WorldWideScience
1

Beam Diagnostic System for High Intensity Proton Linac at KAERI  

CERN Document Server

Beam Diagnostic System for High Intensity Proton Linac at KAERI

2003-01-01

2

Behavior of Stress-Relaxation phenomena in Zr-1.1Nb-0.05Cu  

International Nuclear Information System (INIS)

Zirconium alloys have anisotropic mechanical properties depending on their physical orientations and are widely used as nuclear materials such as cladding tube material. An operation condition of the nuclear reactor requires a high creep resistance, because it is subjected to long period operations, high temperature and high pressure. Generally, it takes a few days or months to do the creep experiment, so it is difficult to get a data in short period. However, there is a way to predict a creep property by using the stress-relaxation in the short term. These studies realized the stress-relaxation through a compressive test of HANA-6 (Zr-1.1Nb-0.05Cu) alloy that was developed by KAERI (Korea Atomic Energy Research Institute), and then predicted the creep property

2010-10-01

3

Inhibitor effect on corrosion of titanium alloys in muriatic solutions of titanium-magnesium production  

International Nuclear Information System (INIS)

Corrosion tests of titanium alloys VTI-0, OT4, VT5-1 and steel Kh18N1OT in 10% and 18% HCl with additions of carnallite at 40 deg C have been carried out. It has been established that titanium alloys in 10% and 18% HCl containing 5 and 10% carnallite are sufficiently corrosion resistant in the presence of 0.1-1% FeCl or HNO_3 and can be used for manufacturing the equipment of recirculation gas scrubbers. Steel Kh18N10T is unstable in all the media tested. It is subjected to intensive pitting. Specimens of steel Kh18N10T have also revealed edge cracking.

4

Characterization and Wear Behavior of Plasma Nitrided Nickel Based Dental Alloy  

British Library Electronic Table of Contents (United Kingdom)

In the present work, the plasma nitriding behavior of a nickel based dental alloy was investigated. Plasma nitriding experiments carried out under constant gas mixture (15% H2?85% N2) for different process parameters including time (4, 6, 10, and 20?h) and temperature (400, 450, 500, and 550??C). Depending on nitriding parameters, it was found that triple or double layers formed on the surface of the samples. Increasing of treatment time and temperature has resulted in a double layer. ?N1 layer was in formed all nitrided samples. However, ?N2 layer is formed only at low temperatures and in short times. Layer growth of nickel based alloys increases until a critical time or a critical temperature reached. Above these critical values, it is observed that the layer thickness decreases. It was ...

2011-01-01

5

FEM Analysis and Measurement of Residual Stress by Neutron Diffraction on the Dissimilar Overlay Weld Pipe  

International Nuclear Information System (INIS)

Much research has been done to estimate the residual stress on a dissimilar metal weld. There are many methods to estimate the weld residual stress and FEM (Finite Element Method) is generally used due to the advantage of the parametric study. And the X-ray method and a Hole Drilling technique for an experimental method are also usually used. The aim of this paper is to develop the appropriate FEM model to estimate the residual stresses of the dissimilar overlay weld pipe. For this, firstly, the specimen of the dissimilar overlay weld pipe was manufactured. The SA 508 Gr3 nozzle, the SA 182 safe end and SA376 pipe were welded by the Alloy 182. And the overlay weld by the Alloy 52M was performed. The residual stress of this specimen was measured by using the Neutron Diffraction device in the HANARO (High-flux Advanced Neutron Application ReactOr) research reactor, KAERI (Korea Atomic Energy Research Institute). Secondly, FEM ...

2010-10-01

6

XPS study of the passive films formed on nitrogen-implanted austenitic stainless steels  

Energy Technology Data Exchange (ETDEWEB)

Austenitic stainless steels (304-type) have been implanted with nitrogen ions in order to investigate the effects of implanted nitrogen on their electrochemical behaviour and on the nature of the passive film formed on the steels in acid (0.5M H{sub 2}SO{sub 4}). Alloys with two nitrogen doses have been prepared (2.5x10{sup 16} and 2x10{sup 17} N atoms/cm{sup 2}). The implanted alloys have been characterized by {sup 15}N-NRA (nuclear reaction analysis) and XPS (X-ray photoelectron spectroscopy). Alloy surfaces with well-defined N concentrations were prepared, prior to the electrochemical measurements, by argon-ion sputtering of the implanted material for a fixed time in order to reach a well-defined point on the nitrogen depth profile. The samples were then transferred without exposure to air to an electrochemical cell mounted in an inert gas glove box. The implanted nitrogen modifies the electrochemical behaviour of the ...

1992-05-01

7

XPS study of the passive films formed on nitrogen-implanted austenitic stainless steels  

International Nuclear Information System (INIS)

Austenitic stainless steels (304-type) have been implanted with nitrogen ions in order to investigate the effects of implanted nitrogen on their electrochemical behaviour and on the nature of the passive film formed on the steels in acid (0.5M H_2SO_4). Alloys with two nitrogen doses have been prepared (2.5x10"1"6 and 2x10"1"7 N atoms/cm"2). The implanted alloys have been characterized by "1"5N-NRA (nuclear reaction analysis) and XPS (X-ray photoelectron spectroscopy). Alloy surfaces with well-defined N concentrations were prepared, prior to the electrochemical measurements, by argon-ion sputtering of the implanted material for a fixed time in order to reach a well-defined point on the nitrogen depth profile. The samples were then transferred without exposure to air to an electrochemical cell mounted in an inert gas glove box. The implanted nitrogen modifies the electrochemical behaviour of the alloy. ...

1992-01-01

8

Experience of HWR nuclear fuel fabrication technology development in Korea  

Energy Technology Data Exchange (ETDEWEB)

Since January, 1981, the project of development of nuclear fuel fabrication technology for Wolsung reactor (CANDU type) was undertaken by KAERI(Korea Advanced Energy Research Institute) and successfully fulfilled with loading 24 fuel bundles made by KAERI in Wolsung reactor in September, 1984. On the basis of this accumulated technology and experience, mass production plan to supply all the nuclear fuels for Wolsung reactor is under way. In this presentation, the Korean experience in the development of the nuclear fuel fabrication technology, safety and performance evaluation of KAERI fuel and the results of irradiation of KAERI fuels in Wolsung reactor will be described.

1985-07-01

9

Experience of HWR nuclear fuel fabrication technology development in Korea  

International Nuclear Information System (INIS)

Since January, 1981, the project of development of nuclear fuel fabrication technology for Wolsung reactor (CANDU type) was undertaken by KAERI(Korea Advanced Energy Research Institute) and successfully fulfilled with loading 24 fuel bundles made by KAERI in Wolsung reactor in September, 1984. On the basis of this accumulated technology and experience, mass production plan to supply all the nuclear fuels for Wolsung reactor is under way. In this presentation, the Korean experience in the development of the nuclear fuel fabrication technology, safety and performance evaluation of KAERI fuel and the results of irradiation of KAERI fuels in Wolsung reactor will be described.

1985-10-29

10

Reliability engineering in aerospace technology. Approach to the assurance of high reliability; Eisei uchu rocket no shinraisei. Koshinraisei eno torikumi  

Energy Technology Data Exchange (ETDEWEB)

This paper describes an approach to the reliability engineering in aerospace technology. To promote development, configuration management (clarifies the base line of technology), reliability management, quality control, safety management, progress management, and cost management are very important. The following example related to reliability was contained for the development of an N-1 rocket in Japan. A timer and amplifier that are old-fashioned but have actual results were supplied from abroad. The induction system that was purchased from abroad contained faulty components in quality control. The improvement in reliability has priority and the first-stage tank was changed to a home-made aluminum alloy that is superior in stress-resistant corrosiveness. An H-II rocket was completely developed in Japan by self-technology. The number of faults to be generated in the H-II rocket decreases as compared with the ...

1995-02-05

11

The upgrade of nuclear material accounting system at KAERI  

International Nuclear Information System (INIS)

The agreement between the government of Republic Of Korea (ROK) and the IAEA for the application of safeguards was signed and entered into force in 1975. The Additional Protocol (AP) to the Safeguards Agreement between the ROK and the IAEA was signed in 1999 and entered into force on 19 February 2004. Also, Implementation of Integrated Safeguards (IS) was started on 1 July, 2008 after a draw of the broader conclusion. The IAEA provides 2 hours notification for Random Interim Inspection (RII) under IS. For RII, the facility has to prepare the inspection documents in a short time. Therefore, KAERI (Korea Atomic Energy Research Institute) developed a new computerized nuclear material accounting system named KASIS (KAERI Safeguards Information treatment System) to treat the data by on-line for RII. For the efficient IS implementation, KAERI has a plan to upgrade the system to reflect the accounting approaches or reporting ...

2010-10-01

12

Seismic Testing of Reactor Components.  

Science.gov (United States)

This report is the final report on the seismic testing of reactor components conducted since 1977 with opening of the vibration laboratory at KAERI. In 1979, forced vibration testing of Wolsung-1 steam generator model using sine dwell and white nosie rand...

1980-01-01

13

Maintenance and fabrication of electronic equipment  

Energy Technology Data Exchange (ETDEWEB)

Solving the maintenance and repair problems of electronic instruments, we have supported the research and development work, and reduced operation costs of the pilot plants in KAERI. In addition, we have improved the maintainability of instruments to use effectively. 18 tabs., 17 figs., 13 refs. (Author) .new.

1995-12-01

14

Maintenance and fabrication of electronic equipment  

Energy Technology Data Exchange (ETDEWEB)

Solving the maintenance and repair problems of electronic instruments, we have supported the research and development work, and reduced operation costs of the pilot plants in KAERI. In addition, we have imposed the maintainability of instruments to use effectively. 15 tabs., 14 figs., 14 refs. (Author) .new.

1994-12-01

15

Development of QA/QC technology in Korea  

International Nuclear Information System (INIS)

KAERI (Korea Advanced Energy Research Institute) has performed research to develop the fabrication technology of CANDU nuclear fuel since 1981. Based on the satisfactory results of in-pile and out-of-pile tests of prototype nuclear fuel and the outstanding performance of 48 KAERI-made nuclear fuels in Wolsung(CANDU) power reactor, Korean government decided KAERI to supply all the nuclear fuels for Wolsung from 1988. In order to guarantee the safety and performance of nuclear fuel manufactured in mass production scale, well-organized quality assurance system and appropriate quality control techniques should be established. To establish the QA system, KAERI reviewed various QA standards and decided to establish QA system based on the 10 CFR 50 Appendix B. Quality control techniques was also revised to fit the mass production even though quality inspection techniques have already been developed during ...

1986-10-06

16

Development of PHWR fuel fabrication in Korea  

Energy Technology Data Exchange (ETDEWEB)

Korea Advanced Energy Research Institute (KAERI) started a research project to develop the PHWR (CANDU) nuclear fuel fabrication technology in 1981. Based on the results of the intensive developmental work, several prototype fuel bundles were fabricated and tested in the Hot Test Loop at KAERI continuously in 1983 and 1984. After that, irradiation test and post-irradiation examination were carried out for two KAERI-made fuel bundles at Chalk River Nuclear Laboratories in Canada in 1984. Since the results of in-pile and out-of-pile tests with prototype fuel bundles proved to be satisfactory, 48 additional fuel bundles were loaded in Wolsung reactor (CANDU) in 1984 and 1985, and all of them were discharged without a defect after excellent performance in the power reactor. In 1985, the Korean government decided that KAERI supplies all the fuel necessary for the Wolsung reactor. For the mass production of ...

1988-01-01

17

Hamiltonian formulation of the N=1 D=10 supergravity coupled to super Yang-Mills theory  

Energy Technology Data Exchange (ETDEWEB)

The authors derive in full details the Hamiltonian formulation of the N = 1D = 10 supergravity coupled to super Yang-Mills theory. In particular, they present the explicit form of the first class constraints and compute the constraints gauge algebra.

1988-01-01

18

Flucytosine for treatment of Candida albicans in H1N1-positive patient  

UK PubMed Central (United Kingdom)

A 17-year-old H1N1-positive patient was successfully extubated after 25 days of ventilatory support for treatment of viral pneumonia which was complicated by empyema thoracis due to Candida...Full Text Available

2010-10-01

19

Epidemiological consequences of an incursion of highly pathogenic H5N1 avian influenza into the British poultry flock  

UK PubMed Central (United Kingdom)

Highly pathogenic avian influenza and in particular the H5N1 strain has resulted in the culling of millions of birds and continues to pose a threat to poultry industries worldwide. The recent outbreak...Full Text Available

2008-01-07

20

Electronic topological transition in an n-BiSb semiconductor alloy in the quantum limit range of magnetic fields for H-parallel C{sub 2}  

Science.gov (United States)

The galvanomagnetic properties of single-crystal samples of the Bi{sub 0.93}Sb{sub 0.07} semiconductor alloy with the electron density n = 1.6 x 10{sup 17} cm{sup -3} in magnetic fields up to 14 T at T = 1.6 K have been investigated. The resistivity {rho} and Hall coefficient R have been measured as functions of the magnetic field directed along the binary axis of a crystal for a current flowing through a sample along the bisector axis; i.e., the components {rho}{sub 22} and R{sub 32,1} have been measured. The strong anisotropy of the electron spectrum of the samples makes it possible to separately observe quantum oscillations of the magnetoresistance {rho}{sub 22}(H) for H -parallel C{sub 2} in low magnetic fields for two equivalent ellipsoids with small extremal cross sections (secondary ellipsoids) and in high magnetic fields for electrons of the ellipsoid with a large extremal cross section (main ellipsoid). An increase ...

2010-08-15

21

Effects of irradiation on the microstructural evolution and corrosion resistance of zirconium alloys  

International Nuclear Information System (INIS)

Zircaloy-2 and Zircaloy-4 tubing materials were irradiated with 1 MeV proton at 350 degrees C to doses of 0.01, 0.1, and 1 dpa respectively. Both microstructure examination and nodular corrosion test (500 degrees C, 1500 psi steam) were performed in order to understand the relationship between the microstructural evolution and the corrosion resistance of these alloys under irradiation. Neutron-irradiated Zircaloy-2 specimens which were obtained from a failed BWR fuel rod cladding were also studied. Specimens of three different neutron fluences were investigated; namely, 2.6x10"2"4, 3.2x10"2"5, 3.8x10"2"5, (E_n#>=#1MeV). The results indicated that the higher the irradiation dose the better the nodular corrosion resistance of both Zircaloy-2 and Zircaloy-4. It is concluded that irradiation-induced precipitate dissolution and irradiation-enhanced diffusion may increase the solute concentration in the matrix and make it ...

1991-08-25

22

Risk Factors and Immunity in a Nationally Representative Population following the 2009 Influenza A(H1N1) Pandemic  

UK PubMed Central (United Kingdom)

BackgroundUnderstanding immunity, incidence and risk factors of the 2009 influenza A(H1N1) pandemic (2009 H1N1) through a national seroprevalence study is necessary for informing...Full Text Available

23

Representations of the conformal Lie algebra in the space of tensor densities on the sphere  

CERN Document Server

Let ${\\mathcal F}_\\lambda(\\mathbb{S}^n)$ be the space of tensor densities on $\\mathbb{S}^n$ of degree $\\lambda$. We consider this space as an induced module of the nonunitary spherical series of the group $\\mathrm{SO}_0(n+1,1)$ and classify $(\\mathrm{so}(n+1,1),\\mathrm{SO}(n+1))$-sim$unitary submodules of ${\\mathcal F}_\\lambda(\\mathbb{S}^n)$ as a function of $\\lambda$.

2003-01-01

24

Replication, Pathogenesis and Transmission of Pandemic (H1N1) 2009 Virus in Non-Immune Pigs  

UK PubMed Central (United Kingdom)

The declaration of the human influenza A pandemic (H1N1) 2009 (H1N1/09) raised important questions, including origin and host range [1],...Full Text Available

25

N = 1 Supersymmetry and the phenomenological pion physics effective action  

International Nuclear Information System (INIS)

In this presentation, I show that it is possible to construct an extension of the phenomenological pion physics effective action by use of chiral and nonminimal 4D, N=1 scalar multiplets. The result obtained differs drastically from the standard low-energy N=1 SQCD theory first suggested by Veneziano and Yankielowicz. (orig.).

1997-05-27

26

Alkane degradation under anoxic conditions by a nitrate-reducing bacterium with possible involvement of the electron acceptor in substrate activation  

UK PubMed Central (United Kingdom)

Microorganisms can degrade saturated hydrocarbons (alkanes) not only under oxic but also under anoxic conditions. Three denitrifying isolates (strains HxN1, OcN1, HdN1) able to grow under anoxic conditions...Full Text Available

2011-02-01

27

The development of PHWR fuel fabrication in Korea  

International Nuclear Information System (INIS)

Korea Advanced Energy Research Institute (KAERI) started a research project to develop the PHWR (CANDU) nuclear fuel fabrication technology in 1981. Based on the results of the intensive developmental work, several prototype fuel bundles were fabricated and tested in the Hot Test Loop at KAERI continuously in 1983 and 1984. After that, irradiation test and post-irrradiation examination were carried out for two KAERI-made fuel bundles at Chalk River Nuclear Laboratories in Canada in 1984. Since the results of in-pile and out-of-pile tests with prototype fuel bundles proved to be satisfactory, 48 additional fuel bundles were loaded in Wolsung reactor (CANDU) in 1984 and 1985, and all of them were discharged without a defect after excellent performance in the power reactor. In 1985, the Korean government decided that KAERI supplies all the fuel necessary for the Wolsung reactor. For the mass production of ...

1987-09-07

28

Korea's experience and program on CANDU fuel R and D and fabrication  

International Nuclear Information System (INIS)

In Korea, a manufacturing process for the fabrication of CANDU 37-element fuel bundles was successfully developed between 1981 and 1986. At Korea Atomic Energy Research Institute (KAERI), more than 20,000 fuel bundles were produced up to May 1992, for use in Wolsung-1 power reactor. At the time of the conference, about 15,000 of these fuel bundles had been irradiated in Wolsung-1, and almost all of them had performed well. From 1995, the commercial fuel production program will be transferred to Korea Nuclear Fuel Company, which is building a plant with a capacity of 400 tons of uranium per year. So-called CANFLEX fuel, more appropriate to advanced fuel cycles, is being developed jointly by AECL and KAERI. The paper includes a listing of the current status of the Republic of Korea's nuclear power plants, with planning projections up to the year 2006. 2 tabs.

1992-10-04

29

Acute Kidney Injury in Critically Ill Patients Infected With 2009 Pandemic Influenza A(H1N1): Report From a Canadian Province  

British Library Electronic Table of Contents (United Kingdom)

Background 2009 pandemic influenza A(H1N1) has led to a global increase in severe respiratory illness. Little is known about kidney outcomes and dialytic requirements in critically ill patients infected with pandemic H1N1. Study Design Prospective observational study. Setting & Participants 50 patients with pandemic H1N1 admitted to any of 7 intensive care units in Manitoba, Canada, were prospectively followed. Outcome & Measurements Outcomes were kidney injury and kidney failure defined using RIFLE (risk, injury, failure, loss, end-stage disease) criteria or need for dialysis therapy. Results The pandemic H1N1 group was composed of 50 critically ill patients with pandemic H1N1 with severe respiratory syndrome (47 confirmed cases, 3 probable). Kidney injury, kidney ...

2010-01-01

30

Titanium Alloys for Medical Instrumentation  

International Science & Technology Center (ISTC)

The New Titanium Alloys With Increased Mechanical Properties and Corrosion Resistance for Medical Instruments and their Coatings

31

Molybdenum Alloys Optimal Structure  

International Science & Technology Center (ISTC)

Determination of Special Molybdenum Alloys Optimal Structure Using the Cybernetic Method

33

Corrosion Protection of special steels and alloys  

International Science & Technology Center (ISTC)

Development of the Corrosion Protection Technology for Special Steels and Alloys

34

Quantization of the Lie algebra so(2n+1) and of the Lie superalgebra osp(1/2n) with preoscillator generators  

CERN Document Server

The Lie algebra so(2n+1) and the Lie superalgebra osp(1/2n) are quantized in terms of 3n generators, called preoscillator generators. Apart from n "Cartan" elements the preoscillator generators are deformed para-Fermi operators in the case of so(2n+1) and deformed para-Bose operators in the case of osp(1/2n). The corresponding deformed universal enveloping algebras U_q[so(2n+1)] and U_q[osp(1/2n)] are the same as those defined in terms of Chevalley operators. The name "preoscillator" is to indicate that in a certain representation these operators reduce to the known deformed Fermi and Bose operators.

1994-01-01

35

Excitation functions of "1"8"6","1"8"7","1"8"8","1"8"9","1"9"0","1"9"2Ir formed in proton-induced reactions on highly enriched "1"9"2Os up to 66 MeV  

International Nuclear Information System (INIS)

Cross sections of proton-induced nuclear reactions on highly enriched "1"9"2Os were measured up to 66 MeV by using the stacked-foil irradiation technique. Excitation functions are presented for the reactions "1"9"2Os(p,n)"1"9"2Ir, "1"9"2Os(p,3n)"1"9"0Ir, "1"9"2Os(p,4n)"1"8"9Ir, "1"9"2Os(p,5n)"1"8"8Ir, "1"9"2Os(p,6n)"1"8"7Ir and "1"9"2Os(p,7n)"1"8"6Ir. No earlier experimental cross-section data could be found in the literature except for the "1"9"2Os(p,n)"1"9"2Ir process. Our new experimental results are compared with theoretical predictions by means of the theoretical model code ALICE/ASH. Integral thick-target yield calculations were also performed for the ...

2010-10-15

36

Defense.gov News Article: DARPA Effort Speeds Biothreat ...  

Science.gov (United States)

... H1N1 a pandemic virus in June 2009, the Defense Advanced Research Projects Agency had a plan to address the crisis. The DARPA effort, called ...

37

Analysis of the Seasonal Effects on Cesium Clocks to Improve ...  

Science.gov (United States)

... XVIII, n. 1, p. 50-67. [2] G. Becker: Zeitskalenprobleme: jahreszeitliche Gangschwankungen von Atomuhren, PTB Mitteilungen 92 2/82, p. 105-113. ...

1987-12-01

39

Maximum overhang  

CERN Document Server

How far can a stack of $n$ identical blocks be made to hang over the edge of a table? The question dates back to at least the middle of the 19th century and the answer to it was widely believed to be of order $\\log n$. Recently, Paterson and Zwick constructed $n$-block stacks with overhangs of order $n^{1/3}$, exponentially better than previously thought possible. We show here that order $n^{1/3}$ is indeed best possible, resolving the long-standing overhang problem up to a constant factor.

2007-01-01

40

Highly Pathogenic H5N1 Avian Influenza: Entry Pathways into North America via Bird Migration  

UK PubMed Central (United Kingdom)

Given the possibility of highly pathogenic H5N1 avian influenza arriving in North America and monitoring programs that have been established to detect and track it, we review intercontinental movements...Full Text Available

41

Coefficient algebra of the minimal representation of the elliptic quantum group  

International Nuclear Information System (INIS)

The algebra of the coefficients in the minimal representation of the A_n_-_1 quantum group, discussed by Felder and Varchenko, is given. Those coefficients are associated with the Boltzmann weights of A_n_-_1"("1") interaction-round-a-face model. The authors show that the algebra satisfies the Yang-Baxter equation. The PBW base for this algebra is also given

2001-07-01

42

Alpha particle induced excitation functions with "1"4"1Pr  

International Nuclear Information System (INIS)

In the present work the excitation functions for the reactions "1"4"1Pr(#alpha#,n)"1"4"4Pm and "1"4"1Pr(#alpha#,2n)"1"4"3Pm have been measured experimentally below 50 MeV #alpha#-particle

1998-12-01

43

Aerosol influenza transmission risk contours: A study of humid tropics versus winter temperate zone  

UK PubMed Central (United Kingdom)

BackgroundIn recent years, much attention has been given to the spread of influenza around the world. With the continuing human outbreak of H5N1 beginning in 2003 and the H1N1 pandemic...Full Text Available

45

New Powder Technologies for Molybdenum Alloy Gun Barrel ...  

Science.gov (United States)

... MOLYBDENUM ALLOY GUN BARREL LINERS o0 in ... NEW POWDER TECHNOLOGIES FOR MOLYBDENUM ALLOY GUN BARREL LINERS ...

1985-06-01

48

Autocatalytic nucleation of omega phase in a beta-titanium alloy  

International Nuclear Information System (INIS)

Observations concerned with the formation of isothermal #omega# in the beta-titanium alloy RMI (38-6-44) are presented as part of a more general study of the aging characteristics of the alloy.

49

The effects of alloying elements and dilution on the hot cracking sensitivity of welds in alloy 800  

International Nuclear Information System (INIS)

Results of hot cracking on welds with compositions between alloy 800 and AWS ER NiCr 3. Investigation of the influence of Si, Mn, Ti and Al on the hot cracking suscpetibility of the alloy 800. (orig.).

52

Metals and alloys : atmospheric corrosion testing : General requirements for field tests  

CERN Document Server

Metals and alloys : atmospheric corrosion testing : General requirements for field tests

1992-01-01

54

Effect of Yttrium on the Microstructure of Titanium Alloys,  

Science.gov (United States)

... Title : Effect of Yttrium on the Microstructure of Titanium Alloys,. ... The yttrium was added in the melting stage as an oxide or in the elemental form. ...

55

Ductile aluminide alloys for high temperature applications  

Energy Technology Data Exchange (ETDEWEB)

Alloys are described which contain nickel, aluminum, boron, iron and in some instances manganese, niobium and titanium.

1987-01-01

56

Corrosion and stress corrosion cracking of alloy 800 in water and steam at elevated temperatures  

International Nuclear Information System (INIS)

The importance that must be attached to the phenomenon of stress corrosion cracking of austenitic alloys is emphasized. The relation between chemical composition of various alloys and their sensitivity to cracking is shown with particular reference to the behaviour of Alloy 800. The different effects of alkaline anc chloride environments are discussed. Studies are reported of the general corrosion of Alloy 800 and other alloys in an environment representative of the primary coolant of PWR reactors; and of the behaviour of various alloys (including Alloy 800) in the conditions envisaged for their use for steam generators with superheat up to about 550 deg.C. (U.K.).

57

Shielding and Criticality Safety Analysis of KSC-1 Cask for the High Burnup PWR Spent Fuels  

International Nuclear Information System (INIS)

KSC-1 (KAERI Shipping Cask-1) was designed and manufactured with a pure domestic technology in 1985 in order to transport a PWR spent fuel assembly from nuclear power plant to PIEF (Post-Irradiation Examination Facility) of KAERI. Since the first transportation of the fuel assembly from Kori-1 NPP was carried out by the cask in 1987, 19 shipments for the PWR spent fuels have been done successfully by now. Maximum discharge burnup of PWR in Korea has been extended from the late 1990s in order to reduce the cost of power generation. From this cause, allowable design values of the initial enrichment and the cooling time for the cask have been changed three times: year 2003, 2007 and 2010. Radiation shielding and criticality of KSC-1 were analyzed for all the PWR fuel type irradiated in Korea NPP to renew the design approval

2010-10-01

58

First lasing of the KAERI compact far-infrared free-electron laser driven by a magnetron-based microtron  

International Nuclear Information System (INIS)

The KAERI compact far-infrared (FIR) free-electron laser (FEL) has been operated successfully in the wavelength range of 97-150 #mu#m. It is the first demonstration of FEL lasing by using a magnetron-based classical microtron. We developed a high precision undulator consisting of 80 periods, with each period being 25 mm. The field strength of the undulator can be changed from 4.5 to 6.8 kG with an amplitude deviation of only 0.05% in r.m.s value. The kinetic energy of the electron beam is 6.5 MeV. The average current and pulse duration of the electron beam macropulses are 45 mA and 5.5 #mu#s, respectively. The measured power of the FEL with the electron beam parameters was more than 50 W for a FIR macropulse having a duration of 4 #mu#s. The spectral width of the FEL was measured to be 0.5% of the central wavelength. The FEL system, aside from the racks for the controlling units, is compact enough to be located inside an area of 3x4 m"2.

2001-12-21

59

Development and Application of Subchannel Analysis Code Technology for Advanced Reactor Systems  

Energy Technology Data Exchange (ETDEWEB)

A study has been performed for the development and assessment of a subchannel analysis code which is purposed to be used for the analysis of advanced reactor conditions with various configurations of reactor core and several kinds of reactor coolant fluids. The subchannel analysis code was developed on the basis of MATRA code which is being developed at KAERI. A GUI (Graphic User Interface) system was adopted in order to reduce input error and to enhance user convenience. The subchannel code was complemented in the property calculation modules by including various fluids such as heavy liquid metal, gas, refrigerant,and supercritical water. The subchannel code was applied to calculate the local thermal hydraulic conditions inside the non-square test bundles which was employed for the analysis of CHF. The applicability of the subchannel code was evaluated for a high temperature gas cooled reactor condition and supercritical pressure conditions with water and Freon. A ...

2006-01-15

60

Feynman rules in N=2 projective superspace. II. Massive hypermultiplets  

International Nuclear Information System (INIS)

For pt.I see ibid., vol.516, p.426-48, 1998. Manifest N=2 supersymmetric hypermultiplet mass terms can be introduced in the projective N=2 superspace formalism. In the case of complex hypermultiplets, where the gauge covariantized spinor derivatives have an explicit representation in terms of gauge prepotentials, it is possible to interpret such masses as vacuum expectation values of an Abelian vector multiplet. The duality transformation that relates the N=2 off-shell projective description of the hypermultiplet to the on-shell description involving two N=1 chiral superfields allows us to obtain the massive propagators of the N=1 complex linear fields in the projective hypermultiplet. The N=1 massive propagators of the component superfields in the projective hypermultiplet suggest a possible ansatz for the N=2 massive propagator, which agrees with an explicit ...

61

Two-phase Flow Regime Maps in Horizontal and Vertical Tubes  

Energy Technology Data Exchange (ETDEWEB)

A safety analysis code to design a pressurized water reactor and to obtain the licenses including entire proprietary rights is under development in domestic R and D project. The tasks of KAERI is to develop the constitutive relations including models for defining flow regimes and flow regime related models for inter-phase friction, wall frictions, wall heat transfer, and interphase heat and mass transfer in the two-phase three-field equations. In this paper, the process will be presented for choosing the best flow regime maps which occur in gas-liquid two-phase flow in horizontal and vertical tubes.

2007-10-15

62

Two-phase Flow Regime Maps in Horizontal and Vertical Tubes  

International Nuclear Information System (INIS)

A safety analysis code to design a pressurized water reactor and to obtain the licenses including entire proprietary rights is under development in domestic R and D project. The tasks of KAERI is to develop the constitutive relations including models for defining flow regimes and flow regime related models for inter-phase friction, wall frictions, wall heat transfer, and interphase heat and mass transfer in the two-phase three-field equations. In this paper, the process will be presented for choosing the best flow regime maps which occur in gas-liquid two-phase flow in horizontal and vertical tubes.

2007-10-01

63

Improvement of assessment methodology for fluid flow characteristics of passive flow control device  

International Nuclear Information System (INIS)

The objective of this study is to establish evaluation and verification guideline for the APR 1400 and to investigate the thermal-hydraulic characteristics for fluidic device is analyzed using FLUENT. The scope and major results of research are flow characteristics for fluidic device. In this study, three-dimensional numerical model for fluidic device is developed adequately for, and results are compared with experimental data performed by VAPER (VAlve Performance Evaluation test Rig) in KAERI with an aim to verify numerical simulation. In addition, the parametric study has also carried out to investigate the effect of major parameters such as velocity and pressure inside FD chamber.

2002-10-01

64

Flow Regime Map Models for the Horizontal and Vertical Pipes for the SPACE code  

Energy Technology Data Exchange (ETDEWEB)

A safety analysis code, named as SPACE, for a pressurized water reactor is under development to obtain a licensing to be used for the PWR design and to hold entire proprietary rights. The task of KAERI is to develop the physical models and correlations which are required to solve the field equations. It can be divided into four parts; i) flow regime determination, ii) wall heat transfer, iii) wall and interfacial friction, iv) interfacial heat and mass transfer. This paper will describe the process to develop the models for the two-phase flow regime maps in the horizontal and vertical pipes.

2008-05-15

65

Flow Regime Map Models for the Horizontal and Vertical Pipes for the SPACE code  

International Nuclear Information System (INIS)

A safety analysis code, named as SPACE, for a pressurized water reactor is under development to obtain a licensing to be used for the PWR design and to hold entire proprietary rights. The task of KAERI is to develop the physical models and correlations which are required to solve the field equations. It can be divided into four parts; i) flow regime determination, ii) wall heat transfer, iii) wall and interfacial friction, iv) interfacial heat and mass transfer. This paper will describe the process to develop the models for the two-phase flow regime maps in the horizontal and vertical pipes.

2008-05-01

66

Basic Science Beamline(TR104) at PEFP  

International Nuclear Information System (INIS)

PEFP(Proton Engineering Frontier Project) is developing beamlines for various application fields by using the high current 100MeV proton linear accelerator. Beamlines were characterized and categorized by the beam energy, average currents, and irradiation conditions. Among these beamlines the TR104 is designed for the basic science and the research of the aerospace. Before the construction and installation of beamlines, we try to practice and prepare the detail process of installation by the precedent study of TR104 beamline in KAERI site. By this work installation process was checked and confirmed for the same condition of the PEFP site

2010-10-01

67

Axiomatic Design Approach for a Reactor Head Structure Assembly  

Energy Technology Data Exchange (ETDEWEB)

Korea Atomic Energy Research Institute (KAERI) has been developing the integral reactor. The reactor head structure assembly (RHSA) is the structure installed over the reactor cover. Due to the characteristics of an integral reactor, there are many instrument cables and power cables coming out from the reactor cover and main components. The RHSA provides an interface location to connect these cables from Architecture Engineer (AE) and System Designer (SD). It also prevents a pipe whip and it prohibits instruments from becoming missiles. In this research, the axiomatic design approach for the RHSA is performed.

2006-07-01

68

Application of porous media approach for multi-dimensional analysis of thermal hydraulic system analysis code, MARS  

Energy Technology Data Exchange (ETDEWEB)

The Porous media approach method was applied to the MULTID component of MARS which was developed by KAERI. This method has been widely used for analysis of large regions containing only fluid and for flows in regions with immersed solids. It can calculate flow distribution more correctly in case of flow area or volume change. Application of this method to the MULTID component in MARS was evaluated and the results were compared with those of CFD code, FLUENT. As a result, the calculated flow distributions of MARS and FLUENT show similar trend, so the effect of porous media in MARS can be applied to the other cases.

2003-10-01

69

A Preliminary Analysis of SMART Reactor Core Using the COREDAX Code  

International Nuclear Information System (INIS)

The 3-D neutronics code COREDAX has been developed based on AFEN (Analytic Function Expansion Nodal) method for x-y-z geometry and for hex-z geometry. In this study, the COREDAX code, as a regulatory review tool independent of the designer's, was applied to the SMART reactor core that was designed by KAERI (Korea Atomic Energy Research Institute). For nuclear cross section generation, the HELIOS lattice code was used in this study. The preliminary results for steady state in various conditions are presented in this paper

2010-10-01

70

Corrosion mode diagrams for alloy 690 TT and alloy 800  

Energy Technology Data Exchange (ETDEWEB)

Due to the well-establish corrosion problems of Alloy 600 as a steam-generator material and the subsequent focus on thermally treated (TT) Alloy 690 and Alloy 800 as alternative materials, a systematic analysis of the corrosion behavior of these two latter alloys is warranted. Corrosion test results for Alloys 690 TT and 800 were collected and organized in the form of corrosion mode diagrams. Selected data for mill annealed (MA) Alloy 600 were also included for reference. The corrosion mode diagrams correlate the modes of corrosion degradation observed in tests as functions of the environment pH and electrochemical potential (ECP). The diagrams confirm that Alloys 690TT shows some susceptibility in caustic environments, and Alloy 800 shows susceptibility in both caustic and highly acidic environments. (authors). 6 figs., ...

1994-12-31

71

Corrosion mode diagrams for alloy 690 TT and alloy 800  

International Nuclear Information System (INIS)

Due to the well-establish corrosion problems of Alloy 600 as a steam-generator material and the subsequent focus on thermally treated (TT) Alloy 690 and Alloy 800 as alternative materials, a systematic analysis of the corrosion behavior of these two latter alloys is warranted. Corrosion test results for Alloys 690 TT and 800 were collected and organized in the form of corrosion mode diagrams. Selected data for mill annealed (MA) Alloy 600 were also included for reference. The corrosion mode diagrams correlate the modes of corrosion degradation observed in tests as functions of the environment pH and electrochemical potential (ECP). The diagrams confirm that Alloys 690TT shows some susceptibility in caustic environments, and Alloy 800 shows susceptibility in both caustic and highly acidic environments. (authors). 6 figs., ...

72

Non-Abelian Duality and Confinement: from N=2 to N=1 Supersymmetric QCD  

CERN Document Server

Recently we discovered and discussed non-Abelian duality in the quark vacua of N=2 super-Yang-Mills theory with the U(N) gauge group and N_f flavors (N_f>N). Both theories from the dual pair support non-Abelian strings which confine monopoles. Now we introduce an N=2-breaking deformation, a mass term \\mu{\\mathcal A}^2 for the adjoint fields. Starting from a small deformation we eventually make it large which enforces complete decoupling of the adjoint fields. We show that the above non-Abelian duality fully survives in the limit of N=1 SQCD, albeit some technicalities change. For instance, non-Abelian strings which used to be BPS-saturated in the N=2 limit, cease to be saturated in N=1 SQCD. Our duality is a distant relative of Seiberg's duality in N=1 SQCD. Both share some common features but have drastic distinctions. This is due to the fact that ...

2011-01-01

73

Multiplexed, rapid detection of H5N1 using a PCR-free nanoparticle-based genomic microarray assay  

UK PubMed Central (United Kingdom)

BackgroundFor more than a decade there has been increasing interest in the use of nanotechnology and microarray platforms for diagnostic applications. In this report, we describe...Full Text Available

75

Ammonia adsorption on the C_3_0B_1_5N_1_5 heterofullerene: DFT study of nuclear magnetic shielding and electric field gradient tensors of N and B nuclei  

International Nuclear Information System (INIS)

Ammonia adsorption on the external surface of C_3_0B_1_5N_1_5 heterofullerene was studied using density functional calculations. Three models of the ammonia-attached C_3_0B_1_5N_1_5 together with the perfect model were optimized at the B3LYP/6-31G"* level. The optimization process reveals that dramatic influences occurred for the geometrical structure of C_3_0B_1_5N_1_5 after ammonia adsorption; the B atom relaxes outwardly and consequently the heterofullerene distorts from the spherical form in the adsorption sites. The chemical shielding (CS) tensors and nuclear quadrupole coupling constants of B and N nuclei were calculated at the B3LYP/6-311G"*"* level. Our calculations reveal that the B atom is chemically bonded to NH_3 molecule. The B atom in the NH_3-attached form has the largest chemical shielding isotropic (CSI) value among the other boron nuclei. The ...

2011-04-01

76

After-Hours Information Given by Telephone by Family Physicians in Ontario  

UK PubMed Central (United Kingdom)

This study describes instructions for after-hours care offered by family physicians' offices when patients telephone the practice. Randomly selected (n=1,680) Ontario family physicians and general practitioners...Full Text Available

2009-11-01

77

2009 Flu Prevention PSA Contest | Flu.gov  

Science.gov (United States)

in cash and is featured on national television. Congratulations to Dr. John Clarke of Baldwin, New York for his video entitled H1N1 Rap by Dr. Clarke. Congrats to the Winning...

2011-09-21

78

Decay of "1"7"7Ta composite system: comparison of excitation functions for the reaction residues occurring in "1"2C + "1"6"5Ho and "1"4N + "1"6"3Dy reactions  

International Nuclear Information System (INIS)

In the reactions induced by heavy ions, the study of breakup of heavy ions followed by the fusion of one of the fragments with the target has been of great interest. The present experiments has been performed with a view to compare the measured excitation functions for the same decay channels in "1"2C + "1"6"5Ho and "1"4N + "1"6"3Dy systems

2000-12-01

79

Malignant duodenal obstructions: palliative treatment with covered expandable nitinol stent  

Energy Technology Data Exchange (ETDEWEB)

To evaluate the feasibility and clinical effectiveness of using a polyurethane-covered expandable nitinol stent in the palliative treatment of malignant duodenal obstruction. Under fluoroscopic guidance, a polyurethane-covered expandable nitinol stent was placed in 12 consecutive patients with malignant duodenal obstructions. All presented with severe nausea and recurrent vomiting. The underlying causes of obstruction were duodenal carcinoma (n=4), pancreatic carcinoma (n=4), gall bladder carcinoma (n=2), distal CBD carcinoma (n=1), and uterine cervical carcinoma (n=1). The sites of obstruction were part I (n=1), part II (n=8), and III (n=3). Due to pre-existing jaundice, eight patients with part II obstructions underwent biliary decompression prior to stent placement. An introducer sheath with a 6-mm outer diameter and stents 16 mm in diameter were employed, ...

2002-04-01

80

Illinois department of public health H1N1/A pandemic communications evaluation survey.  

