.%) was investigated with the help of light microscopy, electron backscatter diffraction (EBSD) and X-ray diffraction technique after annealing in the temperature range from room temperature (RT) to 400 deg. C. Tensile tests at RT were performed to show the influence of the microstructure on mechanical properties. Static recrystallization (SRX) was observed during annealing of as-received alloy at and above 150 deg. C. Twins play an important role during SRX and serve as nucleation sites and preferred paths for growth of grains. The strong basal texture caused by rolling was weakened by SRX. Significant differences in the stress strain curves were observed for as-received and annealed specimens.

2006-09-25

133

Hydrogen effect on cold rolling texture of stable #beta#-titanium alloy  

International Nuclear Information System (INIS)

A study was made into microstructure and texture of cold rolled titanium alloy VT-35 with various hydrogen content aimed to reveal hydrogen influence on the mechanism of cold plastic deformation by rolling. Experiments were carried out using sheets 1.2 mm thick hydrogenated up to hydrogen concentrations from 0.06 to 0.554 mass. %. All specimens constituted a single-phase FCC #beta#-solid solution. It is shown that small hydrogen additions have a plasticizing effect on #beta#-titanium alloys in their cold rolling. The character of texture is dependent on hydrogen concentration and determined by deformation mechanism. 6 refs.; 5 figs.

134

Effect of hydroxyapatite content on the microstructure, thermal and mechanical properties of Ti-based glassy alloy/hydroxyapatite composite prepared by spark plasma sintering  

British Library Electronic Table of Contents (United Kingdom)

In the present paper, the effects of hydroxyapatite (HA) content on the microstructure, thermal and mechanical properties of Ti-based glassy alloy/HA composite prepared by spark plasma sintering (SPS) are investigated. The microstructure of the composites is homogeneous when the HA is lower than 2 wt%. When the HA content is higher than 3 wt%, the crystalline precipitates with size of less than 5 nm are distributed in the glassy matrix. HA decomposes during sintering procedure for the composite with high HA content. With increasing HA addition, compressive strength decreases. Especially for the HA content is over 2 wt%, the strength decreases sharply because of partial crystallization of glassy alloy matrix.

2011-01-01

135

Activation energy for high temperature deformation of Ti-10V alloy on the basis of second strain rate cycles  

International Nuclear Information System (INIS)

Activation energy values for high temperature deformation of a beta -titanium alloy Ti-10V were determined from the flow stress strain rate data taken from the second increasing strain rate cycles, in order to find the rate controlling mechanism. Although the data obtained from first increasing strain rate cycles are considered most appropriated by the author in a previous study due to obvious reasons, the values obtained in present work are again indicative of lattice self diffusion in beta -phase as the rate controlling mechanism for this alloy and nevertheless suggest that two different activation energy values for a deformation process could be possible in a given temperature range, depending upon the data. (author)

2007-12-01

136

Oxide acid-base reaction relating to the inhibition of vandium attack on REY zeolite catalysts. [Rare earth-exchanged yttrium  

Science.gov (United States)

Certain materials, especially Sn, passivate the rare earth-exchanged Y zeolite (REY) used in petrochemical fluid-cracking catalysts against vanadium degradation caused by V impurities in the feed oil. The mechanism of passivation was investigated here from the standpoint of high-temperature oxide acid-base reaction; i.e., where the controlling factors were considered to be Lewis acid-base reactions between V{sub 2}O{sub 5}, the RE oxides, SnO{sub 2}, etc. Molten salt tests at 680{degree}C showed SnO{sub 2}, presumably because of its acidic nature, to be essentially nonreactive with V{sub 2}O{sub 5} or Na{sub 2}O-V{sub 2}O{sub 5} compounds. A hypothesis was developed to explain how the passivation effect by Sn might result from the unique resistivity of SnO{sub 2} to reaction with V{sub 2}O{sub 5}.

1991-05-01

137

Mechanical properties and texture evolution of AZ31 Mg alloy during equal channel angular pressing  

Energy Technology Data Exchange (ETDEWEB)

Microstructure and texture evolution in the AZ31 Mg alloy subject to equal channel angular pressing (ECAP) have been investigated and correlated with the mechanical properties. When AZ31 Mg alloy was ECAPed up to 8 passes following the route B{sub c}, grain refinement occurred effectively. Texture was also changed during ECAP. The original fiber texture of the extruded AZ31 Mg alloy changed to a new texture component of (01 anti 11)[5 anti 2 anti 3 anti 1], and the texture of (01 anti 11)[5 anti 2 anti 3 anti 1] orientation was rotated to (13 anti 46)[7 anti 5 anti 20] orientation after 6-pass ECAP process. The variation of the strength with the pass number was explained by the texture and grain size. The strength data of AZ31 Mg alloys followed the standard Hall-Petch relationship when the similar texture was retained during the ECAP process. Otherwise the effect of texture on ...

2005-07-01

138

Fatigue properties of magnesium alloy under biaxial stress  

Energy Technology Data Exchange (ETDEWEB)

Machines and structures, such as automobiles are usually subjected to biaxial or three-axial stresses instead of uniaxial stress. However, research on a fatigue failure under multi-axial stress has not been fully presented because such experiments are difficult. To solve this problem, we developed the servo biaxial fatigue-testing machine. In this research, we performed the biaxial fatigue tests of a magnesium alloy in order to clarify the effects from different heat treatments. Magnesium alloy is the lightest in weight among metal materials for structural use. The fatigue characteristics of a magnesium alloy are indispensable in order to create the design which ensures the reliability and the safety of the vehicles especially in long-distance run. The main conclusions are summarized as follows; (1) The mechanical property of magnesium alloy AZ31B falls by heat treatment at low ...

2004-07-01

139

Behavior of inert gas contamination in high Ni alloy powder and consolidation powder material; Ko Ni gokin funmatsu funmatsu seikeitai ni okeru fukassei gas seibun no kyodo  

Energy Technology Data Exchange (ETDEWEB)

Inert gas contamination, structure and mechanical properties of consolidated high-Ni alloy powder material were studied to improve its characteristics. In experiment, the chemical composition and fraction of porosity in cross sections of Alloy 625 powder were examined which was produced by Ar gas atomization method impinging supplemental gas jet onto accumulated alloy powder in the bottom of a tank for rapid cooling. The structure and mechanical properties of the alloy rod were also examined which was produced by hot hydrostatic pressing or hot extrusion of the powder filled into a capsule. As a result, although Ar content included in the powder produced by Ar gas atomization method decreased with reduction in grain size, the fine powder less than 22{mu}m still included Ar of nearly 0.5mass-ppm. Obvious correlation was found between the fraction of porosity in ...

1996-07-01

140

Development of materials resistant to metal dusting degradation.  

Energy Technology Data Exchange (ETDEWEB)

Metal dusting corrosion has been a serious problem in the petroleum and petrochemical industries, such as reforming and syngas production systems. This form of deterioration has led to worldwide material loss for 50 years. For the past three years, we have studied the mechanism of metal dusting for Fe- and Ni-base alloys. In this report, we present a correlation between the weight loss and depth of pits that form in Ni-base alloys. Nickel-base alloys were also tested at 1 and 14.8 atm (210 psi), in a high carbon activity environment. Higher system pressure was found to accelerate corrosion in most Ni-base alloys. To reduce testing time, a pre-pitting method was developed. Mechanical scratches on the alloy surface led to fast metal dusting corrosion. We have also developed preliminary data on the performance of weldments of several Ni-base ...

2006-04-24

141

Mechanical properties and corrosion behavior of materials exposed to an experimental, atmospheric fluidized-bed combustor  

Energy Technology Data Exchange (ETDEWEB)

A joint materials test program developed by the Institute for Mining and Minerals Research (IMMR) and the Tennessee Valley Authority (TVA) involved the postexposure mechanical properties and corrosion behavior of candidate structural materials in an experimental, atmospheric fluidized-bed combustor (AFBC). This combustor was operated by Accurex Corporation at Research Triangle Park, North Carolina, under the direction of TVA. The materials studied were Type 304, Type 310, and INCOLOY alloy 800 in the form of disc coupons with and without crevice configurations. Type 304 was also used for mechanical property measurements. The alloys were exposed to the combustor environment at about840/sup 0/C for approximately 330 hours. The ranking in terms of decreasing weight loss was: (1) Type 304, (2) Type 310, and (3) INCOLOY alloy 800. The presence of tight crevices did not enhance the ...

1984-06-01

142

Visualization of direct contact heat transfer between water and molten alloy  

Energy Technology Data Exchange (ETDEWEB)

We have been developing an innovative Steam Generator concept of Fast Breeder Reactors by using liquid-liquid direct contact heat transfer. In this concept, the SG shell is filled with a molten alloys, which is heated by primary sodium. Water is fed into the high temperature molten alloy, and evaporates by direct contact heating. In order to obtain the fundamental information to discuss the heat transfer mechanisms of the direct contact between the water and the alloy, this phenomenon was visualized by real-time neutron radiography. JRR-3M real-time thermal neutron radiography in Japan Atomic Energy Research Institute was used. Followings are main results. (1) The vigorous evaporation occurs in the molten alloy. This phenomena is different from the known phenomenon such as the evaporation of refrigerant R-113 in the water. (2) The evaporation in the bubble has finished in a moment ...

1996-06-01

143

Recent advances and developments in refractory alloys  

Energy Technology Data Exchange (ETDEWEB)

Refractory metal alloys based on Mo, W, Re, Ta, and Nb (Cb) find applications in a wide range of aerospace applications because of their high melting points and high-temperature strength. This paper, presents recent progress in understanding and applications of these alloys. Recent studies to improve the oxidation and mechanical behavior of refractory metal alloys, and particularly Nb alloys, are also discussed. Some Re structures, for extremely high temperature applications (> 2000C), made by CVD and P/M processes, are also illustrated. Interesting work on the development of new W alloys (W-HfC-X) and the characterization of some commercial refractory metals, e.g., K-doped W, TZM, and Nb-1%Zr, continues. Finally, recent developments in high temperature composites reinforced with refractory metal filaments, and refractory metal-based intermetallics, e.g., ...

1993-11-01

144

Promising materials for HTGR high temperature heat exchangers  

International Nuclear Information System (INIS)

The service conditions for high-temperature heat-exchangers with helium coolant of HTGRs and requirements imposed on materials for their production are discussed. The choice of nickel-base alloys with solid-solution hardening for long-term service at high temperatures is grounded. Results of study on properties and structure of types Ni-25Cr-5W-5Mo and Ni-20Cr-20W alloy in the temperature range of 900 deg. - 1,000 deg. C are given. The ageing of Ni-25Cr-5W-5Mo alloy at 900 deg. - 950 deg. C results in decreased corrosion-mechanical properties and is caused by the change of structural metal stability. Alloy with 20% tungsten retains a high stability of both structure and properties after prolonged exposure in helium at above temperatures. The alloy has also increased resistance to delayed fracture and low-cycle fatigue at high temperatures. The developed ...

1989-06-01

145

Numerical Modeling of Magnesium Alloy Sheet Metal Forming at Elevated Temperature  

International Nuclear Information System (INIS)

The development of light-weight vehicle is in great demand for enhancement of fuel efficiency and dynamic performance. The vehicle weight can be reduced effectively by using lightweight materials such as magnesium alloys. However, the use of magnesium alloys in sheet forming processes is still limited because of their low formability at room temperature and the lack of understanding of the forming process of magnesium alloys at elevated temperatures. In this study, uniaxial tensile tests of the magnesium alloy AZ31B-O at various temperatures were performed to evaluate the mechanical properties of this alloy relevant for forming of magnesium sheets. To construct a FLD (forming limit diagram), a forming limit test were conducted at temperature of 100 and 200 deg. C. For the evaluation of the effects of the punch temperature on the formability of a rectangular cup ...

2007-05-17

146

Microstructure evolution and fracture behavior in superplastic deformation of hot-rolled AZ31 Mg alloy sheet  

Energy Technology Data Exchange (ETDEWEB)

Fine-grained AZ31 magnesium alloy sheets were prepared through hot rolling process. The superplastic properties of hot-rolled AZ31 Mg alloy was examined by uniaxial tensile tests at a temperature range 250{proportional_to}450 C and strain rate range 0.7 x 10{sup -3}{proportional_to}1.4 x 10{sup -1} s{sup -1}. Optical and scanning electronic microscope (SEM) were used to observe the microstructure evolution and fracture behavior in superplastic deformation of AZ31 Mg alloy and the values of deformation activation energy at various temperatures were calculated. It is demonstrated that, the hot-rolled AZ31 alloy begins to exhibit superplasticity from 300 C and a maximum elongation of 362.5% is obtained at 400 C and 0.7 x 10{sup -3} s{sup -1}. In the temperature range 300{proportional_to}400 C, the dominant superplastic deformation mechanism is grain boundary sliding (GBS) controlled by ...

2005-07-01

147

Experimental investigation on the fretting wear of alloy 800 in room remperature water  

Energy Technology Data Exchange (ETDEWEB)

Fretting wear test in room temperature water was performed to evaluate the wear coefficient of CANDU (CANadian Deuterium Uranium) steam generator (SG) tube material (Alloy 800) against 410 type martensitic stainless steels. The main focus is to compare the wear behaviors between Alloy 800 and Inconel 690. Test conditions are 10{approx}30N of normal load, 200{approx}450mm of sliding amplitude and 30Hz of frequency. The result indicated that the wear rate of Alloy 800 was higher than those of Inconel 690 at various test condition such as normal loads, sliding amplitudes etc. From the results of SEM observation, there was little evidence of plastic deformation layer that were dominantly formed on the worn surfaces of Inconel 690. Also, wear particles in Alloy 800 were released from contacting asperities deformed by severe plastic flow during fretting wear. Main cause of wear rate between ...

2002-05-01

148

Experimental investigation on the fretting wear of alloy 800 in room remperature water  

International Nuclear Information System (INIS)

Fretting wear test in room temperature water was performed to evaluate the wear coefficient of CANDU (CANadian Deuterium Uranium) steam generator (SG) tube material (Alloy 800) against 410 type martensitic stainless steels. The main focus is to compare the wear behaviors between Alloy 800 and Inconel 690. Test conditions are 10#approx#30N of normal load, 200#approx#450mm of sliding amplitude and 30Hz of frequency. The result indicated that the wear rate of Alloy 800 was higher than those of Inconel 690 at various test condition such as normal loads, sliding amplitudes etc. From the results of SEM observation, there was little evidence of plastic deformation layer that were dominantly formed on the worn surfaces of Inconel 690. Also, wear particles in Alloy 800 were released from contacting asperities deformed by severe plastic flow during fretting wear. Main cause of wear rate between ...

2002-05-01

149

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 1. Roles on corrosion  

Energy Technology Data Exchange (ETDEWEB)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. This paper describes the roles on corrosion. A corrosion test on precipitate-containing and precipitate-free materials made from pure zirconium and a small quantity of iron and chromium, rest potential measurements on an intermetallic compound of Zr(FeCr){sub 2} and zirconium matrix, and a galvanic coupling test of those were performed. Results showed that corrosion behavior of zirconium alloys could be attributed to the electrochemical properties of intermetallic compounds precipitated in each alloy. Namely, the cathodic and anodic polarization characteristics were associated with anodic protection provided by the precipitates on the alloys and the precipitates degradation in ...

2000-07-01

150

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 1. Roles on corrosion  

International Nuclear Information System (INIS)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. This paper describes the roles on corrosion. A corrosion test on precipitate-containing and precipitate-free materials made from pure zirconium and a small quantity of iron and chromium, rest potential measurements on an intermetallic compound of Zr(FeCr)_2 and zirconium matrix, and a galvanic coupling test of those were performed. Results showed that corrosion behavior of zirconium alloys could be attributed to the electrochemical properties of intermetallic compounds precipitated in each alloy. Namely, the cathodic and anodic polarization characteristics were associated with anodic protection provided by the precipitates on the alloys and the precipitates degradation in the ...

2000-07-01

151

Effect of minor alloying element variation on the properties of Alloy 800  

International Nuclear Information System (INIS)

Application of Alloy 800 in steam generator tubing of fast reactors, where continuous service temperature of the order of 550"0C is experienced, has been analyzed with respect to small variations in its chemical composition. Several laboratory melts of Alloy 800 have been prepared and their microstructural and mechanical property changes during simple aging and creep tests at 500 to 600"0C have been studied. It has been found that in the above temperature range precipitation of M_2_3C_6 on the grain boundaries is independent of the Ti : C ratio generally specified for Alloy 800. Gamma prime precipitation occurred in alloys containing as low as 0.5 percent Ti + Al after 1000 h of aging and was accompanied with a creep ductility decline. Upon #gamma# precipitation creep rate was retarded and its reacceleration for test times up to 8500 h at 550"0C was not observed. Based on the ...

152

Corrosion behavior of materials at high temperature by environmental oxidants containing sulfur derivatives: effects of aggressive phase composition on experimental alloys. Final report  

Energy Technology Data Exchange (ETDEWEB)

For a better understanding of sulphidation mechanisms, some alloys (alloy 600, alloy 800, Uranus S, iron-chromium-aluminium-alloy) and metals (iron, chromium, nickel, molybdenum, titanium) were tested at 773, 873, 1 073 K in gaseous sulphur dioxide. Total pressure was 760 torrs. Sulphur dioxide pressure was 760, 100 and 10 torrs. Argon, oxygen, water vapor were used, successively, as pressure complement. Oxygen supply, generally speaking cause decay of corrosion resistance in SO/sub 2/ atmospheres especially at 1 073 K with low ratio p/sub O2//P/sub SO/sub 2//. Water vapor supply act similarly. Temperature laws and pressure laws do not give monotonous rise of corrosion values. There are maximas suggesting corrosion products undertaking a volatilization process. According to test conditions, Uranus S, chromium, alloy 800 (and titanium at some extent) showed good ...

1981-01-01

153

Corrosion and mass transfer of ternary alloys (Fe-Ni-Cr) in anisothermal semi-stagnant Pb17Li  

Energy Technology Data Exchange (ETDEWEB)

Corrosion of several materials including pure metals Fe, Ni, Cr and also Fe-Cr, Fe-Ni-Cr alloys, has been studied in anisothermal Pb17Li (Tmax = 500 deg C; {Delta}T = 60 deg C). The corrosion rate of pure nickel is two orders of magnitude higher than the chromium one and about three orders of magnitude higher than the iron one. Fe-Cr alloys (1.4914) suffers a dissolution rate equal to the one of its major constituent, iron. With regard to the three austenitic materials (316L and NS20 steels, alloy 800), they exhibit a porous corrosion layer mainly constituted of ferrite but containing also a small amount of {sigma} phase in the case of the alloys with higher Ni content, NS30 steel and alloy 800. Mechanism of formation of this layer is discussed.

1990-12-31

154

Anisotropic properties of magnesium sheet AZ31  

Energy Technology Data Exchange (ETDEWEB)

Car weight corresponds directly to fuel consumption and driving performance. So in order to improve the fuel efficiency and performance of a car the weight has to be reduced. Magnesium as a light metal offers a wide range of weight saving opportunities, especially Magnesium wrought alloys with their improved mechanical properties have a high potential for structural applications. Mechanical properties in terms of their quality and anisotropy are dependent on the microstructure of the material and can be characterized by their degree of inhomogeneity, their grain size distribution and their crystallographic texture. Therefore the orientation distribution of grains, the grain size, its size distribution, the chemical composition (precipitates) itself influence the mechanical parameters and their anisotropy. In this presentation first results of mechanical anisotropy are given: ...

2003-07-01

155

Properties of Beta-C trademark (Ti-3Al-8V-6Cr-4Mo-4Zr)  

International Nuclear Information System (INIS)

Beta C trademark, a metastable beta titanium alloy developed by RMI Titanium Company, continues to be used in new applications due to its excellent mechanical properties and resistance to corrosion. New data in this paper include mechanical properties in large sections, cold drawn bar and welds. Fatigue crack growth and corrosion data are added to supplement previously published data.

1993-02-21

156

Sulfidation-resistant alloy/cladding for internal components of coal-conversion equipment. Volume 2. Cladding development. Final report  

Energy Technology Data Exchange (ETDEWEB)

An Fe-19Cr-8Al-0.5Hf alloy has been roll bonded to Alloy 800 to form a protective clad material suitable for use in coal conversion atmospheres. The commercial producibility of both the Fe-19Cr-8Al-0.5Hf alloy and the clad composite has been demonstrated. The clad composite has been shown to exhibit resistance to sulfidation in high sulfur, coal gasification atmospheres low Btu for 2000 hrs at 1800/sup 0/F (1255K). The FeCrAlHf alloy must be preoxidized in the absence of sulfur to form fully protective alumina scales on all surfaces. Useful life of the composite at temperatures of 1400 to 2000/sup 0/F (1033 to 1366K) is governed by reactions at the FeCrAlHf clad alloy 800 interface. The rate of interdiffusion decreases with increasing Ni content and a high Ni alloy such as RA333 appears to be a better substrate than Alloy 800 for a FeCrAlHf ...

1981-12-01

157

Stress corrosion cracking susceptibility of alloy 800  

Energy Technology Data Exchange (ETDEWEB)

Steam generators (SGs) in PWRs and CANDUs are designed for at least a 30-year operating life. However, in the 15-25 years that SGs tubed with Alloy 600 have operated commercially, they have experienced reduced reliability, mainly due to SG tubing degradation. One of the degradation mechanisms that Alloy 600 SG tubing has suffered from is lead-induced stress corrosion cracking (PbSCC) in AVT and near-neutral SG environments. In contrast to Alloy 600 tubing, test data obtained in high temperature water indicate that Alloy 800 is resistant to cracking by lead and lead compounds. For Alloy 800 (cold worked, shot peened), the most aggressive environment is reported to be alkaline with minor concentration of PbO (80 ppm). Work by Max Helie et al. also concluded that Alloy 800 is not sensitive to lead assisted SCC for pH values close to neutrality, ...

2002-07-01

158

Stress corrosion cracking susceptibility of alloy 800  

International Nuclear Information System (INIS)

Steam generators (SGs) in PWRs and CANDUs are designed for at least a 30-year operating life. However, in the 15-25 years that SGs tubed with Alloy 600 have operated commercially, they have experienced reduced reliability, mainly due to SG tubing degradation. One of the degradation mechanisms that Alloy 600 SG tubing has suffered from is lead-induced stress corrosion cracking (PbSCC) in AVT and near-neutral SG environments. In contrast to Alloy 600 tubing, test data obtained in high temperature water indicate that Alloy 800 is resistant to cracking by lead and lead compounds. For Alloy 800 (cold worked, shot peened), the most aggressive environment is reported to be alkaline with minor concentration of PbO (80 ppm). Work by Max Helie et al. also concluded that Alloy 800 is not sensitive to lead assisted SCC for pH values close to neutrality, ...

2002-05-05

159

The influence of powder particle size on the mechanical properties of two rapidly solidified Al-Fe-Ce alloys. Pt. 2; Mechanical properties  

Energy Technology Data Exchange (ETDEWEB)

Two rapidly solidified powders with compositions Al-6.7 wt.% Fe-5.9 wt.% Ce and Al-6.2 wt.% Fe-5.9 wt.% Ce-1.63 wt.% Si were separated into -32 [mu]m and +32 to -63 [mu]m size fractions. Powders from both size fractions were extruded at 500 C. For comparison purposes, extrusion at a lower temperature of 400 C was also performed. In this investigation, tensile property evaluation indicated that processing of finer size fractions at high temperature offers no advantages in terms of the tensile properties but is advantageous in terms of improving the fracture toughness of alloy B. These observations underline the importance of the stability of powder microstructure during thermomechanical processing for the development of optimum mechanical properties. (orig.)

1994-04-01

160

Effect of globular structure op mechanical properties of VT3-1 alloy  

International Nuclear Information System (INIS)

Effect of globular structure parameters - size of primary #alpha#-phase particles (bsub(I)), thickness and amount of plates of secondary #alpha#-phase (bsub(II), #gamma#sub(II#alpha# )) - on a complex of mechanical properties (#sigma#sub(#beta#), S, phi, asub(H), asub(T), Ksub(Q), #sigma#sub(-1), #sigma#_1_0_0"4"5"0, #sigma#sub(0.2/100)) of VT3-1 (#alpha#+#beta#)-titanium alloy is studied. The dependences obtained allow one to determine globular structure parameters, providing necessary mechanical properties. In combination with data on the effect of thermal treatment conditions on structure parameters, results obtained in the paper may be used for structure control to increase a level of required characteristics.

161

Analysis of the mechanical properties of metal-ceramic interfaces using the four-point bending test: application to dental metal-ceramic couples (Pd-Ag, Pd-Au)  

International Nuclear Information System (INIS)

Different semi precious alloys (Pd-Ag, Pd-Au) have been studied after thermal oxidation treatments to analyze the mechanical improvement of the interface between the metal and the ceramic. Using the four point bending test, the authors have analyzed the different steps corresponding to the mechanical evolution of the bi-material : cracking energy on the surface, relaxation energy after first cracking, propagation energy of cracks at the interface zone. It has been shown that some alloys only have a high resistance to the interface cracking and the role played by the interface reactions to improve this property. (orig.).

1993-06-01

162

Electrochemical and chemical dissolution behavior of Zn-Fe alloy coatings and its application to the analysis of Zn-Fe alloy layer. Zn-Fe kei mekki so no bunkyokuter dot yokai kyodo to teiryo bunseki eno oyo  

Energy Technology Data Exchange (ETDEWEB)

As surface treated steel sheets, steel sheets with Zn-Fe coatings as well as double-layer steel sheets with Fe-P alloy coatings on Zn-Fe alloy coatings are often used practically. Two treatment methods, which are used to dissolve only alloy layers without dissolving steel sheets in order to find amount and composition of alloy layersr have already been reported. This report investigates the mechanisms of these methods, particularly the mechanisms to control dissolution of steel sheets. In the alkali-dissolution method, Zn-Fe alloy coatings are dissolved in a strong alkaline solution(NaOH-triethanolamine (TEA)-H{sub 2}O{sub 2}). In this case, steel sheets are insoluble because passive films are formed on the surface. In the cathodic polarization electrolysis method, alloy layers are electrolyzed({minus}l.2V) and dissolved ...

1991-11-01

163

Effect of mating surface on the high temperature wear of 253 MA alloy  

Energy Technology Data Exchange (ETDEWEB)

The wear behaviour of metallic material is influenced by the friction force, which in turn, is governed by the hardness and oxidation kinetics of the mating surface. In view of this, present investigation is undertaken to find the influence of mating surface on the high temperature wear of 253 MA alloy. This alloy is developed for high temperature application. In this work 253 MA alloy is made to slide against two different types of counter face material, namely 100Cr6 steel and PM 1000 alloy, at five different temperatures. 100Cr6 steel gets soften with increase of temperature whereas PM 1000 alloy retains its strength even at high temperature. The friction coefficient and the thickness loss of 253 MA alloy is measured and compared against both variety of mating surfaces as function of temperatures. The morphology of the worn surfaces and the transverse section ...

2004-04-01

164

Microstructure/Mechanical property relationships in bar products of Beta-C trademark (Ti-3Al-8V-6Cr-4Mo-4Zr)  

International Nuclear Information System (INIS)

Beta-C trademark is a metastable beta titanium alloy which can be heat treated to achieve a good combination of properties such as tensile strength, fatigue strength, ductility and toughness, such as needed in aircraft fasteners. Variations in hot and cold processing parameters and solution heat treatment can affect the resultant grain structure which in turn affects subsequent aging response and mechanical properties. Several processing/heat treating routes on round bar are explored in this study to determine the effects on microstructure and various mechanical properties.

1993-02-21

165

A comparative evaluation of welding consumables for dissimilar welds between 316LN austenitic stainless steel and Alloy 800  

Energy Technology Data Exchange (ETDEWEB)

Transition joints in power plants between ferritic steels and austenitic stainless steels suffer from a mismatch in coefficients of thermal expansion (CTE) and the migration of carbon during service from the ferritic to the austenitic steel. To overcome these, nickel-based consumables are commonly used. The use of a trimetallic combination with an insert piece of intermediate CTE provides for a more effective lowering of thermal stresses. The current work envisages a trimetallic joint involving modified 9Cr-1Mo steel and 316LN austenitic stainless steel as the base materials and Alloy 800 as the intermediate piece. Of the two joints involved, this paper describes the choice of welding consumables for the joint between Alloy 800 and 316LN. Four consumables were examined: 316, 16-8-2, Inconel 82 and Inconel 182. The comparative evaluation was based on hot cracking tests and estimation of mechanical properties and coefficient ...

2000-03-01

166

Structure and magnetic properties of nanocrystalline Fe-Mo alloys prepared by mechanosynthesis  

International Nuclear Information System (INIS)

Nanocrystalline samples of Fe_8_0Mo_2_0 and Fe_5_0Mo_5_0 alloys were prepared by the mechanical milling method. The structure, lattice parameters, and crystallite size were determined by the X-ray diffraction. The magnetic properties of the milled products were determined by the Moessbauer spectroscopy. It was observed that in the case of the Fe_8_0Mo_2_0 alloy a solid solution of Mo in Fe was formed with the lattice parameters of the Fe increasing from 0.28659 nm to 0.29240 nm and the crystallite size decreasing from 250 nm to 20 nm. In the case of the Fe_5_0Mo_5_0 alloy there were no clear changes in values of the lattice parameters of Fe and Mo during the milling process, but the crystallite size decreased from 200 to 15 nm. Moessbauer spectra revealed different magnetic phases in the machanosynthesized Fe_Mo samples. In the case of the Fe_8_0Mo_2_0 alloy, the spectrum for the ...

2001-09-23

167

Plastic instability in an omega forming Ti-l5% Mo alloy  

International Nuclear Information System (INIS)

The plastic flow behavior of a #beta#-titanium alloy (Ti-15% Mo) was investigated over a wide range of temperatures and strain rates covering those conditions where the #omega#-phase forms dynamically. Portevin-Le Chatelier (PLC) effect was observed in this alloy at temperatures between 575 and 775 K at a strain rate of 1.31 x 10"-"4 s"-"1. The serrated flow behavior of this alloy could be suppressed by rendering the matrix #beta#-phase more stable against the #beta# to #omega# transformation. PLC bands formed in this alloy, studied at different levels of magnification using light, scanning electron and transmission electron microscopy, showed a high density of deformation bands within the macroscopic PLC band. The following mechanism of serrated flow is proposed; the load drop is ascribed to the sudden flow associated with the formation of deformation bands within which ...

168

Oxidation and chromium depletion of Alloy 800 and 316SS by molten NaNO/sub 3/-KNO/sub 3/ at temperatures above 600/degree/C  

Energy Technology Data Exchange (ETDEWEB)

The corrosion behavior of Alloy 800 and Type 316 stainless steel in molten NaNO/sub 3/-KNO/sub 3/ was studied at temperatures from 605/degree/C to 630/degree/C. Corrosion behavior was significantly different from that previously reported in nitrate melts at temperatures up to 600/degree/C and involved a combination of oxidation, internal nitridation and sodium metallate formation. Corrosion kinetics, determined metallographically, switched from a parabolic to a linear rate equation as temperature increased. Corrosion was uniform and resulted in metal losses on the order of 100 micronsyear at 630/degree/C. Among the alloying elements, chromium was depleted from the alloy as the result of a basic fluxing process. The kinetic equations describing chromium depletion also changed from parabolic to linear with increasing temperature. The effect of the equilibrium chemistry of the melt on the corrosion behavior of the ...

1987-01-01

169

Mechanisms controlling the composition influence on radiation hardening and embrittlement of iron-base alloys  

International Nuclear Information System (INIS)

Classification and ranking of the solid solution on their reaction to the irradiation is suggested on the basis of binary system structure controlled by mixing enthalpy sign, melting temperatures relation of components and solidus curves slope. Several combinations of these characteristics permit to pick out three groups of substitutional elements capable of forming the vacancy-solute atom complexes either low-mobile or fast-mobile ones as compared to monovacancies migration. The radiation hardening (and embrittlement) of binary alloys should be intensified respectively either due to heterogeneous point defect clusters nucleation on solute traps or due to solute atom clusters/ precipitate formation. A local cohesion decrease may also occur especially if low-melting elements (characterized by low surface energy) are segregating on internal sinks or grain boundaries. The predicted specifics of different alloy group under irradiation and during ...

1994-06-20

170

Interactions between creep and corrosion in Alloy 800  

Energy Technology Data Exchange (ETDEWEB)

Metallic components within or immediately adjacent to gasifiers, such as gas distributors, thermowells, transfer lines, and cyclones, are subjected to severe of temperature, pressure, and hostile multicomponent gas environments. Metallic heat exchangers/waste-heat boilers resistant to sulfidation, corrosion. and erosion in low- and medium-Btu gas environments are essential components in large-scale gasification schemes, in both dry ash and slogging type gasifiers. Components, in general. must be resistant to corrosion, erosion, and high-temperature creep. A substantial data base is needed on the mechanical properties of materials exposed to complex gas environments to provide a more viable basis for establishing long-term reliability of components. This work examines high-temperature creep of Alloy 800, a high-chromium alloy widely used in coal conversion systems, after exposure to oxygen and oxygen/sulfur mixed-gas ...

1994-04-01

171

Influence of alloying elements on the irradiation hardening and environmental sensitivity of zirconium alloys  

International Nuclear Information System (INIS)

Ten different alloys of zirconium have been tested with regard to the effect of irradiation on their mechanical properties and their sensitivity to environmentally induced failure. Two different environments were used: iodine vapour and liquid cesium with an addition of 2% cadmium. The neutron dose was 10"2"1n/cm"2 (E>1MeV) and the irradiation temperature was about 300 degrees C. All alloy additions increased the irradiation hardening. Especially notable was the large effect of titanium and tin on irradiation hardening. A limited amount of transmission electron microscopy was carried out in order to find an explanation to the effects. The testing in different environments showed that there is no clear correlation between environmental sensitivity and yield stress. For materials of similar yield stress an alloyed material tends to be more sensitive to environmental cracking than a material which only ...

1991-08-25

172

Fatigue and creep crack growth of Alloy 800 and Alloy 617 at high temperatures  

Energy Technology Data Exchange (ETDEWEB)

A common evaluation is given for creep crack growth and fatigue crack growth experiments which have been performed at the companies ABB, Siemens-KWU and KFA. The materials under investigation were X10NiCrAlTi32 20 (Alloy 800) and NiCr22Col2Mo (Alloy 617). Several production lots and semi-finished materials as well as welded materials have been tested. Testing techniques differed at the different labs. In order to eliminate the influence of individual testing techniques, material from some production lots was investigated at different labs. The given data cover fatigue crack growth (the materials were tested between room temperature and 1050[sup o]C; the influence of temperature, R-ratio, and frequency was investigated) and creep crack growth (Alloy 800 was tested between 550sup(o)C and 900sup(o)C, Inconel 617 between 800sup(o)C and 1000sup(o)C; the evaluation was done on the basis of the fracture ...