Energy Technology Data Exchange (ETDEWEB)

Because of heightened media coverage, a 24-hour news cycle and the potential miscommunication of health messages across all levels of government during the onset of the H1N1 influenza outbreak in spring 2009, the Illinois Department of Public Health (IDPH) decided to evaluate its H1N1 influenza A communications system. IDPH wanted to confirm its disease information and instructions were helping stakeholders prepare for and respond to a novel influenza outbreak. In addition, the time commitment involved in preparing, issuing, monitoring, updating, and responding to H1N1 federal guidelines/updates and media stories became a heavy burden for IDPH staff. The process and results of the H1N1 messaging survey represent a best practice that other health departments and emergency management agencies can replicate to improve ...

2010-09-16

81

A comparison of the low cycle fatigue behavior of alloy 800 and alloy 800H  

International Nuclear Information System (INIS)

The low cycle fatigue testing was carried out to provide a basis for comparison of the behavior of the two kinds of Alloy 800 (low carbon Alloy 800 and high carbon Alloy 800H). The testing was done at temperatures of 500"0C and 650"0C either with or without hold. The results obtained were as follows: (1) At 650"0C, the low-cycle fatigue life was essentially the same for the two alloys on the basis of strain amplitude, but Alloy 800H had a longer life on the basis of stress amplitude. (2) At 500"0C, the two alloys exhibited longer lives than at 650"0C, with Alloy 800 exhibiting 2-3 times longer life than Alloy 800H when compared on the basis of plastic strain range. At this temperature the stress range showed the maximum for Alloy 800H. (3) When a creep effect was introduced either by way of a hold ...

1979-06-01

82

Production of titanium alloys with uniform distribution of heat resisting metals  

International Nuclear Information System (INIS)

Consideration is given to the process of the formation of a titanium sponge alloyed with niobium or tantalum, in the joint metallic reduction of titanium, niobium and tantanum chlorides. A percentage composition of the phases observed and the structure of the alloyed sponge have been studied. It is shown that after one remelting operation of the alloyed sponge the alloys of titanium with niobium and tantalum have a uniform component distribution. At the stage of chloride reduction there appear solid solutions based on titanium and an alloying component. The stage of vacuum separation of the reaction mass is associated with a mutual dissolution of the primary phases and the formation of the solid solutions of the alloyed titanium sponge, which, by their composition, are close to the desired alloy composition. The principal features of the ...

83

Tensile strength of eutectic, directionally solidified alloys based on the Co-Cr-C-system  

International Nuclear Information System (INIS)

The influence of various alloy elements on tensile strength of the eutectic, directionally solidified superalloy 73 C was determined. The tensile properties of the base alloy has been increased by Al, Y and C as alloying elements, while Ni and Ti showed a decreasing effect (alloy softening). However, ductility and thermo-fatigue behaviour had been influenced in a positive way by these elements. The specific meachanism caused by the different elements are discussed. (orig.).

1981-01-01

84

Quartz ceramics alloying  

International Nuclear Information System (INIS)

The following methods of quartz ceramics alloying were considered: alloying of initial quartz glass; introduction of alloying additive into water slip of quartz glass; porous materials impregnation with salt aqueous solutions and subsequent salt thermal decomposition with formation of stable oxides in pores of ceramics. Oxygen free compounds BN, SiB_4, SiC, Si_3N_4, REM oxides and transition metal oxides were used as alloying additives. Main properties of the materials and compositions obtained are presented.

85

Processing and properties of Nb-Ti-base alloys  

Energy Technology Data Exchange (ETDEWEB)

The processing characteristics, tensile properties, and oxidation response of two Nb-Ti-Al-Cr alloys were investigated. One creep test at 650 C and 172 MPa was conducted on the base alloy, which contained 40Nb-40Ti-10Al-10Cr. A second alloy was modified with 0.11 at.% C and 0.07 at.% Y. Alloys were arc melted in a chamber backfilled with argon, drop cast into a water-cooled copper mold, and cold rolled to obtain a 0.8-mm sheet. The sheet was annealed at 1,100 C for 0.5 h. Longitudinal tensile specimens and oxidation specimens were obtained for both the base alloy and the modified alloy. Tensile properties were obtained for the base alloy at room temperature, 400, 600, 700, 800, 900, and 1,000 C and for the modified alloy at room temperature, 400, 600, 700, and 800 C. Oxidation tests the base alloy ...

1993-08-01

86

Processing and properties of Nb-Ti based alloys  

Energy Technology Data Exchange (ETDEWEB)

The processing characteristics, tensile properties, and oxidation response of two Nb-Ti-Al-Cr alloys were investigated. One creep tests at 650{degrees}C and 172 MPa was conducted on the base alloy which contained 40Nb-40-Ti-10Al-10Cr. A second alloy was modified with 0.11 at. % carbon and 0.07 at. % yttrium. Alloys were arc melted in a chamber backfilled with argon, drop cast into a water-cooled copper mold, and cold rolled to obtain a 0.8-mm sheet. The sheet was annealed at 1100{degrees}C for 0.5 h. Longitudinal tensile specimens and oxidation specimens were obtained for both the base alloy and the modified alloy. Tensile properties were obtained for the base alloy at room temperature, 400, 600, 700, 800, 900, and 1000{degrees}C, and for the modified alloy at room temperature, 400, 600, 700, and 800{degrees}C. Oxidation ...

1992-01-01

87

Nickel alloy clad steel plate for flue gas desulfurization applications  

Energy Technology Data Exchange (ETDEWEB)

The use of nickel alloys in Flue Gas Desulfurization (FGD) applications is described. Recently, nickel alloys 625 and C-276 have been clad to carbon steel plate. Production and properties of the clad plate are reviewed and a brief discussion is presented on production, fabrication and welding. Laboratory and field corrosion tests in SO/sub 2/ scrubber environments suggest that alloy 625 and C-276 clad steel plates are as corrosion resistant as the solid alloy plate.

1987-01-01

88

Investigation into superplasticity of Be alloys  

International Nuclear Information System (INIS)

Investigated are the characteristics of high-temperature plastic deformation the velocity sensitivity of flow stresses, deformation curves, flow stresses, deformation before rupture - as well as the structure of beryllium alloys containing nickel (0.5-4 %), yttrium (0.5-2 %) and aluminium (38 %). The alloys containing nickel (2%) and yttrium (0.5 %) are superplastic, however, deformation before fracture of the alloys is lower than that of the unalloyed beryllium. The singularities of high-temperature plastic flow of the alloys and the causes of deterioration of their plasticity are determined.

89

Hydrogen effect or texture and deformation mechanism in #beta#-titanium alloy cold rolling  

International Nuclear Information System (INIS)

The relationships of hydrogen alloyed #beta#-titanium alloy deformation behaviour to its microstructure and texture are investigated. It is shown that plasticity increases and strain induced texture changes at low hydrogen contents (0.1-0.2 mass %). Possible mechanisms responsible for specific features of #beta#-Ti alloy deformation are discussed. The study is made using alloy VT35 doped with hydrogen

1999-09-01

90

Comparative behavior of Alloys 600, 690 and 800 in caustic environments  

Energy Technology Data Exchange (ETDEWEB)

Since 1991, secondary side cracking has become a major concern in EDF steam generators. At 350 C, IGSCC of Alloy 600 was found in pure NaOH solutions from 4 to 500 g/l, with a maximum at 100 g/l. From the present results and available data, IGSCC of Alloy 690 occurred in pure NaOH solutions from 40 to 500 g/l, but the greatest sensitivity was observed at 100 g/l. TG/IGSCC of Alloy 800 became more severe with increasing NaOH solutions, from 10 to 500 g/l. On the whole, the ranking for SCC-resistance was Alloy 600 < Alloy 800 < Alloy 690. A significant improvement was still obtained with 690TT with intergranular carbides (industrial tubes) and perhaps with Alloy 800 NG (nuclear grade), but both alloys cracked at the highest stresses. IGSCC susceptibility of Alloy 600 MA was higher for the tubes ...

1995-12-31

91

Production of intergranular attack of alloy 600, alloy 690, and alloy 800 tubing in tubesheet crevices: Topical report  

Energy Technology Data Exchange (ETDEWEB)

Three model boilers, manufactured to simulate full-size tube sheet crevices, were tested with various secondary side environments. The first was faulted with organics representative of the decomposition of humic acid. The second was faulted with sodium carbonate and sodium hydroxide, while the third was faulted with sodium sulfate and sodium hydroxide. Each model contained seven tubes, which included Alloy 600 in the mill-annealed (MA) and thermally-treated (TT) conditions and Alloy 690 in the thermally-treated condition. Two models contained Alloy 800 tubes in the mill-annealed condition and one had Alloy 800 in the mill-annealed/cold-worked/glass-bead-peened condition. Two different sizes of tubesheet crevices were used in all model boilers. In the organics-faulted boiler, tubes of Alloy 600MA, Alloy 690TT and Alloy 800MA experienced no ...

1987-07-01

92

Production of intergranular attack of alloy 600, alloy 690, and alloy 800 tubing in tubesheet crevices: Topical report  

International Nuclear Information System (INIS)

Three model boilers, manufactured to simulate full-size tube sheet crevices, were tested with various secondary side environments. The first was faulted with organics representative of the decomposition of humic acid. The second was faulted with sodium carbonate and sodium hydroxide, while the third was faulted with sodium sulfate and sodium hydroxide. Each model contained seven tubes, which included Alloy 600 in the mill-annealed (MA) and thermally-treated (TT) conditions and Alloy 690 in the thermally-treated condition. Two models contained Alloy 800 tubes in the mill-annealed condition and one had Alloy 800 in the mill-annealed/cold-worked/glass-bead-peened condition. Two different sizes of tubesheet crevices were used in all model boilers. In the organics-faulted boiler, tubes of Alloy 600MA, Alloy 690TT and Alloy 800MA experienced no ...

93

Laser hardening of titanium-zirconium alloy  

International Nuclear Information System (INIS)

The methods of surface modification of Ti-Zr alloy by laser treatment are considered. Characteristics of laser modification without- and with surface melting and with melting in different gaseous environments and with nickel microalloying are presented. Maximum depth, hardness and corrosion resistance are observed under nickel laser alloying.

94

Development of Mg alloy sheets via strip casting  

Energy Technology Data Exchange (ETDEWEB)

AZ31 and experimental ZMA611 alloys were strip cast into 2 mm thick strips. The as-cast AZ31 alloy strip consists of columnar dendrites. On the other hand, as-cast ZMA611 alloy strip shows equiaxed dendritic structure through the thickness of strip. These alloys were subjected to various thermomechanical treatments and their tensile properties were evaluated. Strip cast AZ31 alloy in H24 condition has equivalent yield and tensile strengths with similar ductility compared to commercial ingot cast AZ31-H24 alloy, indicating that strip casting is a viable process for the fabrication of Mg alloy strips. The ZMA611 alloy has a large volume fraction of fine dispersoid particles in the microstructure, resulting from the beneficial effect of strip casting on microstructural refinement. It has been shown that the ZMA611 ...

2005-07-01

95

Wear resistance of a laser surface alloyed Ti-6Al-4V alloy  

Energy Technology Data Exchange (ETDEWEB)

Laser surface alloying with gaseous nitrogen was utilized to improve the wear resistance of a Ti-6Al-4V alloy. Wear-resistant composite coatings reinforced by hard TiN dendrites were produced 'in-situ' on a substrate of a Ti-6Al-4V alloy. The hardness and wear resistance of the laser alloyed coating under two-body abrasive and block-on-ring full-sliding wear conditions were significantly enhanced. (orig.)

2000-08-01

96

Development of ALLOY 800 for PWR/SG tubings resistant to IGSCC and general corrosion  

Energy Technology Data Exchange (ETDEWEB)

Resistance of ALLOY 800 as a PWR/SG tubings to IGC/IGSCC and Ni, Co release into high temperature water was evaluated as compared with ALLOYs 600 and 690. The study to improve the resistance to IGSCC and general corrosion was also made. From the results, ALLOY 800 was evaluated to be the most reliable among the high Ni alloys tested. In addition, the alloy would obtain further reliability in IGSCC and general corrosion resistance by the combined addition of Ti and Nb, and the prior oxidation treatments, respectively. (author).

1989-07-01

97

Corrosion resistance of #gamma#-solid solution and hardening #gamma#'-phase of nickel alloys in sodium sulfate and chloride melts  

International Nuclear Information System (INIS)

Corrosion testings of model alloys, corresponding by chemical composition to simple and complex-alloyed #gamma#- and #gamma#'-phases of nickel heat-resistant alloys are conducted in sodium sulfate and chloride melts. It is ascertained that heat resistant nickel alloys containing over 50 % of hardening #gamma#'-phase, are subject to disastrous sulfide corrosion (SC). Resistance against SC alloys containing below 50 % of #gamma#'-phase is determined by the resistance of #gamma#-solid solution. 10 refs., 3 figs., 2 tabs.

98

Ultra High Strength Beta Titanium Alloy for Fasteners.  

Science.gov (United States)

... Accession Number : ADD151811. Title : Ultra High Strength Beta Titanium Alloy for Fasteners. Descriptive Note : Journal article,. ...

99

Thermophysical Properties of Matter - The TPRC Data Series. ...  

Science.gov (United States)

... alloys--Lanthanum-- Magnesium--Magnasium &11oy8--Hagn*31Uft compounds--Manxganese--Manganes. alloys-- Mercury ...

2011-05-14

100

THERMAL STABILITY OF ALPHA-BETA TITANIUM ALLOY Ti ...  

Science.gov (United States)

... Accession Number : ADD109273. Title : THERMAL STABILITY OF ALPHA-BETA TITANIUM ALLOY Ti-5Al-2Cr-1Fe,. Corporate Author : ...

1975-08-01

101

THE SUSCEPTAEILITY OF MATERIALS  

Science.gov (United States)

Hilled Bend Spechene of an Alpha-Beta Titanium Alloy. Ti-6M14V. ..... The all beta titanium alloy was nllled from both sides; only the edges were taped. ...

102

Structure and Mechanical Properties of Boron-Doped Cubic ...  

Science.gov (United States)

... by the boron doping in most of the alloys except for Al66Mn9Zr25 + 50 ppm B alloy; permanent deformation at ultimate compressive strength is not ...

103

SIMS imaging studies of the corrosion of alloy 800 and alloy 600 surfaces under secondary side boiler conditions  

Energy Technology Data Exchange (ETDEWEB)

The nickel-rich superalloys Alloy 600 and Alloy 800 have been corroded in mildly alkaline deuterated aqueous conditions typical of secondary coolant circuits in a nuclear power station. The oxide films and substrates of these alloys have been analysed by imaging SIMS depth profiling, which makes it possible to describe elemental distribution in all three dimensions. The measurement of the distribution of the secondary ions NiO[sup -], FeO[sup -] and CrO[sup -] appears useful for detailing the behaviour of nickel, iron and chromium within oxidized phases. The measurement of D[sup -] distribution outlines the extent of oxide hydration. For Alloy 800, evidence of sodium migration into the grain boundaries of the alloy substrate is found. For Alloy 600, no grain boundary sodium ingress can be identified under comparable corrosion conditions. (author).

1992-08-01

104

SIMS imaging studies of the corrosion of alloy 800 and alloy 600 surfaces under secondary side boiler conditions  

International Nuclear Information System (INIS)

The nickel-rich superalloys Alloy 600 and Alloy 800 have been corroded in mildly alkaline deuterated aqueous conditions typical of secondary coolant circuits in a nuclear power station. The oxide films and substrates of these alloys have been analysed by imaging SIMS depth profiling, which makes it possible to describe elemental distribution in all three dimensions. The measurement of the distribution of the secondary ions NiO"-, FeO"- and CrO"- appears useful for detailing the behaviour of nickel, iron and chromium within oxidized phases. The measurement of D"- distribution outlines the extent of oxide hydration. For Alloy 800, evidence of sodium migration into the grain boundaries of the alloy substrate is found. For Alloy 600, no grain boundary sodium ingress can be identified under comparable corrosion conditions. (author).

106

Reduced activation activities  

Energy Technology Data Exchange (ETDEWEB)

Four low activation alloy classes, two austenitic and two ferritic, have been incorporated into the MOTA-1B experiment in the FFTF reactor to provide an early assessment of the suitability of such alloys for reactor service.

1984-01-01

107

Metal dusting behaviour of welded Ni-base alloys with different surface finish  

Energy Technology Data Exchange (ETDEWEB)

Welded Ni-base alloys and Alloy 800 were exposed under metal dusting conditions at 600 C and 650 C for up to 6000 hours. Alloy 800 was attacked very strongly already in the first days and Alloy 600 also rather soon and widespread, on both materials attack started mainly in the heat affected zone. Several surface states of Alloy 600: brushed, ground, sand-blasted and pickled were tried only grinding caused a modest delay and decrease of metal dusting attack. Generally the attack was less widespread but deeper at 650 C than at 600 C, also for Alloy 601 and 602. The latter alloys show minor, mainly local attack, but especially the welds are affected. TIG welding led to better resistance than hand-welding. (Abstract Copyright [2003], Wiley Periodicals, Inc.)

2003-10-01

108

Hydrogen in titanium alloy with 16 at% Mo  

International Nuclear Information System (INIS)

The effect of various hydrogen concentrations on the crystal lattice period and the hardness of titanium alloy was examined, the alloy containing about 16 at.% Mo (27.5 wt. % Mo) and having #beta# structure. The peculiar features of the mechanism of plastic deformation of the alloy were studied after adding hydrogen to it. A dependence of the crystal lattice period on the concentration of hydrogen was obtained for TixMoxH_2 alloy. It has been established that the hardness of the Ti-Mo alloy does not change when hydrogen is added to it. The presence of hydrogen introduces changes into the mechanism of deformation of #beta#-titanium alloy. The configuration of the inverse pole figures after rolling proves that the transverse slip process in an alloy with hydrogen is hampered, and that the coplanar slip process is developing in it.

109

Environmental Cracking of the Alpha-Beta Titanium Alloy, Ti ...  

Science.gov (United States)

... Accession Number : ADD120492. Title : Environmental Cracking of the Alpha-Beta Titanium Alloy, Ti-6Al-6V-2Sn,. Corporate ...

110

Effect of Stress and Strain Path on Cavity Closure During Hot ...  

Science.gov (United States)

... CLOSURE DURING HOT WORKING OF AN ALPHA/BETA TITANIUM ALLOY (PREPRINT) ... HOT WORKING OF AN ALPHA/BETA TITANIUM ALLOY ...

2007-07-01

111

Differences in synchrotron radiation induced gas desorption from stainless steel and aluminium alloy  

CERN Document Server

Differences in synchrotron radiation induced gas desorption from stainless steel and aluminium alloy

1990-01-01

112

Development of a FeCoNb Alloy to be used in Eddy Current ...  

Science.gov (United States)

... Accession Number : ADD336001. Title : Development of a FeCoNb Alloy to be used in Eddy Current Probes for Testing Ferromagnetic Tubes,. ...

113

Development of Lead-Free Copper Alloy-Graphite Castings  

Energy Technology Data Exchange (ETDEWEB)

In this project, graphite is used as a substitute for lead in order to maintain the machinability of plumbing components at the level of leaded brass. Graphite dispersed in Cu alloy was observed to impart good machinability and reduce the sizes of chips during machining of plumbing components in a manner similar to lead. Copper alloys containing dispersed graphite particles could be successfully cast in several plumbing fixtures which exhibited acceptable corrosion rate, solderability, platability, and pressure tightness. The power consumption for machining of composites was also lower than that of the matrix alloy. In addition, centrifugally cast copper alloy cylinders containing graphite particles were successfully made. These cylinders can therefore be used for bearing applications, as substitutes for lead-containing copper alloys. The results indicate that copper graphite ...

1999-10-01

114

DUCTILITY RATIO OF AGED BETA TITANIUM ALLOY  

Science.gov (United States)

... Title : DUCTILITY RATIO OF AGED BETA TITANIUM ALLOY. Corporate Author : NEW YORK UNIV NY SCHOOL OF ENGINEERING AND SCIENCE. ...

1962-01-02

115

Beta-21S: A High Temperature Metastable Beta Titanium Alloy ...  

Science.gov (United States)

... Accession Number : ADD144314. Title : Beta-21S: A High Temperature Metastable Beta Titanium Alloy. Descriptive Note : Conference Proceedings, ...

116

An overview of beta titanium alloy environmental behavior  

International Nuclear Information System (INIS)

Stemming from their unique combination of elevated strength, low density, and good overall corrosion resistance, beta titanium alloys have become attractive candidate materials for critical, high-stress, components in corrosive services. An overview of the comparative corrosion resistance of beta alloys to conventional alpha and alpha/beta titanium alloys in common industrial and aerospace service environments generally reveals attractive behavior depending on the environment and alloy composition and, in some cases, alloy condition. Expanded performance windows are especially noted for the molybdenum-rich beta alloys, particularly in regard to resisting reducing acids, stress corrosion, and high temperature localized chloride attack, along with hydrogen and oxidation resistance. Where applicable, implications of this enhanced corrosion performance on current ...

1993-02-21

117

Decay of "1"7"7T_a composite nucleus. Comparison of excitation functions for the reaction residues occurring in "1"2C + "1"6"5H_0 and "1"4N + "1"6"3D_y reactions  

International Nuclear Information System (INIS)

The experimental has been performed with a view to studying complete and incomplete fusion in "1"4N + "1"6"3D_y system below 7 MeV/nucleon. The excitation functions for several reactions have been measured using the activation technique and compared with the theoretical predictions based on statistical models. The codes ALICE-91 and CASCADE used earlier for the analysis of excitation functions in case of "1"2C + "1"6"5H_0 system have been used here also with the same set of input parameters. It has been observed that the theoretical calculations do not match with the experimental excitation functions well but the overall shape of the excitation function is reproduced satisfactorily. The composite nucleus ("1"7"7T_a) formed in this ("1"4N + "1"6"3D_y) case is the same as the one formed in "1"2C + "1"6"5H_0 system studied earlier. Measured excitation functions for the same decay channels in the two cases ...

2002-10-01

118

The corrosion resistance of alloy 800  

International Nuclear Information System (INIS)

Basic studies of the oxidation resistance of Fe-Cr binary and Fe-Cr-Ni ternary alloys in pure oxygen have shown that the excellent corrosion resistance of Alloy 800 is explicable in terms of the low defect concentrations and diffusion rates in the oxide forming on alloys of this composition in sufficiently oxidising environments. The performance of Alloy 800 in environments of particular importance to nuclear power generation is briefly reviewed to determine to what extent ideas derived from the basic studies of Fe-Cr-Ni ternary alloys are borne out in practice. The good corrosion resistance of Alloy 800 in steam and CO_2 and, to some extent, in molten salt environments is in agreement with the behaviour of ternary alloys in oxygen. Minor aliovalent alloying additions are only expected to have a significant effect on the ...

119

Study of the influence of alloying additions on the passivity of aluminum. Annual report 1 Dec 89-30 Nov 90  

Energy Technology Data Exchange (ETDEWEB)

Whereas supersaturated aluminum alloys demonstrate enhanced passivity, conventional aluminum alloys spontaneously pit in air-saturated chloride solutions. We have concentrated on three areas: evaluation and characterization of Al-W alloys, which exhibit the best corrosion performance of any alloy system studied to date; characterization of the passive-film structure of Al-Mo alloys; and production and characterization of Al-W and Al-Ta powders, which will be used for compaction into bulk material. Surface analysis of the Al-W passive films formed during polarization show surprising little oxidized solute compared to other alloys. These results indicate that the barrier layer formation and electrostatic repulsion mechanisms used to explain the passivity of other alloys are not involved here. Instead the W may act to stabilize the passive film ...

1991-03-01

120

A comparison of the low-cycle fatigue behavior of Alloy 800 and Alloy 800H  

International Nuclear Information System (INIS)

At 650"0C, the low-cycle fatigue life was essentially the same for the two alloys on the basis of strain amplitude, but Alloy 800H had a longer life on the basis of stress amplitude. A 500"0C, Alloy 800 and 800H exhibited longer fatigue lifetime than at 650"0C, with Alloy 800 exhibiting a 2-3 times longer life than Alloy 800H when compared on the basis of plastic strain range, whereas the difference was less pronounced when compared on the basis of stress amplitude. When a creep effect was introduced either by way of a hold time or a reduced frequency, Alloy 800 exhibited a greater reduction in life than did Alloy 800H. The dislocation structure changed from planar to cellular with increase in strain range, and extensive precipitation of M_2_3C_6 was noted within the grains for Alloy 800H and along grain boundaries for ...

121

VIPEX (Vital-area Identification Package EXpert) Software Verification and Validation  

International Nuclear Information System (INIS)

The purposes of this report are (1) to perform a Verification and Validation (V and V) test for the VIPEX(Vital-area Identification Package EXpert) software and (2) to improve a software quality through the V and V test. The VIPEX was developed in Korea Atomic Energy Research Institute (KAERI) for the Vital Area Identification (VAI) of nuclear power plants. The version of the VIPEX which was distributed is 3.2.0.0. The VIPEX was revised based on the first V and V test and the second V and V test was performed. We have performed the following tasks for the V and V test on Windows XP and VISTA operating systems: ? Testing basic functions including fault tree editing ? Testing all kind of functions ? Research for update from Visual BASIC 6.0 to Visual BASIC 2008

2003-12-01

122

The Benchmark Test Results of QNX RTOS  

International Nuclear Information System (INIS)

A Real-Time Operating System(RTOS) is an Operating System(OS) intended for real-time applications. Benchmarking is a point of reference by which something can be measured. The QNX is a Real Time Operating System(RTOS) developed by QSSL(QNX Software Systems Ltd.) in Canada. The ELMSYS is the brand name of commercially available Personal Computer(PC) for applications such as Cabinet Operator Module(COM) of Digital Plant Protection System(DPPS) and COM of Digital Engineered Safety Features Actuation System(DESFAS). The ELMSYS PC Hardware is being qualified by KTL(Korea Testing Lab.) for use as a Cabinet Operator Module(COM). The QNX RTOS is being dedicated by Korea Atomic Energy Research Institute (KAERI). This paper describes the outline and benchmarking test results on Context Switching, Message Passing, Synchronization and Deadline Violation of QNX RTOS under the ELMSYS PC platform

2010-10-01

123

Study on probability of failure for RPV nozzle region under severe accident conditions  

Energy Technology Data Exchange (ETDEWEB)

Most of previous study for creep rupture of RPV lower head under severe accident condition, have been focused on global failure of RPV lower head. In contract, the local failure of the RPV nozzle region has not been studied in detail. The existence and features of nozzle failure in LAVA-ICI specimen of KAERI and LHF-4 specimen of Sandia National Lab., are observed. It is confirmed that the nozzle failure of LHF-4 specimen is due to the hoop stress in the RPV. The tensile tests in various temperatures and the creep rupture tests in various temperatures and stresses, are accomplished. The finite element analysis for LAVA-ICI experiment was confirmed, and the stress and deformation analysis results are used in LAVA-ICI experiment. 17 refs., 34 figs., 3 tabs. (Author)

2001-04-01

124

Severe accident analysis for Wolsung nuclear power plants  

Energy Technology Data Exchange (ETDEWEB)

Severe accident analysis has been performed for the Wolsung nuclear power= plants in Korea to investigate severe accident phenomena of CANDU-600 reactors as a part of Level II PSA study. The accident sequence analyzed in this paper is loss of active heat sinks (LOAH) which is caused by loss of off-site power, diesel generators, and DC power. ISAAC (Integrated Severe Accident Analysis Code) computer code developed by KAERI (Korea Atomic Energy Research Institute) was used in this analysis. This paper describes the important thermal-hydraulics and source term behaviors in the primary system and inside containment, and the failure mechanisms of calandria vessel and containment. In addition, some insights for accident management program (AMP) are also given. (Author) 5 refs., 1 tab., 12 figs.

1997-05-01

125

Severe accident analysis for Wolsung nuclear power  

Energy Technology Data Exchange (ETDEWEB)

Severe accident analysis has been performed for the Wolsung nuclear power plants in Korea to investigate severe accident phenomena of CANDU-600 reactors as a part of Level II PSA study. The accident sequence analyzed in this paper is loss of active heat sinks (LOAH) which is caused by loss of off-site power, diesel generators, and DC power, ISAAC(Integrated Severe Accident Analysis Code) computer code developed by KAERI (Korea Atomic Energy Research Institute) was used in this analysis. This paper describes the important thermal-hydraulics and source term behaviors in the primary system and inside containment, and the failure mechanisms of calandria vessel and containment. In addition, some insights for accident management program (AMP) are also given.

1997-05-01

126

Review of Regulatory Quality Assurance Requirements for the Operation of Nuclear R and D Facilities  

International Nuclear Information System (INIS)

Korea Atomic Energy Research Institute (KAERI) has many R and D facilities in operation, including HANARO research reactor, radioactive waste treatment facility (RWTF), post-irradiation examination facility (PIEF) and irradiated material test facility (IMEF). Recently, nation-wide interest is focused on the safety and security of major industrial facilities. Safe operation of nuclear facilities is imperative because of the consequence of public disaster by radiological release/ contamination, in case of an accident. Recently, Ministry of Science and Technology (MOST) of the Korean government announced amendments of Atomic Energy laws to enforce requirements of the physical protection and radiological emergency. In this paper, the context of amended Atomic Energy laws were reviewed to confirm quality assurance measures and identify additional QA activities, if any, that is required by the amendment

2005-10-27

127

Regulatory Framework for Advanced Fuel Cycle Facility Using Pyroprocess in Korea  

International Nuclear Information System (INIS)

Nuclear power plants of 20 units of in Korea are generating about 700 MTU of spent fuels annually. The inventory of spent fuels in Korea were estimated about 10,087.07 MTU at end of 2008, and the storage space of spent fuels won't be available any more at 2016 due to the saturation of the spent fuel pools in the plants. In addition, in order to reduce carbon emission and correspond to the enormous electricity demand in Korea, 8 units of nuclear power plants are under construction and several more plants are under planning. The 100,000 MTU of spent fuel inventory are expected by the year of 2095 in Korea. Therefore, short term and long term of spent fuel management plans are under discussion and implementation in Korea. As a short term of spent fuel management strategy for the target year of 2016, central or local spent fuel dry interim storage options are mostly under discussion. As a long term of management plan, fast reactor and advanced fuel cycle R and D plan were approved by 255th ...

2010-10-01

128

Multi-Dimensional Analysis for Sodium Hot Pool using MARS-LMR in Steady State  

International Nuclear Information System (INIS)

DBEs (Design Basis Event) of KALIMER-600 (Korea Advanced Liquid Metal Reactor) were analyzed in one dimension by KAERI (Korea Atomic Energy Research Institute). KALIMER-600 is the pool type SFR (Sodium cooled Fast Reactor), thereby the sodium of primary system is prohibited movement to out of a reactor vessel. There are many contacting and including compositions in the sodium hot pool, such as IHX (Intermediate Heat eXchanger), DHX (Decay Heat eXchanger), Pump, UIS (Upper Internal Structure), and core. Moreover, the complex phenomena are occurred in sodium hot pool during steady and transient states. Therefore, the one dimensional analysis is modified to the multi-dimensional analysis through modification of sodium hot pool from one to three dimensions

2010-10-01

129

Insights from Development of Regulatory PSA Model for SMART  

International Nuclear Information System (INIS)

SMART (System-Integrated Modular Advanced Reactor) is a first-of-the-kind integral reactor with 330 MW thermal power under active development by Korea Atomic Energy Research Institute (KAERI) for power generation and seawater desalination. SMART employs various design features that are not typically found in other nuclear power plants. Examples include a unique passive residual heat removal system (PRHRS), and enclosure of a pressurizer, eight helical steam generators, and eight canned reactor coolant pumps inside the reactor pressure vessel. This paper presents risk insights on the SMART reactor gained during the development of a regulatory PSA model by Korea Institute of Nuclear Safety (KINS)

2010-10-01

130

Embedded systems for vacuum control at PEFP  

International Nuclear Information System (INIS)

Development of a front end system for a high energy proton accelerator is in progress at Korea Atomic Energy Research Institute (KAERI) for basic science and industrial applications. The proper vacuum components has been installed and operated successfully between ion source and RFQ. The reliable operation of the accelerator has been completed at vacuum system in the high and ultra high vacuum range under operating conditions. Proper control system for the vacuum instruments, based on PC operated by Windows, has been designed and constructed by control group at PAL. As PC operated by windows with inherent instability does not proper, embedded system can be replaced for reliable operation system, such as VME system operated by vxWorks.

2005-05-26

131

Beam Profile Measurement and its Application to Calculate Beam Emittance Using Wire Scanner for the PEFP 20MeV linac  

International Nuclear Information System (INIS)

A 20-MeV proton accelerator is developed by Proton Engineering Frontier Project (PEFP) at Korea Atomic Energy Research Institute (KAERI). The 20MeV accelerator consists of 50keV proton injector, 3MeV RFQ (Radio frequency Quadrupole), 20MeV DTL (Drift Tube Linac) and 20MeV beam line. The beam profile was measured at the end of the 20MeV beam line with wire scanner. Moreover the beam emittance was calculated from the quad scan method using beam line quadrupole magnets. In this paper, the beam profile measurement results are presented and the emittance measurement from the quad scan method is discussed

2010-10-01

132

Irradiation-assisted stress corrosion cracking in HTH Alloy X-750 and Alloy 625  

International Nuclear Information System (INIS)

In-reactor testing of bolt-loaded compact tension specimens was performed in 360 C water to determine the irradiation-assisted stress corrosion cracking (IASCC) behavior of HTH Alloy X-750 and direct-aged Alloy 625. New data confirm previous results showing that high irradiation levels reduce SCC resistance in Alloy X-750. Heat-to-heat variability correlates with boron content, with low boron heats showing improved IASCC properties. Alloy 625 is resistant to IASCC, as no cracking was observed in any Alloy 625 specimens. Microstructural, microchemical and deformation studies were performed to characterize the mechanisms responsible for IASCC in Alloy X-750 and the lack of an effect in Alloy 625. The mechanisms under investigation are: boron transmutation effects, radiation-induced changes in microstructure and deformation characteristics, and ...

1995-08-06

133

Interrelation between grain boundary characteristics and intergranular stress corrosion cracking of thermally treated alloy 690 and shot peened alloy 800 in high temperature acidic and alkaline solution  

Energy Technology Data Exchange (ETDEWEB)

To clarify the acidic and alkaline Intergranular Stress Corrosion Cracking (IGSCC) mechanism of thermally treated alloy 690 (alloy 690 TT) and shot peened alloy 800 (alloy 800 SP), C-ring tests were conducted in deaerated HCl solutions and in deaerated NaOH solutions at 350degC, compared with the acidic and the alkaline IGSCC susceptibilities of mill-annealed alloy 600 (alloy 600 MA), full-sensitized one (alloy 600 FS) and thermally treated one (alloy 600 TT). Grain boundary characteristics, such as chromium depleted zone and chromium carbide precipitation, were examined using modified Huey test and Transmission Electron Microscopy. Potential-pH diagram for Ni, Cr, Fe-H{sub 2}O system at 350degC was constructed and the solubilities of NiO, Cr{sub 2}O{sub 3} and Fe{sub 3}O{sub 4} were also calculated to evaluate the ...

2001-05-01

134

Interrelation between grain boundary characteristics and intergranular stress corrosion cracking of thermally treated alloy 690 and shot peened alloy 800 in high temperature acidic and alkaline solution  

International Nuclear Information System (INIS)

To clarify the acidic and alkaline Intergranular Stress Corrosion Cracking (IGSCC) mechanism of thermally treated alloy 690 (alloy 690 TT) and shot peened alloy 800 (alloy 800 SP), C-ring tests were conducted in deaerated HCl solutions and in deaerated NaOH solutions at 350degC, compared with the acidic and the alkaline IGSCC susceptibilities of mill-annealed alloy 600 (alloy 600 MA), full-sensitized one (alloy 600 FS) and thermally treated one (alloy 600 TT). Grain boundary characteristics, such as chromium depleted zone and chromium carbide precipitation, were examined using modified Huey test and Transmission Electron Microscopy. Potential-pH diagram for Ni, Cr, Fe-H_2O system at 350degC was constructed and the solubilities of NiO, Cr_2O_3 and Fe_3O_4 were also calculated to evaluate the stability of oxide films which ...

2001-05-01

135

Toroidal rotation braking with n = 1 magnetic perturbation field on JET  

International Nuclear Information System (INIS)

A strong toroidal rotation braking has been observed in plasmas with application of an n = 1 magnetic perturbation field on the JET tokamak. Calculation results from the momentum transport analysis show that the torque induced by the n = 1 perturbation field has a global profile. The maximal value of this torque is at the plasma core region (#rho# < 0.4) and it is about half of the neutral beam injection torque. The calculation shows that the plasma is mainly in the #nu#_-#sq root##nu# regime in the plasma core, but it is close to the transition between the 1/#nu# and #nu#_-#sq root##nu# regimes. The neoclassical toroidal viscosity (NTV) torque in the 1/#nu# and #nu#_-#sq root##nu# regimes is calculated. The observed torque is of a magnitude in between that of the NTV torque in the 1/#nu# and #nu#_-#sq root##nu# regimes. The NTV torque in the #nu#_-#sq root##nu# regimes is enhanced using the ...

2010-10-01

136

The clustering and transmission dynamics of pandemic influenza A (H1N1) 2009 cases in Hong Kong  

British Library Electronic Table of Contents (United Kingdom)

Objectives: Human influenza A (H1N1) 2009 has caused severe epidemics in many countries, but its dynamics in spatial and temporal contexts have so far been poorly appreciated. Methods: A total of 24,414 laboratory confirmed human influenza A (H1N1) 2009 cases reported from May to September 2009 in Hong Kong were evaluated, using a Geographic Information System (GIS)-based approach. Spatio-temporal clustering was assessed after dividing Hong Kong into 4 geographic sectors, 18 districts and 500 m x 500 m cells. Global Moran's I, Local Moran's I and SaTScan(TM) were used in the exploration. Results: Spatio-temporal clusters first appeared on Hong Kong Island at week 3, alongside multiple foci suggestive of infection nidus introduced from abroad. The clusters grew rapidly and became confluent ...

2011-01-01

137

Characteristic findings of pediatric inpatients with pandemic (H1N1) 2009 virus infection among severe and nonsevere illnesses  

British Library Electronic Table of Contents (United Kingdom)

We analyzed the clinical features of inpatients at a Japanese pediatric department who were infected with pandemic (H1N1) 2009 virus. Study participants included 46 children hospitalized from July 2009 to January 2010. Infection with the virus was confirmed using real-time reverse transcriptase polymerase chain reaction (RT-PCR). The epidemic month was October 2009; 34 patients were boys, and median age was 7?years. Pandemic influenza-associated respiratory diseases included pneumonia (n?=?42), bronchitis (n?=?3), and pharyngitis (n?=?1). The median time from onset to admission was 3?days. Children were divided into those with severe (n?=?32) versus nonsevere illnesses (n?=?14) according to Japanese guidelines. Significant features in the severe group were younger age, previous asthmatic a...

2011-01-01

139

Stress Corrosion Cracking Susceptibility of Beta Titanium Alloy 38-6-44: Candidate Alloy for Scout Torsion Bar.  

Science.gov (United States)

The threshold stress itensities for stress corrosion crack propagation in beta titanium alloy 38-6-44, Ti-3Al-8V-6Cr-4Mo-4Zr, has been determined in salt water and methanolic solutions. The alloy was immune to stress corrosion cracking in aqueous sodium c...

1974-01-01

140

Review of the corrosion resistance properties of Alloy 800 in high-temperature steam  

International Nuclear Information System (INIS)

The investigations carried out on Alloy 800 in aqueous high-temperature environments in France as well as in other countries are reviewed. These studies are mainly concerned with nuclear industry where Alloy 800 can be used as structural material for steam generators of PWR, breeders or HTR. As results referred to in the literature on cracking in caustic environmens do not always agree, a discussion is presented on the matter. The behaviour of Alloy 800 in superheated steam is examined. (Auth.).

141

Reactivity of ceramic superconductors with palladium alloys  

Science.gov (United States)

This paper reports Palladium alloy compositions investigated for suitability as a nonreactive material for the processing of ceramic superconductors. Barium-based superconductors were tested on Pd-Au and Pd-Ag alloys for reactivity. Bismuth-based superconductors were tested on a Pd-Ag alloy. The least reactive was found to be 70% Pd-30% Ag for the barium-based high-temperature superconductors (HTSC), whereas 30% Pd-70% Ag was found to be least reactive for bismuth-based HTSC.

1990-06-01

142

Postweld aging of a metastable beta-titanium alloy  

International Nuclear Information System (INIS)

(Nov 1973). United States Greenfield, MA Pierce, CM Chicago, IL.

143

Modification of surface properties of copper-refractory metal alloys  

Energy Technology Data Exchange (ETDEWEB)

The surface properties of copper-refractory metal (CU-RF) alloy bodies are modified by heat treatments which cause the refractory metal to form a coating on the exterior surfaces of the alloy body. The alloys have a copper matrix with particles or dendrites of the refractory metal dispersed therein, which may be niobium, vanadium, tantalum, chromium, molybdenum, or tungsten. The surface properties of the bodies are changed from those of copper to that of the refractory metal.