1992-01-01

173

Fatigue and creep crack growth of Alloy 800 and Alloy 617 at high temperatures  

International Nuclear Information System (INIS)

A common evaluation is given for creep crack growth and fatigue crack growth experiments which have been performed at the companies ABB, Siemens-KWU and KFA. The materials under investigation were X10NiCrAlTi32 20 (Alloy 800) and NiCr22Col2Mo (Alloy 617). Several production lots and semi-finished materials as well as welded materials have been tested. Testing techniques differed at the different labs. In order to eliminate the influence of individual testing techniques, material from some production lots was investigated at different labs. The given data cover fatigue crack growth (the materials were tested between room temperature and 1050"oC; the influence of temperature, R-ratio, and frequency was investigated) and creep crack growth (Alloy 800 was tested between 550sup(o)C and 900sup(o)C, Inconel 617 between 800sup(o)C and 1000sup(o)C; the evaluation was done on the basis of the fracture mechanics ...

174

Behavior at under-film corrosion tips of Zn-Fe alloy coated steel sheets. Zn-Fe gokin mekki koban no tomakushita fushoku ni okeru fushoku sentanbu no kyodo  

Energy Technology Data Exchange (ETDEWEB)

From a macroscopic point of view, corrosion of Zn alloy coated steel sheet occurs by the coating preceding corrosion mechanism; microscopically, however, the coated layer corrosion velocity in the tip of corrosion is different. In order to find the main factors of under-film corrosion of Zn and Zn-Fe alloy coatings in the salt water spray atmospheric exposure test, the correlation between point inflation-exfoliation width and chlorine penetration behavior, point adhesion, and the difference in chlorine penetration behavior due to alloy coating components were investigated. Consequently, the following results were obtained: 1. The better correlation was observed between chlorine penetration distance and point inflation-point exfoliation width. 2. The durability of coating against chlorine penetration improved by increase in point adhesion and Zn content in the coating layer. 3. Zn-Fe (10-20%) ...

1990-09-01

175

Understanding and protecting steam generator materials  

Science.gov (United States)

Solid solution-strengthened nickel base alloys have been used for nuclear stream generator tubing in pressurized water reactors since the beginnings of commercial nuclear power. The purpose of this paper is to recap and update the authors understanding of the relationship between processing, resulting structure, and properties for Alloy 600 and to discuss the requirements for optimized performance in both primary and secondary environments. Potential replacement materials and their performance will be discussed. Also discussed is the role and importance of system chemistry, bulk and local, and control and its relationship to performance. A discussion of potential mechanisms of environmentally assisted failure is also discussed.

1986-01-01

176

Understanding and protecting steam generator materials  

International Nuclear Information System (INIS)

Solid solution-strengthened nickel base alloys have been used for nuclear stream generator tubing in pressurized water reactors since the beginnings of commercial nuclear power. The purpose of this paper is to recap and update the authors understanding of the relationship between processing, resulting structure, and properties for Alloy 600 and to discuss the requirements for optimized performance in both primary and secondary environments. Potential replacement materials and their performance will be discussed. Also discussed is the role and importance of system chemistry, bulk and local, and control and its relationship to performance. A discussion of potential mechanisms of environmentally assisted failure is also discussed.

1986-11-16

177

Study of titanium-niobium alloys manufactured by magnesium thermic reduction of chlorides  

International Nuclear Information System (INIS)

Chemical and phase homogeneity of titanium-niobium sponge, produced by a combined magnesium-thermic reduction of niobium pentachloride and titanium tetrachloride mixtures, is investigated. It is ascertained that a sponge consists of spherical shape particles and has a large number of pores. Particle sizes are reduced with niobium being substituted for titanium from 50-500 #mu#m for titanium sponge to 1-40 #mu#m for niobium one, which testifies to the bormation in a titanium-niobium sponge of an alloy and not a mechanical mixture. A number of solid solutions is detected by X-ray phase analysis. Lattice parameters are determined.

178

Point defect supersaturation and enhanced diffusion in SPE regrown silicon  

Energy Technology Data Exchange (ETDEWEB)

Transient, greatly enhanced diffusion has been observed on annealing solid-phase-epitaxial (SPE) grown Si-Sb alloys. This is shown to be due to a high concentration of interstitials being trapped during SPE regrowth. The migration enthalpy, for diffusion of Sb by an interstitialcy mechanism was measured as 1.8 +/- 0.2 eV. The interstitials eventually condensed into loops, marking the end of the transient. In a SPE grown Si-Bi alloy a similar transient enhanced diffusion was observed, with an activation energy of 2.0 +/- 0.2 eV, but no loops formed. 8 figures, 7 references.

1984-01-01

179

Point defect supersaturation and enhanced diffusion in SPE regrown silicon  

International Nuclear Information System (INIS)

Transient, greatly enhanced diffusion has been observed on annealing solid-phase-epitaxial (SPE) grown Si-Sb alloys. This is shown to be due to a high concentration of interstitials being trapped during SPE regrowth. The migration enthalpy, for diffusion of Sb by an interstitialcy mechanism was measured as 1.8 +/- 0.2 eV. The interstitials eventually condensed into loops, marking the end of the transient. In a SPE grown Si-Bi alloy a similar transient enhanced diffusion was observed, with an activation energy of 2.0 +/- 0.2 eV, but no loops formed. 8 figures, 7 references.

180

Neutron irradiation effects in austenitic alloys  

International Nuclear Information System (INIS)

The post (neutron) -irradiation high-temperature tensile and creep-rupture properties, deformation and fracture characteristics of austenitic alloys, particularly solution annealed Type 316 steel, are surveyed and correlated with the damage structures developed as a function of irradiation temperature (and dose). The mechanisms proposed to explain the irradiation-induced changes in properties and behaviour are summarised. The factors responsible for the observed differences in the post-irradiation and 'in-reactor' creep-rupture properties and behaviour of an austenitic steel are discussed in terms of the helium gas and stress driven growth of small intergranular bubbles and the atom plating associated with their growth and coalescence. (author).

1980-03-01

181

Microstructure, texture and mechanical properties of the magnesium alloy AZ31 processed by ECAP  

Energy Technology Data Exchange (ETDEWEB)

To investigate the influence of equal channel angular pressing on the microstructure and texture of the magnesium alloy AZ31, electron backscattering diffraction and well as neutron diffraction experiments were carried out. Through these experiments it was possible to trace the microstructure and texture evolution with strain accumulated with the increasing number of equal channel angular pressing passes. It was further demonstrated by subsequent compression tests that the microstructural changes produced by equal channel angular pressing have a beneficial effect on both the compressive strength and ductility of AZ31. (orig.)

2008-01-15

182

Electrodynamical and quantum-chemical approaches to modeling the electrochemical and catalytic processes on metals, metal alloys, and semiconductors  

British Library Electronic Table of Contents (United Kingdom)

A problem of the catalytic activity definition for metals, binary metallic alloys, and semiconductor materials is considered within new quantum mechanical and electrodynamics approach in the electron theory of catalysis. The quantitative link between the electron structure parameters of the materials and their catalytic activity on example of simple model reactions of the following type are found: H = H+ + e, O2 + e- = O2-. Copyright 2009 Wiley Periodicals, Inc. Int J Quantum Chem, 2009

2009-01-01

183

Effects of focused ion beam milling on the nanomechanical behavior of a molybdenum-alloy single crystal  

International Nuclear Information System (INIS)

Nanoindentation was performed on a Mo-alloy single crystal to investigate effects of focused ion beam (FIB) milling on mechanical behavior. On a non-FIB-milled surface, pop-ins were observed on all load-displacement curves corresponding to a transition from elastic to plastic deformation. Similar pop-ins were not detected on surfaces subjected to FIB milling. This difference indicates that FIB milling introduces damage that obviates the need for dislocation nucleation during subsequent deformation. A second effect of FIB milling is that it increased the surface hardness. Together, these effects could be the source of the size effects reported in the literature on micropillar tests.

2007-09-10

184

Effect of intense plastic straining on microstructure and mechanical properties of an Al-Mg-Sc alloy  

International Nuclear Information System (INIS)

An Al-5%Mg-0.18%Mn-0.2%Sc-0.08%Zr-0.002%Be was subjected to equal-channel angular extrusion up to true strains of #approx#3 and #approx#8, that resulted in the formation of partially recrystallized and fully recrystallized structure, respectively. It was shown that the alloy with partially recrystallized structure exhibits highest strength and ductility. The material with fully recrystallized structure showed lowest fatigue crack growth rate and highest value of fracture toughness. Reasons of this unusual effect of microstructure on crack propagation resistance under fatigue are discussed.

2010-07-01

185

Comprehensive characterization of fuel, clad and wrapper materials and assemblies for fast reactors - towards design, development and performance  

International Nuclear Information System (INIS)

The paper provides a brief description of the fuel characterization for Fast Breeder Test Reactor (FBTR) and Prototype Fast Breeder Reactor (PFBR). The development and characterization of mechanical properties of Alloy D9 clad and wrapper tubes are discussed. The problems associated with fusion welding of Alloy D9 are outlined. Non-destructive characterization of cladding tubes by optimum encircling eddy current probes, on-line and off-line neural network methods is presented. Both the on-line and off-line neural network methods could readily detect and size defects specified by the designers

2004-01-01

186

GRAIN REFINEMENT OF PERMANENT MOLD CAST COPPER BASE ALLOYS  

Energy Technology Data Exchange (ETDEWEB)

Grain refinement behavior of copper alloys cast in permanent molds was investigated. This is one of the least studied subjects in copper alloy castings. Grain refinement is not widely practiced for leaded copper alloys cast in sand molds. Aluminum bronzes and high strength yellow brasses, cast in sand and permanent molds, were usually fine grained due to the presence of more than 2% iron. Grain refinement of the most common permanent mold casting alloys, leaded yellow brass and its lead-free replacement EnviroBrass III, is not universally accepted due to the perceived problem of hard spots in finished castings and for the same reason these alloys contain very low amounts of iron. The yellow brasses and Cu-Si alloys are gaining popularity in North America due to their low lead content and amenability for permanent mold casting. These alloys ...

2004-04-29

187

The compatibility of alloy 800 in HTR atmospheres  

International Nuclear Information System (INIS)

A thermodynamic analysis of the behaviour of Alloy 800 in helium based atmospheres relevant to the High Temperature Gas Cooled Reactor indicates that, depending upon the precise gas composition, oxidation and carburisation, or carburisation alone may be expected. The prime influence appears to be the moisture level. The morphology and structure of the reaction products are discussed. It is shown that the 'reactive' elements chromium, manganese, titanium and silicon are concentrated in the oxide scale which is normally duplex in structure. Aluminium oxide is formed at grain boundaries and in an internal oxidation zone together with titanium and sometimes silicon. In carburising conditions, mixed titanium-chromium carbides are formed. When this occurs, intergranular penetration is maximised. Weight gain data are assessed and briefly described and a tentative model for the mechanism of corrosion of Alloy 800 in HTR helium is ...

188

Properties and processing of TIMETAL LCB  

Science.gov (United States)

TIMETAL LCB was introduced more than 10 years ago targeting automotive suspension spring applications. The alloy development aim was to use a low-cost formulation by selecting less expensive raw materials than typical beta titanium alloys. Following the first successful application of TIMETAL LCB suspension springs to series production vehicles, the 2000 Volkswagen Lupo FSI, the springs have been used for Ferrari Challenge Stradale since 2003. The most recent development effort was focused on the generation of metallurgical and mechanical service data for the alloy, and the implementation of efficient low cost processing of coils. This paper will introduce various properties of TIMETAL LCB products that can be useful in the design and the consideration of spring applications. Recent progress in the processing of TIMETAL LCB will also be introduced and discussed.

2005-12-01

189

Plasma nitriding of microalloyed steel  

Energy Technology Data Exchange (ETDEWEB)

Microalloyed or high strength low alloy (HSLA) steels are carbon-manganese steels containing small amounts of Nb, V or Ti. The excellent mechanical properties of these alloys, particularly high yield strength, usually obviate the need for expensive quench and tempering operations. Furthermore, the presence of a significant amount of nitride-forming elements in some microalloyed steels has generated interest in the applicability of these alloys as a new generation of nitriding steels. In this paper, a study of the plasma nitriding behaviour of a commercially available microalloyed steel MAXIMA{sup TM} is reported. A comparison is made with a traditional quenched and tempered nitriding steel (En19), plasma nitrided under similar conditions. Optical and scanning electron microscopy in conjunction with microhardness measurements and X-ray diffraction were utilized to characterize the nitrided surfaces. The ...

1995-03-01

190

Measuring back stresses in commercial alloys at elevated temperatures. [922/sup 0/K  

Energy Technology Data Exchange (ETDEWEB)

Strain transient dip tests have been conducted on two commercial heats of Alloy 800 at 922 K. Tests were conducted on both a servo-controlled hydraulic machine and a specially designed dip test machine. Using measured maximum strain changes during dips allowed unambiguous definition of a kinematic variable. The several other methods of interpreting dip test data by attempting to measure strain rates shortly after the unloading decrements were found not to be satisfactory. The nature of the instantaneous unloading strains and the strain transients following unloading are also discussed in terms of the mechanisms of deformation in Alloy 800. 9 figures, 3 tables.

1982-01-01

191

Investigation of weld cracking in alloy 800  

Energy Technology Data Exchange (ETDEWEB)

The subscale Varestraint test has been used to determine the relative hot cracking susceptibility of the fusion zone in four commercial heats of alloy 800. Although all four heats were susceptible to cracking, one heat exhibited a significant increase in cracking relative to the other three. Optical metallography revealed that nearly all the cracking was localized along fusion zone grain boundaries. Microprobe analysis of the grain boundaries detected high concentrations of titanium, silicon, and niobium resulting from partitioning during solidification. The fusion zone hot cracking mechanism in alloy 800 involves the complex interaction of titanium, silicon, niobium, and carbon along the solidification boundaries. SEM and Auger analyses of the hot crack fracture surfaces revealed the presence of (Ti, Nb)-rich carbides, suggesting that these particles precipitate from the liquid which solidifies last on the fracture ...

1984-03-01

192

High temperature deformation behaviour of Ti-10V Alloy and associated activation energy  

International Nuclear Information System (INIS)

High temperature deformation behaviour of an experimental Beta-titanium alloy Ti-10V has been studied in the temperature range 800 to 945 degree C by using the method of crosshead speed cycling. Although subgrain formation was observed but the alloy did not exhibit superplastic behaviour in the entire temperature range studied. A very large initial grain size and elongation of grains during the deformation are considered the main factors responsible for absence of superplastic behaviour. The activation energy values for regions II and III of the ln sigma vs. ln small epsilon plots are close to the lower of the two activation energy values proposed together to describe self diffusion in beta-phase suggesting that the rate controlling mechanism is that for lattice diffusion rather then grain boundary diffusion. (author)

2004-06-01

193

High coercivity in Nd-Fe-Al-Co-B alloys prepared by mechanical milling  

Energy Technology Data Exchange (ETDEWEB)

Nd{sub 40}Fe{sub 30}Al{sub 10}Co{sub 15}B{sub 5} alloys were fabricated by high energy ball milling method under various conditions. Microstructure of the alloys was investigated by X-ray diffraction and electron microscopy techniques. Magnetic properties were characterized by hysteresis and thermomagnetic measurements. The high coercive fields up to 2.36 T have been observed on the samples consisting of Nd{sub 2}(Fe,Co,Al){sub 14}B, Nd{sub 6}(Fe,Co,Al){sub 14} and Nd crystallites imbedded in a residual amorphous matrix.

2008-02-15

194

Electrochemical properties and growth mechanism of passive films on Alloy 690 in high-temperature alkaline environments  

Energy Technology Data Exchange (ETDEWEB)

Passive films formed on Alloy 690 in high-temperature alkaline environments were investigated by potentiodynamic polarization, X-ray photoelectron spectroscopy, transmission electron microscopy and Mott-Schottky approach. Passive current density and donor density of the passive films increase with increasing temperature, due to increased diffusion rates of metallic ions and dehydration of hydroxide phases. The passive films show a duplex structure including an inner layer of fine-grained Cr oxide or spinel oxide and an outer layer of Ni-Fe spinel oxide and Ni hydroxide. A growth model of the passive films on Alloy 690 in high-temperature alkaline environments is proposed and discussed.

2010-10-15

195

Electrochemical properties and growth mechanism of passive films on Alloy 690 in high-temperature alkaline environments  

International Nuclear Information System (INIS)

Passive films formed on Alloy 690 in high-temperature alkaline environments were investigated by potentiodynamic polarization, X-ray photoelectron spectroscopy, transmission electron microscopy and Mott-Schottky approach. Passive current density and donor density of the passive films increase with increasing temperature, due to increased diffusion rates of metallic ions and dehydration of hydroxide phases. The passive films show a duplex structure including an inner layer of fine-grained Cr oxide or spinel oxide and an outer layer of Ni-Fe spinel oxide and Ni hydroxide. A growth model of the passive films on Alloy 690 in high-temperature alkaline environments is proposed and discussed.

2010-10-01

196

A review of the structural characteristics of alloy 800  

International Nuclear Information System (INIS)

The published literature is reviewed and supplemented by current information from the author's laboratory, to show the influence of various compositional, heat treatment and thermomechanical factors on the structural characteristics of Alloy 800. The features discussed include carbon, aluminium, titanium and boron, solution treatment, ageing treatments with and without applied strain, and cold working. Examples of the aspects reviewed include the effect of heat treatment and service or testing temperature on the austenite grain size, and the relative importance of M_2_3C_6 and TiC, the influence of carbon level on gamma prime, the effect of residual or steady stress combined with time at temperature on changes in carbide or gamma prime morphology, and on the appearance of sigma or other intermetallic phases. The questions posed by these features are discussed generally, in terms of their effect on the mechanical properties at ambient and ...

197

Innovative forming and fabrication technologies : new opportunities.  

Energy Technology Data Exchange (ETDEWEB)

The advent of light metal alloys and advanced materials (polymer, composites, etc.) have brought the possibility of achieving important energy reductions into the full life cycle of these materials, especially in transportation applications. 1 These materials have gained acceptance in the aerospace industry but use of light metal alloys needs to gain wider acceptance in other commercial transportation areas. Among the main reasons for the relatively low use of these materials are the lack of manufacturability, insufficient mechanical properties, and increased material costs due to processing inefficiencies. Considering the enormous potential energy savings associated with the use of light metal alloys and advanced materials in transportation, there is a need to identify R&D opportunities in the fields of materials fabrication and forming aimed at developing materials with high specific ...

2008-01-31

198

New deformation mechanisms in fine-grain Mg alloys  

Energy Technology Data Exchange (ETDEWEB)

Deformation mechanisms were investigated in fine-grain (d=7 {mu}m) AZ31 Mg alloy in order to understand their excellent room-temperature ductility. Dislocation cross slip from basal to non-basal planes was found to occur easily at room temperature at a plastic anisotropy factor of only 1.5 instead of several tens to 100 expected from the single crystal CRSS data. Enhanced grain-boundary sliding (GBS) was also found to occur at room temperature. The contribution of GBS strain was found to be approximately 8% of total strain. The enhanced activity of non-basal dislocation slip and GBS was attributed to grain-boundary compatibility effects. Moreover, dynamic recovery was found to occur during deformation at room temperature associated with the formation of recovery twins and small-angle grain boundaries. The occurrence of these deformation mechanisms at room temperature was considered to be a major reason for an excellent ...

2003-07-01

199

Influence of C, N and Nb contents on intergranular corrosion, stress corrosion cracking and mechanical strength of alloy 600  

International Nuclear Information System (INIS)

Dependence of C, N and Nb contents on intergranular corrosion (IGC), strews corrosion cracking (SCC) and mechanical strength of alloy 600 were examined. To evaluate the corrosion resistance of heat affected zone (HAZ), post weld heat treated specimens were used. To evaluate I G C and S C C susceptibility, Ferric Sulfate-Sulfuric Acid Test and High Temperature Water Test were used. Nb is effective as a stabilizer of C. Consequently to prevent corrosion attack on H A Z in high temperature water Nb should be added more than 100 ( % C - 0.005)% and to maintain mechanical strength, Nb should be added more than 3 + 75( %C + %N)%. Modified alloy 600 satisfying above condition was manufactured commercially and its various properties including weldability were confirmed to be excellent.

1985-12-01

200

Effect of rolling conditions on microstructure and mechanical properties of AZ31 Mg alloy  

Energy Technology Data Exchange (ETDEWEB)

The effect of warm rolling under various conditions on the microstructure and mechanical property was investigated using an AZ31 Mg alloy sheet. Several processing parameters such as initial thickness, thickness reduction by a single pass rolling, rolling temperature, roll speed, and roll temperature were varied to elicit an optimum condition for the warm rolling process of AZ31 Mg alloy. Microstructure and mechanical properties were measured for specimens subjected to rolling experiments of various conditions. Warm rolling of 30% thickness reduction per pass was possible without any side-crack at temperatures as low as 200 C under the roll speed of 30 m/min. The initial microstructure before rolling was the mixed one consisting of partially recrystallized and cast structures. Grain refinement was found to occur actively during the warm rolling, producing a very fine grain size of 7 {mu}m after 50% ...

2005-07-01

201

The electron-phonon coupling constant in vanadium  

International Nuclear Information System (INIS)

The electron-phonon coupling constant lambda has been calculated for vanadium. The electron energy bands and wave functions were obtained from a model augmented plane wave muffin-tin potential. The electron-phonon matrix elements were evaluated using the rigid-ion approximation and the measured phonon spectra. The results show that lambda is strongly affected by d-f scattering.

202

Texture development and texture influence on the mechanical properties of the Mg-alloy AZ31  

Energy Technology Data Exchange (ETDEWEB)

The texture influence on tensile tests of AZ31, one of the common Mg alloys, has been studied. Starting material was a rectangular extruded bar, which has a strong texture. Due to the preparation of three tensile samples with 0 , 45 , 90 to the extrusion direction, the initial bar texture influences differently on the mechanical behaviour under tensile load. This results in a variation of the yield strength (90 MPa and 175 MPa) the ultimate tensile strength (250 MPa - 278 MPa) and the final texture. Experimental texture analysis was completed by texture simulations using the VPSC-model (visco plastic self-consistent). The good agreement between experimental and simulated pole figures allows the determination of the activated deformation modes related to the initial texture. (orig.)

2002-07-01

203

Microstructure of a nickel-base ODS powder after mechanical alloying. Mikrostruktur eines ODS-Pulvers auf Nickelbasis nach dem mechanischen Legieren  

Energy Technology Data Exchange (ETDEWEB)

Mechanical alloying is an important pre-requisite for the manufacturing of heat resistant oxide-dispersion-strengthened superalloys. Though the microstructure of these materials after hot extrusion and recrystallization treatment is well documented, little is known about the microstructural evolution during ball-milling. A method was tested to prepare electron transparent foils and extraction replica from powder particles for TEM investigations. The microstructure was found to consist of a Ni-Cr-Al solid solution in which submicron particles of refractory metals were embedded. The extremely fine grainize of about 50 nm is the consequence of severe plastic deformation. Yttria particles could not be detected in the powder after ball milling, but after a heat treatment at 1000 C the well-known fine dispersion of oxide particles was evident. (orig.)

1993-02-01

204

Microstructure and mechanical behaviour of an elevated temperature Mg-rare earth based alloy  

International Nuclear Information System (INIS)

AM-SC1 is a heat treatable magnesium alloy that has been specifically developed to achieve the elevated temperature strength and creep properties necessary for engine block applications. This paper describes the interrelationship between the microstructure and the mechanical properties of AM-SC1. The compressive and tensile strengths are relatively insensitive to temperature up to and including 450 K and the tensile yield behaviour deviates from a standard Hall-Petch relationship at grain sizes below 200 ?m. The microstructural features contributing to the creep resistance are both inter- and intra-granular in nature and are on length scales from nanometers to micrometers. The creep behaviour at 423 K and 450 K is diffusion controlled, with any contribution from the grain boundaries being negligible.

2009-04-15

205

Materials for cold neutron sources: Cryogenic and irradiation effects  

Energy Technology Data Exchange (ETDEWEB)

Materials for the construction of cold neutron sources must satisfy a range of demands. The cryogenic temperature and irradiation create a severe environment. Candidate materials are identified and existing cold sources are briefly surveyed to determine which materials may be used. Aluminum- and magnesium-based alloys are the preferred materials. Existing data for the effects of cryogenic temperature and near-ambient irradiation on the mechanical properties of these alloys are briefly reviewed, and the very limited information on the effects of cryogenic irradiation are outlined. Generating mechanical property data under cold source operating conditions is a daunting prospect. It is clear that the cold source material will be degraded by neutron irradiation, and so the cold source must be designed as a brittle vessel. The continued effective operation of many different cold sources at a number of ...

1990-01-01

206

Grain size effects on the tensile properties and deformation mechanisms of a magnesium alloy, AZ31B, sheet  

International Nuclear Information System (INIS)

The grain size dependence of the tensile properties and the deformation mechanisms responsible for those properties are examined for Mg alloy, AZ31B, sheet. Specifically, the Hall-Petch effect and strain anisotropy (r-value) are characterized experimentally, and interpreted using polycrystal plasticity modeling. {1 0 . 2} extension twins, {1 0 . 1} contraction twins, and so-called 'double-twins' are observed via microscopy and diffraction-based techniques, and the amount of twinning is found to increase with increasing grain size. For the sheet texture and tensile loading condition examined, {1 0 . 2} extension twinning is not expected, yet the polycrystal plasticity model predicts the observed behavior, including this 'anomalous' tensile twinning. The analysis shows that the Hall-Petch strength dependence, of the polycrystal as a whole, is primarily determined by the grain size dependence of the strength of the prismatic slip systems.

2008-07-15

207

Experimental characterisation and modelling of crack initiation and short crack propagation for fatigue life prediction of a #beta#-titanium alloy  

International Nuclear Information System (INIS)

Up to 90% of the life time of cyclically loaded components is determined by short crack initiation and propagation. This stage of the fatigue damage process is strongly influenced by microstructural features, e.g. grain boundaries and crystallographic grain orientation. Therefore LEFM can not be applied in a reasonable manner explaining the demand for a mechanism-related modelling method. The present study deals with mechanical testing and microstructural examinations applied to the relatively new #beta#-titanium alloy LCB. The results are used as data base to develop a new short crack model that is based on the model of Navarro and de los Rios. By using various techniques such as electron back-scattered diffraction and finite-element calculations the origin of crack initiation is revealed and the characteristics of crack propagation is determined. (orig.)

2000-02-24

208

Disordered bcc γ-phase to δ-phase transformation in Zr-rich U-Zr alloy  

British Library Electronic Table of Contents (United Kingdom)

The transformation mechanism of hexagonal delta phase from the disordered bcc gamma phase has not been reported before in the Zr-rich U-Zr alloy system. With the help of X-ray diffraction, transmission electron microscopy (TEM) and high-resolution TEM analyses it was shown that the gamma to delta conversion takes place by the lattice collapse mechanism of omega transformation. It was also ascertained that a higher aging temperature or time promotes the growth of all four variants of the delta phase within a parent gamma grain. In addition, ab initio electronic structure calculations showed that the bcc to hexagonal transformation, involving partial ordering of the parent bcc phase followed by (111) plane collapse, is energetically favorable.

2011-01-01

209

A study on the passive film of Alloy 600 and Alloy 690 formed in the high temperature aqueous solution with additives  

Energy Technology Data Exchange (ETDEWEB)

Alloy 690 and Alloy600 are used as a material for the steam generator tubing in the pressurized water reactor(PWR) of nuclear power plants due to its high corrosion resistance. Although those are a highly corrosion resistance material, their stress corrosion cracking(SCC) have been found on occasion, which are deeply related to a surface oxide film on a base material which have occurred on the primary side as well as the secondary side of a tubing. And The SCC is accelerated in the existing Pb which is the impurity of secondary steam generator components. The Oxide on a steel surface in an aqueous solution above 100 .deg. C is composed of a duplex film structure. The inner layer of the oxide is dense and less porous, which is formed by a growth of the oxide layer on the metal surface. The outer layer of the oxide is less adhesive, which is formed by a dissolution and precipitation mechanism. Growth processes of the inner ...

2008-10-15

210

A study on the passive film of Alloy 600 and Alloy 690 formed in the high temperature aqueous solution with additives  

International Nuclear Information System (INIS)

Alloy 690 and Alloy600 are used as a material for the steam generator tubing in the pressurized water reactor(PWR) of nuclear power plants due to its high corrosion resistance. Although those are a highly corrosion resistance material, their stress corrosion cracking(SCC) have been found on occasion, which are deeply related to a surface oxide film on a base material which have occurred on the primary side as well as the secondary side of a tubing. And The SCC is accelerated in the existing Pb which is the impurity of secondary steam generator components. The Oxide on a steel surface in an aqueous solution above 100 .deg. C is composed of a duplex film structure. The inner layer of the oxide is dense and less porous, which is formed by a growth of the oxide layer on the metal surface. The outer layer of the oxide is less adhesive, which is formed by a dissolution and precipitation mechanism. Growth processes of the inner ...

2008-10-01

211

Microstructure and mechanical properties of magnesium alloy AZ31B laser beam welds  

International Nuclear Information System (INIS)

Microstructure and properties of a Mg AZ31B laser beam weld without filler are studied using electron microscopy, X-ray diffraction and mechanical tests. The microstructure of the weld is characterized by a narrow heat affected zone, columnar grains and precipitate coarsening in the fusion zone. Texture in the fusion zone is significantly different from the texture of the base material. The residual stress distribution observed is similar at the top and the bottom of the weld, maximum tensile residual stress values are observed in the fusion zone. Tensile tests reveal differences in the mechanical behavior of the fusion zone and the parent material, which can be related to the differences of texture and the resulting deformation mechanisms.

2008-06-25

212

Development of Stronger and More Reliable Cast Austenitic Stainless Steels (H-Series) Based on Scientific Design Methodology  

Energy Technology Data Exchange (ETDEWEB)

The goal of this program was to increase the high-temperature strength of the H-Series of cast austenitic stainless steels by 50% and upper use temperature by 86 to 140 F (30 to 60 C). Meeting this goal is expected to result in energy savings of 38 trillion Btu/year by 2020 and energy cost savings of $185 million/year. The higher strength H-Series of cast stainless steels (HK and HP type) have applications for the production of ethylene in the chemical industry, for radiant burner tubes and transfer rolls for secondary processing of steel in the steel industry, and for many applications in the heat-treating industry. The project was led by Duraloy Technologies, Inc. with research participation by the Oak Ridge National Laboratory (ORNL) and industrial participation by a diverse group of companies. Energy Industries of Ohio (EIO) was also a partner in this project. Each team partner had well-defined roles. Duraloy Technologies led the team by identifying the base ...

2006-04-15

213

Improvement in mechanical properties of magnesium alloy (AZ31) sheet fabricated by casting and subsequent plastic working  

Energy Technology Data Exchange (ETDEWEB)

In order to enhance the mechanical properties of magnesium alloy (AZ31) sheet, an integrated sheet-making process including billet casting, extrusion and rolling was attempted. Microstructural analysis was carried out and the mechanical properties at each processing step were also investigated by tensile tests. By an extrusion process of ingot-processed billet, average grain size of billet was reduced from 91.2 to 28.2 {mu}m, and a further reduction in grain size to 16.9 {mu}m was obtained by subsequent rolling of extruded 5 mm thin slab. In the final step, a rolled sheet of 1 mm showed a remarkable refinement in grain size down to 8.8 {mu}m. Regarding mechanical properties, tensile strength and elongation for as-cast billet, as-extruded thin slab and as-rolled sheet increased from 189, 258 to 234 MPa, and from 13, 16.5 to 23%, respectively. (orig.)

2003-07-01

214

Nickel base alloys for future steam turbines; Nickelbasis-Legierungen fuer zukuenftige Dampfturbinen  

Energy Technology Data Exchange (ETDEWEB)

Modern commercial alloys are not suited for future steam turbines of operating temperatures beyond 700 C. {gamma}'-hardened alloys like Waspaloy have good mechanical characteristics but have defects when large batches are melted. {gamma}'/{gamma}''-hardened alloys like Inconel 706, on the other hand, are easy to produce but have insufficient microstructural long-term stability and insufficient creep strength. Mixed crystal solidified alloys like Inconel 617 have excessive yield stress at forging temperatures. Two new alloys were therefore developed. Results so far show that they have good production characteristics but insufficient mechanical characteristics. The reasons for this are currently under investigation. (orig.) [German] Die heutigen kommerziellen Legierungen sind nicht geeignet fuer den Einsatz ...

2003-07-01

215

Alcoa titanium alloy Ti-10V-2Fe-3Al forgings -- Data sheets  

International Nuclear Information System (INIS)

Ti-10V-2Fe-3Al is high strength, metastable beta titanium alloy developed by the Timet Division, Titanium Metals Corporation of America for enhanced forgeability and excellent mechanical property combinations, including deep hardening characteristics. Ti-10-2-3 has been the subject of intense thermomechanical processing (TMP) development and reduction to commercial practice for the full range of open die, closed-die and precision forged products utilized in aerospace and other applications. With commercially proven TMP, Ti-10-2-3 forgings provide a range of strength-fracture toughness combinations from 180 Ksi (1,240 MPa) minimum U.T.S. to 140 Ksi (965 MPa) minimum U.T.S with commensurate fracture toughness. With optimal TMP and these strength-toughness combinations, Ti-10-2-3 forgings are found provide superior smooth and notched fatigue properties critical to aerospace applications over incumbent alpha-beta alloys. The ...

1993-02-21

216

Mechanical properties of titanium-niobium carbon nitride  

Energy Technology Data Exchange (ETDEWEB)

A study was made of the variation in strength characteristics of group IV transition metal carbon nitrides alloyed with carbides or group V metal nitrides. A complex solid solution of titanium-niobium carbonitride was preliminarily synthesized to a homogeneous equilibrium state and then crushed. The calculated quantity of binder metal was added as elemental powders, the mixture was vibration ball milled in ethanol and the plasticized charge was used to press experimental specimens for mechanical testing. The studies showed that the high-temperature strength properties of the new cermet are superior to standard type KNT. The material is thus promising for use in the manufacture of tools. 8 references, 3 figures.

1984-07-01

217

Inhomogeneity of mechanical and fatigue properties of Al-Li alloys extrusions  

Energy Technology Data Exchange (ETDEWEB)

Aluminium-lithium extrusions possess high inhomogeneity of properties across the cross section. Mechanical properties such as R{sub p0,2}, R{sub m} and hardness, but also fatigue properties, change their value in dependence with the cross section position where test specimens were taken. Positions, where extreme values of properties are measured, are characteristic for a given extrusion shape. The positions with different properties have different structure and texture. Properties and structure inhomogeneity is affected mainly by extrusion shape and heat treatment parameters. (orig.)

1996-12-01

218

Mechanodynamical analysis of nickel-titanium alloys for orthodontics application; Analise mecanodinamica de ligas de niquel-titanio para aplicacao ortodontica  

Energy Technology Data Exchange (ETDEWEB)

Nickel-titanium alloys may coexist in more than one crystalline structure. There is a high temperature phase, austenite, and a low temperature phase, martensite. The metallurgical basis for the superelasticity and the shape memory effect relies in the ability of these alloys to transform easily from one phase to another. There are three essential factors for the orthodontist to understand nickel-titanium alloys behaviour: stress; deflection; and temperature. These three factors are related to each other by the stress-deflection, stress-temperature and deflection-temperature diagrams. This work was undertaken with the objective to analyse commercial nickel-titanium alloys for orthodontics application, using the dynamical mechanical analyser - DMA. Four NiTi 0,017 X 0,025'' archwires were studied. The archwires were Copper NiTi 35 deg C (Ormco), Neo Sentalloy F200 ...