1993-10-12

146

Investigation of Destruction Mechanisms in Reactor Steels  

International Science & Technology Center (ISTC)

Investigation of Destruction Mechanisms in Reactor Steels and Alloys under Cycling Deformation

150

General corrosion of ALLOY 800 in high temperature water and its prevention  

Energy Technology Data Exchange (ETDEWEB)

General corrosion behavior of ALLOY 800 in high temperature water was studied in relation to its surface film structure. The surface film formed in water was found to decrease the corrosion rate of ALLOY 800. This film is composed of Ni ferrite, and can be obtained by oxidation in air or steam. Based on these results, air or steam oxidation treatment to inhibit Ni and Co release of ALLOY 800 into high temperature water is proposed. (author).

1989-10-01

151

General corrosion of ALLOY 800 in high temperature water and its prevention  

International Nuclear Information System (INIS)

General corrosion behavior of ALLOY 800 in high temperature water was studied in relation to its surface film structure. The surface film formed in water was found to decrease the corrosion rate of ALLOY 800. This film is composed of Ni ferrite, and can be obtained by oxidation in air or steam. Based on these results, air or steam oxidation treatment to inhibit Ni and Co release of ALLOY 800 into high temperature water is proposed. (author).

154

Effect of aging on the pitting corrosion behavior in Al-Li alloys  

Energy Technology Data Exchange (ETDEWEB)

In the present work, electrochemical measurements and corrosion tests in NaCl solutions were carried out to study the effect of aging treatments on pitting corrosion behavior in a 8090 alloy and its high purity Al-Li binary alloy analogue. The pitting corrosion characteristics and corrosion resistance of the 8090 alloy have been determined in relation to precipitation microstructures. (orig.).

1990-06-01

156

EFFECT OF MICROSTRUCTURE ON THE STRENGTH ...  

Science.gov (United States)

... THE STRENGTH, TOUGHNESS, AND STRESS-CORROSION CRACKING SUSCEPTIBILITY OF A METASTABLE BETA TITANIUM ALLOY (Ti-11. ...

1970-02-01

157

Direct production of niobium titanium alloy during niobium reduction  

International Nuclear Information System (INIS)

This paper describes a process for the direct production of a superconductive niobium-titanium alloy during reduction of niobium pentoxide. It comprises: mixing at least one of titanium metal powder and titanium dioxide powder with niobium pentoxide powder and aluminum powder; heating the resulting mixture to form a niobium-titanium alloy and a slag consisting essentially of aluminum oxide; and separating the alloy and the slag.

1989-10-26

158

Development of zirconium alloys. Part II  

Science.gov (United States)

A number of alloys of zirconium have been investigated as part of a program aimed at improving the high-temperature tensile and creep strength of zirconium. These alloys include aluminum, beryllium, lead, magnesium, molybdenum, niobium, tantalum, tin, titanium, tungsten, vanadium, and zinc, binary and ternary alloys. The data indicate that aluminum, lead, molybdenum niobium, tin, titanium, tungsten, and vanadium can be used successfully to harden zirconium, and that aluminum, tin, titanium, and vanadium are particularly effective in maintaining the strength of zirconium at elevated temperatures.

1952-01-02

159

Corrosion resistance of zinc coatings on depleted uranium and uranium alloys  

Energy Technology Data Exchange (ETDEWEB)

Simulated atmospheric corrosion studies were performed to determine the corrosion protection provided by galvanized zinc coatings on depleted uranium, U-0.75 Ti alloy, and U-6 Nb alloys. The accelerated ASTM tests consisted of exposing the galvanized samples to aqueous and aqueous chloride environments. The test results showed that anodic protection was provided by the electronegative zinc coatings on uranium and uranium alloys. Treating zinc with chromate conversion coatings also provided more protection.

1985-01-27

160

Carbon effect on the structure and plasticity characteristics of titanium #beta#-alloys  

International Nuclear Information System (INIS)

In this paper a study is made of the structure and mechanical properties of the #beta# alloy system Ti-Mo-Zr-Sn (the composition of which is equivalent to the #beta# III alloy used abroad) containing different amounts of carbon. Study of the #beta#-titanium alloy containing 0.1% C revealed the presence of particles of titanium carbide. Separation of the titanium carbide promotes a reduction in impact strength, an increased tendency toward cold shortness, and poorer workability. (author).

161

Ultra high strength beta titanium alloy for fasteners  

International Nuclear Information System (INIS)

A new high strength titanium alloy has been developed primarily intended for fastener applications. While Ti-6Al-4V is used extensively as a fastener alloy in the aerospace industry, its shear strength allowable is limited to 655 MPa (95 ksi). For higher shear strength requirements, various steels or nickel-based alloys are used (up to 860 MPa (125 ksi)), but with the attendant density penalty. This new alloy is intended to provide the 860 MPa shear strength at roughly a 40% weight savings. After screening various alloy systems, the optimum chemistry has been selected as follows: Ti-6.0V-6.2Mo-5.7Fe-3Al. In light of its 125 ksi shear strength goal, the alloy has been designated TIMETAL reg-sign 125.

1993-02-21

162

Tensile properties and bending formability of drawn magnesium alloy pipes  

Energy Technology Data Exchange (ETDEWEB)

Magnesium alloys are being increasingly utilized in a variety of fields as an alternative material to organic materials and aluminum alloys, owing to excellent properties. Those include low density, and excellent damping properties. When compared to organic materials, furthermore, Mg alloy excels at recyclability, heat radiation, and electromagnetic-shielding. Though most of magnesium alloy products are manufactured through die-casting and thixo-molding at present, the demand for the expanding of magnesium wrought alloy market is increasing. Taking full advantage of a drawing technique and applying it to the conventional extruded pipe, we have developed a new type of magnesium alloy pipe. The strength of the developed pipe is significantly higher than that of the conventional one, either extruded or die-casting. Some of the excellent properties were obtained ...

2003-07-01

163

Production of powder titanium alloys with Mo, Zr, Nb additions and their properties  

International Nuclear Information System (INIS)

In order to substitute expensive cast titanium alloys by powder ones the possibility of introduction of powder additions by mechanical stock mixing is studied. It is shown that microstructure of powder alloys of Ti-Zr(1-9%) system is typical for one-phase cast #alpha#-alloys. The Ti-Mo(1-9%) and Ti-Nb(1-9%) system alloys have microstructure typical for two-phase (#alpha#+#beta#)-alloys. For homogeneous structure to be obtained the high temprature annealing is advisable after hot pressing. Alloying with Mo, Zr and Nb permits to increase considerable the strength of powder titanium products (at 9% Mo more than two times).

164

Passivity of high corrosion resistant Cu-Al-Sn alloys  

Energy Technology Data Exchange (ETDEWEB)

In a work studying the corrosion and tarnishing properties of a variety of copper alloys, the alloy Cu-A110-Sn5 was found to show an excellent corrosion resistance in neutral solutions, where copper and most conventional Cu alloys are covered by thick nonprotective surface layers. The passive films formed on this alloy were characterized with electrochemical and photoelectrochemical methods. The pH dependence of the passivation and of the photocurrent behavior of the Cu-A110-Sn5 alloy clearly indicates that the passivity of this alloy in neutral solutions is due to a formation of passive film enriched with aluminum oxide. At corrosion potential a strong increase in the corrosion resistance with time is due to a gradual enrichment of the surface with aluminum oxide. This can be seen in the photocurrent spectra which change from cooper-type to aluminum-type with ...

1993-10-01

165

High-temperature property data: Ferrous alloys  

Energy Technology Data Exchange (ETDEWEB)

In this book over 250 alloys are organized by AISI number into 10 major sections: Irons, Carbon Steels, Alloy Steels, Low Alloy Constructional Steels, Ultra High Strength Steels, Tool Steels, Maraging Steels, Wrought Stainless Steels, Heat Resistnat Casting Alloys, and Iron Based Rought Superalloys. Each alloy record lists the designation, specifications, UNS number, composition, product forms and a comment on the high-temperature properties and applications. Referenced data is then given for physical properties such as density, specific heat, thermal conductivity, thermal expansion, electrical conductivity, Poisson's ratio, moduli of elasticity and rigidity, etc. Mechanical properties follow, and include tensile properties, shearing and bearing properties, impact properties, creep, stress rupture and stress relaxation and fatigue properties. The last part of the ...

1987-01-01

166

Fundamental reasons for the good performance of Alloy 800 in nuclear steam generators  

Energy Technology Data Exchange (ETDEWEB)

It is hypothesized that the good performance of Alloy 800 in steam generator service is due to its relative immunity to two distinct mechanisms of stress corrosion cracking; the argument also applies to intergranular corrosion. One mechanism operates in the high-nickel region (Alloy 600 and nearby model alloys) and is due to internal intergranular oxidation. The other operates in the low-nickel (stainless steel) region and is due to de-alloying of Fe and/or Cr. This latter mechanism may, under special conditions, operate in high-Ni, high-Cr alloys such as 690. Some essential features of the de-alloying mechanism are demonstrated using strong caustic solutions, and the prospect of extending this approach to dilute high-temperature environments is discussed. (author)

2007-07-01

167

Fatigue of magnesium alloys  

Energy Technology Data Exchange (ETDEWEB)

Magnesium alloys show a high specific strength and are therefore increasingly used for light-weight constructions in transportation industry.{sup [1,2]} To predict the behaviour of the material under the influence of cyclic loading it is vital to understand the fatigue behaviour of magnesium alloys. Only when understood properly, it is possible to fully apply the potential weight reduction by using magnesium alloys. A very important aspect in fatigue of magnesium alloys is the influence of a corrosive media and elevated temperatures, of which both are relevant in automotive applications. These two factors tend to have deleterious effects on magnesium alloys and therefore also have to be considered in investigations on the fatigue behaviour of magnesium alloys. (Abstract Copyright [2004], Wiley Periodicals, Inc.)

2004-05-01

168

Colorimetric analysis of opaque porcelain fired to different base metal alloys used in metal ceramic restorations  

British Library Electronic Table of Contents (United Kingdom)

Statement of problem. The popularity of base metal alloys has considerably increased in recent years because of their superior mechanical properties as well as the high cost of noble alloys. However, there is disagreement about their effect on the opaque porcelain color and the color differences among base metal alloys. Purpose. The purpose of this in vitro study was to determine and compare the influence of various commercially available base metal alloys (excluding titanium-based systems) on the resulting color of opaque porcelain with the use of a colorimetric device. Material and methods. Fourteen different types of Ni-Cr and 3 different types of Co-Cr porcelain bonding alloys were selected with a Au-Pd alloy (V-Delta SF) as the control group for colorimetric measurements and determina...

2008-01-01

169

The minimal series of N=1 and N=2 superconformal topological field theory  

International Nuclear Information System (INIS)

We obtain conformal invariant topological field theories with N = 2 supersymmetry by twisting Sevrin, Troost and Van Proeyen's SU(2) x SU(2) x U(1) extended N = 4 superconformal field theories. We expect that the number of physical states is finite although the original N = 4 theories have continuous spectra. It is shown that the number of physical states is actually finite when the central charge c < 6 in the corresponding N = 4 theories. The physical states inherit the structure of the chiral ring in N = 2 superconformal minimal series which is obtained by the reduction from N = 4 theories. We also show that the algebra contains the topological N = 4 superconformal algebra as subalgebra. Therefore a closed set of a finite number of physical states in the topological N = 1 superconformal algebra can also be obtained. (orig.).

1991-06-01

170

R-matrices for highest weight representations of s-circumflexl{sub q}(2,C) at roots of unity  

Energy Technology Data Exchange (ETDEWEB)

The general formula is obtained for R-matrices of s-circumflexl{sub q}(2,C) for the highest weight representations both for general q and for q being a root of unity by generalizing G. Gomez`s and Sierra`s one for semiperiodic representations of s-circumflexl{sub q}(2,C) at roots of unity. In a case of general q, direct matrix form is obtained for the well known Jimbo`s R-matrix. In a case of q{sup N}=1 for semiperiodic and spin j<(N-1)/2 representations the new R-matrices are obtained which together with Jimbo`s one obey the spectral parameter dependent Yang-Baxter equations. (author) 16 refs.

1992-10-01

171

Linear family of Lie brackets on the space of matrices $Mat(n\\times m,\\K)$ and Ado's Theorem  

CERN Document Server

In this paper we classify a linear family of Lie brackets on the space of rectangular matrices $Mat(n\\times m,\\K)$ and we give an analogue of the Ado's Theorem. We give also a similar classification on the algebra of the square matrices $Mat(n, \\K)$ and as a consequence, we prove that we can't built a faithful representation of the $(2n+1)$-dimensional Heisenberg Lie algebra $\\mathfrak{H}_n$ in a vector space $V$ with $\\dim V\\leq n+1$. Finally, we prove that in the case of the algebra of square matrices $Mat(n,\\K)$, the corresponding Lie algebras structures are a contraction of the canonical Lie algebra $\\mathfrak{gl}(n,\\K)$.

2008-01-01

172

Fusion algebras of fermionic rational conformal field theories via a generalized Verlinde formula  

International Nuclear Information System (INIS)

We prove a generalization of the Verlinde formula to fermionic rational conformal field theories. The fusion coefficients of the fermionic theory are equal to sums of fusion coefficients of its bosonic projection. In particular, fusion coefficients of the fermionic theory connecting two conjugate Ramond fields with the identity are either one or two. Therefore, one is forced to weaken the axioms of fusion algebras for fermionic theories. We show that in the special case of fermionic W(2, #delta#)-algebras these coefficients are given by the dimensions of the irreducible representations of the horizontal subalgebra on the highest weight. As concrete examples we discuss fusion algebras of rational models of fermionic W(2, #delta#)-algebras including minimal models of the N = 1 super Virasoro algebra as well as N = 1 super W-algebras SW(3/2, #delta#). (orig.).

1994-02-01

173

Circular map for supercavitating flow in a multiply connected domain  

British Library Electronic Table of Contents (United Kingdom)

A nonlinear free boundary-value problem of supercavitating flow past n + 1 hydrofoils is analyzed. To describe the cavities' closure mechanism, the Tulin-Terentev single-spiral-vortex model is employed. The flow domain is considered as the image of an (n + 1)-connected circular domain. The conformal map is constructed in terms of the solutions to two Riemann-Hilbert problems of the theory of symmetric automorphic functions. One of the problems is homogeneous and its coefficients are continuous functions while the second problem is inhomogeneous and has discontinuous coefficients. The exact solutions to the problems are found by using quasiautomorphic and quasimultiplicative analogs of the Cauchy kernel. The case of a single plate is considered in detail and the numerical results are report...

2009-01-01

174

A Hypothesis: Supplementation with Mushroom-Derived Active Compound Modulates Immunity and Increases Survival in Response to Influenza Virus (H1N1) Infection.  

Science.gov (United States)

We hypothesize that the mushroom-derived active compound may be a potential strategy for increasing survival in response to influenza virus (H1N1) infection through the stimulation of host innate immune response. The validity of the hypothesis can be tested by immune response to influenza infection as seen through survival percentage, virus clearance, weight loss, natural killer cell cytotoxicity, Tumor Necrosis Factor-? (TNF-?) and Interferon-gamma (IFN-?) levels, lytic efficiency in the spleens of mice and inducible nitric oxide synthase mRNA expressions in RAW 264.7 murine macrophage cells. The hypothesis may improve people's quality of life, reduce the medical cost of our healthcare system and eliminate people's fears of influenza outbreak. PMID:21660092

2011-03-20

175

Summary on performance study of corrosion resistance of zirconium alloys  

International Nuclear Information System (INIS)

Zirconium-base alloys are used primarily as fuel cladding material and other core structure material in water cooled nuclear power reactors. Main research achievements and problems about corrosion of zirconium alloys are reviewed; the present theories and challenge are summarized. In the 1980s, great progress had been made towards correlating alloy composition, microstructure and irradiation with corrosion resistance. In the 1990s, main researches are focused on exploring actual mechanism of corrosion, optimizing both alloy composition and microstructure in order to minimize the fuel cycle costs through burnup optimization.

176

Stress corrosion cracking susceptibility of #beta# titanium alloy 38-6-44  

International Nuclear Information System (INIS)

The threshold stress intensities for stress corrosion crack propagation in beta titanium alloy 38-6-44, Ti3Al-8V-6Cr-4Mo-4Zr, has been determined in salt water and methanolic solutions. The alloy was immune to stress corrosion cracking (SCC) in aqueous sodium chloride solutions (marine atmosphere). However, in methanolic solutions, the alloy was very susceptible to SCC. This marked susceptibility in methanolic solutions can be mitigated by the addition of an inhibitor: sodium nitrate. Crack extension in the alloy was transgranular and failure occurred by brittle quasi-cleavage in methanolic solutions.

177

SP-700 titanium alloy data sheets  

International Nuclear Information System (INIS)

SP-700, an emerging #beta#-rich #alpha#+#beta# titanium alloy, is designed to improve superplastic formability as well as mechanical properties over Ti-6Al-4V alloy. Owing to its fine microstructure and low #beta#-transus temperature, it is superplastic-formable at temperature below 1,073K (800 C) with low flow stress. Remarkable workability of this alloy is also retained in conventional Manufacturing processes. Another advantage of SP-700 is heat treatment response which includes deep hardenability and quick aging kinetics. Corrosion resistance and machinability are equivalent to or better than Ti-6Al-4V alloy.

1993-02-21

178

Quench effect on mechanical properties and structure of the TS6 #beta#-titanium alloy  

International Nuclear Information System (INIS)

By the methods of microstructural and electron-microscopic analyses by the tension test and impact test studied is the effect of quenching conditions on structure and mechanical properties of the TS6 titanium-#beta# alloy. It is shown that low temperature quenching from 700 deg C, recommended earlier for analogous VT15 titanium alloy, leads to appearence of intercrystalline fracture and to sharp decrease of impact strength of the TS6 alloy. Established are optimum conditions for quenching of half-finished products and articles of the TS6 alloy depending on their subsequent working or operation.

179

Nature of the magnetic susceptibility of dysprosium. Paramagnetic susceptibility of dysprosium - yttrium alloys  

International Nuclear Information System (INIS)

The paramagnetic susceptibility of single crystals of dysprosium-yttirum alloys is measured in the basal plane and along the hexagonal axis. It is shown that the susceptibility of the alloys obeys the Curie-Weiss law, the effective magnetic moments allong the different directions being the same and the paramagnetic Curie temperatures being different. The difference between the paramagnetic Curie temperatures in the basal plane and along the hexagonal axis is independent of the dysprosium concentration in the alloy. As a comparison with the theoretical models of magnetic anisotropy shows, this is an indication that the magnetic anisotropy of dysprosium - yttrium alloys is of a single-ion nature.

1976-01-01

180

Mechanisms of Alloy 800 corrosion in helium  

International Nuclear Information System (INIS)

Cr_2O_3 scales are found to form on Alloy 800 and a similar pure ternary alloy in air, and 1 and 50 atm. helium containing oxidizing impurities typical of those in an SGHTR. The strong temperature dependence and neglibible helium overpressure dependence indicate that gas transport through the scales is not rate controlling. Surface oxidation rates are therefore controlled by solid state diffusion and the low oxygen partial pressure dependence of the oxidation rate in Alloy 800 is ascribed to the presence of extrinsic defects in the Cr_3O_3 (due to doping by alloying elements) or to the presence of short circuit diffusion paths. (Auth.).

181

Friction stir welding of dissimilar formed Mg alloys (AZ31/AZ91)  

Energy Technology Data Exchange (ETDEWEB)

Friction stir welding of dissimilar formed Mg alloys(AZ31/AZ91) was successfully carried out at the limited welding conditions. In a sound joint, SZ was mainly consisted of AZ31 Mg alloy which was located the retreating side. Dynamic recrystallization and grain growth occurred and {beta} intermetallic compounds of AZ 91 Mg alloy was not observed in SZ. BM had a higher hardness than that of the weld zone. The fracture location was not weld zone but BM of the AZ91 Mg alloy in tensile test. (orig.)

2005-07-01

182

Time-temperature-precipitation and time-temperature-sensitization behavior of highly corrosion resistant nickel-chromium-molybdenum alloys. Das Zeit-Temperatur-Ausscheidungs- und das Zeit-Temperatur-Sensibilisierungs-Verhalten von hochkorrosionsbestaendigen Nickel-Chrom-Molybdaen-Legierungen  

Energy Technology Data Exchange (ETDEWEB)

The time-temperature-precipitation diagrams and the resulting time-temperature-sensitization diagrams have been established and are presented for today's current nickel-chromium-molybdenum alloys C-4, C-276, 22 and the recently developed alloy 59. Compared to those materials alloy 625 behaves differently due to its high niobium content. In addition, also the precipitation and sensitization of alloy G-3 has been established. Under the materials considered alloy C-276 has the strongest tendency to precipitate the intermetallics Mu and P together with the carbide M{sub 6}C at intermediate temperatures, followed by the alloys 22 and 59. The tendency to sensitization in the sense of the 50{mu}m (2 mils) intercrystalline penetration criterion when exposed to the ASTM G-28, method A test solution is greatest with alloy C-276, and decreases ...

1992-05-01

183

The effect of age hardening on creep crack growth in alloy 800  

International Nuclear Information System (INIS)

The creep crack growth properties of two versions of Alloy 800 have been compared at 500 and 600"0C in the Grade II condition in tests up to 10"4 hours duration. The two alloys were a low carbon alloy containing (wt.%) 0.024 C, 0.5 Ti, 0.3 Al (Alloy B) and a higher carbon alloy containing (wt.%) 0.038 C, 0.2-0.3 Ti, 0.2-3.0 Al (Alloy J). At 600"0C, Alloy B attained maximum age hardening in 10"2 hours, whereas J did not harden significantly in time up to 10"4 hours. Both alloys age hardened at 550"0C with Alloy J hardening more rapidly than B. The creep displacements and displacement rates in small compact tension specimens at 600"0C were smaller than Alloy B than in Alloy J. However, failure times were shorter in Alloy B because of lower ...

184

Investigation on corrosion and wear behaviors of nanoparticles reinforced Ni-based composite alloying layer  

Energy Technology Data Exchange (ETDEWEB)

In order to investigate the role of amorphous SiO{sub 2} particles in corrosion and wear resistance of Ni-based metal matrix composite alloying layer, the amorphous nano-SiO{sub 2} particles reinforced Ni-based composite alloying layer has been prepared by double glow plasma alloying on AISI 316L stainless steel surface, where Ni/amorphous nano-SiO{sub 2} was firstly predeposited by brush plating. The composition and microstructure of the nano-SiO{sub 2} particles reinforced Ni-based composite alloying layer were analyzed by using SEM, TEM and XRD. The results indicated that the composite alloying layer consisted of {gamma}-phase and amorphous nano-SiO{sub 2} particles, and under alloying temperature (1000 deg. C) condition, the nano-SiO{sub 2} particles were uniformly distributed in the alloying layer and still kept the amorphous structure. ...

2008-04-30

185

Investigation on corrosion and wear behaviors of nanoparticles reinforced Ni-based composite alloying layer  

International Nuclear Information System (INIS)

In order to investigate the role of amorphous SiO2 particles in corrosion and wear resistance of Ni-based metal matrix composite alloying layer, the amorphous nano-SiO2 particles reinforced Ni-based composite alloying layer has been prepared by double glow plasma alloying on AISI 316L stainless steel surface, where Ni/amorphous nano-SiO2 was firstly predeposited by brush plating. The composition and microstructure of the nano-SiO2 particles reinforced Ni-based composite alloying layer were analyzed by using SEM, TEM and XRD. The results indicated that the composite alloying layer consisted of ?-phase and amorphous nano-SiO2 particles, and under alloying temperature (1000 deg. C) condition, the nano-SiO2 particles were uniformly distributed in the alloying layer and still kept the amorphous structure. The corrosion resistance of composite ...

2008-04-30

186

Novel alloys to improve the electrochemical behavior of zinc anodes for zinc/air battery  

Energy Technology Data Exchange (ETDEWEB)

In our continued efforts for improving the performance of zinc anodes for a Zn/air battery, we now report the preparation of three alloys and improved performances of anodes made up with these alloys. The alloys contained zinc, nickel, and indium with different weight percentages and were calcined at two different temperatures. Out of the six alloys, the alloy which has a composition of zinc 90%, nickel 7.5% and Indium 2.5% and fired at 500{sup o}C is found to be the best. In the case of the hydrogen evolution reaction, this alloy had its potential shifted to a more negative potential. As far as the cyclic voltammograms were concerned, the difference between the anodic and cathodic part was minimal when compared with other alloys. Surprisingly, this alloy had reversibility even after 100 cycles of the cyclic ...

2006-10-06

187

Hydrogen embrittlement of Ni-Cr-Fe alloys  

Energy Technology Data Exchange (ETDEWEB)

The purpose of this work was to investigate the role of chromium on hydrogen embrittlement of Ni-Cr-Fe alloys and thus to develop a better understanding of the low-temperature stress corrosion cracking (SCC) phenomenon. The effect of chromium on hydrogen embrittlement was examined using tensile tests followed by material evaluation via scanning electron microscopy (SEM) and light optical microscopy. Four alloys were prepared with chromium contents ranging from 6 to 35 wt pct. In the uncharged condition, ductility, as measured by the percent elongation or reduction in area, increased as the alloy chromium content increased. Hydrogen appeared to have only minor effects on the mechanical properties of the low-chromium alloys. The addition of hydrogen had a marked effect on the ductility of the higher-chromium alloys. In the 26 pct chromium alloy, the elongation to ...

1997-03-01

188

High temperature fatigue damage in three austenitic alloys  

Energy Technology Data Exchange (ETDEWEB)

A series of cyclic strain controlled tests have been carried out at 600/sup 0/C on three high temperature austenitic iron-based alloys, AISI type 316 stainless steel, Alloy 800 H and Sandvik 253 MA. The tests were carried out under constant total strain control using a constant strain rate of 0.005 s/sup -1/. By considering the changes in modulus throughout the life of each specimen it was found that damage evolution could be successfully predicted as a function of plastic strain range despite the fact that each alloy had been chosen because of a different stress response at 600/sup 0/C. Although each alloy accumulated fatigue damage in a similar manner the longer lives of Sandvik 253 MA and Alloy 800 H at a given total strain range were due to a smaller plastic strain component and a reduced stage I crack propagation rate. In the 253 MA alloy, slip was ...

1988-01-01

189

Dislocation-enhanced hydrogen solubilities in Pd-Ni, Pd-Ag and Pd-Ni-Ag alloys  

Science.gov (United States)

The purpose of this communication is to determine whether the solubility enhancements for cold-worked Pd-Ni alloys increase or decrease with atom fraction of Ni. Substitutional Ni atoms contract and Pd lattice, in contrast to the lattice expansion resulting from substitutional Ag in Pd. The Pd-Ni alloy system forms a continuous series of fcc solid solution alloys over the whole composition range. The solubility enhancements will also be determined for a series of homogeneous, ternary Pd[sub 1[minus]x]Ni[sub 1/2x]Ag[sub 1/2x] alloys for x in the range from 0 to 0.2. For this series of ternary alloys the fcc lattice parameters do not change significantly from that of pure Pd. The alloys used in this research were purchased from Tanaka Kikinzoku Kogyo K.K. The detailed experimental procedure has been described previously. The alloys were all ...

1994-03-01

190

Alternate alloying for environmental resistance; Proceedings of the Symposium, New Orleans, LA, Mar. 2-6, 1986  

Energy Technology Data Exchange (ETDEWEB)

Papers are presented on the development of oxidation- and sulfidation-resistant ferritic alloys; the microstructural stability of sulfidation-resistant FeCrAl stainless steels around 500 C; age hardening in Fe-Mn-Al-C austenitic alloys; the oxidation/corrosion behavior of low-Cr Fe-Cr-Ni alloys containing Zr or Nb; the high temperature oxidation/corrosion of iron-based superalloys; and the role of Mo in the Na/sub 2/SO/sub 4/ induced corrosion of superalloys at high temperature. Topics discussed include the effect of variations of Co content on the cyclic oxidation resistance of selected Ni-base superalloys; high temperature oxidation of Fe based alloys; the morphological development of high temperature oxide scales of Fe-Mn-Al base alloys; and the oxidation of an Fe-Mn-Al-C alloy at 1000 C. Consideration is given to the corrosion properties of Fe-Mn-Al ...

1987-01-01

191

The nucleus "1"4"3Nd attempt on complete spectroscopy  

International Nuclear Information System (INIS)

The 142Nd and 143Nd nucleus excited states have been studied using the "1"4"2","1"4"3Nd(p,p') and "1"4"0Ce(#alpha#,n)"1"4"3Nd reactions. The energy level schemes were determined as well as spectroscopic information about spin, parity and multipolarity of electromagnetic transitions. 54 refs, 25 figs, 9 tabs.

1991-01-01

192

The Coulomb gas representation for SU(2) Wess-Zumino-Witten model in superspace  

Energy Technology Data Exchange (ETDEWEB)

This paper gives a Coulomb gas representation for level kN = 1 supersymmetric SU(2) Kac-Moody algebra in terms of three free scalar superfields. It is clarified how this representation reduces to a Coulomb gas representation for the corresponding bosonic SU(2) Kac-Moody algebra and the free fermionic algebra. The primary superfields and the correlation functions, which satisfy the supersymmetric Knizhnik-Zamolodchikov equation, are also discussed.

1991-09-10

193

Strengh functions of strontium 88 obtained from the analysis of the (#gamma#,n) reaction near the threshold  

International Nuclear Information System (INIS)

The results of photoneutron spectra measurements for the reaction (#gamma#,n) on the Sr-88 nuclei near threshold are presented. The parameters of resonance levels, as well as radiative S_#gamma#"("1") and neutron S_n"("1") strength functions for transitions on the first excited level of Sr-87 were obtained. 2 refs.; 1 fig.; 1 tab.

1987-09-14

194

Preventable H5N1 avian influenza epidemics in the British poultry industry network exhibit characteristic scales  

UK PubMed Central (United Kingdom)

Epidemics are frequently simulated on redundantly wired contact networks, which have many more links between sites than are minimally required to connect all. Consequently, the modelled pathogen can...Full Text Available

2010-04-06

195

Preparation and radiolabeling of IBZM: a potential D-2 specific brain imaging agents for SPECT  

International Nuclear Information System (INIS)

In developing new receptor-site specific brain imaging agents labeled with I-123 for single photon emission computed tomography (SPECT), an analog of raclopride, 3-["1"2"5I]-iodo-N-[(1-ethyl-2-pyrrolidinyl)-methyl]-2-hydroxy-6-me-thoxy benzamide (IBZM), was prepared using a method similar to that reported for raclopride and its derivatives. (author).

197

Extended superconformal algebra from super Toda field theory  

International Nuclear Information System (INIS)

We propose and construct a new type of extended superconformal algebra (ESA) based on the super Toda field theory. Both in the N = 1 ESA and in the N = 2 ESA, an arbitrary value of the central charge is allowed in contrast with the previously known super W-algebra. The generators of ESA are interpreted as the constants of motion in the super Toda field theory. (orig.).

1991-01-01

199

AQ4N: an alkylaminoanthraquinone N-oxide showing bioreductive potential and positive interaction with radiation in vivo.  

UK PubMed Central (United Kingdom)

AQ4N (1,4-bis([2-(dimethylamino-N-oxide)ethyl]amino)5,8-dihydroxy- anthracene-9,10-dione) is a novel alkylaminoanthraquinone N-oxide which, on reduction, forms a stable DNA affinic cytotoxic compound...Full Text Available

1995-07-01

200

Specific features of radiation damage in titanium alpha-alloys  

International Nuclear Information System (INIS)

Titanium base 'alpha'-alloys (Pt-7M, RK-20 and Ti-5Al-2Zr-1.5V) are considered for their behaviour under neutron irradiation. The role of alloying elements in radiation hardening is discussed depending of neutron fluence and irradiation temperature. For PK-20 alloy three stages of change in mechanical properties are revealed which are following: incubation period and weak hardening, intense radiation hardening, radiation hardening attenuation. Irradiation temperature rise results in an increase of incubation period and threshold neutron fluence. A special attention is paid to hydrogen absorption in #alpha#-titanium alloys under irradiation. It is concluded that titanium base 'alpha'-alloys are serviceable as structural materials in nuclear plants with allowance made for peculiar features of their radiation behaviour. 4 refs.; 7 figs.; 1 tab.

201

Protective nitride formation on stainless steel alloys for proton exchange membrane fuel cell bipolar plates  

British Library Electronic Table of Contents (United Kingdom)

Gas nitridation has shown excellent promise to form dense, electrically conductive and corrosion-resistant Cr-nitride surface layers on Ni-Cr base alloys for use as proton exchange membrane fuel cell (PEMFC) bipolar plates. Due to the high cost of nickel, Fe-base bipolar plate alloys are needed to meet the cost targets for many PEMFC applications. Unfortunately, nitridation of Fe-base stainless steel alloys typically leads to internal Cr-nitride precipitation rather than the desired protective surface nitride layer formation, due to the high permeability of nitrogen in these alloys. This paper reports the finding that it is possible to form a continuous, protective Cr-nitride (CrN and Cr2N) surface layer through nitridation of Fe-base stainless steel alloys. The key to form a protective Cr...

2007-01-01

202

Phase composition of the VT22-alloy and its cyclic strength  

International Nuclear Information System (INIS)

In connection with the different cyclical strengths of the two-phase (#alpha# + #beta#) titanium alloy in the case of the acicular and rounded formations of the #alpha#-phase, we have studied, employing the X-ray diffraction method, the phase composition of the alloy and the influence of heat treatment upon it. Using the method of electronic fractography, we examined the fractures in samples destroyed by the asymmetric twisting, in order to find out why the durability of the alloy is dependent upon the #alpha# - phase structure. It has been found that in the BT22 alloy, the decay the #beta#-phase may proceed in two ways; either with the formation of the martensite #alpha#'-phase of the acicular shape or with the separation of the non-martensite round-shaped #alpha#-phase. The character of the phase transformations #beta# - #alpha# or #beta#-#alpha#' is, to a considerable extent, the conseguence of the ...

203

On the performance of surface plasmon resonance based fibre optic sensor with different bimetallic nanoparticle alloy combinations  

Energy Technology Data Exchange (ETDEWEB)

In this work, we have investigated the capability of different bimetallic nanoparticle alloy combinations to be used in fibre optic sensors based on the technique of surface plasmon resonance. The metals considered for this analysis are silver, gold, copper and aluminium. The performance of the sensor with different bimetallic nanoparticle alloy combinations is evaluated and compared numerically. The performance is analysed in terms of three parameters: sensitivity, signal-to-noise ratio (SNR) and operating range for the sensing layer refractive index values. On the basis of the comparison and some logistic criteria, the best possible bimetallic alloy combinations along with a requisite alloy composition ratio are predicted. The bimetallic nanoparticle alloy combination is capable of simultaneously providing larger values of sensitivity, SNR and operating range, which is not ...

2008-03-07

204

Nickel base alloys for future steam turbines  

International Nuclear Information System (INIS)

Modern commercial alloys are not suited for future steam turbines of operating temperatures beyond 700 C. #gamma#'-hardened alloys like Waspaloy have good mechanical characteristics but have defects when large batches are melted. #gamma#'/#gamma#''-hardened alloys like Inconel 706, on the other hand, are easy to produce but have insufficient microstructural long-term stability and insufficient creep strength. Mixed crystal solidified alloys like Inconel 617 have excessive yield stress at forging temperatures. Two new alloys were therefore developed. Results so far show that they have good production characteristics but insufficient mechanical characteristics. The reasons for this are currently under investigation. (orig.)

2003-11-28

205

Mechanical properties, fracture surface characterization, and microstructural analysis of six noble dental casting alloys  

British Library Electronic Table of Contents (United Kingdom)

Statement of problem Because noble dental casting alloys for metal ceramic restorations have a wide range of mechanical properties, knowledge of these properties is needed for rational alloy selection in different clinical situations where cast metal restorations are indicated. Purpose The purpose of this study was to compare the mechanical properties and examine both the fracture and polished surfaces of 6 noble casting alloys that span many currently marketed systems. Five alloys were designed for metal ceramic restorations, and a sixth Type GPT has Type IV alloy for fixed prosthodontics (Maxigold KF) was included for comparison. Material and methods Specimens (n=6) meeting dimensional requirements for ISO Standards 9693 and 8891 were loaded to failure in tension using a universal testin...

2011-01-01

206

Irradiation induced dislocation loop and its influence on the hardening behavior of Fe-Cr alloys by an Fe ion irradiation  

International Nuclear Information System (INIS)

Nano indentation analysis and transmission electron microscopy observation were performed to investigate a microstructural evolution and its influence on the hardening behavior in Fe-Cr alloys after an irradiation with 8 MeV Fe4+ ions at room temperature. Nano indentation analysis shows that an irradiation induced hardening is generated more considerably in the Fe-15Cr alloy than in the Fe-5Cr alloy by the ion irradiation. TEM observation reveals a significant population of the a0 dislocation loops in the Fe-15Cr alloy and an agglomeration of the 1/2a0 dislocation loops in the Fe-5Cr alloy. The results indicate that the a0 dislocation loops will act as stronger obstacles to a dislocation motion than 1/2a0 dislocation loops.

2008-11-01

207

IGC/IGSCC and general corrosion behavior of alloy 800 as a PWR S/G tube material  

Energy Technology Data Exchange (ETDEWEB)

Resistance of Alloy 800 as a PWR S/G tube material to IGC/IGSCC and Ni, Co release into water was evaluated as compared with Alloys 600 and 690. The study to improve the resistance to IGSCC and general corrosion was also made, including the effects of shot-peening on the distribution of the residual stress of the U-bent tubes and the susceptibility to SCC, the stabilizing elements on IGC/IGSCC, and prior oxidation on general corrosion. From the results, shot-peened Alloy 800 was estimated to be the most reliable S/G tube material among the high nickel alloys tested. In addition, the Alloy 800 tube would obtain further reliability in IGSCC and general corrosion resistance by the combined addition of Ti, and Nb, and the prior oxidation of the inner tube surface, respectively.

1987-01-01

208

IGC/IGSCC and general corrosion behavior of alloy 800 as a PWR S/G tube material  

International Nuclear Information System (INIS)

Resistance of Alloy 800 as a PWR S/G tube material to IGC/IGSCC and Ni, Co release into water was evaluated as compared with Alloys 600 and 690. The study to improve the resistance to IGSCC and general corrosion was also made, including the effects of shot-peening on the distribution of the residual stress of the U-bent tubes and the susceptibility to SCC, the stabilizing elements on IGC/IGSCC, and prior oxidation on general corrosion. From the results, shot-peened Alloy 800 was estimated to be the most reliable S/G tube material among the high nickel alloys tested. In addition, the Alloy 800 tube would obtain further reliability in IGSCC and general corrosion resistance by the combined addition of Ti, and Nb, and the prior oxidation of the inner tube surface, respectively.

1987-03-09

209

High-temperature low-cycle fatigue and tensile properties of Hastelloy X and alloy 617 in air and HTGR-helium  

Energy Technology Data Exchange (ETDEWEB)

Results of strain controlled fatigue and tensile tests are presented for two nickel base solution hardened alloys which are reference structural alloys for use in several high temperature gas cooled reactor concepts. These alloys, Hastelloy X Inconel 617, were tested at temperatures ranging from room temperature to 871/sup 0/C in air and impure helium. Materials were tested in the solution annealed as well as in the pre-aged condition where aging consisted of isothermal exposure at one of several temperatures for periods of up to 20,000 h. Comparisons are also given between the strain controlled fatigue lives of these alloys and several other commonly used alloys all tested at 538/sup 0/C.

1981-01-01

210

Forming characteristics of cast magnesium alloy sheets manufactured by roll strip casting process  

Energy Technology Data Exchange (ETDEWEB)

Plastic formability of cast magnesium alloy that were hot rolled after roll strip casting was investigated to ascertain the feasibility of semi-solid strip casting process of AZ31B magnesium alloy. Hot rolling and heat treatment conditions were changed to examine which conditions were appropriate for producing AZ31B wrought magnesium alloys after strip casting process. Microscopic observation of the crystals of the manufactured wrought magnesium alloys was performed. It has been found that a limiting drawing ratio of 2.7 was possible in a warm deep drawing test of the cast magnesium alloy sheets after being hot rolled. (orig.)

2004-07-01

211

Filler metal development for Hastelloy alloy XR. Filler metal for hastelloy alloy XR structure with thick wall  

Energy Technology Data Exchange (ETDEWEB)

In order to develop the filler metal for Hastelloy alloy XR structure with thick wall, the weldability and high temperature strength properties of Hastelloy alloy XR weldment were investigated using the filler metals, which were alloy-designed on the basis of multiple regression analysis. The former was examined through the chemical analysis in the deposited metal, bend test, FISCO cracking test, optical microscopy and hardness measurement. The latter was investigated by means of tensile and creep test. It was found from these results that the crack susceptibility in the weldment was apparent to be lowered without degrading the high temperature strength properties. Therefore, it is concluded that these filler metals possess excellent performance as the filler metal for Hastelloy alloy XR structure with thick wall. (author).