2002-07-01

219

Photoluminescence linewidths in metalorganic vapor phase epitaxially grown ordered and disordered InAlGaP alloys  

International Nuclear Information System (INIS)

The dependence of the photoluminescent properties of In_0_._4_8(Al_yGa_1_-_y)_0_._5_2P alloys (0#<=#y#<=#0.5) on growth temperature and substrate misorientation off GaAs(100) has been studied. Samples were grown using low-pressure metalorganic vapor phase epitaxy. By studying the dependence of ordering behavior in InGaP as a function of substrate misorientation and growth temperature simultaneously, a very large range in low-temperature photoluminescence emission energy---135 meV---has been obtained. The photoluminescence linewidth exhibits a strong, continuous dependence on the extent of atomic ordering (the emission energy) in the alloys. The results indicate that inhomogeneity in the microstructure of the material (i.e., between ''ordered'' domains and the ''disordered'' matrix) is the dominant photoluminescence broadening mechanism. This investigation has allowed a significant optimization of the optical ...

220

Mechanism for transient-enhanced diffusion in ion-implanted silicon  

International Nuclear Information System (INIS)

High-dose ion implantation followed by solid-phase-epitaxial (SPE) growth is now a well-established technique for the production of supersaturated silicon alloys. However, these alloys also contain a high supersaturation of silicon interstitials, which give rise to transient, greatly enhanced dopant diffusion with subsequent heating. In this contribution, the authors present a study of a series of Si-Sb alloys of various concentrations which were made by Sb implantation under various conditions to deduce the origin of the observed transient diffusion. A multiple implant scheme was employed to produce samples with an approximately uniform dopant concentration from 40 to 150 nm in depth, but with the amorphous layer extending to a depth of 380 nm. By scaling the implant doses, alloys with different concentrations in the uniform region were produced, allowing an accurate measure of diffusion coefficients ...

1985-03-01

221

Anti-corrosive properties of an electropolymerized polymer coating on a shape memory alloy surface  

Energy Technology Data Exchange (ETDEWEB)

Acrylonitrile electropolymerization (in an aprotic and anhydrous medium) has been used as a way to build thin, homogeneous and covering polyacrylonitrile layers grafted on the surface of usual metals and specially on copper-based shape memory alloy: Cu-Zn-Al. The results of the study first confirm the possibility of grafting thin and covering polyacrylonitrile layers on Cu-Zn-Al surface. The morphology of the films however is influenced by the geometry of the polycristalline structure of the alloy and its superficial defects. Samples obtained after grafting polyacrylonitrile films were submitted to corrosion tests based on Electrochemical Impedance Spectroscopy (EIS) measurements in a NaCl/H{sub 2}O medium. Results show that some post-treatments of the grafted films are necessary to improve their protective role, while preserving the strong interfacial bondings. Actually, thermal and mechanical cycling of the shape memory ...

1996-01-01

222

On methods for improving the fatigue performance of the wrought magnesium alloys AZ31 and AZ80  

Energy Technology Data Exchange (ETDEWEB)

The tensile and compressive properties as well as LCF and HCF performance of the extruded magnesium alloys AZ31 and AZ80 were determined in extrusion (L) and long-transverse (T) directions. Owing to marked crystallographic textures, both alloys showed pronounced directional mechanical properties in monotonic as well as cyclic loading with strength values in L-direction being significantly superior to those in T-direction. Thermomechanical treatments such as pressing, swaging and rolling were found to increase yield stresses and HCF strengths and to alter the directionality in properties due to textural modifications. To further improve HCF strengths, mechanical surface treatments such as shot peening, roller-burnishing and deep rolling were utilized. The results indicate marked improvements provided that suitable process parameters are used. The improvement of the HCF strengths is explained by the ...

2003-07-01

223

Mo microalloying effect on the glass-forming ability, magnetic, mechanical and corrosion properties of (Fe0.76Si0.096B0.084P0.06)100-xMox bulk glassy alloys  

British Library Electronic Table of Contents (United Kingdom)

The effect of Mo addition on the glass-forming ability (GFA), magnetic properties, mechanical properties and corrosion resistance of (Fe0.76Si0.096B0.084P0.06)100-xMox (x=0, 2, 4 and 6at.%) bulk glassy alloys (BGAs) with high Fe contents was investigated. The 2at.% Mo addition makes the alloy composition approach towards a eutectic point, which could result in an increase in the GFA. The BGA rod with diameters up to 3.5mm was produced by copper mold casting. These BGAs exhibit a rather high saturation magnetization of 0.98-1.51T and lower coercive force of 1.7-2.1A/m. A significant improvement in corrosion resistance was observed with microalloying Mo element in 1N H2SO4 solution. Furthermore, these Fe-based BGAs show super-high strength of ~3.3GPa and Young's modulus of 200GPa.

2011-01-01

224

Limit of pitting corrosion at high-alloyed special steels and NiCrMo alloys in chloride solution; Die Lochkorrosionsbegrenzung bei hochlegierten Sonderedelstaehlen und NiCrMo-Legierungen in Chloridloesung - Einflussfaktoren und Ausmass  

Energy Technology Data Exchange (ETDEWEB)

The phenomenon of the limit of pitting corrosion in direction to positive potentials is studied by potentiokinetic polarization after a jump in the transpassive range and by potentiostatic tests at technical wrought materials and at model alloys of the systems NiCrMo and NiMo in CaCl{sub 2} solution in the concentration range 1 to 9 mol/l chloride at pH-values of 1 to 9 at temperatures of 30 to 110 C. Surface-analytical investigations gives in connection with knowledges from anodic polarization studies directions to the mechanism of the limit of pitting corrosion. Ranges of the limit of pitting corrosion are obtained at materials with a Mo content above 6.5% and contents of chloride of the media above 2 mol/l chloride. Increasing temperatures, increasing contents of chloride and sulfate shift the potential of the limit of pitting corrosion being always above 0.2 V (SCE) at potentiostatic determination to noble direction. There are indications ...

2001-08-01

225

Effects of the dissolved oxygen and pH on a passivity of the oxide film formed on the Alloy 600  

Energy Technology Data Exchange (ETDEWEB)

Alloy 600 is commonly used in the primary systems of PWR plants because of its excellent resistance to a stress corrosion cracking and pitting. But a stress corrosion cracking and pitting corrosion are occasionally observed under PWR conditions, which may be correlated with the passive film on the Alloy 600 surface. There is little information on the composition of films growing on the surface of Alloy 600 at high temperature. Therefore, an understanding of the basic electrochemical behaviors about an anodic dissolution and the passivation of the bare surface of metals and alloys provides important information about localized corrosions like a SCC and pitting. Oxide on the steel surfaces in an aqueous solution above 100 .deg. C is composed of a duplex film structure. The inner layer of the oxide is dense and less porous, which is formed by a growth of the oxide layer on the metal surface. Outer layer of ...

2006-07-01

226

Effects of the dissolved oxygen and pH on a passivity of the oxide film formed on the Alloy 600  

International Nuclear Information System (INIS)

Alloy 600 is commonly used in the primary systems of PWR plants because of its excellent resistance to a stress corrosion cracking and pitting. But a stress corrosion cracking and pitting corrosion are occasionally observed under PWR conditions, which may be correlated with the passive film on the Alloy 600 surface. There is little information on the composition of films growing on the surface of Alloy 600 at high temperature. Therefore, an understanding of the basic electrochemical behaviors about an anodic dissolution and the passivation of the bare surface of metals and alloys provides important information about localized corrosions like a SCC and pitting. Oxide on the steel surfaces in an aqueous solution above 100 .deg. C is composed of a duplex film structure. The inner layer of the oxide is dense and less porous, which is formed by a growth of the oxide layer on the metal surface. Outer layer of ...

2006-05-25

227

State-of-the-art technology for production of seamless tubes in zirconium and titanium alloys  

International Nuclear Information System (INIS)

Zircaloy fabrication plant manufactures all the necessary Zr-2 components like fuel canning tubes, calandria tubes and other rod and sheet products. This plant is having a capacity of producing about 4 lakh nos. of PHWR fuel tubes per annum. These tubes are seamless, thin walled with close dimensional tolerances and stringent mechanical properties. The plant has established all the facilities required to produce these tubes with required quality.

228

Microstructural modifications and high-temperature strength of monocrystalline nickel-base superalloys  

Energy Technology Data Exchange (ETDEWEB)

The examples discussed demonstrate that in order to improve further the high-temperature strength properties of (monocrystalline) nickel-base superalloys, it is expedient to follow two parallel routes, namely alloy development, on the one hand, and suitable modifications of the microstructure by appropriate thermal and mechanical treatments, on the other hand. (orig.)

2000-07-01

229

Hydrogen in nano-sized metals  

Energy Technology Data Exchange (ETDEWEB)

Systems with small sizes show significant changes compared to the bulk system. These changes are of major interest regarding the size reduction of technological applications. The hydrogen-metal system can be used as a model alloy to study small size features: shifted phase boundaries and sloped isotherms are found and, also, new materials structures. Most features can be attributed to surface- and interface contributions as well as to mechanical stress. (Abstract Copyright [2004], Wiley Periodicals, Inc.)

2004-02-01

230

Selective oxidations on vanadiumoxide containing amorphous mixed oxides (AMM-V) with tert.-butylhydroperoxide  

Energy Technology Data Exchange (ETDEWEB)

The catalytic oxygen transfer properties of vanadium containing zeolites and vanadium based sol-gel catalysts with hydrogen peroxides are well known. The severe problem of vanadium leaching caused by the presence of the by-product water has been addressed. To avoid any interference with homogeneously catalyzed reactions, our study focusses on selective oxidations in a moisture-free medium with tert.-butylhydroperoxide. We have investigated the catalytic properties of amorphous microporous materials based on SiO{sub 2}, TiO{sub 2}, ZrO{sub 2} and Al{sub 2}O{sub 3} as matrix material and studied the effects of surface polarity on the oxidation of 1-octene and cyclohexane. (orig.)

1998-12-31

231

On the interaction of vanadium (4) with derivatives 3,4,5-trihydroxy-isoxanthene  

International Nuclear Information System (INIS)

A study was made on interaction of vanadium (4) ions with dyes-pyrogallol red, brompyrogallol red and gallein- in the range of pH = 0-6. The maximal light absorption for gallein and brompyrogallol red is observed at pH=4 and #lambda#max = 545 nm and 560 nm respectively. The compound of vanadium (4) with pyrogalloe red is characterized by the maximal light absorption at pH=5 and #lambda#max=560 nm. Component ratio in all analyzed compounds is equal to 1:2. Molar extinction coefficients for compounds with gallein, pyrogallol red and brompyrogallol red are equal to 5000, 550 and 7400, and logarithms of stability constants - to 9.27, 13.17 and 13.25 respectively.

232

Determination of some minor and trace elements in iron ores by ion exchange chromatography, spectrophotometry and atomic absorption spectrometry  

International Nuclear Information System (INIS)

A method is described for determination of aluminium, cadmium, cobalt, chromium, copper, calcium, magnesium, sodium, potassium, manganese, nickel, lead, strontium, zinc, titanium and vanadium in iron ore. After dissolution, a 1 gram sample of iron ore is applied to a column of AGI-X8 anion exchange resin (chloride form), in 100 ml of 7M HCl. Aluminium, chromium, calcium, magnesium, sodium, potassium, manganese, nickel, lead, strontium, titanium and vanadium are eluted with 7M HCl; iron, copper and cobalt are eluted with 0.5M HCl; cadmium and zinc are eluted with 2M HNO_3. Iron is subsequently removed from copper and cobalt by a solvent extraction with methyl isobutyl ketone. The elements are determined in the eluates by atomic absorption spectrometry, except for titanium and vanadium, which are determined spectrophotometrically.

233

Mechanical properties and structure of low-alloy ultra-high strength steels  

Energy Technology Data Exchange (ETDEWEB)

Mechanical properties of P-LDHA and V-ROL N steels of the Czech production are compared with other ultra-high strength steels produced in the world. The most important results can be summarized into following points: 1. Optimally heat treated P-LDHA steel exhibits substantially better strength characteristics then the V-ROL N steel. 2. Optimal tempering temperature of the P-LDHA steel is 300 C. 3. Basic mechanical properties of P-LDHA steel belong to the top of the UHS steels ranking and are well comparable with those of American 300 M steel. 4. In the low-cycle fatigue region, the P-LDHA steel exhibits slightly better fatigue resistance then the 300 M steel. On the other hand, the high-cycle fatigue resistance of 300 M steel is slightly better then that of the P-LDHA steel. (orig.)

2000-07-01

234

Hydrostatic extrusion of magnesium: process mechanics and performance  

Energy Technology Data Exchange (ETDEWEB)

Following the breakthrough for cast magnesium products, interest is now spreading to wrought applications - triggering a variety of technological questions. A major bottleneck in the manufacture of magnesium sections (profiles) by conventional hot extrusion is the low productivity, with extrusion speeds typically five to ten times lower than for comparable aluminium sections. This paper focuses on the use of hydrostatic extrusion as a means to overcome this problem. On the basis of an analytical model, it is clarified why and how process limits are affected by the process mechanics. Experimental work on the hydrostatic extrusion of the alloys M1A, ZM21 and AZ31 confirms that extrusion speed is indeed multiplied, whereas the resulting mechanical properties are similar to or better than those for conventional extrusions. (orig.)

2003-07-01

235

Thermal-mechanical test on ITER primary first wall mock-ups  

International Nuclear Information System (INIS)

In 1998, in the frame of the ITER EDA phase, an European R and D Programme for the Blanket Design was implemented for developing and selecting the materials and the relevant fabrication procedures for manufacturing the shielding modules of the ITER Primary Wall. The fabrication of several Beryllium armored small scale mock-ups, reproducing representative portions of a Primary Wall panels, was also launched (Fusion Technol. (1998) 195). Further experimental activities were also programmed for investigating the thermal-mechanical behavior of these mock-ups at high heat flux and under thermal fatigue tests. In 2001, the ITER European Home Team decided to assign to ENEA a contract for the thermal fatigue testing of six mock-ups aiming at verifying the reliability of the Beryllium/Dispersion Strengthened Copper alloy/Stainless Steel and Beryllium/Precipitation hardened Copper alloy/Stainless Steel joints manufactured by solid ...

2002-11-01

236

The influence of interfacial structure on the mechanical properties of liquid-phase-sintered aluminium-ceramic composites. [Al-Cu-Mg-Si/SiC  

Energy Technology Data Exchange (ETDEWEB)

The effect of interfacial structure on the mechanical properties of aluminum-ceramic composite materials fabricated by liquid phase sintering was studied. The composites were based on two matrix alloys (powder metallurgy alloys 201 and 601) reinforced with either Al{sub 2}O{sub 3} or SiC particulate. Characterization of the interfacial regions demonstrated that the SiC-matrix interfaces were faceted whereas the Al{sub 2}O{sub 3}-matrix interfaces had an incomplete layer of a silicon-rich amorphous phase. Preferential attack of the particles during sintering is believed to cause the crystallographic facets to form on SiC. Locally high silicon concentrations near Al{sub 2}O{sub 3} particles led to the formation of a glassy phase from the reduction of Al{sub 2}O{sub 3}. The difference in interfacial structure resulted in a higher particle-matrix bond strength and therefore improved composite mechanical ...

1990-10-01

237

Sintering of nano-sized WC-Co powders produced by a gas reduction-carburization process  

Energy Technology Data Exchange (ETDEWEB)

Nanocrystalline cemented tungsten carbide has attracted considerable interests for use in cutting tool because of its superior mechanical properties. In this study, nano-sized powders of mixed WC and Co were prepared from attrition-milled oxides by a gas reduction-carburization process. The effects of compacting pressure, heating schedule, additional ball-milling, and the presence of a grain growth inhibitor on the sintering properties of the nano-sized WC-Co powders were examined. The grain size and phases in WC-Co alloy were clearly affected by compacting pressure. Because of the trapped gases and the lower melting point of the cobalt binder, when a compact of nano-sized WC-Co powder was sintered through a heating schedule with holding steps, the sintered alloy maintained the small size of WC grains without any {eta} phase. In addition, the additional ball-milling improved the microstructure and ...

2006-08-10

238

Sintering of nano-sized WC-Co powders produced by a gas reduction-carburization process  

International Nuclear Information System (INIS)

Nanocrystalline cemented tungsten carbide has attracted considerable interests for use in cutting tool because of its superior mechanical properties. In this study, nano-sized powders of mixed WC and Co were prepared from attrition-milled oxides by a gas reduction-carburization process. The effects of compacting pressure, heating schedule, additional ball-milling, and the presence of a grain growth inhibitor on the sintering properties of the nano-sized WC-Co powders were examined. The grain size and phases in WC-Co alloy were clearly affected by compacting pressure. Because of the trapped gases and the lower melting point of the cobalt binder, when a compact of nano-sized WC-Co powder was sintered through a heating schedule with holding steps, the sintered alloy maintained the small size of WC grains without any #eta# phase. In addition, the additional ball-milling improved the microstructure and ...

2006-08-10

239

Ab initio study of lithium transition metal fluorophosphate cathodes for rechargeable batteries  

Energy Technology Data Exchange (ETDEWEB)

Density functional theory (DFT) calculations using plane-wave methods were performed for Li2TMPO4F, LiTMPO4F, and TMPO4F (TM=V, Mn, Fe, Co, Ni) to address their feasibility as high-voltage cathode materials for Li ion batteries. We computed their structures, average open circuit voltages, and thermal stabilities for step-wise lithiation/delithation (discharge/charge) reactions. The calculations suggest that associated unit cell volume changes are sufficiently small on average that they should not be a significant detriment to the mechanical stability of the cathode. In the nickel case, the calculated volume change deviates from the series by increasing during the first delithiation step. Furthermore, the volume increases for all these materials during the second delithiation step. It appears that the relative volume expansion in the series during delithiation is directly correlated to the degree of d-p rehybridization. Predicted average open circuit voltages ...

2011-08-18

240

Report of the results of the fiscal 1997 regional consortium R and D project. Regional consortium energy field / R and D mesoscopic organ control heat-resistant / wear-resistant metal group composite materials (first fiscal year); 1997 nendo chiiki consortium kenkyu kaihatsu jigyo. Chiiki consortium energy bun`ya / mesoscopic fukuso soshiki seigyo tainetsu taimamosei kinzokuki fukugo zairyo no kenkyu kaihatsu (daiichi nendo) seika hokokusho  

Energy Technology Data Exchange (ETDEWEB)

Out of the R and D of mesoscopic metal group composite materials, the paper described the fiscal 1997 results. In the in-situ method as a composite material making method, elucidated to some degree were chemical composition of Fe-C-Cr-V-Nb-Mo-W-Ni base multi-dimensional alloys, and wear resistance and oxidation resistance of MC type carbide dispersion multi-phase texture crystallizing as primary crystal and eutectic. In the composite material making with ceramic fiber and alloy by the pressure infiltration method, the paper clarified the texture formation mechanism in solidification/heat treatment by a combination of Al alloys and alumina long fiber, and the relation between fiber configuration and wear resistance. By MA and MG methods as the powder metallurgy composite material making method, a composed body of {alpha}-stainless steel of Fe-12%Cr composition and M23C6 of 40-90vol% are designed for ...

1998-03-01

241

Modification of the passivity of iron based alloys through ion implantation  

International Nuclear Information System (INIS)

As an unconventional surface alloying process, ion implantation has been utilized to improve the active-passive behavior and the pitting resistance of martensitic M50 engineering alloy. In a field simulation study, Cr-implantation only at 150 kev to a fluence of 2 x 10"1"7 ions/cm"2 prevented pitting. The best pitting resistance of the steel was obtained with multiple implantations of Cr and Mo. The intermixing effect of high fluence P-implantation into 304 stainless produced an amorphous surface alloy. The removal of the grain boundaries and the uniformity of the resulting structure had a great influence on corrosion properties. REED analysis indicated that the anodic passive films formed on P-implanted 304 stainless steel at 250 mV (SCE) in 0.5M H_2SO_4 was amorphous. Phosphorus and boron were implanted into 316 stainless steel to study the passivity of 316 stainless. Electrochemical experiments were carried out to ...

1764-01-01

242

Phonon density of states in V_3Si  

International Nuclear Information System (INIS)

The observation by inelastic neutron scattering techniques of a high energy peak in the phonon spectrum (14 THz) of V_3Si is reported, and is attributed to a peak in the phonon density of states due to vanadium motions by the incoherent inelastic neutron scattering process.

1988-12-01

243

Influence of vanadium doping on the electrochemical behaviour of MnO{sub 2} rutile; Influence du dopage par le vanadium sur le comportement electrochimique de MnO{sub 2} rutile  

Energy Technology Data Exchange (ETDEWEB)

Vanadium doped manganese bi-oxide has been obtained from a solution containing both cations. The X-ray diffraction of this material indicates a rutile-type phase but the enlargement of some lines supports the existence of several lattice defects. Also the particle size of the doped material is significantly smaller than the one of the non-doped material obtained in the same conditions. The presence of pentavalent vanadium inside the lattice leads to a small amount of trivalent manganese. Electron microscopy shows the existence of defects which have a tendency of becoming well-ordered and to stabilize a sur-structure. At ambient temperature, the electrochemical behaviour of doped manganese bi-oxide is greatly improved when compared to the non-doped phase. This behaviour is due to the presence of numerous lattice defects and to the smaller size of crystallites. In polymer batteries, the behaviour is similar the one of the non-doped material for ...

1996-12-31

244

Heterogeneous catalytic alcoholysis of benzonitrile  

Energy Technology Data Exchange (ETDEWEB)

The authors investigate the possibility of the direct heterogeneous catalytic synthesis of ethylbenzoate from benzonitrile. The catalysts tested were oxides of aluminium, titanium, and vanadium. The main conversion product detected chromatographically was ethylbenzoate; benzaldehyde, benzamide, and benzanilide were also identified. Aluminium oxide was found to be the most effective catalyst.

1986-04-01

246

Chloranilic acid as complex forming reagent for the ultra trace analysis of elements by adsorptive stripping voltammetry; Chloranilsaeure als Komplexbildner fuer die Ultraspurenanalyse von Elementen durch Adsorptions-Stripping-Voltammetrie  

Energy Technology Data Exchange (ETDEWEB)

It is reported about the adsorptive stripping voltammetric determination of uranium, antimony, tin, vanadium and molybdenum using chloranilic acid as complex forming reagent. The determination limits are in the l{sup 1}-range. (orig.) [Deutsch] Es wird ueber die Bestimmung von Uran, Antimon, Zinn, Vanadium und Molybdaen durch Adsorptions-Stripping-Voltammetrie mit Chloranilsaeure als Komplexbildner berichtet. Die Bestimmungsgrenzen liegen im ng l{sup -1} Bereich. (orig.)

1996-12-01

247

Applications of niobium microalloyed ferrite pearlite steels to line pipe and plate  

International Nuclear Information System (INIS)

A variety of advanced controlled rolling techniques have been developed to improve toughness, strength and weldability of niobium-steels. To achieve optimum properties, control of prior stage rolling conditions and accelerated cooling are needed. In low carbon steel, the addition of niobium results in a greater increase in tensile strength than that of vanadium without a loss of toughness. At the same strength level, niobium-steel has less susceptibility to weld cracking and good toughness in the HAZ of its weldments than similar vanadium steels. Separation and formability of niobium steels are also discussed.

1981-11-01

248

PFB Coal Fired Combined Cycle Development Program: turbine materials evaluation, March 1980  

Energy Technology Data Exchange (ETDEWEB)

This report presents the results of cladding technology development under the Coal-Fired Combined Cycle DOE Project. Clad Alloy Development, involved the selection, fabrication and burner rig evaluation of advanced clad alloy composition diffusion-bonded to IN-738. Testing was conducted for up to 5800 hours at 1600/sup 0/F in a simulated PFB environment. Metallographic evaluation showed Co-base cladding alloys PFB-5PM and PFB-6PM (aluminided) and Fe-base alloy GE-2541 to be the most corrosion resistant. The formability and fabricability of sheet material was significantly improved for these alloys by utilizing powder metallurgy techniques. Clad Process Development encompassed processing activities to evaluate sheet alloy formability, bucket surface preparation techniques, platform clad forming, and the activated diffusion bonding (ADB) of corrosion resistant ...

1980-03-01

249

PFB Coal Fired Combined Cycle Development Program: turbine materials evaluation, March 1980  

Energy Technology Data Exchange (ETDEWEB)

This report presents the results of cladding technology development under the Coal-Fired Combined Cycle DOE Project for the period July 1976 through June 1978. Sub-task 3.1, Clad Alloy Development, involved the selection, fabrication and burner rig evaluation of advanced clad alloy compositions diffusion-bonded to IN-738. Testing was conducted for up to 5800 hours at 1600/sup 0/F in a simulated PFB environment. Metallographic evaluation showed Co-base cladding alloys PFB-5PM and PFB-6PM (aluminided) and Fe-base alloy GE-2541 to be the most corrosion resistant. The formability and fabricability of sheet material was significantly improved for these alloys by utilizing powder metallurgy techniques. Sub-task 3.2, Clad Process Development, encompassed processing activities to evaluate sheet alloy formability, bucket surface preparation techniques, platform clad ...

1980-03-01

250

New processing technique for forming flexible A-15 superconducting tapes with extremely high critical current densities  

Energy Technology Data Exchange (ETDEWEB)

A-15 compounds are extremely brittle and difficult to process for practical applications. A novel processing technique was developed to greatly improve the mechanical and superconducting properties of A-15 alloys. The new processing technique can be described as follows: (1) to select compounds that can form the A-15 phase (the selected A-15 compounds in this research were Ti3Nb6Mo3Si4 and Nb99.5-(x + y)AlxSiyB0.5 alloys); (2) to rapidly solidify them into the amorphous state; (3) to anneal the quenched amorphous products into ultra fine-grained single A-15 phase. The extreme grain refinement greatly improved the flexibility and the critical current density of the alloys. The melt spinning technique was used to rapidly solidify Ti3Nb6Mo3Si4 and Nb99.5-(x + y)AlxSiyB0.5 alloys. Ti3Nb6Mo3Si4 alloys were relatively easily formed into the amorphous state. Nb3Al ...

1986-01-01

251

New processing technique for forming flexible A-15 superconducting tapes with extremely high critical current densities  

International Nuclear Information System (INIS)

A-15 compounds are extremely brittle and difficult to process for practical applications. A novel processing technique was developed to greatly improve the mechanical and superconducting properties of A-15 alloys. The new processing technique can be described as follows: (1) to select compounds that can form the A-15 phase (the selected A-15 compounds in this research were Ti3Nb6Mo3Si4 and Nb99.5-(x + y)AlxSiyB0.5 alloys); (2) to rapidly solidify them into the amorphous state; (3) to anneal the quenched amorphous products into ultra fine-grained single A-15 phase. The extreme grain refinement greatly improved the flexibility and the critical current density of the alloys. The melt spinning technique was used to rapidly solidify Ti3Nb6Mo3Si4 and Nb99.5-(x + y)AlxSiyB0.5 alloys. Ti3Nb6Mo3Si4 alloys were relatively easily formed into the amorphous state. Nb3Al ...

252

Investigations into the corrosion resistance of copper aluminium alloys. Effect of phosphorus as corrosion resistant third alloying element in the ternary system CuAl20P1  

International Nuclear Information System (INIS)

The effect of phosphorus on the corrosion resistance of Al-bronzes is studied in detail in this work. A literature review showed that there are a lot of things known about the microstructure and the mechanical properties of Al-bronzes. In spite of their corrosion resistance the corrosion properties and the structure of the protective oxide films of Al-bronzes were seldom a matter of interest. Systematic studies of the influence of different alloying elements on the oxide film and the corrosion properties are rare. Therefore, it is not possible to predict the corrosion resistance of Al-bronzes, made by alloying particular elements. The high corrosion resistance of the new alloy CuAl_2_0P_1 was the reason to investigate the influence of phosphorus on the corrosion properties of Al-bronzes in more detail. A systematic study of the microstructure and the corrosion properties of Cu, CuP_x, CuAl_2_0 and ...

253

Enhanced corrosion resistance by sol-gel-based ZrO_2-CeO_2 coatings on magnesium alloys  

International Nuclear Information System (INIS)

The physical, chemical and mechanical properties of magnesium alloys make them attractive materials for automotive and aerospace applications. However, these materials are susceptible to corrosion and wear. This work discusses the potential of using sol-gel based coatings consisting of ZrO_2 and 15 wt.% of CeO_2. The CeO_2 component provides enhanced corrosion protection, while ZrO_2 impart corrosion as well as wear resistance. Coating deposition was performed by the dip coating technique on two magnesium alloy substrates with different surface finishes: AZ91D (as-casted, sand-blasted, and machined) and AZ31 (rolled and machined). All as-deposited coatings (xerogel coatings) were then subjected to 10 h annealing: a temperature of 180 C was applied to the AZ91D alloy and 140 C to the AZ31 alloy. Morphological and structural properties of the annealed coatings were investigated by ...

2005-02-01

254

Electrochemical investigation of passive film formed on Alloy 600  

Energy Technology Data Exchange (ETDEWEB)

Alloy 600 is used as a material for steam generator tubing in pressurized water reactors(PWR) due to its high corrosion resistance under PWR environment. In spite of its corrosion resistance, stress corrosion cracking(SCC) has occurred on the primary side as well as the secondary side of the tubing. Oxide on steel surfaces in aqueous solution above 100 .deg. C is composed of duplex film structure. Inner layer of the oxide is dense and less porous, which is formed by growth of oxide layer on metal surface. Outer layer of the oxide is loose adhesive, which is formed by dissolution precipitation mechanism. Growth processes occur at the metal/oxide and oxide/electrolyte interfaces and are controlled by transport of the layer forming species through the layer, i.e. by the inward diffusion of oxygen including electrolyte species and the outward diffusion of metal cations. Understanding of basic electrochemical behaviors about anodic dissolution and ...

2005-07-01

255

The role of fatigue variability in life prediction of an #alpha#+#beta# titanium alloy  

International Nuclear Information System (INIS)

The fatigue life variability of the #alpha#+#beta# titanium alloy, Ti-6Al-2Sn-4Zr-6Mo increased with decreasing stress level. The variability in life was found to be due to segregation of lives due to two failure mechanisms. A bimodal cumulative distribution model was shown to accurately describe the combined failure modes. The nominal failure processes for the two regimes were similar, with crack nucleation occurring in equiaxed #alpha#p particles, irrespective of life or stress level. However the variability in life was not controlled by the size of the crack-nucleating #alpha#p, but rather by the ability of the material to distribute deformation and avoid early crack nucleation.

2004-06-10

256

The pressure- and temperature dependence of the electrical resistivity of some amorphous Fe-B alloys  

International Nuclear Information System (INIS)

We report measurements of the electrical resistivity of the amorphous alloys Fe"4"0Ni"4"0P"1"4B"6 (Metglas 2826), Fe"3"2Ni"3"6Cr"1"4Pr"1"2B"6 (Metglas 2826A) Fe"8"0B"2"0 (Metgals 2605) and Fe"7"5B"2"5 as a function of pressure and temperature. The pressure is varied between 0 and 12 GPa, the temperature between 1.2 and 380 K. At low temperatures the pressure dependence yields additional information on the scattering mechanism. (orig.).

257

TIMETAL reg-sign 21S property data  

International Nuclear Information System (INIS)

TIMETAL reg-sign 21S, which has the nominal weight percent composition 15Mo, 3Al, 3Nb, and 0.2Si, is a metastable beta titanium alloy that offers a unique combination of high strength, good elevated temperature properties, and extraordinary environmental degradation resistance. It was developed by TIMET in 1988 as a foil matrix material for titanium metal matrix composites for the NASP, but currently monolithic applications are of much more significance. Among the alloy's unique properties are a high resistance to attack by commercial aircraft hydraulic fluids (commonly referred to as Skydrol trademark, which will be the term used in this paper) at all temperatures, which has led to its use in nacelle components on the Boeing 777 and other commercial aircraft. This paper provides an overview of the physical and mechanical properties of TIMETAL reg-sign 21S.

1993-02-21

258

Research on corrosion resistance of steam generator tube  

International Nuclear Information System (INIS)

In order to improve the reliability of PWR steam generators, we have performed research to improve the tubing material and tube-support-plate configuration, based on our wide operating experience, and have developed and verified Alloy TT690 as the optimum tubing material and the BEC (Broached Egg Crate) type tube-support design. In the research, we have studied the metallurgical mechanism of the alloy to improve its corrosion resistance, evaluated corrosion susceptible region quantitatively, estimated the actual environment in a steam generator and confirmed the reliability by a model boiler test over a long period. It has been verified that the steam generator with the latest design has higher reliability with respect to the corrosion resistance of tubes. (author).

259

First principles investigations of formation of ordered omega phases in Zr-Al alloys  

International Nuclear Information System (INIS)

First-principles density functional theory (DFT) based calculations were performed to study the electronic and cohesive properties of all the intermediate ordered phases appearing in the transformation from bcc-based #beta# to hexagonal ordered #omega# phase in Zr_3Al alloy. Full-potential linear augmented plane wave (FPLAPW) method under the GGA was employed to establish the stability hierarchy and structure-property correlations. Further, effective pair potentials upto the fourth nearest neighbours were extracted, which, subsequently, were used for the thermodynamics analysis of the thermally-induced #beta##->##omega# transformation. The lattice collapse mechanism involving the concept of the onset of a displacement wave where the extent of collapse is viewed as an amplification of the displacement wave was employed for further analysis. (author)

2005-12-05

260

Enhanced diffusion from interstitial trapping during solid-phase-epitaxial growth of silicon alloys. Draft  

Energy Technology Data Exchange (ETDEWEB)

During the recrystallization by solid-phase-epitaxial (SPE) growth of supersaturated silicon alloys, a high concentration of interstitials is trapped. These are released by subsequent heating causing a transient (greatly enhanced) diffusion of the substitutional dopant by an interstitialcy mechanism. The enhancement may be as much as five orders of magnitude over tracer values, and shows an activation energy of only 1.8 +- 0.2 eV. Following the transient, the interstitials condense into loops, allowing an independent estimate to be made of their concentration. From these observations, we propose that during ion implantation, a fraction of the implanted dopants can acquire their natural valency, and retain it as the crystallization interface passes. For group V dopants this creates the trapped interstitials, giving transient enhanced diffusion when they are released by subsequent annealing.

1984-08-01

261

Enhanced diffusion from interstitial trapping during solid-phase-epitaxial growth of silicon alloys  

Energy Technology Data Exchange (ETDEWEB)

During the recrystallization by solid-phase-expitaxial (SPE) growth of supersaturated silicon alloys, a high concentration of interstitials is trapped. These are released by subsequent heating causing a transient (greatly enhanced) diffusion of the substitutional dopant by an interstitialcy mechanism. The enhancement may be as much as five orders of magnitude over tracer values, and shows an activation energy of only 1.8 +/- 0.2 eV. Following the transient, the interstitials condense into loops, allowing an independent estimate to be made of their concentration. From these observations, it is proposed that during ion implantation, a fraction of the implanted dopants can acquire their natural valency, and retain it as the crystallization interface passes. For group V dopants this creates the trapped interstitials, giving transient enhanced diffusion when they are released by subsequent annealing. 12 references, 6 figures.