1991-11-01

212

Fabrication and characterization of Pd/Ag alloy hollow spheres by the solvothermal method  

Energy Technology Data Exchange (ETDEWEB)

Pd/Ag alloy hollow spheres have been synthesized in ethylene glycol solution by the solvothermal method and have been characterized extensively. TEM results have revealed the formation of Pd/Ag hollow spheres. Moreover, HRTEM results confirmed the formation of Pd/Ag alloy spheres, where the lattice fringe spacing is 0.229 nm corresponding to the (111) plane of Pd/Ag alloy. SEM, XRD and UV-vis results have further suggested the formation of alloy hollow spheres. The preliminary results showed the reaction time may be an importance factor influencing the formation of Pd/Ag alloy hollow spheres.

2008-03-15

213

Electrochemical behaviour of multicomponent Zr-Ti-V-Mn-Cr-Ni alloys in alkaline solution  

Energy Technology Data Exchange (ETDEWEB)

The effect of the composition of multicomponent Zr-Ti-V-Mn-Cr-Ni alloys on their hydrogen-storage capacity and on the rate of electrosorption/desorption hydrogen was investigated under potentiodynamics as well as single-pulse and long-term galvanostatic conditions. The main characteristics of alloys and alloy electrodes were determined by their structural analysis by means of X-ray diffraction and scanning electron microscope, by specific surface area test and by determination of the hydrogen absorption/desorption isotherms in the gas/solid phase system. It was found that only the alloys with a manganese content below a threshold could be used as electrode materials for Ni-MH batteries, whereas the modification of the electrode material by micro-encapsulation of alloy particles should limit the dissolution of manganese from the electrode material in a strong alkaline solution. ...

1996-01-01

214

Effects of rolling condition on warm deep drawability of magnesium alloy sheets produced by twin-roll strip casting  

Energy Technology Data Exchange (ETDEWEB)

Effects of rolling conditions on warm deep drawability of cast magnesium alloy that were hot rolled after roll strip casting were investigated to ascertain the feasibility of twin-roll strip casting process of AZ31B magnesium alloy. Hot rolling and heat treatment conditions were changed to examine which conditions were appropriate for producing AZ31B wrought magnesium alloys after strip casting process. Microscopic observation of the crystals of the manufactured wrought magnesium alloys was performed. It has been found that a limiting drawing ratio of 2.7 was possible in a warm deep drawing test of the cast magnesium alloy sheets after being hot rolled. (orig.)

2005-07-01

215

Development of plasticity processing of magnesium alloys  

Energy Technology Data Exchange (ETDEWEB)

Recent developments on plastic forming technology of magnesium alloys are presented. Attempts have been undergoing with an aim at forming magnesium alloy parts at lower temperatures. It is believed that fine microstructure magnesium alloys usually have much higher plasticity at lower temperatures and even room temperatures. Extrusion is a method to form magnesium profile products and tube products, which is also one of the effective ways to make fine microstructure magnesium alloys. Superplasticity forming is another method to form high plasticity magnesium alloys. Hot forming of magnesium sheet parts is an important process to form magnesium products. Some developments related to above issues are discussed in the present paper. (orig.)

2003-07-01

216

Corrosion resistance of tungsten and molybdenum alloys with #approx# 30 at.% Re in nitrogen- and oxygen-containing environments  

International Nuclear Information System (INIS)

Formation kinetics and composition of products of interaction of binary and ternary tungsten-molybdenum-rhenium alloys containing 30#+-#3 at.% (27-47 weight %) Re with products of thermal dissociation of ammonia and nitrogen-oxygeneous mixtures are studied. Mo-45% Re-10%W ternary alloy occupies intermediate position between W-27%Re and Mo-47%Re binary alloys, while its corrosion resistance and corrosion nature are close to those of W-Re and mechanical features - to those of Mo-Re alloy. It is explained by the fact, that the variation of W and Mo ration occurs in thin surface layer of ternary alloys in contrast to the initial state and the enrichment of near-the-surface layer with tungsten occurs under hot and cold deformation, at aging in the air, and during oxidation-reduction treatment. 4 refs.; 7 figs.

217

Corrosion behavior of sputter-deposited W-Nb alloys in NaCl and NaOH solutions  

International Nuclear Information System (INIS)

The corrosion behavior of the sputter-deposited amorphous or nanocrystalline W-Nb alloys is studied in 10% NaCl, 0.1 and 1 M NaOH solutions at 24 deg. C, open to air using immersion tests and electrochemical measurements. Niobium metal acts synergistically with tungsten in enhancing the corrosion resistance of the W-Nb alloys so as to show lower corrosion rates than the corrosion rates of the alloy-constituting elements in almost all examined solutions. Corrosion rates of W-Nb alloys are about more than one order of magnitude less than that of the sputter-deposited tungsten and even lower than that of sputter-deposited niobium. The stability of the anodic passive films formed on the W-Nb alloys increase with niobium content.

2008-05-29

218

Converting hcp Mg-Al-Zn alloy into bcc Mg-Li-Al-Zn alloy by electrolytic deposition and diffusion of reduced lithium atoms in a molten salt electrolyte LiCl-KCl  

Energy Technology Data Exchange (ETDEWEB)

A body-centered cubic (bcc) Mg-12Li-9Al-1Zn (wt.%) alloy was fabricated in air by electrolysis from LiCl-KCl molten salt at 500 deg. C. Electrolytic deposition of Li atoms on cathode (Mg-Al-Zn alloy) and diffusion of the Li atoms formed the bcc Mg-Li-Al-Zn alloy with 12 wt.% Li and only 0.264 wt.% K. Low K concentration in the bcc Mg alloy strip after the electrolysis process resulted from 47% atomic size misfit between K and Mg atoms and low solubility of K in Mg matrix.

2007-04-15

219

Converting hcp Mg-Al-Zn alloy into bcc Mg-Li-Al-Zn alloy by electrolytic deposition and diffusion of reduced lithium atoms in a molten salt electrolyte LiCl-KCl  

British Library Electronic Table of Contents (United Kingdom)

A body-centered cubic (bcc) Mg-12Li-9Al-1Zn (wt.%) alloy was fabricated in air by electrolysis from LiCl-KCl molten salt at 500degreeC. Electrolytic deposition of Li atoms on cathode (Mg-Al-Zn alloy) and diffusion of the Li atoms formed the bcc Mg-Li-Al-Zn alloy with 12wt.% Li and only 0.264wt.% K. Low K concentration in the bcc Mg alloy strip after the electrolysis process resulted from 47% atomic size misfit between K and Mg atoms and low solubility of K in Mg matrix.

2007-01-01

220

Caburization kinetics of alloy-800 in liquid sodium at 550_0C  

International Nuclear Information System (INIS)

Preliminary observations on the isothermal carbon transfer in low-carbon Alloy-800 exposed in sodium with AISI-304 type of steel at 550_0 are reported. The alloy was found to undergo a carburization comparable or slightly lower than that observed for the AISI-304 stainless steel for carbon activities above 6 x 10 /sup -3/ at 550_0C, but was not found to decarburize below such a carbon activity value. In the examined range the chemical composition of the alloys does not affect the process out of the experimental uncertainty of measure. Conclusions concerning the effective diffusion for carbon in the alloy are formulated. Preliminary relationships were found for an empirical evaluation of the carburization of the Alloy-800 in sodium of known carbon activity.

221

Anisotropy of the structure and mechanical properties of low-alloy tungsten  

Energy Technology Data Exchange (ETDEWEB)

The authors examine the relationship of the structure and mechanical properties of similar alloys of tungsten with rhenium produced by the powder metallurgy method by sintering powders. Since the alloys were deformed by rolling, we examine the effect of the resultant anisotropy of the structure on the properties of the metal in various directions. The tests were conducted on an alloy of tungsten with 2 wt.% rhenium and, for comparison purposes, an alloy of tungsten with additions of oxides of yttrium and hafnium. The mechanical properties of the alloys, i.e., strength, cracking resistance, cold shortness temperature, were determined in the bend test. Structural examination was carried out using an optical microscope, electron scanning microscopy, and the method of transmission electron microscopy.

1987-12-01

222

Advances in amorphous and nanocrystalline magnetic materials  

International Nuclear Information System (INIS)

Recent advances made in the area of amorphous and nanocrystalline alloys exhibiting high saturation inductions are reviewed. A new chemical composition was identified that achieves a saturation induction of 1.64 T in an iron-based amorphous alloy. This alloy, when used in electrical transformers, shows a much improved performance over the existing amorphous alloy. Nanocrystalline FeCoCuNbSiB alloys are found to have saturation induction levels reaching 1.7 T. These materials are suited for use in sensors and inductors carrying large currents. Some of these nanocrystalline alloys show a BH squareness ratio exceeding 90%, which can be utilized in pulse power devices. Recent developments in the applications of these materials are also pointed out.

2006-09-01

223

Fatigue behavior of Alloy 690 and Alloy 800 SG tubing at temperatures up to 330{sup o}C in very high cycle fatigue regime  

Energy Technology Data Exchange (ETDEWEB)

During the service in nuclear power plants, steam generator (SG) tubing will suffer from a vibration with a frequency from 30-40 Hz. This means that SG tubing will undergo a very high cycle fatigue process during the design life time (25 years=about 3x10{sup 10}cycles). The material degradation and the very high cycle fatigue life of SG tubing materials due to the vibration are therefore of concern. In this investigation, the fatigue properties of Alloy 690 and Alloy 800 SG tubing in the very high cycle fatigue regime (higher than 10{sup 7} cycles) and strain controlled fatigue at temperatures up to 330{sup o}C have been investigated. The fatigue properties of SG tubing of Alloy 690 are comparable to that of wrought material. The strain controlled fatigue properties of Alloy 690 and Alloy 800 are slightly better at 288{sup o}C than at room temperature (RT). At the stress near the ...

2007-07-01

224

Fatigue behavior of Alloy 690 and Alloy 800 SG tubing at temperatures up to 330"oC in very high cycle fatigue regime  

International Nuclear Information System (INIS)

During the service in nuclear power plants, steam generator (SG) tubing will suffer from a vibration with a frequency from 30-40 Hz. This means that SG tubing will undergo a very high cycle fatigue process during the design life time (25 years=about 3x10"1"0cycles). The material degradation and the very high cycle fatigue life of SG tubing materials due to the vibration are therefore of concern. In this investigation, the fatigue properties of Alloy 690 and Alloy 800 SG tubing in the very high cycle fatigue regime (higher than 10"7 cycles) and strain controlled fatigue at temperatures up to 330"oC have been investigated. The fatigue properties of SG tubing of Alloy 690 are comparable to that of wrought material. The strain controlled fatigue properties of Alloy 690 and Alloy 800 are slightly better at 288"oC than at room temperature (RT). At the stress near the fatigue endurance, ...

2007-08-19

225

Reactor fuel cladding tube with excellent corrosion resistance and method of manufacturing the same  

International Nuclear Information System (INIS)

The present invention provides a fuel cladding tube having an excellent corrosion resistance and thus a long life, and a suitable manufacturing method therefor. Namely, in the fuel cladding tube, the outer circumference of an inner layer made of a zirconium base alloy is coated with an outer layer made of a metal more corrosion resistant than the zirconium base alloy. Ti or a titanium alloy is suitable for the corrosion resistant metal. In addition, the outer layer can be coated by a method such as vapor deposition or plating, not limited to joining of the inner layer material and the outer layer material. Specifically, a composite material having an inner layer made of a zirconium alloy coated by the outer material made of a titanium alloy is applied with hot fabrication at a temperature within a range of from 500 to 850degC and at a fabrication rate of not less than 5%. The ...

1993-07-14

226

Probabillistic Sensitivity Analysis in Life-Prediction of an alpha + beta Titanium Alloy.  

Science.gov (United States)

Probabilistic sensitivities using the score function method are developed for a lifing analysis of an alpha + beta titanium alloy in a round bar under axial fatigue load. Sensitivities with respect to the statistical inputs of the crack initiation size (a...

2008-01-01

227

On the possible relation between the absence of superconductivity in Au and Pd-Ag alloys and the negative sign of the Hall coefficient  

International Nuclear Information System (INIS)

Available data are presented which support the supposition that metals and alloys with a negative low-temperature Hall coefficient are apparently not superconducting. (author).

1983-01-01

228

Molar and excess volumes of liquid In-Sb, Mg-Sb, and Pb-Sb alloys  

Energy Technology Data Exchange (ETDEWEB)

By a direct Archimedes' technique, volumetric data were obtained for liquid In, Mg, Pb, and Sb and mixtures of In-Sb, Mg-Sb, and Pb-Sb. In this paper the excess volumes for the alloys studied are presented and discussed.

1990-04-01

229

Improvement of structure and mechanical properties of cast titanium alloys using rapid heat treatment  

Energy Technology Data Exchange (ETDEWEB)

The possibility of rapid heat treatment (RHT) application to titanium castings has been studied. It was shown that such treatment provides a significant improvement of intragrain structure and mechanical properties of cast ({alpha}+{beta})-titanium alloys. ((orig.))

1995-01-01

230

High damping Fe-Mn martensitic alloys for engineering applications  

International Nuclear Information System (INIS)

Conventional methods for reducing vibration in engineering designs (i.e. by stiffening or detuning) may be undesirable or inadequate in conditions where size or weight must be minimized or where complex vibration spectra exist. Alloys which combine high damping capacity with good mechanical properties can provide attractive technical and economic solutions to problems involving seismic, shock and vibration isolation. To meet these trends, we have developed a new high damping Fe-17%Mn alloy. Also, the alloy has advantages of good mechanical properties and is more economical than any other known damping alloys (a quarter the cost of non-ferrous damping alloy). Thus, the high damping Fe-17%Mn alloy can be widely applied to household appliances, automobiles, industrial facilities and power plant components with its excellent damping capacity (SDC, 30%) and ...

2000-06-01

231

Electrolysis of halide-containing solutions with platinum based amorphous metal alloy anodes  

Energy Technology Data Exchange (ETDEWEB)

A process for the generation of halogens from halide-containing solutions includes the step of conducting electrolysis of the solutions in an electrolytic cell having a platinum based amorphous metal alloy anode.

1985-12-24

232

Electrochemical properties of Si/Ni alloy-graphite composite as an anode material for Li-ion batteries  

International Nuclear Information System (INIS)

Si/Ni alloy and graphite composites were synthesized using arc-melting followed by high energy mechanical milling (HEMM). Alloy particles comprising of NiSi2, NiSi and Si phases were distributed finely and uniformly on the surface of graphite in the composites obtained after Hem. The composite containing 60 wt.% of Si/Ni alloy exhibited a stable capacity of ?780 mAh/g. Fourier transform infrared spectroscopy (FTIR) analysis confirmed that some bonds were formed between alloy and graphite after HEMM, which appeared to retain the electrical connection between alloy and graphite during cycling. X-ray diffraction (XRD) analysis indicated that NiSi2 and NiSi phases, which acted as an inactive alloy matrix remained invariant during charge and discharge. In addition to NiSi2 and NiSi phases, disordered graphite layers also played the role of media for the accommodation ...

2005-09-30

233

Electrochemical corrosion behavior of AZ91D alloy in ethylene glycol  

Energy Technology Data Exchange (ETDEWEB)

The effect of concentration on the corrosion behavior of Mg-based alloy AZ91D was investigated in ethylene glycol-water solutions using electrochemical techniques i.e. potentiodynamic polarization, electrochemical impedance measurements (EIS) and surface examination via scanning electron microscope (SEM) technique. This can provide a basis for developing new coolants for magnesium alloy engine blocks. Corrosion behavior of AZ91D alloy by coolant is important in the automotive industry. It was found that the corrosion rate of AZ91D alloy decreased with increasing concentration of ethylene glycol. For AZ91D alloy in chloride >0.05 M or fluoride <0.05 M containing 30% ethylene glycol solution, they are more corrosive than the blank (30% ethylene glycol-70% water). However, at concentrations <0.05 for chloride or >0.05 M for fluoride containing ethylene ...

2009-11-01

234

Electrochemical corrosion behavior of AZ91D alloy in ethylene glycol  

International Nuclear Information System (INIS)

The effect of concentration on the corrosion behavior of Mg-based alloy AZ91D was investigated in ethylene glycol-water solutions using electrochemical techniques i.e. potentiodynamic polarization, electrochemical impedance measurements (EIS) and surface examination via scanning electron microscope (SEM) technique. This can provide a basis for developing new coolants for magnesium alloy engine blocks. Corrosion behavior of AZ91D alloy by coolant is important in the automotive industry. It was found that the corrosion rate of AZ91D alloy decreased with increasing concentration of ethylene glycol. For AZ91D alloy in chloride >0.05 M or fluoride 0.05 M for fluoride containing ethylene glycol solution, some inhibition effect has been observed. The corrosion of AZ91D alloy in the blank can be effectively inhibited by addition of 0.05 mM paracetamol that reacts ...

2009-11-01

235

Development of modified 9 Cr-1 Mo steel for elevated-temperature service  

International Nuclear Information System (INIS)

The status of development and commercialization of a modified 9 Cr-1 Mo alloy is presented. The alloy is modified by the addition of 0.06 to 0.10% Nb and 0.18 to 0.25% V. The alloy is recommended for use in the normalized and tempered condition (1040"0C for 1 h, air cooled to room temperature; 760"0C for 1 h, air cooled to room temperature). Heat treatment, Charpy impact, tensile, and creep properties of the alloy are described in detail along with a brief description of other properties. The modified alloy has creep strength that exceeds that of standard 9 Cr-1 Mo and 2 1/4 Cr-1 Mo steels for the temperature range from 427 to 704"0C. The total-elongation and reduction-of-area values for all test temperatures and rupture times up to 22,500 h exceed 15 and 70%, respectively. The estimated design allowable stresses for this alloy are higher than those for standard ...

1983-06-19

236

Correlation of mechanical properties with microstructure of Alloy 800 after annealing at 800 - 1000 "0C  

International Nuclear Information System (INIS)

The microstructures of so called high temperature alloys, which have been developed for service temperatures up to 800"0C, are not necessarily stable at higher temperatures. The mobility of alloying elements is very high in FeCrNi alloys at 950 "0C e.g. iron, chromium or nickel can diffuse up to 0.1 mm distance in one year, which is about a grain diameter. Interstitials like carbon or nitrogen show a four orders of magnitude higher diffusivity than the alloying elements. In addition, the carbon solubility in this type of alloy is reported to be very low. Therefore the alloys are supersaturated with carbon after heat treatment above 1100 "0C and water quenching although the absolute carbon content is very low. At service temperatures around 800"0C the solubility of carbon is still about one order of magnitude lower than at heat treatment temperature. This will ...

1981-05-01

237

Comparison of Optical and SEM BSE Imaging Techniques for Quantifying Alpha-Beta Titanium Alloy Microstructures (Preprint).  

Science.gov (United States)

Quantitative metallography is often used to confirm the proper processing of aerospace metallic materials. A microstructural feature of great importance for titanium alloys processed in the alpha-beta phase field is the volume fraction of primary alpha. S...

2006-01-01

238

Carburization and tensile behavior of alloy 800 in liquid sodium  

International Nuclear Information System (INIS)

The carbon transfer has been analyzed in the Alloy 800/sodium/stainless steel system by determining the carbon-uptake of Alloy 800 foils, which were exposed in liquid sodium of known carburizing potential. Under equilibrium condistions between 650 and 550_0C the measured total carbon concentrations in the Alloy 800 tabs were found to be roughly related to the carbon activities of the sodium environment by the equation already stated for the 18 Cr-8/10 Ni stainless steels, extrapolated to the chemical composition of the Ni-rich austenitic alloy. However the Alloy 800 was not found to undergo any decarburization in low-carbon activity environments. The carbon diffusion kinetics was determined as a function of temperature, it was found to be similar to that reported for the AISI-304 type of steel. The effects of sodium exposure on microstructural and mechanical properties of several ...

239

Carburization and tensile behavior of Alloy 800 in liquid sodium  

Energy Technology Data Exchange (ETDEWEB)

The carbon transfer has been analyzed in the Alloy 800/sodium/stainless steel system by determining the carbon-uptake of Alloy 800 foils, which were exposed in liquid sodium of known carburizing potential. Under equilibrium conditions between 650 and 550/sup 0/C the measured total carbon concentrations in the Alloy 800 tabs were found to be roughly related to the carbon activities of the sodium environment by the equation already stated for the 18 Cr-8/10 Ni stainless steels, extrapolated to the chemical composition of the Ni-rich austenitic alloy. However the Alloy 800 was not found to undergo any decarburization in low-carbon activity environments. The carbon diffusion kinetics was determined as a function of temperature, it was found to be similar to that reported for the AISI-304 type of steel. The effects of sodium exposure on microstructural and mechanical properties of ...

1983-05-01

240

Absorption and diffusion of hydrogen in palladium-silver alloys by density functional theory  

Science.gov (United States)

The vibrational states, absorption energies, and diffusions of H in Pd and Pd1-xAgx(0Pd-Ag alloys should avoid the Ag-rich areas.

2002-11-01

241

Wettability of binary and ternary alloys of the system Al-Si-Mg with SiC particulates  

Science.gov (United States)

The authors have presented results of an investigation of wettability of SiC particulates by liquid alloys of the Al-Si-Mg system. The evaluation of wetting has been carried out through the determination of the threshold pressure for infiltration of packed SiC particulates by the liquid alloy. The results indicate that whereas Si and Mg additions do not affect wetting, in the case of the ternary alloys the contact angle decreases in an amount proportional to the content of Mg[sub 2]Si.

1994-12-01

242

Wear and friction measurements on CVD coated carbon alloy bearing surfaces  

Energy Technology Data Exchange (ETDEWEB)

A series of ball-on-disc wear and friction measurements were made for surfaces which have a chemical vapour deposition carbon silicon alloy layer on a carbon substrate (fine grain POCO graphite). Nitrogen ion irradiation was used to improve the wear resistance of the carbon alloy surface. For comparison, measurements were also taken for alumina against alumina. It was found that the lowest friction coefficient and lowest wear occurred for ion irradiated coated samples containing 4% Si in the alloy and that the performance was superior to that of alumina. ((orig.))

1995-03-01

243

Wear and friction measurements on CVD coated carbon alloy bearing surfaces  

International Nuclear Information System (INIS)

A series of ball-on-disc wear and friction measurements were made for surfaces which have a chemical vapour deposition carbon silicon alloy layer on a carbon substrate (fine grain POCO graphite). Nitrogen ion irradiation was used to improve the wear resistance of the carbon alloy surface. For comparison, measurements were also taken for alumina against alumina. It was found that the lowest friction coefficient and lowest wear occurred for ion irradiated coated samples containing 4% Si in the alloy and that the performance was superior to that of alumina. ((orig.)).

244

Total corrosion and film analysis of SUS and Ni base alloy in supercritical water  

International Nuclear Information System (INIS)

... Toshiba Corporation, Isogo Engineering Center, Yokohama, Kanagawa (Japan)

2005-09-01

245

The effects of high-temperature exposure on the properties of heat-resistant alloys  

Energy Technology Data Exchange (ETDEWEB)

The exposure of heat-resistant alloys to high temperature can significantly change their mechanical properties. This paper presents and analyzes data on the effect of thermal exposure on the tensile and impact behavior of three cast materials -- the HK-40, HP-50, and 21Cr-32Ni-Fe alloys -- and of wrought material -- Alloy 800. The changes in tensile and impact properties caused by high-temperature exposure are reviewed. Reasons for these property changes and needs for considering them in the design, operation, and life assessment of high-temperature equipment are discussed.

1994-12-31

247

Study of the natural and passive oxide films formed on Ni-Mo single crystal alloys by ion channelling and nuclear microanalysis  

Energy Technology Data Exchange (ETDEWEB)

The chemical properties of alloys in a given environment are to a large extent governed by the surface composition. Changes of the surface composition during passivation are important features in this respect. Previous studies of single crystal Ni-Mo alloys surfaces have been reported. The aim of this work was to obtain quantitative data, for the natural oxide and the passive films formed on Ni-6% Mo(100) and (110) alloys, using Rutherford backscattering spectroscopy and nuclear reaction analysis.

1988-07-01

248

Study of the natural and passive oxide films formed on Ni-Mo single crystal alloys by ion channelling and nuclear microanalysis  

International Nuclear Information System (INIS)

The chemical properties of alloys in a given environment are to a large extent governed by the surface composition. Changes of the surface composition during passivation are important features in this respect. Previous studies of single crystal Ni-Mo alloys surfaces have been reported. The aim of this work was to obtain quantitative data, for the natural oxide and the passive films formed on Ni-6% Mo(100) and (110) alloys, using Rutherford backscattering spectroscopy and nuclear reaction analysis. (author).

1987-10-19

249

Structural transformations of metastable #alpha#''-phase during cold deformation  

International Nuclear Information System (INIS)

Phase transformations occuring during cold deformation in hardened #alpha#+#beta# titanium alloy of the Ti-Al-Mo-Zr-Sn-Si system with 10% summary content of alloying elements are studied by X-ray diffraction analysis. Two stages of trapsformation of metastable #alpha#''-phase are found. A conclusiop is made that ability of the alloy containing #alpha#''-phase to cold deformation is determined by the presence of favourable texture, by high degree of metastability and by volume portion of #alpha#''-phase in the alloy structure.

250

Raising the durability of bucket wheel excavator teeth  

Energy Technology Data Exchange (ETDEWEB)

Describes performance of excavator teeth manufactured with a new hard alloy. The alloy was developed by the Donetskii Politeknicheskii Institute. Its composition consists of a high-chromium steel with a larger amount of titanium than serial alloy, and a nitrogen additive. Trial tests of new alloy teeth were carried out in the Severnyi and Vershinskii coal surface mines. The teeth were attached to EhRP, EhPG and EhR bucket wheel excavators. Abrasive wear of 129 experimental teeth and 134 serial teeth was compared for different excavation conditions. Test results are tabulated; advantages of the new experimental teeth are listed. 3 refs.

1993-07-01

251

Pitting corrosion of nickel base alloys in halide media  

International Nuclear Information System (INIS)

A computerized corrosion measuring system (EG and G model 350 A) was used to study the influence of Cr, Mo, Ti, Nb and W on the pitting corrosion of nickel base alloys in 3% NaCl at 90"0C. The electrochemical parameters under investigation are the corrosion potential E_c_o_r_r, pitting potential E_p and protection potential E_p_p. The corrosion behaviour of nickel base alloys were studied by using pitting scan and potentiostatic techniques. Values of corrosion potential, pitting potential and protection potential were used for a ranking of alloys for corrosion resistance.

1988-03-06

252

Operating experience with condenser tubes made from copper alloys and new developments; Betriebserfahrungen mit Kondensatorrohren aus Kupferlegierungen und aktuelle Entwicklungen  

Energy Technology Data Exchange (ETDEWEB)

Copper alloys are a suitable tubing material for turbine condensers and heat exchangers. Due to problems with corrosions copper alloys increasingly are displaced by high-grade steel and titanium. Blockages and surface formation in the pipes, disturbance of the oxide coating formation, erosion and quality faults with the production are the causes for the corrosion. In the contribution under consideration counter measures are designated for the solution of the problems with corrosions. The application limits for different copper alloys are designated. Recommendations for the optimized operation are given.

2008-07-01

253

Nanocrystallization of the amorphous Fe_1_4Ni_4_0Zr_7B_1_2 alloys studied by the Moessbauer spectroscopy  

International Nuclear Information System (INIS)

Formation of the soft magnetic nanostructure in amorphous Fe_1_4Ni_4_0Zr_7B_1_2 alloy due to heat treatment is studied by the Moessbauer, differential scanning calorimetry, and X-ray diffraction techniques. Annealing at temperatures 520-580 "oC leads to the formation of extremely soft nanocrystalline alloy as revealed by the rf-Moessbauer measurements. The superparamagnetic behaviour was observed for the alloy annealed at 620-640 "oC. At higher annealing temperatures good soft magnetic properties deteriorate. (author)

2001-09-23

255

Examination of electrochemical behavior and structure of oxide films on Ni/sub 60/Nb/sub 40/ alloy in amorphous and crystalline states  

Energy Technology Data Exchange (ETDEWEB)

Experiments were conducted which established that the higher passivating capacity of Ni/sub 60/Nb/sub 40/ alloys in the amorphous state and higher efficiency of the anodic process of generation of chlorine (2 N NaCl + HCl to pH = 0) in comparison with the crystalline state are determined by higher homogeneity and density of the passive films formed on the amorphous alloy and by higher electron conduction which depends directly on the difference in the structure of the passive films formed on the alloys in the amorphous and crystalline states.

1988-05-01

256

Environmental Influence on Passive Films Formed on Alloy 22  

Energy Technology Data Exchange (ETDEWEB)

The passive corrosion rate of Alloy 22 is exceptionally low in a wide range of aqueous solutions, temperatures and electrochemical potentials, Alloy 22 contains approximately 22% chromium (Cr) by weight; thus, it forms a Cr-rich passive film in most environments. Very little is known about the composition, thickness and other properties of this passive film. The aim of this research was to determine the general characteristics of the oxide film that forms on Alloy 22, as a function of solution pH, temperature and applied electrochemical potential.

2002-10-07

257

Electron microscopy study of thermomechnical deformation conditions effect on the structure of two-phase (#alpha#+#beta#) titanium alloys  

International Nuclear Information System (INIS)

The methods of optical and transmission electron microscopy were used to study the influence of different programmes of hot deformation on the structure formation of (#alpha#+#beta#) titanium alloy VT9. The #beta# alloy VT-15 was studied at the same time in order to simulate the dislocation structure generated in the process of hot deformation. During the hot deformation of two-phase titanium alloys in both #beta# and (#alpha#+#beta#) ranges there is found to be an optimum range of deformation in which a homogeneous, polygonized structure is formed.

258

Electrochemical behavior of Alloy 800 under steam generators temperature and pressure conditions comparison, based on (I,E) polarization curves, with 316L and A533B steels  

Energy Technology Data Exchange (ETDEWEB)

We propose a dissolution-passivation model to account for the electrochemical behavior of Alloy 800 and 316L stainless steel under steam generators operating conditions. This model is similar to the one defined for nickel, considering the known importance of this element on the studied alloys. The comparison of the rates of the elementary steps points out the favorable influence of dissolved oxygen and phosphate ions on the dissolution of Alloy 800, even in the presence of chloride ions. The sensitivity of 316L SS is greater, especially because of the lowest stability of oxide-like intermediate.

1992-12-31

259

Electrochemical behavior of Alloy 800 under steam generators temperature and pressure conditions comparison, based on (I,E) polarization curves, with 316L and A533B steels  

International Nuclear Information System (INIS)

We propose a dissolution-passivation model to account for the electrochemical behavior of Alloy 800 and 316L stainless steel under steam generators operating conditions. This model is similar to the one defined for nickel, considering the known importance of this element on the studied alloys. The comparison of the rates of the elementary steps points out the favorable influence of dissolved oxygen and phosphate ions on the dissolution of Alloy 800, even in the presence of chloride ions. The sensitivity of 316L SS is greater, especially because of the lowest stability of oxide-like intermediate.

1991-08-25

261

Effect of tritium and helium-3 on the lifetime properties of Pd-Ag alloys in ITER tritium purification technology  

Energy Technology Data Exchange (ETDEWEB)

An experimental verification for long-term performance of a Pd-Ag permeation in ITER tritium fusion cleanup units (FCU) is needed. In addition, information is required on the influence of tritium and {sup 3}He decay on the physical and chemical properties of Pd-Ag alloys (V-1). The results of the investigations of alloys (V-1) (mechanical properties and microstructure) after long-term usage exposition in tritium are given in this report. The experimental conditions (temperature, pressure, clearance, {sup 3}He concentrations) and the previous conclusions on the V-1 alloy performance are presented. (orig.).

1996-10-01

262

Effect of protective coatings on the high-temperature fatigue of heat-resistant alloys  

Energy Technology Data Exchange (ETDEWEB)

The fatigue properties of EP539LM alloy with an Al-Nb-Si fused slurry coating and a Co-Cr-Al-Y electron-beam coating are investigated experimentally in vacuum and in air at 900 C. It is found that the protective coatings reduce the fatigue life of the specimens both in vacuum and in air, with the electron-beam coating affecting the fatigue life of the alloy to a lesser degree than the fused slurry coating. The negative effect of the coatings on the fatigue life of the alloy is attributed largely to the properties of the coating material. 7 references.

1986-08-01

263

Effect of cross rolling parameters on texture formation and parameters on texture formation and anisotropy of mechanical properties of (#alpha#+#beta#)-titanium alloy sheets  

International Nuclear Information System (INIS)

Formation of basis type texture at rolling of Ti + 6.0% Al + 1.5% V + 1.0% Mo system alloy with initial prismatic texture is investigated by means of X-ray techniques. Variations of mechanical features in titanium alloy sheets depending on temperature-deformation conditions of rolling are investigated. Main conditions for formation of the intensive basis textute in the investigated alloy sheets which provides for isotropic properties in sheet plane and for increased ductility are determined.

264

DEFORMATION BEHAVIOR OF AN OMEGA HARDENED ...  

Science.gov (United States)

... Accession Number : ADD100229. Title : DEFORMATION BEHAVIOR OF AN OMEGA HARDENED ALPHA-BETA TITANIUM ALLOY,. ...

265

Corrosion behaviour of non-ferrous metals in sea water  

Energy Technology Data Exchange (ETDEWEB)

The most typical kinds of corrosion of brasses are selective corrosion (dezincification) and stress corrosion. Prevention against these kinds of corrosion lies in application of arsenic alloy addition and appropriate heat treatment removing internal stresses as well as in maintaining the arsenic and phosphorus contents on a proper level. The most typical corrosion of cupronickels is the local corrosion. Selective corrosion occurs less often and corrosion cracking caused by stress corrosion in sea water does not usually occur. Crevice corrosion is found especially in places of an heterogeneous oxidation of the surface under inorganic deposits or under bio-film. Common corrosive phenomena for brasses and cupronickels are the effects caused by sea water flow and most often the impingement attack. Alloy additions improve resistance to the action of intensive sea water flow but situation in this field requires further improvement, especially if the ...

2004-07-01

266

Characteristics of the Mechanical Properties and the Fractures ...  

Science.gov (United States)

... Accession Number : ADA136144. Title : Characteristics of the Mechanical Properties and the Fractures of an Alpha Beta Titanium Alloy,. ...

1983-11-18

267

BNES materials conference a status review of alloy 800  

International Nuclear Information System (INIS)

Existing applications of Alloy 800 are summarized, with particular reference to its use in various types of reactor. The need for a co-ordinated research and development programme is stressed, and the variables to be explored are outlined. The papers relating to the problem of corrosion and cracking in water and steam are considered. the strength and ductility of Alloy 800 is considered. Finally, sections of the summary deal with the use of Alloy 800 for (a) sodium cooled fast reactor boiler tubes; (b) the high temperature gas cooled reactor; and (c) PWR steam generator tubes. (U.K.).

268

Application properties of AB{sub 2}-type hydrogen absorbing alloys  

Energy Technology Data Exchange (ETDEWEB)

Use of hydrogen absorbing alloys in various practical applications is always connected with the problem of production of starting alloys. The transition from laboratory samples to small-scale production involves the change of furnace and its operation mode and this has an effect on the preparation method of mixture of starting metal. Also, for some applications such as thermosorption compressors the exact values of thermodynamical parameters of reaction are needed. In the present work we present the results of investigation of series Laves phase hydrogen-absorbing alloys which can be promising in for use in different devices. 1 ref.

1998-07-01

269

The influence of process parameters on forged magnesium alloys  

Energy Technology Data Exchange (ETDEWEB)

Two extruded magnesium alloys, AZ31 and AZ61 were selected to evaluate the influence of process parameters on the material forgeability. The processing parameters considered for forging magnesium alloys were: compression load in the range 55 KN to 60 KN and forging temperature, in the range of ambient temperature to 300 C. Uniaxial compression tests were conducted to establish the strain-temperature relationship. The influences of process parameters on the microstructure were also evaluated. (orig.)

2003-07-01

270

Structural features of twins in transition class alloy Ti-Al-Mo-V-Cr  

International Nuclear Information System (INIS)

The alloy of Ti-Al-Mo-V-Cr system is studied for its structure in a strained state and specific features of #beta#-#alpha# transformation in a #beta#-matrix and deformation twins on ageing. It is determined that preliminary deformation initiates the decomposition of solid solution on aging. In a metastable #beta#-titanium alloy the substructure of deformation twins is shown to vary essentially with aluminium and chromium partial substitution for molybdenum and vanadium

1999-11-01

271

Strontium as modifier for AlSi and AlSiCu alloys  

International Nuclear Information System (INIS)

The optimum of strontium amount for good modification of AK7, AK9, AK11, AK52, AK104 alloys was determined on the base of the analysis of microstructural changes. The stability of the modifier was investigated on the way of successive remelting of billets. The influence of amount of modifier on the impact strength of the alloys was established. (author)

272

Mechanical properties of (alpha+beta)-titanium alloys with various structure within the temperature range of 20 to -196 deg C  

International Nuclear Information System (INIS)

The influence of structure on mechanical properties in the course of tensile tests in a wide range of temperatures was studied, using the VT16 structure thermally strengthened (alpha+beta)-titanium alloy by way of example. It is ascertained that transition from ductile to brittle fracture at the temperature of -196 deg C is observed only in coarse-grain alloy having alpha-eldging of beta grains.

273

Magnesium foam produced from bulk AZ31 magnesium alloy sheets  

Energy Technology Data Exchange (ETDEWEB)

Using commercial AZ31 magnesium alloy sheets, we produced a foamable preform sheet containing titanium hydride (TiH{sub 2}) powder through diffusion-bonding and hot-rolling of four cycles. Heating the preform sheets in Ar atmosphere, we obtained closed-cell magnesium alloy foams with various porosities. The foamed specimen at 883 K showed the maximum porosities of 77%. (orig.)

2005-07-01

274

Low temperature superplasticity of a metastable #beta#-titanium alloy  

International Nuclear Information System (INIS)

Superplasticity in Ti alloys has been widely investigated in the past and superplastic forming of aerospace components has thus been developed over the last two decades. The Ti alloy most studied in this framework is undoubtedly the Ti-6Al-4V (wt %) alloy, for which maximum elongations are obtained in the temperature range [880-900C]. The development of the superplastic properties has been demonstrated to be in close relation with quite similar volume fractions of the #alpha# and #beta# phases, the #beta# transus temperature for this alloy ranging from 980-1000 C. Attempts have been carried out to reduce the temperature of superplastic forming of Ti-6Al-4V by the addition of elements like Fe, Co, or Ni. Such an introduction of alloying elements indeed results in a decrease of the optimum forming temperature to values as low as 820 C. This decrease is mainly attributed to a change in ...

275

Implantation-plasma treatment of martensitic steel and titanium alloy  

Energy Technology Data Exchange (ETDEWEB)

One of the effective methods of deep modification of the surface of steels and alloys is the combination of ion implantation and plasma nitriding. In this work, the long-range effect is demonstrated in the case of combination of the effect of high- and low-energy ions of nitrogen on a martensitic steel for each ion implantation is usually not effective, and a titanium alloy used widely in industry.

2001-07-01

276

Grain boundaries structure and mechanical properties of aluminium alloys  

Energy Technology Data Exchange (ETDEWEB)

The paper discusses the problem of influence of grain boundaries structure on mechanical properties of aluminium alloys at elevated temperatures. Showed the data amount of grain boundaries close to special and a random of grain boundaries. The results of calculation of contribution of different mechanisms of deformation to the total deformation for alloys with different types of grain boundaries are given. (orig.)

1996-08-01

277

Formation of interphase layers in titanium alloys under repeated loading  

International Nuclear Information System (INIS)

Cyclic strength of #alpha#+#beta#-titanium alloy BT3-1 is studied under load frequencies of 33 and 300 Hz. The increase in the cyclic strength with growing frequency is caused by formation of FCC interphase layers of titanium hydrides. Their formation is one of possible ways of raising the fatigue strength of titanium alloys. Peculiarities of FCC interlayer formation in #alpha#+#beta# phases under loading frequency variation are revealed.

278

Effect of cooling conditions during heat treatment on mechanical properties of titanium alloy VT3-1  

International Nuclear Information System (INIS)

Effect of cooling rates within the wide range (0.003-45 grad/s) on the complex of mechanical properties of (#alpha#-#beta#)-titanium alloy VT3-1 is studied in the process of heat treatment. Cooling conditions of semifinished product made of this alloy with a different structure providing optimum combination of strength, ductility fracture toughness, heat resistance, and endurance are determined.

279

Development of lead-free copper alloy graphite castings. Annual report, January--December 1995  

Energy Technology Data Exchange (ETDEWEB)

The distribution of graphite particles in graphite containing copper alloy was further improved very significantly using several procedures and technological modifications. The developed techniques attacked the graphite distribution problem in two ways. Realizing that clustering of very fine (5um) graphite particles is one of the two major problems, a pretreatment process has been developed using aluminum powders to deagglomerate graphite particles. Along with this, a two-stage stirring technique was used to first incorporate and then to distribute uniformly the deagglomerated particles in the melt. During this year, based on these developments, several components were cast to evaluate the castability of Cu alloy-graphite melts. In addition, machinability tests were done to clearly established that addition of graphite particles improve the machinability of copper MMC alloys over and above that of monolithic copper ...

1996-10-01

280

Deep drawing and impact extrusion of magnesium alloys at room temperature  

Energy Technology Data Exchange (ETDEWEB)

Magnesium alloys and composites are potentially highly attractive materials for lightweight design in the automotive industry - if common forming technologies, i.e., deep drawing and cold extrusion, are applicable to them; so far, this is seldom the case. The authors have tested some candidate Mg alloys and discuss the results of their measurements in detail. The Figure shows a typical workpiece part obtained by a deep-drawing technique. (Abstract Copyright [2003], Wiley Periodicals, Inc.)

2003-04-01

281

Decomposition of metastable solid solution in #beta#-titanium alloy  

International Nuclear Information System (INIS)

Peculiarities of metastable #beta#-solid solution decmposition in titanium alloy VT30 in the process of isothermal ageing in the range 500-650 deg C are investigated. Using the methods of transmittion electron microscopy, X-ray diffraction analysis, etc., it is shown that in the case of alloy quenching from the temperature below the point of complete polymorphous transformation (T_t_._t_.), as well as after warm rolling the course of subsequent decomposition of solid solution can be consierably complicated.

282

Corrosion resistance of metals in hot hydroxide solutions  

International Nuclear Information System (INIS)

Effect of hydroxide nature, concentration and temperature on corrosion resistance of domestic steels and alloys to hot NaOH, KOH, LiOH solutions is considered. It is ascertained that by corrosion growth in relation to stainless steels and nickel alloys, the hydroxides are placed in the following sequence: LiOHalloy tendency to cracking is manifested, are determined. 12 refs., 12 figs.

283

Corrosion in power plant condensers  

International Nuclear Information System (INIS)

A historical overview of corrosion problems found in power plant condensers and mitigation procedures is presented. The paper is organized according to alloy type and failure mode. Alloys considered are copper-base alloys, stainless steels and titanium. Failure modes discussed include erosion-corrosion, sulfide attack, environmentally assisted cracking, galvanic corrosion, steam condensate corrosion, pitting corrosion, and dealloying. Mitigation procedures discussed include cathodic protection, ferrous ion injection, as well as tube cleaning and layup practices.

284

Calculation method of elastic moduli of textured two-phase titanium alloys  

International Nuclear Information System (INIS)

On the basis of symmetry way of texture description a calculation method of elastic moduli of two-phase titanium alloys with rolling texture has been suggested. Efficiency of the calculation formulas is checked by comparing the calculation results of Young modulus anisotropy in the sheet plane of (#alpha#+#beta#)-titanium alloy VT23 with the experimental data.

285

Verification of safety critical software  

Energy Technology Data Exchange (ETDEWEB)

To assure quality of safety critical software, software should be developed in accordance with software development procedures and rigorous software verification and validation should be performed. Software verification is the formal act of reviewing, testing of checking, and documenting whether software components comply with the specified requirements for a particular stage of the development phase[1]. New software verification methodology was developed and was applied to the Shutdown System No. 1 and 2 (SDS1,2) for Wolsung 2,3 and 4 nuclear power plants by Korea Atomic Energy Research Institute(KAERI) and Atomic Energy of Canada Limited(AECL) in order to satisfy new regulation requirements of Atomic Energy Control Boars(AECB). Software verification methodology applied to SDS1 for Wolsung 2,3 and 4 project will be described in this paper. Some errors were found by this methodology during the software development for SDS1 and were corrected by software designer. ...

1996-12-01

286

Verification of safety critical software  

International Nuclear Information System (INIS)

To assure quality of safety critical software, software should be developed in accordance with software development procedures and rigorous software verification and validation should be performed. Software verification is the formal act of reviewing, testing of checking, and documenting whether software components comply with the specified requirements for a particular stage of the development phase[1]. New software verification methodology was developed and was applied to the Shutdown System No. 1 and 2 (SDS1,2) for Wolsung 2,3 and 4 nuclear power plants by Korea Atomic Energy Research Institute(KAERI) and Atomic Energy of Canada Limited(AECL) in order to satisfy new regulation requirements of Atomic Energy Control Boars(AECB). Software verification methodology applied to SDS1 for Wolsung 2,3 and 4 project will be described in this paper. Some errors were found by this methodology during the software development for SDS1 and were corrected by software designer. ...

1996-01-01

287

Trapping technology for gaseous fission products from voloxidation process  

Energy Technology Data Exchange (ETDEWEB)

The objective of this report is to review the different technologies for trapping the gaseous wastes containing Cs, Ru, Tc, {sup 14}C, Kr, Xe, I and {sup 3}H from a voloxidation process. Based on literature reviews and KAERI's experimental results on the gaseous fission products trapping, appropriate trapping method for each fission product has been selected considering process reliability, simplicity, decontamination factor, availability, and disposal. Specifically, the most promising trapping method for each fission product has been proposed for the development of the INL off-gas trapping system. A fly ash filter is proposed as a trapping media for a cesium trapping unit. In addition, a calcium filter is proposed as a trapping media for ruthenium, technetium, and {sup 14}C trapping unit. In case of I trapping unit, AgX is proposed. For Kr and Xe, adsorption on solid is proposed. SDBC (Styrene Divinyl Benzene Copolymer) is also proposed as a conversion ...

2005-05-15

288

Supporting Thermal Hydraulic Calculations for the SGTR Event Tree of SMART Level 1 PSA  

International Nuclear Information System (INIS)

SMART (System integrated Modular Advanced ReacTor) , is under development at the Korea Atomic Energy Research Institute (KAERI). SMART is an integral type pressurized water reactor which contains a pressurizer, 4 reactor coolant pumps (RCPs), and 8 steam generator cassettes(S/Gs) in a single reactor vessel. This reactor has substantially enhanced its safety with an integral layout of its major components, 4 trains of safety injection system (SIS), and an adoption of 4 trains of passive residual heat removal system (PRHRS) instead of an active auxiliary feedwater system . The thermal power is 330 MWth. During the conceptual design stage, a preliminary PSA was performed. PSA results identified that a steam generator tube rupture (SGTR) is one of the most important initiating events which results in a high core damage frequency. Clear understanding of accident progression with various combinations of the safety systems helps to develop an event tree of SGTR accident ...

2010-10-01

289

MARS CODE MANUAL VOLUME V: Models and Correlations  

International Nuclear Information System (INIS)

Korea Advanced Energy Research Institute (KAERI) conceived and started the development of MARS code with the main objective of producing a state-of-the-art realistic thermal hydraulic systems analysis code with multi-dimensional analysis capability. MARS achieves this objective by very tightly integrating the one dimensional RELAP5/MOD3 with the multi-dimensional COBRA-TF codes. The method of integration of the two codes is based on the dynamic link library techniques, and the system pressure equation matrices of both codes are implicitly integrated and solved simultaneously. In addition, the Equation-Of-State (EOS) for the light water was unified by replacing the EOS of COBRA-TF by that of the RELAP5. This models and correlations manual provides a complete list of detailed information of the thermal-hydraulic models used in MARS, so that this report would be very useful for the code users. The overall structure of the manual is modeled on the structure of the ...

2002-09-01

290

Generation of proton-induced nuclear reaction data for C, Fe, Cu and Pb and their benchmark with a deterministic transport code KASKAD-S  

International Nuclear Information System (INIS)

The new proton-induced nuclear reaction data for C, Fe, Cu and Pb for KASKAD-S have been generated using a newly developed data preparation system. The new system utilizes the NJOY and TRANSX codes to prepare these data with the latest evaluation instead of using the SADCO code with the built-in nuclear data. Auxiliary codes have been developed to help the conversion of TRANSX output into the reaction data for running the KASKAD-S. The basic nuclear data selected for this work are the LA150 and KAERI high energy files whose energy ranges are up to 150 and 250 MeV, respectively. The total neutron yields were calculated using KASKAD-S and the new reaction data up to 250 MeV bombarding energy. The calculations were compared with the measurements or MCNPX calculations when the measured data were absent. The comparison shows that our calculations give an overall good agreement with the measurements and MCNPX calculations except around 30 MeV where large discrepancies ...

2003-10-01

291

Flowcytometry of {gamma}-ray irradiated mouse ovary  

Energy Technology Data Exchange (ETDEWEB)

This study was carried out to evaluate the biochemical and morphological effects of ionizing radiation on ovary. Immature mice (ICR, 3 week-old) were irradiated at a dose of LD{sub 80(30)} at KAERI. The ovaries were collected after 6 hours, 12 hours, 1 day, and 2 days post irradiation. To analyze the morphological changes, histological staining with hematoxylin-eosin, immuno- histochemical preparation using in situ 3'-end labeling was performed. DNA fragmentation analysis and flowcytometric evaluation of DNA extracted from whole ovary were performed. As a result of DNA fragmentation analysis, DNA fragments with 185, 370, and 555 base pairs were clearly shown at 6 hours post irradiation. The percentage of A{sub 0} cell cycle was significantly increased in the irradiated group than control. In situ 3'-end labeled follicles were increased at 6 hours post irradiation. The radiation-induced follicular atresia was taken place via an apoptotic ...

1998-10-01

292

Feasibility study on production of Co-60 in PHWR  

Energy Technology Data Exchange (ETDEWEB)

The purpose of this study is to analyze the safeties and the economics for Co-60 production from Wolsung PHWR and to verify the feasibility on the manufacturing of the final Co-60 source for industrial irradiation. The feasibility of reactor conversion was carried out with KEPCO collaboration. Through the site survey on the experience of Gentililly-2 in Canada, a feasibility of plant conversion, changes in design, equipment and tools for Co-60 production was verified. It was estimated that the reactor conversion would not impose adverse impact on plant safety. For the encapsulation of radiation source and storage of the final products, a modification of concrete hot cell at KAERI was primary concerns. The installation and improvement of facilities are needed to avoid cross contamination and extra radiation exposure. Main items for these are pressure gauge, separated HEPA filter the ceiling separation, extra-shielding and ceiling hoist system. At present, storage ...

2000-05-01

293

Evaluation of Core Bypass Flow in the Prismatic VHTR with a Multi-block Experiment  

International Nuclear Information System (INIS)

The core of Prismatic Modular Reactor (PMR) consists of assemblies of hexagonal graphite fuel and reflector elements. The core bypass flow of Very High Temperature Reactor (VHTR) is defined as the core flow that does not pass through the coolant channels but passes through the bypass gap between fuel elements. The increase in bypass flow makes the decrease in effective coolant flow. Since the core bypass flow has a negative impact on safety and efficiency of VHTR, core bypass phenomena have to be investigated to improve the core thermal margin of VHTR. For this purpose, the international project, I-NERI project, has been carried out since 2008. I-NERI project is collaborative project that KAERI and SNU of Korea side and INL, ANL and TAMU of U.S side are involved. In order to evaluate the core bypass flow, the multicolumn and multi-layer experimental facility is designed by SNU. In this experiment, the effect of cross-flow and local variation of bypass gap on the ...

2010-10-01

294

Environmental impact assessment around TRIGA research reactor  

International Nuclear Information System (INIS)

Population distribution, atmospheric change, X/Q, characteristics of terrestrial ecosystem around Seoul site were surveyed. Environmental radiation and radioactivities such as gross#alpha#, gross#beta#, Cs-137, Sr-90 and H-3 of various environmental samples were analyzed. The values of environmental radiation dose tended to increase gradually in the light of the recent five years' results of environmental radiation monitoring around the nuclear power plants from 1980 to 1984, however, the changes were not significant. In addition, continuous assessment of environmental radiation monitoring on the roofs of main building and life science building at KAERI showed that the environmental radiation dose tended to increase a little during the night time. Judging from the above results, it is concluded that environmental contamination level by radioactive materials could be ignored in the case of radioisotope production or experiment using radioisotopes except the release ...

1985-04-01

295

Economic analysis of fuel recycle  

International Nuclear Information System (INIS)

Economic analysis was performed at KAERI with the assistance of US DOE to compare single reactor fuel cycle costs for a once-through option and a thermal recycle option to operate 1 GWe of a PWR plant for its lifetime. A reference fuel cycle cost was first calculated for each option with best estimated reference input data. Then a sensitivity analysis was performed changing each single value of such fuel cycle component costs as yellow cake price, enrichment charges, spent fuel storage cost, reprocessing cost, spent fuel disposal cost and reprocessing waste disposal cost. Savings due to thermal recycle in requirements of uranium, conversion, and enrichment were examined using formulas suggested by US DOE, while MOX fabrication penalty was accounted for. As a result of the reference fuel cycle cost analysis, it is calculated that the thermal recycle option is marginally more economical than the once-through option. The major factors affecting the comparative costs ...

1985-05-19

296

Development of fission Mo-99 production technology  

Energy Technology Data Exchange (ETDEWEB)

This R and D project is planed to supply domestic demands of Mo-99 through fission route, and consequently this project will be expected to rise up utilization of HANARO and KAERI's capability for marketing extension into domestic and oversea radiopharmaceutical market. HEU and LEU target types are decided and designed for fission Mo-99 production in domestic. Experimental study of target fabrication technology was performed and developed processing equipments. And conceptual design of target loading/unloading in/from HANARO device are performed. Tracer test of Mo-99 separation and purification process was performed, test results reach to Mo-99 recovery yield above 80% and decontamination factor above 1600. Combined Mo-99 separation and purification process was decided for hot test scheduled from next year, and performance test was performed. Conceptual design for modification of existing hot cell for fission Mo-99 production facility was performed and ...

2001-05-01

297

Core Heat Transfer Model Validation of the TASS/SMR-S Code using the Bennett's Test  

International Nuclear Information System (INIS)

The SMART (System-integrated Modular Advanced ReacTor) which is a 330 MWt advanced integral PWR was developed by the KAERI (Korea Atomic Energy Institute) for electricity generation and seawater desalination. A thermal hydraulic evaluation and analysis of the SMART is performed by the TASS /SMR-S (Transient And Setpoint Simulation/System integrated Modular Reactor-Safety). The TASS/SMR-S code has various models reflecting the design features of the SMART such as the drift flux model, the core models (core power and core heat transfer model), the component models, and the specific models. One of the core models is the core heat transfer model. The role of this model is to calculate the heat flux and radial temperature profiles at a fuel rod surface using the relevant heat transfer correlations for all of the heat transfer modes. Also it is modeled to meet the requirements of the 10 CFR 50 appendix K EM model for the CHF (Critical Heat Flux) and post CHF conditions. ...

2010-10-01

298

Conceptual Framework of Economic Evaluation on SMRs  

International Nuclear Information System (INIS)

Korea Atomic Energy Research Institute(KAERI) launched a project to develop an integral reactor in 1996. The reactor called as System Integrated Modular Advanced Reactor(SMART) which is a kind of small modular reactors (SMRs). Since the early 1990s, there has been renewed interest in the development and application of small and medium sized integral reactors. 2009 assessment by the IAEA under its Innovative Nuclear Power Reactor and Fuel Cycle (INPRO) program concluded that there could be 96 SMRs in operation around the world by 2030 in its 'high' case, and 43 units in the 'low' case, none of them in the USA. The reason of the increased demand mostly comes from the fact that SMRs are thought to be more suitable for developing countries with small electrical grid capacity, insufficient infrastructure and limited investment capability than developed ones. However, it has disadvantage in the point of scale of economy. So, it should be compared the amount of this ...

2010-10-01

299

Conceptual Design for BOP of the Sodium-Cooled Fast Reactor  

International Nuclear Information System (INIS)

The heavy dependence on nuclear power eventually raise the issues of an efficient utilization of uranium resources, which Korea presently imports from abroad, end of a spent fuel storage. From the viewpoint that sodium-cooled fast Reactors (SFRs) have the potential of an enhanced safety by utilizing inherent safety characteristics, trans-uranics (TRU) reduction and resolving the spent fuel storage problems through a proliferation-resistant actinide recycling. SFRs are sure to be most promising nuclear power operation. The Korea Atomic Energy Research Institute (KAERI) has been developing SFR design technologies since 1997. And nowadays, the preliminary heat balance of the demonstration SFR is calculated. However, in order to verify design condition of the NSSS, it is necessary to set the heat balance and the conceptual design for BOP of the SFR as a part of the SFR design technique development business. Moreover, in order to confirm whether the heat balance can ...

2010-10-01

300

An analysis of PZR and related system design features for KNGR  

Energy Technology Data Exchange (ETDEWEB)

The development of KNGR (Korean Next Generation Reactor) is now in progress. KAERI is developing KNGR which is a advanced active PWR (pressurized water reactor) and 1350 MW electric capacities and is by based on UCN(Ulchin) 3 and 4 nuclear power plant which is a Korean standard PWR. In this report, the PZR (pressurizer) and Related System Design Features for KNGR which include PZR volume, PPCS (pressurizer safety valve)were analyzed. First, the Design Parameters between KNGR compared to UCH 3 and 4 were compared, and second, advanced design features of KNGR compared to UCN 3 and 4 were analyzed. After the present analysis, it has been concluded that the safety margins for the PZR level and pressure of KNGR were more increased by the larger PZR volume than those of UCN 3 and 4, for PZR minimum water level at reactor/turbine trip and PZR maximum pressure at LOCV(loss of condenser vacuum) of KNGR were higher and lower, respectively than those of UCN 3 and 4. Also, it ...

1995-12-01

301

A study on the treatment of radioactive liquid wastes using synthetic by air intake system  

International Nuclear Information System (INIS)

In this study based on the mass transfer theory, experiments for the evaporation rates depending on various conditions were carried out through the operation of the existing Natural Evaporation Facility in KAERI. Evaporation media were made of the cotton and polyester. Air circulation in the facility was forced by exhausting fans. The evaporation rate and the decontamination factor were calculated by the result of experiment. The evaporation rate increased as the flow rate of air supply, the feed rate of liquid waste, and the temperature of supplied air increased. As for the humility of supplied air, the evaporation rate was getting higher as the humidity was getting lower. As the result of this study, operation conditions of the Natural Evaporation Facility are optimized as follows; The air temperature above 8C .deg., the air humidity below 70%, the air flow rate 1.14-1.47 m/sec, and the liquid waste feed rate 4.6l/hr.m"2. The decontamination factor and the ...

2003-11-27

302

Vacuum distillation refining and recycling of magnesium alloys  

Energy Technology Data Exchange (ETDEWEB)

Purification parameters of the vacuum distillation process for AM50A and AZ31B magnesium alloy were studied. The vacuum distillation tests were kept at 580 C to 620 C up to 10 h under a vacuum pressure of about 1 Pa. The purification ratio for AM50A magnesium alloy increases with increasing the purification time. The chemical compositions of materials deposited purifying at 580 C for AM50A magnesium alloy almost satisfy the values for pure magnesium specified by JIS standard specification. The chemical compositions of deposited materials at 600 C for AZ31B magnesium alloy satisfy the values specified by the standard specification except for Zn. (orig.)

2003-07-01

303

TEM analyses of heterogeneous nucleation of internally oxidised multi-component Ag-Zn-based alloys  

Energy Technology Data Exchange (ETDEWEB)

The aim of our research was to identify structures and chemical compositions of phases formed during internal oxidation of multi-component Ag-Zn-Mg-based alloys. Since the ability of inoculation mostly depends on large free energy of formation of oxides of microalloying elements and their crystallographic similarity, Mg in quantities of 0.001-0.5 mass% was selected as a micro-alloying element. These correspond to the quantities of 0.005-2.5 vol.% of MgO in the selected Ag-Zn-based alloys. Ag-based metal matrix, heterogeneous nuclei of MgO and oxide (ZnO) of the main alloying element were analysed by transmission electron microscopy (TEM). Structural inter-connections among them were also investigated and analysed. In situ phenomenon of heterogeneous nucleation of MgO and ZnO was proved. (orig.)

2001-11-01

304

Structure transformation and gain in properties of cast high-temperature T-6242 alloy by thermo-hydrogen treatment  

International Nuclear Information System (INIS)

Thermohydrogen treatment effect on microstructure and mechanical properties is studied for a cast heat resistant pseudo-#alpha#-titanium alloy Ti-6242 (Ti-6Al-2Sn-4Zn-2Mo) widely used as a heat resistant material with operating temperature up to 500 deg C. It is shown that reversible hydrogen alloying is a promising alternative to thermomechanical treatment for transformation of (#alpha#+#beta#)-titanium alloy structure. The application of thermohydrogen treatment is noted to be of particular efficiency for shaped casting technology as it allows a noticeable increase of mechanical properties at a lower cost. The alloy after thermohydrogen treatment and subsequent heat treatment in the (#alpha#+#beta#) - range possesses high values of yield strength fatigue properties, creep resistance and has a satisfactory ductility. A consideration is also given to thermohydrogen treatment effect on fatigue crack ...

305

Structure and properties of a metastable #beta#-alloy aged after plastic deformation  

International Nuclear Information System (INIS)

Phase and structural transformations in a multicomponent (5.05 mas.% Mo-4.95V-3.00Cr-3.05Al) metastable #beta#-titanium alloy on aging after plastic deformation are studied using methods of electron microscopy and X-ray diffraction analysis. The alloy is deformed by twinning in a #left brace#332#right brace# system, and even at initial stages the formation of a twin skeleton takes place in the structure, on further loading the deformation of the skeleton is by secondary twinning resulting in a high plasticity of the alloy. On annealing mechanical twins transform into #alpha#-phase - a ductile twin skeleton is replaced by a rigid skeleton of #alpha#-phase plates. The aging enhances the yield strength of the alloy but decreases sharply its plasticity

2004-12-01

306

Stress-induced martensitic transformation of metastable #beta#-titanium alloy  

International Nuclear Information System (INIS)

The constituent phases and associated deformed microstructure of the quenched Ti-xNb-(0.5-1.5) at.% Si alloy consisting of non-cytotoxicity elements, where x = 24-30 at.%, were investigated to provide pseudoelasticity for biomedical and sensor applications. Optical microscopy revealed that stress-induced martensitic transformation takes place during the deformation in the present alloys. It is confirmed from the X-ray diffraction results of the deformed specimens that the crystal structure of the stress-induced martensite phase is the orthorhombic so-called #alpha#'' structure. Within the alloys having #beta#(bcc) phase studied Nb-poor region appeared to exhibit a dominant behavior for stress-induced martensitic transformation than Nb-rich region. This result suggests that metastable #beta# phase is superior to stable #beta# phase for the occurrence of stress-induced martensitic transformation in the present ...

2007-03-25

307

Polarity of prismatic facets delimiting WC grains in WC-Co alloys  

British Library Electronic Table of Contents (United Kingdom)

This study reports a determination of the polarity of WC facets in WC-Co alloys sintered at the liquid state. In these alloys, WC grains are delimited by basal facets and two sets of {101 0} prismatic facets, one set of facets being much more developed than the other. A variation of the shape is observed as a function of the composition of the alloy. High resolution transmission electron microscopy is used to investigate the polarity of the prismatic facets owing to the typical triangular patterns appearing on the images. The effect of the composition is investigated using two alloys with different carbon potentials and one containing VC and Cr3C2 as grain growth inhibitors. The interpretation of the images shows that in all cases, the same set of prismatic planes is favoured.

2010-01-01

308

On the temperature sensing capability of a fibre optic SPR mechanism based on bimetallic alloy nanoparticles  

Energy Technology Data Exchange (ETDEWEB)

In this work, we have investigated the capability of different bimetallic nanoparticle alloy combinations to be used in fibre optic temperature sensing based on the technique of surface plasmon resonance (SPR). The metals considered for the present analysis are silver, gold and aluminium. The analysis is derived mainly from the thermo-optic effect along with some fundamental concepts of metal optics such as surface scattering, phonon-electron scattering and electron-electron scattering. The performance of the sensor with three different bimetallic nanoparticle alloy combinations is evaluated and compared, numerically, in terms of its sensitivity and accuracy. On the basis of the comparison and some logistic criterion, we predict the best possible bimetallic alloy combination along with a requisite alloy composition ratio that simultaneously provides higher values of both sensitivity and accuracy which ...

2009-02-21

309

Microstructures and tensile properties of wrought magnesium alloys processed by ECAE  

Energy Technology Data Exchange (ETDEWEB)

Magnesium alloys are ideal candidates to benefit from equal channel angular extrusion (ECAE) because of their poor forming characteristics due to a hcp structure. In this study, ECAE processing was applied to ZK31 and AZ31 magnesium alloys under various conditions. The grain size of as-ECAE specimens decreases with decreasing the processing temperature, however, the grain size decreases slightly with increasing number of repetitive processing. Both the tensile strength and 0.2% proof stress of as-ECAE specimens are high when processed at low temperature, but the elongation is high when processed at high temperature. Crystal orientation is different in the two alloys and it also varies according to the processing temperature for the two alloys. The difference of the crystal orientation influences the tensile properties, especially 0.2% proof stress. (orig.)

2003-07-01

310

Microstructural aspects of the corrosion of Alloy 800  

International Nuclear Information System (INIS)

Transmission electron microscopy studies on solution-annealed Alloy 800 revealed small (100-200 nm), spherical-shaped titanium carbide (face centered cubic structure) and large (200 nm-5 #mu#m), faceted titanium nitride (hexagonal structure) particles randomly distributed in the austenite matrix. The volume fraction of former particles was found to be greater than that of the latter. Corrosion studies of the alloy in acidic, chlorides and acidic chloride environments at room temperature indicated that the passivity of Alloy 800 was adversely affected by the addition Cl"- ions. X-ray photoelectron spectroscopy revealed that the surface film formed on the alloy at the onset of passivity consisted of Cr"3"+ (as Cr_2O_3), without any Fe"3"+/Fe"2"+ or Ni"2"+. Scanning electron microscopy studies indicated initiation of pitting at large, faceted particles, not at small, spherical-shaped ones.

2004-12-01

311

Machinability of magnesium alloy in ultra-precision diamond cutting  

Energy Technology Data Exchange (ETDEWEB)

This paper deals with an experimental study of ultra-precision diamond cutting of magnesium alloy (AZ31). In order to investigate the machinability such as the cutting force and the surface integrity and understand the problems in a micro cutting, the experiments on the diamond cutting of magnesium alloy and pure aluminum with an ultra-precision turning machine has been carried out. The machinability of magnesium alloy was compared with that of pure aluminum and discussed. Consequently, both the thrust force component and the surface roughness obtained by cutting of magnesium alloy became larger than that of pure aluminum. It was also found that the inclusions or the defects in the work material caused to generate the scratches on the finished surface and influenced the integrity of mirror surface. (orig.)

2003-07-01

312

Influence of carbon and nitrogen on corrosion resistance of high purity Fe-50mass% Cr alloys  

International Nuclear Information System (INIS)

High purity Fe-50mass%Cr alloys containing (C+N) in the range of 30 to 500 mass ppm were prepared and their corrosion resistance was investigated. Pitting potential in a 3.5mass%NaCl solution at 343K rose with reducing (C+N) content. Alloys containing (C+N) at less than 100 mass ppm did not sustain pitting corrosion. However, alloys containing 500 mass ppm (C+N) corroded severely in 6%FeCl_3+1/20N HCl solutions. Heat treatment at 923K was recognized as influencing corrosion resistance due to precipitation of carbonitrides only in the case of the alloy containing 500 mass ppm (C+N). (orig.).

313

ISO - ISO Standards - TC 156 - Corrosion of metals and alloys  

Wastenet

...ISO - ISO Standards - TC 156 - Corrosion of metals and alloys go to main navigation go to content area go to search International Standards for Business,...ISO Members FAQs Fr ISO Store Products ISO Standards By TC TC 156 Corrosion of metals and alloys ISO Store ISO Standards By ICS By ...aerospace standards Publications and e-products ISO Concept Database (ISO/CDB) Copyright TC 156 - Corrosion of metals and alloys Items to be displayed: Published ...responsibility of TC 156 Secretariat Standard and/or project Stage ICS 3ISO/WD 7441 Corrosion of metals and alloys Determination of bimetallic corrosion in outdoor ...

314

High temperature deformation of the Al-5Cr-2Zr alloy as a function of powder particle diameter  

International Nuclear Information System (INIS)

The powder particle size, D, influences the creep behaviour of Al-Cr-Zr alloys. The alloy studied in this work, Al-5Cr-2Zr (mass%), was prepared by argon atomization. Three size fractions of powder particles were selected: 24-50 #mu#m, 50-100#mu#m and 100-200 #mu#m in diameter. They were consolidated by extrusion. Independently of D, the flow behaviour of the alloy can be described by the power law equation. As test temperature increases, the stress exponent n decreases up to a value close to 5. A decrease of D causes an increase of n and delays the alloy degradation at high temperature. (Author) 11 refs.

1998-01-01

315

Development of a new Pb-free solder: Sn-Ag-Cu  

Energy Technology Data Exchange (ETDEWEB)

With the ever increasing awareness of the toxicity of Pb, significant pressure has been put on the electronics industry to get the Pb out of solder. This work pertains to the development and characterization of an alloy which is Pb-free, yet retains the proven positive qualities of current Sn-Pb solders while enhancing the shortcomings of Sn-Pb solder. The solder studied is the Sn-4.7Ag-1.7Cu wt% alloy. By utilizing a variety of experimental techniques the alloy was characterized. The alloy has a melting temperature of 217{degrees}C and exhibits eutectic melting behavior. The solder was examined by subjecting to different annealing schedules and examining the microstructural stability. The effect of cooling rate on the microstructure of the solder was also examined. Overall, this solder alloy shows great promise as a viable alternative to Pb-bearing solders and, as such, an ...

1995-02-10

316

Design and microstructural analysis of magnesium alloys for dynamical applications  

British Library Electronic Table of Contents (United Kingdom)

A microanalytical characterization of cast magnesium alloys of eutectic origin based on the Mg?Al?Ca ternary matrix system has been carried out in order to investigate the influence of alloying elements on their microstructure as well as microchemistry-processing-microstructural relations using structure-sensitive techniques of electron microscopy, mechanical spectroscopy (internal friction), X-ray diffractometry, and advanced microanalytical methods including electron probe compositional analysis. Following the data obtained here there is direct correlation of microstructure with creep properties of the new experimental magnesium alloys. The creep and heat-induced properties of the multicomponent magnesium alloys containing low range of inexpensive additions of titanium (0.07?0.2%) or str...

2011-01-01

317

Cycleable graphite/FeSi{sub 6} alloy composite as a high capacity anode material for Li-ion batteries  

Energy Technology Data Exchange (ETDEWEB)

FeSi{sub 6}/graphite composite was prepared by mechanical ball milling. The FeSi{sub 6} alloy particles consist of an electrochemically active silicon phase and inactive phases FeSi{sub 2}, distributed uniformly in the graphite matrix. The composite anode offers a large reversible capacity (about 800 mAh g{sup -1}) and good cycleability, due to the buffering effect of the inactive FeSi{sub 2} phase and graphite layers on the volumetric changes of Si phase during lithium-Si alloying reaction. Since FeSi{sub 6} alloy is a low-cost industrial material, this alloy compound provides a possible alternative for development of high capacity lithium-ion batteries. (author)

2008-10-01

318

Comparison on the growth of oxide films formed in alloy 800 and alloy 600 in an aqueous medium at high temperature  

International Nuclear Information System (INIS)

Alloy 800 and Alloy 600 are well known for their resistance to corrosion in an aqueous medium at high pressure and temperature, for which they have been widely used for more than 3 decades in different structural components of water refrigerated nuclear reactors, especially as material for the steam generator tubes (SG) in these nuclear plants. The SG tubes in the Atucha I and Embalse Nuclear Plants are made with Alloy 800. The speed of corrosion of these materials in a reactor's refrigerant medium, while very small is perfectly measurable and can be described by parabolic or logarithmic type kinetics. In other words this speed is high in the first states of growth during the formation of a protective oxide film but then drops to almost stationary values. One characteristic of these films is the formation of a double layer (or duplex): i) an internal adhering layer, of approximately constant thickness, formed by small ...

2006-12-01

319

Capacitive behaviour and electronic structure of passive films formed on nickel base alloy type Inconel 600; influence of Cr and Fe  

International Nuclear Information System (INIS)

The study of passive films formed on a nickel base alloy type Inconel 600 is performed by capacitance measurements (Mott-Schottky approach). This research is supported by the passivation study of the alloying elements Ni, Cr, Fe and high purity alloys Ni-Cr, Ni-Fe, Ni-Cr-Fe. The results obtained show that the capacitive behaviour of the Inconel 600 in the passive state is similar to that on a p-n heterojunction to which a barrier zone of nickel oxide is added. The individual or combined action of alloying elements on the development of this kind of electronic structure is discussed. (authors). 5 refs., 6 figs.

1994-01-01

320

Bulk amorphous and nanocrystalline Al83Fe17 alloys prepared by consolidation of mechanically alloyed amorphous powder  

British Library Electronic Table of Contents (United Kingdom)

In the present work, bulk amorphous and nanocrystalline Al83Fe17 alloys were obtained by consolidation of mechanically alloyed powders. Mechanical alloying of Al-17% Fe powder mixture yielded powder with an amorphous structure. Thermal behaviour of the milling product was examined using differential scanning calorimetry. This investigation revealed that the amorphous phase crystallised above 380^oC. The amorphous powder was compacted under a pressure of 7.7GPa in different conditions: at 380^oC for 600s and at 1000^oC for 180s. Structural investigations of the bulk material revealed that the amorphous structure was retained after consolidation process applied at 380^oC. Compaction under high pressure at 1000^oC caused crystallisation of the amorphous phase and appearance of metastable nano...

2010-01-01

321

Alloy 800 specifications in compliance with component requirements  

Energy Technology Data Exchange (ETDEWEB)

In view of the importance of the material Alloy 800 in high-temperature reactor plants (HTR), a material data bank was established which is used for statistical evaluation of mechanical and physical material behaviour. Based on investigations on the interconnection between the mechanical properties at high temperatures and the metallurgical parameters, different types of Alloy 800 were specified in compliance with the component requirements. In addition, aspects of corrosion and toughness behaviour were taken into consideration. The specifications and strength characteristics for the different variants of Alloy 800 were incorporated into draft DIN standards after discussion and approval in expert committees. Further important characteristics of the mechanical and physical material behaviour were summarized in HTR material data sheets so as to furnish an improved basis for the design and stress analyses of ...

1990-04-01

322

Alloy 800 specifications in compliance with component requirements  

International Nuclear Information System (INIS)

In view of the importance of the material Alloy 800 in high-temperature reactor plants (HTR), a material data bank was established which is used for statistical evaluation of mechanical and physical material behaviour. Based on investigations on the interconnection between the mechanical properties at high temperatures and the metallurgical parameters, different types of Alloy 800 were specified in compliance with the component requirements. In addition, aspects of corrosion and toughness behaviour were taken into consideration. The specifications and strength characteristics for the different variants of Alloy 800 were incorporated into draft DIN standards after discussion and approval in expert committees. Further important characteristics of the mechanical and physical material behaviour were summarized in HTR material data sheets so as to furnish an improved basis for the design and stress analyses of ...

323

A two-component Frenkel-Kontorowa model for surface alloy formation  

Energy Technology Data Exchange (ETDEWEB)

It has been shown by recent experiments that bulk immiscible metals (e.g. Ag/Cu, Ag/Co and Au/Ni) can form binary alloys on certain surfaces where the substrate mediates the elastic misfits between the two components, thus relieving the elastic strain in the overlayer. These novel surface alloys exhibit a rich phase structure. We formulate a two-component Frenkel-Kontorova model in one dimension to study surface alloy formation. This model can naturally incorporate dislocation formation that plays a crucial role in determining the actual structure of the system. Using energy minimization calculations we provide a phase diagram in terms of average alloy composition and the energy of mixing. Monte Carlo simulations were also performed to study the structure and interaction of the emerging dislocations.

2003-04-02

324

Study of superficial films and of electrochemical behaviour of some nickel base alloys and titanium base alloys in solution representation of granitic, argillaceous and salted ground waters  

Energy Technology Data Exchange (ETDEWEB)

The corrosion behaviour of the stainless steels 304, 316 Ti, 25Cr-20Ni-Mo-Ti, nickel base alloys Hastelloy C4, Inconel 625, Incoloy 800, Ti and Ti-0.2% Pd alloy has been studied in the aerated or deaerated solutions at 20/sup 0/C and 90/sup 0/C whose compositions are representative of interstitial ground waters: granitic or clay waters or salt brine. The electrochemical techniques used are voltametry, polarization resistance and complexe impedance measurements. Electrochemical data show the respective influence of the parameters such as temperature, solution composition and dissolved oxygen, addition of soluble species chloride, fluoride, sulfide and carbonates, on which depend the corrosion current density, the passivation and the pitting potential. The inhibition efficiency of carbonate and bicarbonate activities against pitting corrosion is determined. In clay water at 90/sup 0/C, Ti and Ti-Pd show very high passivation aptitude and a broad ...

1985-01-01

325

Effect of PbO on the repassivation kinetics of alloy 690  

Energy Technology Data Exchange (ETDEWEB)

Effects of PbO on the repassivation kinetics of alloy 690TT were examined using the rapid scratching electrode technique under a potentiostatic condition to elucidate the influence of PbO on SCC resistance of the alloy. The repassivation kinetics of the alloy was analyzed in terms of the current density flowing from the scratch, i(t), as a function of the charge density that has flowed from the scratch, q(t). Repassivation on the scratched surface of the alloy occurred in two kinetically different processes; passive film initially nucleated and grew according to the place exchange model in which log i(t) is linearly proportional to q(t) with a slope of 1/K, and then grew according to the high field ion conduction model in which log i(t) is linearly proportional to 1/q(t) with a slope of cBV. 1/K and cBV are parameters representing the SCC susceptibility as well as repassivation rate of the ...

2000-07-01

326

Effect of PbO on the repassivation kinetics of alloy 690  

International Nuclear Information System (INIS)

Effects of PbO on the repassivation kinetics of alloy 690TT were examined using the rapid scratching electrode technique under a potentiostatic condition to elucidate the influence of PbO on SCC resistance of the alloy. The repassivation kinetics of the alloy was analyzed in terms of the current density flowing from the scratch, i(t), as a function of the charge density that has flowed from the scratch, q(t). Repassivation on the scratched surface of the alloy occurred in two kinetically different processes; passive film initially nucleated and grew according to the place exchange model in which log i(t) is linearly proportional to q(t) with a slope of 1/K, and then grew according to the high field ion conduction model in which log i(t) is linearly proportional to 1/q(t) with a slope of cBV. 1/K and cBV are parameters representing the SCC susceptibility as well as repassivation rate of the ...

2000-08-24

327

The Effect of Recasting on Bond Strength between Porcelain and Base-Metal Alloys  

British Library Electronic Table of Contents (United Kingdom)

Abstract Purpose: Long-term success of metal ceramic restorations depends on metal ceramic bond strength. The purpose of this study was to determine whether recasting of base-metal alloys has any effect on metal ceramic bond strength. Materials and Methods: Super Cast and Verabond base-metal alloys were used to cast 260 wax patterns. The alloy specimens were equally divided into five groups and cast as: group A 0.0%, B 25%, C 50%, D 75%, and E 100% once-cast alloy. Each group was divided into two subgroups: the first group was cast with Super Cast and the second with Verabond. In each subgroup half of the cast alloys were veneered with Vita VMK 68 and the others with Ceramco 3. Results: Recasting decreased bond strength (p < 0.006) when used for 50% once-cast alloy. Group E with 100% new S...

2011-01-01

328

Surface improvement and biocompatibility of TiAl{sub 24}Nb{sub 10} intermetallic alloy using rf plasma nitriding  

Energy Technology Data Exchange (ETDEWEB)

The present work describes the surface improvement and biocompatibility of TiAl{sub 24}Nb{sub 10} intermetallic alloy using rf plasma nitriding. The nitriding process was carried out at different plasma power from 400 W to 650 W where the other plasma conditions were fixed. Grazing incidence X-ray diffractometry (GIXRD), Auger electron spectroscopy (AES), tribometer and a nanohardness tester were employed to characterize the nitrided layer. Further potentiodynamic polarization method was used to describe the corrosion behavior of the un-nitrided and nitrided alloy. It has been found that the Vickers hardness (HV) and corrosion resistance values of the nitrided layers increase with increasing plasma power while the wear rates of the nitrided layers reduce by two orders of magnitude as compared to those of the un-nitrided layer. This improvement in surface properties of the intermetallic alloy is due to formation of a thin ...

2007-09-30

329

Surface improvement and biocompatibility of TiAl_2_4Nb_1_0 intermetallic alloy using rf plasma nitriding  

International Nuclear Information System (INIS)

The present work describes the surface improvement and biocompatibility of TiAl_2_4Nb_1_0 intermetallic alloy using rf plasma nitriding. The nitriding process was carried out at different plasma power from 400 W to 650 W where the other plasma conditions were fixed. Grazing incidence X-ray diffractometry (GIXRD), Auger electron spectroscopy (AES), tribometer and a nanohardness tester were employed to characterize the nitrided layer. Further potentiodynamic polarization method was used to describe the corrosion behavior of the un-nitrided and nitrided alloy. It has been found that the Vickers hardness (HV) and corrosion resistance values of the nitrided layers increase with increasing plasma power while the wear rates of the nitrided layers reduce by two orders of magnitude as compared to those of the un-nitrided layer. This improvement in surface properties of the intermetallic alloy is due to formation of a thin modified ...