1984-01-01

262

Embryo-damage induced nucleation of microcracks in an aluminum alloy under impact loading  

Energy Technology Data Exchange (ETDEWEB)

The nucleation of microdamage under dynamic loading was investigated through planar impact experiments accomplished with a light gas gun. The microscopic observation of recovered and sectioned specimens showed that microcracks were nucleated only by cracking of brittle particles inside material. However, for comparison the in situ static tensile tests on the same material conducted with a scanning electron microscope showed that the microcracks were nucleated by many forms those were fracture of ductile matrix, debonding particles from matrix and cracking of brittle particles. The quantitative metallographic observations of the specimens subjected to impact loading showed that most of the cracked particles were situated on grain boundaries of the aluminum matrix. These facts suggested the concept of critical size and incubation time of submicroscopic cavities in the dynamic case and the mechanism of embryo-damage induced nucleation by fracture of brittle particles ...

1995-06-01

263

Electrodeposition and characterization of Ni-Co/SiC nanocomposite coatings  

British Library Electronic Table of Contents (United Kingdom)

Ni-Co/SiC nanocomposite coatings were electrodeposited in a modified watt type of Ni-Co bath containing 20nm SiC particles to be codeposited. Potentiodynamic polarization tests were conducted to study the effect of the SiC particulates on the electrodeposition of Ni and Co. Scanning electron microscopy was used to assess the morphology of the Ni-Co alloy and Ni-Co/SiC nanocomposite coatings. The distribution of the particulates in the matrix was considered by means of transmission electron microscopy. Applying nanomechanical testing instruments coupled to atomic force microscopy, mechanical properties of the alloy and composite coatings were studied and compared. The presence of 11vol.% SiC in the Ni-Co matrix increased hardness more than 60%. The average depth of scratch in the mentioned ...

2011-01-01

264

Effect of heat treatment on tensile properties and fracture toughness of two-phase #alpha#+#beta# titanium alloy Ti-6Al-2Mo-2Cr  

International Nuclear Information System (INIS)

In the paper results of the investigation on the effect of microstructure on room temperature tensile properties and fracture toughness of two-phase #alpha#+#beta# titanium alloy Ti-6Al-2Mo-2Cr have been presented. Microstructure has been varied by changes in the cooling rate from the solution treatment temperature and aging time and temperature. Mechanical properties examined show dependence on the treatment conditions, especially aging conditions. It has been attributed mainly to the amount and morphology of #alpha# phase obtained after heat treatment. The higher volume fraction of lamellar #alpha# structure, the higher fracture toughness. (author)

1998-05-17

265

Behavior of Stress-Relaxation phenomena in Zr-1.1Nb-0.05Cu  

International Nuclear Information System (INIS)

Zirconium alloys have anisotropic mechanical properties depending on their physical orientations and are widely used as nuclear materials such as cladding tube material. An operation condition of the nuclear reactor requires a high creep resistance, because it is subjected to long period operations, high temperature and high pressure. Generally, it takes a few days or months to do the creep experiment, so it is difficult to get a data in short period. However, there is a way to predict a creep property by using the stress-relaxation in the short term. These studies realized the stress-relaxation through a compressive test of HANA-6 (Zr-1.1Nb-0.05Cu) alloy that was developed by KAERI (Korea Atomic Energy Research Institute), and then predicted the creep property

2010-10-01

266

Asymmetrical mechanical behavior of a precipitation hardened beta titanium alloy  

International Nuclear Information System (INIS)

Precipitation-hardened single crystals of a beta (bcc) Ti--40 at. percent V--1.0 at. percent Si alloy were deformed in compression at 77 and 298"0K. The dependence of the yield stress upon aging time at 843"0K for solution-treated crystals shows two maxima which are caused by silicide precipitates. The orientation dependence of the yield stress and of the active macroscopic slip plane were determined as a function of aging time. The solution-treated as well as aged crystals exhibit an asymmetry of both the yield stress and the plane of slip, the degree of asymmetry being larger at 77 than at 298"0K. The asymmetry of slip and yielding is not affected by the presence of precipitation hardening. Results indicate that the effect of the dislocation core structure on dislocation motion is independent of the presence of precipitates. (auth).

267

Solid-state amorphization reaction in mechanically deformed Al_xHf_1_0_0_-_x multilayered composite powders and the effect of annealing  

International Nuclear Information System (INIS)

Single phase amorphous Al_xHf_1_0_0_-_x alloys with a wide amorphization range (33#<=#x#<=#75) were synthesized by the solid-state interdiffusion of pure polycrystalline Al and Hf powders at room temperature using a rod-milling technique. The mechanisms of metallic glass formation and competing crystallization processes in the mechanically deformed composite powders were investigated by means of X-ray diffraction, differential thermal analysis, scanning electron microscopy and transmission electron microscopy. The numerous intimate layered composite particles of the diffusion couples that formed during the first and intermediate stages of milling (0-173 ks) are intermixed to form amorphous phase(s) upon heating to about 980 K by so-called thermally assisted solid-state amorphization (TASSA). The amorphization heat formation for the binary Al_xHf_1_0_0_-_x system via TASSA, #DELTA#H"T"A"S"S"A_a, was measured directly ...

1999-03-04

268

Weld solidification and HAZ liquation in a metastable-beta titanium alloy-Beta-21S  

International Nuclear Information System (INIS)

Beta-21S is a new, metastable-beta titanium alloy which exhibits excellent oxidation resistance and mechanical properties at elevated temperatures. From a weld solidification standpoint, this alloy chemistry is of particular interest because its major beta-stabilizing elements (Mo and Nb) both exhibit equilibrium partitioning ratios (k_o) greater than unity, indicating their simultaneous partitioning during weld solidification to the initial solid to form (i.e., dendrite cores), and correspondingly their depletion in the final regions of solidification (i.e., dendrite interstices). Such elemental partitioning, if retained down to room temperature, may be expected to promote local variations in the postweld aging response. The objectives of the present investigation were to characterize Gas Tungsten-Arc weld solidification and HAZ liquation phenomena in Beta-21S and to examine the influence of residual microsegregation in ...

269

The use of alloy 800 in the THTR steam generator  

International Nuclear Information System (INIS)

In 1972 a consortium consisting of Gebruder Sulzer A.G., Winterthur and EVT, Energie- und Verfahrenstechnik G.m.b.H., Stuttgart, was awarded the contract by HBR, Hochtemperatur Reaktorbau G.m.b.H., Koln/Mannheim, for the design, manufacture and installation of the 6 steam generator units for the prototype 300 MWe Thorium High Temperature Reactor (THTR) at Schmehausen, Germany. The design and manufacture of the 6 units is done by Sulzer; installation of the units as well as the manufacture of the external pipework and headers is done by EVT. The units are built under semiclean conditions in a special workshop at CCM-Sulzer in mantes, France. This workshop had been used previously for the manufacture of the steam generators for the nuclear power plants St. Laurent I, II, Vandellos (500 Mwe each) and EL-4 (70 Mwe). The present paper defines the operating conditions and the chemical composition of the materials used, including Alloy 800. Reasons for the choice of ...

270

Surface treatment of Ti-6Al-4V alloy by rf plasma nitriding  

Energy Technology Data Exchange (ETDEWEB)

The Ti-6Al-4V alloy was treated by inductively coupled rf plasma nitriding. The effects of plasma-processing time in the range of 5-35 min on the microstructure and the mechanical properties of the plasma-nitrided Ti-6Al-4V samples were studied. The plasma power input was adjusted at 450 W and pure N{sub 2} gas was introduced to establish a treatment pressure of 8.0-8.4 x 10{sup -2} mbar. The characteristics of the nitrided layers have been investigated by microhardness testing, surface roughness measurements, optical microscopy, and x-ray diffraction. The results show that the surface microhardness increases as the plasma-processing time increases to reach 2000 HV0.1 at a plasma-processing time of 35 min. A high nitriding rate of 2.81 {mu}m{sup 2} s{sup -1} at a plasma-processing time of 25 min was achieved. The formation of the hard phases TiN, Ti{sub 2}N, and Ti(N) in the Ti-6Al-4V surfaces are found to be the reason for the increased ...

2007-10-03

271

Surface treatment of Ti-6Al-4V alloy by rf plasma nitriding  

International Nuclear Information System (INIS)

The Ti-6Al-4V alloy was treated by inductively coupled rf plasma nitriding. The effects of plasma-processing time in the range of 5-35 min on the microstructure and the mechanical properties of the plasma-nitrided Ti-6Al-4V samples were studied. The plasma power input was adjusted at 450 W and pure N_2 gas was introduced to establish a treatment pressure of 8.0-8.4 x 10"-"2 mbar. The characteristics of the nitrided layers have been investigated by microhardness testing, surface roughness measurements, optical microscopy, and x-ray diffraction. The results show that the surface microhardness increases as the plasma-processing time increases to reach 2000 HV0.1 at a plasma-processing time of 35 min. A high nitriding rate of 2.81 #mu#m"2 s"-"1 at a plasma-processing time of 25 min was achieved. The formation of the hard phases TiN, Ti_2N, and Ti(N) in the Ti-6Al-4V surfaces are found to be the reason for the increased microhardness. Surface ...

2007-10-03

272

Study of fractures in cast parts of high-strength aluminum alloy  

Energy Technology Data Exchange (ETDEWEB)

Results are presented from studies on the quality of cast parts made by counterpressure casting of high-strength aluminum alloy AMKh-605, and Al-Cu-Mn-Cr alloys (5.6-6.4% Cu, 0.25-0.55% Mn, 0.20-0.55% Cr, 0.20-0.45% Ti, 0.08-0.25% Zr, less than or equal to0.25% Fe, less than or equal to0.25% Si, less than or equal to0.05% Mg). Chill castings were heat treated by quenching from 450/sup 0/C (20 hours) in water, aging at 160/sup 0/C for five hours with cooling in air. Fractograms of tensile specimens are presented. Scanning electron microscopy allows an ambiguous determination of the cause of failure of a part, be it at initial crystallization crack defects or burns, and also allows a relationship to be established between structure and mechanical properties.

1985-03-01

273

Pitting corrosion resistance of high-alloy OCTG in CO_2 environment as affected by chlorides and sulfides  

International Nuclear Information System (INIS)

High general corrosion resistance of high-alloy OCTG (oil country tubular goods) to CO_2 may be limited by pitting corrosion in presence of chlorides and sulfides. The pitting resistance of 13% Cr steel, duplex and high Ni austenitic stainless steels have been examined by electrochemical measurements in a high temperature, high pressure autoclave simulating the well conditions. Each steel shows the pitting potential in CO_2-NaCl-H_2O system, the value of which being less noble as the Cl"- concentration and the temperature increase. The presence of H_2S is also detrimental. High alloying additions of Cr and Mo enhance pitting resistance whether or not H_2S is present. The corrosion potentials of these steels in the simulating well conditions in which oxygen is absent do not exceed the pitting potential. Therefore, pitting corrosion can not occur by the passivity break through mechanism.

274

Oxide growth on aluminium alloys in the presence of ammonium fluoborate  

Energy Technology Data Exchange (ETDEWEB)

The aim of this study as to determine the mechanisms involved in using ammonium fluoborate as a reducing atmosphere when preheating a high magnesium content aluminium alloy. Rutherford Backscattering (RBS) has been the major technique used in the analysis of samples, it revealed significant reduction in both the diffusion of magnesium to the surface and the calculated oxide thickness in the presence of NH{sub 4}BF{sub 4}. At temperatures above 500 deg C in air, SEM images revealed depressions and voids due to incipient melting at various stages, around the grain boundaries. Grain boundaries effectively acted as pipes aiding the diffusion of magnesium to the surface. These results have been verified through compositional analysis with both RBS and auger electron spectroscopy (AES). Results from NH{sub 4}BF{sub 4} atmosphere preheat conditions showed significant improvements. It was verified experimentally that above 500 deg C , AA5182 ...

1996-12-31

275

Oxidation resistance of slurry aluminides on high temperature titanium alloys  

International Nuclear Information System (INIS)

Slurry aluminizing is one method of protecting titanium alloys and intermetallics at temperatures at which oxidation would otherwise significantly degrade mechanical properties. The technique produces a continuous layer of alumina-forming TiAl_3 on exposed surfaces. The influence of composition, film thickness, and diffusion temperature upon the oxidation resistance of these slurry aluminides was studied in cyclic tests to 816degC (1500deg F). Degradation of slurry aluminized #beta#-titanium alloy and #alpha#-Z titanium aluminide intermetallic occurs by localized oxidation at cracks in the coating layer. These cracks are probably due to mismatch of coefficients of thermal expansion between the coatings and substrates. Addition of silicon to the slurry modifies the oxidation behaviour around a crack by introducing a continuous layer of titanium silicide at the boundary of the aluminide coating and substrate, thereby ...

276

High temperature friction and wear characteristics of superalloys X-750 and 188 for use in low heat rejection engines  

Energy Technology Data Exchange (ETDEWEB)

Engineering materials for use in low heat rejection engines are required to function under stringent tribological conditions. Severe wear damage and high friction between the components of the tribosystem limit the number of potential materials suitable for such application conditions. The superalloys X-750 and 188 are composed of alloying elements that not only promote a high mechanical and chemical stability but may also result in a reduced wear rate and friction coefficient at elevated temperatures. As a part of the DOE-ECUT Tribology program at Argonne, the present study was undertaken to evaluate the tribological characteristics of these alloys that will also be utilized as the substrates for ion beam deposited lubricous coatings. A wear test rig that crudely simulated the sliding conditions between a piston ring and a cylinder liner in an operating engine was utilized for friction and wear studies. The test results ...

1988-01-01

277

High temperature deformation behavior of AZ31 Mg alloy  

Energy Technology Data Exchange (ETDEWEB)

High temperature deformation behavior of AZ31 Mg alloy was investigated in this study on the basis of a processing map ({epsilon} {approx} 0.6). To construct a processing map, compression tests were carried out at various temperatures and strain rates. Two regions of high deformation efficiency ({eta}) were identified as: (1) a dynamic recrystallization (DRX) domain at 250 C and 1/s and (2) a superplasticity domain at 450 C and 10{sup -4}/s. The average grain size observed in the DRX region was considerably smaller (2.9{mu}m) than in any other region. In the superplastic condition, tensile elongation to failure approached to 1040%. At the high Z regions, flow softening occurred resulting from the dynamic recrystallization but below 10{sup 10} of Z value, flow hardening occurred due to the grain growth. Possible deformation mechanisms operating at high temperature were discussed in relation to the activation energy. A two-stage deformation ...

2005-07-01

278

Fracture behavior of heat-affected zone in low alloy steels  

International Nuclear Information System (INIS)

Past elastic-plastic fracture studies for leak-before-break (LBB) assessment of low alloy steel pipings have been focused mostly on the behavior of base metals and their weld metals. In contrast, the heat-affected zone (HAZ) of a welded pipe has not been studied in detail primarily because the size of the HAZ is too small to make specimens for mechanical properties measurements. In this study, microstructural analyses, microhardness tests, tensile tests and J-R tests have been conducted as a function of distance from a fusion line and temperature for HAZ materials of SA106Gr.C low alloy piping steels. For the ferrite-pearlite steels such as SA106Gr.C, the HAZ specimens showed a higher yield strength and fracture toughness compared with those of its base metal. These characteristics, despite of grain coarsening, can be explained by cleaner microstructures of HAZ materials with a finer morphology of carbides compared with ...

2001-11-01

279

Effect of low copper content and heat treatment on intergranular corrosion of model AlMgSi alloys  

International Nuclear Information System (INIS)

Certain 6000-series extrusions may develop susceptibility to intergranular corrosion (IGC) by improper heat treatment, especially if copper is present as an alloying element. Although occurrence of IGC in such cases is documented, the underlying mechanisms are not adequately explained. We present corrosion data for two model alloys, having different Cu content and Mg:Si ratio, showing that the susceptibility to IGC depended primarily on the Cu content and secondly on thermal processing. Low Cu samples (0.0005 wt.% Cu) were essentially resistant to IGC. High Cu samples (0.12 wt.% Cu), which were air cooled after extrusion, exhibited significant IGC. However, IGC susceptibility was reduced significantly as a result of artificial aging to peak strength. Water quenched high Cu samples were essentially resistant to IGC. However, slight IGC susceptibility was introduced after aging. Electron optical characterisation revealed ...

2006-01-01

280

Development of a new wear-resistant material: TiC/TiNi composite  

Energy Technology Data Exchange (ETDEWEB)

In this work, an attempt was made to develop a novel type of wear-resistant composite employing a TiNi alloy matrix reinforced by hard particles. Titanium carbide was chosen as the reinforcing phase because of its high hardness and TiNi alloy as the matrix due to its pseudoelasticity and good toughness. TiC particles may sustain external load, while the TiNi matrix may accommodate deformation, absorb impact energy and retain the hard particles. Such a combination is expected to lead to an enhanced wear resistance, compared to TiNi alloy. As a matter of fact, some efforts were previously made to develop TiNi-matrix composite reinforced by ceramic particles. However, the emphasis of those studies was put on effects of the reinforcing particles on the phase transformation behavior, shape memory effect and some mechanical properties of the composite; no attempt was made to explore the potential benefit of ...

1999-10-22

281

Study on warm caliber rolling of magnesium alloy  

Energy Technology Data Exchange (ETDEWEB)

The warm caliber rolling was experimented using the AZ31 magnesium alloy round bar of 20 mm in diameter machined from cast ingot materials. In warm caliber rolling in final size of 10 mm in diameter at 623 K via 8passes, each width-spreading, the change of each microstructure, X-ray analysis of final texture and final mechanical properties were investigated. Microstructure, texture and mechanical properties of warm caliber rolled round bar at 473 K via latter 4passes were compared with those at 623 K consistently. Obtained results are as follows: (1) The width-spreading in caliber rolling of round bar is relatively large, compared with that in flat rolling of the flat bar. The largeness of width-spreading of round bar makes the shape control of cross section difficult, and causes the cracks around the free surface. (2) Finer microstructure and inclined c axis of hexagonal lattice of 10 degrees to vertical direction of the ...

2003-07-01

282

Phenomenological 3D and 1D consistent models for shape-memory alloy materials  

Science.gov (United States)

The paper deals with the modeling and the development of a numerical procedure for the analysis of shape-memory alloy (SMA) elements in order to predict the main features of SMA devices. A 3D SMA model in the framework of small strain theory is developed starting from the thermo-mechanical model proposed by Souza et al. (Eur J Mech A/Solids 17:789-806, 1998) and modified by Auricchio and Petrini (Int J Numer Methods Eng 55:1255-1284, 2002). The aim of this paper is to propose some more modifications to the original model, to derive its consistent 1D formulation, to clarify the mechanical meaning of the material parameters governing the constitutive model. A robust time integration algorithm is developed in the framework of the finite element method and a new beam finite element is proposed. Some numerical applications and a comparison with experimental data available in literature are carried out in order to assess the ...

2009-08-01

283

Modeling of the relaxation kinetics of metastable tensile strained Si:C alloys  

Energy Technology Data Exchange (ETDEWEB)

In order to enhance the performance of CMOS transistors, embedded epitaxial layers of Si:C can be used. In the present work, Si:C layers with Carbon contents up to 1.9 at-% and in-situ Phosphorus doping up to 4 x 10{sup 20}At/cm{sup 3} have been investigated. Due to the low solubility of Carbon in Silicon (0.0004 at.-% at the melting point), all layers considered in this work are metastable and tend to relax. Since it is crucial to the application to retain the strain of those layers, the responsible mechanisms must be understood. The relaxation during thermal treatment was studied by high resolution X-ray diffraction and was found to behave differently, depending on Carbon content and Phosphorus doping concentration. In this work, we propose a relaxation mechanism based on a kick-out reaction of substitutional Carbon which is accelerated by Phosphorus content through transient enhanced diffusion. We simulate the time evolution of layer ...

2010-07-01

284

Long-term reliability of amorphous alloy wound core distribution transformers  

Energy Technology Data Exchange (ETDEWEB)

In order to verify long-term reliability of amorphous alloy wound core distribution transformers, accelerated aging tests and field trials used by actual transformers were practiced. As for accelerated aging tests, short-circuit tests were added to imitate mechanical stress in operation on a utility's distribution system. As a result, even after the equivalent of 30 years, which was the normal expected transformer's life, magnetic characteristic was unchanged, so these transformers could be operated. Also, about field trials, two hundred transformers of four kinds were installed on a utility's distribution system to look into no-load characteristics. They were equipped with a mechanism to measure load current, background vibration and lightning surge current, so the influence for magnetic characteristic could be inspected. As a result, remarkable change wasn't seen even after six months.

1994-01-01

285

A mechanistic understanding of the formability of magnesium: examining the role of temperature on the deformation mechanisms  

Energy Technology Data Exchange (ETDEWEB)

The possibility of improving the cold formability of wrought magnesium alloys is considered in light of their good hot forming characteristics. Magnesium alloy AZ31B sheet is selected as a model system. Parameters affecting formability, such as strain hardening rate, strain rate sensitivity, and the degree of anisotropy are examined systematically by conducting tensile tests over a range of temperatures (room temperature to 250 C) and strain rates (1 x 10{sup -5} to 0.1 s{sup -1}). The plastic anisotropy and deformation texture evolution are examined in samples aligned with the sheet rolling and transverse directions. Polycrystal plasticity simulations using a viscoplastic self-consistent (VPSC) formulation are used to model the observed anisotropy and texture evolution. The adjustable parameters in the model are the relative critical resolved shear stresses of the dislocation mechanisms known to operate within magnesium. ...

2003-07-01

286

Substitution of molybdenum for tungsten in alloys of the cold working steel 60 WCrV 7. Legierungsaustausch von Wolfram durch Molybdaen beim Kaltarbeitsstahl 60 WCrV 7  

Energy Technology Data Exchange (ETDEWEB)

The effect of partial and total replacement of tungsten by molybdenum on the mechanical technical properties were investigated with the cold work steel 60 WCrV 7 (DIN 1.2550). While maintaining the total quantity of tungsten atoms and/or molybdenum atoms in the steel, no differences occur in the type of the separated carbides. After annealing in the range of the pearlite stage with annealing times of up to 150 h, the carbide phases M/sub 23/C/sub 6/ and MC are, besides alpha iron, also present. In short-time annealed states also M/sub 6/C carbides occur. These are formed during austeniting and remain in the steel as residual carbides in austeniting treatment carried out under normal conditions. Compared with tungsten alloyed steel, there is an increased formation of M/sub 6/C carbides in molybdenum alloyed steels during austeniting. By a long-time annealing treatment in the range of the pearlite stage, the M/sub 6/C ...

1985-12-11

287

Slow strain-rate testing of Alloy 800 in molten-nitrate salts  

Energy Technology Data Exchange (ETDEWEB)

An experimental technique has been developed to examine the interaction between deformation and the exposure of certain high temperature structural alloys to oxidizing molten salt environments. The experimental program involved performing a series of long-term tensile tests over a wide range of strain rates. Fracture strain reduction in area and ultimate strength (UTS) were monitored as parameters indicative of an alloy's susceptibility to environmental degradation. For Incoloy Alloy 800 tested at 600/sup 0/C in the salt medium and at initial strain rates between 2 x 10/sup -7/ sec/sup -1/ and 1 x 10/sup -5/ sec/sup -/1 no appreciable loss of ductility, as measured by reduction in area, was observed relative to control specimens tested in air at the same temperature and strain rates. Similarly, fracture strain and UTS were essentially unaffected by exposure to the oxidizing environment. The structure of the oxide ...

1982-01-01

288

Load-carrying capabilities of refractory alloys for space reactor power applications  

International Nuclear Information System (INIS)

To achieve sufficient thermodynamic efficiency, space nuclear power systems must operate above 1000"0C. A quantitative evaluation of the existing mechanical properties data for the refractory alloys relevant to space nuclear power systems design lifetimes up to seven years at temperatures up to 1400"0C is being conducted. The most important properties for space nuclear power systems are long-term high-temperature (>1000"0C) creep strength and ductility, low-temperature (<400"0C) fracture toughness [including ductile-to-brittle transition temperature, (DBTT)], and ductility at high strain rates; of special concern are the above properties for weldments of refractory alloys, composition, applied stress, test temperature, test environment (e.g., vacuum, lithium), and thermomechanical treatment (TMT) history. Currently being evaluated are, in order of ascending mp, selected alloys of niobium (e.g., ...

1985-01-14

289

Load-carrying capabilities of refractory alloys for space reactor power applications  

Energy Technology Data Exchange (ETDEWEB)

To achieve sufficient thermodynamic efficiency, space nuclear power systems must operate above 1000/sup 0/C. A quantitative evaluation of the existing mechanical properties data for the refractory alloys relevant to space nuclear power systems design lifetimes up to seven years at temperatures up to 1400/sup 0/C is being conducted. The most important properties for space nuclear power systems are long-term high-temperature (>1000/sup 0/C) creep strength and ductility, low-temperature (<400/sup 0/C) fracture toughness (including ductile-to-brittle transition temperature, (DBTT)), and ductility at high strain rates; of special concern are the above properties for weldments of refractory alloys, composition, applied stress, test temperature, test environment (e.g., vacuum, lithium), and thermomechanical treatment (TMT) history. Currently being evaluated are, in order of ascending mp, selected alloys ...

1985-01-01

290

Theoretical investigations of strength of a flexible tube made of NiTi; Festigkeitstheoretische Untersuchungen einer flexiblen Huelse aus NiTi  

Energy Technology Data Exchange (ETDEWEB)

A flexible, steerable tube (distal end) of an endoscope for the application in the laparoscopic surgery has been analyzed by means of the finite-element-method (FEM). The unusual mechanical and thermal features of the used shape memory alloy (SMA) of NiTi were taken in account. The analyses showed that the strains remain in the super-elastic region up to the maximum bending of 90 and no plastic deformations occur. The application of the shape optimization (CAO) made possible finding the optimal structure of the distal end and therefore powerful reducing the maximum strains in the critical regions. (orig.)

2000-04-01

291

CRC materials science and engineering handbook. Third edition  

Energy Technology Data Exchange (ETDEWEB)

This definitive reference is organized in an easy-to-follow format based on materials properties. It features new and existing data verified through major professional societies in the materials fields, such as ASM International and the American Ceramic Society. The third edition has been significantly expanded, most notably by the addition of new tabular material for a wide range of nonferrous alloys and various materials. The contents include: Structure of materials; Composition of materials; Phase diagram sources; Thermodynamic and kinetic data; Thermal properties of materials; Mechanical properties of materials; Electrical properties of materials; Optical properties of materials; Chemical properties of materials.

1999-01-01

292

Anodic oxide coatings on metals and anodic protection /2nd revised and enlarged edition/. Anodnye oksidnye pokrytiia na metallakh i anodnaia zashchita /2nd revised and enlarged edition/  

Energy Technology Data Exchange (ETDEWEB)

The theoretical principles underlying the formation of oxide and, in particular, anodic oxide coatings on metals produced by chemical oxidation, anodizing in solutions, and anodizing in cold plasmas are reviewed. The mechanisms and conditions of anodic oxidation are described, and the structure of anodic oxide coatings on aluminum, magnesium, beryllium, zinc, cadmium, iron, cobalt, nickel, titanium, zirconium, tantalum, and chromium alloys is examined. Attention is also given to various applictins of anodized coatings. 54 references.

1985-01-01

293

Stress corrosion cracking: 1965-1990  

Energy Technology Data Exchange (ETDEWEB)

Advances in the theory and practice of stress corrosion cracking (SCC) are reviewed for the period 1965-1990. The proceedings of two landmark conferences are used as a basis for discussion: Ohio State University (1967) and Kohler, WI (1988). The discussion is developed around the following topics: metal-environment combinations, testing, fractography, metallurgical aspects, electrochemical aspects and crack chemistry, mechanisms, and prediction and mitigation. It is concluded that the main developments since 1967 are the recognition of the lack of specificity of SCC environments, the use of slow strain rate and fracture mechanics testing, quantitative SEM fractography, studies of grain boundary structure and compositions, transient electrochemistry of bare metal surfaces, measurement and modelling of crack chemistry, elaboration of several SCC models, including slip-dissolution and film induced cleavage, and mitigation by ...

1990-01-01

294

On the solid-fluid transition zone in welding analysis  

Energy Technology Data Exchange (ETDEWEB)

Equilibrium and energy equations have been developed in describing the solid-fluid transition zone during the melting and solidification of the binary alloys. Due to the existence of the transition region exhibited both solid and fluid phases at the same material point from continuum point of view, mixture theory was utilized to analyze the region. Unlike the Stefan problem, the latent heat due to the phase change appears as a source term in the heat equation. The molten fluid is treated as a thermoviscous and incompressible fluid, whereas the solid is thermoviscoplastic described by the Bodner-Partom/Walker type of constitutive equations. Thermal mechanical behaviors of the solid and the fluid phases are determined separately because of insignificant mechanical interactions between them. Volume fractions of the phases are obtained according to the equilibrium phase diagram. The simulation process of the transition zone and ...

1993-01-01

295

New wear resistant composite material  

Energy Technology Data Exchange (ETDEWEB)

A composite material consisting of WC-Co particles in a steel matrix was fabricated by sintering mixtures of WC-Co particles and a steel powder and infiltrating the sintered pieces with a copper alloy. Its wear resistance and mechanical properties were studied as a function of the content in WC-Co particles and other characteristics of the composite material microstructure. Infiltration provided a simple means to obtain a strong cohesion between WC-Co particles and the steel matrix. An effective matrix protection against wear is obtained with relatively low additions of particles especially with a silica abrasive which is soft with respect to cemented carbide. The experimental results show that this material has good mechanical properties and wear resistance. Depending upon abrasion resistance, wear losses are reduced up to 10 times by a 30 vol% addition of cemented carbide particles.

1983-01-01

296

In-situ solid-state synthesis of Mg composite with Mg{sub 2}Si dispersoids  

Energy Technology Data Exchange (ETDEWEB)

Super light and high performance Mg{sub 2}Si/Mg composites, which had excellent mechanical properties, were developed via the combination of solid-state synthesis and hot extrusion process. In this study, cold compacting (CP) and repeated plastic working (RPW) were firstly carried out for the mixture of Mg-Si powders, and the refinement of both Mg grains and dispersoids. Each specimen was evaluated by observation of microstructure and tensile test. As a result, it was understood that Mg{sub 2}Si dispersoids were refined and dispersed into Mg matrix, and were flowed along extrusion direction. And their mechanical properties were higher than the conventional die casting alloys. Also the effect of RPW as the improvement of properties and the decrease of synthesis temperature were confirmed. (orig.)

2005-07-01

297

Computational modeling of dynamic-failure mechanisms in armor/anti-armor materials. Final report, 1 Oct 88-30 Sep 91  

Energy Technology Data Exchange (ETDEWEB)

The purpose of this project was to develop improved dynamic failure models for brittle materials (primarily ceramics). The approach to developing these failure models was to establish a database (ACERAM) in which fundamental material properties and processing information could be directly correlated with ballistic performance data. Under this contract, a comprehensive literature search was conducted, many contacts were established in the armor/anti-armor research and development community, and database development was undertaken. A more limited project was also undertaken to assess and compare the effects of material properties and penetration mechanisms on the ballistic performance of depleted uranium and tungsten alloy penetrators.

1991-02-01

298

Prediction of Corrosion of Advanced Materials and Fabricated Components  

Energy Technology Data Exchange (ETDEWEB)

The goal of this project is to provide materials engineers, chemical engineers and plant operators with a software tool that will enable them to predict localized corrosion of process equipment including fabricated components as well as base alloys. For design and revamp purposes, the software predicts the occurrence of localized corrosion as a function of environment chemistry and assists the user in selecting the optimum alloy for a given environment. For the operation of existing plants, the software enables the users to predict the remaining life of equipment and help in scheduling maintenance activities. This project combined fundamental understanding of mechanisms of corrosion with focused experimental results to predict the corrosion of advanced, base or fabricated, alloys in real-world environments encountered in the chemical industry. At the heart of this approach is the development of models ...

2007-09-29

299

Carbon steel corrosion rates and mechanisms in aqueous nickel chloride at 300C  

International Nuclear Information System (INIS)

Rapid corrosion of PWR steam generator carbon steel support structures and consequential denting of steam generator tubes led to considerable investigation of the mechanism of corrosion and for palliatives. The basic mechanism is now fairly well understood. Chloride present in the boiler feedwater from condenser leakage is concentrated in the support plate crevice as a result of the superheat present. This leads to the formation of a low pH acid ferrous chloride environment either through the hydrolysis of a weak base chloride such as MgCl_2 or the combined action of a neutral chloride with an oxidizing agent. Rapid attack of the carbon steel ensues with the Fe_3O_4 corrosion product forming at the metal/oxide interface. This oxide has a volume approximately twice that of the steel consumed and thus eventually fills the crevice between the tube and the support plate. Oxide growth continues leading to compression of the ...

1985-03-01

300

Molybdenum Alloys Optimal Structure  

International Science & Technology Center (ISTC)

Determination of Special Molybdenum Alloys Optimal Structure Using the Cybernetic Method

302

Corrosion Protection of special steels and alloys  

International Science & Technology Center (ISTC)

Development of the Corrosion Protection Technology for Special Steels and Alloys

303

Pathway and Surface Mechanism Studies of 1,3-butadiene Selective Oxidation Over Vanadium-Molybdenum-Oxygen Catalysts  

Energy Technology Data Exchange (ETDEWEB)

The partial oxidation of 1,3-butadiene has been investigated over VMoO catalysts synthesized by sol-gel techniques. Surface areas were 9-14 m{sup 2}/g, and compositions were within the solid solution regime, i.e. below 15.0 mol % MoO{sub 3}/(MoO{sub 3} + V{sub 2}O{sub 5}). Laser Raman Spectroscopy and XRD data indicated that solid solutions were formed, and pre- and post-reaction XPS data indicated that catalyst surfaces contained some V{sup +4} and were further reduced in 1,3-butadiene oxidation. A reaction pathway for 1,3-butadiene partial oxidation to maleic anhydride was shown to involve intermediates such as 3,4-epoxy-1-butene, crotonaldehyde, furan, and 2-butene-1,4-dial. The addition of water to the reaction stream substantially increased catalyst activity and improved selectivity to crotonaldehyde and furan at specific reaction temperatures. At higher water addition concentrations, furan selectivity increased from 12% to over 25%. The catalytic effects of water addition were ...

2002-05-27

304

Wear and friction coefficient of particle reinforced Ti-alloys  

Energy Technology Data Exchange (ETDEWEB)

Particulate Reinforced Titanium matrix composites (PRTi) exhibit some improved specific mechanical properties in comparison with those of unreinforced titanium alloys as a result of the combination of the high strength and stiffness of ceramic particles with the toughness and damage tolerance provided by the metal matrix. The poor tribological properties of the titanium exclude titanium alloys from applications where wear resistance is required (brakes, rotating parts, sliding parts). The addition of ceramic particles improves the tribological properties of metals sensitive to adhesive and /or abrasive wear significantly. In this work, the wear resistance and the friction coefficient of Ti6Al-6V-2Sn reinforced with TiC particles and Ti6Al-4V reinforced with SiC particles (prototype material) are compared with the unreinforced alloys. Pin on disc and pin on ring tests were carried out against standard ...

2004-11-01

305

Spectrophotometric determination of vanadium(V) with 2-carbethoxy-5-hydroxy-1-(4-tolyl)-4-pyridone  

International Nuclear Information System (INIS)

Vanadium(V) in aqueous HCl, HNO_3 or H_2SO_4 solutions is extracted with 2-carbethoxy-5-hydroxy-1-(4-tolyl)-4-pyridone (HA) dissolved in CHCl_3 and determined spectrophotometrically, Depending on the composition of the aqueous phase, two complexes are formed. At pH 1 (HCl, HNO_3, H_2SO_4) VO_2A(HA)_2 is formed with maximal absorption at 478 nm. However, from 4-5 M HCl, VO_2Cl(HA)_3 is extracted, and has maximal absorption at 615 nm. The same complex is extracted from 2-3 M HNO_3 or 3-4 M H_2SO_4 if enough chloride is added. Solutions of both complexes follow Beer's law and the molar extinction coefficients are 4.15x10"3 1.mole"-"1cm"-"1 at 478 nm and 5.10x10"3 at 615 nm. The determination of vanadium at both wavelengths is very simple, fast and selective. The composition of the complexes was established by the usual methods as well as by characterization of the isolated crystalline compounds by elemental analysis and infrared spectroscopy. ...

1975-01-01

306

Preparation, characterization and properties of thermochromic tungsten-doped vanadium dioxide by thermal reduction and annealing  

International Nuclear Information System (INIS)

Thermochromic tungsten-doped vanadium dioxide (VO2) powders were successfully synthesized by thermal reduction using V2O5 as a vanadium precursor. The products were characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM) and differential scanning calorimetry (DSC). The results indicated that W was successfully doped into the crystal lattice of VO2 matrix, and prepared tungsten-doped VO2 had a rod-like morphology. The effects of reducing temperature and annealing temperature on the crystallographic structures were also discussed. The phase transition temperature (Tt) of VO2 could be simply tuned by changing the doping concentration of tungsten. When the doping concentration was 1.58 mol%, the Tt could be reduced to 37.8 oC from initial 69.5 oC, suggesting that tungsten-doped VO2 possesses prominent thermochromic properties and optical switching characters. It has shown that this ...

2010-08-20

307

Nonequilibrium statistical mechanics  

CERN Document Server

Nonequilibrium statistical mechanics

2001-01-01

308

Vanadium based amorphous mixed oxides used as negative electrodes of lithium batteries; Oxydes mixtes amorphes a base de vanadium comme electrodes negatives de batteries au lithium  

Energy Technology Data Exchange (ETDEWEB)

This paper presents recent results concerning the chemical and electrochemical synthesis, the electrochemical properties and the characterization of two new families of amorphous oxides of formula Li{sub x}MVO{sub 4} (1

1996-12-31

309

The effect of V and W addition on the high temperature strength properties of 12%Cr-15%Mn austenitic steels  

International Nuclear Information System (INIS)

The effect of W and V on the high temperature strength properties of 12%Cr-15%Mn austenitic steels was studied from the view point of precipitation hardening and internal stress. The contribution of W addition to the tensile and creep-rupture strength was not so large. By contrast the combined addition of W and V increased the strength considerably. These are resulted from the precipitation of fine vanadium nitride (VN) within grains and the enhancement of M_2_3C_6 type carbide precipitation at grain boundaries. The V added material had large internal stress value which is considered to be due to dislocation movement disturbed by fine vanadium nitrides. (author).

310

Occurrence of metals in petroleum and hydrocarbon products and methods for their determination  

Energy Technology Data Exchange (ETDEWEB)

Petroleum, known to be a source of a vast variety of organic compounds, is also a depository of valuable mineral components. Vanadium and nickel are the most important metal components of crude petroleum, with their concentrations reaching a few tenths of a percent. Their percentage increases 2- to 5-fold in the hydrocarbon products. The vanadium content in processed petroleum products is given. Therefore, the extraction of metals from petroleum is becoming an increasing important task. At present, there is no petroleum processing technology aimed solely at obtaining organic components. The occurrence of metals and other trace elements in petroleum and hydrocarbon products is discussed on the basis of available literature and experimental data. Techniques for isolating metals from petroleum and hydrocarbon products and their quantitative determination are considered.

1995-07-01

311

A new vanadium Schiff base complex as catalyst for oxidation of alcohols  

British Library Electronic Table of Contents (United Kingdom)

The monoanionic bidentate Schiff base, N-(phenolyl)-benzaldimine (HL), has been employed to synthesize a new vanadium(IV) complex of general composition [VO(L)2] (where L = O, N donor of Schiff base). The ligand and complex have been fully characterized by elemental analyses, molar conductance data, FT-IR, 1H- and 13C-NMR, and UV-Vis spectroscopies. Oxidation of alcohols to their corresponding aldehydes and ketones was conducted by this complex catalyst using Oxone as oxidant under biphasic reaction conditions (CH2Cl2/H2O) and tetra-n-butylammonium bromide as phase transfer agent under air at room temperature.

2010-01-01

312

A method for determining the origin of bitumoids  

Energy Technology Data Exchange (ETDEWEB)

The invention is associated with organic geochemistry and may be used in conducting geological exploration operations for oil and gas. The purpose of the invention is to increase the precision of the method for determining the genesis of bitumoids. This is achieved through determining the isotopic composition of nickel or vanadium and from the anomalously high values of the isotopic ratio of Ni-58 to Ni-62 or from the anomalously low values of the isotopic ratio of vanadium, a conclusion is drawn about the epigenetic nature of the bitumoids. The proposed method is characterized by greater resolution due to the fact that the values of the isotopic ratios for oil bearing and water bearing structures are essentially not superimposed. The proposed method exceeds the resolution of metal metering studies in conducting geological exploration for oil and gas by 2 to 3 times.

1983-01-01

313

Zn-Al alloy as a new anode-metal of a zinc-air battery  

Energy Technology Data Exchange (ETDEWEB)

Low operating power and short cycle life are 2 of the main draw-backs of zinc-air batteries, despite the fact that various attempts have been made to develop improved zinc (Zn) anodes. This study investigated the performance of a Zn anode with a substantial addition of aluminium (Al). Rolled sheets of Zn-Al alloys of varying amounts of Zn and Al were used to prepare the anodes. Results of the study showed that the cells had higher open circuit voltages (OCV) values as well as a higher specific anode capacity. It was observed that specific anode capacity increased with higher current loading. The Zn{sub 59}Al{sub 41} and Zn{sub 67}Al{sub 33} sheets showed the highest performance with high OCV values of between 1540 and 1560 mV, as well as the largest specific anode capacity of 750-800 mAh per g at a discharge current of 200 mA. The 2-phase structure of the Zn-Al sheets was considered to be useful in reducing anode-passivation, and increasing anode-utilization due to ...

2006-01-15

314

Selection study of self actuated shutdown system for a large scale FBR  

International Nuclear Information System (INIS)

The Self Actuated Shutdown System (SASS) is now under development for use in a large scale FBR, in order to establish the passive shutdown capability against the postulated ATWS events, i.e. ULOF, UTOP and ULOHS. The function of SASS makes use of the safety characteristics of a liquid metal cooled FBRs such as a large subcooling and low pressure system. The insertion of the control rods insertion is assured even in the most conservative seismic design condition by employing articulate rods and the SASS will be installed into the detaching mechanism employing a curie point the magnet alloy. ULOF analysis of the present FBR shows that coolant boiling inception is prevented if a control rod of the SASS is detached at the uppermost temperature of 680degC for the Curie point magnet, and after the reactor shutdown the coolant temperature is kept below 600degC by the pony motor flow. Therefore the SASS will establish passive shutdown capability ...

1995-04-23

315

Photoluminescence linewidths in metalorganic vapor phase epitaxially grown ordered and disordered InAlGaP alloys  

Science.gov (United States)

The dependence of the photoluminescent properties of In{sub 0.48}(Al{sub {ital y}}Ga{sub 1{minus}{ital y}}){sub 0.52}P alloys (0{le}{ital y}{le}0.5) on growth temperature and substrate misorientation off GaAs(100) has been studied. Samples were grown using low-pressure metalorganic vapor phase epitaxy. By studying the dependence of ordering behavior in InGaP as a function of substrate misorientation and growth temperature simultaneously, a very large range in low-temperature photoluminescence emission energy---135 meV---has been obtained. The photoluminescence linewidth exhibits a strong, continuous dependence on the extent of atomic ordering (the emission energy) in the alloys. The results indicate that inhomogeneity in the microstructure of the material (i.e., between ordered'' domains and the disordered'' matrix) is the dominant photoluminescence broadening mechanism. This ...

1992-12-01

316

Photoluminescence linewidths in metalorganic vapor phase epitaxially grown ordered and disordered InAlGaP alloys  

Energy Technology Data Exchange (ETDEWEB)

The dependence of the photoluminescent properties of In{sub 0.48}(Al{sub {ital y}}Ga{sub 1{minus}{ital y}}){sub 0.52}P alloys (0{le}{ital y}{le}0.5) on growth temperature and substrate misorientation off GaAs(100) has been studied. Samples were grown using low-pressure metalorganic vapor phase epitaxy. By studying the dependence of ordering behavior in InGaP as a function of substrate misorientation and growth temperature simultaneously, a very large range in low-temperature photoluminescence emission energy---135 meV---has been obtained. The photoluminescence linewidth exhibits a strong, continuous dependence on the extent of atomic ordering (the emission energy) in the alloys. The results indicate that inhomogeneity in the microstructure of the material (i.e., between ordered'' domains and the disordered'' matrix) is the dominant photoluminescence broadening mechanism. This ...

1992-12-01

317

Creep and fatigue of alloy 800 in helium  

International Nuclear Information System (INIS)

Proposals for use of Alloy 800 as a H.T.R. boiler material have prompted studies of its creep and high temperature fatigue properties in impure helium with comparative tests in air. In impure helium, as expected in a H.T.R., reactions of potential importance are selective oxidation (of chromium, aluminium and titanium) and possibly carburisation from carbon monoxide or methane. In air, general oxidation will occur, possibly accompanied by nitridation. The effects of these reactions will depend on specimen geometry and the nature of the deformation. Two important possibilities are: (i) that environment affects the structure and properties of a surface zone of material undegoing uniform deformation (this may modify creep rate and crack nucleation); and (ii) that environment affects behaviour of a small region (e.g. at the root of a notch or ahead of a crack) in a specimen undergoing non-uniform deformation (this will modify crack growth and hence rupture life or ...

318

Correlation between electrochemical properties and corrosion resistance of zirconium alloys  

International Nuclear Information System (INIS)

The electrochemical behavior of some zirconium alloys including Zry-2 with various #SIGMA#Ai from 2.5 x 10"-"2"0 to 1.2 x 10"-"1"7 (h), modified Zry-2 with iron contents of 0.15, 0.25, and 0.5%, and standard Zry-4 was studied by measuring anodic polarization curves in sulfuric acid solution. The results of these electrochemical tests were compared with those of steam autoclave tests. In Zry-2, the current peak was observed at 1250 mV (versus SCE) on the anodic polarization curve, and this peak area increased with #SIGMA#Ai and with the size of secondary precipitates. Also, this peak was closely correlated with nodular corrosion resistance as expected from the above results. As iron contents in modified Zry-2 increased, the current peak at 1,250 mV decreased and a new peak at 1,900 mV appeared. The former peak disappeared and the latter peak increased further at 0.5% iron. In Zry-4, the current peak was observed at 1,900 mV, but not at 1,250 mV, and this behavior ...

1995-09-11

319

A Flow Stress Formulation of Magnesium Alloy at Elevated Temperature  

International Nuclear Information System (INIS)

Dynamic recrystallization (DRX) is the main softening mechanism of magnesium alloy AZ31B in hot deformation. Theoretically, in the flow rule the atomic diffusibility and the driving force of dislocation migration are dependent on the temperature, and the dislocation density and the cumulation of grain boundary energy are dependent on the strain rate. The peak stress will appear when the flow driving force and resistance force reach a balance, after which the stress descending will take place due to recrystallization fraction. Since the DRX is a thermally activated process, the recrystallized volume fraction can be regarded as the function of strain through Avrami equation. Based on this idea, the paper proposes a new constitutive model characterizing dynamic recrystallization for magnesium alloy AZ31B. The model is described by a peak stress and a strain softening rate, in which the peak stress depends only on ...

2007-05-17

320

Processing of A-15 Nb_3Si, Nb_3Ge and Nb_3(AlSi) superconducting ribbons by the chill-block spinning machine  

International Nuclear Information System (INIS)

A processing technique for A-15 compounds which has improved mechanical and superconducting properties has been developed. This technique consists of rapid solidification of the alloy by the chill block spinning machine (CBSM) to form amorphous ribbons and by subsequent annealing crystallizes the stable or metastable fine grain flexible A-15 structure. The CBSM has been modified so that all the processing parameters could be controlled and optimized for each alloy composition. By the improved CBSM it was possible to form amorphous Nb_3Si, Nb_3Ge and Nb_3(AlSi) ribbons with more than 80% reproducible rate. Critical current density measurements are limited by contact resistance. A Cu plating technique was introduced in this research that made the contact resistance three orders of magnitude lower than that obtained by other methods. This plated coating also gave an additional mechanical support to the ...

321

Processing of A-15 Nb sub 3 Si, Nb sub 3 Ge and Nb sub 3 (AlSi) superconducting ribbons by the chill-block spinning machine  

Energy Technology Data Exchange (ETDEWEB)

A processing technique for A-15 compounds which has improved mechanical and superconducting properties has been developed. This technique consists of rapid solidification of the alloy by the chill block spinning machine (CBSM) to form amorphous ribbons and by subsequent annealing crystallizes the stable or metastable fine grain flexible A-15 structure. The CBSM has been modified so that all the processing parameters could be controlled and optimized for each alloy composition. By the improved CBSM it was possible to form amorphous Nb{sub 3}Si, Nb{sub 3}Ge and Nb{sub 3}(AlSi) ribbons with more than 80% reproducible rate. Critical current density measurements are limited by contact resistance. A Cu plating technique was introduced in this research that made the contact resistance three orders of magnitude lower than that obtained by other methods. This plated coating also gave an additional mechanical ...

1989-01-01

322

Phase transformation and mechanical properties of the Ti_5_0Zr_3_0Nb_1_0Ta_1_0 alloy with low modulus and biocompatible  

International Nuclear Information System (INIS)

The beta transformation characteristics and mechanical properties of the #beta# titanium alloy Ti_5_0Zr_3_0Nb_1_0Ta_1_0 in the temperature range between 200 and 900 deg. C have been studied by means of X-ray diffraction (XRD), Vickers hardness (HV), and tensile test techniques. In the as-rolled state, only #beta#-phase was identified by XRD. Upon heat-treating at 250 deg. C for 4 h, the #alpha#-phase was precipitated from the #beta#-phase matrix, and leading to an increase of Vickers hardness. A maximum HV value was observed at 400 deg. C, and then HV value decreased with increasing heat-treating temperature. Above 650 deg. C, HV value remained almost constant. During heat-treating at 300-650 deg. C, the decomposition of the metastable #beta#-phase has been found to proceed through a phase separation reaction leading to the formation of #beta#-Ti and #beta#-Zr b.c.c. solid solution phases rather than the formation of solute rich and solute lean ...

2005-04-19

323

New Forming Limits For Light Alloys By Means Of Electromagnetic Forming And Numerical Simulation Of The Process  

Science.gov (United States)

It is well known that one of the main advantages of the high speed forming (HSF) processes is the improvement in the forming limits of the used materials.Using the Electromagnetic Forming (EMF) technology two materials have been tested with different mechanical and physical properties: the AA5754 aluminium and the AZ31B magnesium alloys.The EMF process principle can be described as follows: A significant amount of electrical energy is stored in a bank of capacitors which are suddenly discharged releasing all the stored energy. This electric discharge runs through a coil which generates an intense transient magnetic field. At the same time transient Eddy currents are induced in the electrically conductive part placed some millimetres far from the coil. Another intense magnetic field is generated due to those Eddy currents but on the opposite direction as the one generated by the coil. A big magnetic repulsion force is created between the part ...

2007-04-07

324

New Forming Limits For Light Alloys By Means Of Electromagnetic Forming And Numerical Simulation Of The Process  

International Nuclear Information System (INIS)

It is well known that one of the main advantages of the high speed forming (HSF) processes is the improvement in the forming limits of the used materials.Using the Electromagnetic Forming (EMF) technology two materials have been tested with different mechanical and physical properties: the AA5754 aluminium and the AZ31B magnesium alloys.The EMF process principle can be described as follows: A significant amount of electrical energy is stored in a bank of capacitors which are suddenly discharged releasing all the stored energy. This electric discharge runs through a coil which generates an intense transient magnetic field. At the same time transient Eddy currents are induced in the electrically conductive part placed some millimetres far from the coil. Another intense magnetic field is generated due to those Eddy currents but on the opposite direction as the one generated by the coil. A big magnetic repulsion force is created between the part ...

2007-04-07

325

On the Potential for Vacancy Annihilation as a Mechanism for Conditioning in Pu-1.9 at.% Ga  

Energy Technology Data Exchange (ETDEWEB)

The {delta} {yields} {alpha}{prime} martensitic transformation in Pu-1.9 at.% Ga occurs when the alloy is cooled below about -100 C. This transformation exhibits anomalous behavior, where the isothermal transformation proceeds atypically with double-C kinetics. Recent work has revealed that an ambient temperature isothermal hold (referred to as conditioning) prior to the transformation has different effects depending on whether transformation proceeds in the upper- or lower-C of the double-C: the amount of transformation is increased with conditioning in the upper-C, while the transformation in the lower-C seems to be engendered by conditioning. The mechanism by which conditioning affects the low-temperature {delta} {yields} {alpha}{prime} transformation is thus of great importance to understanding the transformation itself as well as the general circumstances that can affect a martensitic phase transformation. Using differential scanning ...

2009-03-09

326

Mechanical properties of Fe -10Ni -7Mn martensitic steel subjected to severe plastic deformation via cold rolling and wire drawing  

Energy Technology Data Exchange (ETDEWEB)

Fe-Ni-Mn martensitic steels are one of the major groups of ultra-high strength steels that have good mechanical properties and ductility in as annealed condition but they suffer from severe inter-granular embitterment after aging. In this paper, the effect of heavy shaped cold rolling and wire drawing on the mechanical properties of Fe-Ni-Mn steel was investigated. This process could provide a large strain deformation in this alloy. The total strain was {epsilon} {approx}7. Aging behavior and tensile properties of Fe-10Ni-7Mn were studied after aging at 753 K. The results showed that the ultimate tensile strength and ductility after cold rolling, wire drawing and aging increased up to 2540 MPa and 7.1 %, respectively, while the conventional steels show a premature fracture stress of 830 MPa with about zero ductility after aging.

2010-07-01

327

Mechanical properties of Fe -10Ni -7Mn martensitic steel subjected to severe plastic deformation via cold rolling and wire drawing  

International Nuclear Information System (INIS)

Fe-Ni-Mn martensitic steels are one of the major groups of ultra-high strength steels that have good mechanical properties and ductility in as annealed condition but they suffer from severe inter-granular embitterment after aging. In this paper, the effect of heavy shaped cold rolling and wire drawing on the mechanical properties of Fe-Ni-Mn steel was investigated. This process could provide a large strain deformation in this alloy. The total strain was #epsilon# #approx#7. Aging behavior and tensile properties of Fe-10Ni-7Mn were studied after aging at 753 K. The results showed that the ultimate tensile strength and ductility after cold rolling, wire drawing and aging increased up to 2540 MPa and 7.1 %, respectively, while the conventional steels show a premature fracture stress of 830 MPa with about zero ductility after aging.

2010-07-01

329

New Powder Technologies for Molybdenum Alloy Gun Barrel ...  

Science.gov (United States)

... MOLYBDENUM ALLOY GUN BARREL LINERS o0 in ... NEW POWDER TECHNOLOGIES FOR MOLYBDENUM ALLOY GUN BARREL LINERS ...

1985-06-01

331
332

Autocatalytic nucleation of omega phase in a beta-titanium alloy  

International Nuclear Information System (INIS)

Observations concerned with the formation of isothermal #omega# in the beta-titanium alloy RMI (38-6-44) are presented as part of a more general study of the aging characteristics of the alloy.

333

Radioisotope space power generator annual report for the period October 1, 1976-September 30, 1978  

Energy Technology Data Exchange (ETDEWEB)

Techniques for fabricating P-type (Cu,Ag)/sub 2/Se with mesh-type bonds have been developed and are being evaluated for long-term use. In addition, methods for reducing vapor suppression by the use of coatings and/or baffling continue to show gains. The N-type alloy Gd/sub 2/Se/sub 3/ has been shown to be thermally unstable. It undergoes a sluggish cubic-to-orthorhombic phase change below 1000/sup 0/C, with an accompanying degradation in mechanical and thermoelectric properties. Fabrication studies conducted with the (Bi,Sb)/sub 2/(Se,Te)/sub 3/ alloys showed these materials to be sensitive to oxygen contamination if reproducible properties are to be obtained. Preparation of powdered material by explosive techniques was investigated. This technique appears to be useful in preparing homogeneous -325 mesh material, but it does not yield a useful amount of submicron-size powder.

1980-01-01

334

Progress on fatigue characterization of ITER primary first wall mock-ups  

International Nuclear Information System (INIS)

In 2001, EFDA has assigned to ENEA a contract for the thermomechanical testing of six mock-ups of the ITER primary wall module. These small scale mock-ups, reproducing representative portions of the reference ITER primary wall panels, were fabricated during ITER EDA phase by solid hot isostatic pressing (HIPping) of an AISI 316L stainless steel back structure to a alumina dispersion strengthened (DS)-Cu alloy heat sink armored with beryllium tiles. The experimental program, carried-out at ENEA Brasimone CEF 1-2 thermal hydraulic facility, was focused on the thermal mechanical testing of these mock-ups aiming at verifying which tile geometry and manufacturing procedure assures the required reliability of the beryllium/DS-Cu alloy/SS joints at high incident heat flux (>0.8 MW/m"2) both at steady state and under thermal fatigue tests. The paper presents the progress in the experimental activity of the first test campaign ...

2003-09-01

335

PVD-CrN coated magnesium alloy AZ91hp and steel 100Cr6 - investigation on the influence of the substrate material on coating properties; PVD-CrN Beschichtungen auf Magnesium AZ91hp und Stahl 100Cr6 - Untersuchung des Substrateinflusses auf die Schichteigenschaften  

Energy Technology Data Exchange (ETDEWEB)

PVD-chromium-nitride coated samples of substrates of the magnesium alloy AZ91hp and the roller and ball bearing steel 100Cr6 were investigated regarding structure, mechanical characteristics, adhesion and internal stresses. For the coatings the parameters layer thickness and substrate BIAS voltage were varied. Both substrate materials were coated in one lad. Results of the X-ray analysis of the internal stresses show significant differences between the coated magnesium and the coated steel substrates. In the case of the variation of the substrate BIAS voltage, for the coated steel a dependency of the internal stresses to coating parameters could be obtained. For the coated magnesium no dependency was recognizable. The coating structure was examined with scanning electron microscopy. Element depth profiles of the coated samples were performed with SIMS. (orig.)

2001-03-01

336

Microstructural evolution of WC-Co alloys  

Energy Technology Data Exchange (ETDEWEB)

The microstructural development and grain-coarsening behavior of WC-Co alloys, with and without a VC additive, were investigated. The primary goal was to determine the mechanism through which VC acts as a grain-growth inhibitor. The study involved long-time sintering experiments (1 to 100 hours) on fully dense material, nascent stage sintering (90 to 1,320 seconds) starting with the green compact, and surrogate liquid phase experiments to characterize the WC powder prior to sintering. Quantitative microstructural analysis using intercept length distributions was performed for the long-term sintering. The nascent stage experiments involved the measurement of the specific surface area (S{sub v}) of each type of interface separately allowing the determination of the contribution of each developing entity to the overall microstructural evolution. The VC addition has been found to enhance the breakup of multigrained particles in the earliest stages ...

1991-01-01

337

Microstructural evolution of WC-Co alloys  

International Nuclear Information System (INIS)

The microstructural development and grain-coarsening behavior of WC-Co alloys, with and without a VC additive, were investigated. The primary goal was to determine the mechanism through which VC acts as a grain-growth inhibitor. The study involved long-time sintering experiments (1 to 100 hours) on fully dense material, nascent stage sintering (90 to 1,320 seconds) starting with the green compact, and surrogate liquid phase experiments to characterize the WC powder prior to sintering. Quantitative microstructural analysis using intercept length distributions was performed for the long-term sintering. The nascent stage experiments involved the measurement of the specific surface area (S_v) of each type of interface separately allowing the determination of the contribution of each developing entity to the overall microstructural evolution. The VC addition has been found to enhance the breakup of multigrained particles in the earliest stages of ...

338

Microstructural development inside the stress induced martensite variant in a Ti-Ni-Nb shape memory alloy  

Energy Technology Data Exchange (ETDEWEB)

The microstructural development inside the stress induced martensite (SIM) variants in Ti-Ni-Nb alloy with various degrees of deformation have been revealed by electron microscopic observations. The orientation relationship between the SIM and the parent phase has been found: [1{bar 1}0]{sub M}{parallel}[11{bar 1}]{sub B2}, (001){sub M} 5{degree} away from (101){sub B2}. The lattice invariant shear of the SIM variants at the slightly deformed stage is dominantly (11{bar 1}) Type I twin. Besides the ordinary slip, the adjustment and development of the internal secondary twinning from (11{bar 1}) Type I twin to {l_angle}011{r_angle} Type II/ or (011) Type I twin, (001)compound twin and (111) Type I twin happen concurrently or in combination inside the SIM variants with the further deformation. The corresponding deformation mechanisms include stress induced reorientation of SIM substructural bands by the most favorably oriented twin system, stress ...

2000-04-03

339

Localized deformation and IASCC initiation in austenitic stainless steels  

International Nuclear Information System (INIS)

Localized deformation may play a key role in the underlying mechanism of irradiation assisted stress corrosion cracking (IASCC) in light water reactor core components. In this study, four austenitic alloys, 18Cr8Ni, 15Cr12Ni, 13Cr15Ni and 21Cr32Ni, with different stacking fault energies were irradiated to 1 and 5 dpa at 360 deg. C using 3.2 MeV protons. Interrupted constant extension rate tensile (CERT) tests were conducted in a simulated BWR environment to determine IASCC susceptibility. In order to characterize the localized deformation in slip channels and grain boundaries, parallel CERT experiments were also performed in an argon atmosphere. Results show that the IASCC susceptibility of the tested alloys increases with increasing irradiation dose and decreasing stacking fault energy. IASCC tends to initiate at locations where slip channels intersect grain boundaries. Localized deformation in the form of grain boundary ...

2008-12-01

340

Iron Aluminide Hot Gas Filters  

Energy Technology Data Exchange (ETDEWEB)

Currently, high temperature filter systems are in the demonstration phase with the first commercial scale hot filter systems being installed on integrated gasification combined cycle (IGCC) and pressurized fluid bed combustion cycle (PBFC) systems (70 MW). They are dependent on the development of durable and economic high temperature filter systems. These filters are mostly ceramic tubes or candles. Ceramic filter durability has not been high. Failure is usually attributed to mechanical or thermal shock: they can also undergo significant changes due to service conditions. The overall objective of this project is to commercialize weldable, crack resistant filters which will provide several years service in advanced power processes. The specific objectives of this project are to develop corrosion resistant alloys and manufacturing processes to make Iron Aluminide filter media, and to use a ``short term`` exposure apparatus supported by other ...

1996-12-31

341

Effect of mean stress (stress ratio) and aging on fatigue-crack growth in a metastable beta titanium alloy, Ti-10V-2Fe-3Al  

International Nuclear Information System (INIS)

The effect of mean stress, or the stress ratio (R), on the fatigue-crack growth (FCG) behavior of #alpha#-aged and #omega#-aged microstructures of the beta titanium alloy Ti-10V-2Fe-3Al was investigated. While the mean stress had a negligible effect on the FCG behavior of the #alpha#-aged microstructure, a strong effect was observed in the #omega#-aged microstructure. In particular, the values of the threshold stress-intensity range (#DELTA#K_t_h) exhibited a strong dependence on R in the #omega#-aged microstructure, while this dependence was weak in the #alpha#-aged microstructure. These effects seem to arise primarily from fracture-surface roughness-induced crack closure. The crack closure levels for the #alpha#-aged microstructure were found to be very low compared to those for the #omega#-aged microstructure. Transmission electron microscopy and scanning electron microscopy studies of microstructures and fracture surfaces were performed to gain insight into the ...

2000-03-01

342

Effect of VC and NbC additions on microstructure and properties of ultrafine WC-10Co cemented carbides  

British Library Electronic Table of Contents (United Kingdom)

The nanocomposite WC-Co powders were prepared through planetary ball milling method. Effects of grain growth inhibitor addition and the vacuum sintering parameters on the microstructure and properties of ultrafine WC-10Co cemented carbides were investigated using X-ray diffractometer, scanning electron microscope and mechanical property tester. The results show that VC and NbC additions can refine the WC grains, decrease the volume fraction of Co3W3C phase in ultrafine WC-10Co cemented carbides, and increase the hardness and fracture toughness of the base alloys. After sintering for 60 min at 1400 degreeC, the average grain size and hardness of ultrafine-grained WC-10Co-1VC cemented carbide are 470 nm and HRA 91.5, respectively. The fracture toughness of cemented carbide WC-10Co-1NbC alloy...

2009-01-01

343

Cracking of Alloy 800 tubing in superheated steam in a solar receiver  

Energy Technology Data Exchange (ETDEWEB)

The solar central receiver at the Barstow Pilot Plant is a once-through steam boiler consisting of vertical arrays of Alloy 800 tubes. Water/steam leaks associated with tube bends near the receiver outlet were observed after 16 service months. The leaks resulted from through-wall cracks localized in the crown of tube bends operating in the temperature range from 550 to 650/sup 0/C. Initiation occurred on the ID (steam side) of the tube and propagated transgranular through the tube wall. Cracking was axial and circumferential; in general, the circumferential cracks were more severe than the axial cracks. Thick oxide layers showed on the ID of the receiver tubes; a 25-..mu..m thick oxide layer had formed on tubing which operated at 650/sup 0/C. In addition, an enhanced oxidation layer was observed along a narrow band in the crown of the tube. This band was up to five times thicker than the oxide elsewhere in the tube. All cracking was associated with this enhanced ...

1985-10-01

344

Characteristics of deep penetration laser welding of dissimilar metal Ni-based cast superalloy K418 and alloy steel 42CrMo  

Science.gov (United States)

Experimental trials of autogenous deep penetration welding between dissimilar cast Ni-based superalloy K418 and alloy steel 42CrMo flat plates with 5.0 mm thickness were conducted using a 3 kW continuous wave (CW) Nd:YAG laser. The influences of laser output power, welding velocity and defocusing distance on the morphology, welding depth and width as well as quality of the welded seam were investigated. Results show that full keyhole welding is not formed on both K418 and 42CrMo side, simultaneously, due to the relatively low output power. Partial fusion is observed on the welded seam near 42CrMo side because of the large disparity of thermal physical and high-temperature mechanical properties of these two materials. The microhardness of the laser-welded joint was also examined and analyzed. It is suggested that applying negative defocusing in the range of Raylei length can increase the welding depth and improve the coupling efficiency of the ...

2007-09-01

345

Anisotropy of tensile properties of extruded magnesium alloy AZ31  

Energy Technology Data Exchange (ETDEWEB)

The mechanical behaviour of wrought magnesium alloy AZ31 has been characterised by tensile testing at room temperature. Tests were carried out at various strain rates between 0.00003 s{sup -1} and 0.01 s{sup -1} on material which had been extruded to a bar of approximately 6 mm thick, and 80 mm wide. Specimens were machined from three orientations relative to the extrusion direction: parallel, perpendicular, and 45 from the extrusion direction. Significant variations of the properties were observed depending on the extrusion orientation and strain rate. At all strain rates the yield stress declined as the test orientation was rotated away from the extrusion direction. Parallel to the extrusion direction, the yield stress was found to increases markedly with increasing strain rate, whereas at 45 and 90 a lesser influence of strain rate was observed. The work hardening exponent was also influenced by the test orientation. Metallographic studies ...

2003-07-01

346

Research on laser welding of cast Ni-based superalloy K418 turbo disk and alloy steel 42CrMo shaft  

Energy Technology Data Exchange (ETDEWEB)

Exploratory experiments of laser welding cast Ni-based superalloy K418 turbo disk and alloy steel 42CrMo shaft were conducted. Microstructure of the welded seam was characterized by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), energy-dispersive spectrometer (EDS). Mechanical properties of the welded seam were evaluated by microhardness and tensile strength testing. The corresponding mechanisms were discussed in detail. Results showed that the laser-welded seam had non-equilibrium solidified microstructures consisting of FeCr{sub 0.29}Ni{sub 0.16}C{sub 0.06} austenite solid solution dendrites as the dominant and some fine and dispersed Ni{sub 3}Al {gamma}' phase and Laves particles as well as little amount of MC short stick or particle-like carbides distributed in the interdendritic regions. The average microhardness of the welded seam was relatively uniform and lower than ...

2008-04-03

347

Research on laser welding of cast Ni-based superalloy K418 turbo disk and alloy steel 42CrMo shaft  

International Nuclear Information System (INIS)

Exploratory experiments of laser welding cast Ni-based superalloy K418 turbo disk and alloy steel 42CrMo shaft were conducted. Microstructure of the welded seam was characterized by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), energy-dispersive spectrometer (EDS). Mechanical properties of the welded seam were evaluated by microhardness and tensile strength testing. The corresponding mechanisms were discussed in detail. Results showed that the laser-welded seam had non-equilibrium solidified microstructures consisting of FeCr_0_._2_9Ni_0_._1_6C_0_._0_6 austenite solid solution dendrites as the dominant and some fine and dispersed Ni_3Al #gamma#' phase and Laves particles as well as little amount of MC short stick or particle-like carbides distributed in the interdendritic regions. The average microhardness of the welded seam was relatively uniform and lower than that of the base metal ...

2008-04-03

348

High temperature oxidation of metals: vacancy injection and consequences on the mechanical properties; Consequences de l'oxydation haute temperature sur l'injection de defauts et le comportement mecanique des materiaux metalliques  

Energy Technology Data Exchange (ETDEWEB)

The aim of this work is to account for the effects of the high temperature oxidation of metals on their microstructure and their mechanical properties. 'Model' materials like pure nickel, pure iron and the Ni-20Cr alloy are studied. Nickel foils have been oxidised at 1000 C on one side only in laboratory air, the other side being protected from oxidation by a reducing atmosphere. After the oxidation treatment, the unoxidized face was carefully examined by using an Atomic Force Microscope (AFM). Grain boundaries grooves were characterised and their depth were compared to the ones obtained on the same sample heat treated in the reducing atmosphere during the same time. They are found to be much deeper in the case of the single side oxidised samples. It is shown that this additional grooving is directly linked to the growth of the oxide scale on the opposite side and that it can be explained by the diffusion of the vacancies ...