2007-09-30

330

Study of transformation behavior in a Ti-4.4 Ta-1.9 Nb alloy  

International Nuclear Information System (INIS)

An alloy of composition Ti-4.4 wt.% Ta-1.9 wt.% Nb is being developed as a structural material for corrosion applications, as titanium and its alloys possess excellent corrosion resistance in many oxidizing media. The primary physical metallurgy database for the Ti-4.4 wt.% Ta-1.9 wt.% Nb alloy is being presented for the first time. Determination of the #beta# transus, M_s temperature and classification of the alloy have been carried out, employing a variety of microscopy techniques, X-ray diffraction (XRD), micro-hardness and differential scanning calorimetry (DSC). The #beta# transition temperature or #beta# transus determined using different experimental techniques was found to agree very well with evaluations based on empirical calculations. Based on chemistry and observed room temperature microstructure, the alloy has been classified as an #alpha# + #beta# titanium ...

2005-01-15

331

Straining electrode behavior and corrosion resistance of nickel base alloys in high temperature acidic solution  

International Nuclear Information System (INIS)

Repassivation behavior and IGA resistance of nickel base alloys containing 0#approx#30 wt% chromium was investigated in high temperature acid sulfate solution. (1) The repassivation rate was increased with increasing chromium content. And so the amounts of charge caused by the metal dissolution were decreased with increasing chromium content. (2) Mill-annealed Alloy 600 suffered IGA at low pH environment below about 3.5 at the fixed potentials above the corrosion potential in 10%Na_2SO_4+H_2SO_4 solution at 598K. On the other hand, thermally-treated Alloy 690 was hard to occur IGA at low pH environments which mill-annealed Alloy 600 occurred IGA. (3) It was considered that the reason, why nickel base alloys containing high chromium content such as Alloy 690 (60%Ni-30%Cr-10%Fe) had high IGA/SCC resistance in high temperature acidic solution containing sulfate ...

1991-08-25

332

Stable atomic structure and magnetism of Pt-Cr binary surface alloys on Pt(0 0 1): First-principle calculations  

International Nuclear Information System (INIS)

The possibility of Pt-Cr surface alloys formation on Pt(0 0 1) was investigated and their magnetism was calculated by the full-potential linearized augmented plane wave (FLAPW) method with eight different atomic configurations. The most stable structure was calculated to be the Pt-segregated L1_2 ferromagnetic surface alloy. A_3B types (L1_2 or D0_2_2) were more stable compared to AB types (L1_0). It implies that the A_3B type surface alloys may be formed when depositing a monolayer of Cr on Pt(0 0 1). It was found from the total energy calculations that there exists a strong tendency of the Pt segregation. The segregation further stabilizes the surface alloy significantly. The work function of the most stable surface alloy was calculated to be 6.02 eV and the magnetic moment of the surface Cr was much enhanced to 3.3 #mu# _B. It is a quite interesting finding that the coupling ...

2006-09-01

333

SIMS study of compositional changes observed in a PuO_2 heat source cladding alloy  

International Nuclear Information System (INIS)

Secondary ion mass spectrometry (SIMS) has been used to investigate changes that occur in an advanced Ir-0.3W alloy during high temperature aging. This alloy is used to clad "2"3"8PuO_2 heat sources used in thermoelectric generators for deep space reconnaissance satellites. Long-term direct contact with PuO_2 at 1400"0C leads to physical and chemical changes within the cladding alloy that affect its metallurgical properties. SIMS was used to show that Cr, Fe, Ni, and in some cases O, diffuse from the PuO_2 into the alloy. Thorium and aluminum diffuse out of the alloy in these same regions. This SIMS study suggests that inward O diffusion and subsequent formation of ThO_2 on grain boundaries may stabilize the alloy against enhanced grain growth.

1983-10-11

334

SIMS study of compositional changes observed in a PuO/sub 2/ heat source cladding alloy  

Energy Technology Data Exchange (ETDEWEB)

Secondary ion mass spectrometry (SIMS) has been used to investigate changes that occur in an advanced Ir-0.3W alloy during high temperature aging. This alloy is used to clad /sup 238/PuO/sub 2/ heat sources used in thermoelectric generators for deep space reconnaissance satellites. Long-term direct contact with PuO/sub 2/ at 1400/sup 0/C leads to physical and chemical changes within the cladding alloy that affect its metallurgical properties. SIMS was used to show that Cr, Fe, Ni, and in some cases O, diffuse from the PuO/sub 2/ into the alloy. Thorium and aluminum diffuse out of the alloy in these same regions. This SIMS study suggests that inward O diffusion and subsequent formation of ThO/sub 2/ on grain boundaries may stabilize the alloy against enhanced grain growth.

1983-01-01

335

Optimizing the microstructure of implant alloy TiAl5Fe2.5 by microprobe analysis  

International Nuclear Information System (INIS)

For optimizing the microstructure of the (#alpha# + #beta#)-titanium alloy TiAl5Fe2.5 the content of the two alloying elements aluminium and iron in the #alpha#- and #beta#-phase was determined by microprobe analysis. The alloys with the composition of the #alpha#- and of the #beta#-phase at 850 degC TiAl6Fe0.5 (#alpha#-phase) and TiAl3.5Fe6.5 (#beta#-phase) were prepared by arc melting and rolling at 850 degC. The mechanical properties of the '#alpha#'- and of the '#beta#'-phase-alloy are compared with the properties of the (#alpha# + #beta#)-alloy TiAl5Fe2.5 in the as rolled and swaged condition and after an additional aging at 550 degC. By this optimizing process it was possible to achieve a tensile strength of Rsub(m) = 1012 N/mm"2, an yield strength of Rsub(p0.2) 954 N/mm"2 and an elongation at fracture A = 14.5% in the TiAl5Fe2.5-alloy, although the degree ...

1985-05-13

336

Optimization of INCOLOY alloy 800 mechanical properties for various power plant requirements  

International Nuclear Information System (INIS)

The AMSE Boiler Code development of design stresses and their optimization for alloys 800 and 800H for conventional and nuclear power plants have coincided with many successful trial installations of these grades of alloy 800. These trial installations, along with laboratory tests, have shown that alloy 800H can be used for long times with a retention of good mechanical properties, including ductility. While gamma prime can be formed, it soon loses its detrimental effect on ductility in service. Sensitization of the alloy also occurs but it, too, has a decreasing effect on corrosion resistance with time in service, especially at elevated temperatures. The authors discuss all of these aspects and conclude that alloy 800 perhaps with low carbon control in the annealed (1800 to 1950degF)(982 to 1066degC) condition gives the optimum combination of properties to 1050degF(566degC) and ...

337

On the evolution of quasicrystalline and crystalline phases in rapidly quenched Al-Co-Cu-Ni alloy  

International Nuclear Information System (INIS)

The occurrence of stable decagonal quasicrystalline phase in Al-Co-Ni and Al-Cu-Co alloys through conventional solidification is well established. Earlier, we have studied the effect of Cu substitution in place of Co in the Al_7_0Co_1_5Ni_1_5 alloy. Here we report the structural/micro-structural changes with substitution of Cu for Ni in rapidly solidified Al-Co-Ni alloys. The melt spun ribbons have been characterized using X-ray diffractometry, scanning and transmission electron microscopy. With an increase in Cu content in the melt spun Al_7_0Co_1_5Cu _xNi_1_5_-_x (x = 0-15 at.%) alloys, the relative amount of the decagonal phase decreased up to 10 at.% of Cu. At this composition, the quaternary alloy showed the co-existence of decagonal quasicrystal and superstructure of #tau#_3 vacancy ordered crystalline phases. The decagonal phase containing Cu showed more disordering than ...

2007-03-25

338

Hydrogen transport behavior of Timetal-21S alloy  

International Nuclear Information System (INIS)

Ti-15Mo-2.7Nb-3Al-0.2Si (Timetal-21S), a metastable #beta#-titanium alloy, is a candidate material for titanium matrix composite structures in hydrogen-fueled hypersonic planes because of its excellent formability and adequate mechanical properties in the 500--800 C temperature range. The alloy is strengthened through the precipitation of fine #alpha# particles in the #beta# matrix. The mechanical properties and microstructures are controlled by a solutionizing/aging heat treatment. A major concern in using titanium alloys in hydrogen service is the embrittlement caused by the precipitation of hydrides. It is believed that the large solubility of hydrogen in the #beta#-phase would preclude the precipitation of hydrides in Beta titanium alloys, especially at low hydrogen pressures. However, depending on the hydrogen content, a shift in the ductile/brittle transition temperatures to levels much higher ...

339

Development of a filler metal for Hastelloy alloy XR weldment  

Energy Technology Data Exchange (ETDEWEB)

The weldability and high temperature strength properties of tungsten-inert-gas (TIG) weldments of Hastelloy alloy XR were investigated by using two different heats of filler metals; the first (HXRF1) was designed on the basis of multiple regression analysis; the second (HXRF2) was the reference material. Bend tests, the FISCO cracking test and optical metallography were used to evaluate weldability. Tensile and creep tests were performed at 900deg C to evaluate high temperature strength properties. The results of weldability tests for both alloys showed good performance. The tensile properties of the weldments were remarkably improved in particular with respect to high temperature ductility. The creep rupture strength in the weldments made with alloy-designed HXRF1 was much higher than those of the Hastelloy alloy XR-II base metal with a higher B content. Furthermore, the creep properties were stable ...

1991-11-01

340

Development of a filler metal for Hastelloy alloy XR weldment  

International Nuclear Information System (INIS)

The weldability and high temperature strength properties of tungsten-inert-gas (TIG) weldments of Hastelloy alloy XR were investigated by using two different heats of filler metals; the first (HXRF1) was designed on the basis of multiple regression analysis; the second (HXRF2) was the reference material. Bend tests, the FISCO cracking test and optical metallography were used to evaluate weldability. Tensile and creep tests were performed at 900deg C to evaluate high temperature strength properties. The results of weldability tests for both alloys showed good performance. The tensile properties of the weldments were remarkably improved in particular with respect to high temperature ductility. The creep rupture strength in the weldments made with alloy-designed HXRF1 was much higher than those of the Hastelloy alloy XR-II base metal with a higher B content. Furthermore, the creep properties were stable ...

341

Critical pitting potential of aluminium alloys. Aluminum gokin no koshoku den prime i  

Energy Technology Data Exchange (ETDEWEB)

Pitting corrosion measuring method for almunum alloys sold on the market was studied. By addition of a little quantity of Cu {sup ++} ion, corrosion potential of alminum alloys rapidly approachs to pitting corrosion potential in the solution including chloride. After Cu {sup ++} ion of 5ppm is added in advance into the solution including chrolide to measure the pitting corrosion potential, alminum alloy test pieces are imersed into the solution in the atmospheric air, then the stable corrosion potential is shown after three-minite imersion, and this potential is defined to the pitting corrosion potential. The pitting corrosion potential can be easily measured by this method stated above (copper ion method). The values measured by copper ion method is comparatively agreed with that measured by the existing potentio dynamic method. The pitting corrosion potential have a straight lined relation with the logarithm of Cl {sup -} ...

1990-02-15

342

Crack tip oxidation of a superalloy in molten nitrate salt  

Energy Technology Data Exchange (ETDEWEB)

Alloy 800 has been proposed for use in the receiver tube panel arrays of advanced solar central receiver (SCR) designs. In this application the alloy will be exposed to a molten mixture of sodium and potassium nitrate salts at temperatures ranging up to approximately 600/sup 0/C While these salts are routinely used in a variety of applications including metal heat treating and process heat transfer, common industrial experience has been limited to maximum temperatures of 400/sup 0/C - 450/sup 0/C. There is, therefore, considerable interest in the compatibility of these salts with containment alloys at the higher temperatures associated with SCR designs. Additionally, the containment alloy may be subject to thermally induced fatigue damage resulting from intermittent cloud cover and diurnal cycling. Previous work has found that slower near-threshold fatigue crack growth rates (FCGR) in ...

1983-04-01

343

Constant extension rate (CERT) testing of alloy 690 and 800 nuclear steam generator tubing  

Energy Technology Data Exchange (ETDEWEB)

Constant extension rate (CERT) tests were performed on Alloy 690 and Alloy 800 nuclear steam generator tubing specimens. For the Alloy 690 specimens, tests were performed in deaerated 10% sodium hydroxide solutions at 315 deg C with a +100 mV applied potential. For the Alloy 800 specimens, tests were performed in deaerated 5% sodium hydroxide solutions at 343 deg C with no applied potential. The test specimens were machined from tubing which was produced by different manufacturing processes and in different heat treated conditions. The Alloy 690 tubing was tested in six different thermomechanical conditions, while the Alloy 800 tubing was tested in four different thermomechanical conditions. The results from the test program include a complete microstructural examination using light-optical and scanning electron microscopy. The CERT test results (such as maximum ...

1994-12-31

344

A CANDU utility perspective on using world experience to manage Alloy 800 SG tube degradation  

Energy Technology Data Exchange (ETDEWEB)

In response to European operating experience regarding Alloy 800 steam generator (SG) tube cracking, New Brunswick Power Nuclear (NBPN) recognized two important shortcomings in the industry SG technical support framework. First, information exchange networks between utilities with Alloy 800 SG tubing should be strengthened. Second and more importantly, there is a need for consistent industry guidance for Alloy 800 SG tubing degradation management, supported by clear technical bases. It is NBPN's perspective that this guidance can be improved immediately using the extensive amount of laboratory and field data that is available for Alloys 600, 690, and 800, and EPRI methodology developed to predict the performance of Alloy 690. NBPN has initiated the development of a performance-based inspection plan. This effort is based on demonstrated improvement factors for ...

2007-07-01

345

A CANDU utility perspective on using world experience to manage Alloy 800 SG tube degradation  

International Nuclear Information System (INIS)

In response to European operating experience regarding Alloy 800 steam generator (SG) tube cracking, New Brunswick Power Nuclear (NBPN) recognized two important shortcomings in the industry SG technical support framework. First, information exchange networks between utilities with Alloy 800 SG tubing should be strengthened. Second and more importantly, there is a need for consistent industry guidance for Alloy 800 SG tubing degradation management, supported by clear technical bases. It is NBPN's perspective that this guidance can be improved immediately using the extensive amount of laboratory and field data that is available for Alloys 600, 690, and 800, and EPRI methodology developed to predict the performance of Alloy 690. NBPN has initiated the development of a performance-based inspection plan. This effort is based on demonstrated improvement factors for ...

2007-08-19

346

Tritium and "1"4C in the environment around Wolsong nuclear power plant  

International Nuclear Information System (INIS)

To understand the environmental dispersion trend of "3H and "1"4C discharged from the Wolsung nuclear power plant, the present levels of "3H and "1"4C in environmental samples in the vicinity of the Wolsong site were studied. During 1992 through 2002, the annual means of HTO and "1"4C concentrations in air collected at three sampling stations around Wolsong nuclear power plant were in the range of 1.13 #approx# 29.2 Bq m"-"3 and 0.33 #approx# 0.40 Bq g-C"-"1 respectively, decreasing with distance from the site. The annual mean of TFWT concentrations in pine needle was in the range of 104 #approx# 790 Bq L"-"1 at N-1 and 62.8 #approx# 298 Bq L"-"1 at S"-"2, while the annual mean of "1"4C concentration was in the range of 0.335 #approx# 0.897 g-C"-"1 at N-1 and 0.254 #approx# 0.332 Bq g-C"-"1 #approx# at S"-"2, showing elevated value than a 0.25 Bq g-C"-"1 of background level. (author)

2003-09-01

347

Structural Change Accompanying Crystallization in the Lithium Ion Conductive Li{sub 2}S-SiS{sub 2}-Li{sub 3}PO{sub 4} Oxysulfide Glasses  

Energy Technology Data Exchange (ETDEWEB)

The structural change of the (100-x)(0.6Li{sub 2}S{center_dot}0.4SiS{sub 2})centre dotxLi{sub 3}PO{sub 4} oxysulfide glassesduring crystallization was analyzed by means of solid-state nuclear magnetic resonance (NMR) and X-ray photoelectron spectroscopy (XPS). The unique tetrahedral units of SiO{sub n}S{sub 4-n} (n=1,2,3) and PO{sub n}S{sub 4-n} (n=1,2,3) present in the glass samples vanished and the SiS{sub 4}, PS{sub 4}, SiO{sub 4} units increased with proceeding of the crystallization process. Nonbridging sulfur and oxygen atoms decreased while bridging oxygens and S{sup 2-} increased with proceeding of the crystallization process. Large structural difference between the glass and the corresponding crystallized sample explained the high stability against crystallization found in the oxysulfide glass with the composition of X=5. (author)

1999-02-01

348

Structural Change Accompanying Crystallization in the Lithium Ion Conductive Li[sub 2]S-SiS[sub 2]-Li[sub 3]PO[sub 4] Oxysulfide Glasses  

Energy Technology Data Exchange (ETDEWEB)

The structural change of the (100-x)(0.6Li[sub 2]S[center dot]0.4SiS[sub 2])centre dotxLi[sub 3]PO[sub 4] oxysulfide glassesduring crystallization was analyzed by means of solid-state nuclear magnetic resonance (NMR) and X-ray photoelectron spectroscopy (XPS). The unique tetrahedral units of SiO[sub n]S[sub 4-n] (n=1,2,3) and PO[sub n]S[sub 4-n] (n=1,2,3) present in the glass samples vanished and the SiS[sub 4], PS[sub 4], SiO[sub 4] units increased with proceeding of the crystallization process. Nonbridging sulfur and oxygen atoms decreased while bridging oxygens and S[sup 2-] increased with proceeding of the crystallization process. Large structural difference between the glass and the corresponding crystallized sample explained the high stability against crystallization found in the oxysulfide glass with the composition of X=5. (author)

1999-02-01

349

Roper resonance and S_1_1(1535) from lattice QCD  

International Nuclear Information System (INIS)

Using the constrained-curve fitting method and overlap fermions with the lowest pion mass at 180 MeV, we observe that the masses of the first positive and negative parity excited states of the nucleon tend to cross over as the quark masses are taken to the chiral limit. Both results at the physical pion mass agree with the experimental values of the Roper resonance (N"1"/"2"+(1440)) and S_1_1 (N"1"/"2"-(1535)). This is seen for the first time in a lattice QCD calculation. These results are obtained on a quenched Iwasaki 16"3x28 lattice with a=0.2 fm. We also extract the ghost #eta#"'N states (a quenched artifact) which are shown to decouple from the nucleon interpolation field above m_#pi##approx#300 MeV. From the quark mass dependence of these states in the chiral region, we conclude that spontaneously broken chiral symmetry dictates the dynamics of light quarks in the nucleon.

2005-01-06

350

Roper resonance and S11(1535) from lattice QCD  

International Nuclear Information System (INIS)

Using the constrained curve fitting method and overlap fermions with the lowest pion mass at 180 MeV, we observe that the masses of the first positive and negative parity excited states of the nucleon tend to cross over as the quark masses are taken to the chiral limit. Both results at the physical pion mass agree with the experimental values of the Roper resonance (N"1"/"2"+ (1440)) and S_1_1 (N"1"/"2"-(1535)). This is seen for the first time in a lattice QCD calculation. These results are obtained on a quenched Iwasaki 16"3 x 28 lattice with a = 0.2 fm. We also extract the ghost #eta#(prime) N states (a quenched artifact) which are shown to decouple from the nucleon interpolation field above m_#pi# #approx# 300 MeV. From the quark mass dependence of these states in the chiral region, we conclude that spontaneously broken chiral symmetry dictates the dynamics of light quarks in the nucleon.

351

On mutually unbiased bases  

CERN Document Server

Mutually unbiased bases for quantum degrees of freedom are central to all theoretical investigations and practical exploitations of complementary properties. Much is known about mutually unbiased bases, but there are also a fair number of important questions that have not been answered in full as yet. In particular, one can find maximal sets of ${N+1}$ mutually unbiased bases in Hilbert spaces of prime-power dimension ${N=p^\\m}$, with $p$ prime and $\\m$ a positive integer, and there is a continuum of mutually unbiased bases for a continuous degree of freedom, such as motion along a line. But not a single example of a maximal set is known if the dimension is another composite number ($N=6,10,12,...$). In this review, we present a unified approach in which the basis states are labeled by numbers ${0,1,2,...,N-1}$ that are both elements of a Galois field and ordinary integers. This dual nature permits a ...

2010-01-01

352

Measurement and analysis of alpha particle induced reactions on praseodymium  

International Nuclear Information System (INIS)

Excitation functions (EFs) for the reaction "1"4"1Pr(#alpha#, n)"1"4"4Pm and "1"4"1Pr(#alpha#, 2n)"1"4"3Pm have been measured using "1"4"1Pr as a target up to 50 MeV #alpha#-particle energy. Stacked foil activation technique and #gamma#-ray spectroscopy using 100 cm"3 Ge (Li) detector, has been used. Excitation functions are also calculated theoretically using Blann's geometry dependent hybrid (GDH) model code ALICE-91, with and without inclusion of pre-equilibrium particle emission. It has been observed that high-energy tails of the EFs are dominated by pre-equilibrium reaction mechanism. With the accepted set of input parameter, initial exciton number n_0=4 (2p + 2n + 0h), a good qualitative agreement is found. However, quantitative agreement for this magic nucleus"1"4"1Pr is also good when theoretical calculations are normalized by a multiple factor of 0.5. (author)

2005-04-01

353

Intraoperative electron beam therapy and external photon beam therapy with lumpectomy as primary treatment for early breast cancer  

International Nuclear Information System (INIS)

Between 1984 and 1988, seven women with breast cancer were treated with intraoperative electron beam therapy (IOEBT). All patients were Caucasian. Patient age ranged from 37 to 62 (median 53) years. Histopathology was infiltrating duct carcinoma (6/7) or medullary carcinoma (1/7). Four tumors were staged T1 N0 MO, one T1 N1 MO, one T2 N1 MO, and one lesion was recurrent. At the time of primary lumpectomy or axillary node dissection, a dose of 10 or 15 Gy IOEBT was administered to the tumor bed with 6 or 9 MeV electrons through the lumpectomy wound. All patients received 45 or 50 Gy over five to six weeks with 6 MV photons to the breast and, in four patients, to the regional nodes. Three patients received adjuvant chemotherapy and tamoxifen. No post-operative complications were observed. All patients are alive as of August, 1989, with no evidence of recurrent disease. Excellent cosmesis is the rule. ...

354

Topological Defects in the Moduli Sector of String Theory  

CERN Document Server

We point out that the moduli sector of the $(2,2)$ string compactification with its nonperturbatively preserved non-compact symmetries is a fertile framework to study global topological defects, thus providing a natural source for the large scale structure formation. Based on the target space modular invariance of the nonperturbative superpotential of the four-dimensional N=1 supersymmetric string vacua, topologically stable stringy domain walls are found. They are supersymmetric solutions, thus saturating the Bogomolnyi bound. It is also shown that there are moduli sectors that allow for the global monopole-type and texture-type configurations whose radial stability is ensured by higher derivative terms.

1991-01-01

355

Solid-phase synthesis and pharmacological evaluation of novel nucleoside-tethered dinuclear platinum(II) complexes  

British Library Electronic Table of Contents (United Kingdom)

Three novel inosine-based dinuclear platinum complexes have been synthesized via a solid-phase strategy. In these compounds, the metal is linked both to the N-7 of the purine nucleus and to the terminal amine group of a hexylamine side chain installed on N-1. Cis- or trans- diamine as well as ethylenediamine ligands are coordinated to platinum along with a chloride. The synthesised complexes were tested against four different human tumor cell lines. One of these complexes proved to be more cytotoxic than cisplatin against the MCF7 cancer cell line in a short-term exposure assay.

2011-01-01

356

Shell effects in the symmetric-modal fission of pre-actinide nuclei  

International Nuclear Information System (INIS)

Mass distributions of fragments in the low-energy fission of nuclei from "1"8"7Ir to "2"1"3At have been analysed. This analysis has shown that shell effects in symmetric-mode fragment mass yields from the fission of pre-actinide nuclei could be described if one assumes the existence of two strongly deformed neutron shells in the arising fragments with neutron numbers N_1#approx#52 and N_2#approx#68. A new method has been proposed for quantitatively describing the mass distributions of the symmetric fission mode for pre-actinides with A#approx#180-220. (orig.)

1998-09-21

357

Resonance scattering of Lyman-. cap alpha. radiation by hydrogen in the ground state  

Energy Technology Data Exchange (ETDEWEB)

We calculate the cross section for the resonance scattering of Lyman-..cap alpha.. radiation by spinless nonrelativistic hydrogen atoms in the ground state using a two-level model. A generalization of Dirac's resonance scattering theory is used together with the exact matrix elements for the electromagnetic interaction. In contrast to the usual treatments in which only the dipole approximation for the matrix elements are taken, the shift in position of the resonance is finite and has a value of 75% of the Lamb shift of the n=1 state. Whether this latter fact is significant in renormalization calculations is left open.

1980-11-01

358

Numerical simulation of internal reconnection event in spherical tokamak  

Energy Technology Data Exchange (ETDEWEB)

Three-dimensional magnetohydrodynamic simulations are executed in a full toroidal geometry to clarify the physical mechanisms of the Internal Reconnection Event (IRE), which is observed in the spherical tokamak experiments. The simulation results reproduce several main properties of IRE. Comparison between the numerical results and experimental observation indicates fairly good agreements regarding nonlinear behavior, such as appearance of localized helical distortion, appearance of characteristic conical shape in the pressure profile during thermal quench, and subsequent appearance of the m=2/n=1 type helical distortion of the torus. (author)

1999-07-01

359

Matrix Model, Kutasov Duality and Factorization of Seiberg-Witten Curves  

Energy Technology Data Exchange (ETDEWEB)

We study the duality of N=1 gauge theories in the presence of a massless adjoint field. We calculate the superpotential using the factorization method and compare with the result obtained by applying Kutasov duality. The latter result is just the leading term of the former, indicating that Kutasov duality is exact only in the IR limit as claimed in the original literature. We also study various checks for the equivalence of the calculational methods developed recently: factorization methods, diagrammatic expansion, loop equations, integrating fluxes.

2003-09-29

360

Extended conformal algebras with N=1 supersymmetry  

Energy Technology Data Exchange (ETDEWEB)

Extended conformal algebras with supersymmetry (super-W/sub n/ algebra) is constructed and the algebras are shown to exist for special values of the central charge c. The super-W/sub n/ algebra containing currents of spin (5/2, 3) has a unitary representation (c=10/7) and a non-unitary one (c=-5/2), and the super-W/sub n/ algebra containing currents of spins (2, 5/2) has a non-unitary representation (c=-6/5).

1988-12-29

361

Excitation of Plasma Fluctuations near ion Giro frequencies during RF Plasma Heating in URAGAN-3M Torsatron  

International Nuclear Information System (INIS)

Currentless plasma in Uragan-3M (U-3M) is produced and heated by absorption of RF power in the region of Alfven waves (AW). The process of plasma heating was explained in (2) as a result of Cherenkov absorption of energy of the fast (EM) and slow (kinetic Alfven) waves by electrons and turbulent ion heating due to excitation of short wave ion Bernstein waves (IBW). In this report we present results of studies of plasma density fluctuations showing existence of a narrow bands near the frequencies of ? ? n?ci (n=1,2,3).

2006-01-01

362

Computerized tomography of adrenal glands in the investigation of Cushing's syn  

International Nuclear Information System (INIS)

Computerized tomography of the adrenal glands was performed in 10 patients with Cushing's syndrome using a G.E. 8800 CT/T Body Scanner. The tomographic findings of unilateral adrenal masses in 4 patients were confirmed by surgery. In the remaining 6 patients, computerized tomography did not identify any masses, and both glands were well visualized and showed normal shape. In these patients, measurement of the adrenal glands revealed both normal (n=1) and enlarged glands (n=5). The findings of adrenalectomy (n=4) or transphenoidal surgery and follow-up (n=2) established the diagnosis of adrenal phyperplasia in all patients. (Author).

363

Solubility limits of #alpha#' SIAION solid solutions in the system Si,Al,Y/N,O  

International Nuclear Information System (INIS)

The solubility limit of #alpha#'-SiAlON solid solutions on the Si_3N_4-YN:3AlN composition join in the system Si_3N_4-YN-AlN has been determined at 1800 degrees C. The end members of these solid solutions are Y_0_._4_3Si_1_0_._7Al_1_._3N_1_6 and Y_0_._8Si_9_._6Al_2_._4N_1_6. Unit-cell dimensions of the #alpha#'-SiAlON solid solutions in the system Si,Al,Y/N,O can be expressed as follows: a_0 (Angstrom) = 7.752 + 0.045m + 0.009n, c_0 (Angstrom) = 5.620 + 0.048m + 0.009n, where the #alpha#'-SiAlON solid solution has the formula Y_xSi_1_2_-_(_m _+ _n_)Al_m_+_nN_1_6_-_nO_n. The single-phase boundary of the solid solution #alpha#'-SiAlON on the composition triangle Si_3N_4-YN:3AlN-Al;N:Al_2O_3 is delineated. The present paper also reports the phase relationships involving #alpha#'-SiAlON.

364

Quantitative descriptions of nonlinear gravitational galaxy clustering  

Energy Technology Data Exchange (ETDEWEB)

In order to investigate nonlinear gravitational galaxy clustering, three different quantitative analyses were carried out: two-point correlation functions, {xi}(r); fractal dimensions, D{sub q}; and f(N) statistics. The relation between the exponent {gamma} of the correlation function ({xi}(r) {proportional to} r{sup -{gamma}}) and the fractal dimensions, D{sub q}, was derived with the help of the probability distribution function, f(N), for finding N galaxies within a volume V. The methods were applied to analyze the results of N-body simulations with power law initial density fluctuations ( {delta}{sub k} {sup 2} {proportional to} k{sup n}, n = 1, 0, -1 and -2). These analyses show that the exponent, {gamma}, of the power law {xi}(r) is approximately 2 in the nonlinear regime for models with n = 1 and 0. For models with n = -1 and -2, the correlation functions ...

1990-01-01

365

Histopathological and immunohistochemical findings of 20 autopsy cases with 2009 H1N1 virus infection.  

Science.gov (United States)

Twenty autopsy cases with 2009 pandemic influenza A (2009 H1N1) virus infection, performed between August 2009 and February 2010, were histopathologically analyzed. Hematoxylin-eosin staining, immunohistochemistry for type A influenza nucleoprotein antigen, and real-time reverse transcription-PCR assay for viral RNA were performed on formalin-fixed and paraffin-embedded specimens. In addition, the D222G amino acid substitution in influenza virus hemagglutinin, which binds to specific cell receptors, was analyzed in formalin-fixed and paraffin-embedded trachea and lung sections by direct sequencing of PCR-amplified products. There were several histopathological patterns in the lung according to the most remarkable findings in each case: acute diffuse alveolar damage (DAD) with a hyaline membrane (four cases), organized DAD (one case), acute massive intra-alveolar edema with variable degrees of hemorrhage (three cases), neutrophilic ...

2011-08-26

366

Sulfidation-resistant alloy/cladding for internal components of coal-conversion equipment. Volume 2. Cladding development. Final report  

Energy Technology Data Exchange (ETDEWEB)

An Fe-19Cr-8Al-0.5Hf alloy has been roll bonded to Alloy 800 to form a protective clad material suitable for use in coal conversion atmospheres. The commercial producibility of both the Fe-19Cr-8Al-0.5Hf alloy and the clad composite has been demonstrated. The clad composite has been shown to exhibit resistance to sulfidation in high sulfur, coal gasification atmospheres low Btu for 2000 hrs at 1800/sup 0/F (1255K). The FeCrAlHf alloy must be preoxidized in the absence of sulfur to form fully protective alumina scales on all surfaces. Useful life of the composite at temperatures of 1400 to 2000/sup 0/F (1033 to 1366K) is governed by reactions at the FeCrAlHf clad alloy 800 interface. The rate of interdiffusion decreases with increasing Ni content and a high Ni alloy such as RA333 appears to be a better substrate than Alloy 800 for a FeCrAlHf ...

1981-12-01

367

Stress corrosion cracking susceptibility of alloy 800  

Energy Technology Data Exchange (ETDEWEB)

Steam generators (SGs) in PWRs and CANDUs are designed for at least a 30-year operating life. However, in the 15-25 years that SGs tubed with Alloy 600 have operated commercially, they have experienced reduced reliability, mainly due to SG tubing degradation. One of the degradation mechanisms that Alloy 600 SG tubing has suffered from is lead-induced stress corrosion cracking (PbSCC) in AVT and near-neutral SG environments. In contrast to Alloy 600 tubing, test data obtained in high temperature water indicate that Alloy 800 is resistant to cracking by lead and lead compounds. For Alloy 800 (cold worked, shot peened), the most aggressive environment is reported to be alkaline with minor concentration of PbO (80 ppm). Work by Max Helie et al. also concluded that Alloy 800 is not sensitive to lead assisted SCC for pH values close to neutrality, whereas it could be ...

2002-07-01

368

Stress corrosion cracking susceptibility of alloy 800  

International Nuclear Information System (INIS)

Steam generators (SGs) in PWRs and CANDUs are designed for at least a 30-year operating life. However, in the 15-25 years that SGs tubed with Alloy 600 have operated commercially, they have experienced reduced reliability, mainly due to SG tubing degradation. One of the degradation mechanisms that Alloy 600 SG tubing has suffered from is lead-induced stress corrosion cracking (PbSCC) in AVT and near-neutral SG environments. In contrast to Alloy 600 tubing, test data obtained in high temperature water indicate that Alloy 800 is resistant to cracking by lead and lead compounds. For Alloy 800 (cold worked, shot peened), the most aggressive environment is reported to be alkaline with minor concentration of PbO (80 ppm). Work by Max Helie et al. also concluded that Alloy 800 is not sensitive to lead assisted SCC for pH values close to neutrality, whereas it could be ...

2002-05-05

369

Electronic structure and pitting behavior of 3003 aluminum alloy passivated under various conditions  

International Nuclear Information System (INIS)

Passivity of aluminum (Al) alloy 3003 in air and in aqueous solutions without and with chloride ions was characterized by electrochemical measurements, including cyclic polarization, electrochemical impedance spectroscopy (EIS), localized EIS and potential of zero charge, Mott-Schottky analysis and secondary ion mass spectroscopy (SIMS) technique. Stability, pitting susceptibility and repassivation ability of Al alloy 3003 under various film-forming conditions were determined. Results demonstrated that passive films formed on 3003 Al alloy in air and in Na2SO4 solution without and with NaCl addition show an n-type semiconductor in nature. The passive film formed in chloride-free solution is most stable, and that formed in chloride-containing solution is most unstable, with the film formed in air in between. Pitting of Al alloy 3003 passivated both in air and in aqueous solutions is inevitable in the ...

2009-07-01

370

Electrochemical behavior of Ti-Cr alloys in artificial saliva  

Energy Technology Data Exchange (ETDEWEB)

In this study, the corrosion behavior of commercially pure titanium (c.p. Ti), Ti-6Al-4V and five new experimental Ti-Cr alloys was evaluated through open-circuit potential (OCP) and potentiodynamic polarization measurement in an artificial saliva containing fluoride. Electron spectroscopy for chemical analysis (ESCA) was used to characterize the composition of the passive films on the alloy after potentiodynamic polarization measurement. It was found that in standard artificial saliva the OCP increases with higher Cr content in Ti-Cr alloys. In 0.5% NaF artificial saliva, the OCP decreases with decreasing Cr in Ti-Cr alloys, and all but Ti-5Cr remain consistently higher than those of c.p Ti and Ti-6Al-4V. Linear polarization results show that artificial saliva and artificial saliva containing 0.5% NaF result in different corrosion behavior in Ti-Cr alloys, c.p.Ti and Ti-6Al-4V. The ...

2009-11-13

371

Electrochemical behavior of Ti-Cr alloys in artificial saliva  

International Nuclear Information System (INIS)

In this study, the corrosion behavior of commercially pure titanium (c.p. Ti), Ti-6Al-4V and five new experimental Ti-Cr alloys was evaluated through open-circuit potential (OCP) and potentiodynamic polarization measurement in an artificial saliva containing fluoride. Electron spectroscopy for chemical analysis (ESCA) was used to characterize the composition of the passive films on the alloy after potentiodynamic polarization measurement. It was found that in standard artificial saliva the OCP increases with higher Cr content in Ti-Cr alloys. In 0.5% NaF artificial saliva, the OCP decreases with decreasing Cr in Ti-Cr alloys, and all but Ti-5Cr remain consistently higher than those of c.p Ti and Ti-6Al-4V. Linear polarization results show that artificial saliva and artificial saliva containing 0.5% NaF result in different corrosion behavior in Ti-Cr alloys, c.p.Ti and Ti-6Al-4V. The ...

2009-11-13

372

XPS study of passive films formed on molybdenum-implanted austenitic stainless steels  

Energy Technology Data Exchange (ETDEWEB)

Austenitic stainless steels have been implanted with molybdenum ions (Mo[sup +], 100 keV, 2.5 x 10[sup 16] atoms cm[sup -2]). The implanted material has been characterized by XPS and RBS. The implanted region has a thickness of [approx] 1000 A with a maximum molybdenum concentration of [approx] 9 at.% Mo located at [approx] 210 A from the surface. The effects of implanted molybdenum on the passivation of the alloy in 0.5 M H[sub 2]SO[sub 4] have been investigated by electrochemistry and XPS. After XPS analysis the samples were transferred without exposure to air into a glove-box with an inert atmosphere. The electrochemical behaviour of the alloy is significantly modified by the implanted molybdenum. The major effect is that the activation peak disappears. A bilayer structure (outer hydroxide/inner oxide) of the passive film is observed for both the implanted and non-implanted alloys and the thicknesses of the films are ...

1992-06-01

373

XPS study of passive films formed on molybdenum-implanted austenitic stainless steels  

International Nuclear Information System (INIS)

Austenitic stainless steels have been implanted with molybdenum ions (Mo"+, 100 keV, 2.5 x 10"1"6 atoms cm"-"2). The implanted material has been characterized by XPS and RBS. The implanted region has a thickness of #approx# 1000 A with a maximum molybdenum concentration of #approx# 9 at.% Mo located at #approx# 210 A from the surface. The effects of implanted molybdenum on the passivation of the alloy in 0.5 M H_2SO_4 have been investigated by electrochemistry and XPS. After XPS analysis the samples were transferred without exposure to air into a glove-box with an inert atmosphere. The electrochemical behaviour of the alloy is significantly modified by the implanted molybdenum. The major effect is that the activation peak disappears. A bilayer structure (outer hydroxide/inner oxide) of the passive film is observed for both the implanted and non-implanted alloys and the thicknesses of the films are similar. On the implanted ...

1991-10-01

374

Visualization of direct contact heat transfer between water and molten alloy  

Energy Technology Data Exchange (ETDEWEB)

We have been developing an innovative Steam Generator concept of Fast Breeder Reactors by using liquid-liquid direct contact heat transfer. In this concept, the SG shell is filled with a molten alloys, which is heated by primary sodium. Water is fed into the high temperature molten alloy, and evaporates by direct contact heating. In order to obtain the fundamental information to discuss the heat transfer mechanisms of the direct contact between the water and the alloy, this phenomenon was visualized by real-time neutron radiography. JRR-3M real-time thermal neutron radiography in Japan Atomic Energy Research Institute was used. Followings are main results. (1) The vigorous evaporation occurs in the molten alloy. This phenomena is different from the known phenomenon such as the evaporation of refrigerant R-113 in the water. (2) The evaporation in the bubble has finished in a moment due to high heat ...

1996-06-01

375

U.S. Contribution 1994 Summary Report Task T12: Compatibility and irradiation testing of vanadium alloys  

Energy Technology Data Exchange (ETDEWEB)

Vanadium alloys exhibit important advantages as a candidate structural material for fusion first wall/blanket applications. These advantages include fabricability, favorable safety and environmental features, high temperature and high wall load capability, and long lifetime under irradiation. Vanadium alloys with (3-5)% chromium and (3-5)% titanium appear to offer the best combination of properties for first wall/blanket applications. A V-4Cr-4Ti alloy is recommended as the reference composition for the ITER application. This report provides a summary of the R&D conducted during 1994 in support of the ITER Engineering Design Activity. Progress is reported for Vanadium Alloy Production, Welding, Physical Properties, Baseline Mechanical Properties, Corrosion/Compatibility, Neutron Irradiation Effects, Helium Transmutation Effects on Irradiated Alloys, and the Status of Irradiation ...

1995-03-01

376

The radiation hardening and microstructural defect evolution in ion irradiated Fe-Cr alloys with irradiation temperature  

International Nuclear Information System (INIS)

Generally, neutron, ion and electron Irradiations cause a substantial amount of hardening and significantly alter the deformation behavior of metals and alloys at relatively low irradiation temperatures. A radiation hardening is caused by the formation of microstructural defects such as dislocation loops, voids and precipitates under irradiation. Therefore, it is important to have a better knowledge of the irradiation induced microstructural defects under irradiation condition. As a part of the National mid- and long-term atomic energy R and D program, we are dealing with the radiation hardening behavior in Fe-Cr binary alloy. Fe-Cr binary alloy is a base alloy of Ferritic/Martensitic steel(F/M steel) planning to use for the Gen IV nuclear system. In this work, we investigated the radiation hardening and microstructural defect evolution in ion irradiated Fe-Cr alloys with ...