2004-11-15

349

Effects of irradiation on the microstructural evolution and corrosion resistance of zirconium alloys  

International Nuclear Information System (INIS)

Zircaloy-2 and Zircaloy-4 tubing materials were irradiated with 1 MeV proton at 350 degrees C to doses of 0.01, 0.1, and 1 dpa respectively. Both microstructure examination and nodular corrosion test (500 degrees C, 1500 psi steam) were performed in order to understand the relationship between the microstructural evolution and the corrosion resistance of these alloys under irradiation. Neutron-irradiated Zircaloy-2 specimens which were obtained from a failed BWR fuel rod cladding were also studied. Specimens of three different neutron fluences were investigated; namely, 2.6x10"2"4, 3.2x10"2"5, 3.8x10"2"5, (E_n#>=#1MeV). The results indicated that the higher the irradiation dose the better the nodular corrosion resistance of both Zircaloy-2 and Zircaloy-4. It is concluded that irradiation-induced precipitate dissolution and irradiation-enhanced diffusion may increase the solute concentration in the matrix and make it distributed more evenly which in turn ...

1991-08-25

350

Creep-microcrack growth in alloy 800 HT at elevated temperatures  

Energy Technology Data Exchange (ETDEWEB)

The aim of the presented investigation was to gain information about the behaviour of the initiation and growth of intercrystalline creep cracks during creep deformation from the evaluation of metallographic micrographs. The austenitic steel X10 NiCrAlTi 32 20 HT (Alloy 800 HT) was investigated by carrying out creep tests at 800 and 900 C with different nominal stresses until fracture. Additional tests are carried out on certain creep strains in the late tertiary creep stage. The creep tests are followed by a metallographic investigation of the crept specimens. The statistical distribution of the microcrack lengths was used to estimate the rate of crack initiation and crack growth. It is found that the rate of growth of the intercrystalline creep cracks in Alloy 800 HT is dependent on the applied stress and the creep strain reached. The rate of growth of long cracks was only slightly higher than that of short cracks and was lower than ...

1997-05-01

351

The separation and determination of trace elements in iron ore  

International Nuclear Information System (INIS)

The separation, concentration, and determination of trace elements in iron ores are described. After the sample has been dissolved, the iron is separated by liquid-liquid extraction with a liquid cation-exchanger, di-(2-ethylhexyl) phosphoric acid. The trace elements aluminium, cadmium, calcium, chromium, cobalt, copper, lead, magnesium, manganese, mercury, potassium, sodium, vanadium, and zinc are determined in the aqueous phase by atomic-absorption spectrophotometry.

2008-05-01

352

Kinetics of low-temperature radiation hardening of metallic materials under irradiation  

British Library Electronic Table of Contents (United Kingdom)

A formula is obtained which describes the kinetics of low-temperature radiation hardening caused by creation of dislocation loops of interstitial type during irradiation. The radiation hardening of aluminum and vanadium is estimated using this formula and results of experiments on studying processes of nucleation and growth of interstitial dislocation loops in these materials by transparent electron microscopy. It is shown that the proposed formula is valid for description of the kinetics of low-temperature radiation hardening.

2011-01-01

353

Josephson junctions as heterodyne detectors  

International Nuclear Information System (INIS)

Heterodyne detection with a point-contact Josephson junction has been investigated both experimentally and theoretically. The measured performance of the device at 36 GHz is in good agreement with the theory. By operating vanadium point contacts at 1.4 K, the authors have achieved a single-sideband (SSB) mixer noise temperature of 54 K with a conversion gain of 1.35 and a signal bandwidth on the order of 1 GHz. A potentially impressive performance for these devices at submillimeter wavelengths can be extrapolated from the results.

354

Cold fusion method  

International Nuclear Information System (INIS)

In a cold fusion method by electrolysis, a hydrogen occluding material mainly comprising vanadium is used as a material for a negative electrode, and lithium isotopes are incorporated in the material by more than 93%. That is, the ratio of lithium 7 ("7Li) isotope is increased to higher than the natural existent ratio, so that tritium ("3H) concentration in the hydrogen occluding material can be increased, to attain energy at high efficiency. (T.M.).

1993-03-02

355

Accelerated aging tests with a resid hydrotreating catalyst  

International Nuclear Information System (INIS)

The author discusses the accelerated aging tests performed using Hondo and Maya as aging resids with a commercial large pore hydrotreating catalyst. The results from these tests were compared with those obtained under a normal full life test. The test resid was a sample of a typical refinery charge and the activities for sulfur and vanadium removal were determined at 720"0F after successive brief periods of exposure to the heavier oils.

1988-12-02

356

The effects of alloying elements and dilution on the hot cracking sensitivity of welds in alloy 800  

International Nuclear Information System (INIS)

Results of hot cracking on welds with compositions between alloy 800 and AWS ER NiCr 3. Investigation of the influence of Si, Mn, Ti and Al on the hot cracking suscpetibility of the alloy 800. (orig.).

359

Metals and alloys : atmospheric corrosion testing : General requirements for field tests  

CERN Document Server

Metals and alloys : atmospheric corrosion testing : General requirements for field tests

1992-01-01

361

Effect of Yttrium on the Microstructure of Titanium Alloys,  

Science.gov (United States)

... Title : Effect of Yttrium on the Microstructure of Titanium Alloys,. ... The yttrium was added in the melting stage as an oxide or in the elemental form. ...

362

Ductile aluminide alloys for high temperature applications  

Energy Technology Data Exchange (ETDEWEB)

Alloys are described which contain nickel, aluminum, boron, iron and in some instances manganese, niobium and titanium.

1987-01-01

363

Corrosion and stress corrosion cracking of alloy 800 in water and steam at elevated temperatures  

International Nuclear Information System (INIS)

The importance that must be attached to the phenomenon of stress corrosion cracking of austenitic alloys is emphasized. The relation between chemical composition of various alloys and their sensitivity to cracking is shown with particular reference to the behaviour of Alloy 800. The different effects of alkaline anc chloride environments are discussed. Studies are reported of the general corrosion of Alloy 800 and other alloys in an environment representative of the primary coolant of PWR reactors; and of the behaviour of various alloys (including Alloy 800) in the conditions envisaged for their use for steam generators with superheat up to about 550 deg.C. (U.K.).

364

The rapid nitriding of Al alloys with the controlling of plasma power density and pretreatments  

Energy Technology Data Exchange (ETDEWEB)

The properties of AlN make this material very attractive for optical, electronic, and tribological application. Also, if the AlN could be formed on the Al surface to enhance its surface properties, Al could be applied for the lightening of machine parts. However, a dense oxide film exists on the surface of Al, which prevents the formation of the Al nitride even during plasma nitriding and plasma coating process. In this study, plasma nitriding has been tried to form an AlN layer on Al after the surface activation processes. During the plasma nitriding, the density of the nitrogen ions was amplified by means of controlling the power of the Al substrates. The film thickness, microstructural features and the mechanical properties such as hardness and wear properties of the AlN layer were examined as a function of the process parameters of pretreatment and plasma nitriding

2010-05-15

365

SiGeC materials  

Energy Technology Data Exchange (ETDEWEB)

The growth and properties of Si{sub 1{minus}y}C{sub y} and Si{sub 1{minus}x{minus}y}Ge{sub x}C{sub y} alloys pseudomorphically strained on Si(001) will be reviewed. Although the bulk solubility of carbon in silicon is small, epitaxial layers with more than 1 at.% C can be fabricated. The relation between substitutional and interstitial carbon incorporation will be presented. Substitutionally incorporated C atoms allow strain manipulation, including the growth of strain-free or inversely strained Si{sub 1{minus}x{minus}y}Ge{sub x}C{sub y} layers. The mechanical properties, microscopic structure, thermal stability, as well as the influence of C atoms on band structure will be discussed.

1996-12-31

366

Point defects in dilute nitride III-N-As and III-N-P  

International Nuclear Information System (INIS)

We provide a brief review of our recent results from optically detected magnetic resonance studies of grown-in non-radiative defects in two most important dilute nitride systems-Ga(In)NAs grown on GaAs substrates and Ga(Al,In)NP grown on Si and GaP substrates. These results have led to the identification of defect complexes in the alloys, involving intrinsic defects such as As_G_a antisites and Ga_i self-interstitials. They have also shed light on formation mechanisms of the defects and on their role in non-radiative carrier recombination that is harmful to the performance of potential optoelectronic and photonic devices based on these dilute nitrides.

2006-04-01

367

Plasma nitriding of Fe-18Cr-9Ni in the range of 723-823 K  

Energy Technology Data Exchange (ETDEWEB)

To clarify the mechanism of plasma nitriding, the authors examined the optical microstructure, the hardness, the precipitation, and the concentration of dissolved nitrogen in Fe-18Cr-9Ni nitrided using plasma in the range of 723-823 K. Compared with ammonia-gas nitriding, the features of plasma nitriding are the formation of small chromium-nitride precipitates (CrN), the absence of an externally nitrided layer, the high concentration of dissolved nitrogen, and the high hardness (HV = 1,200). The diffusion coefficient of nitrogen in the present alloy was determined using the growth rate of the internally nitrided layer, based on calculations used in internal oxidation. Plasma- and gas-nitriding were also compared with respect to the growth rate of the nitrided layer.

1991-08-01

368

On the mechanism of the anodic protection of aluminium alloy AA5182 by emeraldine base coatings  

Energy Technology Data Exchange (ETDEWEB)

Aluminium AA5182 coupons covered by a polyaniline film in the emeraldine base (EB) form showed increasing corrosion potential and decreasing corrosion current as a function of the thickness of the polymer layer. The cathodic reaction was proved not limited by diffusion of species inside the electrolyte solution and oxygen had no effect on the electrochemical behaviour of the coated samples. An EB coating on indium tin oxide conducting layer appeared slightly electroactive in neutral media. The IR spectra of aluminium coated samples, before and after heating in argon atmosphere, confirmed a redox reaction between the polymer film and the metal. This galvanic coupling can explain the good protective behaviour of emeraldine base against corrosion of aluminium.

2007-03-01

369

Nanostructured Nb2O5-natural hydroxyapatite formed by the mechanical alloying method: A bulk composite  

British Library Electronic Table of Contents (United Kingdom)

The aim of this study was to develop a nanostructured Nb2O5-natural hydroxyapatite bulk composite to serve as an alternative biocompatible bulk material for implants. A set of samples of hydroxyapatite from fish bones with different concentrations of Nb2O5 were designed. They were prepared through a milling process, compacted under different pressures (350, 450, 550 and 650MPa) and sintered in air atmosphere at 1000^oC for 1h. The results revealed that the prepared composites presented strong interactions between the two elements and showed improvement in the sinterability with significant densification and microstructure changes, suggesting that they are promising for implants meant to replace bone tissues.

2011-01-01

370

Ion nitriding; Proceedings of the International Conference, Cleveland, OH, Sept. 15-17, 1986  

Energy Technology Data Exchange (ETDEWEB)

The present conference discusses plasma-assisted surface coating/modification processes, the applications to date of ion nitriding, the effects of nitrogen on metal surfaces, ion nitriding mechanisms in Cr, Al and Cr + Al-containing 1040 steel, ion nitriding of Al and its alloys, life enhancement for forging dies, novel anode plasma nitriding developments, and a comparative study of the pulsed and dc ion-nitriding behavior in specimens with blind holes. Also discussed are the influence of heating method on ion nitriding, surface hardening of marage steels by ion nitriding without core hardness reduction, plasma nitriding of nodular cast iron sput gears, NbN composites for superconductors, the carburization of tungsten in a glow discharge methane plasma, economic considerations concerning plasma nitriding, and the corrosion properties obtained by ion nitriding.

1987-01-01

371

Interface-induced conversion of infrared to visible light at semiconductor interfaces  

International Nuclear Information System (INIS)

Efficient, low-temperature conversion of infrared light into visible light (red, orange, green) is reported at single heterojunctions and undoped quantum wells of GaAs and ordered Al_xGa_1_-_xInP_2; an increase in photon energy of 700 meV is obtained. The signal originates from the high-band-gap layers and disappears only if the excitation energy is tuned below the GaAs band gap. The intensity of the up-converted photoluminescence (PL) is found to decrease significantly slower with increasing temperature than that of the regular PL and it remains observable up to 200 K. Interface-induced cold Auger processes along with the presence of trapped states for both electrons and holes in these ordered alloys account for this nonlinear mechanism. A colinear double-beam experiment confirms this. copyright 1996 The American Physical Society.

372

Hydriding properties of a mechanically milled Mg-50 wt.% ZrFe{sub 1.4}Cr{sub 0.6} composite  

Energy Technology Data Exchange (ETDEWEB)

The ball-milling method was used to produce Mg-50 wt.% ZrFe{sub 1.4}Cr{sub 0.6} composite. The thermodynamic, kinetic, and cycling properties, as well as the resistance to oxidation were examined. This composite possesses excellent kinetic properties, even at moderate temperature. Scanning electron microscopy, energy-dispersive spectrum, transmission electron microscopy and X-ray diffraction were used to characterize the composite before and after hydriding. The fine ZrFe{sub 1.4}Cr{sub 0.6} particles covering Mg particles acting as a ''catalytic film'', a significant amount of imperfections and some alloy powder in the Mg matrix introduced by ball milling all contributed to the enhanced absorption/desorption rate. (orig.)

2000-02-02

373

Homolytic cleavage C-C bond in the electrooxidation of ethanol and bioethanol  

British Library Electronic Table of Contents (United Kingdom)

Nowadays, the studies are focused on the search of better electrocatalysts that promote the complete oxidation of ethanol/bioethanol to CO2. To that end, amorphous bi-catalytic catalysts of composition Ni59Nb40Pt1-xYx (Y=Cu, Ru, x=0.4% at.) have been developed, obtained by mechanical alloying, resulting in higher current densities and an improvement in tolerance to adsorbed CO vs. Ni59Nb40Pt1 catalyst. By using voltammetric techniques, the appearance of three oxidation peaks can be observed. The first peak could be associated with the electrooxidative process of ethanol/bioethanol to acetaldehyde, the second peak could be the oxidation of acetaldehyde to acetic acid, and the last peak might be the final oxidation to CO2. Chrono-amperometric experiments show qualitative poisoning of catalyt...

2011-01-01

374

Features of local atomic structure of nanocrystalline disordered Fe-M (M=Ge, Sn, Al, Si) alloys: EXAFS-study  

International Nuclear Information System (INIS)

The EXAFS-study (Fe, Sn and Ge K-edges) of disordered by mechanical activation binary supersaturated nanocrystalline solid solutions Fe-Al, Fe-Ge, Fe-Sn and Fe-Si is presented. The EXAFS-spectra are processed by solving the inverse binary problem, using the EXAFS-spectrum of the Fe K-edge only or combining the EXAFS-spectra on two K-edges, Fe and Ge or Fe and Sn. The parameters of partial correlation functions indicate chemical short-range ordering, high local static distortions in the lattice, increasing with metalloid content. The macrostructure of other type is forming through an initial, 'local' stage within the bcc lattice.

2007-05-21

375

Electrochemical noise in corrosion  

International Nuclear Information System (INIS)

By varying different variables (potential, chloride content, surface pretreatment etc.) it is possible to show the effect of increasingly harsher corrosion conditions on passive-layer stability. These changes will not be detected by conventional methods e.g. measurement of passive current density, until a very late stage. Electrochemical noise measurement will allow the action of inhibitors to be detected in a rapid and effective manner. High-alloy steels and titanium claddings subjected to pitting corrosion in chloride-containing media demonstrate how to use this method for problem solutions and to open up new practical applications. The effect of mechanical stresses (natural, tensile) on the corrosion system can be detected by electrochemical noise which opens up new methods for crack corrosion studying and monitoring. (orig./DG).

1993-10-07

376

Electrochemical behavior of antimony and electrodeposition of Mg-Li-Sb alloys from chloride melts  

British Library Electronic Table of Contents (United Kingdom)

The electrochemical behavior of Sb(III) ions was investigated in LiCl-KCl molten salt at 673K. The reaction mechanism and transport parameters of electroactive species were determined by transient electrochemical techniques (such as cyclic voltammetry, square wave voltammetry, chronopotentiometry and chronoamperometry) at a molybdenum electrode. The results showed that electrochemical reduction of Sb(III) in LiCl-KCl melts occurred in a reaction step with an exchange of three electrons. A voltammogram with a different scan rate in LiCl-KCl containing 1.45x10^-^4molcm^-^3 SbCl3 showed that the deposition/dissolution reaction of Sb(III) ions was not completely reversible. The diffusion coefficient of Sb(III) ions was 1.65(+/-0.01)x10^-^5cm^-^2s^-^1 at 673K. The electroreduction of Sb(III) io...

2011-01-01

377

A micro-alloyed ferritic steel strengthened by nanoscale precipitates  

British Library Electronic Table of Contents (United Kingdom)

A ferritic steel with finely dispersed precipitates was investigated to reveal the fundamental strengthening mechanisms. The steel has a yield strength of 760MPa, approximately three times higher than that of conventional Ti-bearing high strength hot-rolled sheet steels, and its ultimate tensile strength reaches 850MPa with an elongation-to-failure value of 18%. Using energy dispersive X-ray spectroscopy (EDXS) and transmission electron microscope (TEM), fine carbides TiC with an average diameter of 10nm were observed in the ferrite matrix of the 0.08%Ti steel, and some cubic M23C6 precipitates were also observed at the grain boundaries and the interior of the grains. The finely dispersed TiC precipitates in the matrix provide matrix strengthening. The estimated magnitude of precipitation ...

2011-01-01

378

Vibration characteristics of SMA composite beams with different boundary conditions  

Energy Technology Data Exchange (ETDEWEB)

Recently, the development of shape memory alloy (SMA) actuators, in the forms of wire, thin film and stent have been found increasingly in the fields of materials science and smart structures and engineering. The increase in attraction for using these materials is due to their many unique materials, mechanical, thermal and thermal-mechanical properties, which in turn, evolve their subsequent shape memory, pseudo-elasticity and super-elasticity properties. In this paper, a common type of SMA actuator, Nitinol wires, were embedded into advanced composite structures to modulate the structural dynamic responses, in terms of natural frequency and damping ratio by using its shape memory and pseudo-elastic properties. A simple theoretical model is introduced to estimate the natural frequency of the structures before and after actuating the embedded SMA wires. The damping ratios of different SMA composite beams were measured ...

2002-12-15

379

Modeling grain size during hot deformation of IN 718  

Energy Technology Data Exchange (ETDEWEB)

Aerospace gas turbine disks operate in an environment of relatively high stresses caused by centrifugal forces and elevated temperatures. These severe conditions necessitate the need for materials with high temperature strength and good low cycle fatigue resistance. One class of alloys used for this task is the nickel base superalloys, out of which, IN 718 is the most widely used in the aerospace industry. The properties of IN 718 are attributed to the combined effects of the chemistry, heat treatment, and microstructure. The chemistry is tailored not only for solid solution strengthening but also for precipitation hardening developed during heat treatment, which combined with a fine grained microstructure lead to excellent mechanical properties such as low cycle fatigue resistance and elevated temperature strength. The properties of a gas turbine disk are sensitive to the microstructure, in particular the grain size, which is dependent on the ...

1999-12-17

380

Effect of the fabrication process on fatigue performance of U3Si2 fuel plate with sandwich structure  

Science.gov (United States)

U3Si2 Al fuel plate is one of the dispersion fuel structure materials recently developed and widely used in research reactors. The mechanical properties of this structural material, especially the fatigue performance, are strongly dependent on its fabrication process. To investigate the effects of these processing technologies, the fatigue tests for the different specimens were carried out. The S N curves indicate that the fabrication processing technologies of U3Si2 fuel plate, such as the addition of U3Si2 particles into aluminum powder to form the fuel meat, holding and rolling the processes of meat and cladding of 6061-Al alloy, plays an important role in improving the mechanical properties and fatigue performance of this fuel plate. In addition, some factors that influence the crack initiation and propagation are summarized based on the fatigue images that are in situ observations with SEM. The critical criterion for ...

2005-06-01

381

Corrosion mode diagrams for alloy 690 TT and alloy 800  

Energy Technology Data Exchange (ETDEWEB)

Due to the well-establish corrosion problems of Alloy 600 as a steam-generator material and the subsequent focus on thermally treated (TT) Alloy 690 and Alloy 800 as alternative materials, a systematic analysis of the corrosion behavior of these two latter alloys is warranted. Corrosion test results for Alloys 690 TT and 800 were collected and organized in the form of corrosion mode diagrams. Selected data for mill annealed (MA) Alloy 600 were also included for reference. The corrosion mode diagrams correlate the modes of corrosion degradation observed in tests as functions of the environment pH and electrochemical potential (ECP). The diagrams confirm that Alloys 690TT shows some susceptibility in caustic environments, and Alloy 800 shows susceptibility in both caustic and highly acidic environments. (authors). 6 figs., ...

1994-12-31

382

Corrosion mode diagrams for alloy 690 TT and alloy 800  

International Nuclear Information System (INIS)

Due to the well-establish corrosion problems of Alloy 600 as a steam-generator material and the subsequent focus on thermally treated (TT) Alloy 690 and Alloy 800 as alternative materials, a systematic analysis of the corrosion behavior of these two latter alloys is warranted. Corrosion test results for Alloys 690 TT and 800 were collected and organized in the form of corrosion mode diagrams. Selected data for mill annealed (MA) Alloy 600 were also included for reference. The corrosion mode diagrams correlate the modes of corrosion degradation observed in tests as functions of the environment pH and electrochemical potential (ECP). The diagrams confirm that Alloys 690TT shows some susceptibility in caustic environments, and Alloy 800 shows susceptibility in both caustic and highly acidic environments. (authors). 6 figs., ...

383

Isolating the effect of radiation-induced segregation in irradiation-assisted stress corrosion cracking of austenitic stainless steels  

International Nuclear Information System (INIS)

Post-irradiation annealing was used to help identify the role of radiation-induced segregation (RIS) in irradiation-assisted stress corrosion cracking (IASCC) by preferentially removing dislocation loop damage from proton-irradiated austenitic stainless steels while leaving the RIS of major and minor alloying elements largely unchanged. The goal of this study is to better understand the underlying mechanisms of IASCC. Simulations of post-irradiation annealing of RIS and dislocation loop microstructure predicted that dislocation loops would be removed preferentially over RIS due to both thermodynamic and kinetic considerations. To verify the simulation predictions, a series of post-irradiation annealing experiments were performed. Both a high purity 304L (HP-304L) and a commercial purity 304 (CP-304) stainless steel alloy were irradiated with 3.2 MeV protons at 360 deg. C to doses of 1.0 and 2.5 dpa. Following irradiation, ...

2002-04-01

384

The creep and intergranular cracking behavior of Ni-Cr-Fe-C alloys in 360 degree C water  

International Nuclear Information System (INIS)

Mechanical testing of controlled-purity Ni-xCr-9Fe-yC alloys at 360 C revealed an environmental enhancement in IG cracking and time-dependent deformation in high purity and primary water over that exhibited in argon. Dimples on the IG facets indicate a creep void nucleation and growth failure mode. IG cracking was primarily located at the interior of the specimen and not necessarily linked to direct contact with the environment. Controlled potential CERT experiments showed increases in IG cracking as the applied potential decreased, suggesting that hydrogen is detrimental to the mechanical properties. It is proposed that the environment, through the presence of hydrogen, enhances IG cracking by enhancing the matrix dislocation mobility. This is based on observations that dislocation-controlled creep controls the IG cracking of controlled-purity Ni-xCr-9Fe-yC in argon at 360 C and grain boundary cavitation and sliding ...

1995-03-26

385

Mechanism of r. f. plasma nitriding of Ti-6Al-4V alloy  

Energy Technology Data Exchange (ETDEWEB)

The objective of the current study was the gradual development of the formation of the nitride layer during inductive r.f. plasma nitriding. The study centers on characterization of refined layers and plasma diagnostics in the vicinity of the sample, and raises critical questions of how the layers and interfacial microstructure might affect the near-surface properties. The composition of the plasma near the surface of the sample (plasma layer) was examined by optical emission spectroscopy and mass spectrometry during plasma nitriding and while sputtering the sample after the nitriding process. It was observed that during the nitriding process, the plasma layer contains Ti, NH[sub n] species, N (or/and N[sup +]), H[sub n] species (or/and H[sup +][sub 2]). However, when the nitrided sample was exposed to argon plasma, Ti, Al and NH were observed. It was found that two distinct sublayers, comprising [delta]-TiN and [delta]-TiN + [epsilon]-Ti[sub 2]N phases, were formed with ...

1993-08-15

386

Evaluation of a process for the decontamination of radioactive hotspots due to activated stellite particles  

International Nuclear Information System (INIS)

Some of the Indian pressurized heavy water reactors (PHWRs) which use Stellite balls in the ball and screw mechanism of the adjustor rod drive mechanism in the moderator circuit have encountered high radiation fields in the moderator system due to "6"0Co. Release of particulate Stellite is responsible for the hotspots in addition to the general uniform contamination of internal surfaces with "6"0Co. Extensive laboratory studies have shown that it is possible to dissolve these Stellite particles by adopting a three-step redox process with permanganic acid as the oxidizing agent. These investigations with inactive Stellite in powder form helped to optimize the process conditions. Permanganic acid was found to have the highest dissolution efficiency as compared to alkaline and nitric acid permanganate. The susceptibility of Stellite to corrode or dissolve was found to depend on the concentration of the permanganate, pH and temperature of the ...

2011-06-01

387

A comparison of the low cycle fatigue behavior of alloy 800 and alloy 800H  

International Nuclear Information System (INIS)

The low cycle fatigue testing was carried out to provide a basis for comparison of the behavior of the two kinds of Alloy 800 (low carbon Alloy 800 and high carbon Alloy 800H). The testing was done at temperatures of 500"0C and 650"0C either with or without hold. The results obtained were as follows: (1) At 650"0C, the low-cycle fatigue life was essentially the same for the two alloys on the basis of strain amplitude, but Alloy 800H had a longer life on the basis of stress amplitude. (2) At 500"0C, the two alloys exhibited longer lives than at 650"0C, with Alloy 800 exhibiting 2-3 times longer life than Alloy 800H when compared on the basis of plastic strain range. At this temperature the stress range showed the maximum for Alloy 800H. (3) When a creep effect was introduced either by way of a hold ...

1979-06-01

388

Production of titanium alloys with uniform distribution of heat resisting metals  

International Nuclear Information System (INIS)

Consideration is given to the process of the formation of a titanium sponge alloyed with niobium or tantalum, in the joint metallic reduction of titanium, niobium and tantanum chlorides. A percentage composition of the phases observed and the structure of the alloyed sponge have been studied. It is shown that after one remelting operation of the alloyed sponge the alloys of titanium with niobium and tantalum have a uniform component distribution. At the stage of chloride reduction there appear solid solutions based on titanium and an alloying component. The stage of vacuum separation of the reaction mass is associated with a mutual dissolution of the primary phases and the formation of the solid solutions of the alloyed titanium sponge, which, by their composition, are close to the desired alloy composition. The principal features of the ...

389

Tensile strength of eutectic, directionally solidified alloys based on the Co-Cr-C-system  

International Nuclear Information System (INIS)

The influence of various alloy elements on tensile strength of the eutectic, directionally solidified superalloy 73 C was determined. The tensile properties of the base alloy has been increased by Al, Y and C as alloying elements, while Ni and Ti showed a decreasing effect (alloy softening). However, ductility and thermo-fatigue behaviour had been influenced in a positive way by these elements. The specific meachanism caused by the different elements are discussed. (orig.).

1981-01-01

390

Quartz ceramics alloying  

International Nuclear Information System (INIS)

The following methods of quartz ceramics alloying were considered: alloying of initial quartz glass; introduction of alloying additive into water slip of quartz glass; porous materials impregnation with salt aqueous solutions and subsequent salt thermal decomposition with formation of stable oxides in pores of ceramics. Oxygen free compounds BN, SiB_4, SiC, Si_3N_4, REM oxides and transition metal oxides were used as alloying additives. Main properties of the materials and compositions obtained are presented.

391

Processing and properties of Nb-Ti-base alloys  

Energy Technology Data Exchange (ETDEWEB)

The processing characteristics, tensile properties, and oxidation response of two Nb-Ti-Al-Cr alloys were investigated. One creep test at 650 C and 172 MPa was conducted on the base alloy, which contained 40Nb-40Ti-10Al-10Cr. A second alloy was modified with 0.11 at.% C and 0.07 at.% Y. Alloys were arc melted in a chamber backfilled with argon, drop cast into a water-cooled copper mold, and cold rolled to obtain a 0.8-mm sheet. The sheet was annealed at 1,100 C for 0.5 h. Longitudinal tensile specimens and oxidation specimens were obtained for both the base alloy and the modified alloy. Tensile properties were obtained for the base alloy at room temperature, 400, 600, 700, 800, 900, and 1,000 C and for the modified alloy at room temperature, 400, 600, 700, and 800 C. Oxidation tests the base alloy ...

1993-08-01

392

Processing and properties of Nb-Ti based alloys  

Energy Technology Data Exchange (ETDEWEB)

The processing characteristics, tensile properties, and oxidation response of two Nb-Ti-Al-Cr alloys were investigated. One creep tests at 650{degrees}C and 172 MPa was conducted on the base alloy which contained 40Nb-40-Ti-10Al-10Cr. A second alloy was modified with 0.11 at. % carbon and 0.07 at. % yttrium. Alloys were arc melted in a chamber backfilled with argon, drop cast into a water-cooled copper mold, and cold rolled to obtain a 0.8-mm sheet. The sheet was annealed at 1100{degrees}C for 0.5 h. Longitudinal tensile specimens and oxidation specimens were obtained for both the base alloy and the modified alloy. Tensile properties were obtained for the base alloy at room temperature, 400, 600, 700, 800, 900, and 1000{degrees}C, and for the modified alloy at room temperature, 400, 600, 700, and 800{degrees}C. Oxidation ...

1992-01-01

393

Nickel alloy clad steel plate for flue gas desulfurization applications  

Energy Technology Data Exchange (ETDEWEB)

The use of nickel alloys in Flue Gas Desulfurization (FGD) applications is described. Recently, nickel alloys 625 and C-276 have been clad to carbon steel plate. Production and properties of the clad plate are reviewed and a brief discussion is presented on production, fabrication and welding. Laboratory and field corrosion tests in SO/sub 2/ scrubber environments suggest that alloy 625 and C-276 clad steel plates are as corrosion resistant as the solid alloy plate.

1987-01-01

394

Investigation into superplasticity of Be alloys  

International Nuclear Information System (INIS)

Investigated are the characteristics of high-temperature plastic deformation the velocity sensitivity of flow stresses, deformation curves, flow stresses, deformation before rupture - as well as the structure of beryllium alloys containing nickel (0.5-4 %), yttrium (0.5-2 %) and aluminium (38 %). The alloys containing nickel (2%) and yttrium (0.5 %) are superplastic, however, deformation before fracture of the alloys is lower than that of the unalloyed beryllium. The singularities of high-temperature plastic flow of the alloys and the causes of deterioration of their plasticity are determined.

395

Comparative behavior of Alloys 600, 690 and 800 in caustic environments  

Energy Technology Data Exchange (ETDEWEB)

Since 1991, secondary side cracking has become a major concern in EDF steam generators. At 350 C, IGSCC of Alloy 600 was found in pure NaOH solutions from 4 to 500 g/l, with a maximum at 100 g/l. From the present results and available data, IGSCC of Alloy 690 occurred in pure NaOH solutions from 40 to 500 g/l, but the greatest sensitivity was observed at 100 g/l. TG/IGSCC of Alloy 800 became more severe with increasing NaOH solutions, from 10 to 500 g/l. On the whole, the ranking for SCC-resistance was Alloy 600 < Alloy 800 < Alloy 690. A significant improvement was still obtained with 690TT with intergranular carbides (industrial tubes) and perhaps with Alloy 800 NG (nuclear grade), but both alloys cracked at the highest stresses. IGSCC susceptibility of Alloy 600 MA was higher for the tubes ...

1995-12-31

396

Synthesis, characterization and catalytic activities of vanadium complexes containing ONN donor ligand derived from 2-aminoethylpyridine  

British Library Electronic Table of Contents (United Kingdom)

Reaction between [V^I^VO(acac)2] and the ONN donor Schiff base Hpydx-aepy (I) (Hpydx-aepy=Schiff base obtained by the condensation of pyridoxal and 2-aminoethylpyridine) resulted in the formation of a complex [V^I^VO(acac)(pydx-aepy)] (1). Addition of aqueous 30% H2O2 to 1 yields the poor stable oxidoperoxidovanadium(V) complex [V^VO(O2)(pydx-aepy)] (2). Its formation has also been demonstrated in solution by treating 1 with H2O2 in methanol. Reaction of vanadium exchanged zeolite-Y with I in methanol followed by aerial oxidation gave zeolite-Y encapsulated dioxidovanadium(V) complex, abbreviated as [V^VO2(pydx-aepy)]-Y (4). The crystal and molecular structure of 1 has been determined, confirming the ONN binding mode of the ligand. The encapsulated complex [V^VO2(pydx-aepy)]-Y (4) catalyse...

2011-01-01

397

Radiological safety aspects associated with the handling, storage and disposal of self power neutron detectors in TAPS - 3 and 4  

International Nuclear Information System (INIS)

At Tarapur Atomic Power Station 3 and 4, 540 MWe Pressurised Heavy Water Reactors, core being large in size requires a continuous in core monitoring for local flux disturbances. Nearly 200 Self Powered Neutron Detectors (SPNDs) of the Straight Individually Replaceable (SIR) type are distributed in the reactor core. For purpose of reactor regulation and protection, cobalt SPNDs that have a prompt response for changes in power is used for in-core flux mapping, vanadium SPNDs that provide accurate measure of neutron flux, even though having slow response is used In core SPNDs are placed in Vertical Flux Units (VFU) and Horizontal Flux Units (HFUs). These SPNDs were to be replaced at regular intervals to meet the design intent. Cobalt SPNDs have dose rates of the order of 1000 Gy/h and the Mineral Insulated (MI) cables of Vanadium SPNDs have dose rates of the order of 100 Gy/h. So far 3 Cobalt SPNDs were removed from HFUs and are being stored in ...

2006-11-13

398

Irradiation hardening of ferritic steels: Effect of composition  

International Nuclear Information System (INIS)

Irradiation of ferritic steels with neutrons in the temperture range of room temperature to #propor to# 450deg C results in lattice hardening, which causes an increase in strength and a decrease in ductility. Eight reduced-activation Cr-W-V stels with chromium concentration varying from 2.25 to 12% were irradiated at 365deg C to #propor to# 7 dpa in the Fast Flux Test Facility. A steel with 2.25% Cr and the combination of 2% W and 0.25% V hardened less than those containing vanadium or tungsten alone or a steel with 1% W and 0.25% V. The amount of hardening was similar for Cr-W-V steels with constant vanadium and tungsten concentrations and containing 2.,25, 5, and 9% Cr; a steel with 12% Cr hardened considerably more. Specimens of two conventional Cr-Mo steels, 9Cr-1MoVNb and 12Cr-1MoVW, were also irradiated, and the hardening of these steels was similar to analogous reduced-activation steels. (orig.).

1989-12-04

399

V51 Knight Shift in Fine V3Si Particles  

Science.gov (United States)

The Knight shift of vanadium (KV) in fine V3Si particles was studied. The average diameter (\\bar{d}) ranged from 60 to 8000 A. The strong temperature dependence of the KV characteristic of high-Tc A-15 compounds was weakened in the particles. KV at 77 K increased with a decrease in \\bar{d}. The above-mentioned trends were consistent with a broadening of the sharp peak in the electronic density of states around the Fermi energy in particles resulting from a perturbation of the surface.

1987-12-01

400

Study of penetration depth for V"+ with low energy implanted in peanut seeds  

International Nuclear Information System (INIS)

The penetration depth and concentration distribution for vanadium ions with low energy implanted into the dry peanut seeds is determined by scanning electron microscope and X-ray energy dispersion spectrometer. The results show that the depth-concentration distribution is a Gaussian distribution with a long tail and the maximum penetration depth is about 13.6 #mu#m for V"+ with 200 keV in cotyledon of the peanut. The experimental result of the implanted V"+ range in the peanut seeds is compared with the calculating value of the TRIM95

2002-11-01

401

Microstructure of spray converted nanostructured tungsten carbide-cobalt composite  

Energy Technology Data Exchange (ETDEWEB)

This paper reports the presence of face centered cubic cobalt precipitates inside tungsten carbide in nanocomposite of WC-Co synthesized by spray conversion processing. EDS was used to identify the presence and micro-diffraction was employed to determine the nature of the precipitates. There is entrapment of cobalt in tungsten carbide during the spray conversion process used to form WC/Co powder. During consolidation, at high temperatures, the cobalt attains enough mobility to precipitate inside WC. A vanadium containing compound was seen at the interfaces in samples which incorporated VC as a grain growth inhibitor. (orig.)

1996-05-01

402

Influence of microalloying on the corrosion resistance of steel in saturated calcium hydroxide  

International Nuclear Information System (INIS)

The influence of microalloying vanadium or titanium on improving the corrosion resistance of mild steel in saturated calcium hydroxide solution was investigated. Potential-time, potentiodynamic polarization, and impedance measurement techniques were employed. The corrosion products have been examined by infrared and X-ray diffraction analysis and by scanning electron microscopy. It has been shown that the grain refining, due to microalloying, plays an important role in enhancing the corrosion resistance of steel. Scales of calcite and iron oxides on top of a protective oxide are formed on the investigated steels.

403

Production of intergranular attack of alloy 600, alloy 690, and alloy 800 tubing in tubesheet crevices: Topical report  

Energy Technology Data Exchange (ETDEWEB)

Three model boilers, manufactured to simulate full-size tube sheet crevices, were tested with various secondary side environments. The first was faulted with organics representative of the decomposition of humic acid. The second was faulted with sodium carbonate and sodium hydroxide, while the third was faulted with sodium sulfate and sodium hydroxide. Each model contained seven tubes, which included Alloy 600 in the mill-annealed (MA) and thermally-treated (TT) conditions and Alloy 690 in the thermally-treated condition. Two models contained Alloy 800 tubes in the mill-annealed condition and one had Alloy 800 in the mill-annealed/cold-worked/glass-bead-peened condition. Two different sizes of tubesheet crevices were used in all model boilers. In the organics-faulted boiler, tubes of Alloy 600MA, Alloy 690TT and Alloy 800MA experienced no ...

1987-07-01

404

Production of intergranular attack of alloy 600, alloy 690, and alloy 800 tubing in tubesheet crevices: Topical report  

International Nuclear Information System (INIS)

Three model boilers, manufactured to simulate full-size tube sheet crevices, were tested with various secondary side environments. The first was faulted with organics representative of the decomposition of humic acid. The second was faulted with sodium carbonate and sodium hydroxide, while the third was faulted with sodium sulfate and sodium hydroxide. Each model contained seven tubes, which included Alloy 600 in the mill-annealed (MA) and thermally-treated (TT) conditions and Alloy 690 in the thermally-treated condition. Two models contained Alloy 800 tubes in the mill-annealed condition and one had Alloy 800 in the mill-annealed/cold-worked/glass-bead-peened condition. Two different sizes of tubesheet crevices were used in all model boilers. In the organics-faulted boiler, tubes of Alloy 600MA, Alloy 690TT and Alloy 800MA experienced no ...

405

Study of propane partial oxidation on vanadium-containing catalysts  

Energy Technology Data Exchange (ETDEWEB)

The present results indicate that maximum selectivity to acrylic acid can be reached over V-P-Zr-O catalysts. When the hydrocarbon concentration is 5.1 vol.% the selectivity is about 30% at quite high paraffin conversion. Conclusively, some explanations to the observed facts can be given. The V-P-O catalyst promotion with lanthanum by means of mechanochemical treatment is distinguished by the additive uniform spreading all over the matrix surface. Such twophase system is highly active in propane conversion (lanthanum oxide) and further oxidation of the desired products. The similar properties are attributed to V-P-Bi-La-O catalyst. Bismuth, tellurium and zirconium additives having clearly defined acidic properties provoke the surface acidity strengthening and make easier desorption of the acidic product (acrylic acid) from the surface lowering its further oxidation. Additionally, since bismuth and zirconium are able to form phosphates and, according to, to create space limitations for ...

1998-12-31

406

Preparation of vanadium III oxidic compounds, and dehydrogenation of paraffins  

Energy Technology Data Exchange (ETDEWEB)

A process is described for making a compound selected from a crystalline spinel of the formula A/sup II/V/sub 2-x//sup III/C/sub x//sup III/O/sub 4/ formula (1) or a crystalline perovskite of the formula D/sup III/V/sub 1-y//sup III/C/sub y//sup III/O/sub 3/ formula (2) from a pentavalent vanadium compound, where A is one or more of Mg, Zn, Mn, Fe, Co, Ni, Cu and Cd; D is one ore more of Y, the rare earths and Bi; C is one or more of Al, Ga, Cr, Fe and Co, x is zero to <2, and y is zero to<1. The process comprises (1) reducing a pentavalent vanadium oxidic compound to substantially the V/sup III/ state by heating at 100/sup 0/C. or less an aqueous medium slurry or solution of the pentavalent compound containing a reducing agent selected from hydrazine and a hydrocarbylhydrazine, (2) providing in the aqueous medium either before, during or after the reducing step, A/sup II/, D/sup III/ and C/sup III/ cations in solution in the ratio called ...

1988-04-12

407

Laser hardening of titanium-zirconium alloy  

International Nuclear Information System (INIS)

The methods of surface modification of Ti-Zr alloy by laser treatment are considered. Characteristics of laser modification without- and with surface melting and with melting in different gaseous environments and with nickel microalloying are presented. Maximum depth, hardness and corrosion resistance are observed under nickel laser alloying.

408

Development of Mg alloy sheets via strip casting  

Energy Technology Data Exchange (ETDEWEB)

AZ31 and experimental ZMA611 alloys were strip cast into 2 mm thick strips. The as-cast AZ31 alloy strip consists of columnar dendrites. On the other hand, as-cast ZMA611 alloy strip shows equiaxed dendritic structure through the thickness of strip. These alloys were subjected to various thermomechanical treatments and their tensile properties were evaluated. Strip cast AZ31 alloy in H24 condition has equivalent yield and tensile strengths with similar ductility compared to commercial ingot cast AZ31-H24 alloy, indicating that strip casting is a viable process for the fabrication of Mg alloy strips. The ZMA611 alloy has a large volume fraction of fine dispersoid particles in the microstructure, resulting from the beneficial effect of strip casting on microstructural refinement. It has been shown that the ZMA611 ...

2005-07-01

409

Wear resistance of a laser surface alloyed Ti-6Al-4V alloy  

Energy Technology Data Exchange (ETDEWEB)

Laser surface alloying with gaseous nitrogen was utilized to improve the wear resistance of a Ti-6Al-4V alloy. Wear-resistant composite coatings reinforced by hard TiN dendrites were produced 'in-situ' on a substrate of a Ti-6Al-4V alloy. The hardness and wear resistance of the laser alloyed coating under two-body abrasive and block-on-ring full-sliding wear conditions were significantly enhanced. (orig.)

2000-08-01

410

Development of ALLOY 800 for PWR/SG tubings resistant to IGSCC and general corrosion  

Energy Technology Data Exchange (ETDEWEB)

Resistance of ALLOY 800 as a PWR/SG tubings to IGC/IGSCC and Ni, Co release into high temperature water was evaluated as compared with ALLOYs 600 and 690. The study to improve the resistance to IGSCC and general corrosion was also made. From the results, ALLOY 800 was evaluated to be the most reliable among the high Ni alloys tested. In addition, the alloy would obtain further reliability in IGSCC and general corrosion resistance by the combined addition of Ti and Nb, and the prior oxidation treatments, respectively. (author).

1989-07-01

411

Corrosion resistance of #gamma#-solid solution and hardening #gamma#'-phase of nickel alloys in sodium sulfate and chloride melts  

International Nuclear Information System (INIS)

Corrosion testings of model alloys, corresponding by chemical composition to simple and complex-alloyed #gamma#- and #gamma#'-phases of nickel heat-resistant alloys are conducted in sodium sulfate and chloride melts. It is ascertained that heat resistant nickel alloys containing over 50 % of hardening #gamma#'-phase, are subject to disastrous sulfide corrosion (SC). Resistance against SC alloys containing below 50 % of #gamma#'-phase is determined by the resistance of #gamma#-solid solution. 10 refs., 3 figs., 2 tabs.

412

Ultra High Strength Beta Titanium Alloy for Fasteners.  

Science.gov (United States)

... Accession Number : ADD151811. Title : Ultra High Strength Beta Titanium Alloy for Fasteners. Descriptive Note : Journal article,. ...

413

Thermophysical Properties of Matter - The TPRC Data Series. ...  

Science.gov (United States)

... alloys--Lanthanum-- Magnesium--Magnasium &11oy8--Hagn*31Uft compounds--Manxganese--Manganes. alloys-- Mercury ...

2011-05-14

414

THERMAL STABILITY OF ALPHA-BETA TITANIUM ALLOY Ti ...  

Science.gov (United States)

... Accession Number : ADD109273. Title : THERMAL STABILITY OF ALPHA-BETA TITANIUM ALLOY Ti-5Al-2Cr-1Fe,. Corporate Author : ...

1975-08-01

415

THE SUSCEPTAEILITY OF MATERIALS  

Science.gov (United States)

Hilled Bend Spechene of an Alpha-Beta Titanium Alloy. Ti-6M14V. ..... The all beta titanium alloy was nllled from both sides; only the edges were taped. ...

416

SIMS imaging studies of the corrosion of alloy 800 and alloy 600 surfaces under secondary side boiler conditions  

Energy Technology Data Exchange (ETDEWEB)

The nickel-rich superalloys Alloy 600 and Alloy 800 have been corroded in mildly alkaline deuterated aqueous conditions typical of secondary coolant circuits in a nuclear power station. The oxide films and substrates of these alloys have been analysed by imaging SIMS depth profiling, which makes it possible to describe elemental distribution in all three dimensions. The measurement of the distribution of the secondary ions NiO[sup -], FeO[sup -] and CrO[sup -] appears useful for detailing the behaviour of nickel, iron and chromium within oxidized phases. The measurement of D[sup -] distribution outlines the extent of oxide hydration. For Alloy 800, evidence of sodium migration into the grain boundaries of the alloy substrate is found. For Alloy 600, no grain boundary sodium ingress can be identified under comparable corrosion conditions. (author).

1992-08-01

417

SIMS imaging studies of the corrosion of alloy 800 and alloy 600 surfaces under secondary side boiler conditions  

International Nuclear Information System (INIS)

The nickel-rich superalloys Alloy 600 and Alloy 800 have been corroded in mildly alkaline deuterated aqueous conditions typical of secondary coolant circuits in a nuclear power station. The oxide films and substrates of these alloys have been analysed by imaging SIMS depth profiling, which makes it possible to describe elemental distribution in all three dimensions. The measurement of the distribution of the secondary ions NiO"-, FeO"- and CrO"- appears useful for detailing the behaviour of nickel, iron and chromium within oxidized phases. The measurement of D"- distribution outlines the extent of oxide hydration. For Alloy 800, evidence of sodium migration into the grain boundaries of the alloy substrate is found. For Alloy 600, no grain boundary sodium ingress can be identified under comparable corrosion conditions. (author).

419

Reduced activation activities  

Energy Technology Data Exchange (ETDEWEB)

Four low activation alloy classes, two austenitic and two ferritic, have been incorporated into the MOTA-1B experiment in the FFTF reactor to provide an early assessment of the suitability of such alloys for reactor service.

1984-01-01

420

Metal dusting behaviour of welded Ni-base alloys with different surface finish  

Energy Technology Data Exchange (ETDEWEB)

Welded Ni-base alloys and Alloy 800 were exposed under metal dusting conditions at 600 C and 650 C for up to 6000 hours. Alloy 800 was attacked very strongly already in the first days and Alloy 600 also rather soon and widespread, on both materials attack started mainly in the heat affected zone. Several surface states of Alloy 600: brushed, ground, sand-blasted and pickled were tried only grinding caused a modest delay and decrease of metal dusting attack. Generally the attack was less widespread but deeper at 650 C than at 600 C, also for Alloy 601 and 602. The latter alloys show minor, mainly local attack, but especially the welds are affected. TIG welding led to better resistance than hand-welding. (Abstract Copyright [2003], Wiley Periodicals, Inc.)

2003-10-01

421

Environmental Cracking of the Alpha-Beta Titanium Alloy, Ti ...  

Science.gov (United States)

... Accession Number : ADD120492. Title : Environmental Cracking of the Alpha-Beta Titanium Alloy, Ti-6Al-6V-2Sn,. Corporate ...

422

Effect of Stress and Strain Path on Cavity Closure During Hot ...  

Science.gov (United States)

... CLOSURE DURING HOT WORKING OF AN ALPHA/BETA TITANIUM ALLOY (PREPRINT) ... HOT WORKING OF AN ALPHA/BETA TITANIUM ALLOY ...

2007-07-01

423

Differences in synchrotron radiation induced gas desorption from stainless steel and aluminium alloy  

CERN Document Server

Differences in synchrotron radiation induced gas desorption from stainless steel and aluminium alloy

1990-01-01

424

Development of a FeCoNb Alloy to be used in Eddy Current ...  

Science.gov (United States)

... Accession Number : ADD336001. Title : Development of a FeCoNb Alloy to be used in Eddy Current Probes for Testing Ferromagnetic Tubes,. ...

425

Development of Lead-Free Copper Alloy-Graphite Castings  

Energy Technology Data Exchange (ETDEWEB)

In this project, graphite is used as a substitute for lead in order to maintain the machinability of plumbing components at the level of leaded brass. Graphite dispersed in Cu alloy was observed to impart good machinability and reduce the sizes of chips during machining of plumbing components in a manner similar to lead. Copper alloys containing dispersed graphite particles could be successfully cast in several plumbing fixtures which exhibited acceptable corrosion rate, solderability, platability, and pressure tightness. The power consumption for machining of composites was also lower than that of the matrix alloy. In addition, centrifugally cast copper alloy cylinders containing graphite particles were successfully made. These cylinders can therefore be used for bearing applications, as substitutes for lead-containing copper alloys. The results indicate that copper graphite ...

1999-10-01

426

DUCTILITY RATIO OF AGED BETA TITANIUM ALLOY  

Science.gov (United States)

... Title : DUCTILITY RATIO OF AGED BETA TITANIUM ALLOY. Corporate Author : NEW YORK UNIV NY SCHOOL OF ENGINEERING AND SCIENCE. ...

1962-01-02

427

Beta-21S: A High Temperature Metastable Beta Titanium Alloy ...  

Science.gov (United States)

... Accession Number : ADD144314. Title : Beta-21S: A High Temperature Metastable Beta Titanium Alloy. Descriptive Note : Conference Proceedings, ...

428

An overview of beta titanium alloy environmental behavior  

International Nuclear Information System (INIS)

Stemming from their unique combination of elevated strength, low density, and good overall corrosion resistance, beta titanium alloys have become attractive candidate materials for critical, high-stress, components in corrosive services. An overview of the comparative corrosion resistance of beta alloys to conventional alpha and alpha/beta titanium alloys in common industrial and aerospace service environments generally reveals attractive behavior depending on the environment and alloy composition and, in some cases, alloy condition. Expanded performance windows are especially noted for the molybdenum-rich beta alloys, particularly in regard to resisting reducing acids, stress corrosion, and high temperature localized chloride attack, along with hydrogen and oxidation resistance. Where applicable, implications of this enhanced corrosion performance on current ...

1993-02-21

429

Hydrogen embrittlement, revisited by in situ electrochemical nanoindentation  

Energy Technology Data Exchange (ETDEWEB)

The fine scale mechanical probing capability of NI-AFM was used to examine hydrogen interaction with plasticity. To realize this, an electrochemical three electrode setup was incorporated into the NI-AFM. The developed ECNI-AFM is capable of performing nanoindentation as well as imaging surfaces inside electrolytes. The developed ECNI-AFM setup was used to examine the effect of cathodically charged hydrogen on dislocation nucleation in pure metals and alloys. It was shown that hydrogen reduces the pop-in load in all of the tested materials except Cu. The reduced pop-in load can be interpreted as the HELP mechanism. Classical dislocation theory was used to model the homogeneous dislocation nucleation and it was shown that H reduces the activation energy for dislocation nucleation in H sensitive metals which are not undergoing a phase transformation. The activation energy for dislocation nucleation is related to the material ...

2007-07-01

430

An extended CT scale technique for evaluating periprosthetic bone lesions - an in vitro study; Extended-field CT-Technik zur Evaluation von periprothetischen Knochenlaesionen  

Energy Technology Data Exchange (ETDEWEB)

Purpose: In the present study the reduction of artifacts using an extended CT scale technique was examined in 5 vitallium and 5 titanium-aluminium-vanadium tumor prostheses. Methods: 5 titanium-aluminium-vanadium and 5 vitallium distal femur Mutars {sup trademark} tumor prostheses (Mutars {sup trademark} - Modular Universal Tumor And Revision System) were implanted in 10 human femur specimens. 110 artifical drill hole lesions of 1 mm, 2 mm, 3 mm, 5 mm and 8 mm diameter were placed in the bone around the hexagonal stem of the tumor prosthesis and furthermore in the proximal part of the femur. All specimens were examined using conventional CT and an extended CT scale technique in a slice thickness of 3 mm. Results: In the proximal part of the femur all drill holes could be detected using 3 mm slices, no artefacts were observed. Along the hexagonal stem smooth lines arising from each hexagonal plane could be observed. This made it impossible to ...

2001-12-01

431

The corrosion resistance of alloy 800  

International Nuclear Information System (INIS)

Basic studies of the oxidation resistance of Fe-Cr binary and Fe-Cr-Ni ternary alloys in pure oxygen have shown that the excellent corrosion resistance of Alloy 800 is explicable in terms of the low defect concentrations and diffusion rates in the oxide forming on alloys of this composition in sufficiently oxidising environments. The performance of Alloy 800 in environments of particular importance to nuclear power generation is briefly reviewed to determine to what extent ideas derived from the basic studies of Fe-Cr-Ni ternary alloys are borne out in practice. The good corrosion resistance of Alloy 800 in steam and CO_2 and, to some extent, in molten salt environments is in agreement with the behaviour of ternary alloys in oxygen. Minor aliovalent alloying additions are only expected to have a significant effect on the ...

432

A comparison of the low-cycle fatigue behavior of Alloy 800 and Alloy 800H  

International Nuclear Information System (INIS)

At 650"0C, the low-cycle fatigue life was essentially the same for the two alloys on the basis of strain amplitude, but Alloy 800H had a longer life on the basis of stress amplitude. A 500"0C, Alloy 800 and 800H exhibited longer fatigue lifetime than at 650"0C, with Alloy 800 exhibiting a 2-3 times longer life than Alloy 800H when compared on the basis of plastic strain range, whereas the difference was less pronounced when compared on the basis of stress amplitude. When a creep effect was introduced either by way of a hold time or a reduced frequency, Alloy 800 exhibited a greater reduction in life than did Alloy 800H. The dislocation structure changed from planar to cellular with increase in strain range, and extensive precipitation of M_2_3C_6 was noted within the grains for Alloy 800H and along grain boundaries for ...

433

Surface modification of 30CrNiMo8 low-alloy steel by active screen setup and conventional plasma nitriding methods  

Energy Technology Data Exchange (ETDEWEB)

In this paper, we report on a comparative study of active screen plasma nitriding (ASPN) and conventional dc plasma nitriding (CPN) behavior of 30CrNiMo8 low-alloy steel that has been examined under various process conditions. The process variables included active screen setup parameters (screen and iron plate top lids placed on the screen setup with 8 mm of hole size), treatment temperature (550 and 580 deg. C), gas mixture (75/25 and 25/75 of N{sub 2}/H{sub 2}) and treatment time (5 and 10 h) in 500 Pa pressure. The structure and phases composition of the diffusion zone and compound layer were studied by X-ray diffraction (XRD), microhardness tests, light optical microscopy and scanning electron microscopy (SEM). It was observed that treated sample surfaces in both CPN and ASPN methods consist of {gamma}' and {epsilon} phases, and while the nitriding time and/or temperature increases, the intensity of {epsilon} phase in the compound layer will increase ...

2007-12-30

434

Surface modification of 30CrNiMo8 low-alloy steel by active screen setup and conventional plasma nitriding methods  

International Nuclear Information System (INIS)

In this paper, we report on a comparative study of active screen plasma nitriding (ASPN) and conventional dc plasma nitriding (CPN) behavior of 30CrNiMo8 low-alloy steel that has been examined under various process conditions. The process variables included active screen setup parameters (screen and iron plate top lids placed on the screen setup with 8 mm of hole size), treatment temperature (550 and 580 deg. C), gas mixture (75/25 and 25/75 of N_2/H_2) and treatment time (5 and 10 h) in 500 Pa pressure. The structure and phases composition of the diffusion zone and compound layer were studied by X-ray diffraction (XRD), microhardness tests, light optical microscopy and scanning electron microscopy (SEM). It was observed that treated sample surfaces in both CPN and ASPN methods consist of #gamma#' and #epsilon# phases, and while the nitriding time and/or temperature increases, the intensity of #epsilon# phase in the compound layer will increase for ASPN and ...

2007-12-30

435

Passivity behavior of melt-spun Mg-Y Alloys  

Energy Technology Data Exchange (ETDEWEB)

Several Mg-Y binary ribbons with Y content up to {approx}17.9 at.% were fabricated by melt-spinning. X-ray diffraction (XRD) revealed that the phase structure changes with increasing Y content from extended solid solution to partially amorphous, and then fully intermetallic Mg{sub 24}Y{sub 5}. Anodic potentiodynamic polarization performed in 0.01 M NaCl electrolyte (pH=12) revealed improved anodic passivity behavior compared to pure Mg for all the Mg-Y alloys. X-ray photoelectron spectroscopy (XPS) revealed that the improved passivity of Mg-Y was more related to the elemental oxidation state rather than the concentration of the surface components. To study the effect of Cl{sup -} ion on the passivity behavior, anodic potentiodynamic and potentiostatic polarization were performed on Mg-17.9 at.% Y in alkaline (pH=12) NaCl electrolytes containing Cl{sup -} ion in the concentration range from 0.00 to 0.50 M. The passive films formed in 0.01 M NaCl electrolyte were ...

2003-12-15

436

Passivity behavior of melt-spun Mg-Y Alloys  

International Nuclear Information System (INIS)

Several Mg-Y binary ribbons with Y content up to #approx#17.9 at.% were fabricated by melt-spinning. X-ray diffraction (XRD) revealed that the phase structure changes with increasing Y content from extended solid solution to partially amorphous, and then fully intermetallic Mg_2_4Y_5. Anodic potentiodynamic polarization performed in 0.01 M NaCl electrolyte (pH=12) revealed improved anodic passivity behavior compared to pure Mg for all the Mg-Y alloys. X-ray photoelectron spectroscopy (XPS) revealed that the improved passivity of Mg-Y was more related to the elemental oxidation state rather than the concentration of the surface components. To study the effect of Cl"- ion on the passivity behavior, anodic potentiodynamic and potentiostatic polarization were performed on Mg-17.9 at.% Y in alkaline (pH=12) NaCl electrolytes containing Cl"- ion in the concentration range from 0.00 to 0.50 M. The passive films formed in 0.01 M NaCl electrolyte were similar to the native ...

2003-12-15

437

Inflow behavior observation of molten mold powder between mold and solidified shell by continuous casting simulator using Sn-Pb alloy and stearic acid  

Energy Technology Data Exchange (ETDEWEB)

High productivity and high quality slab machine have been recently required in continuous casting process to lower the cost of steel production. It is important to know the inflow behavior of mold powder between mold and solidified shell to develop higher-speed casting. The purpose in this study is to make clear she mechanism of lubrication between mold and solidified shell. Sn-5mass%Pb alloy and stearic acid were used as substituted of liquid steel and molten mold powder in the experiment simulated continuous casting machine. Direct observation on inflow behavior of mold powder was made experimentally by a digital video camera. The friction force between mold and solidified shell was measured by a load cell which was set under the mold. Mold powder flowed into the aperture between mold and solidified shell during both positive strip time period and negative strip time period and the amount of powder consumption in positive strip time period ...

2000-06-01

438

Environmentally assisted cracking in light water reactors. Semiannual report, October 1993--March 1994. Volume 18  

International Nuclear Information System (INIS)

This report summarizes work performed by Argonne National Laboratory (ANL) on fatigue and environmentally assisted cracking (EAC) in light water reactors (LWRs) during the six months from October 1993 to March 1994. EAC and fatigue of piping, pressure vessels, and core components in LWRs are important concerns in operating plants and as extended reactor lifetimes are envisaged. Topics that have been investigated include (a) fatigue of low-alloy steel used in piping, steam generators, and reactor pressure vessels, (b) EAC of wrought and cast austenitic stainless steels (SSs), and (c) radiation-induced segregation and irradiation-assisted stress corrosion cracking (IASCC) of Type 304 SS after accumulation of relatively high fluence. Fatigue tests have been conducted on A302-Gr B low-alloy steel to verify whether the current predictions of modest decreases of fatigue life in simulated pressurized water reactor water are valid for high-sulfur heats ...

2007-09-01

439

Development of MHD generator channel walls, 1  

International Nuclear Information System (INIS)

Experimental results of compatibility tests on ceramics-metal bonded structures performed under high heat flux conditions in splash test apparatus are reported. Emphasis is placed on results of the channel wall design and its critical operating conditions under MHD environment. The module design of one cold type and three semihot type insulators have been tested. These materials were Al_2O_3, Al_2MgO_4, LaAlO_4, MgO and Sialon ceramics. The methods of cold type ceramics-metal bonding structure were studied on Al_2O_3 and Spinel spray coating technology. The refractory metallizing and ceramics-metal graded structure manufactured by HIP technologies were applied to bonding between the MgO or LaAlO_4 and metallic cooling system. The Sialon non-bonding structure was tested with mechanical supported cooling system by shrinc fitting method. The results indicated that the bonding structures made of the MgO(MG-S) with Copper and Fe-Ni Alloy relaxation ...

440

Delayed Hydride Cracking Mechanism in Zirconium Alloys and Technical Requirements for In-Service Evaluation of Zr-2.5Nb Tubes with Flaws  

International Nuclear Information System (INIS)

In association with periodic inspection of CANDU nuclear power plant components, Canadian Standards Association issued CSA N285.8 in 2005 as technical requirements for in-service evaluation of zirconium alloy pressure tubes in CANDU reactors. This first version, CSA N285.8 involves procedures for, firstly, the evaluation of pressure tube flaws, secondly, the evaluation of pressure tube to calandria tube contact and, thirdly, the assessment of a reactor core, and material properties and derived quantities. The evaluation of pressure tube flaws includes delayed hydride cracking evaluation the procedures of which are stipulated based on the existing delayed hydride cracking models. For example, the evaluation of flaw-tip hydride precipitation during reactor cooldown involves a procedure to calculate the equilibrium hydrogen equivalent concentration in solution at the flaw tip, Htipas follows: Htip=Hfexp[- (VH delta no.)/RT], where Hf is the total bulk hydrogen ...

2007-05-10

441

A 5{sup th} generation Ni-base single crystal superalloy with superior elevated temperature properties  

Energy Technology Data Exchange (ETDEWEB)

The National Institute of Materials Science (NIMS) has utilized the in-house alloy design program to develop a 5{sup th} generation Ni-base single crystal superalloy, TMS-196 with superior high temperature creep, thermo mechanical fatigue (TMF) and oxidation resistance by incorporating further ruthenium (Ru) and chromium (Cr) content over the compositions of 4{sup th} generation superalloys. With Ru additions in advanced superalloys to enhance phase stability, higher content of refractory elements can be accommodated to provide further strengthening; the associated oxidation resistance can be improved by the increase in Cr additions. In present article, TMS-196 has been subjected to cyclic/isothermal oxidation tests at 1100 C and 900 C, creep at conditions between 800 C{proportional_to}1100 C/137MPa{proportional_to}735MPa and TMF cycles. Preliminary studies indicate that the surface of oxidized TMS-196 can exhibit continuous alumina layer ...

2006-07-01

442

The non-linear fitting method to analyze the measured M-S plots of bipolar passive films  

Energy Technology Data Exchange (ETDEWEB)

Mott-Schottky (M-S) analysis is an effective approach to investigate the electronic property of passive films of metals, and it is well suitable for the passive film with single space charge capacitance. But there is no proper method to analyze the C{sub sc}{sup -2} vs. V{sub m} plots of passive films with several space charge capacitances in series connection, such as bipolar passive films. In this paper, the relationship between the space charge capacitance of the bipolar passive film and the applied potential was deduced and the features of corresponding plots were given out simultaneously. Accordingly, a non-linear fitting method was presented to analyze the C{sub sc}{sup -2} vs. V{sub m} plots of bipolar passive films. Then the method was used to study the semiconductor characteristics of bipolar passive films formed on the surface of Nickel base alloy after being corroded in the environments with high temperatures and high partial pressures of H{sub ...

2010-02-28

443

The non-linear fitting method to analyze the measured M-S plots of bipolar passive films  

International Nuclear Information System (INIS)

Mott-Schottky (M-S) analysis is an effective approach to investigate the electronic property of passive films of metals, and it is well suitable for the passive film with single space charge capacitance. But there is no proper method to analyze the Csc-2 vs. Vm plots of passive films with several space charge capacitances in series connection, such as bipolar passive films. In this paper, the relationship between the space charge capacitance of the bipolar passive film and the applied potential was deduced and the features of corresponding plots were given out simultaneously. Accordingly, a non-linear fitting method was presented to analyze the Csc-2 vs. Vm plots of bipolar passive films. Then the method was used to study the semiconductor characteristics of bipolar passive films formed on the surface of Nickel base alloy after being corroded in the environments with high temperatures and high partial pressures of H2S/CO2. The fitting results indicate that the ...

2010-02-28

444

Properties of superconducting Cu-rich composites containing V_3Si or V_3Ga  

International Nuclear Information System (INIS)

Superconducting Cu-rich composites containing the A-15 compounds V_3Si or V_3Ga were made by the ''Tsuei'' process (melting into ingots followed by cold working and heat treatment). Superconducting transition temperatures of the composites were measured. X-ray diffraction analyses were performed. Microstructures were studied using both the optical metallograph and the scanning electron microscope. For some composites containing V_3Ga, the critical current densities as functions of transverse magnetic field up to 60 kG, and as functions of temperature from 4.2 to 12"0K were measured. It was found that the Tsuei process does not work for the composites containing V_3Si, but works satisfactorily for V_3Ga; reasons are discussed. Relations between measured properties and various metallurgical factors such as alloy compositions, cross-section reduction ratios, and heat treatment are discussed. The mechanism for the observed superconductivity in the ...

445

Precipitation during controlled cooling of magnesia-partially-stabilized zirconia  

Energy Technology Data Exchange (ETDEWEB)

A study has been made of the precipitation and growth processes which occur during cooling from solution treatment and under isothermal hold conditions in a magnesia-partially-stabilized zirconia alloy. Three types of precipitate have been identified which develop during cooling or during isothermal hold treatments just above and below the eutectoid temperature. These precipitate forms are termed (i) primary, (ii) large random, and (iii) secondary. Further precipitation, slow growth of existing precipitates, and subeutectoid decomposition result when an additional 1100/sup 0/C aging treatment is given to the previously cooled material. It is shown that type (iii) secondary precipitates from rapidly within the temperature range of 1300/sup 0/ to 1375/sup 0/C. The secondary precipitates are largely responsible for the improved room-temperature strength properties of the heat-treated samples. The formation and effects on mechanical properties of ...

1986-07-01

446

Precipitation during controlled cooling of magnesia-partially-stabilized zirconia  

International Nuclear Information System (INIS)

A study has been made of the precipitation and growth processes which occur during cooling from solution treatment and under isothermal hold conditions in a magnesia-partially-stabilized zirconia alloy. Three types of precipitate have been identified which develop during cooling or during isothermal hold treatments just above and below the eutectoid temperature. These precipitate forms are termed (i) primary, (ii) large random, and (iii) secondary. Further precipitation, slow growth of existing precipitates, and subeutectoid decomposition result when an additional 1100"0C aging treatment is given to the previously cooled material. It is shown that type (iii) secondary precipitates from rapidly within the temperature range of 1300"0 to 1375"0C. The secondary precipitates are largely responsible for the improved room-temperature strength properties of the heat-treated samples. The formation and effects on mechanical properties of each type of ...

447

Plastic zone and pileup around large indentations  

International Nuclear Information System (INIS)

Mechanical properties of cold-worked molybdenum, grade 4 titanium, and an #alpha#-#beta# titanium alloy are measured with tensile tests and by indentations using conical indenters with 105, 120, and 137 deg included angles. The extent of plastic deformation and pileup around an indentation is measured using profilometry. Various models predicting the extent of plastic deformation and pileup are compared to the actual measured values. As inferred from indentation, the calculated yield strength of the material from the mean pressure does not correlate well to the yield strength measured by tensile testing. The plastic zone size surrounding an indentation can also be used to determine the yield strength of the material, and this does correlate to the yield strength measured by tensile tests. Furthermore, the extent of plastic deformation is relatively independent of the included angle of the indenter for the range of materials used in this system. ...

448

Photoelectrochemistry of disordered passive films  

Energy Technology Data Exchange (ETDEWEB)

A theoretical model, which describes subband gap photoexcitation involving localized electronic states, was developed. The escape probability of a charge carrier trapped in a localized state is considered via Poole-Frenkel, direct tunneling, or phonon-assisted tunneling processes, as competing escape mechanisms. Photoelectrochemical experiments were performed on the passive films formed on zirconium and amorphous iron-zirconium alloys and on pure HfO/sub 2/ films and HfO/sub 2/ films implanted with varying concentrations of xenon. These films were found to possess some degree of disorder depending on the substrate, the thickness of the film, and the extent of implantation. The spectral dependence of the photocurrent in all of the films studied is considerably different from what was found for crystalline passive films. The potential dependence of the photocurrent yields Poole-Frenkel behavior. Reverse tunneling processes were also observed at ...