2009-05-01

377

The influence of yttrium (Y) on the corrosion of Mg-Y binary alloys  

International Nuclear Information System (INIS)

Research highlights: #-># The Y-intermetallic can accelerate corrosion and Y can increase the protectiveness of the surface layer. #-># In 0.1 M NaCl, the corrosion rate of Mg-Y alloys increased with increasing Y due to the Y intermetallic. #-># In 0.1 M NaCl, there was filiform corrosion. #-># In 0.1 M Na_2SO_4, the corrosion rate of Mg-Y alloys decreased with increasing Y in the range 3-7%Y. #-># Hydrogen evolution was observed from particular parts of the alloy surface. - Abstract: Corrosion of Mg-Y alloys was studied using electrochemical evaluations, immersion tests and direct observations. There were two important effects. In 0.1 M NaCl, the corrosion rate increased with increasing Y content due to increasing amounts of the Y-containing intermetallic. In 0.1 M Na_2SO_4, the corrosion rate decreased with increasing Y content above 3%, attributed to a more protective surface film, ...

2010-11-01

378

The Effect of Applied Pressure During Feeding of Critical Cast Aluminum Alloy Components With Particular Reference to Fatigue Resistance  

Energy Technology Data Exchange (ETDEWEB)

the medium to long freezing range alloys of aluminum such as A356, A357, A206, 319 for example are known to exhibit dispersed porosity, which is recognized as a factor affecting ductility, fracture toughness, and fatigue resistance of light alloy castings. The local thermal environment, for example, temperature gradient and freezing from velocity, affect the mode of solidification which, along with alloy composition, heat treatment, oxide film occlusion, hydrogen content, and the extent to which the alloy contracts on solidification, combine to exert strong effects on the porosity formation in such alloys. In addition to such factors, the availability of liquid metal and its ability to flow through the partially solidified casting, which will be affect by the pressure in the liquid metal, must also be considered. The supply of molten metal will thus be controlled by the volume of ...

2003-06-30

379

Synthesis of MgB{sub 2} from gas atomized Mg alloy powders and its superconductivity  

Energy Technology Data Exchange (ETDEWEB)

Superconducting MgB{sub 2} samples were prepared by the sintering of a mixture of fine Mg (or Mg alloy) powder produced by gas-atomization and B powder. The single MgB{sub 2} phase with a superconducting onset temperature of 38 K was obtained by sintering at 1073 K for the pure Mg or AZ31 alloy powders. In the case of AZ31, the superconducting MgB{sub 2} was obtained by sintering at a low temperature of 873 K for 50 h although a long sintering time of 100 h is needed to obtain a single MgB{sub 2} phase for Mg powder. This indicates that the AZ31 alloy enhances a formation rate of superconducting MgB{sub 2} at the low temperature through the formation of the partial melting phase. Thus, the gas-atomized fine Mg or AZ31 alloy powders are useful for preparation of a superconducting MgB{sub 2} and in particular AZ31 alloy is effective for the low temperature fabrication of MgB{sub 2}. ...

2003-07-01

380

Results of in-house cone-cup testing of low to high temperature SPF-alloys  

Energy Technology Data Exchange (ETDEWEB)

Material testing of SPF-sheet is usually done with coupon hot tensile testing. The optimum range of strain rates is determined with stepped strain tests. To overcome the problem of very few available testing facilities and time consuming and costly procedure, cone cup testing has been developed since long. This test can be generated directly in the workshop, no machining of samples is necessary and it is very much related to the real SPF-process. The analysis of suitable temperature and strain rate is done by simple measurement of resulting cone height. This paper describes a unique and novel variant of the above mentioned baseline design. It provides on-line data of the actual status of the cone cup forming resulting from the applied, constant pressure. Strain rate variations as a result from texture or from the alloy-related behaviour is detectable. Thinning and ''hardening'' behaviour of different alloys ...

2004-07-01

381

Research on deformation characteristic of AZ31Mg alloy and its constitutive equations  

Energy Technology Data Exchange (ETDEWEB)

Superplasticity of polycrystalline metallic materials is a phenomenon which shows hundreds to thousands of percents of large plastic deformation without necking in a steady state of low stress, when the uni-axial tensile loading is done in some special thermo-mechanical conditions (some limited ranges of properly high temperature and low strain rate). The main mechanism of superplastic phenomenon is the grain boundary sliding, while the main mechanism of usual plastic deformation is the trans-granular sliding. In this research, the possibility of superplastic deformation in a magnesium alloy (AZ31Mg alloy) was experimentally investigated, because generally speaking, the magnesium alloy whose atomic structure is hexagonal does not have enough formability in a form of trans-granular sliding mechanism. In this paper, the detail of experimental results are shown and discussed. Moreover, the constitutive equations of Mg ...

2004-07-01

382

Recent advances and developments in refractory alloys  

Energy Technology Data Exchange (ETDEWEB)

Refractory metal alloys based on Mo, W, Re, Ta, and Nb (Cb) find applications in a wide range of aerospace applications because of their high melting points and high-temperature strength. This paper, presents recent progress in understanding and applications of these alloys. Recent studies to improve the oxidation and mechanical behavior of refractory metal alloys, and particularly Nb alloys, are also discussed. Some Re structures, for extremely high temperature applications (> 2000C), made by CVD and P/M processes, are also illustrated. Interesting work on the development of new W alloys (W-HfC-X) and the characterization of some commercial refractory metals, e.g., K-doped W, TZM, and Nb-1%Zr, continues. Finally, recent developments in high temperature composites reinforced with refractory metal filaments, and refractory metal-based intermetallics, e.g., Nb{sub 3}Al, Nb{sub ...

1993-11-01

383

Promising materials for HTGR high temperature heat exchangers  

International Nuclear Information System (INIS)

The service conditions for high-temperature heat-exchangers with helium coolant of HTGRs and requirements imposed on materials for their production are discussed. The choice of nickel-base alloys with solid-solution hardening for long-term service at high temperatures is grounded. Results of study on properties and structure of types Ni-25Cr-5W-5Mo and Ni-20Cr-20W alloy in the temperature range of 900 deg. - 1,000 deg. C are given. The ageing of Ni-25Cr-5W-5Mo alloy at 900 deg. - 950 deg. C results in decreased corrosion-mechanical properties and is caused by the change of structural metal stability. Alloy with 20% tungsten retains a high stability of both structure and properties after prolonged exposure in helium at above temperatures. The alloy has also increased resistance to delayed fracture and low-cycle fatigue at high temperatures. The developed alloy of ...

1989-06-01

384

Numerical Modeling of Magnesium Alloy Sheet Metal Forming at Elevated Temperature  

International Nuclear Information System (INIS)

The development of light-weight vehicle is in great demand for enhancement of fuel efficiency and dynamic performance. The vehicle weight can be reduced effectively by using lightweight materials such as magnesium alloys. However, the use of magnesium alloys in sheet forming processes is still limited because of their low formability at room temperature and the lack of understanding of the forming process of magnesium alloys at elevated temperatures. In this study, uniaxial tensile tests of the magnesium alloy AZ31B-O at various temperatures were performed to evaluate the mechanical properties of this alloy relevant for forming of magnesium sheets. To construct a FLD (forming limit diagram), a forming limit test were conducted at temperature of 100 and 200 deg. C. For the evaluation of the effects of the punch temperature on the formability of a rectangular cup drawing with AZ31B-O, ...

2007-05-17

385

Microstructure fracture toughness and fatigue crack growth rate in titanium alloys; Proceedings of the 1987 TMS-AIME Annual Symposium, Denver, CO, Feb. 24, 25, 1987  

Science.gov (United States)

The papers contained in this volume provide an overview of recent theoretical and experimental research related to the fracture toughness and fatigue crack growth characteristics of titanium alloys. Topics discussed include room temperature fatigue crack propagation in beta-titanium alloys, fatigue crack growth rate acceleration in alpha+beta Ti alloys, influence of transformed beta microstructures on fatigue crack growth rates in Ti-6Al-4V, and the role of inclusion and pore content on the fracture toughness of powder processed blended elemental Ti-10V-2Fe-3Al. Papers are also presented on fatigue crack growth measurements in an alpha-beta titanium alloy, the effects of thermal processing variation on the properties of Ti-6Al-4V, and the effect of microstructure on ductility and fracture toughness of alpha+beta titanium alloys.

1987-01-01

386

Microstructure evolution and fracture behavior in superplastic deformation of hot-rolled AZ31 Mg alloy sheet  

Energy Technology Data Exchange (ETDEWEB)

Fine-grained AZ31 magnesium alloy sheets were prepared through hot rolling process. The superplastic properties of hot-rolled AZ31 Mg alloy was examined by uniaxial tensile tests at a temperature range 250{proportional_to}450 C and strain rate range 0.7 x 10{sup -3}{proportional_to}1.4 x 10{sup -1} s{sup -1}. Optical and scanning electronic microscope (SEM) were used to observe the microstructure evolution and fracture behavior in superplastic deformation of AZ31 Mg alloy and the values of deformation activation energy at various temperatures were calculated. It is demonstrated that, the hot-rolled AZ31 alloy begins to exhibit superplasticity from 300 C and a maximum elongation of 362.5% is obtained at 400 C and 0.7 x 10{sup -3} s{sup -1}. In the temperature range 300{proportional_to}400 C, the dominant superplastic deformation mechanism is grain boundary sliding (GBS) controlled by grain boundary ...

2005-07-01

387

Microstructural evolution of the surface of Mg-Al-based alloy by hydrogen treatment  

Energy Technology Data Exchange (ETDEWEB)

The present paper describes the development of ultra-fine grains on the surface of AZ31 alloys caused by hydrogenation and dehydrogenation treatment, so-called HDDR process. Upon hydrogenation process, disproportionation reaction occurred in forming of MgH{sub 2}, Mg{sub 0.42}Al{sub 0.58}, and Al phases. In the following desorption process, the three phases were re-solved into the AZ31 alloy. As a result of the HDDR phenomena, the grain size of AZ31 alloy powders was reduced down to about 100 nm after the heat treatment at 350 C under a hydrogen pressure of 7 MPa for 24 h. The grain size tended to be increased with increasing process temperatures. In addition, the HDDR process was also applied to AZ31 alloy plates. By the HDDR process at 450 C, the grain size was reduced to less than 500 nm, where hydrogenated layer thickness was limited to be in the range of about 20 {mu}m from the surface. The Vickers ...

2003-07-01

388

Influence of metallurgical factors on corrosion and electrochemical behavior of structural materials  

Energy Technology Data Exchange (ETDEWEB)

An analysis of the passive films formed on amorphous alloys of the system Fe-10% Cr-5% Mo-P-metalloid and Fe-10% Cr-5% Mo-B-Si revealed that they are more markedly enriched with chromium in silicon-free alloys. In silicon-containing amorphous alloys the passive films were highly enriched with silicon, which occurred in these films in the form of a corrosion product close to SiO/sub 2/. As shown by the investigations of a study of the anodic behavior of Fe/sub 40/Ni/sub 40/P/sub 14/B/sub 6/ and Fe/sub 40/Ni/sub 38/Mo/sub 4/B/sub 18/, phosphorus facilitates the passivation of amorphous alloys by reducing the solution current in the active state and enriching the surface layers of the metal in the form of a black prepassivation film which also contains nickel and iron. The behavior of Fe-Ni amorphous alloys containing only boron as metalloid additive differs little from that of ...

1986-07-01

389

Influence of metallurgical factors on corrosion and electrochemical behavior of structural materials  

International Nuclear Information System (INIS)

An analysis of the passive films formed on amorphous alloys of the system Fe-10% Cr-5% Mo-P-metalloid and Fe-10% Cr-5% Mo-B-Si revealed that they are more markedly enriched with chromium in silicon-free alloys. In silicon-containing amorphous alloys the passive films were highly enriched with silicon, which occurred in these films in the form of a corrosion product close to SiO_2. As shown by the investigations of a study of the anodic behavior of Fe_4_0Ni_4_0P_1_4B_6 and Fe_4_0Ni_3_8Mo_4B_1_8, phosphorus facilitates the passivation of amorphous alloys by reducing the solution current in the active state and enriching the surface layers of the metal in the form of a black prepassivation film which also contains nickel and iron. The behavior of Fe-Ni amorphous alloys containing only boron as metalloid additive differs little from that of crystalline alloys of ...

1986-01-01

390

Grain-boundary self-diffusion of alloy 800 and influence of S, P and C on grain-boundary diffusion and creep cavity formation in alloy 800  

Energy Technology Data Exchange (ETDEWEB)

Alloy 800 is an austenitic Fe-Ni-Cr steel containing relatively minor but important amounts of carbon, aluminium and titanium. Special grades of alloy 800 known as 800H, 800HT and 800LC differ in the concentrations of these elements. In addition to these industrial specifications, further melts were prepared containing phosphorous or sulphur. Using a radioactive tracer method the bulk and grain-boundary diffusion of {sup 59}Fe was investigated in these alloys in the temperature range 800 to 1000 C. For evaluation of the diffusion profiles the approximation of Suzuoka was used, which considers the depletion of the tracer on the surface. By autoradiography it was confirmed that such depletion occurs. In alloy 800H the activation energy of grain-boundary diffusion of {sup 59}Fe was found to be (209{+-}17) kJ/mol; dissolved elements, especially phosphorous, increase the activation energy. The same materials ...

1999-10-01

391

Grain-boundary self-diffusion of alloy 800 and influence of S, P and C on grain-boundary diffusion and creep cavity formation in alloy 800  

International Nuclear Information System (INIS)

Alloy 800 is an austenitic Fe-Ni-Cr steel containing relatively minor but important amounts of carbon, aluminium and titanium. Special grades of alloy 800 known as 800H, 800HT and 800LC differ in the concentrations of these elements. In addition to these industrial specifications, further melts were prepared containing phosphorous or sulphur. Using a radioactive tracer method the bulk and grain-boundary diffusion of "5"9Fe was investigated in these alloys in the temperature range 800 to 1000 C. For evaluation of the diffusion profiles the approximation of Suzuoka was used, which considers the depletion of the tracer on the surface. By autoradiography it was confirmed that such depletion occurs. In alloy 800H the activation energy of grain-boundary diffusion of "5"9Fe was found to be (209#+-#17) kJ/mol; dissolved elements, especially phosphorous, increase the activation energy. The same materials - aged ...

392

Grain boundary self-diffusion of alloy 800 as affected by sulphur, phosphorous and carbon  

Energy Technology Data Exchange (ETDEWEB)

Using a radioactive tracer method the bulk and grain boundary diffusion of {sup 59}Fe was determined in industrial alloy 800 and melts of alloy 800 with additional P and S in the temperature range 800 to 1000 C. The use of the approximation of Suzuoka was confirmed by autoradiographs. In alloy 800 H the activation energy of grain boundary diffusion of {sup 59}Fe is (209 {+-} 17)kJ/mol. Dissolved elements especially P increase the activation energy of the grain boundary diffusion of Fe by their segregation to the grain boundaries. In addition the influence of the grain boundary diffusion on the growth of creep cavities was investigated in the same materials, and the chemical composition of the creep cavities and grain boundaries were analysed by Auger electron spectroscopy (AES). For alloy 800 + 0.088 wt-%P an enrichment of about 14 at-%P was observed at the grain boundaries. The addition of P clearly ...

1999-08-01

393

Grain boundary self-diffusion of alloy 800 as affected by sulphur, phosphorous and carbon  

International Nuclear Information System (INIS)

Using a radioactive tracer method the bulk and grain boundary diffusion of "5"9Fe was determined in industrial alloy 800 and melts of alloy 800 with additional P and S in the temperature range 800 to 1000 C. The use of the approximation of Suzuoka was confirmed by autoradiographs. In alloy 800 H the activation energy of grain boundary diffusion of "5"9Fe is (209 #+-# 17)kJ/mol. Dissolved elements especially P increase the activation energy of the grain boundary diffusion of Fe by their segregation to the grain boundaries. In addition the influence of the grain boundary diffusion on the growth of creep cavities was investigated in the same materials, and the chemical composition of the creep cavities and grain boundaries were analysed by Auger electron spectroscopy (AES). For alloy 800 + 0.088 wt-%P an enrichment of about 14 at-%P was observed at the grain boundaries. The addition of P clearly enhances ...

1998-07-06

394

Experimental investigation on the fretting wear of alloy 800 in room remperature water  

Energy Technology Data Exchange (ETDEWEB)

Fretting wear test in room temperature water was performed to evaluate the wear coefficient of CANDU (CANadian Deuterium Uranium) steam generator (SG) tube material (Alloy 800) against 410 type martensitic stainless steels. The main focus is to compare the wear behaviors between Alloy 800 and Inconel 690. Test conditions are 10{approx}30N of normal load, 200{approx}450mm of sliding amplitude and 30Hz of frequency. The result indicated that the wear rate of Alloy 800 was higher than those of Inconel 690 at various test condition such as normal loads, sliding amplitudes etc. From the results of SEM observation, there was little evidence of plastic deformation layer that were dominantly formed on the worn surfaces of Inconel 690. Also, wear particles in Alloy 800 were released from contacting asperities deformed by severe plastic flow during fretting wear. Main cause of wear rate between ...

2002-05-01

395

Experimental investigation on the fretting wear of alloy 800 in room remperature water  

International Nuclear Information System (INIS)

Fretting wear test in room temperature water was performed to evaluate the wear coefficient of CANDU (CANadian Deuterium Uranium) steam generator (SG) tube material (Alloy 800) against 410 type martensitic stainless steels. The main focus is to compare the wear behaviors between Alloy 800 and Inconel 690. Test conditions are 10#approx#30N of normal load, 200#approx#450mm of sliding amplitude and 30Hz of frequency. The result indicated that the wear rate of Alloy 800 was higher than those of Inconel 690 at various test condition such as normal loads, sliding amplitudes etc. From the results of SEM observation, there was little evidence of plastic deformation layer that were dominantly formed on the worn surfaces of Inconel 690. Also, wear particles in Alloy 800 were released from contacting asperities deformed by severe plastic flow during fretting wear. Main cause of wear rate between ...

2002-05-01

396

Evaluation of microstructures and mechanical properties in the HAZ of SA 508 Gr.4N Low Alloy Steel  

International Nuclear Information System (INIS)

In the heat-affected zones (HAZ) of low alloy steels used for nuclear pressure vessel, microstructural changes, such as grain coarsening, carbide precipitation, and martensite formation, generally occur and cause a deterioration of toughness and an increase in sensitivity to brittle fracture. Metallographic analyses of low alloy steel welds reveal significantly different regions in HAZ microstructures. In 2-pass welds, there were seven characteristic regions in the HAZ determined by the peak temperature, to which the region was exposed during the weld thermal cycle: a coarse-grained region, a fine-grained region, an intercritical region, and subcritical region. The coarse-grained region can be categorized into four zones according to the reheating temperature as follows : an unaltered coarse-grained zone (UCGHAZ), a supercritically reheated coarse grained zone (SCRCGHAZ), an intercritically reheated coarse-grained zone (ICRCGHAZ), and an ...

2006-11-02

397

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 2. Roles on hydrogen pickup  

Energy Technology Data Exchange (ETDEWEB)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. In the previous paper, corrosion mechanism was elucidated by the anodic protection-precipitates degradation model. This paper describes the roles on hydrogen pickup. 633 K pure water autoclave test was performed on high purity zirconium, Zr-0.2Fe, Zr-0.2Cr, and Zr-0.1Fe-0.1Cr alloys. Hydrogen analysis after the corrosion test showed that hydrogen pickup ratio of Zr-0.2Fe alloy was about 80%. It was much higher than about 30% of pure Zr and about 10% of both Zr-0.2Cr and Zr-0.1Fe-0.1Cr alloys. Larger hydrogen content was introduced into Zr-0.2Fe alloy than the other ones by the cathodic hydrogen charging under coulombic equivalence. The precipitates at ...

2000-08-01

398

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 2. Roles on hydrogen pickup  

International Nuclear Information System (INIS)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. In the previous paper, corrosion mechanism was elucidated by the anodic protection-precipitates degradation model. This paper describes the roles on hydrogen pickup. 633 K pure water autoclave test was performed on high purity zirconium, Zr-0.2Fe, Zr-0.2Cr, and Zr-0.1Fe-0.1Cr alloys. Hydrogen analysis after the corrosion test showed that hydrogen pickup ratio of Zr-0.2Fe alloy was about 80%. It was much higher than about 30% of pure Zr and about 10% of both Zr-0.2Cr and Zr-0.1Fe-0.1Cr alloys. Larger hydrogen content was introduced into Zr-0.2Fe alloy than the other ones by the cathodic hydrogen charging under coulombic equivalence. The precipitates at ...

2000-08-01

399

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 1. Roles on corrosion  

Energy Technology Data Exchange (ETDEWEB)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. This paper describes the roles on corrosion. A corrosion test on precipitate-containing and precipitate-free materials made from pure zirconium and a small quantity of iron and chromium, rest potential measurements on an intermetallic compound of Zr(FeCr){sub 2} and zirconium matrix, and a galvanic coupling test of those were performed. Results showed that corrosion behavior of zirconium alloys could be attributed to the electrochemical properties of intermetallic compounds precipitated in each alloy. Namely, the cathodic and anodic polarization characteristics were associated with anodic protection provided by the precipitates on the alloys and the precipitates degradation in ...

2000-07-01

400

Electrochemical roles of precipitates on uniform corrosion and hydrogen pickup of zirconium alloys, 1. Roles on corrosion  

International Nuclear Information System (INIS)

Substantial roles of precipitates such as Zr-Fe-Cr type intermetallic compounds on uniform corrosion and hydrogen pickup of zirconium alloys in pure water autoclave tests were investigated from an electrochemical point of view. This paper describes the roles on corrosion. A corrosion test on precipitate-containing and precipitate-free materials made from pure zirconium and a small quantity of iron and chromium, rest potential measurements on an intermetallic compound of Zr(FeCr)_2 and zirconium matrix, and a galvanic coupling test of those were performed. Results showed that corrosion behavior of zirconium alloys could be attributed to the electrochemical properties of intermetallic compounds precipitated in each alloy. Namely, the cathodic and anodic polarization characteristics were associated with anodic protection provided by the precipitates on the alloys and the precipitates degradation in the ...

2000-07-01

401

Effect of solute content on plasma nitriding behavior of Fe-Cr alloys; Fe-Cr gokin purazuma chikka kyodo ni oyobosu yoshitsu nodo no eikyo  

Energy Technology Data Exchange (ETDEWEB)

It has been clarified by the present authors, based on the plasma nitriding of Fe-Cr alloys and Fe-Ti alloys carried out at the temperature under 550{degree}C hitherto, that an internal nitriding layer is formed due to the fine dispersion of the particles of Cr nitride and Ti nitride in {gamma}{prime} Fe4N layer on the specimen surface. In this study, the plasma nitriding of Fe-Cr alloys are carried out at 650{degree}C, and the effects of the solute (Cr) content on the structures, nitride and the thickness distribution are examined. The main results obtained therefrom are indicated hereafter. In accordance with the observation on the cross-sectional structure of the alloys, only the nitriding layer deduced as the dispersion and precipitation of the particles of Cr nitride from {alpha}-Fe of the mother phase is formed, while {gamma}{prime}-Fe4N layer, which is found at the temperature under 550{degree}C, ...

1996-03-15

402

Effect of minor alloying element variation on the properties of Alloy 800  

International Nuclear Information System (INIS)

Application of Alloy 800 in steam generator tubing of fast reactors, where continuous service temperature of the order of 550"0C is experienced, has been analyzed with respect to small variations in its chemical composition. Several laboratory melts of Alloy 800 have been prepared and their microstructural and mechanical property changes during simple aging and creep tests at 500 to 600"0C have been studied. It has been found that in the above temperature range precipitation of M_2_3C_6 on the grain boundaries is independent of the Ti : C ratio generally specified for Alloy 800. Gamma prime precipitation occurred in alloys containing as low as 0.5 percent Ti + Al after 1000 h of aging and was accompanied with a creep ductility decline. Upon #gamma# precipitation creep rate was retarded and its reacceleration for test times up to 8500 h at 550"0C was not observed. Based on the findings, increased Ti ...

403

Corrosion behavior of materials at high temperature by environmental oxidants containing sulfur derivatives: effects of aggressive phase composition on experimental alloys. Final report  

Energy Technology Data Exchange (ETDEWEB)

For a better understanding of sulphidation mechanisms, some alloys (alloy 600, alloy 800, Uranus S, iron-chromium-aluminium-alloy) and metals (iron, chromium, nickel, molybdenum, titanium) were tested at 773, 873, 1 073 K in gaseous sulphur dioxide. Total pressure was 760 torrs. Sulphur dioxide pressure was 760, 100 and 10 torrs. Argon, oxygen, water vapor were used, successively, as pressure complement. Oxygen supply, generally speaking cause decay of corrosion resistance in SO/sub 2/ atmospheres especially at 1 073 K with low ratio p/sub O2//P/sub SO/sub 2//. Water vapor supply act similarly. Temperature laws and pressure laws do not give monotonous rise of corrosion values. There are maximas suggesting corrosion products undertaking a volatilization process. According to test conditions, Uranus S, chromium, alloy 800 (and titanium at some extent) showed good corrosion resistance. ...

1981-01-01

404

Corrosion and mass transfer of ternary alloys (Fe-Ni-Cr) in anisothermal semi-stagnant Pb17Li  

Energy Technology Data Exchange (ETDEWEB)

Corrosion of several materials including pure metals Fe, Ni, Cr and also Fe-Cr, Fe-Ni-Cr alloys, has been studied in anisothermal Pb17Li (Tmax = 500 deg C; {Delta}T = 60 deg C). The corrosion rate of pure nickel is two orders of magnitude higher than the chromium one and about three orders of magnitude higher than the iron one. Fe-Cr alloys (1.4914) suffers a dissolution rate equal to the one of its major constituent, iron. With regard to the three austenitic materials (316L and NS20 steels, alloy 800), they exhibit a porous corrosion layer mainly constituted of ferrite but containing also a small amount of {sigma} phase in the case of the alloys with higher Ni content, NS30 steel and alloy 800. Mechanism of formation of this layer is discussed.

1990-12-31

405

Charge redistribution in ion-beam-mixed Pd-Ag alloys  

Science.gov (United States)

Charge flow and valence/d-band behavior in ion-beam-mixed (IBM) Pd1-xAgx (x = 0.5-0.9) alloys have been studied by X-ray photoemission measurement of the valence bands and of core-level binding energy shifts and X-ray absorption near-edge structure. We correlated the observed Ag 3d5/2 core-level shifts in these IBM alloys, relative to the elemental Ag, with the White Line area changes at the Pd and Ag L3-edge to investigate the charge redistribution at the Ag site. The results indicate that there is a decrease in sp-like conduction electron and a negligible change in the number of d-electrons at the Ag site upon alloying. These results are in line with our previous results in which Pd gains d-charges and loses sp-type charges. This electron redistribution due to hybridization in the alloy leads small net charge transfer from the Ag site to the Pd site in accordance with electronegativity predictions. ...

1996-08-01

406

An evaluation of corrosion resistant alloys by field corrosion test in Japanese refuse incineration plants  

Energy Technology Data Exchange (ETDEWEB)

As the first step for development of the corrosion resistant superheater tube materials of 500 C, 100 ata used in high efficient waste-to-energy plants, field corrosion tests of six conventional alloys were carried out at metal temperatures of 450 C and 550 C for 700 and 3,000 hours in four typical Japanese waste incineration plants. The test results indicate that austenitic alloys containing approximately 80 wt% [Cr+Ni] show excellent corrosion resistance. When the corrosive environment is severe, intergranular corrosion of 40{approximately}200 {micro}m depth occurs in stainless steel and high alloyed materials. It is confirmed quantitatively that corrosion behavior is influenced by environmental corrosion factors such as Cl concentration and thickness of deposits on tube surface, metal temperature, and flue gas temperature. The excellent corrosion resistance of high [Cr+Ni+Mo] alloys such as ...

1995-12-01

407

An evaluation of corrosion resistant alloys by field corrosion test in Japanese refuse incineration plants  

International Nuclear Information System (INIS)

As the first step for development of the corrosion resistant superheater tube materials of 500 C, 100 ata used in high efficient waste-to-energy plants, field corrosion tests of six conventional alloys were carried out at metal temperatures of 450 C and 550 C for 700 and 3,000 hours in four typical Japanese waste incineration plants. The test results indicate that austenitic alloys containing approximately 80 wt% [Cr+Ni] show excellent corrosion resistance. When the corrosive environment is severe, intergranular corrosion of 40#approx#200 microm depth occurs in stainless steel and high alloyed materials. It is confirmed quantitatively that corrosion behavior is influenced by environmental corrosion factors such as Cl concentration and thickness of deposits on tube surface, metal temperature, and flue gas temperature. The excellent corrosion resistance of high [Cr+Ni+Mo] alloys such as ...

1995-03-26

408

Texture development of AZ31 magnesium alloy during ECAE processing  

Energy Technology Data Exchange (ETDEWEB)

Mg-3%Al-1%Zn (AZ31) alloy was subjected to ECAE processing at 523 and 573 K. Microstructure observation and texture analysis were carried out using optical microscope and SEM-EBSD technique in order to investigate the process of microstructural changes including texture development during ECAE processing. Grain refinement during ECAE processing is enhanced by dynamic continuous recrystallization. The texture of the ECAE-processed AZ31 alloy specimens change with ECAE processing temperature, and the textural changes relate to deformation mechanisms that change with ECAE processing temperature. (orig.)

2003-07-01

409

Structural origin of optical bowing in semiconductor alloys p  

Energy Technology Data Exchange (ETDEWEB)

The principle of conservation and transferability of chemical bonds explains the recent discovery by extended x-ray absorption fine-structure measurements of two unequal anion-cation bond lengths R/sub A/C and R/sub B/C in A/sub x/B/sub 1-x/C zinc-blende semiconductor alloys despite the close adherence of the lattice constant to the average value (Vegard rule). This bond alternation, manifested as a structural distortion to a local chalcopyrite coordination around the anions, explains also most of the observed optical bowing in semiconductor alloys.

1983-08-22

410

Structural origin of optical bowing in semiconductor alloys p  

International Nuclear Information System (INIS)

The principle of conservation and transferability of chemical bonds explains the recent discovery by extended x-ray absorption fine-structure measurements of two unequal anion-cation bond lengths R/sub A/C and R/sub B/C in A/sub x/B/sub 1-x/C zinc-blende semiconductor alloys despite the close adherence of the lattice constant to the average value (Vegard rule). This bond alternation, manifested as a structural distortion to a local chalcopyrite coordination around the anions, explains also most of the observed optical bowing in semiconductor alloys.

411

Structural Phase Transition in AuZn Alloys  

Energy Technology Data Exchange (ETDEWEB)

AuxZn1-x alloys undergo a shape memory martensitic transformation whose temperature and nature (continuous or discontinuous) is strongly composition dependent. Neutron diffraction experiments were performed on single crystals of x=50 and 52 to explore the structural changes occurring at the transition temperature. A transverse modulation with wavevector q0=(1/3,1/3,0) develops below the transition temperature, with no observable change in lattice parameter. However, the Bragg peak width shows a broadening suggesting an unresolved rhombohedral distortion similar to what has been observed in NiTi-Fe alloys.

2009-05-03

412

Strain induced hardening in Ti-3Al-4V at 910 deg. C  

International Nuclear Information System (INIS)

High temperature deformation behavior of an alpha + beta titanium alloy Ti-3Al-4V has been investigated at 910 deg. C. by using the method of cross head speed cycling. On the basis of flow stress, strain rate and strain rate sensitivity data, the alloy was found to exhibit strain hardening at this temperature which resulted in degradation in superplastic properties of the alloy. A high beta-phase volume fraction and grain-growth in both alpha and beta phases were considered responsible for the observed hardening effect. (author)

413

Reversible Movement of Homogenously Nucleated Dislocations in a #beta#-Titanium Alloy  

International Nuclear Information System (INIS)

We demonstrate reversible movement of (1/2)[110](110) dislocation loops generated from nanodisturbances in a #beta#-titanium alloy. High resolution transmission electron microscope observations during an in situ tensile test found three reversible deformation mechanisms, nanodisturbances, dislocation loops and martensitic transformation, that are triggered in turn with increasing applied stress. All three mechanisms contribute to the nonlinear elasticity of the alloy. The experiments also revealed the evolution of the dislocation loops to disclination dipoles that cause severe local lattice rotations.

2009-01-30

414

Pitting corrosion of copper and copper alloys. (Latest citations from the Metals Abstracts alloys index database). Published Search  

Energy Technology Data Exchange (ETDEWEB)

The bibliography contains citations concerning the pitting corrosion of copper and copper alloys, in different media, with some references to methods for protecting against such corrosion. Included are factors contributing to the onset of pitting corrosion. Emphasis is placed on exposure to water, especially in tubing for heat exchangers and water conduits. Many of the citations present studies on exposure to sea water. Some references pertain to the detection of pitting corrosion in installations and the evaluation of the degree of pitting present. (Contains 250 citations and includes a subject term index and title list.)

1993-09-01

415

Pitting corrosion of copper and copper alloys. (Latest citations from the EI Compendex*plus database). Published Search  

Energy Technology Data Exchange (ETDEWEB)

The bibliography contains citations concerning the pitting corrosion of copper and copper alloys by different media, with some references to methods that protect against such corrosion. Included are factors contributing to the onset of pitting corrosion. Emphasis is placed on exposure to water, especially in heat exchanger tubing and water conduits. Studies are included which examine corrosion in metals containing small amonts of copper where corrosion is attributable to changes in alloying. (Contains a minimum of 158 citations and includes a subject term index and title list.)

1994-04-01

416

On the hydrogen etching mechanism in plasma nitriding of metals  

International Nuclear Information System (INIS)

Iron alloys and aluminum were nitrogen implanted in a controlled oxygen atmosphere and the role of hydrogen on the surface etching mechanisms studied. The surface composition was analyzed by in situ photoemission electron spectroscopy (XPS). In iron alloys, hydrogen strongly etches oxygen, improving nitrogen retention on the surface. On the other hand, hydrogen removes nitrogen from aluminum surfaces, with a deleterious effect on the nitriding effectiveness. The oxygen removal in iron alloys is associated with the catalytic effect of electrons in d-orbitals and the nitrogen removal in aluminum is associated with a steric effect.

2006-12-15

417

Occurrence of magnetism in superconductors  

Science.gov (United States)

We discuss how magnetic phenomena affect superconductivity in simple metals, transition metals and alloys thereof, and dilute Rare-Earth alloys. It is shown both qualitatively and quantitatively that superconductors are sensitive probes for studying itinerant spin excitations, local spin excitations associated with nearly magnetic impurities, the effect of the atomic environment on the stability of local magnetic moments, and the nature of the spin order in Rare-Earth alloys. Also, we discuss how magnetic impurities can be used to study the electronic configuration which is responsible for superconductivity in Laves-phase crystals like A-15 compounds and ..beta..-W crystals, for example.

1970-12-14

418

Mechanical properties of joints welded in halogen-containing controlled atmosphere  

International Nuclear Information System (INIS)

Studied are the mechanical properties of welded joints and heat affected zones of the Kh8N10T steel and OT4 and VT1-2 titanium alloys on welding in Ar+deltaF_6 and Ar+CCl_2F_2 mixtures contributed to a decrease of porosity. Tensile and impact tests of welded joints have revealed that additions of sulfur hexafluoride into argon causes a decrease of impact strength in titanium alloy when the tensile strength does not depend on the composition of a halogen-containing atmosphere. Freon (CCl_2F_2) additions decrease only slightly the impact strength of the investigated alloys.

419

Impacts of amorphous metal-based transformers on energy efficiency and environment  

International Nuclear Information System (INIS)

Magnetic properties of a recently developed Fe-based amorphous alloy with a high saturation induction of 1.65 T are reviewed. The increased saturation induction is fully utilized in transformers with reduced magnetic losses, physical sizes and audible noises, minimizing some of the drawbacks of amorphous metal-based transformers based on a currently available amorphous alloy. Impacts of this on the worldwide energy savings and reduction of greenhouse gas emissions are discussed. A recent effort in achieving a saturation induction beyond 1.65 T in nanocrystalline alloys is mentioned.

2008-10-01

420

Hot workability, microstructural control and rate-controlling mechanisms in cast-homogenized AZ31 magnesium alloy  

Energy Technology Data Exchange (ETDEWEB)

Optimum conditions for microstructural control in industrial hot working of cast and homogenized AZ31 magnesium alloys are evaluated by using a processing map. The recommended window for bulk metal working of this alloy is the domain in the temperature range 300-450 C and strain rate range 1-10 s{sup -1}, and the optimum processing parameters are 400 C and 10 s{sup -1}, where grain-boundary self diffusion is the rate-controlling mechanism. (Abstract Copyright [2009], Wiley Periodicals, Inc.)

2009-03-15

421

High temperature fatigue example of creep life time prediction for grade 2 alloy 800 at 550 C  

Energy Technology Data Exchange (ETDEWEB)

Experimental data on the material characteristics of structures subjected to thermal and mechanical cycling are needed for designing structural parts for creep and creep-fatigue interaction. Moreover, high-temperature low-cycle fatigue data are not sufficient to predict the fatigue creep lifetime. In order to check the reliability of steam generators, tests on pipe materials are conducted under cyclic thermal loading. The tests have been performed on an iron-nickel chromium alloy (alloy 800). Isothermal low-cycle fatigue tests have been conducted at 550 C. 15 refs.

1994-04-01

422

Evaluation of SCC susceptibility of alloy 800 under CANDU SG secondary-side conditions  

Energy Technology Data Exchange (ETDEWEB)

As part of a coordinated program, AECL is developing a set of tools to aid with the prediction and management of steam generator performance. Although stress corrosion cracking (of Alloy 800) has not been detected in any operating steam generator, for life management it is necessary to develop mechanistic models to predict the conditions under which stress corrosion cracking is plausible. Therefore, constant extension rate tests were carried out for Alloy 800 under various steam generator crevice chemistry conditions at applied potentials. These tests were designed to evaluate the stress corrosion cracking susceptibility of Alloy 800 under CANDU( steam generator operating conditions. Based on the experimental results, the recommended electrochemical corrosion potential/pH zone for Alloy 800 determined by electrochemical polarization measurements was verified with the respect of stress corrosion cracking ...

2006-07-01

423

Evaluation of SCC susceptibility of alloy 800 under CANDU SG secondary-side conditions  

International Nuclear Information System (INIS)

As part of a coordinated program, AECL is developing a set of tools to aid with the prediction and management of steam generator performance. Although stress corrosion cracking (of Alloy 800) has not been detected in any operating steam generator, for life management it is necessary to develop mechanistic models to predict the conditions under which stress corrosion cracking is plausible. Therefore, constant extension rate tests were carried out for Alloy 800 under various steam generator crevice chemistry conditions at applied potentials. These tests were designed to evaluate the stress corrosion cracking susceptibility of Alloy 800 under CANDU( steam generator operating conditions. Based on the experimental results, the recommended electrochemical corrosion potential/pH zone for Alloy 800 determined by electrochemical polarization measurements was verified with the respect of stress corrosion cracking ...

2006-11-26

424

Energetical analysis of sensitivity of hydrogen embrittlement of ordered alloys  

Science.gov (United States)

Intermetallic compounds are regarded as highly promising for applications as high temperature structural materials. However, recent studies have demonstrated that a number of ordered alloys exhibit environmental embrittlement when tested in various environments at ambient temperature. When exposed to hydrogen gas or electrolytically charged with hydrogen, a significant ductility loss has been reported. The reaction of water vapor with reactive elements in the crack tip results in the generation of atomic hydrogen which diffuses from the surface to the interior and causes embrittlement. In this paper, the authors try to analyze the sensitivity of hydrogen embrittlement of ordered alloys based upon energetical considerations.

1993-10-01

425

Electron microscopy analysis of grain boundary structure and composition in superplastically deformed Al-Mg alloys  

Energy Technology Data Exchange (ETDEWEB)

Evaluation of grain boundary composition and structure in superplastically deformed AA5083-based alloys (Al-4.5Mg-1.6Mn-0.2Zr) was carried out in a field-emission gun transmission electron microscope (FEG-TEM). During superplastic deformation at high homologous temperatures materials undergo extensive grain boundary sliding (GBS) which creates a flow of defects in the near-boundary region. Recent literature has shown that the grain-boundary composition in Al-Mg alloys is not necessarily the same as the matrix, and that these differences can have an effect on GBS.

1996-12-31

426

Electron combinational light scattering in disordered Ti_x_-_1Fe_x alloys: theory and experiment  

International Nuclear Information System (INIS)

Theoretical description of Raman scattering in disordered alloys of Ti and Zr with transition metals of groups 5-8 of the Mendeleev Periodic System in critical range of concentrations (CRC) is given. Results of Raman scattering experiment in the system Ti_1_-_xF_x at 0.0005alloys studied near CRC is shown.

427

Effect of deformation on corrosion behavior of Ti-23Nb-0.7Ta-2Zr-O alloy  

International Nuclear Information System (INIS)

The influence of deformation on the corrosion behavior of a newly developed multifunctional beta titanium alloy Ti-23Nb-0.7Ta-2Zr-O (mol%) in Ringer's solution at 310 K was evaluated using an electron backscatter diffraction technique and electrochemical measurements. The results showed that the effect of deformation on the corrosion resistance of the beta titanium alloy is complicated. Small levels of plastic deformation are detrimental to the corrosion resistance, whereas large deformations tend to eliminate this detrimental effect.

2009-03-01

428

Effect of #alpha#-phase morphology and distribution on the tensile ductility of a metastable beta titanium alloy  

International Nuclear Information System (INIS)

In a program to develop a metastable beta alloy with improved fracture toughness, it was found that the tensile ductility of the alloy Ti-8 Mo-4.5 Cr-2.5 Al was strongly dependent on both processing history and annealing temperature. Evaluation of the microfracture mode of tensile samples by scanning electron microscope and metallographic techniques showed that the presence of a continuous grain boundary alpha is the most significant parameter controlling the ductility and is highly detrimental. It is concluded that, for optimum processing, the material must be worked prior to aging to avoid this grain boundary phase.

429

Diffusion bonding on superplastic-aluminum and -magnesium alloys  

Energy Technology Data Exchange (ETDEWEB)

The superplastic characteristics and diffusion bonding behaviors were investigated in commercial 7475 aluminum alloy and AZ31 magnesium alloy sheets. In this study, the presently used materials behaved in a superplastic manner at {proportional_to} 773 K (7475Al) and {proportional_to} 523 K (AZ31). Then, by the theoretical relationship between pressure and time, these materials were successfully diffusion bonded at the superplastic temperatures. The bonding strength was more than 65 MPa. The experimental bonding conditions in high quality joining, times and pressures, were good agreed with prediction analysis. (orig.)

2004-07-01

430

Damping measurements of the magnesium wrought alloys AZ31, AZ61 and AZ80 after indirect and hydrostatic extrusion  

Energy Technology Data Exchange (ETDEWEB)

Magnesium cast parts as well as indirectly and hydrostatically extruded profiles were used in order to investigate the influence of different microstructures on the damping behaviour of magnesium AZ-alloys. Especially, hydrostatic extrusion leads to a significant grain refinement in the extruded profile compared to indirect extrusion. Strain dependent damping measurements were carried out at room temperature using alloys AZ31, AZ61 and AZ80. Damping was determined as the logarithmic decrement of free bending beam vibrations. The results of these measurements after indirect and hydrostatic extrusion are shown and discussed. (orig.)

2005-07-01

431

Creep properties of modified 9 Cr-1 Mo steel  

Energy Technology Data Exchange (ETDEWEB)

Creep properties of modified 9 Cr-1 Mo steel, an alloy significantly improved in elevated-temperature strength over 2 1/4 Cr-1 Mo and other similar alloys, are presented here. Data are primarily on material in the normalized and tempered condition. Effects of variables such as isothermal annealing treatment, cold work, normalizing temperature, tempering temperature, notch, and biaxial stress state have also been examined. Data analysis and comparisons have shown that modified 9 Cr-1 Mo alloy is very insensitive in response to several material variables, heat treatments, and specimen design variables.

1983-01-01

432

Corrosion and protection of magnesium alloy AZ31D by a new conversion coating  

Energy Technology Data Exchange (ETDEWEB)

A chromium-free conversion coating for magnesium alloys were described. The conversion coating could be obtained when AZ31D magnesium alloy was immersed in a solution containing a manganese salt, phosphate and an inhibitor. Corrosion resistance of the chemical conversion coating was evaluated by anodizing polarization curve and salt immersion. XRD analysis showed that the conversion coating was mainly composed of Mn{sub 3}(PO{sub 4}){sub 2}. The morphology of the coating is observed by using SEM. The effect of electrolyte pH and concentration of inhibitor on coating growth are investigated. (orig.)

2003-07-01

433

Anomaliously high radiation hardening of iron-chromium alloys  

International Nuclear Information System (INIS)

Argon ions irradiation of 12% Cr steels and Fe/Cr alloys results in the hardening up to 10000 MPa. This value exceeds the hardening level even for martensitic transformation. Along with the increase of microhardness following irradiation the shape of X-ray graph of the affected materials changes considerable. Hardening value and behavior are determined by temperature radiation doze, preliminary ageing, extent of cold strain and alloying. The odserved phenomenon is supposed to be caused by irradiation-induced structural transformations. Reversibility of radiation hardening of the materials in question was observed.

434

An influence of ion bombardment on plasma nitriding process of Ti6Al14V alloy at 843 K temperature  

International Nuclear Information System (INIS)

This work presents results of investigations on d.c. glow discharge nitriding of #alpha#+#beta# Ti-6Al-4V titanium alloy. The treatment was performed at 843 K in nitrogen-hydrogen atmosphere, pressure 300 Pa. Special attention was paid to nitriding mechanism and determination of the role of ion bombarding in nitriding process of titanium alloys. Produced as a result of d.c. plasma nitriding surface layers were subjected to macroscopic observations, microstructure studies, microhardness testing and X-ray analysis. (author)

2004-06-20

435

Ab initio study of the elastic anomalies in Pd-Ag alloys  

International Nuclear Information System (INIS)

Ab initio total-energy calculations, based on the exact muffin-tin orbital method, are used to determine the elastic properties of Pd1-xAgx random alloys in the face-centered-cubic crystallographic phase. The compositional disorder is treated within the coherent-potential approximation. The single crystal and polycrystalline elastic constants and the Debye temperature are calculated for the whole range of concentration, 0?x?1. It is shown that the variation in the elastic parameters of Pd-Ag alloys with chemical composition strongly deviates from a simple linear or parabolic trend. The complex electronic origin of these anomalies is demonstrated.

2009-02-15

436

A study on the grain refining effects of carbon inoculation by C{sub 2}Cl{sub 6} addition on AZ31 magnesium alloy  

Energy Technology Data Exchange (ETDEWEB)

The effects of carbon inoculation by C{sub 2}Cl{sub 6} addition were investigated using commercial AZ31 magnesium alloy. The additions of C{sub 2}Cl{sub 6} to AZ31 magnesium alloy significantly reduce the grain size from 280 {mu}m to about 120 {mu}m and the tensile properties are also increased due to grain refinement. EPMA analysis shows that Al-C-O compounds are formed in the castings which are considered to function as nucleants. (orig.)

2003-07-01

437

A review of the behaviour of alloy 800 in liquid sodium  

International Nuclear Information System (INIS)

Although there is service experience of Alloy 800 as tubing for superheaters in conventional and nuclear (HTR) power stations and in PWR heat exchangers, there is no corresponding service experience in sodium-cooled fast reactor steam generators. However, some limited experimental studies have been made of corrosion behaviour, and of possible structure modifications and effects on mechanical properties which occur during exposure of this material to a high temperature sodium environment, and these are summarised in the paper. It is concluded that further work needs to be done before Alloy 800 can be confidently endorsed for use as tubing in fast reactor steam generators. (author).

438

iMAST Quarterly, Number 1, 1998  

Science.gov (United States)

... Airframe System Technoloqies Laser fabricated flooring Composite sandwich panels for noise control Spray formed HS aluminum alloys Protective ...

2011-05-14

439

[Magnetic thin film research]: Progress report year 2  

Energy Technology Data Exchange (ETDEWEB)

The work in the past year has primarily involved four areas of magnetic thin films: amorphous rare earth-transition metal alloys, epitaxial CoPt{sub 3} and Ni-Pt alloy thin films, amorphous rare earth doped Si (a new class of dilute magnetic semiconductor with large negative magnetoresistance which the authors have discovered), and exchange-coupled antiferromagnetic insulators. In the amorphous alloys, they made a systematic study of the effects of local anisotropy, macroscopic (perpendicular) anisotropy, and exchange constant on the fundamental (and practical) properties of these magnetic alloys, as originally described in the grant proposal. The work on the epitaxial Co-Pt (and more recently Ni-Pt) alloys was originally undertaken as a comparison study to the amorphous alloys. Crystalline Co-Pt alloys have many striking similarities to the ...

1996-09-01

440

Workability and Heat Treatment Characteristics of Beta ...  

Science.gov (United States)

... Accession Number : ADD135317. Title : Workability and Heat Treatment Characteristics of Beta Titanium Alloy, Ti-15V-3Cr-3Sn-3Al,. ...

1986-04-01

441

View larger image for ISS022-E-26137 - Earth Sciences and Image ...  

Science.gov (United States)

The Asarco-Mission complex (image left) is an active producer of copper and molybdenum (important in making steel and other metal alloys), ...

442

The estimation of lifetime distribution of Alloy 800 steam generator tubing  

Energy Technology Data Exchange (ETDEWEB)

Alloy 800 has been used for steam generator (SG) tubing for more than 30 years, primarily in CANDU reactors worldwide and in reactors in Germany. Extensive laboratory testing and in-service experience suggest that the Alloy 800 tubing has excellent resistance to corrosion-related degradation under appropriate operating conditions. In planning refurbishment of nuclear plants stations, a key concern is the longevity of existing SGs up to the 60-year lifetime of the refurbished plant. The paper reviews an existing methodology based on the concept of the improvement factor, and refines its estimation based on data specific to CANDU operating conditions. The paper presents a more advanced Bayesian probabilistic approach to estimate the degradation free lifetime distribution of Alloy 800 tubing, which is used to quantify the probability of degradation during the service life and to evaluate the impact of potential occurrences of ...

2009-10-15

443

The estimation of lifetime distribution of Alloy 800 steam generator tubing  

International Nuclear Information System (INIS)

Alloy 800 has been used for steam generator (SG) tubing for more than 30 years, primarily in CANDU reactors worldwide and in reactors in Germany. Extensive laboratory testing and in-service experience suggest that the Alloy 800 tubing has excellent resistance to corrosion-related degradation under appropriate operating conditions. In planning refurbishment of nuclear plants stations, a key concern is the longevity of existing SGs up to the 60-year lifetime of the refurbished plant. The paper reviews an existing methodology based on the concept of the improvement factor, and refines its estimation based on data specific to CANDU operating conditions. The paper presents a more advanced Bayesian probabilistic approach to estimate the degradation free lifetime distribution of Alloy 800 tubing, which is used to quantify the probability of degradation during the service life and to evaluate the impact of potential occurrences of ...

2009-10-01

444

The Effect of Morpholine/Boric Acid/Hydrazine Chemistry on ...  

Science.gov (United States)

... the effect of MBH on steam generator crevice corrosion; model boiler test results show that MBH is effective against denting corrosion and Alloy 600 ...

445

Surface modification of magnesium base alloys by gas/plasma nitridation  

Energy Technology Data Exchange (ETDEWEB)

Gas and plasma nitriding processes were executed in the magnesium with modification by titanium in search for an effective surface treatment method for magnesium alloys. Magnesium-nitrogen system has completely no solid solution or solubility, so that nitride should be only formed by eutectic reaction in the liquid phase. Hence, magnesium is difficult or nearly impossible to have its surface modified by nitriding. Addition of nitride forming element into magnesium enables us to lower the onset temperature of nitriding. Magnesium-titanium alloys with 1 to 5 wt% are yielded by the bulk mechanical alloying and, subjected to gas nitriding for various process conditions. Successful co-formation of Mg{sub 3}N{sub 2} as well as TiN becomes a proof to demonstrate the possibility of gas/plasma nitriding in the solid-state magnesium with aid of nitride former. (orig.)

2000-07-01

447

Stress, hydrogen segregation, and fracture in #alpha#-#beta# titanium alloys  

International Nuclear Information System (INIS)

Strain embrittlement in Ti base alloys during tensile testing was investigated. Results show that in an #alpha#-#beta# titanium alloy the local activity of H in alpha phase (#alpha#/sub H//sup #alpha#) increases and activity of H in beta phase (#alpha#/sub H//sup #beta#) decreases as the equiaxed #alpha# particle size decreases at constant volume fraction of phases. Thus with decreasing particle size there would be a tendency for H to move from #alpha# to #beta#, decreasing the H content of #alpha#. Also whether H tended to move from #beta# to #alpha# or from #alpha# interiors to the #alpha#-#beta# interface this tendency would be reduced by surface tension effects, making the alloy less susceptible to embrittlement.

448

Protective nitride formation on stainless steel alloys for proton exchange membrane fuel cell bipolar plates  

Energy Technology Data Exchange (ETDEWEB)

Gas nitridation has shown excellent promise to form dense, electrically conductive and corrosion-resistant Cr-nitride surface layers on Ni-Cr base alloys for use as proton exchange membrane fuel cell (PEMFC) bipolar plates. Due to the high cost of nickel, Fe-base bipolar plate alloys are needed to meet the cost targets for many PEMFC applications. Unfortunately, nitridation of Fe-base stainless steel alloys typically leads to internal Cr-nitride precipitation rather than the desired protective surface nitride layer formation, due to the high permeability of nitrogen in these alloys. This paper reports the finding that it is possible to form a continuous, protective Cr-nitride (CrN and Cr{sub 2}N) surface layer through nitridation of Fe-base stainless steel alloys. The key to form a protective Cr-nitride surface layer was found to be the initial formation of oxide during nitridation, ...

2007-01-01

449

Protective nitride formation on stainless steel alloys for proton exchange membrane fuel cell bipolar plates  

Energy Technology Data Exchange (ETDEWEB)

Gas nitridation has shown excellent promise to form dense, electrically conductive and corrosion-resistant Cr-nitride surface layers on Ni-Cr base alloys for use as proton exchange membrane fuel cell (PEMFC) bipolar plates. Due to the high cost of nickel, Fe-base bipolar plate alloys are needed to meet the cost targets for many PEMFC applications. Unfortunately, nitridation of Fe-base stainless steel alloys typically leads to internal Cr-nitride precipitation rather than the desired protective surface nitride layer formation, due to the high permeability of nitrogen in these alloys. This paper reports the finding that it is possible to form a continuous, protective Cr-nitride (CrN and Cr{sub 2}N) surface layer through nitridation of Fe-base stainless steel alloys. The key to form a protective Cr-nitride surface layer was found to be the initial formation of oxide during nitridation, ...

2007-11-22

450

Properties of the passive films formed on ferritic stainless steels in Cl/sup -/ Solutions  

Energy Technology Data Exchange (ETDEWEB)

The pitting resistance of Fe-Cr and Fe-Cr-Mo alloys has been correlated with characteristics of the passive films analyzed by Auger electron spectroscopy (AES). Increased film protectiveness as a result of increased Cr in the alloy can be directly attributed to Cr enrichment of the film and decreased film thickness. Increased Mo in the alloy or passivation at noble potentials promotes passive film resistance to breakdown, but neither does much to change the macrocharacteristics of the film. Rather, it is suggested that the roles of alloying and/or passivation conditions are related to the susceptibility and distribution of weak points of the film. In solutions in which pitting occurs, chloride is generally not incorporated into the film, suggesting that the role of halides is to interact with weak points of the film at the solution/film interface. At 260/sup 0/C, the films are much thicker and likely to ...

1986-10-01

451

Processing of Titanium Alloys.  

Science.gov (United States)

... information about, utilized, or discussed these subjects: basic topics: overview materials and material types: ti-6al-4v, ti1100, ti17 , ti6242, imi 550 ...

452

Phonon - Drag Thermopo wer in Dilute Copper Alloys - NASA ...  

Science.gov (United States)

ing materials were ASARCO, 59 purity, copper, silver and gold, while the silicon was Dow-Corning semi- conductor grade (69 purity). ...

453

Part Repairing Using A Hybrid Manufacturing System (Preprint ...  

Science.gov (United States)

... [11]Richter, K., Orban, S., and Nowotny, S., Laser cladding of the titanium alloy TI6242 to restore damaged blades, Proceedings of the 23rd ...

2007-03-01

454

Osseointegration of zirconia implants compared with titanium: an in vivo study  

UK PubMed Central (United Kingdom)

BackgroundTitanium and titanium alloys are widely used for fabrication of dental implants. Since the material composition and the surface topography of a biomaterial play a fundamental...Full Text Available

456

Manufacturing of oxide-dispersion-strengthened steels with the use of preliminary surface oxidation  

British Library Electronic Table of Contents (United Kingdom)

Regularities of deformation-induced dissolution of a surface layer of iron oxides in matrixes of iron-based alloys with bcc and fcc lattices have been studied by the methods of M?ssbauer spectroscopy, transmission electron microscopy, and X-ray diffraction. A method of producing iron alloys strengthened by dispersed oxide nanoparticles and alloyed with elements possessing a high affinity to oxygen (titanium and yttrium) has been proposed, which implies a dynamic dissolution of a surface layer of iron oxides upon strong cold deformation and a precipitation of secondary yttrium and titanium nanooxides upon a subsequent high-temperature sintering of mechanically alloyed powders. There has been demonstrated a possibility of oxide strengthening of pure iron upon its interaction with air without...

2011-01-01

457

METAShield - NASA Technical Report Server (NTRS)  

Science.gov (United States)

alloy (Ti6242 or T i l 100) was utilized. Parametric studies were performed to investigate variations of displacements and stresses with sandwich and ...

458

Low cost fabrication of sheet structure using a new beta titanium alloy, Ti-15V-3Cr-3Al-3Sn  

Science.gov (United States)

Development efforts have been undertaken to improve the processing and structural efficiencies of

1982-01-01

459

Investigations for judging the working behaviour of components made of alloy 800 and alloy 617 under creep stress. Untersuchungen zur Beurteilung des Betriebsverhaltens kriechbeanspruchter Bauteile aus Alloy 800 und Alloy 617  

Energy Technology Data Exchange (ETDEWEB)

The program introduced here for determining and describing the multi-axial creep of pipes is based, on the one hand, on the results of the nuclear process heat prototype plant material program and, on the other hand, on the possible load conditions which arise for evaluating accidents or extreme working situations. The basis of a theoretical description of multi-axial creep is the invariant theory in which both the von Mises configuration change hypothesis and the Norton creep law are included. Combined tension and torsion are also considered in detail, the superimposition of cyclic stresses in the tensile threshold area is discussed and cases of partial relaxation are explained. Experimental results for the discussed loads are introduced, which have led to satisfactory agreement between theory and experiment. (orig./MM).

1987-01-01

460

Investigation of passive films on nickel Alloy 690 in lead-containing environments  

Energy Technology Data Exchange (ETDEWEB)

Passive films formed on Alloy UNS N06690 were investigated in simulated crevice chemistries. It was found the role of lead in corrosion processes is strongly dependent on the pH value of the testing solutions. At pH 1.5 the effect of lead is narrowly noticeable; while at pH 12.7, lead has a significant influence on the electrochemical performance of alloy UNS N06690. The lead alters the surface morphologies at both pH and account for higher hydroxide content in the surface film at pH 12.7. The lead incorporation hinders the formation of spinel oxides during the passivation in alkaline solution. Nanoindentation tests indicate a significant lead-induced degradation in the mechanical properties of passive films. The passivation degradation is attributed to detrimental effects of lead via interrupting the dehydration process and hindering the formation of protective layers on the alloy surface.

2008-09-01

461

Investigation of erosion-corrosion of 3003 aluminum alloy in ethylene glycol-water solution by impingement jet system  

British Library Electronic Table of Contents (United Kingdom)

Erosion-corrosion (E-C) of 3003 aluminum (Al) alloy in ethylene glycol-water solutions were studied by weight-loss and electrochemical measurements as well as surface characterization through an impingement jet system. Al alloy E-C is dominated by erosion components, i.e., pure erosion and corrosion-enhanced erosion, which account for 92-97% of the total E-C rate under the various conditions in this work. Contribution from corrosion components, including pure corrosion and erosion-enhanced corrosion, is slight. With the increase of fluid flow velocity and sand concentration, the total E-C rate increases. Compared with the significant increase of the rates of erosion components, the increase of the rate of corrosion component is negligible. Upon fluid flow, passivity of Al alloy that develo...

2009-01-01

462

Interfacial ultrafine-grained structures on aluminum alloy 6061 joint and copper alloy 110 joint fabricated by magnetic pulse welding  

British Library Electronic Table of Contents (United Kingdom)

Magnetic pulse welding is a solid state impact welding process, similar to explosive welding, which produces metallurgical bond by oblique high-speed impact between two metal bodies. This violent impact removes the metal surface oxide layers and then joins the two atomic level clean metal surfaces together by the incidental compression pressure. The impact velocity is at 200?400?m/s and the being welded metal surface undergoes severe plastic deformation with strain rate in the order of 106?107?s?1. The ultrafine-grained structure was observed on the welded interface. This article studied two types of similar material lap joint interfaces and the base metals were aluminum alloy 6061 and copper alloy 110. Nano-indentation testing shows that the welded interfaces have significantly greater ha...

2010-01-01

466

Glassy Carbon, Alloys  

Science.gov (United States)

... 2.2.1 Polymerization of DVB Under Pressure DVB was polymerized at 300*C in thin-walled Pd-Ag capsules at pressures up to 60,000 psi. ...

1972-07-27

467

Evaluation method for corrosion resistance of zirconium alloy  

International Nuclear Information System (INIS)

The present invention concerns a method of evaluating corrosion resistance of a zirconium alloy easily and in a short period of time. An anode polarization curve of the zirconium alloy is measured to obtain an anode polarization curve expressed by logarithm. The curve is converted to a potential-current density curve expressed by absolute values. The peak area in the curve of the converted potential-current density is indicated by numerical values. Further, the corrosion resistance of the zirconium alloy is evaluated based on the peak area converted into the numerical values as a reference. This method is based on the finding that the peak area has a close relation with nodular corrosion resistance, and the corrosion resistance can be judged with respect to a specific zircaloy-2. (T.M.).

1993-03-26

471

Effect of welding parameters on hot cracking susceptibility of alloy 800  

Energy Technology Data Exchange (ETDEWEB)

The varestraint cracking test was carried out to assess the hot cracking tendency of alloy 800 at different welding conditions and augmented strain levels. The test results revealed that the hot cracking susceptibility of alloy 800 increases with increasing the heat input and augmented strain levels. This emphasizes the role of constraint either internally induced or externally applied to the welded structure. A cracking threshold or the minimum augmented strain ([epsilon][sub min]) below which no hot cracking takes place has been found to be 0.25 for alloy 800. Also, the Critical Strain Rate to Time (CSS) required to cause cracking was found to be 6.42x10[sup -3] sec[sup -1] at welding condition of 100 Amp, 13 Volt and 140 mm/min. (author).

1994-08-01

472

Effect of welding parameters on hot cracking susceptibility of alloy 800  

International Nuclear Information System (INIS)

The varestraint cracking test was carried out to assess the hot cracking tendency of alloy 800 at different welding conditions and augmented strain levels. The test results revealed that the hot cracking susceptibility of alloy 800 increases with increasing the heat input and augmented strain levels. This emphasizes the role of constraint either internally induced or externally applied to the welded structure. A cracking threshold or the minimum augmented strain (#epsilon#_m_i_n) below which no hot cracking takes place has been found to be 0.25 for alloy 800. Also, the Critical Strain Rate to Time (CSS) required to cause cracking was found to be 6.42x10"-"3 sec"-"1 at welding condition of 100 Amp, 13 Volt and 140 mm/min. (author).

473

Effect of chemical composition on the structure and mechanical properties of Mn-Al-C alloys in the magnetic region  

Energy Technology Data Exchange (ETDEWEB)

The thermal stability and deformability of Mn-Al-C alloys containing 0.6 pct C are investigated experimentally as a function of excess phase content. It is shown that an increase in Mn content from 68.9 to 73.5 pct leads to increased stability of the high-temperature epsilon phase. The enrichment of the system Mn-Al-Cu in Mn and Al above the optimum composition leads to the formation of nonmagnetic excess phases, eta and beta, which reduce the magnetization of the alloy. In addition, a decrease in thermal stability is observed in the alloy with 73.5 pct Mn due to the decomposition of the ferromagnetic phase. 7 references.

1988-01-01

474

Effect of alloying on the phase transformations and properties of a nickel alloy  

Energy Technology Data Exchange (ETDEWEB)

The phase transformations and properties of a precipitation-hardened Ni-Cr-based alloy are investigated as a function of C, B, Nb, and Cr contents. It is found that the primary role of Nb consists in the formation of an independent phase, delta-Ni3Nb, a part of a gamma/gamma-prime-delta eutectoid (for high C and B concentrations) and in stimulating the gamma-sigma reaction consecutively with the gamma double prime-delta reaction (for low C and B concentrations). In both cases, the long-term strength characteristics of the Nb-alloyed system are relatively low. The substitution of boron for carbon contributes to a reduction in the number of nucleation sites for topologically close-packed phases and to the formation of more stable (with respect to excess compounds) M3B2 and MB2 borides. The high-boron material exhibits better properties and phase stability under mechanical and thermal loading. 13 references.

1986-07-01

475

ELECTRICAL AND OPTICAL PROPERTIES OF LEAD-TIN ...  

Science.gov (United States)

... Abstract : Single crystals of Pb(x)Sn(1-x)Te alloy have been grown with o = or thin film evaporator. ...

1969-09-03

476

Dual-ion irradiation effects on microstructure of austenitic alloys  

International Nuclear Information System (INIS)

An Fe-15Cr-20Ni ternary model alloy and a Type 316 stainless steel were irradiated by dual-ions at 1 to 50 appm of He/dpa ratios, to investigate the helium effects on microstructural development in austenitic alloys under irradiation. Quantitative analysis on resultant microstructures revealed that the Frank loop nucleation rate and the network dislocation density positively correlate and Frank loop growth rate negatively correlate with the He/dpa ratio, while the cavity growth rate has its peak at an intermediate helium injection rate. Although He/dpa dependence of various microstructural features were similar for the model alloy and the 316SS, the rates of their development and the mechanism which had assisted cavity growth were significantly different in these two materials. (orig.).

477

Development of materials resistant to metal dusting degradation.  

Energy Technology Data Exchange (ETDEWEB)

Metal dusting corrosion has been a serious problem in the petroleum and petrochemical industries, such as reforming and syngas production systems. This form of deterioration has led to worldwide material loss for 50 years. For the past three years, we have studied the mechanism of metal dusting for Fe- and Ni-base alloys. In this report, we present a correlation between the weight loss and depth of pits that form in Ni-base alloys. Nickel-base alloys were also tested at 1 and 14.8 atm (210 psi), in a high carbon activity environment. Higher system pressure was found to accelerate corrosion in most Ni-base alloys. To reduce testing time, a pre-pitting method was developed. Mechanical scratches on the alloy surface led to fast metal dusting corrosion. We have also developed preliminary data on the performance of weldments of several Ni-base alloys in a metal ...

2006-04-24

478

Creep performance and microstructure of the iron alloy Alloy 800 HT  

International Nuclear Information System (INIS)

The examination of the high-temperature properties of the alloy Alloy 800HT has shown that both the creep performance and the microstructure of the material can be purposefully set by the initial heat treatment. At the high temperatures applied, (700-900 C), a rapid softening process sets in induced by carbide precipitation, stabilization, and coarsening. This softening process causes creep velocities strongly accelerating as a function of duration of the heat treatment prior to the creep test. The identified cause of the softening effect is a change in particle size that could be verified by SEM and TEM. It is shown that two different carbide precipitate size classes are responsible for the softening effect. While the precipitates dectable by TEM become effective primarily via interactions with dislocations, the carbide precipitates detectable only by SEM contribute to a hardening of the grain boundaries and the matrix.(orig./CB)

1997-11-28

479

Corrosion resistance of materials of construction for high temperature sulfuric acid service in thermochemical IS process. Alloy 800, Alloy 600, SUSXM15J1 and SiC  

International Nuclear Information System (INIS)

Exposure tests of candidate materials were carried out up to 1000 hr in the sulfuric acid environments of thermochemical hydrogen production IS process, focusing on the corrosion of welded portion and of crevice area. In the gas phase sulfuric acid decomposition condition at 850degC, welded samples of Alloy 800 and of Alloy 600 showed the same good corrosion resistance as the base materials. In the boiling condition of 95 wt% sulfuric acid solution, test sample of SiC showed the same good corrosion resistance. Also negligible corrosion was observed in crevice corrosion. (author)

2006-07-01

480

Corrosion behaviour of Alloy 800 in high temperature aqueous solutions: Electrochemical studies  

International Nuclear Information System (INIS)

The anodic behaviour and passivity breakdown of Alloy 800 in aqueous solutions of sodium chloride, sodium sulphate and sodium bicarbonate were studied by electrochemical techniques in the temperature range from 60 C to 280 C. The pitting resistance and pitting morphology of the alloy in chloride plus sulphate and chloride plus bicarbonate mixtures, at 60 C and 280 C, were also examined. Increasing bicarbonate or sulphate additions to chloride solutions shift the characteristic pitting potential of Alloy 800 to higher values, both at low and high temperatures. Changes in pitting morphology were observed in sulphate containing solutions while the morphology of the attack found in bicarbonate containing solutions was similar to that in pure chloride solutions. Finally, no localized or substantial generalized corrosion was detected in pure sulphate or bicarbonate solutions at any temperature. (orig.).

481

Corrosion behavior of iron and nickel base alloys in high temperature and pressure water  

International Nuclear Information System (INIS)

In equipment industries, the equipments handling industrial water and pure water are numerous. In power generation including nuclear power generation, water serves as a working medium. Review is made on the experiences in the corrosion of iron and nickel base alloys in high temperature, high pressure water and the results of researches derived from them. Under high temperature and high pressure, carbon steel, low alloy steel, stainless steel and high nickel alloy cause corrosion even in pure water. But in the case of serious corrosion, chlorine, oxygen, alkali and others in water take part. The following matters are described: corrosion by steam; stress corrosion cracking in pure water; corrosion by impurities in high temperature, high pressure pure water, i.e. chlorine ions, dissolved oxygen, and alkali; corrosion under radiation. (J.P.N.).

482

Commercial Contract Training, Marine Corps Area VOTEC ...  

Science.gov (United States)

... Plaster Foundry facings_ Casting: (Non-ferrous Ferrous Alloy .___) Cupola furnace Core baking oven_ _ Metallurgy__ Thermite casting__ ...

1975-06-01

483

Chemical composition and electronic structure of passive films formed on Alloy 600 in acidic solution  

Energy Technology Data Exchange (ETDEWEB)

The chemical composition and the semiconducting properties of passive films formed on nickel based alloy (Alloy 600) in acidic sulphate solution, pH 2.0 at room temperature were studied using Auger analysis, voltammetric techniques and the Mott-Schottky approach. The results obtained revealed that the presence of both chromium and mixed nickel-iron oxides in the films leads to the development of a p-n heterojunction, which controls their electronic structure, similarly manner to the case of stainless steels and Alloy 600 in borate buffer solution. This behavior has been interpreted as representing of an oxide system, which has a duplex character, with an inner p-type semiconducting region, mainly formed by chromium oxide and an outer n-type semiconducting region, containing iron oxide. It could also be observed that the nickel oxide present in the films acts as a barrier layer conferring improved protection.

2008-03-15

484

Chemical composition and electronic structure of passive films formed on Alloy 600 in acidic solution  

International Nuclear Information System (INIS)

The chemical composition and the semiconducting properties of passive films formed on nickel based alloy (Alloy 600) in acidic sulphate solution, pH 2.0 at room temperature were studied using Auger analysis, voltammetric techniques and the Mott-Schottky approach. The results obtained revealed that the presence of both chromium and mixed nickel-iron oxides in the films leads to the development of a p-n heterojunction, which controls their electronic structure, similarly manner to the case of stainless steels and Alloy 600 in borate buffer solution. This behavior has been interpreted as representing of an oxide system, which has a duplex character, with an inner p-type semiconducting region, mainly formed by chromium oxide and an outer n-type semiconducting region, containing iron oxide. It could also be observed that the nickel oxide present in the films acts as a barrier layer conferring improved protection.

2008-03-01

485

Caustic stress corrosion cracking studies at 288 C (550 F) using the straining electrode technique--comparison of Alloy 600, Alloy 800, and Type 304 stainless steel  

International Nuclear Information System (INIS)

Constant pull rate tests were conducted on tensile specimens of Inconel Alloy 600, Incoloy Alloy 800, and Type 304 stainless steel in deaerated 10% NaOH solution at 288 C (550 F) with a cover gas of 5% H_2 in N_2. The pull rate used for most experiments was 3.3 x 10"-"6 cm/s, which corresponds to an initial strain rate of 3 x 10"-"6 s"-"1. The electrical potential of the specimens was controlled by a potentiostat using a nickel wire as a hydrogen reference electrode. Under open circuit conditions, Type 304 stainless steel specimens cracked rapidly, but Alloys 600 and 800 specimens exhibited only ductile fracture. However, cracks readily formed in Alloy 800 specimens at potentials in the +50 to +300 mV range and in Alloy 600 specimens at potentials in the +150 to +250 mV range. Scanning electron microscope (SEM) photographs of some of the cracked specimen surfaces showed the ...

486

Carnegie -Mellon University - NASA Technical Report Server (NTRS)  

Science.gov (United States)

Procedures for a New High-Strength, Beta Titanium Alloy having. Superior Formability, " Technical Report AFML-TR-69-171, Air ...

487

Assessment of effects of Fort St. Vrain HTGR primary coolant on Alloy 800. Final report  

Energy Technology Data Exchange (ETDEWEB)

A comprehensive review was conducted of primary helium coolant chemistry data, based on current and past operating histories of helium-cooled, high-temperature reactors (HTGRs), including the Fort St. Vrain (FSV) HTGR. A reference observed FSV reactor coolant environment was identified. Further, a slightly drier expected FSV coolant chemistry was predicted for reactor operation at 100% of full power. The expected environment was compared with helium test environments used in the US, United Kingdom, Germany, France, and Japan. Based on a comprehensive review and analysis of mechanical property data reported for Alloy 800 tested in controlled-impurity helium environments (and in air when appropriate for comparison), an assessment was made of the effect of FSV expected helium chemistry on material properties of alloy 800, with emphasis on design properties of the Alloy 800 material utilized in the FSV steam generators.

1982-08-01

488

Assessment of effects of Fort St. Vrain HTGR primary coolant on Alloy 800. Final report  

International Nuclear Information System (INIS)

A comprehensive review was conducted of primary helium coolant chemistry data, based on current and past operating histories of helium-cooled, high-temperature reactors (HTGRs), including the Fort St. Vrain (FSV) HTGR. A reference observed FSV reactor coolant environment was identified. Further, a slightly drier expected FSV coolant chemistry was predicted for reactor operation at 100% of full power. The expected environment was compared with helium test environments used in the US, United Kingdom, Germany, France, and Japan. Based on a comprehensive review and analysis of mechanical property data reported for Alloy 800 tested in controlled-impurity helium environments (and in air when appropriate for comparison), an assessment was made of the effect of FSV expected helium chemistry on material properties of alloy 800, with emphasis on design properties of the Alloy 800 material utilized in the FSV steam generators.

489

Application of alloy 800 in PWRs  

International Nuclear Information System (INIS)

Alloy 800 has been used by Siemens since 1968 and is now used by KWU for U-tubed steam generators in PWR's. The particular grade of alloy 800 that is used is within the ASTM-Specification B 163, but there have been modifications in composition to improve the corrosion resistance. First the permitted upper limit of carbon was reduced to 0.04% and was then further reduced to 0.03% and a stabilisation ratio of Ti : C >= 12 and Ti : C + N >= 8 was specified. The minimum permitted chromium and nickel levels were increased to 20% and 32% respectively. The maximum permitted levels of other elements or impurities were reduced. At the final fabrication stage peening with glass beads on the outer surface was specified to introduce a compressive stress to depth greater than that allowed for production flaws. An account is given of the behaviour of the alloy in service in four power plants already in operation, and future ...

490

Analysis of the fatigue strength of welded joints produced by different techniques in materials of the type 'alloy 800'  

International Nuclear Information System (INIS)

The alloy type 'alloy 800' with its different variants is used for numerous components in high-temperature reactor (HTR) plants, e.g. for hot-gas conductors, the high-pressure part of steam generators, superheaters, steam collecting vessels and live steam conductors. This study deals with the evaluation of creep rupture tests on 28 welded joints of alloy 800 with an accumulated test duration of 410 years, with the objective to obtain quantitative information on a possible loss of strength in comparison with the unwelded material. The longest test period of an individual test amounted to 98,000 h and the analyzed test temperature range lay between 550"0 and 1000"0C. (orig./MM).

1988-11-25

491

Analysis of the creep strain-time behavior of alloy 800  

Energy Technology Data Exchange (ETDEWEB)

The high-nickel austenitic alloy 800 (in both the mill-annealed and the solution-treated grades) has several attractive properties that make it a good candidate for service attractive properties that make it a good candidate for service at elevated temperatures in corrosive environments. One such property is creep resistance. This report analyzes the elevated-temperature creep behavior of the mill-annealed grade, generally referred to simply as alloy 800. (The solution-treated grade is known as alloy 800H). Available data over the temperature range from 538 to 760/sup 0/C were collected and evaluated to yield mathematically approximations for creep-rupture and strain-time behavior for use in design calculations. However, the creep behavior of this material is extremely complex, and the analysis presented here contains substantial uncertainties. All results in this report should be considered preliminary because of limited ...

1983-05-01

492

Amorphization of Zr_6_0Al_1_5Ni_2_5 surface layers by laser processing for corrosion resistance  

International Nuclear Information System (INIS)

It is generally known that a number of metallic glasses have excellent corrosion resistance in a variety of chemically hostile environments. Consequently, the use of laser cladding to coat a massive crystalline material such as aluminium with a layer of a metallic glass has obvious advantages. In this paper, the authors will show that the formation of a predominantly amorphous layer of Zr_6_0Al_1_5NI_2_5 alloy by laser processing is possible, if the obstacles to amorphization are overcome. In addition, evidence of the excellent corrosion resistance of this alloy in a NaCl solution will be given. A comparative study of the corrosion behavior of this amorphous alloy with pure aluminium and Al-Cr alloy will be done, in order to complete previous studies of laser processed coatings of aluminum substrates.

493

Alpha/Beta Heat Treatment of a Titanium Alloy with a Non ...  

Science.gov (United States)

... transformed at 705°C. The cooling rate and temperature dependence of matrix decomposition for Ti6242 was thus similar to that for Ti64 x [9]. ...

2006-08-01

494

Alloying element diffusion in alloy 800 H (UNS N08810) and alloy 617 (UNS N06617)  

Energy Technology Data Exchange (ETDEWEB)

Samples of alloy 800 H (LJNS N08810) and alloy 617 (UNS N06617) were oxidized in a simulated process gas atmosphere. The principal elements of the gaseous environment were 50% H{sub 2}O, 35% H{sub 2} and 5% of CO{sub 2}, CO, and CH{sub 4}, respectively. The experiments were carried out at temperatures from 850 C to 950 C for exposures ranging from 600 to 5,000 hours. After the exposure, the alloy surfaces showed compact oxide layers, which resulted in a depleted zone of oxidizing elements in the substrate layer. Using Electron Probe Microanalysis (EPMA), concentration profiles and the extension of the depleted zone were measured. Calculated theoretical profiles were then fitted to the EPMA-measured profiles, using Fick`s second law of diffusion and resolved by a finite difference method and diffusion coefficients as fitting parameters. The diffusion coefficients for chromium may be represented as D = Do exp.(-Q/RT) with the ...

1996-10-01

495

Alloy 800 welding experience at UKAEA Springfields  

International Nuclear Information System (INIS)

Investigatins into the welding of alloy 800 at the Reactor Fuel Element Laboratories, Springfields, commenced about three years ago following an extended development programme on tube to tube plate welding of low alloy and stainless steels for the Prototype Fast Reactor. The techniques and approach developed for critical fuel element welding applications had proved equally suitable for the precision welding requirements on the much heavier sections of heat exchangers. It had been demonstrated that the same control of weld quality and profile could be achieved with consistency and the permissible range of critical parameters could be readily defined. Because of this, development work was continued to include other materials, such as alloy 800, which might be of potential use. The tungsten inert gas (T.I.G.) arc welding process is used, and the equipment, including the control system, is described. Tube to tube-plate welding, ...

497

A probabilistic approach to the estimation of lifetime distribution of Alloy 800 SG tubing  

Energy Technology Data Exchange (ETDEWEB)

Alloy 800 has been used for steam generator (SG) tubing for more than 30 years, primarily in CANDU reactors and in reactors in Germany. Extensive laboratory testing and in-service experience suggest that the Alloy 800 tubing has excellent resistance to corrosion-related degradation under specified and appropriate operating conditions. In planning refurbishment of CANDU stations, a key concern is the longevity of existing SGs up to the 60 year lifetime of the refurbished plant. The paper reviews an existing methodology based on the concept of the improvement factor, and estimates it based on experimental data specific to CANDU operating conditions. The paper presents a more advanced probabilistic approach to estimate the degradation free lifetime distribution of Alloy 800 tubing, which is used to quantify the probability of degradation during the service life and to evaluate the impact of potential occurrences of degradation ...

2008-07-01

498

A probabilistic approach to the estimation of lifetime distribution of Alloy 800 SG tubing  

International Nuclear Information System (INIS)

Alloy 800 has been used for steam generator (SG) tubing for more than 30 years, primarily in CANDU reactors and in reactors in Germany. Extensive laboratory testing and in-service experience suggest that the Alloy 800 tubing has excellent resistance to corrosion-related degradation under specified and appropriate operating conditions. In planning refurbishment of CANDU stations, a key concern is the longevity of existing SGs up to the 60 year lifetime of the refurbished plant. The paper reviews an existing methodology based on the concept of the improvement factor, and estimates it based on experimental data specific to CANDU operating conditions. The paper presents a more advanced probabilistic approach to estimate the degradation free lifetime distribution of Alloy 800 tubing, which is used to quantify the probability of degradation during the service life and to evaluate the impact of potential occurrences of degradation ...

2008-06-01

500

8 - NASA Technical Reports Server  

Science.gov (United States)