1987-01-01

449

Microstructure and magnetic properties of nanocrystalline Fe75Si20M5 (M = Al, B, Cr) powders  

International Nuclear Information System (INIS)

Nanocrystalline Fe75Si20M5 (M = Al, B and Cr) powders were synthesized by mechanical alloying in a planetary ball mill from high purity elemental powders. Evolution of non-equilibrium solid solutions of ?-Fe[Si,(Al, B, Cr)] with a nanocrystalline structure was accompanied by the introduction of a large number of dislocation defects in the course of the milling process. Fe sites get substituted by Si and M (M = Al, B, Cr) atoms during the milling process. The structural change and the resulting disorder are reflected in the changes in the lattice parameter and average magnetic moment of the powders milled for various time periods. The effective magnetic anisotropy increases linearly with the milling time. An increase in coercivity with increasing milling time was observed which could be attributed to the introduction of dislocations and the reduction in the powder particle size during milling. The presence of dislocations and grain boundaries ...

2008-08-21

450

Manufacturing of small scale W monoblock mockups by hot radial pressing  

International Nuclear Information System (INIS)

In the frame of the European Technology R and D programme for International thermonuclear experimental reactor (ITER) and in the area of high heat flux plasma facing components (HHFC), representative small-scale mock-ups were manufactured and tested to compare different concepts and joining technologies (i.e. active brazing, hot isostatic pressing (HIPping), diffusion bonding, etc.). On the basis of the results obtained by thermal fatigue tests, the monoblock concept resulted to be the most robust one, particularly when the HIPping manufacturing technology is used. Within this programme, ENEA developed an alternative technique for manufacturing plasma-facing components with a monoblock geometry of the ITER machine. The basic idea of this technique, named hot radial pressing (HRP), is to perform a radial diffusion bonding between the cooling tube and the armour tile by pressurising the internal tube only and by keeping the process parameters within the range in which the ...

2003-09-01

451

Long-life bismuth liquid metal ion source for focussed ion beam micromachining application  

International Nuclear Information System (INIS)

Liquid metal ion sources (LMISs) with Ga as ion species are widely used in focused ion beam (FIB) technology for micromachining and surface treatment on the sub-micron and nano-scale. Key features of a LMIS for investigating mechanical properties and 3D-microfabrication of materials are long life-time, high brightness, stable ion current and a highly effective milling ability for the material to be modified. In order to increase the material removal rate, heavier ions than Ga and their clusters should be applied. Bismuth (Bi) is the heaviest, non-radio-active element in the periodic table, is non-toxic and exhibits a low melting point. We have thus produced a long-life (about 1000 h) Bi LMIS with a good beam performance, applicable in any FIB system. Since Bi is the only element in this source, it is not necessary to separate it from other ions by a mass filter. Investigation of the sputtering rate of NiTi shape memory alloys using Ga and Bi ...

2008-09-15

452

Leading research on supermetal. Part 1. Large-scale materials (iron system); Super metal no sendo kenkyu. 1. Ogata sozai (tetsukei)  

Energy Technology Data Exchange (ETDEWEB)

Supermetal with critical characteristics is under advanced investigation for further improvement of metal materials. Although iron is most frequently used as structural material among various metals, it should be used more carefully and effectively because of resource limitation and global environmental problem. It is essential to draw various excellent properties much more from iron and to improve recyclability. In particular, the best way to meet these requirements is achievement of more fine structure and higher purity. Since the lowest crystalline grain size is now limited to nearly 10{mu}m, metallic structure composed of grains below 1{mu}m is expected by mesoscopic control. Various methods have been studied to achieve ultra-fine crystalline structure, and study of precise heat treatment control and ultra-strength metallurgy is required. Heat treatment in magnetic field and layered structure by mechanical alloying are also promising. ...

1996-03-01

453

Interface-induced conversion of infrared to visible light at semiconductor interfaces  

Science.gov (United States)

Efficient, low-temperature conversion of infrared light into visible light (red, orange, green) is reported at single heterojunctions and undoped quantum wells of GaAs and ordered Al{sub {ital x}}Ga{sub 1{minus}{ital x}}InP{sub 2}; an increase in photon energy of 700 meV is obtained. The signal originates from the high-band-gap layers and disappears only if the excitation energy is tuned below the GaAs band gap. The intensity of the up-converted photoluminescence (PL) is found to decrease significantly slower with increasing temperature than that of the regular PL and it remains observable up to 200 K. Interface-induced cold Auger processes along with the presence of trapped states for both electrons and holes in these ordered alloys account for this nonlinear mechanism. A colinear double-beam experiment confirms this. {copyright} {ital 1996 The American Physical Society.}

1996-08-01

454

Inhibition of corrosion resistant alloys in hot hydrochloric acid solutions  

Energy Technology Data Exchange (ETDEWEB)

Weight loss measurements were performed in 20% and 28% hydrochloric acid at 90/sup 0/C on carbon steel, 22Cr5Ni duplex stainless steel, and two superaustenitic steels - 27Cr31Ni3Mo and 19Cr25Ni4Mo -, in presence of organic substances used singly or mixed. The organic substances examined were quaternary ammonium salts (1-4-pyridyl)-pyridinium chloride hydrochloride, dodecylpyridiniumchloride, benzyldimethylstearylammonium chloride, and dodecyltrimethylammonium bromide), alkynols (1-octyn-3-ol, propargyl alcohol) and trans-cinnamaldehyde. The synergistic effect of potassium iodide on the inhibitive efficiency of the organic substances was studied. The variations of corrosion rate during the test time (normally six hours) were recorded by means of polarization resistance measurements. Polarization curves were also recorded. The results showed that the corrosion rates of the four steels examined can be reduced to less than 1 mg/cm/sup -2/ . h/sup -1/ using ternary inhibitor mixtures ...

1988-12-01

455

Indentation plastic displacement field: Part II. The case of hard films on soft substrates  

Energy Technology Data Exchange (ETDEWEB)

The plastic displacements around Knoop indentations made in hard titanium/aluminum multilayered films on soft aluminum alloy substrates have been studied. Indentations were cross-sectioned and imaged using the focused-ion-beam (FIB) milling and high-resolution scanning electron microscopy (SEM), respectively. The FIB milling method has the advantage of removing material in a localized region without producing mechanical damage to the specimen. The micrographs of the cross-sectioned indentations indicate that most of the plastic deformation around the indentation is dominated by the soft aluminum substrate. There is a very small change in the multilayered film thickness around the indentation{emdash}less than 10{percent}. The plastic deformation of the thin film resembles a membrane being deflected by a localized pressure gradient across the membrane. Stress-induced voids are also observed in the multilayered film, especially in the area around ...

1999-06-01

456

High temperature strengthening mechanism of hafnium carbide in a tungsten-rhenium matrix  

Energy Technology Data Exchange (ETDEWEB)

The interrelationship between the testing temperature and HfC strength increment of an arc-melted W-3.6Re-0.4HfC was determined from 1950 K to 2980 K in a vacuum of better than 1.3{times}10{sup {minus}5} Pa (10{sup {minus}7} torr). The present research was focused on the characteristic temperature at which the rapid coarsening of HfC particles occurred and the effect of the second-phase particle size on the high temperature strength properties of this material. It was found that the HfC particle strengthening was effective in a W-Re matrix up to a characteristic temperature of 2450 K in the short-term tensile test. Carbon was found to be the rate-limiting solute in the HfC particle growth. The strength of HfC strengthened alloy at temperature above 0.5 T{sub m} is proportional to the square root of particle volume fraction. The yield strengths of W-3.6Re-0.26HfC calculated based on the particle statistical distribution had good agreement with the experimental ...

1991-01-01

457

High temperature strengthening mechanism of hafnium carbide in a tungsten-rhenium matrix  

International Nuclear Information System (INIS)

The interrelationship between the testing temperature and HfC strength increment of an arc-melted W-3.6Re-0.4HfC was determined from 1950 K to 2980 K in a vacuum of better than 1.3x10"-"5 Pa (10"-"7 torr). The present research was focused on the characteristic temperature at which the rapid coarsening of HfC particles occurred and the effect of the second-phase particle size on the high temperature strength properties of this material. It was found that the HfC particle strengthening was effective in a W-Re matrix up to a characteristic temperature of 2450 K in the short-term tensile test. Carbon was found to be the rate-limiting solute in the HfC particle growth. The strength of HfC strengthened alloy at temperature above 0.5 T_m is proportional to the square root of particle volume fraction. The yield strengths of W-3.6Re-0.26HfC calculated based on the particle statistical distribution had good agreement with the experimental values from 1950 K to 2980 K. ...

1991-01-06

458

High temperature mechanical properties of a {beta}-Si{sub 3}N{sub 4} whisker reinforced aluminium alloy composite produced by squeeze casting  

Energy Technology Data Exchange (ETDEWEB)

The {beta}-Si{sub 3}N{sub 4}w/6061 Al composite was fabricated by the squeeze casting and extruded with the extrusion ratios of 44 and 100 at 773 K. Its tensile strength and superplastic characteristics were investigated and the following results were obtained: (1) the {beta}-Si{sub 3}N{sub 4}w/6061 Al composite exhibits the tensile strengths of about 400 MPa at room temperature and of about 250 MPa at 773 K; (2) the m value of the composite pulled at 818 K is 0.33 in the strain rate range from 0.02 up to 1.0 s{sup {minus}1}; (3) the total elongation of the composite becomes about 173 % at the strain rate of 0.02 s{sup {minus}1} even in the case of the high volume fraction of 0.25; (4) no reaction product on the surface of {beta}-Si{sub 3}N{sub 4} whisker after removing a matrix by etching was detected except AlN; (5) the fracture surface of the composite includes the melt matrix and small filaments, which shows that interfacial sliding should promote HSRS in addition to fine grain ...

1995-06-01

459

Focused ion-beam line profiles: A study of some factors affecting beam broadening  

Energy Technology Data Exchange (ETDEWEB)

The current--density profile of a focused ion beam (FIB) has a central peak accompanied by broader ``wings`` that, while unimportant in lithographic applications, can lead to unwanted effects during an implantation operation. The origin of the wings, and hence the best way to minimize them, is not clear and needs further study. We have measured the line profiles of several of the ions available in our FIB machine as a function of a number of variables, under ultrahigh vacuum (UHV) conditions. No effects are observed from changes in emission current or deliberate defocusing of the objective lens. There are some changes with beam aperture and/or current, but the biggest differences seem to be associated with a change of source type and hence, possibly, with a change in the source/extractor configuration or in the alloy and the emission process. The wing amplitudes are appreciably lower than many previously observed, and their profiles, at least for the lighter ions ...

1995-11-01

460

Focused ion-beam line profiles: A study of some factors affecting beam broadening  

International Nuclear Information System (INIS)

The current--density profile of a focused ion beam (FIB) has a central peak accompanied by broader ''wings'' that, while unimportant in lithographic applications, can lead to unwanted effects during an implantation operation. The origin of the wings, and hence the best way to minimize them, is not clear and needs further study. We have measured the line profiles of several of the ions available in our FIB machine as a function of a number of variables, under ultrahigh vacuum (UHV) conditions. No effects are observed from changes in emission current or deliberate defocusing of the objective lens. There are some changes with beam aperture and/or current, but the biggest differences seem to be associated with a change of source type and hence, possibly, with a change in the source/extractor configuration or in the alloy and the emission process. The wing amplitudes are appreciably lower than many previously observed, and their profiles, at least for the lighter ions ...

461

Fabrication, structure and consolidation of NiAl-Al_2O_3 mechanically alloyed nanocomposite powders  

International Nuclear Information System (INIS)

Reactive milling of NiO + Al powder mixture resulted in the formation of NiAl-Al_2O_3 nanocomposite powders, with a crystallite size of about 20 nm. The Hall-Williamson analysis revealed that NiAl showed an orientation dependent crystallite size after short processing time and orientation dependent internal strain after long milling time. Both anisotropies were removed by heating the powders in the differential scanning calorimetry. Calorimetric studies showed one exothermic effect attributed to the reduction reaction of NiO and endothermic one associated with melting of Al. Two methods were applied for powders compaction: resistance sintering and pulse electric discharge. In both cases the densities of abut 90% of the theoretical value were achieved. A significant increase in average NiAl crystallites size in compacted samples was observed, up to several hundreds of nanometers.(author)

2001-09-23

462

Enhancement of surface properties of 45{number_sign} steel using plasma immersion ion implantation  

Energy Technology Data Exchange (ETDEWEB)

45{number_sign} steel, which has good mechanical strength and is relatively cheap, is a common constituent in industrial components, such as precision gears, piston columns of oil pumps, and so on. However, since the working environment of these industrial parts is sometimes quite harsh and unforgiving, they are vulnerable to wear and corrosion. Replacing 45{number_sign} steel with stainless or alloy steel increases the cost significant, and a better alternative is to improve its surface properties and lifetime using plasma immersion ion implantation (PIII). The authors have devised a variety of treatment processes using PIII, including radio-frequency (RF) plasma nitriding, RF plasma nitriding and nitrogen PIII, Ti deposition in conjunction with nitrogen PIII (IBED), as well as Cr deposition followed by nitrogen PIII (IBED). To assess the efficacy of the processes, the microhardness and mass loss due to wear were measured for both the ...

1997-12-31

463

Effects of composition and temperature on irradiation hardening of pressure vessel steels  

International Nuclear Information System (INIS)

The effects of key metallurgical variables on the low fluence hardening in a set of A533B model steels were evaluated over a wide range of irradiation temperatures. Above about 163 degrees C hardening increased with higher copper and nickel contents, as is typical of the pressure vessel operating regime around 290 degrees C. However, at 121 degrees C the hardening was generally lower and unaffected by copper and nickel variations. This observation of decreased hardening with lower temperature (e.g. an open-quotes invertedclose quotes temperature dependence) is tentatively attributed to a reduced contribution of copper precipitation. Tensile data for a set of commercial steels with a range of (uncontrolled) compositions also showed minimal sensitivity to copper variations at 121 degrees C. Unlike the hardness data no systematic reductions in the yield stress increases were observed between 163 and 121 degrees C. However, the ultimate tensile strength did decrease at the lower ...

1991-08-25

464

Development of structural steels for nuclear application - Enhancement of corrosion resistance of stainless steels for nuclear power plant  

Energy Technology Data Exchange (ETDEWEB)

Fe-Cr-Mn stainless steel is one of the candidate materials for the 1`st wall materials and structural applications of fusion reactor as regards reduced radioactivation properties than Fe-Cr-Ni austenitic stainless steels. This report deals with the effects of annealing and aging heat treatment on the microstructure, mechanical properties and corrosion resistance of Fe-Cr-Mn alloys varying Mn and W contents, which were made using vacuum high frequency induction furnace. Increasing Mn contents, austenite phase was increased, and maximum .epsilon. martensite phase was formed at about 21% Mn. W-addition made small amount of ferrite phase in the matrix, and the ferrite contents were increased with raising annealing temperature. Increased Mn contents reduced tensile stress and yield stress but increased the elongation. W-addition raised the high temperature tensile properties. The variation of Mn contents had no influenced on corrosion resistance. ...

1996-07-01

465

Corrosion control. 2. ed.  

International Nuclear Information System (INIS)

The purpose of this text is to train engineers and technologists not just to understand corrosion but to control it. Materials selection, coatings, chemical inhibitors, cathodic and anodic protection, and equipment design are covered in separate chapters. High-temperature oxidation is discussed in the final two chapters ne on oxidation theory and one on controlling oxidation by alloying and with coatings. This book treats corrosion and high-temperature oxidation separately. Corrosion is divided into three groups: (1) chemical dissolution including uniform attack, (2) electrochemical corrosion from either metallurgical or environmental cells, and (3) stress-assisted corrosion. Corrosion is logically grouped according to mechanisms rather than arbitrarily separated into different types of corrosion as if they were unrelated. For those university students and industry personnel who approach corrosion theory very hesitantly, this text will present ...

466

Corrosion control. 2. ed  

Energy Technology Data Exchange (ETDEWEB)

The purpose of this text is to train engineers and technologists not just to understand corrosion but to control it. Materials selection, coatings, chemical inhibitors, cathodic and anodic protection, and equipment design are covered in separate chapters. High-temperature oxidation is discussed in the final two chapters ne on oxidation theory and one on controlling oxidation by alloying and with coatings. This book treats corrosion and high-temperature oxidation separately. Corrosion is divided into three groups: (1) chemical dissolution including uniform attack, (2) electrochemical corrosion from either metallurgical or environmental cells, and (3) stress-assisted corrosion. Corrosion is logically grouped according to mechanisms rather than arbitrarily separated into different types of corrosion as if they were unrelated. For those university students and industry personnel who approach corrosion theory very hesitantly, this text will present ...

2001-07-01

467

Crack growth behaviour of low alloy steels for pressure boundary components under transient light water reactor operating conditions (CASTOC)  

Energy Technology Data Exchange (ETDEWEB)

The CASTOC project addresses environmentally assisted cracking (EAC) phenomena in low alloy steels used for pressure boundary components in both Western type boiling water reactors (BWR) and Russian type pressurised water reactors (VVER). It comprises the four work packages (WP): inter-laboratory comparison test (WP1); EAC behaviour under static load (WP2), EAC behaviour under cyclic load and load transients (WP3); evaluation of the results with regard to their relevance for components in practice (WP4). The use of sophisticated test facilities and measurement techniques for the on-line detection of crack advances have provided a more detailed understanding of the mechanisms of environmentally assisted cracking and provided quantitative data of crack growth rates as a function of loading events and time, respectively. The effect of several major parameters controlling EAC was investigated with particular emphasis on the transferability of the ...

2004-07-01

469

Stress Corrosion Cracking Susceptibility of Beta Titanium Alloy 38-6-44: Candidate Alloy for Scout Torsion Bar.  

Science.gov (United States)

The threshold stress itensities for stress corrosion crack propagation in beta titanium alloy 38-6-44, Ti-3Al-8V-6Cr-4Mo-4Zr, has been determined in salt water and methanolic solutions. The alloy was immune to stress corrosion cracking in aqueous sodium c...

1974-01-01

470

Review of the corrosion resistance properties of Alloy 800 in high-temperature steam  

International Nuclear Information System (INIS)

The investigations carried out on Alloy 800 in aqueous high-temperature environments in France as well as in other countries are reviewed. These studies are mainly concerned with nuclear industry where Alloy 800 can be used as structural material for steam generators of PWR, breeders or HTR. As results referred to in the literature on cracking in caustic environmens do not always agree, a discussion is presented on the matter. The behaviour of Alloy 800 in superheated steam is examined. (Auth.).

471

Reactivity of ceramic superconductors with palladium alloys  

Science.gov (United States)

This paper reports Palladium alloy compositions investigated for suitability as a nonreactive material for the processing of ceramic superconductors. Barium-based superconductors were tested on Pd-Au and Pd-Ag alloys for reactivity. Bismuth-based superconductors were tested on a Pd-Ag alloy. The least reactive was found to be 70% Pd-30% Ag for the barium-based high-temperature superconductors (HTSC), whereas 30% Pd-70% Ag was found to be least reactive for bismuth-based HTSC.

1990-06-01

472

Postweld aging of a metastable beta-titanium alloy  

International Nuclear Information System (INIS)

(Nov 1973). United States Greenfield, MA Pierce, CM Chicago, IL.

477

General corrosion of ALLOY 800 in high temperature water and its prevention  

Energy Technology Data Exchange (ETDEWEB)

General corrosion behavior of ALLOY 800 in high temperature water was studied in relation to its surface film structure. The surface film formed in water was found to decrease the corrosion rate of ALLOY 800. This film is composed of Ni ferrite, and can be obtained by oxidation in air or steam. Based on these results, air or steam oxidation treatment to inhibit Ni and Co release of ALLOY 800 into high temperature water is proposed. (author).

1989-10-01

478

General corrosion of ALLOY 800 in high temperature water and its prevention  

International Nuclear Information System (INIS)

General corrosion behavior of ALLOY 800 in high temperature water was studied in relation to its surface film structure. The surface film formed in water was found to decrease the corrosion rate of ALLOY 800. This film is composed of Ni ferrite, and can be obtained by oxidation in air or steam. Based on these results, air or steam oxidation treatment to inhibit Ni and Co release of ALLOY 800 into high temperature water is proposed. (author).

481

Effect of aging on the pitting corrosion behavior in Al-Li alloys  

Energy Technology Data Exchange (ETDEWEB)

In the present work, electrochemical measurements and corrosion tests in NaCl solutions were carried out to study the effect of aging treatments on pitting corrosion behavior in a 8090 alloy and its high purity Al-Li binary alloy analogue. The pitting corrosion characteristics and corrosion resistance of the 8090 alloy have been determined in relation to precipitation microstructures. (orig.).

1990-06-01

482

EFFECT OF MICROSTRUCTURE ON THE STRENGTH ...  

Science.gov (United States)

... THE STRENGTH, TOUGHNESS, AND STRESS-CORROSION CRACKING SUSCEPTIBILITY OF A METASTABLE BETA TITANIUM ALLOY (Ti-11. ...

1970-02-01

483

Direct production of niobium titanium alloy during niobium reduction  

International Nuclear Information System (INIS)

This paper describes a process for the direct production of a superconductive niobium-titanium alloy during reduction of niobium pentoxide. It comprises: mixing at least one of titanium metal powder and titanium dioxide powder with niobium pentoxide powder and aluminum powder; heating the resulting mixture to form a niobium-titanium alloy and a slag consisting essentially of aluminum oxide; and separating the alloy and the slag.

1989-10-26

484

Corrosion resistance of zinc coatings on depleted uranium and uranium alloys  

Energy Technology Data Exchange (ETDEWEB)

Simulated atmospheric corrosion studies were performed to determine the corrosion protection provided by galvanized zinc coatings on depleted uranium, U-0.75 Ti alloy, and U-6 Nb alloys. The accelerated ASTM tests consisted of exposing the galvanized samples to aqueous and aqueous chloride environments. The test results showed that anodic protection was provided by the electronegative zinc coatings on uranium and uranium alloys. Treating zinc with chromate conversion coatings also provided more protection.

1985-01-27

485

Ultra high strength beta titanium alloy for fasteners  

International Nuclear Information System (INIS)

A new high strength titanium alloy has been developed primarily intended for fastener applications. While Ti-6Al-4V is used extensively as a fastener alloy in the aerospace industry, its shear strength allowable is limited to 655 MPa (95 ksi). For higher shear strength requirements, various steels or nickel-based alloys are used (up to 860 MPa (125 ksi)), but with the attendant density penalty. This new alloy is intended to provide the 860 MPa shear strength at roughly a 40% weight savings. After screening various alloy systems, the optimum chemistry has been selected as follows: Ti-6.0V-6.2Mo-5.7Fe-3Al. In light of its 125 ksi shear strength goal, the alloy has been designated TIMETAL reg-sign 125.

1993-02-21

486

Tensile properties and bending formability of drawn magnesium alloy pipes  

Energy Technology Data Exchange (ETDEWEB)

Magnesium alloys are being increasingly utilized in a variety of fields as an alternative material to organic materials and aluminum alloys, owing to excellent properties. Those include low density, and excellent damping properties. When compared to organic materials, furthermore, Mg alloy excels at recyclability, heat radiation, and electromagnetic-shielding. Though most of magnesium alloy products are manufactured through die-casting and thixo-molding at present, the demand for the expanding of magnesium wrought alloy market is increasing. Taking full advantage of a drawing technique and applying it to the conventional extruded pipe, we have developed a new type of magnesium alloy pipe. The strength of the developed pipe is significantly higher than that of the conventional one, either extruded or die-casting. Some of the excellent properties were obtained ...

2003-07-01

487

Passivity of high corrosion resistant Cu-Al-Sn alloys  

Energy Technology Data Exchange (ETDEWEB)

In a work studying the corrosion and tarnishing properties of a variety of copper alloys, the alloy Cu-A110-Sn5 was found to show an excellent corrosion resistance in neutral solutions, where copper and most conventional Cu alloys are covered by thick nonprotective surface layers. The passive films formed on this alloy were characterized with electrochemical and photoelectrochemical methods. The pH dependence of the passivation and of the photocurrent behavior of the Cu-A110-Sn5 alloy clearly indicates that the passivity of this alloy in neutral solutions is due to a formation of passive film enriched with aluminum oxide. At corrosion potential a strong increase in the corrosion resistance with time is due to a gradual enrichment of the surface with aluminum oxide. This can be seen in the photocurrent spectra which change from cooper-type to aluminum-type with ...

1993-10-01

488

Fatigue of magnesium alloys  

Energy Technology Data Exchange (ETDEWEB)

Magnesium alloys show a high specific strength and are therefore increasingly used for light-weight constructions in transportation industry.{sup [1,2]} To predict the behaviour of the material under the influence of cyclic loading it is vital to understand the fatigue behaviour of magnesium alloys. Only when understood properly, it is possible to fully apply the potential weight reduction by using magnesium alloys. A very important aspect in fatigue of magnesium alloys is the influence of a corrosive media and elevated temperatures, of which both are relevant in automotive applications. These two factors tend to have deleterious effects on magnesium alloys and therefore also have to be considered in investigations on the fatigue behaviour of magnesium alloys. (Abstract Copyright [2004], Wiley Periodicals, Inc.)

2004-05-01

489

Summary of Dissimilar Metal Joining Trials Conducted by Edison Welding Institute  

International Nuclear Information System (INIS)

Under the direction of the NASA-Glenn Research Center, the Edison Welding Institute (EWI) in Columbus, OH performed a series of non-fusion joining experiments to determine the feasibility of joining refractory metals or refractory metal alloys to Ni-based superalloys. Results, as reported by EWI, can be found in the project report for EWI Project 48819GTH (Attachment A, at the end of this document), dated October 10, 2005. The three joining methods used in this investigation were inertia welding, magnetic pulse welding, and electro-spark deposition joining. Five materials were used in these experiments: Mo-47Re, T-111, Hastelloy X, Mar M-247 (coarse-grained, 0.5 mm to several millimeter average grain size), and Mar M-247 (fine-grained, approximately 50 (micro)m average grain size). Several iterative trials of each material combination with each joining method were performed to determine the best practice joining method. Mo-47Re was found to be joined easily to ...

490

Summary of Dissimilar Metal Joining Trials Conducted by Edison Welding Institute  

Energy Technology Data Exchange (ETDEWEB)

Under the direction of the NASA-Glenn Research Center, the Edison Welding Institute (EWI) in Columbus, OH performed a series of non-fusion joining experiments to determine the feasibility of joining refractory metals or refractory metal alloys to Ni-based superalloys. Results, as reported by EWI, can be found in the project report for EWI Project 48819GTH (Attachment A, at the end of this document), dated October 10, 2005. The three joining methods used in this investigation were inertia welding, magnetic pulse welding, and electro-spark deposition joining. Five materials were used in these experiments: Mo-47Re, T-111, Hastelloy X, Mar M-247 (coarse-grained, 0.5 mm to several millimeter average grain size), and Mar M-247 (fine-grained, approximately 50 {micro}m average grain size). Several iterative trials of each material combination with each joining method were performed to determine the best practice joining method. Mo-47Re was found to be joined easily to ...

2005-11-18

491

Re-formation and re-crystallisation behaviour of {gamma}`-free ODS nickel-based alloy PM 1000; Umform- und Rekristallisationsverhalten der {gamma}`-freien ODS Nickel-Basis-Legierung PM 1000  

Energy Technology Data Exchange (ETDEWEB)

The aim of this work was the examination of the coarse grain recrystallisation of the {gamma}-free ODS nickel-based alloy PM 1000 depending on the various parameters due to the processing during heat treatment. After isotropic hot compacting (HIP) of the mechanically alloyed powder, one observes a homogeneous sub-microscopic fine grain structure which can coarsen during high temperature heat treatment, due to sufficiently high driving force from the grain boundary energy via abnormal grain growth to 600 times its size. The setting of the elongated high temperature resistant recrystallisation structure is, however, not connected with this. The dependence of the sucess of re-crystallisation on the re-forming parameters (re-forming temperature and degree of re-forming) was shown by a socalled re-forming card. In order to achieve re-crystallisation to a coarse and aligned grain structure, apart from a certain absolute minimum ...

1996-05-01

492

Stress corrosion cracking susceptibility of #beta# titanium alloy 38-6-44  

International Nuclear Information System (INIS)

The threshold stress intensities for stress corrosion crack propagation in beta titanium alloy 38-6-44, Ti3Al-8V-6Cr-4Mo-4Zr, has been determined in salt water and methanolic solutions. The alloy was immune to stress corrosion cracking (SCC) in aqueous sodium chloride solutions (marine atmosphere). However, in methanolic solutions, the alloy was very susceptible to SCC. This marked susceptibility in methanolic solutions can be mitigated by the addition of an inhibitor: sodium nitrate. Crack extension in the alloy was transgranular and failure occurred by brittle quasi-cleavage in methanolic solutions.

493

Nature of the magnetic susceptibility of dysprosium. Paramagnetic susceptibility of dysprosium - yttrium alloys  

International Nuclear Information System (INIS)

The paramagnetic susceptibility of single crystals of dysprosium-yttirum alloys is measured in the basal plane and along the hexagonal axis. It is shown that the susceptibility of the alloys obeys the Curie-Weiss law, the effective magnetic moments allong the different directions being the same and the paramagnetic Curie temperatures being different. The difference between the paramagnetic Curie temperatures in the basal plane and along the hexagonal axis is independent of the dysprosium concentration in the alloy. As a comparison with the theoretical models of magnetic anisotropy shows, this is an indication that the magnetic anisotropy of dysprosium - yttrium alloys is of a single-ion nature.

1976-01-01

494

Friction stir welding of dissimilar formed Mg alloys (AZ31/AZ91)  

Energy Technology Data Exchange (ETDEWEB)

Friction stir welding of dissimilar formed Mg alloys(AZ31/AZ91) was successfully carried out at the limited welding conditions. In a sound joint, SZ was mainly consisted of AZ31 Mg alloy which was located the retreating side. Dynamic recrystallization and grain growth occurred and {beta} intermetallic compounds of AZ 91 Mg alloy was not observed in SZ. BM had a higher hardness than that of the weld zone. The fracture location was not weld zone but BM of the AZ91 Mg alloy in tensile test. (orig.)

2005-07-01

495

Time-temperature-precipitation and time-temperature-sensitization behavior of highly corrosion resistant nickel-chromium-molybdenum alloys. Das Zeit-Temperatur-Ausscheidungs- und das Zeit-Temperatur-Sensibilisierungs-Verhalten von hochkorrosionsbestaendigen Nickel-Chrom-Molybdaen-Legierungen  

Energy Technology Data Exchange (ETDEWEB)

The time-temperature-precipitation diagrams and the resulting time-temperature-sensitization diagrams have been established and are presented for today's current nickel-chromium-molybdenum alloys C-4, C-276, 22 and the recently developed alloy 59. Compared to those materials alloy 625 behaves differently due to its high niobium content. In addition, also the precipitation and sensitization of alloy G-3 has been established. Under the materials considered alloy C-276 has the strongest tendency to precipitate the intermetallics Mu and P together with the carbide M{sub 6}C at intermediate temperatures, followed by the alloys 22 and 59. The tendency to sensitization in the sense of the 50{mu}m (2 mils) intercrystalline penetration criterion when exposed to the ASTM G-28, method A test solution is greatest with alloy C-276, and decreases ...

1992-05-01

496

The effect of age hardening on creep crack growth in alloy 800  

International Nuclear Information System (INIS)

The creep crack growth properties of two versions of Alloy 800 have been compared at 500 and 600"0C in the Grade II condition in tests up to 10"4 hours duration. The two alloys were a low carbon alloy containing (wt.%) 0.024 C, 0.5 Ti, 0.3 Al (Alloy B) and a higher carbon alloy containing (wt.%) 0.038 C, 0.2-0.3 Ti, 0.2-3.0 Al (Alloy J). At 600"0C, Alloy B attained maximum age hardening in 10"2 hours, whereas J did not harden significantly in time up to 10"4 hours. Both alloys age hardened at 550"0C with Alloy J hardening more rapidly than B. The creep displacements and displacement rates in small compact tension specimens at 600"0C were smaller than Alloy B than in Alloy J. However, failure times were shorter in Alloy B because of lower ...

497

Investigation on corrosion and wear behaviors of nanoparticles reinforced Ni-based composite alloying layer  

Energy Technology Data Exchange (ETDEWEB)

In order to investigate the role of amorphous SiO{sub 2} particles in corrosion and wear resistance of Ni-based metal matrix composite alloying layer, the amorphous nano-SiO{sub 2} particles reinforced Ni-based composite alloying layer has been prepared by double glow plasma alloying on AISI 316L stainless steel surface, where Ni/amorphous nano-SiO{sub 2} was firstly predeposited by brush plating. The composition and microstructure of the nano-SiO{sub 2} particles reinforced Ni-based composite alloying layer were analyzed by using SEM, TEM and XRD. The results indicated that the composite alloying layer consisted of {gamma}-phase and amorphous nano-SiO{sub 2} particles, and under alloying temperature (1000 deg. C) condition, the nano-SiO{sub 2} particles were uniformly distributed in the alloying layer and still kept the amorphous structure. ...

2008-04-30

498

Investigation on corrosion and wear behaviors of nanoparticles reinforced Ni-based composite alloying layer  

International Nuclear Information System (INIS)

In order to investigate the role of amorphous SiO2 particles in corrosion and wear resistance of Ni-based metal matrix composite alloying layer, the amorphous nano-SiO2 particles reinforced Ni-based composite alloying layer has been prepared by double glow plasma alloying on AISI 316L stainless steel surface, where Ni/amorphous nano-SiO2 was firstly predeposited by brush plating. The composition and microstructure of the nano-SiO2 particles reinforced Ni-based composite alloying layer were analyzed by using SEM, TEM and XRD. The results indicated that the composite alloying layer consisted of ?-phase and amorphous nano-SiO2 particles, and under alloying temperature (1000 deg. C) condition, the nano-SiO2 particles were uniformly distributed in the alloying layer and still kept the amorphous structure. The corrosion resistance of composite ...

2008-04-30

499

Weld integrity of the superconducting cable aluminium jackets of W7-X  

Energy Technology Data Exchange (ETDEWEB)

The Wendelstein 7-X (W7-X) modular stellarator is under construction at the Max-Planck-Institut fuer Plasmaphysik in Greifswald, Germany. The W7-X magnet system contains 70 coils made up from helium cooled superconducting cables in aluminium alloy (EN AW-6063) jackets. Several hundred connections of the jacket to the cable joints are made by aluminium-to-aluminium welds. Due to geometrical and thermal boundary conditions these welds cannot be accomplished free from defects. Microscopic analyses of the welds show that a variety of small flaws such as cracks and pores develop during welding. The welds have thus to be dimensioned accordingly, and appropriate weld qualification, investigation and testing has to be done in order not to jeopardise the structural integrity and leak tightness. The weld is mechanically loaded during cool-down due to the difference in thermal contractions between the GRP insulation and the aluminium, and during operation ...

2009-06-15